Battery filling hole sealing structure and battery

Through a two-layer sealing structure, using a combination of fluororubber sealing nails and welding parts, the problem of weak sealing of the battery injection hole is solved, achieving a highly reliable and easy-to-assemble sealing effect, ensuring the safety and sealing performance of the battery. .

CN118299774BActive Publication Date: 2024-10-18SVOLT ENERGY TECHNOLOGY CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410719573.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-05
Publication Date
2024-10-18
Estimated Expiration
2044-06-05

AI Technical Summary

Technical Problem

The existing battery injection hole sealing method is prone to seal failure or battery cover cracking during installation, use and transportation, and the installation of sealing nails is difficult.

Method used

It adopts a two-layer sealing structure, including sealing nails and sealing covers. The sealing nails are made of fluorine rubber with a compression rate between 5.08% and 10.6%. The first and second sealing surfaces are formed by combining the accommodation groove and the welding part. The inclination and arc chamfering of the groove improve the sealing effect.

Benefits of technology

A good sealing effect of the liquid injection hole is achieved, the reliability of the sealing and the ease of assembly are improved, and the risks of electrolyte leakage and battery cover damage are avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118299774B_ABST
    Figure CN118299774B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of battery technology, and specifically discloses a battery injection hole sealing structure and a battery, wherein the battery injection hole sealing structure comprises a battery cover, a sealing nail and a sealing cover. The sealing nail is made of elastic material, and the sealing nail is interference fit with the injection hole on the battery cover. The compression rate Ψ of the sealing nail along its radial direction satisfies the value range of 5.08%-10.6%, thereby ensuring that the first sealing surface between the sealing nail and the injection hole has a good sealing effect, and the sealing nail is easily pressed into the injection hole without damaging the battery cover. The sealing cover is arranged in a receiving groove on the battery cover, and the sealing cover is welded to the side wall of the receiving groove and forms a second sealing surface at the welding point. The injection hole is sealed by setting a two-layer sealing structure of a first sealing surface and a second sealing surface, which greatly improves the sealing effect of the injection hole, and the electrolyte is not easy to leak. The present invention also provides a battery, which is sealed by the above-mentioned battery injection hole sealing structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of batteries, and in particular to a battery liquid injection hole sealing structure and a battery. Background Art

[0002] Generally speaking, a battery includes a shell with an open top and a battery cover. The battery cover is arranged at the top of the shell and connected to the shell so that the shell forms a relatively closed space. The battery cover is provided with an injection hole for injecting electrolyte into the battery or replenishing electrolyte. In order to prevent leakage from the injection hole later, the injection hole needs to be sealed.

[0003] In the prior art, sealing is usually performed by inserting a sealing pin into the injection hole and interfering with the inner wall of the injection hole. However, in this sealing method, if the interference fit between the sealing pin and the injection hole is small, there is a risk that the sealing pin will fall out of the injection hole during installation, long-term use and transportation, resulting in failure of the seal of the injection hole, leakage of electrolyte inside the shell, and safety hazards of the battery. If the interference fit between the sealing pin and the injection hole is large, it is easy to cause the battery cover to crack, which also poses a safety hazard. In addition, when the interference fit between the sealing pin and the injection hole is large, the installation of the sealing pin is also difficult. Summary of the invention

[0004] The object of the present invention is to provide a battery liquid injection hole sealing structure and a battery, the liquid injection hole has a good sealing effect, high reliability and is easy to assemble.

[0005] To achieve the above object, the present invention adopts the following technical solutions:

[0006] In one aspect, the present invention provides a battery liquid filling hole sealing structure, comprising:

[0007] A battery cover, wherein the battery cover is provided with an injection hole, the injection hole is used to inject electrolyte into the battery shell, and a receiving groove is provided on the side of the battery cover away from the electrolyte, the receiving groove is coaxial with the injection hole and is connected to each other;

[0008] The sealing pin is made of fluororubber, the sealing pin is arranged in the injection hole and has an interference fit with the inner wall of the injection hole, and a first sealing surface is formed between the sealing pin and the inner wall of the injection hole; the compression rate of the sealing pin along the radial direction of the sealing pin is Ψ, and the value range of Ψ is 5.08%-10.6%;

[0009] A sealing cover is arranged in the receiving groove, the sealing cover comprises a shielding portion, a buffer portion and a welding portion, the buffer portion is arranged in the circumference of the shielding portion, the welding portion is arranged in the circumference of the buffer portion, the projection of the shielding portion on the battery cover plate along the axial direction of the injection hole completely covers the injection hole and the sealing nail, the welding portion is welded to the side wall of the receiving groove and forms a second sealing surface at the welding position;

[0010] The side wall of the accommodating groove is inclined, and the angle between the side wall of the accommodating groove and the bottom wall of the accommodating groove is α, and the value range of α is 95°-175°; the outer peripheral surface of the welding part is inclined, and the angle between the outer peripheral surface of the welding part and the bottom wall of the accommodating groove is β, 0°<β-α≤5°.

[0011] Optionally, an end of the injection hole communicating with the accommodating groove is provided with an arc chamfer, the arc chamfer protrudes toward the direction where the sealing pin is located, and the radius of the arc chamfer is r, and the value range of r is 0.1mm-0.5mm.

[0012] Optionally, the height of the injection hole along the axial direction of the injection hole is H, and the height of the first sealing surface along the axial direction of the injection hole is H1; the value range of H is 0.6mm-2.0mm, and the value range of H1 is 0.5mm-1.5mm.

[0013] Optionally, the height of the battery cover plate along the axial direction of the injection hole is A, and the value range of A is 1.5 mm-3 mm;

[0014] The depth of the receiving groove along the axial direction of the injection hole is B, and the value range of B is 0.9mm-1.3mm;

[0015] After the sealing cover is installed in the accommodating groove, the end face of the sealing cover facing away from the electrolyte is not higher than the end face of the battery cover facing away from the electrolyte, and the distance between the end face of the sealing nail facing away from the electrolyte and the end face of the battery cover facing away from the electrolyte is b, and the value range of b is 0.1mm-0.5mm.

[0016] Optionally, after welding the welding portion to the side wall of the receiving groove, the penetration depth is h, the penetration width is w, the value range of h is 0.5mm-1.5mm, and the value range of w is 0.5mm-1.0mm.

[0017] Optionally, at least a portion of the sealing cover protrudes in a direction away from the sealing pin to form an escape space.

[0018] On the other hand, the present invention provides a battery, comprising a battery cover, a shell and a battery cell, wherein the battery cell is arranged in the shell, the battery cover is snap-fitted and welded to the shell, and an injection hole is provided on the battery cover, and the injection hole is sealed using the battery injection hole sealing structure in any of the above schemes.

[0019] The beneficial effects of the present invention are:

[0020] The present invention provides a battery injection hole sealing structure, comprising a battery cover, a sealing nail and a sealing cover. The battery cover is provided with an injection hole, and the injection hole can inject electrolyte into the shell. The sealing nail is made of elastic material, and the sealing nail is pressed into the injection hole by a nail pressing device. The peripheral side of the sealing nail is interference fit with the inner wall of the injection hole, and the compression rate Ψ of the sealing nail along its radial direction meets the value range of 5.08%-10.6%, thereby ensuring that the first sealing surface between the sealing nail and the injection hole has a good sealing effect. At the same time, the nail pressing device can also smoothly press the sealing nail into the injection hole, will not damage the battery cover, and is easy to assemble. A receiving groove is provided on the side of the battery cover away from the electrolyte, and a sealing cover is arranged in the receiving groove, and the projection of the shielding part of the sealing cover on the battery cover along the axial direction of the injection hole completely covers the injection hole and the sealing pin, the welding part of the sealing cover is welded to the side wall of the receiving groove and forms a second sealing surface at the welding part, and the welding part and the shielding part are connected by a buffer part; the angle between the side wall of the receiving groove and the bottom wall of the receiving groove is α, and the value range of α is 95°-175°; the outer peripheral surface of the welding part is inclined, and the angle between the outer peripheral surface of the welding part and the bottom wall of the receiving groove is β, 0°<β-α≤5°, and the welding part and the side wall of the receiving groove are interference fit. Thus, the injection hole is sealed by the two-layer sealing structure of the first sealing surface and the second sealing surface, which further improves the sealing effect of the injection hole and prevents the electrolyte from leaking from the injection hole.

[0021] The present invention also provides a battery, including a battery cover, a shell and a battery cell, wherein the battery cell is arranged in the shell, and the battery cover is buckled and welded to the shell. The battery cover is provided with an injection hole, and the injection hole is sealed by the above-mentioned battery injection hole sealing structure. The reliability of the injection hole sealing is increased by a two-layer sealing structure of a sealing nail and a sealing cover. And the compression rate Ψ of the sealing nail along the radial direction of the sealing nail is controlled within the range of 5.08%-10.6%, thereby ensuring that the sealing effect between the sealing nail and the injection hole is good, and the nail pressing device can also smoothly press the sealing nail into the injection hole without damaging the battery cover. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments of the present invention. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the contents of the embodiments of the present invention and these drawings without paying any creative work.

[0023] Figure 1 It is a schematic diagram of the assembly structure of the battery cover plate and the sealing pin in an embodiment of the present invention;

[0024] Figure 2 It is a schematic diagram of the assembly structure of the battery cover plate, the sealing pin and the sealing cover in an embodiment of the present invention;

[0025] Figure 3 It is a partial enlarged view of the assembly structure of the battery cover plate and the sealing cover in the embodiment of the present invention;

[0026] Figure 4 This is a schematic diagram of the structure of a sealing pin in an embodiment of the present invention;

[0027] Figure 5 It is a structural schematic diagram of a sealing cover in an embodiment of the present invention;

[0028] Figure 6 The structure of the battery in the embodiment of the present invention is shown in FIG. Figure 1 ;

[0029] Figure 7 The structure of the battery in the embodiment of the present invention is shown in FIG. Figure 2 .

[0030] In the figure:

[0031] 100, battery cover; 110, liquid injection hole; 120, accommodating groove; 121, bottom wall; 122, side wall; 130, arc chamfer; 200, shell; 300, sealing nail; 310, sealing part; 320, liquid injection part; 400, sealing cover; 410, shielding part; 4101, avoidance space; 420, buffer part; 430, welding part; 500, battery cell. DETAILED DESCRIPTION

[0032] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0033] In the description of the present invention, it should be noted that the orientations or positional relationships indicated by the terms "center", "up", "down", "left", "right", "vertical", "horizontal", "inside", "outside", etc. are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used for descriptive purposes and cannot be understood as indicating or implying relative importance. Among them, the terms "first position" and "second position" are two different positions, and the first feature "above", "above" and "above" the second feature include the first feature being directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. The first feature "below", "below" and "below" the second feature include the first feature being directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0034] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0035] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0036] This embodiment provides a battery filling hole sealing structure, such as Figure 1 and Figure 6 As shown, the battery filling hole sealing structure includes a battery cover 100, a sealing nail 300 and a sealing cover 400. The battery cover 100 is used to buckle with the shell 200 to form a receiving space, and the receiving space contains a battery cell 500. The battery cover 100 is provided with a filling hole 110, through which electrolyte can be injected into the shell 200. In order to prevent the electrolyte from leaking from the filling hole 110, a two-layer sealing structure is used in this embodiment to seal the filling hole 110.

[0037] Specifically, see Figure 1, the first layer of sealing structure is composed of a battery cover plate 100 and a sealing pin 300. A liquid injection hole 110 is provided on the battery cover plate 100, and the sealing pin 300 is made of an elastic material, which can be elastically deformed when under pressure. The sealing pin 300 is pressed into the liquid injection hole 110 by a nail pressing device, and the surrounding side of the sealing pin 300 is interference fit with the inner wall of the liquid injection hole 110. At this time, the sealing pin 300 is compressed along its radial direction, so that a first sealing surface is formed between the sealing pin 300 and the inner wall of the liquid injection hole 110, and the gap between the sealing pin 300 and the inner wall of the liquid injection hole 110 is blocked by the first sealing surface to prevent leakage of electrolyte. Optionally, the compression rate of the sealing pin 300 along the radial direction of the sealing pin 300 is Ψ, and the value range of Ψ is 5.08%-10.6%, where the radial direction of the sealing pin 300 is Figure 1 When the compression rate Ψ of the sealing pin 300 along its radial direction meets the above range, it can ensure that the first sealing surface between the sealing pin 300 and the injection hole 110 has a good sealing effect, and the helium leak detection rate value is within 1×10 -6 pa·m 3 At the same time, the nail pressing device can also smoothly press the sealing nail 300 into the injection hole 110 without damaging the battery cover 100.

[0038] The calculation formula of the compression rate Ψ of the sealing pin 300 along the radial direction of the sealing pin 300 is as follows:

[0039]

[0040] Wherein, D is the diameter of the portion of the sealing pin 300 located inside the injection hole 110, d is the inner diameter of the injection hole 110, and C is the radial deformation amount when the portion of the sealing pin 300 located inside the injection hole 110 is compressed.

[0041] Exemplarily, when the diameter D of the portion of the sealing nail 300 located in the injection hole 110 is 3.2 mm, the inner diameter d of the injection hole 110 may be 3.0 mm. When the diameter D of the portion of the sealing nail 300 located in the injection hole 110 is 3.5 mm, the inner diameter d of the injection hole 110 may be 3.4 mm. Of course, in other embodiments, the diameter D of the portion of the sealing nail 300 located in the injection hole 110 and the inner diameter d of the injection hole 110 may also be other values, which are not listed here. As long as the compression rate Ψ is within the above-mentioned required range, the sealing requirements can be met. Optionally, the sealing nail 300 is integrally injection molded with fluororubber, and its Shore hardness is 60 degrees to 80 degrees. Its rigidity is stronger than that of polyolefins and polypropylene. Its insulation resistance is greater than 200MΩ at an alternating voltage of 500V, and it can resist strong acid and strong alkali corrosion. After being immersed in the electrolyte, the volume change rate is less than 35%, the mass change rate is less than 20%, and the service life is long.

[0042] Furthermore, the second sealing structure is composed of a battery cover plate 100 and a sealing cover 400. Figure 2 In this embodiment, a receiving groove 120 is provided on the side of the battery cover 100 away from the electrolyte, and the receiving groove 120 is coaxial with the injection hole 110 and is connected to each other. The sealing cover 400 is arranged in the receiving groove 120, and the projection of the sealing cover 400 on the battery cover 100 along the axial direction of the injection hole 110 completely covers the injection hole 110 and the sealing nail 300. The sealing cover 400 is welded to the side wall 122 of the receiving groove 120 and forms a second sealing surface at the welding point. Among them, the axial direction of the injection hole 110 is Figure 2 Thus, the gap between the sealing cover 400 and the side wall 122 of the receiving groove 120 can be blocked by the second sealing surface between the sealing cover 400 and the battery cover plate 100, further preventing leakage of the electrolyte and achieving a better sealing effect.

[0043] See also Figure 1 and Figure 4 In this embodiment, the sealing nail 300 includes a sealing portion 310 and a liquid injection portion 320. Before injecting the electrolyte, the liquid injection portion 320 of the sealing nail 300 can be pre-installed in the liquid injection hole 110. After injecting the electrolyte, the sealing portion 310 of the sealing nail 300 is pressed into the liquid injection hole 110 using a nail pressing device. At this time, the sealing portion 310 of the sealing nail 300 and the liquid injection hole 110 are located in the same horizontal plane. The diameter of the sealing portion 310 of the sealing nail 300 is D, and the compression rate of the sealing portion 310 in the radial direction is Ψ, and the value range of Ψ is 5.08%-10.6%, wherein the radial direction of the sealing portion 310 is Figure 1 The X-axis direction.

[0044] Furthermore, an arc chamfer 130 is provided at one end of the sealing pin 300 that is pressed into the injection hole 110, that is, the end at which the injection hole 110 is connected to the accommodating groove 120. The arc chamfer 130 protrudes toward the direction of the sealing pin 300. Through the setting of the arc chamfer 130, on the one hand, the sealing portion 310 of the sealing pin 300 can be more easily pressed into the injection hole 110. On the other hand, a clearance space can also be formed at the arc chamfer 130 to reserve some space for the deformation of the sealing pin 300, thereby avoiding deviation when the pressing nail device presses the sealing pin 300, and trying to ensure that the axial direction of the sealing pin 300 is the same as the axial direction of the injection hole 110, that is, both are along the Y-axis direction.

[0045] In some embodiments, the radius of the arc chamfer 130 is r, and the value range of r is 0.1mm-0.5mm. For example, the radius r of the arc chamfer 130 can be 0.1mm, 0.2mm, 0.3mm, 0.4mm or 0.5mm, etc. The radius r of the arc chamfer 130 should not be too small. When r is too small, the clearance space is small and the guiding effect is not obvious; of course, the radius r of the arc chamfer 130 should not be too large. When r is too large, the contact surface between the sealing portion 310 of the sealing pin 300 and the inner wall of the injection hole 110 is small, that is, the area of ​​the first sealing surface is small, the sealing effect is reduced, and the sealing requirements cannot be met. Of course, in some embodiments, the arc chamfer 130 can also be replaced by an inverted cone chamfer.

[0046] Furthermore, in this embodiment, the height of the injection hole 110 along the axial direction of the injection hole 110 is H, and the height of the first sealing surface along the axial direction of the injection hole 110 is H1. The height of the first sealing surface is the effective sealing height between the injection hole 110 and the sealing portion 310 of the sealing pin 300, and the effective sealing height is also H1. Due to the existence of the arc chamfer 130, H1 is less than H. Optionally, the value range of H is 0.6mm-2.0mm, and the value range of H1 is 0.5mm-1.5mm. Exemplarily, when H is 0.6mm, r can be 0.1, and H1 is 0.5mm. When H is 2.0mm, r can be 0.5mm, and H1 is 1.5mm. Thereby, the area of ​​the first sealing surface is ensured to be large enough to ensure good sealing of the injection hole 110. It should be noted that the height H of the injection hole 110 is equal to the sum of the height H1 of the first sealing surface and the radius r of the arc chamfer 130, that is, H=H1+r. The specific value of r can be adjusted in time according to the height H of the injection hole 110 and the sealing requirements.

[0047] See also Figure 2 and Figure 5 , after the sealing nail 300 and the battery cover 100 are installed, the sealing cover 400 can be installed in the receiving groove 120 of the battery cover 100. Among them, except for the position where the injection hole 110 is set on the battery cover 100, the height of the battery cover 100 along the axial direction of the injection hole 110 is A, and the value range of A is 1.5mm-3mm. The depth of the receiving groove 120 along the axial direction of the injection hole 110 is B, and the value range of B is 0.9mm-1.3mm. For example, when the height A of the battery cover 100 is set to 1.5mm, the depth B of the receiving groove 120 is 0.9mm. When the height A of the battery cover 100 is set to 3mm, the depth of the receiving groove 120 is 1.3mm. Of course, the height A of the battery cover 100 and the depth B of the receiving groove 120 can also be set to other values ​​within the above range, which are not listed here one by one.

[0048] After the sealing cover 400 is installed in the receiving groove 120 and welded with the side wall 122 of the receiving groove 120, the end face of the sealing cover 400 facing away from the electrolyte is not higher than the end face of the battery cover 100 facing away from the electrolyte. Optionally, the distance between the end face of the sealing nail 300 facing away from the electrolyte and the end face of the battery cover 100 facing away from the electrolyte is b, and the value range of b is 0.1mm-0.5mm. For example, b can be 0.1mm, 0.2mm, 0.3mm, 0.4mm or 0.5mm, etc. Through the above arrangement, the sealing cover 400 is completely embedded in the receiving groove 120. On the one hand, it can reduce the occupied space of the battery cover 100 after assembly; on the other hand, it also avoids the sealing cover 400 from being scratched when it protrudes from the end face of the battery cover 100 facing away from the electrolyte, thereby affecting the connection strength between the sealing cover 400 and the battery cover 100.

[0049] As an optional solution, the sealing cover 400 in this embodiment includes a shielding portion 410, a buffer portion 420 and a welding portion 430, wherein the buffer portion 420 is arranged in the circumference of the shielding portion 410, the welding portion 430 is arranged in the circumference of the buffer portion 420, and the shielding portion 410, the buffer portion 420 and the welding portion 430 are all located in the accommodating groove 120, that is, the heights of the shielding portion 410, the buffer portion 420 and the welding portion 430 are all less than the depth B of the accommodating groove 120. The projection of the shielding portion 410 on the battery cover plate 100 along the axial direction of the injection hole 110 completely covers the injection hole 110 and the sealing nail 300, and the welding portion 430 is welded to the side wall 122 of the accommodating groove 120. The buffer portion 420 can effectively relieve welding stress, so that the welding strength of the welding portion 430 and the side wall 122 of the accommodating groove 120 is high, the welding quality is good, and the sealing effect of the second sealing surface formed at the welding point is good.

[0050] For example, the weld depth of the welded portion 430 and the side wall 122 of the receiving groove 120 after welding is h, and the weld width is w. The value range of h is 0.5 mm-1.5 mm, and the value range of w is 0.5 mm-1.0 mm. For example, h can be 0.5 mm, 0.8 mm, 1.0 mm, 1.2 mm, or 1.5 mm, etc. W can be 0.5 mm, 0.6 mm, 0.7 mm, 0.8 mm, 0.9 mm, or 1.0 mm, etc.

[0051] See also Figure 2 and Figure 3, the side wall 122 of the receiving groove 120 in this embodiment is inclined, and the angle between the side wall 122 of the receiving groove 120 and the bottom wall 121 of the receiving groove 120 is α. By adopting the above arrangement, on the one hand, the side wall 122 of the receiving groove 120 can play a certain guiding role when installing the sealing cover 400, which is convenient for the sealing cover 400 to be installed in the receiving groove 120, which is conducive to rapid assembly; on the other hand, the inclined side wall 122 can improve the welding yield when the sealing cover 400 is welded to the battery cover plate 100, ensuring high connection strength and good sealing effect at the welding point. Exemplarily, the value range of α is 95°-175°. For example, α can be 95°, 100°, 120°, 130°, 150°, 160° or 175°, etc.

[0052] Furthermore, the outer circumferential surface of the welding portion 430 is inclined, and the angle between the outer circumferential surface of the welding portion 430 and the bottom wall 121 of the receiving groove 120 is β, 0°<β-α≤5°. That is to say, the inclination angle of the outer circumferential surface of the welding portion 430 is greater than the inclination angle of the bottom wall 121 of the receiving groove 120. In this embodiment, the diameter of the sealing cover 400 is greater than the diameter of the receiving groove 120, so that the sealing cover 400 and the side wall 122 of the receiving groove 120 are interference fit, so that the contact between the sealing cover 400 and the battery cover plate 100 is closer, and the sealing effect of the second sealing surface is better. In addition, the sealing cover 400 is made of a rigid material, such as aluminum metal or aluminum alloy material, and the sealing cover 400 is radially ( Figure 2 The amount of deformation that can be compressed (in the X-axis direction) is small, so the interference between the sealing cover 400 and the side wall 122 of the accommodating groove 120 should not be too large.

[0053] Continue to see Figure 2 , at least part of the sealing cover 400 protrudes in a direction away from the sealing pin 300, and a relief space 4101 is formed at the protruding part. The relief space 4101 is directly opposite to the sealing pin 300, and can avoid the end of the sealing pin 300 away from the electrolyte side, that is, the relief space 4101 can avoid the sealing portion 310 of the sealing pin 300, so as to form a gap between the sealing portion 310 of the sealing pin 300 and the sealing cover 400, thereby avoiding the interaction force between the sealing pin 300 and the sealing cover 400, affecting the welding quality, and further causing the connection strength between the sealing cover 400 and the battery cover plate 100 to decrease.

[0054] In some embodiments, the shielding portion 410 of the sealing cover 400 may be raised in a direction away from the sealing pin 300, and the buffer portion 420 abuts against the bottom wall 121 of the receiving groove 120, thereby forming an escape space 4101 at the center of the shielding portion 410, and the diameter of the escape space 4101 is greater than the diameter of the sealing portion 310, so that the escape space 4101 can accommodate the sealing portion 310. In addition, in some embodiments, the shielding portion 410 of the sealing cover 400 may be raised in a direction away from the sealing pin 300, and there is a gap between the buffer portion 420 and the bottom wall 121 of the receiving groove 120, and the diameter of the escape space 4101 is greater than the diameter of the sealing portion 310. Since there is a gap between the buffer portion 420 and the bottom wall 121 of the receiving groove 120, the volume of the escape space 4101 is larger.

[0055] This embodiment also provides a battery, see Figure 6 The battery can be a square battery, which includes a battery cover 100, a shell 200 and a battery cell 500. The battery cell 500 is arranged in the shell 200, and the battery cover 100 is buckled and welded to the shell 200. A liquid injection hole 110 is provided on the battery cover 100, and the liquid injection hole 110 is sealed by the above-mentioned battery liquid injection hole sealing structure. Specifically, an elastically deformable sealing nail 300 is pressed into the liquid injection hole 110, and a rigid sealing cover 400 with a small deformation amount is provided in the accommodating groove 120 circumferentially of the liquid injection hole 110. The reliability of the sealing of the liquid injection hole 110 is increased by a two-layer sealing structure.

[0056] In addition, the compression rate of the sealing nail 300 along the radial direction of the sealing nail 300 is controlled within the range of 5.08%-10.6%. Thus, while ensuring a good sealing effect between the sealing nail 300 and the injection hole 110, the nail pressing device can also smoothly press the sealing nail 300 into the injection hole 110 without damaging the battery cover 100.

[0057] In some embodiments, the battery may also be a blade battery. Figure 7 The blade battery also includes a battery cover 100, a shell 200 and a battery cell 500. The battery cell 500 is arranged in the shell 200, and the battery cover 100 is buckled and welded to the shell 200. An injection hole 110 is provided on the battery cover 100, and the injection hole 110 is sealed using the above-mentioned battery injection hole sealing structure. Specifically, an elastically deformable sealing nail 300 is pressed into the injection hole 110, and a rigid sealing cover 400 with a small deformation amount is provided in the accommodating groove 120 circumferentially of the injection hole 110. The reliability of the sealing of the injection hole 110 is increased by a two-layer sealing structure.

[0058] The sealing pins 300 and the battery cover plate 100 of different sizes meeting the above size range requirements are preassembled, and the preassembled battery cover plate 100 is subjected to helium inspection and pressure resistance test, and the results are shown in Table 1.

[0059] Table 1

[0060]

[0061] By pre-assembling the sealing nail 300 and the battery cover plate 100 of the above size specifications and performing helium inspection, it can be seen that when the inner diameter d of the injection hole 110, the diameter D of the sealing nail 300, the compression rate Ψ, the height H1 of the first sealing surface (i.e., the effective sealing height), and the height H of the injection hole all meet the above requirements, the sealing effect of the first layer sealing structure of each sample of the embodiment is good, the pressure resistance value can reach 0.9 MPa, and the helium leak detection rate value is within 1×10 -6 pa·m 3 / s or less, meeting the sealing requirements. In addition, the compression rate Ψ of the sealing nail 300 meets the value range of 5.08%-10.6%, and the nail pressing device can easily press the sealing nail 300 into the injection hole 110, and the pressure of the nail pressing device pressing the sealing nail 300 is 1000N-1500N.

[0062] The sealing pins 300 and battery cover plates 100 of different sizes that do not meet the above size range requirements are pre-assembled, and the pre-assembled battery cover plates 100 are subjected to helium inspection and pressure resistance test. The results are shown in Table 2.

[0063] Table 2

[0064]

[0065] By pre-assembling the sealing pins 300 and the battery cover plate 100 of the above size specifications and performing helium inspection and pressure resistance tests, it can be seen that the samples in the above comparative examples either have poor sealing or encounter difficulties in assembly and production.

[0066] For example, in samples 1, 2, and 3, although the height H1 of the first sealing surface (i.e., the effective sealing height) satisfies the value range of 0.5 mm to 1.5 mm, the compression rate Ψ is lower than the minimum value of the value range of 5.08% to 10.6%. Although the nail pressing device can easily press the sealing nail 300 into the injection hole 110, the helium leak detection rate value is 1×10 -7 pa·m 3 / s or less, but the pressure resistance is poor. When the pressure value exceeds 0.9 MPa, the sealing pin 300 is easy to fall out of the injection hole 110, resulting in a defective product.

[0067] In samples 4, 5, 6, and 7, although the height H1 of the first sealing surface meets the value range of 0.5 mm to 1.5 mm, the compression rate Ψ is higher than the maximum value of the value range of 5.08% to 10.6%. -6 pa·m 3 / s or less, which meets the requirements and the withstand voltage value exceeds 0.9MPa. However, the nail pressing device encounters difficulties in pressing the sealing nail 300 into the injection hole 110, and it is necessary to increase the pressure (greater than 2000N) pressing the sealing nail 300 down, and the sealing nail 300 may not be pressed into the injection hole 110, resulting in poor assembly. In addition, during the nail pressing process, the sealing nail 300 may easily cause the battery cover 100 to crack, resulting in a defective product.

[0068] In samples 8 and 9, the compression ratio Ψ of samples 8 and 9 is less than the minimum value of the value range of 5.08%-10.6%, and the height H1 of the first sealing surface is lower than the minimum value of the value range of 0.5mm-1.5mm. Although the nail pressing device can easily press the sealing nail 300 into the injection hole 110, the helium leak detection rate value is 1×10 -7 pa·m 3 / s or less, but the pressure resistance is poor. When the pressure value exceeds 0.9 MPa, the sealing pin 300 is easy to fall out of the injection hole 110, resulting in a defective product.

[0069] In sample 10, the compression rate Ψ of sample 10 meets the value range of 5.08%-10.6%, but the height H1 of the first sealing surface is lower than the minimum value of the value range of 0.5mm-1.5mm. Although the nail pressing device can easily press the sealing nail 300 into the injection hole 110, the helium leak detection rate value is 1×10 -7 pa·m 3 / s or less, but the pressure resistance is poor. When the pressure value exceeds 0.9 MPa, the sealing pin 300 is easy to fall out of the injection hole 110, resulting in a defective product.

[0070] In samples 11 and 12, the height H1 of the first sealing surface is higher than the maximum value of the value range of 0.5 mm-1.5 mm, the compression rate Ψ meets the value range of 5.08%-10.6%, and the helium leak rate value is within 1×10 -6 pa·m 3 / s or less, meeting the helium test requirements, and the withstand voltage value can also reach 0.9MPa, meeting the sealing requirements. However, this requires increasing the height H of the injection hole 110 of the battery cover 100, which exceeds 2mm. The existing manufacturing process is not easy to manufacture, and difficulties are encountered when processing the injection hole 110. The product may have poor processing problems, and the increase in the height H of the injection hole 110 means that the height A of the battery cover 100 needs to be increased, resulting in an increase in the weight of the battery cover 100, an increase in cost, and a decrease in space utilization.

[0071] In summary, when the size specifications of the sealing nail 300 and the battery cover plate 100 meet the required values ​​of the diameter D of the sealing nail 300, the inner diameter d of the injection hole 110, the compression rate Ψ, the height H1 of the first sealing surface and the height H of the injection hole, it can basically ensure that the effect of sealing the injection hole 110 is good, the pressure resistance value meets the requirements, and it is easy to assemble.

[0072] The present embodiment also includes a second sealing structure. After the sealing pin 300, the sealing cover 400 and the battery cover 100 are assembled, a helium test and a pressure test are performed, wherein the helium leak rate value is 1×10 -8 pa·m 3 / s or less, the withstand voltage value can reach 1.2MPa, the sealing performance and compressive strength are improved, and the battery safety performance is better.

[0073] Obviously, the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.

[0074] Note that in the description of this specification, the description with reference to the terms "some embodiments", "other embodiments", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

Claims

1. A battery filling hole sealing structure, characterized in that: include: A battery cover plate (100), wherein the battery cover plate (100) is provided with a liquid injection hole (110), the liquid injection hole (110) being used to inject electrolyte into a battery housing (200), and a receiving groove (120) is provided on the battery cover plate (100) on a side facing away from the electrolyte, the receiving groove (120) being coaxial with the liquid injection hole (110) and being in communication with each other; The sealing pin (300) is made of fluororubber. The sealing pin (300) is arranged in the injection hole (110) and is interference-fitted with the inner wall of the injection hole (110). A first sealing surface is formed between the sealing pin (300) and the inner wall of the injection hole (110). The compression rate of the sealing pin (300) along the radial direction of the sealing pin (300) is Ψ, and the value range of Ψ is 5.08%-10.6%. A sealing cover (400) is arranged in the receiving groove (120), the sealing cover (400) comprises a shielding portion (410), a buffer portion (420) and a welding portion (430), the buffer portion (420) is arranged in the circumference of the shielding portion (410), the welding portion (430) is arranged in the circumference of the buffer portion (420), and the projection of the shielding portion (410) on the battery cover plate (100) along the axial direction of the injection hole (110) completely covers the injection hole (110) and the sealing pin (300), and the welding portion (430) is welded to the side wall (122) of the receiving groove (120) and forms a second sealing surface at the welding position; The side wall (122) of the containing groove (120) is arranged tilted, and the angle between the side wall (122) of the containing groove (120) and the bottom wall (121) of the containing groove (120) is α, and the value range of α is 95°-175°; the outer peripheral surface of the welding portion (430) is arranged tilted, and the angle between the outer peripheral surface of the welding portion (430) and the bottom wall (121) of the containing groove (120) is β, 0°<β-α≤5°; The height of the injection hole (110) along the axial direction of the injection hole (110) is H, and the height of the first sealing surface along the axial direction of the injection hole (110) is H1; the value range of H is 0.6 mm-2.0 mm, and the value range of H1 is 0.5 mm-1.5 mm.

2. The battery filling hole sealing structure according to claim 1, characterized in that: An arc chamfer (130) is provided at one end of the injection hole (110) communicating with the accommodating groove (120), and the arc chamfer (130) protrudes in the direction of the sealing pin (300). The radius of the arc chamfer (130) is r, and the value range of r is 0.1 mm-0.5 mm.

3. The battery liquid filling hole sealing structure according to claim 1, characterized in that: The height of the battery cover plate (100) along the axial direction of the liquid injection hole (110) is A, and the value range of A is 1.5 mm-3 mm; The depth of the accommodating groove (120) along the axial direction of the liquid injection hole (110) is B, and the value range of B is 0.9 mm-1.3 mm; After the sealing cover (400) is installed in the accommodating groove (120), the end surface of the sealing cover (400) facing away from the electrolyte is not higher than the end surface of the battery cover (100) facing away from the electrolyte, and the distance between the end surface of the sealing nail (300) facing away from the electrolyte and the end surface of the battery cover (100) facing away from the electrolyte is b, and the value range of b is 0.1 mm-0.5 mm.

4. The battery liquid filling hole sealing structure according to claim 1, characterized in that: After welding, the welding portion (430) and the side wall (122) of the receiving groove (120) have a fusion depth of h and a fusion width of w, wherein the value range of h is 0.5 mm-1.5 mm, and the value range of w is 0.5 mm-1.0 mm.

5. The battery liquid filling hole sealing structure according to claim 1, characterized in that: At least a portion of the sealing cover (400) protrudes in a direction away from the sealing pin (300) to form an escape space (4101).

6. A battery, characterized in that: The invention comprises a battery cover plate (100), a shell (200) and a battery cell (500), wherein the battery cell (500) is arranged in the shell (200), the battery cover plate (100) and the shell (200) are buckled and welded together, and a liquid injection hole (110) is provided on the battery cover plate (100), and the liquid injection hole (110) is sealed by using the battery liquid injection hole sealing structure described in any one of claims 1 to 5.

Citation Information

Patent Citations

  • Battery cover plate and battery

    CN218448386U