Prism structure, brightness enhancement film, backlight module and display device

By designing a prism combination of isosceles trapezoids and isosceles triangles and horizontal steps in the prism structure, dense and uneven peak and valley lines are formed, which solves the problem of picture interference between the brightness enhancement film and the liquid crystal glass panel and simplifies mold processing. , improve production efficiency.

CN118311701BActive Publication Date: 2024-10-01苏州弘德光电材料科技有限公司 +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410756865.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-13
Publication Date
2024-10-01
Estimated Expiration
2044-06-13

AI Technical Summary

Technical Problem

When the existing technology avoids the picture interference phenomenon between the brightness enhancement film and the liquid crystal glass panel, there are problems such as reduced area utilization due to angle cutting, long processing time of oblique-engraved molds, and difficulty in processing molds with complex microstructures. There is no effective method yet. solution.

Method used

A prism design with a stepped composite microstructure is adopted. The cross-section of the first prism part is an isosceles trapezoid, and the cross-section of the second prism part is an isosceles triangle. Horizontal steps are set at the junction to form dense peaks with uneven widths. Valley line to avoid picture interference.

Benefits of technology

It achieves the effect of avoiding screen interference, while simplifying the mold processing process, improving production efficiency, and avoiding problems of loss of area utilization and extension of processing time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118311701B_ABST
    Figure CN118311701B_ABST
Patent Text Reader

Abstract

The present invention discloses a prism structure, a brightness enhancement film, a backlight module and a display device, and relates to the field of optical film technology. The prism structure includes: at least one first prism portion; a flat-top structure, which is opened on the top of the first prism portion; and a second prism portion, whose bottom is connected to the flat-top structure; wherein the cross-section of the first prism portion is an isosceles trapezoid, the cross-section of the second prism portion is an isosceles triangle, and the bottom width of the second prism portion is smaller than the width of the flat-top structure; and at least one horizontal step is provided at the junction of at least one first prism portion and the second prism portion. The present invention solves the problem that the current method of avoiding image interference is to cut by turning an angle, but cutting by turning an angle will lose area utilization; at the same time, the oblique engraving mold will increase the mold processing time and reduce production efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of optical films, and in particular to a prism structure, a brightness enhancement film, a backlight module and a display device. Background Art

[0002] Since the optical films of the brightness enhancement film series have a regular and repetitive microstructure design, they will produce unexpected image interference with the liquid crystal glass panel that also has a regular and repetitive arrangement. In order to solve the problem of image interference, the simplest way is to perform angle cutting so that the prism structure is not parallel or perpendicular to the pixels of the liquid crystal panel, which can effectively avoid the occurrence of interference. However, this method will sacrifice the area utilization efficiency of the optical film coil and greatly increase the cost; another way is to use an oblique processing mold to first process the oblique prism structure on the microstructure mold for optical transfer, so that the transferred prism structure itself has a certain deflection angle and is not parallel to the edge of the coil, which can avoid the area loss caused by angle cutting, but this method takes a long time to process the mold and is not conducive to the long-term production of the enterprise.

[0003] In addition to the above method of rotating the microstructure to avoid image interference between the brightness enhancement film and the liquid crystal panel pixels, another method is to design a messy and irregular microstructure to avoid image interference problems by using the irregularity of the structure itself.

[0004] Patent No. CN101666461B proposes a prism sheet of a backlight module, which includes a substrate and a plurality of microstructure units; the substrate has a side, and the side has an extension direction; the plurality of microstructure units are bonded to the surface of the substrate, and the bonding surfaces bonded to the surface of the substrate have different extension directions and extension lengths; the extension directions and extension lengths of these bonding surfaces are combined to form a resultant vector, and the direction of the resultant vector forms an angle with the extension direction of the side of the substrate, and the angle range of the angle is between negative 45 degrees and positive 45 degrees. By using a fish fin-shaped irregular protrusion microstructure, image interference is avoided.

[0005] Patent No. CN105137644B proposes an interference reduction optical brightness enhancement film, which includes a substrate layer and a structural layer, wherein the structural layer is closely attached to the substrate layer, and the structural layer includes a plurality of prism structures, wherein the cross section of the prism structure is an isosceles triangle, and the angle of the vertex angle of the isosceles triangle is changed alternately. By using the alternating change of the vertex angle, the change of the prism height and the bottom width is formed to avoid image interference.

[0006] From the above solutions to avoid screen interference, cutting at an angle will result in a loss of area utilization; oblique engraving of the mold will increase mold processing time and reduce production efficiency; and although the complex microstructure solution has a variety of patterns, no matter which complex pattern is used, there is a common problem of mold processing difficulties, and the more complex the microstructure, the longer the mold processing time and the lower the efficiency. There is currently no effective solution to the above problems. Summary of the invention

[0007] Purpose of the invention: To provide a prism structure, a brightness enhancement film, a backlight module and a display device to solve the above problems existing in the prior art.

[0008] Technical solution: A prism structure, comprising: at least one first prism portion; a flat-top structure, opened on the top of the first prism portion; and a second prism portion, whose bottom is connected to the flat-top structure; wherein the cross-section of the first prism portion is an isosceles trapezoid, the cross-section of the second prism portion is an isosceles triangle, and the bottom width of the second prism portion is smaller than the width of the flat-top structure; and at least one horizontal step is provided at the junction of at least one first prism portion and the second prism portion.

[0009] Preferably, a central axis of the first prism portion is coaxially arranged with or offset from a central axis of the second prism portion.

[0010] Preferably, at least one first horizontal step is provided at one side junction of the first prism portion and the second prism portion, and / or at least one second horizontal step is provided at another side junction of the first prism portion and the second prism portion.

[0011] Preferably, when there are multiple groups of the first prism parts, and they are stacked in order from large to small, the outer surface of the first prism part forms a continuous composite microstructure with a plurality of stepped platforms.

[0012] Preferably, the first vertex angle of the first prism portion is θ1, and the second vertex angle of the second prism portion is θ2; wherein the value range of θ1 and θ2 is: 85-95°.

[0013] Preferably, the angle difference between the first vertex angle θ1 and the second vertex angle θ2 is in the range of |θ1-θ2|≤2°.

[0014] Preferably, the first vertex angle of the first prism portion is θ1, and the second vertex angle of the second prism portion is θ2; wherein θ1 and θ2 are both 90°.

[0015] Preferably, the length of the first horizontal step is W1, W1≥0, and the length of the second horizontal step is W2, W2≥0; wherein W1 and W2 are equal or unequal, and both cannot be 0 at the same time.

[0016] In order to achieve the above objective, according to another aspect of the present application, a brightness enhancement film is also provided.

[0017] The brightness enhancement film according to the present application comprises the prism structure as described above;

[0018] The invention also includes: a substrate layer, wherein the substrate layer is connected to the first prism portion at a side away from the second prism portion.

[0019] In order to achieve the above objective, according to another aspect of the present application, a backlight module is also provided.

[0020] The backlight module according to the present application includes the brightness enhancement film as described above.

[0021] In order to achieve the above objective, according to another aspect of the present application, a display device is also provided.

[0022] The display device according to the present application includes the backlight module as described above.

[0023] Beneficial effect: In the embodiment of the present application, a composite microstructure with steps is adopted, the cross-section of the first prism portion is an isosceles trapezoid, the cross-section of the second prism portion is an isosceles triangle, and the bottom width of the second prism portion is smaller than the width of the flat-top structure; and at least one horizontal step is provided at the junction of at least one of the first prism portion and the second prism portion, so that the peak and valley lines projected to the bottom become dense and uneven in width, thereby achieving the technical effect of avoiding image interference, and further solving the current method of avoiding image interference by angle cutting, but angle cutting will lose area utilization; at the same time, oblique engraving of the mold will increase the mold processing time and reduce production efficiency; and, although the messy microstructure scheme has a variety of patterns, no matter which messy pattern is used, there is a common problem of mold processing difficulty, and the more messy the microstructure, the longer the mold processing time and the worse the efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 is a three-dimensional schematic diagram of the prism structure of the present invention;

[0025] Figure 2 It is a front view of the prism structure of the present invention

[0026] Figure 3 is a schematic diagram of the outline of the prism structure of the present invention;

[0027] Figure 4is a schematic diagram of a symmetrical composite microstructure of a prism structure of the present invention;

[0028] Figure 5 is a schematic diagram of an asymmetric composite microstructure of a prism structure of the present invention;

[0029] Figure 6 is a schematic diagram of combining multiple groups of prisms of the prism structure of the present invention;

[0030] Figure 7 is a schematic diagram of the numbering of the prism structure of the present invention;

[0031] Figure 8 It is a graph of the peak-to-valley lines of equal width at the normal viewing angle of the existing prism;

[0032] Fig. 9 is a schematic structural diagram of Embodiment 1 of the prism structure of the present invention;

[0033] Fig.10 is a schematic structural diagram of Embodiment 2 of the prism structure of the present invention;

[0034] Fig.11 is a schematic structural diagram of Embodiment 3 of the prism structure of the present invention;

[0035] Fig.12 is a schematic structural diagram of Embodiment 4 of the prism structure of the present invention;

[0036] Fig.13 is a schematic structural diagram of Embodiment 5 of the prism structure of the present invention;

[0037] Fig.14 is a schematic structural diagram of Example 6 of the prism structure of the present invention;

[0038] Fig.15 is a structural schematic diagram of Example 7 of the prism structure of the present invention;

[0039] Fig.16 is a schematic structural diagram of Example 8 of the prism structure of the present invention;

[0040] Fig.17 is a schematic structural diagram of Example 9 of the prism structure of the present invention;

[0041] Fig.18 is a schematic structural diagram of Embodiment 10 of the prism structure of the present invention;

[0042] Fig.19 is a schematic structural diagram of Example 11 of the prism structure of the present invention;

[0043] Fig. 20 is a schematic structural diagram of Example 12 of the prism structure of the present invention; and

[0044] Fig.21 It is a schematic structural diagram of comparative example 2 of the prism structure of the present invention.

[0045] The accompanying drawings are marked as follows:

[0046] 10. a first prism portion;

[0047] 101, flat roof structure; 1011, first level step; 1012, second level step;

[0048] 20. A second prism portion. DETAILED DESCRIPTION

[0049] In order to enable those skilled in the art to better understand the solution of the present application, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present application.

[0050] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequential order. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present application described here. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0051] In addition, the terms "installed", "set", "provided with", "connected", "connected", and "socketed" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0052] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.

[0053] The present application relates to a prism structure, a brightness enhancement film, a backlight module and a display device. Figure 1-7As shown, the prism structure includes: a combination of at least a first prism portion 10 and a second prism portion 20; the prism structure combination refers to a part of an optical device or instrument, including one or more prisms for processing light. In optics, prisms are usually used to refract, reflect or disperse light to achieve various optical effects.

[0054] Furthermore, a plurality of first prism portions 10 arranged in an orderly array in the horizontal direction form a first prism layer, which can achieve good optical performance.

[0055] The flat-top structure 101 is provided on the top of the first prism portion 10 . By providing the flat-top structure 101 on the top of the first prism portion 10 , the lower half of the microstructure body is formed, and at the same time, the effect of facilitating molding and coordinating with other components can be achieved.

[0056] The bottom of the second prism portion 20 is connected to the flat-top structure 101 ; by connecting the bottom of the second prism portion 20 to the flat-top structure 101 , a protruding upper part of the microstructure can be formed.

[0057] The cross section of the first prism part 10 is an isosceles trapezoid, the cross section of the second prism part 20 is an isosceles triangle, and the bottom width of the second prism part 20 is smaller than the width of the flat-top structure 101; and at least one horizontal step is provided at the junction of at least one of the first prism part 10 and the second prism part 20. By setting the cross section of the first prism part 10 to an isosceles trapezoid, the top can be horizontal, so that the required optical performance can be obtained; at the same time, a good matching effect with the second prism part 20 can be achieved.

[0058] By setting the cross section of the second prism portion 20 to be in the shape of an isosceles triangle, good optical performance can be achieved, and at the same time, the effect of being easy to implement and convenient to operate can be achieved.

[0059] The bottom width of the second prism portion 20 is smaller than the width of the flat-top structure 101 ; the desired microstructure can be formed by compounding, thereby obtaining the desired optical performance.

[0060] At least one horizontal step is provided at the junction of at least one of the first prism parts 10 and the second prism part 20. By providing at least one horizontal step at the junction of the first prism part 10 and the second prism part 20, the effect of changing the prism structure can be achieved, thereby forming a composite microstructure with steps, and then the peak and valley lines projected to the bottom become dense and uneven in width, and finally a good anti-interference effect is achieved.

[0061] In order to better understand the technical problem to be solved by this application, the following explanation is given:

[0062] like Figure 8As shown, what interferes with the liquid crystal glass pixels are mainly the lines formed by the peaks and valleys of the prism structure, which are caused by the consistent regularity of the lines.

[0063] Therefore, the prism needs to be designed so that the tip shakes left and right, or up and down, or the prisms are arranged side by side with high and low numbers, so as to avoid the appearance of lines with uniform spacing.

[0064] Alternatively, it is known that irregular microstructure shapes can also avoid the image interference problem, but special-shaped microstructure tools that are not isosceles triangular prisms are not very common.

[0065] Therefore, obtaining a random arrangement from a new mold processing method is an approach that can be further developed.

[0066] The present invention adopts secondary processing to produce a microstructure with a stepped platform, such as Figure 1-2 shown.

[0067] The stepped terrace microstructure consists of two sets of prisms, such as Figure 3 As shown, the first prism (large prism) has a flat top structure 101, forming the lower half of the microstructure body, and the second prism (small prism) forms the convex upper half of the microstructure. Among them, the large prism alone is a traditional brightness enhancement film prism structure.

[0068] Depend on Figure 4 It can be seen that due to the composition of large and small prisms, a composite microstructure with steps is formed. Therefore, compared with the traditional prism structure, the peak and valley lines projected to the bottom become dense and the width is uneven.

[0069] or Figure 5 As shown, the second prism can be tilted to either side, and the resulting peak-to-valley line spacing will be more chaotic.

[0070] By adopting the above-mentioned shape, peak-valley lines with non-fixed spacing can be formed, thereby avoiding the image interference phenomenon that may be formed between the microstructure optical film and the pixels of the liquid crystal glass panel.

[0071] This method does not increase the difficulty of microstructure processing, and only requires one processing with a flat-top prism tool, and then a secondary processing with a sharp-angle prism tool at the same displacement speed to simply form the required microstructure. It is an effective method to obtain an uneven peak-valley line structure with a regular processing procedure to avoid image interference.

[0072] or Figure 6 As shown, three or more groups of prisms may be combined to form other step prism microstructures. The design conditions of the microstructure are the same as above.

[0073] From the above description, it can be seen that the present application achieves the following technical effects:

[0074] In the embodiment of the present application, a stepped composite microstructure is adopted, wherein the cross section of the first prism portion 10 is an isosceles trapezoid, the cross section of the second prism portion 20 is an isosceles triangle, and the bottom width of the second prism portion 20 is smaller than the width of the flat-top structure 101; and at least one horizontal step is provided at the junction of at least one of the first prism portion 10 and the second prism portion 20, so that the peak and valley lines projected to the bottom become dense and have uneven widths, thereby achieving the technical effect of avoiding image interference, and further solving the current method of avoiding image interference by angle cutting, but angle cutting will lose area utilization; at the same time, oblique engraving of the mold will increase the mold processing time and reduce production efficiency; and, although the messy microstructure scheme has a variety of patterns, no matter which messy pattern is used, there is a common problem of mold processing difficulties, and the more messy the microstructure, the longer the mold processing time and the worse the efficiency.

[0075] Further, the central axis of the first prism portion 10 is coaxially arranged or offset from the central axis of the second prism portion 20. It can be understood that by coaxially arranging the central axis of the first prism portion 10 and the central axis of the second prism portion 20, it is possible to obtain a plurality of steps symmetrical about the central axis.

[0076] By setting the central axis of the first prism portion 10 and the central axis of the second prism portion 20 in an offset manner, the bottom of the second prism portion 20 is placed at any position other than the central axis of the first prism portion 10, and the bottom of the second prism portion 20 needs to be completely on the flat-top structure 101; at this time, the second prism portion 20 is offset and set on the flat-top structure 101 of the first prism portion 10, even if the small prisms are biased to either side, so that the spacing between the peak and valley lines formed is more chaotic.

[0077] With such a design, peak-to-valley lines with non-fixed spacing can be formed, thereby avoiding the image interference phenomenon that may be formed between the microstructure optical film and the pixels of the liquid crystal glass panel.

[0078] Further, at least one first horizontal step 1011 is provided at one side of the intersection of the first prism portion 10 and the second prism portion 20, and / or at least one second horizontal step 1012 is provided at the other side of the intersection of the first prism portion 10 and the second prism portion 20. It can be understood that, because the bottom width of the second prism portion 20 is smaller than the width of the flat-top structure 101, and after the second prism portion 20 is completely disposed on the flat-top structure 101 of the first prism portion 10, no matter where the second prism portion 20 is located on the flat-top structure 101, a horizontal step will be reserved at both ends or at either end of the flat-top structure 101;

[0079] For example, the second prism portion 20 is disposed at the leftmost side close to the flat-top structure 101. At this time, a horizontal step is reserved on the right side of the flat-top structure 101.

[0080] The second prism portion 20 is arranged at the rightmost side close to the flat-top structure 101. At this time, a horizontal step is reserved on the left side of the flat-top structure 101.

[0081] The second prism portion 20 is arranged in the middle of the flat-top structure 101. At this time, a horizontal step is reserved on both the left and right sides of the flat-top structure 101. Of course, there are two other situations regarding the position of the second prism: 1. If the central axis position of the second prism portion 20 is aligned with the vertical center line of the flat-top structure 101, at this time, the horizontal steps on both sides are equal, and at the same time, the microstructure formed by the first prism portion 10 and the second prism portion 20 is arranged symmetrically about the central axis.

[0082] 2. If the central axis position of the second prism portion 20 is not consistent with the vertical center line position of the flat-top structure 101, the horizontal steps on both sides are not equal. At the same time, the shape of the microstructure formed by the first prism portion 10 and the second prism portion 20 is more irregular.

[0083] Furthermore, when there are multiple groups of the first prism parts 10, and they are stacked in order from large to small, the outer surface of the first prism part 10 forms a continuous composite microstructure with a plurality of stepped platforms. It can be understood that by combining multiple groups of prisms, a composite microstructure with a plurality of stepped platforms can be formed on the outer surface of the prism, thereby further improving the shape of the prism so that the outer surface of the prism has a better anti-interference effect.

[0084] like Figure 7 As shown, the first vertex angle of the first prism portion 10 is θ1, and the second vertex angle of the second prism portion 20 is θ2; wherein the value range of θ1 and θ2 is: 85-95°. It can be understood that by setting the vertex angles of the first prism portion 10 and the second prism portion 20 in the above range, a prism with an isosceles right triangle structure or a similar structure can be obtained and the prism can be easily processed and formed while obtaining the required optical performance.

[0085] Furthermore, the angle difference between the first vertex angle θ1 and the second vertex angle θ2 is in the range of |θ1-θ2|≤2°. It can be understood that a good constraint effect on the shape of the prism can be achieved, and at the same time, a good matching effect of the two prisms can be achieved, thereby ensuring good optical performance. If the angle difference is too large, there is a risk that the microstructure cannot be processed.

[0086] Further, the first vertex angle of the first prism portion 10 is θ1, and the second vertex angle of the second prism portion 20 is θ2; wherein θ1 and θ2 are both 90°. It can be understood that by adopting the form of isosceles right triangles for both prism portions, the effect of easy processing and forming can be achieved. At the same time, a flat-top structure 101 is provided on the top of the first prism, and cooperates with the second prism portion 20, so as to obtain the desired anti-interference optical performance.

[0087] Further, the length of the first horizontal step 1011 is W1, W1≥0, and the length of the second horizontal step 1012 is W2, W2≥0; wherein W1 and W2 are equal or unequal, and both cannot be 0 at the same time. It can be understood that by limiting the length of the first horizontal step 1011 and the length of the second horizontal step 1012 as above, the desired optical shape can be obtained.

[0088] Specifically, when W1=0 and W2 is not 0, the second prism portion 20 is disposed close to the left side of the flat-top structure 101 of the first prism portion 10 .

[0089] When W1 is not 0 and W2 = 0, the second prism portion 20 is disposed close to the right side of the flat-top structure 101 of the first prism portion 10 .

[0090] When W1 and W2 are equal and both are not 0, the second prism portion 20 is located at the center of the flat-top structure 101 of the first prism portion 10 .

[0091] When W1 and W2 are not equal and are not 0, the second prism portion 20 is located in the middle of the flat-top structure 101 of the first prism portion 10 , and may be disposed close to any side of the flat-top structure 101 .

[0092] The specific examples are further described below:

[0093] First, in the following embodiments and comparative examples, a non-rotating prism microstructure is used to observe the image performance to ensure the accuracy of the results.

[0094] Secondly, during observation, the brightness enhancement film is placed in the backlight module, and a diffusion film is placed on it, and then covered with a corresponding liquid crystal glass panel, and then observed visually.

[0095] It should be noted that the various types of LCD display brands used in the test results are common and easily available products on the market, so there is no specialness in the results.

[0096] Example 1

[0097] like Fig. 9As shown, the bottom width of the first prism portion 10 is 70 μm, the height H from the bottom edge to the flat-top structure 101 is 30 μm, the first vertex angle θ1 is 90°, and the length W1 of the first horizontal step 1011 is 2 μm; the second vertex angle θ2 of the second prism portion 20 is 90°, and the length W2 of the second horizontal step 1012 is 0.

[0098] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed no interference, Brand 2 showed slight interference, and Brand 3 showed no interference.

[0099] Example 2

[0100] like Fig.10 As shown, the difference between Embodiment 2 and Embodiment 1 is that the length W2 of the second horizontal step 1012 is 1 μm.

[0101] At this time, after testing, the brightness enhancement film display results are: Brand 1 shows no interference, Brand 2 shows no interference, and Brand 3 shows no interference.

[0102] Example 3

[0103] like Fig.11 As shown, the difference between Embodiment 3 and Embodiment 1 is that the length W2 of the second horizontal step 1012 is 2 μm.

[0104] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed no interference, Brand 2 showed slight interference, and Brand 3 showed slight interference.

[0105] Example 4

[0106] like Fig.12 As shown, the difference between Embodiment 4 and Embodiment 1 is that the length W2 of the second horizontal step 1012 is 3 μm.

[0107] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed slight interference, Brand 2 showed no interference, and Brand 3 showed no interference.

[0108] Example 5

[0109] like Fig.13 As shown, the difference between Example 5 and Example 1 is that the length W1 of the first horizontal step 1011 is 3 μm.

[0110] At this time, after testing, the brightness enhancement film display results are: Brand 1 shows no interference, Brand 2 shows no interference, and Brand 3 shows no interference.

[0111] Example 6

[0112] like Fig.14As shown, the difference between Example 6 and Example 1 is that the length W1 of the first horizontal step 1011 is 3 μm; and the length W2 of the second horizontal step 1012 is 3 μm.

[0113] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed slight interference, Brand 2 showed slight interference, and Brand 3 showed slight interference.

[0114] Example 7

[0115] like Fig.15 As shown, the difference between Example 7 and Example 1 is that the length W1 of the first horizontal step 1011 is 3 μm; and the length W2 of the second horizontal step 1012 is 5 μm.

[0116] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed slight interference, Brand 2 showed no interference, and Brand 3 showed slight interference.

[0117] Example 8

[0118] like Fig.16 As shown, the difference between Example 8 and Example 1 is that the height H from the bottom edge to the flat-top structure 101 is 16 μm; and the length W2 of the second horizontal step 1012 is 3 μm.

[0119] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed slight interference, Brand 2 showed slight interference, and Brand 3 showed slight interference.

[0120] Example 9

[0121] like Fig.17 As shown, the difference between Example 9 and Example 1 is that the height H from the bottom edge to the flat-top structure 101 is 16 μm; and the length W1 of the first horizontal step 1011 is 3 μm.

[0122] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed no interference, Brand 2 showed slight interference, and Brand 3 showed no interference.

[0123] Example 10

[0124] like Fig.18 As shown, the difference between Example 10 and Example 1 is that the height H from the bottom edge to the flat-top structure 101 is 16 μm, the length W1 of the first horizontal step 1011 is 3 μm, and the length W2 of the second horizontal step 1012 is 5 μm.

[0125] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed slight interference, Brand 2 showed no interference, and Brand 3 showed slight interference.

[0126] Embodiment 11

[0127] like Fig.19 As shown, the difference between Example 11 and Example 1 is that the length W1 of the first horizontal step 1011 is 3 μm; the second vertex angle θ2 of the second prism portion 20 is 92°, and the length W2 of the second horizontal step 1012 is 5 μm.

[0128] At this time, after testing, the brightness enhancement film display results are: Brand 1 shows no interference, Brand 2 shows no interference, and Brand 3 shows no interference.

[0129] Example 12

[0130] like Fig. 20 As shown, the difference between Example 12 and Example 1 is that the first vertex angle θ1 is 92°, the length W1 of the first horizontal step 1011 is 3 μm, and the length W2 of the second horizontal step 1012 is 4 μm.

[0131] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed slight interference, Brand 2 showed no interference, and Brand 3 showed no interference.

[0132] Comparative Example 1

[0133] The difference between Comparative Example 1 and Example 1 is that the conventional brightness enhancement film only has the first prism layer 1 .

[0134] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed obvious interference, Brand 2 showed obvious interference, and Brand 3 showed obvious interference.

[0135] Comparative Example 2

[0136] like Fig.21 As shown, the difference between Comparative Example 2 and Example 1 is that the height H from the bottom edge to the flat-top structure 101 is 16 μm, the length W1 of the first horizontal step 1011 is 3 μm, and the length W2 of the second horizontal step 1012 is 3 μm.

[0137] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed obvious interference, Brand 2 showed no interference, and Brand 3 showed obvious interference.

[0138] Comparative Example 3

[0139] The difference between Comparative Example 3 and Example 1 is that the first vertex angle θ1 is 75°; and the second vertex angle θ2 is 75°.

[0140] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed slight interference, Brand 2 showed slight interference, and Brand 3 showed slight interference.

[0141] Comparative Example 4

[0142] The difference between Comparative Example 4 and Example 1 is that the first vertex angle θ1 is 100°; and the second vertex angle θ2 is 100°.

[0143] At this time, after testing, the brightness enhancement film showed the following results: Brand 1 showed slight interference, Brand 2 showed slight interference, and Brand 3 showed slight interference.

[0144] The results of various embodiments and comparative examples are shown in Table 1:

[0145] Table 1

[0146]

[0147] From the above test results we can see that:

[0148] 1. It can be seen from Examples 1-4 and Comparative Example 1 that, under the premise that other parameters remain unchanged, as the length of the second horizontal step 1012 continues to increase, although slight interference may occur, the overall anti-interference capability can still be improved.

[0149] 2. It can be seen from Examples 5-7 and Comparative Example 1 that, under the premise that other parameters remain unchanged, by increasing the length of the first horizontal step 1011 and the length of the second horizontal step 1012, although slight interference may occur, the overall anti-interference ability can still be improved.

[0150] 3. It can be seen from Examples 1, 8-10 and Comparative Example 1 that, under the premise that other parameters remain unchanged, by reducing the height H from the bottom edge to the flat-top structure 101 and changing the length of the first horizontal step 1011 and the length of the second horizontal step 1012, although slight interference may occur, the overall anti-interference ability can still be improved.

[0151] 4. It can be seen from Examples 11-12 and Comparative Example 1 that, under the premise that other parameters remain unchanged, by changing the first vertex angle θ1 and the second vertex angle θ2, although slight interference may occur, the overall anti-interference ability can still be improved.

[0152] 5. It can be seen from Examples 1, 8-10 and Comparative Examples 1-2 that, under the premise that other parameters remain unchanged, by reducing the height H from the bottom edge to the flat-top structure 101 and setting the length of the first horizontal step 1011 and the length of the second horizontal step 1012 to be equal, a more obvious interference phenomenon will appear. It is particularly noted that in Comparative Example 2, the height H is 16 μm, and the first and second horizontal steps are both 3 μm, so that the protruding height of the second prism is also exactly 16 μm, resulting in a relatively consistent projection width of the peak-to-valley line, small variability, and reduced anti-interference ability.

[0153] 6. It can be seen from Example 1, Example 3, Example 6 and Comparative Example 2 that although the overall anti-interference effect of Comparative Example 2 is not good, it also has a good anti-interference effect in some brands. Therefore, under the premise that the horizontal steps on both sides are equal, the anti-interference effect is occasionally poor; therefore, the unequal horizontal steps on both sides are the most preferred state, followed by the symmetrical state. Compared with Example 3 and Example 6, although these two embodiments have equal first and second horizontal step widths and belong to the left-right symmetrical structure, the height H is larger, so that the protruding height of the second prism is significantly smaller than H, resulting in a large change in the peak-to-valley line width, avoiding the risk of interference. Therefore, it can be seen that the setting of the height H and the horizontal step width should try to avoid making the peak-to-valley line width present a fixed value, which can avoid the risk of interference to a large extent.

[0154] 7. It can be seen from Example 1, Comparative Example 1 and Comparative Examples 3-4 that, under the premise that other parameters remain unchanged, changing the first vertex angle θ1 and the second vertex angle θ2, although the anti-interference ability is improved, the optical gain effect is greatly attenuated due to the special angle values, and it cannot be used on brightening film products.

[0155] In summary, from the results, although it is difficult to predict the image interference caused by the prism structure on the liquid crystal glass panel, it can be observed after the actual finished product is assembled to verify the interference effect. Compared with comparative example 1-2, although slight interference occurs in some images in embodiment 1-12, it is obvious that the image interference has been greatly improved and alleviated compared with the comparative example. In addition, the design condition of non-interference can be obtained from the size and arrangement differences of any prism microstructure with stepped platform.

[0156] The present invention also has the following beneficial effects:

[0157] The present invention proposes a new chaotic microstructure design, which avoids the long time and difficulty of mold processing and can obtain a disordered interference-avoiding microstructure with good effect in a simple processing method.

[0158] The present application also relates to a brightness enhancement film, comprising the prism structure as described above;

[0159] The invention further comprises: a substrate layer, wherein the substrate layer is connected to the first prism part 10 at a side away from the second prism part 20 .

[0160] Specifically, the substrate layer is the base layer of the entire film, and is usually composed of one or more materials. Preferably, the material of the substrate layer includes, but is not limited to, any one of polyethylene terephthalate (PET), polycarbonate (PC) or polymethyl methacrylate (PMMA), which has excellent mechanical properties, transparency and heat resistance, and serves as the main substrate layer in the composite brightness enhancement film, providing strength and stability while maintaining the transparency of the material.

[0161] More preferably, the thickness of the substrate layer is 50-250 um. It can be understood that a good supporting effect can be achieved.

[0162] The present application also relates to a backlight module that can be used in a liquid crystal display device to improve the display quality of the display device. The backlight module of this embodiment includes a light guide plate and other known structures such as a light emitting unit, which will not be described in detail here. The light guide plate is provided with the above-mentioned brightness enhancement film on one side of the light emitting surface.

[0163] The present application also relates to a display device, comprising a display panel and the above-mentioned backlight module, wherein the backlight module is used to provide a backlight source for the display panel.

[0164] The display device of this embodiment may be any product or component with a display function, such as a liquid crystal panel, electronic paper, a liquid crystal television, a liquid crystal display, a digital photo frame, a mobile phone, and a tablet computer.

[0165] The preferred embodiments of the present invention are described in detail above in conjunction with the accompanying drawings. However, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the present invention, various equivalent transformations can be made to the technical scheme of the present invention, and these equivalent transformations all belong to the protection scope of the present invention.

Claims

1. A prismatic structure, characterized in that: include: At least one first prism portion (10); A flat-top structure (101) is provided on the top of the first prism portion (10); and A second prism portion (20), the bottom of which is connected to the flat-top structure (101); The cross section of the first prism portion (10) is an isosceles trapezoid, the cross section of the second prism portion (20) is an isosceles triangle, and the bottom width of the second prism portion (20) is smaller than the width of the flat-top structure (101); and at least one horizontal step is provided at the junction of at least one of the first prism portion (10) and the second prism portion (20); The first prism parts (10) are in multiple groups and are stacked in order from large to small, and the outer surface of the first prism parts (10) forms a continuous composite microstructure with a plurality of stepped platforms; The length of the first prism portion (10) is the same as the length of the second prism portion (20).

2. The prism structure according to claim 1, characterized in that: The central axis of the first prism portion (10) and the central axis of the second prism portion (20) are coaxially arranged or offset from each other.

3. The prism structure according to claim 1, characterized in that: At least one first horizontal step (1011) is provided at a junction of one side of the first prism portion (10) and the second prism portion (20), and / or at least one second horizontal step (1012) is provided at a junction of the other side of the first prism portion (10) and the second prism portion (20).

4. The prism structure according to claim 1, characterized in that: The first vertex angle of the first prism portion (10) is θ1, and the second vertex angle of the second prism portion (20) is θ2; wherein the value range of θ1 and θ2 is: 85-95°.

5. The prism structure according to claim 4, characterized in that: The angle difference between the first vertex angle θ1 and the second vertex angle θ2 has a value range of |θ1-θ2|≤2°.

6. The prism structure according to claim 1, characterized in that: The first vertex angle of the first prism portion (10) is θ1, and the second vertex angle of the second prism portion (20) is θ2; wherein θ1 and θ2 are both 90°.

7. The prism structure according to claim 3, characterized in that: The length of the first horizontal step (1011) is W1, W1≥0, and the length of the second horizontal step (1012) is W2, W2≥0; wherein W1 and W2 are equal or unequal, and both cannot be 0 at the same time.

8. Brightness enhancement film, characterized in that: comprising a prism structure as claimed in any one of claims 1 to 7; It also comprises: a substrate layer, wherein the substrate layer is connected to the first prism portion (10) at a side away from the second prism portion (20).

9. A backlight module, characterized in that: Comprising the brightness enhancement film as claimed in claim 8.

10. A display device, characterized in that Comprising the backlight module as claimed in claim 9.