Aluminum alloy component casting mold

By adopting a cooling structure and a retaining ring heat dissipation structure in the aluminum alloy wheel hub casting mold, combined with the linkage structure of the side mold, efficient mold release operation is achieved, solving the low mold release efficiency and high risk of blank drop in the prior art. The problem has improved the cooling and solidification efficiency of aluminum alloy wheel hubs and the cost-effectiveness of mold manufacturing.

CN118080825BActive Publication Date: 2024-11-01KUNSHAN ZHONGYITE MACHINERY IND
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410118397.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-01-29
Publication Date
2024-11-01
Estimated Expiration
2044-01-29

AI Technical Summary

Technical Problem

Existing aluminum alloy wheel casting molds are inefficient during the release process and have high risk of blank drop.

Method used

A cast mold of aluminum alloy component including top mold, base, bottom mold and side mold is designed. The cooling structure and the retaining ring heat dissipation structure are adopted. The retaining ring heat dissipation structure is converted into Hydraulic mold release structure, which uses hydraulic drive blank to release mold from the bottom mold.

Benefits of technology

It improves the demolding efficiency, reduces the risk of blank drop, and accelerates the cooling and solidification efficiency of aluminum alloy wheel hubs during the cooling and solidification stage, reducing mold manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118080825B_ABST
    Figure CN118080825B_ABST
Patent Text Reader

Abstract

The invention provides a casting forming mold for an aluminum alloy component, and relates to the technical field of aluminum alloy wheel hub casting molds. The mold comprises a top mold, a base, a bottom mold, and a side mold. A cooling plate is arranged inside the side mold, and cooling structures are arranged in the top mold, the bottom mold, and the cooling plate. A retaining ring heat dissipation structure is arranged inside the bottom mold, and the retaining ring heat dissipation structure is used to cool a blank through the bottom mold, and can assist in demolding the blank. Through the above technical scheme, its purpose is that the retaining ring heat dissipation structure is arranged in the water cooling stage of the blank, and cools the retaining ring part of the wheel hub on the bottom mold by injecting coolant into the heat dissipation cavity through a rhombus shell, and in the process of dispersing the side mold, the lower layer part of the partition plate in the heat dissipation cavity is pressurized by a booster pipe fitting, so as to drive the demolding top ring and the blank to be lifted, and demolded from the bottom mold. The structure is reasonably distributed and occupies a small space.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of aluminum alloy wheel hub casting molds, in particular to an aluminum alloy component casting molding mold. Background Art

[0002] The automobile aluminum alloy wheel hub is integrally cast. The aluminum alloy melt liquid is poured into the wheel hub mold, and then demoulded after solidification through water cooling. It is also manufactured through precision machining and surface treatment.

[0003] In the prior art, during the demolding process of the aluminum alloy wheel hub casting mold, after the driving mold is dispersed, the blank is moved out with the top mold and demolded through the ejection structure. The demolding efficiency is low and the risk of the blank falling is high. Therefore, the present invention proposes an aluminum alloy component casting mold. Summary of the invention

[0004] The purpose of the present invention is to solve the shortcomings of the prior art in that during the demoulding process of the aluminum alloy wheel hub blank in the casting mold, after the driving mold is dispersed, the blank is moved out with the top mold and then demoulded through the ejection structure, resulting in low demoulding efficiency and high risk of the blank falling.

[0005] In order to achieve the above-mentioned purpose, the present invention adopts the following technical scheme: a casting mold for an aluminum alloy component, comprising a top mold, a base, a bottom mold, and a side mold, wherein a cooling plate is arranged inside the side mold, and cooling structures are arranged in the top mold, the bottom mold, and the cooling plate, and a retaining ring heat dissipation structure is arranged inside the bottom mold, and the retaining ring heat dissipation structure is used to cool the blank through the bottom mold and assist the blank in demolding; the retaining ring heat dissipation structure comprises four heat dissipation cavities opened in the bottom mold, and the interiors of the heat dissipation cavities are all sealed and slidably connected with partition plates, and a demolding top ring is arranged on the top of the bottom mold, and the demolding top ring is fixed to the partition plate The interior of the heat dissipation cavity is divided into an upper and lower layer by a partition plate. A U-shaped tube is fixedly connected on the outer wall of the heat dissipation cavity for connecting the upper and lower cavities of the partition plate. Both ends of the U-shaped tube connected to the heat dissipation cavity are slidably connected with movable blocking balls. The upper and lower layers of the heat dissipation cavity are respectively connected with a liquid outlet short tube and a liquid inlet short tube. The heat dissipation cavity is fixedly connected with a boosting pipe fitting through the liquid inlet short tube. A linkage structure is transmission-connected on the outer wall of the side mold. The boosting pipe fitting is transmission-connected to the side mold through the linkage structure. The boosting pipe fitting can use the power of the side mold to pressurize the coolant in the lower cavity of the partition plate.

[0006] Furthermore, the boost pipe fitting includes a diamond-shaped shell, which is installed on a base, and the two sides of the interior of the diamond-shaped shell are respectively connected to the injection pipe and the liquid guiding pipe, and a boost cavity is opened inside the diamond-shaped shell, and the boost cavity is located between the injection pipe and the liquid guiding pipe. The interior of the boost cavity is sealed and slidably connected with a boost piston, and an injection hole is opened between the bottom mold and the injection pipe, and the injection hole is located at one end of the boost cavity, and a drainage hole is opened between the other end of the boost cavity and the liquid guiding pipe, and the liquid guiding pipe is connected to the liquid inlet short pipe.

[0007] Furthermore, there are two injection holes, and the boosting cavity is provided with a buffer section between the two injection holes. The buffer section is used to balance the internal hydraulic pressure of the boosting piston when the boosting piston moves between the two injection holes, provide a buffer distance, and then pressurize the interior of the lower cavity of the partition plate after the side mold is completely separated from the blank.

[0008] Furthermore, a push rod is fixedly connected to the outer side wall of the movable blocking ball, and the push rod is sealingly and slidably connected to the U-shaped tube. The end of the push rod away from the movable blocking ball is fixedly connected to a trigger top plate. The trigger top plate is used to push the movable blocking ball to slide out of the U-shaped tube through the push rod when the side mold is closed, so that the U-shaped tube can connect the upper and lower chambers of the partition plate. A spring is fixedly connected between the trigger top plate and the outer side wall of the U-shaped tube. The spring is used to drive the movable blocking ball into the internal closed tube mouth of the U-shaped tube through the trigger top plate when the side mold is dispersed.

[0009] Furthermore, the upper surface of the demoulding top ring is an inclined surface, which is used for sealing connection with the bottom mold and the demoulding top ring when the side mold is closed.

[0010] Furthermore, the cooling structure includes a cooling cavity, a water injection pipe and a water discharge pipe. The top mold, the bottom mold, the side mold and the cooling plate are all provided with cooling cavities. The cooling cavity inside the cooling plate is connected with the cooling cavity inside the side mold. The cooling cavities on the top mold are connected to each other through two annular tubes. The cooling cavities on the bottom mold are connected to each other through two annular tubes. The cooling cavities on the side mold and the cooling plate are connected to each other. The annular tubes are respectively connected with a water injection pipe and a water discharge pipe.

[0011] Furthermore, the cavities on the top mold and the bottom mold are used to cool the spoke portion of the blank, and the cavities on the side molds and the cooling plate are used to cool the bead seat portion of the blank.

[0012] Furthermore, the liquid inlet short pipes on two adjacent heat dissipation chambers are connected to each other, and the liquid outlet short pipes on two adjacent heat dissipation chambers are connected to each other.

[0013] Furthermore, the linkage structure includes a linkage slide, a directional slide groove and a driving rod. The side wall of the base is provided with a directional slide groove, the interior of the directional slide groove is slidably connected with a linkage slide, the upper surface of the linkage slide is fixedly connected with a driving rod, the driving rod is transmission connected to the side mold, the linkage slide is fixedly connected to a component in the boosting pipe fitting, and the linkage slide is transmission connected to the side mold through the driving rod, so as to provide power to the boosting pipe fitting.

[0014] Compared with the prior art, the advantages and positive effects of the present invention are:

[0015] 1. In the present invention, the blank is cooled and cooled on the top mold, the bottom mold and the side mold by means of a cooling structure, and the cooling and solidification efficiency of the hub is accelerated by setting a retaining ring heat dissipation structure. After the side mold is dispersed, the movement and linkage structure of the side mold are utilized to convert the retaining ring heat dissipation structure into a hydraulic structure for driving the demoulding top ring to drive the blank to be demoulded from the bottom mold. The blank is directly demoulded during the dispersion of the side mold, thereby improving the efficiency of demoulding the blank.

[0016] 2. In the present invention, the heat dissipation structure of the retaining ring is set up. During the water cooling stage of the blank, the coolant is injected into the heat dissipation cavity through the diamond-shaped shell, and the retaining ring part of the hub is cooled on the bottom mold. In the process of side mold dispersion, the lower part of the partition plate in the heat dissipation cavity is pressurized by the booster pipe fitting, which drives the demoulding top ring and the blank to be ejected from the bottom mold. The structure is reasonably distributed and occupies little space.

[0017] 3. In the present invention, the setting of the heat dissipation structure of the retaining ring not only accelerates the solidification of the blank, but also can lift the blank for demoulding and use, thereby reducing the mold manufacturing cost.

[0018] 4. In the present invention, the cooling cavities at the spoke positions on the top mold and the bottom mold are interconnected through an annular tube, and cooling water is introduced into each cavity at the same time through a water injection pipe to act on the spoke position of the blank. After cooling water is injected into the cooling cavities on the side mold and the cooling plate at the same time, it acts on the tire bead seat position synchronously, thereby improving the cooling and shaping effect of the blank. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 The present invention provides an overall three-dimensional schematic diagram of a casting mold for an aluminum alloy component;

[0020] Figure 2 An exploded diagram of a casting mold for an aluminum alloy component is provided for the present invention;

[0021] Figure 3 The present invention provides a schematic structural diagram of a bottom mold and a cooling plate in a casting mold for an aluminum alloy component;

[0022] Figure 4The present invention provides a schematic structural diagram of a side mold and a cooling plate in a casting mold for an aluminum alloy component;

[0023] Figure 5 The present invention provides a schematic structural diagram of a top die of an aluminum alloy component casting mold;

[0024] Figure 6 The present invention provides a bottom structure schematic diagram of a bottom mold in a casting mold for an aluminum alloy component;

[0025] Figure 7 The present invention provides a schematic diagram of the bottom structure of a side mold and a push rod in a casting mold for an aluminum alloy component;

[0026] Figure 8 The present invention provides a schematic structural diagram of a heat dissipation structure of a bottom mold and a retaining ring in a casting mold for an aluminum alloy component;

[0027] Fig. 9 The present invention proposes an exploded diagram of a heat dissipation structure of a bottom mold and a retaining ring in a casting mold for an aluminum alloy component;

[0028] Fig.10 The present invention provides a schematic structural diagram of a heat dissipation structure of a retaining ring in a casting mold for an aluminum alloy component;

[0029] Fig.11 for Fig.10 Enlarged schematic diagram of part A.

[0030] Legend: 1. Top mold; 11. Base;

[0031] 2. Bottom mold; 21. Side mold; 22. Cooling plate;

[0032] 3. Cooling chamber; 31. Ring pipe; 32. Water injection pipe; 33. Water discharge pipe;

[0033] 4. Heat dissipation structure of retaining ring; 41. Heat dissipation cavity; 42. Partition plate; 43. Demolding top ring; 44. U-shaped tube; 45. Movable blocking ball; 46. Liquid inlet short tube; 47. Liquid outlet short tube;

[0034] 5. Pressurized pipe fittings; 51. Liquid injection pipe; 52. Pressurized cavity; 53. Pressurized piston; 54. Liquid guide pipe; 55. Buffer section; 56. Liquid injection hole; 57. Liquid discharge hole;

[0035] 6. linkage structure; 61. linkage slide plate; 62. directional slide groove; 63. driving rod;

[0036] 7. Push rod; 71. Trigger top plate; 72. Spring. DETAILED DESCRIPTION

[0037] In order to more clearly understand the above-mentioned purpose, features and advantages of the present invention, the present invention is further described below in conjunction with the accompanying drawings and embodiments. It should be noted that the embodiments of the present application and the features in the embodiments can be combined with each other without conflict.

[0038] In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention may also be implemented in other ways than those described herein. Therefore, the present invention is not limited to the specific embodiments of the following disclosure.

[0039] Aluminum alloy wheel casting molds are usually equipped with cooling structures to accelerate the cooling and solidification of aluminum alloy parts. The cooling cavities opened inside the top mold, bottom mold and side molds occupy a lot of space. During the demolding process, if the matching demolding parts are independently set outside the top mold, the production cost will increase and the demolding operation steps will be cumbersome. If the ejector parts are set inside the top mold, the space of the cooling cavity will be occupied and the cooling effect will be reduced.

[0040] To this end, an embodiment of the present invention provides a casting mold for an aluminum alloy component, the purpose of which is at least to reserve the required space for the cooling structure and ensure the cooling effect of the cooling structure, while simplifying the demolding operation steps and improving the demolding efficiency.

[0041] Embodiment, according to Figure 1 - Fig.11 ,like Figure 1 and Figure 2 As shown in, an aluminum alloy component casting mold provided by an embodiment of the present invention includes a top mold 1, a base 11, a bottom mold 2, and a side mold 21, wherein a cooling plate 22 is arranged inside the side mold 21, and cooling structures are arranged in the top mold 1, the bottom mold 2 and the cooling plate 22, and a retaining ring heat dissipation structure 4 is arranged inside the bottom mold 2, and the retaining ring heat dissipation structure 4 is used to cool the blank through the bottom mold 2, and can assist the blank in demolding; as shown in Figure 8-10In the embodiment, the retaining ring heat dissipation structure 4 includes four heat dissipation cavities 41 opened in the bottom mold 2, the interiors of the heat dissipation cavities 41 are sealed and slidably connected with partition plates 42, the top of the bottom mold 2 is provided with a demoulding top ring 43, the demoulding top ring 43 is fixedly connected to the partition plates 42, the interiors of the heat dissipation cavities 41 are divided into upper and lower layers by the partition plates 42, the outer wall of the heat dissipation cavity 41 is fixedly connected with a U-shaped tube 44 for connecting the upper and lower cavities of the partition plates 42, both ends of the U-shaped tube 44 connected to the heat dissipation cavity 41 are slidably connected with movable blocking balls 45, the upper and lower layers of the heat dissipation cavity 41 are respectively connected with a liquid outlet short tube 47 and a liquid inlet short tube 46, the heat dissipation cavity 41 is fixedly connected with a booster pipe 5 through the liquid inlet short tube 46, the outer wall of the side mold 21 is transmission-connected with a linkage structure 6, the booster pipe 5 is transmission-connected with the side mold 21 through the linkage structure 6, the The booster pipe 5 can use the power of the side mold 21 to boost the coolant in the lower cavity of the partition plate 42. When the side mold 21 is dispersed, the movable blocking ball 45 blocks the U-shaped tube 44, and the coolant is squeezed into the lower cavity of the partition plate 42 through the booster pipe 5 and the liquid inlet short tube 46 to increase the hydraulic pressure of the lower layer of the partition plate 42, thereby lifting the blank through the demoulding top ring 43 to separate the blank from the bottom mold 2, and when the side mold 21 is closed, the partition plate 42 is extracted. The cooling liquid in the lower cavity of the plate 42 drives the demoulding top ring 43 to reset, so that the top mold 1, the bottom mold 2, the side mold 21 and the demoulding top ring 43 are sealed and connected. In the cooling and solidification stage, the cooling liquid is injected into the cavity of the lower layer of the demoulding top ring 43 through the booster pipe 5 and the liquid inlet short pipe 46. The cooling liquid enters the upper cavity of the partition plate 42 through the U-shaped tube 44, exchanges heat with the bottom mold 2, and improves the cooling and solidification fixing effect on the retaining ring part of the aluminum alloy wheel hub blank.

[0042] like Figure 6 and Figure 8 In the embodiment, the liquid inlet short tubes 46 on two adjacent heat dissipation chambers 41 are connected to each other, and the liquid outlet short tubes 47 on two adjacent heat dissipation chambers 41 are connected to each other; Figure 8 and Fig. 9 In the figure, the upper surface of the demolding top ring 43 is an inclined surface, which is used to seal and connect the side mold 21 with the bottom mold 2 and the demolding top ring 43 when the side mold 21 is closed. When the side mold 21 is closed, pressure is applied along the inclined surface of the demolding top ring 43 to improve the sealing performance of the bottom mold 2, the side mold 21 and the demolding top ring 43.

[0043] like Fig.11In the embodiment, the pressurizing pipe 5 comprises a diamond-shaped shell, which is mounted on the base 11. The two sides of the interior of the diamond-shaped shell are connected to the injection pipe 51 and the liquid guide pipe 54 respectively. A pressurizing cavity 52 is provided inside the diamond-shaped shell. The pressurizing cavity 52 is located between the injection pipe 51 and the liquid guide pipe 54. A pressurizing piston 53 is sealed and slidably connected inside the pressurizing cavity 52. ​​An injection hole 56 is provided between the bottom mold 2 and the injection pipe 51. The injection hole 56 is located at one end of the pressurizing cavity 52. ​​A discharge hole 56 is provided between the other end of the pressurizing cavity 52 and the liquid guide pipe 54. The liquid hole 57, the liquid guide pipe 54 is connected with the liquid inlet short tube 46, and when the side mold 21 is dispersed, it can drive the boosting piston 53 to move in the boosting cavity 52, one side of the boosting piston 53 squeezes the coolant, and enters the liquid guide pipe 54 through the discharge hole 57, and is injected into the lower cavity of the partition plate 42 through the liquid guide pipe 54 and the liquid inlet short tube 46, and the other side of the boosting piston 53 is replenished with cooling liquid through the injection hole 56 to balance the internal hydraulic pressure of the boosting cavity 52; the injection hole 56 is provided with two, and the boosting cavity 52 is provided with a buffer section 55 (such as Fig.11 The buffer section 55 is used to balance the internal hydraulic pressure of the booster piston 53 when the booster piston 53 moves between the two injection holes 56, provide a buffer distance, and then pressurize the interior of the lower cavity of the partition plate 42 after the side mold 21 is completely separated from the blank.

[0044] like Fig.10In the embodiment, the outer side wall of the movable blocking ball 45 is fixedly connected with a push rod 7, and the push rod 7 is sealingly and slidably connected to the U-shaped tube 44. The end of the push rod 7 away from the movable blocking ball 45 is fixedly connected with a trigger top plate 71. The trigger top plate 71 is used to push the movable blocking ball 45 to slide out of the U-shaped tube 44 through the push rod 7 when the side mold 21 is closed, so that the U-shaped tube 44 can connect the upper and lower chambers of the partition plate 42. A spring 72 is fixedly connected between the trigger top plate 71 and the outer side wall of the U-shaped tube 44. The spring 72 is used to drive the movable blocking ball 45 to enter the internal closed pipe mouth of the U-shaped tube 44 through the trigger top plate 71 when the side mold 21 is dispersed. In the initial stage of dispersion of the side mold 21, before the movable blocking ball 45 enters the U-shaped tube 44 for blocking, the booster pipe 5 moves toward the partition plate When the coolant is squeezed into the lower layer of the partition plate 42, the coolant in the lower chamber of the partition plate 42 can still enter the upper chamber of the partition plate 42 through the U-tube 44 to balance the internal hydraulic pressure of the heat dissipation cavity 41. It should be noted that in the stage of closing the side mold 21, when the side mold 21 does not drive the movable blocking ball 45 to disengage from the U-tube 44 by pushing the trigger top plate 71, the upper and lower layers of the partition plate 42 are in a sealed isolation state, so that the booster pipe 5 extracts excessive coolant from the lower cavity of the partition plate 42, so that the internal hydraulic pressure of the lower cavity of the partition plate 42 is in a negative pressure state, thereby ensuring that before the side mold 21 is closed, the partition plate 42 has driven the demolding top ring 43 to seal and merge with the bottom mold 2, so that after the side mold 21 is closed, the U-tube 44 is in a connected state, balancing the internal hydraulic pressure difference between the upper and lower layers of the partition plate 42, and ensuring that the next demolding operation is carried out normally.

[0045] like Figure 2 In the figure, the linkage structure 6 includes a linkage slide 61, a directional slide groove 62 and a driving rod 63. The side wall of the base 11 is provided with a directional slide groove 62. The linkage slide 61 is slidably connected inside the directional slide groove 62. The upper surface of the linkage slide 61 is fixedly connected with the driving rod 63. The driving rod 63 is transmission-connected to the side mold 21. The linkage slide 61 is fixedly connected to the components in the boost pipe fitting 5. The linkage slide 61 is transmission-connected to the side mold 21 through the driving rod 63, which is used to provide power to the boost pipe fitting 5. When the side mold 21 disperses to the outside, the two side molds 21 simultaneously pull the driving rod 63 at the angle position to move outward. The driving rod 63 pulls the boost piston 53 to move through the linkage slide 61, squeezes the coolant into the heat dissipation chamber 41, and when the side mold 21 is reset, it pulls the boost piston 53 at the angle position to move, and extracts the coolant inside the heat dissipation chamber 41.

[0046] like Figure 3-7In the embodiment, the cooling structure includes a cooling cavity 3, a water injection pipe 32 and a water discharge pipe 33. The top mold 1, the bottom mold 2, the side mold 21 and the cooling plate 22 are all provided with cooling cavities 3. The cooling cavity 3 inside the cooling plate 22 is connected with the cooling cavity 3 inside the side mold 21. The cooling cavities 3 on the top mold 1 are interconnected through two annular tubes 31. The cooling cavities 3 on the bottom mold 2 are interconnected through two annular tubes 31. The cooling cavities 3 on the side mold 21 and the cooling plate 22 are interconnected. The annular tubes 31 are respectively connected with a water injection pipe 32 and a water discharge pipe 33. The cavities on the top mold 1 and the bottom mold 2 are used to cool the spoke part of the blank. The cavities on the side mold 21 and the cooling plate 22 are used to cool the tire bead seat part of the blank.

[0047] In this embodiment, cooling water is introduced into the cavities inside the top mold 1, the bottom mold 2, the side mold 21, and the cooling plate 22 through the water injection pipe 32. The water injection pipe 32 introduces the cooling water into the cooling cavities 3 on the top mold 1 and the bottom mold 2 at the same time through the annular pipe 31, and discharges the cooling water through the annular pipe 31 and the drain pipe 33 connected to the cooling cavity 3. The cooling water flows continuously, thereby cooling the spokes of the blank in each cooling cavity 3 at the same time. The water injection pipe 32 introduces cooling water into the cooling cavity 3 in the side mold 21 and the cooling plate 22, so that the cooling water enters the cooling cavity 3 located at the tire bead seat position of the blank, and cools the tire bead seat part of the blank. The coolant is introduced into the heat dissipation cavity 41 through the liquid inlet short tube 46 and then discharged through the liquid outlet short tube 47 to cool the retaining ring part of the blank. The cooling cavity 3 covers the inner and outer sides of the blank in a large range, and performs cooling and cooling treatment simultaneously, thereby improving the efficiency of cooling and solidifying the blank.

[0048] In this embodiment, during the demoulding process of the mold, Figure 2 As shown, after the top mold 1 rises, the lower retaining ring of the wheel hub is located between the bottom mold 2 and the side mold 21, so it can be directly separated from the blank, and then the side mold 21 is controlled to disperse synchronously to the surroundings. The side mold 21 drives the blank to be lifted on the bottom mold 2 while dispersing through the retaining ring heat dissipation structure 4, the boost pipe 5 and the linkage structure 6, thereby completing the demolding of the blank.

[0049] In this embodiment, during the cooling and solidification stage of the blank, cooling water is injected into the cooling cavity 3 through the water injection pipe 32 and discharged through the water discharge pipe 33, and the cooling water is continuously circulated through the cooling cavity 3 in the top mold 1, the bottom mold 2, the side mold 21 and the cooling plate 22 to cool the inner and outer sides of the blank to solidify the aluminum alloy wheel hub; Fig.11 In the embodiment, the head of the boosting piston 53 is located between the two injection holes 56, so that the coolant injected into the boosting cavity 52 through the injection pipe 51 and the injection hole 56 enters the liquid guide pipe 54 through the drainage hole 57, and enters the lower layer of the partition plate 42 in the heat dissipation cavity 41 through the liquid guide pipe 54 and the liquid inlet short pipe 46. Fig.10 In the middle, the side mold 21 drives the ejector rod 7 to push the movable blocking ball 45 into the heat dissipation cavity 41 by pushing the trigger ejector plate 71, so that the U-shaped tube 44 connects the upper and lower layers of the heat dissipation cavity 41 separated by the partition plate 42. The coolant in the lower layer of the partition plate 42 enters the upper layer of the partition plate 42 through the U-shaped tube 44 and flows to the outside of the mold through the liquid outlet short tube 47. The coolant is continuously introduced, so that the retaining ring part of the aluminum alloy wheel hub blank can be cooled and the solidification and forming of the blank can be accelerated.

[0050] When the blank is solidified and needs to be demoulded and taken out, after the top mold 1 rises, the side mold 21 separates from the trigger top plate 71 during the dispersion process. Under the elastic action of the spring 72 itself, the movable blocking ball 45 is driven by the top rod 7 to reset and block the two ends of the U-shaped tube 44, so that the upper and lower layers of coolant on the partition plate 42 are not connected to each other, the coolant on the upper layer of the partition plate 42 is connected to the liquid outlet short tube 47, and the coolant on the lower layer of the partition plate 42 is connected to the liquid inlet short tube 46. When the side mold 21 is dispersed, the driving rod 63 drives the linkage slide plate 61 to move, such as Fig.11 In the embodiment, the linkage slide plate 61 drives the boost piston 53 to move inside the boost cavity 52, pushing the coolant to flow into the liquid guide pipe 54 through the drain hole 57. Fig.10 In the process, the liquid guide pipe 54 injects the coolant into the lower layer of the partition plate 42 in the heat dissipation cavity 41 through the liquid inlet short pipe 46, so that the hydraulic pressure of the lower layer of the partition plate 42 in the heat dissipation cavity 41 is increased, and the coolant in the upper layer of the partition plate 42 is squeezed out of the heat dissipation cavity 41 through the liquid outlet short pipe 47, and the partition plate 42 drives the demoulding top ring 43 and the blank to be lifted, so that the blank is separated from the bottom mold 2, and the demoulding of the aluminum alloy wheel hub blank is completed;

[0051] By continuously injecting coolant into the injection pipe 51, during the cooling and solidification stage of the blank, the coolant enters the heat dissipation cavity 41 through the liquid inlet short pipe 46 and is then discharged through the liquid outlet short pipe 47, thereby accelerating the solidification and forming of the blank. In the process of demolding the blank, the power dispersed by the side mold 21 is used to drive the booster piston 53. After passing through the buffer section 55, the push rod 7 drives the movable blocking ball 45 to reset, thereby blocking the circulation of the coolant between the upper and lower layers of the partition plate 42, and squeezing the coolant into the lower layer of the partition plate 42 through the drain hole 57 and the liquid guide pipe 54, thereby increasing the hydraulic pressure of the coolant in the lower layer of the partition plate 42 in the heat dissipation cavity 41, and driving the blank to be lifted through the demolding top ring 43 to complete demolding, that is, accelerating the solidification and fixation of the blank during the cooling stage. During the demolding stage, the retaining ring heat dissipation structure 4 is converted into a hydraulic structure through the linkage structure 6 to assist demolding. The structural layout is reasonable, the space occupied is small, and the mold manufacturing cost is reduced.

[0052] The above are only preferred embodiments of the present invention and are not intended to limit the present invention in other forms. Any technician familiar with the profession may use the technical contents disclosed above to change or modify them into equivalent embodiments with equivalent changes and apply them to other fields. However, any simple modification, equivalent change and modification made to the above embodiments based on the technical essence of the present invention without departing from the technical solution of the present invention still falls within the protection scope of the technical solution of the present invention.

Claims

1. A casting mold for an aluminum alloy component, comprising a top mold (1), a base (11), a bottom mold (2), and a side mold (21), characterized in that: A cooling plate (22) is provided inside the bottom mold (2), cooling structures are provided in the top mold (1), the bottom mold (2) and the cooling plate (22), and a retaining ring heat dissipation structure (4) is provided inside the bottom mold (2), the retaining ring heat dissipation structure (4) is used to cool the blank through the bottom mold (2) and can also assist in demoulding the blank; The retaining ring heat dissipation structure (4) comprises four heat dissipation cavities (41) opened in the bottom mold (2), the interior of each heat dissipation cavity (41) is sealed and slidably connected to a partition plate (42), a demoulding top ring (43) is provided on the top of the bottom mold (2), the demoulding top ring (43) is fixedly connected to the partition plate (42), the interior of each heat dissipation cavity (41) is divided into an upper and lower layer by the partition plate (42), a U-shaped tube (44) is fixedly connected to the outer wall of the heat dissipation cavity (41), and is used to connect the upper and lower cavity layers of the partition plate (42), and the U-shaped tube (44) is connected to the heat dissipation cavity ( The two ends of the heat dissipation cavity (41) are slidably connected with movable blocking balls (45), the upper and lower layers of the heat dissipation cavity (41) are respectively connected with a liquid outlet short tube (47) and a liquid inlet short tube (46), the heat dissipation cavity (41) is fixedly connected with a booster pipe (5) through the liquid inlet short tube (46), the outer wall of the side mold (21) is transmission-connected with a linkage structure (6), the booster pipe (5) is transmission-connected with the side mold (21) through the linkage structure (6), and the booster pipe (5) can use the power of the side mold (21) to boost the coolant in the lower chamber of the partition plate (42); The boost pipe (5) comprises a rhombus-shaped shell, which is mounted on a base (11). Two sides of the interior of the rhombus-shaped shell are connected to a liquid injection pipe (51) and a liquid guide pipe (54) respectively. A boost cavity (52) is provided inside the rhombus-shaped shell. The boost cavity (52) is located between the liquid injection pipe (51) and the liquid guide pipe (54). A boost piston (53) is sealingly and slidably connected inside the boost cavity (52). A liquid injection hole (56) is provided between the bottom mold (2) and the liquid injection pipe (51). The liquid injection hole (56) is located at one end of the boost cavity (52). A liquid discharge hole (57) is provided between the other end of the boost cavity (52) and the liquid guide pipe (54). The liquid guide pipe (54) is connected to a liquid inlet short pipe (46). Two injection holes (56) are provided, and a buffer section (55) is provided between the two injection holes (56) of the pressurizing cavity (52). The buffer section (55) is used to balance the internal hydraulic pressure of the pressurizing piston (53) when the pressurizing piston (53) moves between the two injection holes (56), and to provide a buffer distance, so as to pressurize the interior of the lower cavity of the partition plate (42) after the side mold (21) is completely separated from the blank; The cavities on the top mold (1) and the bottom mold (2) are used to cool the spoke portion of the blank, and the cavities on the side mold (21) and the cooling plate (22) are used to cool the bead seat portion of the blank.

2. The aluminum alloy component casting mold according to claim 1, characterized in that: The outer wall of the movable blocking ball (45) is fixedly connected with a push rod (7), and the push rod (7) is sealingly slidably connected to the U-shaped tube (44). The end of the push rod (7) away from the movable blocking ball (45) is fixedly connected with a trigger top plate (71). The trigger top plate (71) is used to push the movable blocking ball (45) to slide out of the U-shaped tube (44) through the push rod (7) when the side mold (21) is closed, so that the U-shaped tube (44) can connect the upper and lower chambers of the partition plate (42). A spring (72) is fixedly connected between the trigger top plate (71) and the outer wall of the U-shaped tube (44). The spring (72) is used to drive the movable blocking ball (45) to enter the internal closed tube opening of the U-shaped tube (44) through the trigger top plate (71) when the side mold (21) is dispersed.

3. The aluminum alloy component casting mold according to claim 1, characterized in that: The upper surface of the demoulding top ring (43) is an inclined surface, and is used for sealing connection with the bottom mold (2) and the demoulding top ring (43) when the side mold (21) is closed.

4. The aluminum alloy component casting mold according to claim 1, characterized in that: The cooling structure comprises a cooling cavity (3), a water injection pipe (32) and a water discharge pipe (33); the top mold (1), the bottom mold (2), the side mold (21) and the cooling plate (22) are all provided with cooling cavities (3); the cooling cavity (3) inside the cooling plate (22) is connected to the cooling cavity (3) inside the side mold (21); the cooling cavities (3) on the top mold (1) are connected to each other via two annular pipes (31); the cooling cavities (3) on the bottom mold (2) are connected to each other via two annular pipes (31); the cooling cavities (3) on the cooling plate (22) are connected to each other via two annular pipes (31); and the annular pipes (31) are respectively connected to the water injection pipe (32) and the water discharge pipe (33).

5. The aluminum alloy component casting mold according to claim 1, characterized in that: The liquid inlet short tubes (46) on two adjacent heat dissipation chambers (41) are connected to each other, and the liquid outlet short tubes (47) on two adjacent heat dissipation chambers (41) are connected to each other.

6. The aluminum alloy component casting mold according to claim 1, characterized in that: The linkage structure (6) comprises a linkage slide plate (61), a directional slide groove (62) and a driving rod (63); a directional slide groove (62) is provided on a side wall of the base (11); a linkage slide plate (61) is slidably connected inside the directional slide groove (62); a driving rod (63) is fixedly connected to the upper surface of the linkage slide plate (61); the driving rod (63) is transmission-connected to the side mold (21); the linkage slide plate (61) is fixedly connected to a part in the boost pipe fitting (5); the linkage slide plate (61) is transmission-connected to the side mold (21) via the driving rod (63) and is used to provide power to the boost pipe fitting (5).