A cavity device and monitoring method for real-time monitoring of the surface smoothness of trench deposits.

By using a cavity device based on a plasma reaction chamber in the manufacturing of microelectronic devices and using reflected light to observe the flatness of the trench deposition surface, the problems of limited measurement range, difficulty in capturing dynamic changes and high equipment cost in the existing technology are solved. Real-time, economical flatness monitoring and analysis is achieved.

CN118392085BActive Publication Date: 2024-10-29SHANGHAI BANGXIN SEMI TECHNOLOGY CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410843320.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-27
Publication Date
2024-10-29
Estimated Expiration
2044-06-27

AI Technical Summary

Technical Problem

Existing technologies have problems such as limited measurement range, inability to capture dynamic changes, high equipment costs, complex operations, and process interruptions when monitoring the surface flatness of trench deposition in microelectronic device manufacturing.

Method used

Using a cavity device based on a plasma reaction cavity, through external light sources, light-transmitting sheets, double-layer multi-core optical fibers, collimation equipment and spectral analysis equipment, the flatness of the trench deposition surface is observed using reflected light, and the reflected light is monitored and analyzed in real time. Strength, avoid process interruptions, and reduce equipment costs.

Benefits of technology

It realizes real-time monitoring of trench deposition surface flatness without interrupting the process, reduces costs, simplifies data analysis, improves the ability to capture dynamic changes, and enhances the signal-to-noise ratio.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118392085B_ABST
    Figure CN118392085B_ABST
Patent Text Reader

Abstract

A cavity device and monitoring method for real-time monitoring of the surface flatness of a groove deposition relate to the field of microelectronic device manufacturing technology. The device comprises: an external light source, a double-layer multi-core optical fiber, a collimation device, a spectrum analysis device, a light-transmitting sheet, and a sealing device. With this structure, the surface flatness of the groove deposition can be observed using reflected light during the etching process, and the flatness of the upper surface of the deposited film layer can be reflected by real-time observation of the reflected light intensity on the upper surface of the deposited film layer. The device and method can realize real-time monitoring of the surface flatness without interrupting the process during the groove deposition process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of microelectronic device manufacturing, and in particular to a cavity device and a monitoring method for real-time monitoring of groove deposition surface flatness. Background Art

[0002] Trench deposition is a thin film deposition technique that is commonly used to form trench structures in microelectronic device manufacturing. A trench is a recess or ridge etched into the surface of a semiconductor material. Trench deposition technology can fill these trenches with materials to change or enhance the performance of semiconductor devices.

[0003] Trench deposition usually uses methods such as chemical vapor deposition (CVD) or physical vapor deposition (PVD). In chemical vapor deposition, the required material gas is introduced into the trench, and solid material is deposited on the surface through chemical reaction. In physical vapor deposition, the material is deposited on the trench surface in the form of atoms or molecules through physical means such as thermal evaporation and sputtering.

[0004] Trench deposition technology has a wide range of applications in microelectronic devices, such as forming a trench between the gate and source / drain in a transistor to improve electronic conduction performance. In addition, trench deposition can also be used to manufacture MEMS (micro-electromechanical systems) devices, optical devices, and biosensors.

[0005] In the manufacture of microelectronic devices, the flatness of groove deposition is of great significance to the functional performance, structural stability, process consistency, etc. of the device, and will also affect the quality and performance of downstream process steps. Controlling and monitoring the flatness of groove deposition is a key step to ensure the quality and performance of the device. By adopting appropriate process parameters, real-time monitoring and feedback, the flatness of the groove can be optimized and the device can be ensured to have consistent quality and performance during the production process.

[0006] At present, the industry generally uses in-situ surface profile measurement technology to interrupt the process, take samples and slices to observe the surface flatness of the groove deposition. In-situ surface profile measurement is a method for real-time monitoring of the surface flatness of the groove deposition. The following are several commonly used in-situ surface profile measurement methods:

[0007] In-situ Scanning Electron Microscope (SEM): In-situ SEM can be used to observe and measure the surface morphology and geometry during the trench deposition process in real time. SEM uses an electron beam to scan the sample surface and generates an image by detecting reflected and scattered electron signals. By continuously scanning the sample surface, real-time surface images can be obtained to evaluate the flatness of the trench.

[0008] In-situ atomic force microscopy (AFM): In-situ AFM uses the tip of the probe to scan the sample surface and measure the topology and height differences of the surface. By performing in-situ AFM measurements during the trench deposition process, the surface morphology of the deposited film can be observed and recorded in real time, thereby evaluating the flatness of the trench.

[0009] In-situ interferometry: Interferometry can evaluate the flatness of the groove by measuring the relative thickness variation between the deposited film and the substrate. In-situ interferometry uses the density, spacing, and shape variation of the interference fringes to infer the surface flatness of the deposited film. This method can provide real-time surface profile information.

[0010] In-situ surface profilometry can provide real-time surface topography and geometry information during the trench deposition process to evaluate the flatness of the trench. Through real-time monitoring, problems in the deposition process can be detected and corrected in a timely manner, and deposition parameters can be optimized to ensure that the trench flatness meets the requirements. However, there are also some disadvantages:

[0011] Limited measurement range: In-situ surface profiling methods can usually only measure small areas. For example, in-situ SEM and AFM can usually only scan the surface in a very small area and cannot fully evaluate the entire groove. This may lead to an insufficient understanding of the overall surface flatness.

[0012] Inability to capture dynamic changes: In-situ surface profilometry methods are primarily applicable to static or slowly changing surfaces. When there are rapid changes or dynamic evolutions in the trench deposition process, these methods may not be able to provide accurate real-time measurements. Therefore, other methods are needed to monitor the deposition process with rapid and dynamic changes.

[0013] High requirements for equipment: In-situ surface profile measurement methods require dedicated equipment, such as SEM, AFM or interferometer. These devices are usually expensive and require professional technicians to operate and maintain. This increases the cost of the equipment and the complexity of use.

[0014] Interruption of process flow: In-situ surface profiling methods usually require the sample to be removed from the deposition apparatus for measurement, which interrupts the deposition process. This can cause interruptions and delays in the process flow, increasing production time and costs.

[0015] Complex data interpretation and analysis: The data generated by in-situ surface profilometry methods usually require further interpretation and analysis to extract relevant information about the groove flatness. This requires complex processing and interpretation of the data, requiring expertise and experience. Summary of the invention

[0016] In view of the shortcomings of the in-situ surface profile measurement method currently commonly used in the industry in monitoring the surface flatness of groove deposition, the present disclosure provides a chamber device and a monitoring method for real-time monitoring of the surface flatness of groove deposition. With the device, the surface flatness of groove deposition can be observed using reflected light during the etching process, and the flatness of the upper surface of the deposited film layer can be reflected by real-time observation of the reflected light intensity on the upper surface of the deposited film layer. In this way, real-time monitoring of the surface flatness is achieved without interrupting the process during the groove deposition process.

[0017] The present disclosure provides a chamber device for real-time monitoring of the surface flatness of a groove deposition, a plasma reaction chamber based on a wafer surface groove deposition process, and mainly includes: an external light source, a light-transmitting sheet, a sealing device, a double-layer multi-core optical fiber, a collimation device, and a spectrum analysis device, wherein:

[0018] The light-transmitting sheet is installed at the light-transmitting hole on the upper part of the reaction chamber and is sealed on the upper cover plate by a sealing device;

[0019] The collimation device and the double-layer multi-core optical fiber are both arranged outside the reaction chamber, the output end of the collimation device is aligned with the light-transmitting sheet, and the input end is connected to the double-layer multi-core optical fiber;

[0020] The double-layer multi-core optical fiber includes: two inner and outer ring optical fibers, wherein the outer ring optical fibers have multiple fibers and surround the inner ring optical fibers; wherein the inner ring optical fibers are used to inject light into the cavity, and the outer ring optical fibers are used to collect light reflected from the cavity;

[0021] The external light source is connected to the inner ring optical fiber of the double-layer multi-core optical fiber, and is vertically irradiated to the surface of the wafer to be deposited through the collimating device and the light-transmitting sheet, and the reflected light is received by the outer ring optical fiber of the double-layer multi-core optical fiber;

[0022] The outer ring optical fiber is connected to a spectrum analysis device for analyzing the intensity of the reflected light to determine the flatness of the deposition result on the groove surface.

[0023] Furthermore, since the use environment of the present disclosure is in a plasma reaction chamber, there is an excited plasma glow inside the chamber during use, which greatly interferes with the capture of reflected light, which is a problem that needs to be solved. In this regard, the external light source of the present disclosure preferably uses a broadband light source, and the wavelength is far away from the glow wavelength of plasma radiation, avoiding the band of spontaneous radiation excited by the reactant plasma in the reaction chamber, and selecting an observation band to increase the signal-to-noise ratio of the signal captured by the spectrometer.

[0024] Furthermore, the external light source is a halogen lamp or a xenon lamp.

[0025] Furthermore, the double-layer multi-core optical fiber uses inner and outer ring optical fibers with equal diameters, with 1 inner ring and 6 outer rings. The inner layer is incident and the outer layer is reflected, which better captures the reflected light. No matter from which angle the slightly divergent incident light is emitted, it can be captured by the outer ring optical fiber.

[0026] Furthermore, the light-transmitting sheet is made of sapphire.

[0027] The method for monitoring the flatness of the groove deposition surface of the above-mentioned chamber device comprises the following steps:

[0028] The light entering the cavity is collimated by the collimation device, and the angle between the light path and the wafer surface is calibrated and adjusted to the vertical direction;

[0029] The outer ring of optical fibers captures the reflected light;

[0030] The spectrum analysis equipment connected to the outer ring optical fiber analyzes the intensity of the captured reflected light, and analyzes the flatness of the groove deposition on the wafer surface based on the intensity of the reflected light.

[0031] Compared with the prior art, the beneficial effects of the present invention are:

[0032] (1) By using the structure provided by the present disclosure, the surface flatness of the groove deposition can be measured in real time using the reflection method. The reflected light is captured by the reflection principle, and the flatness of the surface to be measured is analyzed by analyzing the captured light intensity. Only the intensity of the reflected light is analyzed, and no analysis result is required. The device is more economical and practical, and the response is faster.

[0033] (2) It can capture dynamic changes during the process without interrupting the process flow, without the need to purchase additional SEM equipment, which can save costs compared to existing methods;

[0034] (3) The data analysis is very simple. It only requires real-time observation of the light intensity signal received by the spectrometer. The flatness of the deposited film surface can be analyzed by analyzing the reflected light intensity signal, which provides a very practical way to analyze the flatness of the groove deposition surface.

[0035] (4) The plasma background light is processed to increase the signal-to-noise ratio of the actual reflected light intensity. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] The above and other objects, features and advantages of the present disclosure will become more apparent through a more detailed description of exemplary embodiments of the present disclosure in conjunction with the accompanying drawings, wherein like reference numerals generally represent like components throughout the exemplary embodiments of the present disclosure.

[0037] Figure 1 is a schematic diagram of the working principle of an exemplary cavity structure according to the present disclosure;

[0038] Figure 2 is a schematic diagram of an exemplary double-layer seven-core optical fiber;

[0039] Figure 3 is a schematic diagram of an exemplary cavity structure;

[0040] Figure 4 This is the reflection situation before the groove is filled;

[0041] Figure 5 This is the reflection during the trench filling process;

[0042] Figure 6 Fill the groove with late reflections;

[0043] Figure 7 The light intensity changes captured by the spectrometer during the trench filling process. DETAILED DESCRIPTION

[0044] The preferred embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although the preferred embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided to make the present disclosure more thorough and complete, and to fully convey the scope of the present disclosure to those skilled in the art.

[0045] The present disclosure proposes a cavity structure, which mainly includes: an external light source, a light-transmitting sheet, a sealing device, a double-layer multi-core optical fiber, a collimation device, and a spectral analysis device. By using this structure, reflected light can be used to observe the flatness of the groove deposition surface during the etching process, and the flatness of the upper surface of the deposited film layer can be reflected by real-time observation of the reflected light intensity on the upper surface of the deposited film layer.

[0046] This solution can capture dynamic changes in the process without interrupting the process flow, without the need to purchase additional SEM equipment, which can save costs compared to existing methods. The data analysis is also very simple, only real-time observation of the light intensity signal received by the spectrometer is required, and the flatness of the deposited film surface is analyzed by analyzing the reflected light intensity signal, which provides a very practical method for analyzing the flatness of the groove deposition surface.

[0047] In an exemplary embodiment, the specific structural diagram of the cavity is as shown in the attached Figure 3 As shown in the figure, it mainly includes: external light source, Y-shaped seven-core optical fiber, collimator, spectrometer, sapphire glass, and a pressing piece used as a sealing device. Figure 1 shown.

[0048] The specific structure is as follows: a light-transmitting hole is opened on the top of the reaction chamber, and a sapphire sheet is installed. The sapphire sheet is sealed on the upper cover plate by a sealing device. The external light source is connected to the middle core of the seven-core optical fiber, connected to the collimator and irradiated vertically to the surface of the wafer to be deposited. The reflected light is received by the six cores of the outer ring of the seven-core optical fiber, and the six cores of the outer ring are connected to the spectrometer to receive the light intensity signal. The flatness of the deposition result of the groove surface is analyzed by obtaining the light intensity signal received by the spectrometer.

[0049] Since there is plasma in the filling process in the cavity, that is, a certain intensity of background light, the light source preferably uses a light source with a higher light intensity, and the wavelength is as far away from the glow wavelength of plasma radiation as possible, which can improve the signal-to-noise ratio. In this embodiment, a halogen lamp or xenon lamp with a wide bandwidth is selected to avoid the wavelength of spontaneous radiation of the reaction plasma in the cavity, and the reflected light intensity of a specific wavelength is analyzed by a spectrometer, which can greatly improve the signal-to-noise ratio. For example, for a reactant with a wavelength of 777nm, the main observation wavelength is a wavelength of 230nm.

[0050] The light entering the cavity needs to be collimated by a collimator, and the angle between the light path and the wafer surface must be calibrated and adjusted to a vertical direction. At this time, the reflected light collection optical fiber can collect reflected light with greater intensity.

[0051] In this embodiment, as a preferred embodiment, the double-layer multi-core optical fiber uses a Y-type seven-core optical fiber, and the optical fiber cross section is as shown in the attached Figure 2 As shown in the figure, the seven-core optical fiber is divided into an inner ring and an outer ring. The inner ring is connected to the light source, and the outer ring is connected to the spectrometer with six cores. The seven-core solution is for the case where the diameters of the inner and outer ring optical fibers are the same. Of course, other numbers of optical fibers can also be used. The outer ring is equipped with more optical fibers to ensure that the outer ring can receive the light no matter where the incident light in the middle is deflected, to prevent the light from not being received when it is severely deflected.

[0052] During the trench filling process, the above device works as follows:

[0053] (1) Before the groove is filled, the upper surface of the wafer is grooved. The bottom of each groove and the middle platform between the two grooves are relatively flat. The middle area of ​​the optical fiber is connected to the light source and is the incident light area. Considering that the incident light has a certain diffusion angle, it is reflected by the groove plane and is captured more concentratedly by the edge area of ​​the optical fiber. At this time, the intensity of the reflected light obtained by the spectrometer is relatively high. Its working state is as follows: Figure 4 As shown;

[0054] (2) During the groove filling process, the filling material in the groove is relatively irregular, and the overall trend is that the edge is filled quickly and the middle is filled slowly. At this time, there is a large inclined surface on the upper surface of the filling material, which causes the angle between the incident light reaching the surface and the incident surface to be far from 90°. There is a large angle between the reflected light and the incident light. The outer ring fiber of the seven-core fiber captures less reflected light. At this time, the intensity of the reflected light obtained by the spectrometer is weak. Its working state is as follows: Figure 5 As shown;

[0055] In the later stage of groove filling, the groove is basically filled completely and presents a flat plane as a whole. At this time, the upper surface of the filler is relatively flat, and the angle between the incident light reaching the surface and the incident surface is close to 90°. The outer ring fiber of the seven-core fiber captures more reflected light. At this time, the intensity of the reflected light fed back by the spectrometer is strong. Its working state is as follows: Figure 6 As shown;

[0056] The light intensity captured by the spectrometer, such as Figure 7 As shown, the flatness of the wafer surface can be detected to reflect the real-time situation of the groove deposition flatness.

[0057] The present disclosure uses the reflection method to measure the surface flatness of the groove deposition in real time, uses the reflection principle to capture the reflected light, and analyzes the flatness of the surface to be measured by analyzing the captured light intensity. Similar to this is the interference method for measuring the surface profile, which analyzes the theoretical profile information of the object from the spectrum of the reflected light on the surface of the measured object, resolves the three-dimensional morphology of the object surface, and thus measures the surface flatness. In contrast, the present disclosure only focuses on the intensity of the reflected light, and does not need to analyze the results. The device is more economical and practical, responds more quickly, and the essential physical principles are also different.

[0058] The above technical scheme is only an exemplary embodiment of the present invention. For those skilled in the art, it is easy to make various types of improvements or modifications based on the application methods and principles disclosed in the present invention, and it is not limited to the method described in the above specific embodiment of the present invention. Therefore, the method described above is only preferred and does not have a restrictive meaning.

Claims

1. A chamber device for real-time monitoring of groove deposition surface flatness, based on a plasma reaction chamber, characterized in that: include: External light source, light-transmitting sheet, sealing equipment, double-layer multi-core optical fiber, collimation equipment, spectrum analysis equipment, including: The light-transmitting sheet is installed at the light-transmitting hole on the upper part of the reaction chamber and is sealed on the upper cover plate by a sealing device; The collimation device and the double-layer multi-core optical fiber are both arranged outside the reaction chamber, the output end of the collimation device is aligned with the light-transmitting sheet, and the input end is connected to the double-layer multi-core optical fiber; The double-layer multi-core optical fiber includes: two inner and outer ring optical fibers, wherein the outer ring optical fibers have multiple fibers and surround the inner ring optical fibers; wherein the inner ring optical fibers are used to inject light into the cavity, and the outer ring optical fibers are used to collect light reflected from the cavity; The external light source is connected to the inner ring optical fiber of the double-layer multi-core optical fiber, and is vertically irradiated to the surface of the wafer to be deposited through the collimating device and the light-transmitting sheet, and the reflected light is received by the outer ring optical fiber of the double-layer multi-core optical fiber; The outer ring optical fiber is connected to a spectrum analysis device for analyzing the intensity of the reflected light to determine the flatness of the deposition result on the groove surface.

2. The chamber device for real-time monitoring of groove deposition surface flatness according to claim 1, characterized in that: The external light source is a broadband light source, and the wavelength is far away from the glow wavelength of plasma radiation.

3. The chamber device for real-time monitoring of groove deposition surface flatness according to claim 2, characterized in that: The external light source is a halogen lamp or a xenon lamp.

4. The chamber device for real-time monitoring of groove deposition surface flatness according to claim 1 or 2, characterized in that: The double-layer multi-core optical fiber uses seven-core optical fibers with equal diameters in the inner and outer rings, with 1 in the inner ring and 6 in the outer ring.

5. The chamber device for real-time monitoring of groove deposition surface flatness according to claim 4, characterized in that: The light-transmitting sheet is a sapphire sheet.

6. A method for monitoring the flatness of a groove deposition surface of a chamber device according to any one of claims 1 to 5, comprising the following steps: The light entering the cavity is collimated by the collimation device, and the angle between the light path and the wafer surface is calibrated and adjusted to the vertical direction; The outer ring of optical fibers captures the reflected light; The spectrum analysis equipment connected to the outer ring optical fiber analyzes the intensity of the captured reflected light, and analyzes the flatness of the groove deposition on the wafer surface based on the intensity of the reflected light.

Citation Information

Patent Citations

  • Dual-wavelength coaxial optical fiber sensor for detecting surface defect of steel ball and method

    CN107014828A

  • Measuring device and method

    CN111430257A

  • Semiconductor manufacturing apparatus

    JP2002367966A