Method and device for producing low-elongation fused line for fly fishing main line
By using liquid crystal polymer fibers or aromatic fibers and mixed resin glue to combine rigid line forming machines, the elongation of the main line core line of fly fishing is reduced, and the production efficiency and product quality are improved through cooling and dust removal device, which solves the problem of The problems of high elongation of core wires and discontinuous coating in the prior art.
Patent Information
- Application Number
- CN202410367000.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2024-02-05
- Filing Date
- 2024-03-28
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-03-28
AI Technical Summary
The core line of the fly fishing main line has too high elongation during high-temperature plasticization processing, resulting in fatigue, cracking and falling off of the surface plastic layer. The existing coating device cannot ensure continuous cooling of the fishing line, affecting output.
Liquid crystal polymer fiber or aromatic polyamide fiber is used as the core wire, mixed resin glue is coated, and shaped and cured by a rigid line forming molder, and combined with a cooling and dust removal device to ensure the continuity and quality of resin coating.
The elongation of the main line core line of fly fishing is reduced to 3%-5%, the service life is improved, and the production efficiency is improved through cooling and dust removal devices, ensuring the smooth coating of resin and product quality.
Smart Images

Figure CN118186648B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of fishing gear production equipment, and in particular to a method and a device for producing a low-elongation fused line used for a fly fishing main line. Background Art
[0002] In the international market, the structure of the main line of fly fishing is usually composed of a core line and a plastic layer, and the plastic layer is made of PVC or PU material. The core line of the main line of fly fishing bears the main force. During production, since the plastic layer of the main line of fly fishing must undergo a high-temperature plasticization process of 180℃--260℃, the core line of the main line of fly fishing must have high temperature resistance. Nylon multifilament or polyester multifilament is commonly used in the market, and the core line of the main line of fly fishing is made by braiding 16 strands. It is also because of the 16-strand braiding that this core line has a high elongation, usually around 20%--30%. Such a high elongation will cause the life fatigue, cracking and shedding of the plastic layer on the surface of the main line of fly fishing during the long-term stress contraction of the main line. Therefore, low elongation is the main technical indicator of the core line of the main line of fly fishing. It is of great significance to develop the core line of the main line of fly fishing with low elongation performance.
[0003] When producing fishing lines, it is usually necessary to coat the fishing lines with resin. Chinese patent CN210104177U discloses a coating device for producing fishing lines, which is characterized by comprising a coating extrusion mechanism and a multifilament extrusion mechanism, wherein the coating extrusion mechanism comprises a rubber extrusion head and a vertically arranged coating tank, wherein the rubber extrusion head is fixedly connected to the bottom of the coating tank, a wire outlet hole is provided at the bottom of the coating tank, a wire inlet hole is provided at the top of the coating tank, a preformed extrusion hole is provided on the rubber extrusion head, and the preformed extrusion hole is provided just below the wire outlet hole; the multifilament extrusion mechanism is provided in the coating tank, and the multifilament extrusion mechanism comprises an extrusion head and a vertically arranged coating tank; the rubber extrusion head is fixedly connected to the bottom of the coating tank, a wire outlet hole is provided at the bottom of the coating tank, a wire inlet hole is provided at the top of the coating tank, a preformed extrusion hole is provided on the rubber extrusion head, and the preformed extrusion hole is provided just below the wire outlet hole; the multifilament extrusion mechanism is provided in the coating tank, and the multifilament extrusion mechanism comprises an extrusion head and a multifilament extrusion head. A pressure roller assembly and a forming roller assembly, wherein the forming roller assembly is located below the squeezing roller assembly; the squeezing roller assembly comprises a plurality of horizontally arranged squeezing rollers, which are evenly spaced vertically and arranged just below the wire inlet hole; the forming roller assembly comprises a plurality of horizontally arranged forming rollers, which are provided with annular shaping grooves, the axes of the forming rollers are parallel to the axes of the squeezing rollers, and the plurality of forming rollers are evenly spaced vertically and arranged just above the wire outlet hole; a fixed bracket for mounting the squeezing roller and the forming roller is fixedly provided in the coating tank, the fixed bracket is fixedly connected to the coating tank, and both ends of the squeezing roller and the forming roller are mounted on the fixed bracket.
[0004] Although the above scheme can complete the coating of the resin, it is necessary to ensure that no dust adheres to the fishing line before the resin is coated, otherwise the resin will not adhere. In addition, the fishing line usually undergoes a cooling step before the resin adheres. For example, Chinese patent CN216682974U discloses a cooling device for fishing line production. Although the device can cool the fishing line, it cannot perform continuous cooling, which seriously affects the production. Summary of the invention
[0005] In view of the above problems, a method and device for producing a low-elongation fused line for a fly fishing main line are provided. The technical problem to be solved by the present invention is achieved through the following technical solutions. The present invention is a method for producing a low-elongation fused line for a fly fishing main line, which is characterized in that the low-elongation fused line uses liquid crystal polymer fiber LCP or aromatic polyamide fiber F12 as a core line, and then a mixed resin glue is coated on the core line, and finally a rigid line former is used to shape and solidify the low-elongation fused line.
[0006] In order to solve the problems of the prior art, the present invention provides a method for producing a low-elongation fused line for a fly fishing main line, comprising the following steps: the low-elongation fused line uses liquid crystal polymer fiber LCP or aromatic polyamide fiber F12 as a core line, then coats the core line with mixed resin glue, and finally uses a rigid line former to shape and cure the low-elongation fused line.
[0007] Preferably, the core wire feeding system first sends the liquid crystal polymer fiber LCP or the aromatic polyamide fiber F12 into a cooling and dust removal device for cooling and dust removal, and then sends it into a coating tank and immerses it in the mixed resin in the coating tank. After entering the coating tank, the core wire bypasses all the extrusion rollers and forming rollers in turn, is repeatedly extruded and forced to be dispersed and coated by the extrusion rollers, and then is repeatedly formed into a circle and twisted into a wire by the forming roller; after being led out of the coating tank, it is shaped by a rigid wire former, and finally is cured and wound up to obtain the product.
[0008] Preferably, the mixed resin uses PE bonding special resin made of terpene phenolic resin, PP elastic plastic and ethyl acetate solvent as the main resin.
[0009] Preferably, during the subsequent forming process, the forming retraction shaft groove is made into a rolling bearing structure to increase the radial extrusion force, reduce the friction damage caused by dragging, and increase the roundness of the fusion line.
[0010] Preferably, a silicone rubber elastic qualitative mold structure is added at the exit of the low-elongation fusion line to improve the roundness of the low-elongation fusion line.
[0011] The present invention also relates to a low-elongation fused line production device for fly fishing main lines, the device produces low-elongation fused lines by a low-elongation fused line production method for fly fishing main lines, and is characterized in that the production device comprises a cooling and dust removal device, the cooling and dust removal device comprises an outer shell and a partition; the outer shell is a rectangular shell structure, the bottom of the outer shell stores clean water, and the two sides of the outer shell are respectively provided with a feed port and a discharge port; the partition is vertically arranged inside the outer shell, the bottom of the partition extends below the clean water level in the outer shell, the partition divides the outer shell into a first cavity and a second cavity, the feed port is located at the upper part of the first cavity, the discharge port is located at the upper part of the second cavity, rotating wheels are respectively arranged at the feed port, the discharge port and the bottom of the partition, and the low-elongation fused line is respectively wound around the three rotating wheels; the cooling and dust removal steps are as follows:
[0012] Under the guidance of the rotating wheel, the low extension fusion line enters the first cavity from the feed port and is immersed in the clean water at the bottom of the shell. Then the low extension fusion line passes through the bottom of the partition and enters the second cavity, and is finally discharged from the discharge port.
[0013] Preferably, the cooling and dust removal device also includes a cooling device, which is arranged in the first cavity, and the cooling device includes a sealing assembly and an atomizer; the sealing assembly is arranged at the feed port; the atomizer is arranged on the side wall of the outer shell on one side of the first cavity, and the atomizer can inject atomized water vapor into the first cavity, and the sealing assembly limits the water vapor from overflowing from the feed port.
[0014] Preferably, the cooling and dust removal device further comprises a first water removal device, which is disposed in the second cavity and performs preliminary water removal on the low-extension fusion line.
[0015] Preferably, the cooling and dust removal device also includes a second water removal device, which includes a water suction wheel and a second rotary drive; the water suction wheel is rotatably arranged along the width direction of the outer shell above the rotating wheel located on the discharge port, and the outer periphery of the water suction wheel is coated with a flexible water absorbent material, and the flexible water absorbent material is in contact with the side wall of the rotating wheel located on the discharge port; the second rotary drive is arranged on one side of the water suction wheel.
[0016] Preferably, the second water removal device further comprises a drying device, which is arranged on the upper part of the water suction wheel and wraps the upper half of the water suction wheel, and the drying device dries the upper half of the water suction wheel.
[0017] Compared with the prior art, the present invention has the following beneficial effects:
[0018] 1. The method for producing low-elongation fusion line for fly fishing main line of the present invention adopts liquid crystal polymer fiber or aromatic polyamide fiber as core line, and adopts "mixed resin glue + rigid line former" to form low-elongation fusion line. Since the fiber multifilament is arranged in bundles and is not woven, its elongation is controlled within the range of 3%-5%. This low-elongation fusion line is used as the core line of fly fishing main line, which is a new composite monofilament structure design.
[0019] 2. The present invention uses mixed resin glue to make the fusion line, which also increases the adhesion between the fusion line and the plastic layer, thereby improving the service life of the fly fishing main line.
[0020] 3. The present invention provides a cooling and dust removal device to ensure that the resin in the coating tank will not fall off when being coated on the low-elongation fusion line due to dust adhering to the low-elongation fusion line, thereby ensuring the quality of the low-elongation fusion line. At the same time, the present invention can ensure that the low-elongation fusion line is continuously transported inside it, which greatly improves production efficiency compared to traditional cooling devices. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a three-dimensional schematic diagram of a low-elongation fused line production device for fly fishing main lines.
[0022] Figure 2 It is a side view of a low extension fused line production device for fly fishing main line.
[0023] Figure 3 It is a low-elongation fusion line production device for fly fishing main lines Figure 2 Schematic cross-sectional view at AA in the middle.
[0024] Figure 4 It is a cutaway perspective schematic diagram of a low-elongation fused line production device for fly fishing main lines.
[0025] Figure 5 This is a three-dimensional schematic diagram of a low-elongation fused line production device for fly fishing main lines with the sponge removed.
[0026] Figure 6 It is a three-dimensional schematic diagram of a low-elongation fused line production device for fly fishing main lines, with a sponge and a drying device removed.
[0027] Figure 7 It is a three-dimensional schematic diagram of a low-elongation fused line production device for fly fishing main lines, with a drying device, a sealing assembly and a drying device removed.
[0028] Figure 8 It is a low-elongation fusion line production device for fly fishing main lines Figure 7 A local enlarged schematic diagram of point B in the middle.
[0029] Fig. 9 This is a schematic diagram of a low-extension fused line production device for a fly fishing main line when producing a low-extension fused line.
[0030] The numbers in the figure are:
[0031] 1. Shell; 2. Partition; 3. Cooling device; 31. Sealing assembly; 311. Sponge; 312. Mounting frame; 32. Atomizer; 4. First water removal device; 41. First rotary drive; 42. Gear; 43. Rack; 44. Pressing plate; 45. Guide rod; 46. Spring; 47. Scraper; 48. Guide rail; 5. Second water removal device; 51. Suction wheel; 52. Second rotary drive; 53. Drying device; 531. Dryer; 532. Separation plate; 533. Filter; 534. Drying shell; 6. Low-elongation fusion line; 7. Coating tank; 8. Rigid wire former. DETAILED DESCRIPTION
[0032] In order to further understand the features, technical means, specific objectives and functions of the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0033] Reference Figure 1-Figure 9 : The production method of low-elongation fusion line for fly fishing main line includes the following steps: the low-elongation fusion line 6 uses liquid crystal polymer fiber LCP or aromatic polyamide fiber F12 as the core line, and then a mixed resin glue is coated on the core line, and finally a rigid line former 8 is used to shape and solidify it.
[0034] Reference Figure 1-Figure 9 The core wire feeding system first feeds the liquid crystal polymer fiber LCP or the aromatic polyamide fiber F12 into the cooling and dust removal device for cooling and dust removal, and then feeds it into the coating tank 7 and immerses it in the mixed resin in the coating tank 7. After entering the coating tank 7, the core wire bypasses all the squeezing rollers and the forming rollers in turn, is repeatedly squeezed and forced to be dispersed and coated by the squeezing rollers, and then is repeatedly formed into a circle and twisted into a wire by the forming rollers; after being led out from the coating tank 7, it is shaped by the rigid wire former 8, and finally is cured and wound up to obtain the product.
[0035] The coating tank 7 is prior art, and the specific structure of the coating tank 7 can be seen in Chinese patent CN210104177U, so the structure of the coating tube is not repeated here. The structure of the rigid linear former 8 is also prior art, so it is not repeated here.
[0036] Reference Figure 1-Figure 9 The mixed resin adopts terpene phenolic resin, PP elastic plastic and ethyl acetate solvent to make PE bonding special resin as main resin.
[0037] Reference Figure 1-Figure 9: During the subsequent forming process, the forming retraction shaft groove is made into a rolling bearing structure to increase the radial extrusion force, reduce the friction damage caused by dragging, and increase the roundness of the fusion line.
[0038] Reference Figure 1-Figure 9 : At the exit of the low-elongation fusion line 6, a silicone rubber elastic qualitative mold structure is added to improve the roundness of the low-elongation fusion line 6.
[0039] The silicone rubber elastic shaping mold structure refers to a template with a shaping circular hole, the diameter of which is the same as the final finished product diameter of the low-elongation fusion line 6. After processing, the low-elongation fusion line 6 passes through the shaping circular hole of the template to achieve the final shaping effect.
[0040] Reference Figure 1-Figure 3 :The present invention also relates to a low-elongation fusion line production device for fly fishing main line, the device produces low-elongation fusion line 6 through the low-elongation fusion line production method for fly fishing main line, and is characterized in that the production device includes a cooling and dust removal device, the cooling and dust removal device includes an outer shell 1 and a partition 2; the outer shell 1 is a rectangular shell structure, the bottom of the outer shell 1 stores clean water, and the two sides of the outer shell 1 are respectively provided with a feed port and a discharge port; the partition 2 is vertically arranged inside the outer shell 1, and the bottom of the partition 2 extends to below the clean water level in the outer shell 1, the partition 2 divides the outer shell 1 into a first cavity and a second cavity, the feed port is located at the upper part of the first cavity, and the discharge port is located at the upper part of the second cavity, and rotating wheels are respectively arranged at the feed port, the discharge port and the bottom of the partition 2, and the low-elongation fusion line 6 is respectively wound on the three rotating wheels; the cooling and dust removal steps are as follows:
[0041] Under the guidance of the rotating wheel, the low extension fusion line 6 enters the first cavity from the feed port and is immersed in the clean water at the bottom of the shell 1. Then the low extension fusion line 6 passes through the bottom of the partition 2 and enters the second cavity, and is finally discharged from the discharge port.
[0042] After the low-elongation fusion line 6 is discharged from the discharge port of the outer shell 1, it enters the coating tank 7 for resin coating. At this time, there is no dust on the low-elongation fusion line 6, which ensures the smooth coating of the resin. When the low-elongation fusion line 6 enters the outer shell 1 from the feed port, the low-elongation fusion line 6 is first wound from the upper part of the rotating wheel, and then enters the first cavity. Then the low-elongation fusion line 6 is immersed in water and bypasses the lower part of the rotating wheel at the bottom of the partition 2, and then leaves the water surface and enters the second cavity and bypasses the upper part of the rotating wheel at the discharge port. When the low-elongation fusion line 6 enters the clean water at the bottom of the outer shell 1, it can not only cool down, but also the dust attached to the low-elongation fusion line 6 will be washed away by the clean water. In this way, it is ensured that the resin in the coating tank 7 will not fall off due to dust sticking to the low-elongation fusion line 6 when being coated on the low-elongation fusion line 6, thereby ensuring the quality of the low-elongation fusion line 6.
[0043] Reference Figure 1 and Figure 2-Figure 5 : The cooling and dust removal device also includes a cooling device 3, which is arranged in the first cavity. The cooling device 3 includes a sealing component 31 and an atomizer 32; the sealing component 31 is arranged at the feed port; the atomizer 32 is arranged on the side wall of the shell 1 on one side of the first cavity, and the atomizer 32 can inject the atomized water vapor into the first cavity. The sealing component 31 limits the water vapor from overflowing from the feed port.
[0044] The sealing assembly 31 includes a sponge 311 and a mounting frame 312. The mounting frame 312 is horizontally fixed on the feed port, and the sponge 311 is set on the mounting frame 312. The sponge 311 blocks the feed port. It is worth noting that since the sponge 311 is a flexible material and the low-elongation fusion line 6 itself has a thin diameter, the low-elongation fusion line 6 can pass through the connection between the sponge 311 and the feed port. Since the sponge 311 is set, the upper part of the first cavity is completely sealed. The atomizer 32 atomizes the water vapor and sprays it into the first cavity. The atomized water vapor can cool the low-elongation fusion line 6 faster. After the water vapor adheres to the low-elongation fusion line 6, it enters the clean water in the outer shell 1 together with the low-elongation fusion line 6.
[0045] Reference Figure 6-Figure 8 The cooling and dust removal device also includes a first water removal device 4, which is arranged in the second cavity. The first water removal device 4 performs preliminary water removal on the low-extension fusion line 6.
[0046] When the low-elongation fusion line 6 enters the second cavity from the clean water at the bottom of the shell 1, water droplets are attached to the low-elongation fusion line 6. If the water droplets on the low-elongation fusion line 6 are not removed, when the low-elongation fusion line 6 enters the coating tank 7, it is easy for the resin to fail to be coated. This is because water does not want to dissolve with most of the resin. Even if water is compatible with some of the resin, the unwiped water on the low-elongation fusion line 6 will reduce the performance of the resin after contacting with the resin in the coating tank 7. In this way, after the low-elongation fusion line 6 is cooled, the water on the low-elongation fusion line 6 is removed to ensure that the resin is stably coated on the low-elongation fusion line 6. The first water removal device 4 includes a first rotary driver 41, a gear 42, a rack 43, a pressing plate 44, and a guide rod 45. , spring 46, scraper 47 and guide rail 48, the guide rail 48 is fixedly arranged on the inner wall of the shell 1 at an angle, the extension direction of the guide rail 48 is perpendicular to the extension direction of the low extension fusion line 6 located in the second cavity, two scrapers 47 are arranged, the two scrapers 47 are respectively located on both sides of the low extension fusion line 6 in the second cavity, the scraper 47 slides along the extension direction of the guide rail 48, and the two scrapers 47 have two movement modes when moving, one of which is approaching each other and the other is moving away from each other. The side of the scraper 47 close to the low extension fusion line 6 is made of rubber material, so that when the two scrapers 47 clamp the low extension fusion line 6, the end of the scraper 47 in contact with the low extension fusion line 6 will be deformed, so that the scraper 4 7 can better scrape off the moisture on the low extension fusion line 6, the guide rod 45 is fixedly arranged along the moving direction of the scraper 47 at one end of the scraper 47 away from the low extension fusion line 6, the pressing plate 44 is slidably arranged on the guide rod 45 along the axial direction of the guide rod 45, and there is a gap between the pressing plate 44 and the scraper 47, the spring 46 is arranged in the gap along the axis of the guide rod 45, and the two ends of the spring 46 are fixedly connected to the pressing plate 44 and the scraper 47 respectively, the rack 43 is arranged at one end of the pressing plate 44 along the extension direction of the guide rail 48, and the rack 43 is fixedly connected to the end of the pressing plate 44. Since there are two scrapers 47, there are also two racks 43. A gear 42 is arranged between the two racks 43, and both sides of the gear 42 The first rotation driver 41 is respectively engaged with the two racks 43. The first rotation driver 41 is arranged at the end of the gear 42. The first rotation driver 41 drives the gear 42 to rotate. The first rotation driver 41 is preferably a servo motor. When the first rotation driver 41 is started, the first rotation driver 41 drives the gear 42 to rotate, so that the two racks 43 move under the drive of the gear 42, and the two pressing plates 44 corresponding to the two racks 43 can approach or move away from each other. When the two pressing plates 44 approach each other, the spring 46 located between the pressing plate 44 and the scraper 47 is compressed. At this time, the elastic force of the spring 46 acts on the scraper 47. Conversely, when the two pressing plates 44 move away from each other, the spring 46 located between the pressing plate 44 and the scraper 47 is gradually reset.At this time, the elastic force of the spring 46 gradually decreases, and the pressing force of the scraper 47 on the low extension fusion line 6 also gradually decreases. It is worth noting that when the scraper 47 is used to scrape the water drops on the low extension fusion line 6, the pressure of the scraper 47 on the low extension fusion line 6 should not be too large, otherwise the scraper 47 is likely to tear the surface of the low extension fusion line 6 when scraping the water on the low extension fusion line 6. In this case, a pressure sensor needs to be provided in the scraper 47, and a maximum pressure value is set for the pressure sensor. When the pressure value monitored by the pressure sensor reaches the maximum pressure value, the first The rotary drive 41 stops running. Since the low extension fusion line 6 passes through the clean water at the bottom of the shell 1 when entering the second cavity from the first cavity, the clean water in the shell 1 will inevitably decrease after long-term use. Therefore, it is necessary to replenish the clean water in the shell 1 in time. A water level sensor is provided on the side wall of the shell 1. At the same time, a water inlet is also provided on one side of the shell 1. When the water inlet is opened, the external water is replenished into the shell 1. The water level sensor is used to monitor the lowest water level of the shell 1. When the water level in the shell 1 drops to the lowest water level, the water inlet is opened.
[0047] Reference Figure 6 and Figure 7 : The cooling and dust removal device also includes a second water removal device 5, which includes a water suction wheel 51 and a second rotary driver 52; the water suction wheel 51 is rotatably arranged above the rotating wheel located on the discharge port along the width direction of the outer shell 1, and the outer periphery of the water suction wheel 51 is coated with a flexible water-absorbing material, and the flexible water-absorbing material is in contact with the side wall of the rotating wheel located on the discharge port; the second rotary driver 52 is arranged on one side of the water suction wheel 51.
[0048] The second rotary driver 52 is preferably a servo motor. When the second rotary driver 52 is started, the water absorption wheel 51 rotates driven by the second rotary driver 52. The rotating water absorption wheel 51 completely absorbs the water remaining on the low-elongation fusion line 6 through the flexible water absorption material coated on its outer side.
[0049] Reference Figure 1-Figure 5 The second water removal device 5 further comprises a drying device 53, which is disposed on the upper portion of the water suction wheel 51 and wraps the upper half of the water suction wheel 51, and dries the upper half of the water suction wheel 51.
[0050] The drying device 53 includes a dryer 531, a separation plate 532, a filter 533 and a drying shell 534. The drying shell 534 is covered on the upper part of the water suction wheel 51, the separation plate 532 is arranged at the bottom of the drying shell 534, the filter 533 is arranged at the top of the drying shell 534, and a heating wire is arranged on the inner wall of the drying shell 534. The dryer 531 is arranged on one side of the filter 533. The dryer 531 extracts the air in the drying shell 534, and the outside air enters the drying shell 534 through the filter 533. In this way, when the water suction wheel 51 rotates into the drying shell 534 driven by the second rotary driver 52 after absorbing moisture, the moisture on the water suction wheel 51 can be dried, thereby ensuring the water absorption effect of the water suction wheel 51.
[0051] The above embodiments only express one or several implementation modes of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the present invention. It should be pointed out that, for those of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the attached claims.
Claims
1. A method for producing a low-elongation fused line for a fly fishing main line, characterized in that: The following steps are involved: The low-elongation fusion wire (6) uses liquid crystal polymer fiber LCP or aromatic polyamide fiber F12 as a core wire. The core wire feeding system first feeds the liquid crystal polymer fiber LCP or aromatic polyamide fiber F12 into a cooling and dust removal device for cooling and dust removal, and then feeds it into a coating tank (7) and immerses it in the mixed resin in the coating tank (7). After entering the coating tank (7), the core wire passes through all the squeezing rollers and the forming rollers in sequence, and is repeatedly squeezed and forcibly dispersed and coated by the squeezing rollers, and then repeatedly formed into a circle and stranded into a wire by the forming rollers; after being led out of the coating tank (7), it is shaped by a rigid wire former (8), and finally cured and rolled to obtain the obtained wire. The cooling and dust removal device comprises a shell (1) and a partition (2); The outer shell (1) is a rectangular shell structure, clean water is stored at the bottom of the outer shell (1), and a feed inlet and a discharge outlet are respectively provided on both sides of the outer shell (1); The partition (2) is vertically arranged inside the outer shell (1), and the bottom of the partition (2) extends below the clear water level in the outer shell (1). The partition (2) divides the outer shell (1) into a first cavity and a second cavity. The feed port is located at the upper part of the first cavity, and the discharge port is located at the upper part of the second cavity. Rotating wheels are respectively arranged at the feed port, the discharge port and the bottom of the partition (2), and the low-extension fusion line (6) is respectively wound around the three rotating wheels; The cooling and dust removal device also includes a cooling device (3), the cooling device (3) is arranged in the first cavity, the cooling device (3) includes a sealing component (31) and an atomizer (32), the sealing component (31) is arranged at the feed inlet, the atomizer (32) is arranged on the side wall of the housing (1) on one side of the first cavity, the atomizer (32) can inject atomized water vapor into the first cavity, and the sealing component (31) limits the water vapor from overflowing from the feed inlet; The cooling and dust removal device further comprises a first water removal device (4), the first water removal device (4) being arranged in the second cavity, the first water removal device (4) performing preliminary water removal on the low extension fusion line (6), the first water removal device 4 comprising a first rotary driver 41, a gear 42, a rack 43, a pressing plate 44, a guide rod 45, a spring 46, a scraper 47 and a guide rail 48, the guide rail 48 being fixedly arranged on the inner wall of the housing 1 in an inclined manner, the extension direction of the guide rail 48 being perpendicular to the extension direction of the low extension fusion line 6 in the second cavity, two scrapers 47 being arranged, the two scrapers 47 being respectively arranged on both sides of the low extension fusion line 6 in the second cavity, the scrapers 47 sliding along the extension direction of the guide rail 48; The cooling dust removal device further comprises a second water removal device (5), the second water removal device (5) comprising a water suction wheel (51) and a second rotary drive (52), the water suction wheel (51) being rotatably arranged above a rotating wheel located on the discharge port along the width direction of the housing (1), the outer periphery of the water suction wheel (51) being coated with a flexible water-absorbing material, the flexible water-absorbing material being in contact with a side wall of the rotating wheel located on the discharge port, the second rotary drive (52) being arranged on one side of the water suction wheel (51), the second water removal device (5) further comprising a drying device (53), the drying device (53) being arranged on the upper part of the water suction wheel (51) and wrapping the upper half of the water suction wheel (51), the drying device (53) drying the upper half of the water suction wheel (51); The cooling and dust removal steps are as follows: under the guidance of the rotating wheel, the low-extension fusion line (6) enters the first cavity from the feed port and is immersed in the clean water at the bottom of the shell (1); then the low-extension fusion line (6) passes through the bottom of the partition (2) and enters the second cavity, and is finally discharged from the discharge port.
2. The method for producing a low-elongation fused line for a fly fishing main line according to claim 1, characterized in that: The mixed resin adopts terpene phenolic resin, PP elastic plastic and ethyl acetate solvent as the main resin of PE bonding special resin.
3. The method for producing a low-elongation fused line for a fly fishing main line according to claim 1, characterized in that: During the subsequent forming process, the forming retraction shaft groove is made into a rolling bearing structure to increase the radial extrusion force, reduce the friction damage caused by dragging, and increase the roundness of the fusion line.
4. The method for producing a low-elongation fused line for a fly fishing main line according to claim 1, characterized in that: At the exit of the low-elongation fusion line (6), a silicone rubber elastic qualitative mold structure is added to improve the roundness of the low-elongation fusion line (6).