Drying equipment

By dividing the lithium battery electrode into a coating area, a thinning area, and a ceramic area, and using a combination of laser and infrared heaters for drying, the problem of inconsistent drying speeds of the inner and outer slurry layers in the infrared drying method is solved, thus improving drying quality and production efficiency.

CN118437603BActive Publication Date: 2026-11-17SHENZHEN HYMSON LASER INTELLIGENT EQUIP CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410570795.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-05-09
Publication Date
2026-11-17
Estimated Expiration
2044-05-09

AI Technical Summary

Technical Problem

Existing infrared drying methods result in inconsistent drying speeds of the inner and outer layers of the lithium battery electrode slurry, which can easily cause surface cracks or bubbles on the electrode, affecting product quality.

Method used

A combined laser and infrared heater drying device is used. The electrode is divided into a coating area, a thinning area and a ceramic area. Laser and infrared heaters are used to dry the area separately. The laser heats the inner layer of the coating area, and the infrared heaters heat the thinning area and the ceramic area. A light-shielding component prevents the laser from irradiating these areas.

Benefits of technology

This effectively avoids the problem of inconsistent drying speeds between the inner and outer layers of slurry, improves drying quality, prevents surface cracking and bubbles in the electrode, and increases production efficiency and energy utilization.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118437603B_ABST
    Figure CN118437603B_ABST
Patent Text Reader

Abstract

This invention discloses a drying device, relating to the field of battery processing technology. The drying device is used for drying battery electrodes, which have a coating area, a thinning area, and a ceramic area. The thinning area is located between the coating area and the ceramic area. The drying device includes a housing, a conveying mechanism, and a heating mechanism. The housing forms a drying chamber. The conveying mechanism transports the battery electrodes into the drying chamber. The heating mechanism includes: a laser heater, located in the housing and above the conveying mechanism, for emitting laser light towards the coating area; a light-shielding component, covering the thinning area and the ceramic area to block the laser light emitted by the laser heater from irradiating the thinning area and the ceramic area; and a first infrared heater, located on the side of the light-shielding component facing the thinning area and the ceramic area, for emitting infrared light towards the thinning area and the ceramic area. The technical solution provided by this invention solves the problem of surface cracking caused by inconsistent drying speeds of the inner and outer layers of slurry during existing battery electrode drying processes.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of battery processing technology, and in particular to a drying device. Background Technology

[0002] Lithium-ion batteries are a type of battery that uses lithium metal or lithium alloys as positive / negative electrode materials and a non-aqueous electrolyte solution. The positive electrode material is often manganese dioxide, and the negative electrode material is often metallic lithium or other alloys. During the production of lithium-ion battery electrodes, after coating, the electrodes typically need to be dried using electrode drying equipment. If the electrodes are not effectively dried during this process, residual moisture and solvents in the electrodes will not completely evaporate, potentially causing the coated material to crack and peel off, battery malfunctions, or even air bubbles.

[0003] Currently, a common drying method for lithium battery electrodes is infrared drying. This method involves placing the electrodes in a drying chamber and drying them with infrared heating. For example, infrared heating lamps or infrared heating plates can be used to generate heat, and then the electrodes are dried directly through thermal radiation.

[0004] Infrared drying is a simple and small-sized equipment with low manufacturing cost because it does not require a heating fan. However, some energy is lost in the form of light energy, resulting in insufficient energy utilization. In addition, when infrared heat is conducted to the battery electrode, the slurry in the inner and outer layers dries at different speeds. This can cause the slurry on the surface to dry first, while the slurry in the inner layer remains wet. Continuing to dry can easily cause the electrode surface to crack or produce bubbles, which seriously affects product quality. Summary of the Invention

[0005] The main objective of this invention is to propose a drying device that aims to solve the problem of surface cracking caused by inconsistent drying speeds of inner and outer slurry layers during the drying of existing battery electrodes.

[0006] To achieve the above objectives, the present invention provides a drying apparatus for drying battery electrode sheets, wherein the battery electrode sheet has a coating area, a thinning area, and a ceramic area, the thinning area being disposed between the coating area and the ceramic area, and the drying apparatus comprising:

[0007] The cabinet has an internal drying chamber.

[0008] A transmission mechanism is used to transport the battery electrode sheets into the drying chamber;

[0009] Heating mechanism, the heating mechanism comprising:

[0010] A laser heater is disposed in the housing and above the transmission mechanism, and is used to emit laser light into the coating area;

[0011] A light-shielding component is disposed above the thinned area and the ceramic area to block the laser emitted by the laser heater from irradiating the thinned area and the ceramic area; and

[0012] A first infrared heater is disposed on the side of the light-shielding assembly facing the thinned area and the ceramic area, and is used to emit infrared light to the thinned area and the ceramic area.

[0013] In one embodiment, the light-shielding assembly includes a light-shielding cover fixedly disposed on the housing and covering the thinned area and the ceramic area, wherein the first infrared heater is disposed on the side of the light-shielding cover facing the thinned area and the ceramic area.

[0014] In one embodiment, the light-shielding assembly further includes a first temperature detection element, which is fixedly disposed on the light-shielding cover and used to detect the temperature of the thinned area and the ceramic area in real time.

[0015] In one embodiment, the light shield is provided with an air extraction port, which is connected to an external pneumatic device and is used to extract the gas that evaporates inside the light shield.

[0016] In one embodiment, the drying equipment further includes a second temperature detection element, which is fixedly disposed in the housing and spaced apart from the laser heater, and is used to detect the temperature of the coating area in real time.

[0017] In one embodiment, the housing has an input end and an output end opposite to each other. The transmission mechanism conveys the battery electrode into the drying chamber through the input end and outputs it through the output end. The laser heater has a first end away from the transmission mechanism and a second end close to the transmission mechanism, and is inclined from the first end to the second end toward the input end.

[0018] In one embodiment, the drying equipment further includes a second infrared heater, which is disposed within the drying chamber and upstream of the heating mechanism, and is positioned above the transmission mechanism to pre-dry the battery electrode.

[0019] In one embodiment, the drying equipment further includes a third infrared heater, which is disposed within the drying chamber and downstream of the heating mechanism, and is positioned above the transmission mechanism to perform post-drying of the battery electrode sheets.

[0020] In one embodiment, the housing is provided with an air inlet and an air outlet, both of which are connected to the drying chamber. The drying equipment also includes a blowing device, which is located in the housing and is used to provide airflow from the air inlet to the air outlet into the drying chamber.

[0021] In one embodiment, the housing is provided with an explosion vent, which is located in the housing and communicates with the drying chamber.

[0022] In one embodiment, the drying equipment further includes a pressure detector, which is fixedly installed in the housing and used to detect the pressure inside the drying chamber in real time.

[0023] In one embodiment, the drying equipment further includes a gas concentration detector, which is fixedly installed in the housing and used to detect the gas concentration in the drying chamber in real time.

[0024] In the technical solution of this invention, the drying equipment is used to dry coated battery electrodes in sections. The battery electrodes are divided into a coating area, a thinning area, and a ceramic area, and then placed in a drying chamber within a housing for drying. During drying, the battery electrodes are conveyed and output into the drying chamber via a transmission mechanism, and a heating mechanism installed within the housing heats and dries each section of the battery electrodes separately. The coating area has a thicker slurry and a stronger ability to absorb laser light; therefore, laser drying is used to dry the coating area. The high-temperature laser emitted by the laser heater can directly penetrate the outer layer of the slurry in the coating area, allowing the inner layer of the slurry in the coating area to be dried first, preventing the binder and conductive agent in the slurry from rising to the surface and detaching from the battery electrode. Since the ceramic area has a weaker ability to absorb laser light and the thinning area is thinner, infrared drying is used to dry the thinning area and the ceramic area. A first infrared heater emits high-temperature infrared light towards the thinning area and the ceramic area, using thermal radiation to dry them. In addition, to prevent the laser emitted by the laser heater from irradiating the thinned area and the ceramic area, a light-shielding component is installed above the thinned area and the ceramic area to block the laser. This solution uses a combination of laser and infrared drying methods to dry the different areas with large thickness differences on the battery electrode sheet separately, avoiding the problem of inconsistent drying speeds of the slurry between the inner and outer layers, and effectively ensuring the drying quality of the battery electrode sheet. Attached Figure Description

[0025] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on the structures shown in these drawings without creative effort.

[0026] Figure 1 This is a schematic diagram of a structure of an embodiment of the drying equipment provided by the present invention;

[0027] Figure 2 This is a schematic diagram of the structure of a battery electrode sheet in one embodiment of the present invention;

[0028] Figure 3 A schematic diagram of the structure of the laser heater emitting laser light to the battery electrode in one embodiment of the drying equipment provided by the present invention;

[0029] Figure 4 This is a schematic diagram of the heating mechanism in another embodiment of the drying equipment provided by the present invention;

[0030] Figure 5 A schematic diagram of the structure of the light-shielding component in another embodiment of the drying equipment provided by the present invention;

[0031] Figure 6 A schematic diagram of another embodiment of the drying equipment provided by the present invention;

[0032] Figure 7 This is a schematic diagram of another embodiment of the drying equipment provided by the present invention.

[0033] Explanation of icon numbers:

[0034] 10. Battery electrode; 101. Coating area; 102. Thinning area; 103. Ceramic area;

[0035] 100. Drying equipment; 1. Housing; 11. Input end; 12. Output end; 13. Air inlet; 14. Air outlet; 15. Explosion vent; 2. Transmission mechanism; 3. Heating mechanism; 31. Laser heater; 311. First end; 312. Second end; 32. Light shielding assembly; 321. Light shield; 3211. Air extraction port; 322. First temperature detection element; 33. First infrared heater; 4. Second temperature detection element; 5. Second infrared heater; 6. Third infrared heater; 7. Blowing device; 8. Pressure detector; 9. Gas concentration detector.

[0036] The realization of the objective, functional features and advantages of the present invention will be further explained in conjunction with the embodiments and with reference to the accompanying drawings. Detailed Implementation

[0037] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.

[0038] It should be noted that if the embodiments of the present invention involve directional indications (such as up, down, left, right, front, back, etc.), the directional indications are only used to explain the relative positional relationship and movement of the components in a specific posture. If the specific posture changes, the directional indications will also change accordingly.

[0039] Furthermore, if the embodiments of this invention involve descriptions such as "first" or "second," these descriptions are for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined with "first" or "second" may explicitly or implicitly include at least one of those features. Additionally, the use of "and / or" or "and / or" throughout the text includes three parallel solutions. For example, "A and / or B" includes solution A, solution B, or a solution where both A and B are satisfied simultaneously. Furthermore, the technical solutions of the various embodiments can be combined with each other, but this must be based on the ability of those skilled in the art to implement them. When the combination of technical solutions is contradictory or impossible to implement, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection claimed by this invention.

[0040] Infrared drying is a simple and small-sized equipment with low manufacturing cost because it does not require a heating fan. However, some energy is lost in the form of light energy, resulting in insufficient energy utilization. In addition, when infrared heat is conducted to the battery electrode, the slurry in the inner and outer layers dries at different speeds. This can cause the slurry on the surface to dry first, while the slurry in the inner layer remains wet. Continuing to dry can easily cause the electrode surface to crack or produce bubbles, which seriously affects product quality.

[0041] This invention proposes a drying device.

[0042] Please see Figures 1 to 4 In one embodiment of the present invention, the drying apparatus 100 is used for drying battery electrode 10, the battery electrode 10 having a coating area 101, a thinning area 102, and a ceramic area 103, the thinning area 102 being disposed between the coating area 101 and the ceramic area 103; the drying apparatus 100 includes:

[0043] Box 1, with a drying chamber inside;

[0044] The transmission mechanism 2 is used to transport the battery electrode 10 into the drying chamber;

[0045] Heating mechanism 3, which includes:

[0046] A laser heater 31 is disposed in the housing 1 and located above the transmission mechanism 2, and is used to emit laser light into the coating area 101;

[0047] A light-shielding component 32 is disposed above the thinning area 102 and the ceramic area 103 to block the laser emitted by the laser heater 31 from irradiating the thinning area 102 and the ceramic area 103; and

[0048] The first infrared heater 33 is disposed on the side of the light-shielding assembly 32 facing the thinning region 102 and the ceramic region 103, and is used to emit infrared light to the thinning region 102 and the ceramic region 103.

[0049] In the technical solution of this invention, the drying equipment 100 is used to perform zoned drying of the coated battery electrode 10. The battery electrode 10 is divided into a coating area 101, a thinning area 102, and a ceramic area 103, and then placed in a drying chamber within a housing 1 for drying. During drying, the battery electrode 10 is conveyed and output into the drying chamber via a transfer mechanism 2, and the heating mechanism 3 installed within the housing 1 heats and dries each zone of the battery electrode 10 separately. The slurry in coating area 101 is relatively thick and has a strong ability to absorb laser light. Therefore, laser drying is used to dry coating area 101. The high-temperature laser emitted by laser heater 31 can directly penetrate the outer layer of slurry in coating area 101, allowing the inner layer of slurry in coating area 101 to be dried first, preventing the binder and conductive agent in the slurry from floating to the surface of the battery electrode 10 due to heat. Since ceramic area 103 has a weak ability to absorb laser light and thinning area 102 is relatively thin, infrared drying is used to dry thinning area 102 and ceramic area 103. The first infrared heater 33 emits high-temperature infrared light towards thinning area 102 and ceramic area 103, using thermal radiation to dry them. In addition, to prevent the laser emitted by laser heater 31 from irradiating thinning area 102 and ceramic area 103, a light-shielding component 32 is provided above thinning area 102 and ceramic area 103 to block the laser. This solution uses a combination of laser and infrared drying methods to dry the battery electrode 10 separately for areas with significant thickness differences, thus avoiding the problem of inconsistent drying speeds of the slurry between the inner and outer layers and effectively ensuring the drying quality of the battery electrode 10.

[0050] Specifically, this solution employs a combined laser and infrared drying method. Due to the faster drying speed of laser drying, it reduces energy loss compared to traditional hot air drying alone. It also avoids the problem of the outer slurry drying before the inner slurry dries, as is common in infrared drying alone. The NMP (N-methylpyrrolidone) solvent in the inner slurry evaporates as a gas through the outer layer, effectively preventing surface cracking of the battery electrode 10. Furthermore, it avoids the problems of poor energy control in the thinning zone 102 and inconsistent laser absorption between the ceramic zone 103 and the coating zone 101 during laser drying alone, preventing excessive temperature and boiling in the thinning zone 102, thus effectively ensuring drying quality. In addition, laser drying, with its high energy density and high speed, significantly increases the drying speed, thereby improving the production efficiency of the battery electrode 10.

[0051] In one embodiment of the present invention, please refer to Figure 4 and Figure 5 The light-shielding component 32 includes a light-shielding cover 321, which is fixedly mounted on the housing 1 and covers the thinning area 102 and the ceramic area 103. This light-shielding cover 321 separates the ceramic area 103 and the thinning area 102 from the coating area 101, preventing the laser from affecting the drying of the ceramic area 103 and the thinning area 102. A first infrared heater 33 is located on the side of the light-shielding cover 321 facing the thinning area 102 and the ceramic area 103, allowing the ceramic area 103 and the thinning area 102 to be heated individually by the first infrared heater 33 built into the light-shielding cover 321. It should be noted that the first infrared heater 33 can be an infrared heating lamp or an infrared heating plate, as long as it can emit high-temperature infrared light.

[0052] In one embodiment of the present invention, please refer to Figure 5 The light-shielding assembly 32 also includes a first temperature detection element 322, which is fixedly mounted on the light-shielding cover 321 and used to detect the temperature of the thinned area 102 and the ceramic area 103 in real time. This prevents the infrared radiation temperature generated by the first infrared heater 33 from being too high, thus preventing edge cracking and embrittlement of the battery electrode 10. Optionally, the first temperature detection element 322 is a temperature detection probe, and multiple temperature detection probes are evenly spaced inside the light-shielding cover 321 to ensure the accuracy of temperature measurement. It should be noted that the first temperature detection element 322 can communicate with the PLC system and feed back the detected temperature data to the PLC system in a timely manner. This allows the PLC system to modify the output power of the first infrared heater 33 based on the feedback data, thereby controlling the heating temperature of the thinned area 102 and the ceramic area 103.

[0053] In one embodiment of the present invention, please refer to Figure 5During the heating process of the thinning zone 102 and the ceramic zone 103, the NMP solvent in the slurry will evaporate and diffuse inside the light shield 321 to form mist. The diffused mist will affect the infrared light irradiation of the first infrared heater 33 to the thinning zone 102 and the ceramic zone 103. In this embodiment, the light shield 321 is provided with an exhaust port 3211 and the exhaust port 3211 is connected to an external pneumatic device to promptly extract the NMP mist that evaporates inside the light shield 321 to the outside.

[0054] In one embodiment of the present invention, please refer to Figure 1 The drying equipment 100 also includes a second temperature detection element 4, which is fixedly installed in the housing 1 and spaced apart from the laser heater 31. It is used to monitor the temperature of the coating area 101 in real time, preventing excessively high laser temperatures from the laser heater 31 and avoiding the problem of excessively fast drying speed in the coating area 101, which could create a drying seam between the coating area 101 and the ceramic area 103, affecting aesthetics. Optionally, the second temperature detection element 4 is an infrared thermometer, and the infrared light emitted by the infrared thermometer can cover the entire coating area 101, thus ensuring accurate temperature measurement. It should be noted that the second temperature detection element 4 can also communicate with a PLC system and promptly feed back the detected temperature data to the PLC system. This allows the PLC system to modify the output power of the laser heater 31 based on the feedback data, thereby controlling the heating temperature of the coating area 101.

[0055] In one embodiment of the present invention, please refer to Figure 6 The housing 1 is provided with an input end 11 and an output end 12. The transmission mechanism 2 conveys the battery electrode 10 into the drying chamber through the input end 11 and outputs it through the output end 12. Considering that the battery electrode 10 has different drying requirements, the laser heater 31 can be tilted. For example, the laser heater 31 can be divided into a first end 311 away from the transmission mechanism 2 and a second end 312 close to the transmission mechanism 2. Optionally, the laser heater 31 is tilted from the first end 311 to the second end 312 towards the input end 11, so that the energy density of the laser irradiation on each part of the coating area 101 is different, so as to achieve step heating or cooling.

[0056] In one embodiment of the present invention, please refer to Figure 6 and Figure 7The drying equipment 100 also includes a second infrared heater 5, which is located in the drying chamber and upstream of the heating mechanism 3. The second infrared heater 5 is also located above the transmission mechanism 2 to pre-dry the battery electrode 10. Thus, in this embodiment, the drying of the battery electrode 10 can be divided into two stages: the first is the preheating stage, which is carried out by the second infrared heater 5. In this stage, the entire battery electrode 10 is rapidly heated to a certain temperature (this temperature is lower than the floating temperature of the binder and conductive agent inside the slurry). In this stage, a small amount of NMP solvent and a small amount of water evaporate. The second is the constant temperature drying stage, which is carried out by the heating mechanism 3. In this stage, the slurry solvent in the inner layer of the coating area 101 migrates to the surface due to capillary action and continuously evaporates until it is completely vaporized. The coating area 101 gradually shrinks to complete the drying process.

[0057] In one embodiment of the present invention, please refer to Figure 1 and Figure 7 The drying equipment 100 also includes a third infrared heater 6, which is located in the drying chamber and downstream of the heating mechanism 3, and is positioned above the transmission mechanism 2 to perform post-drying of the battery electrode 10. In this embodiment, after the battery electrode 10 is dried at a constant temperature by the heating mechanism 3, in order to prevent the slurry inside the thicker coating area 101 from containing residual moisture or solvents such as NMP, a post-drying stage can be added to further dry the battery electrode 10, thereby ensuring the drying effect of the battery electrode 10 and preventing the battery performance from being affected due to incomplete drying.

[0058] In one embodiment of the present invention, please refer to Figure 1 The housing 1 is equipped with an air inlet 13 and an air outlet 14, both of which are connected to the drying chamber. The drying equipment 100 also includes a blowing device 7, which is located in the housing 1 and is used to provide airflow from the air inlet 13 to the air outlet 14 into the drying chamber. Thus, during the drying process in the coating area 101, the airflow generated by the blowing device 7 and the air inlet 13 can promptly blow away the NMP solvent volatilized on the battery electrode 10, and extract it through the air outlet 14 to the outside of the housing 1 for centralized treatment. It should be noted that the blowing device 7 can be an air knife, which mainly consists of air knife blades and nozzles. The air knife blades serve as air guides, and different numbers of blades and their tilt angles can be changed according to different needs to achieve different drying effects. The nozzles change the airflow direction to a certain extent, and their opening angle can be adjusted.

[0059] In one embodiment of the present invention, please refer to Figure 1During the drying process of the battery electrode 10, a large amount of NMP solvent in the slurry will evaporate and generate a large amount of mist, which will permeate the inside of the drying chamber. Since the drying chamber is irradiated by the high temperature laser emitted by the laser heater 31, the NMP concentration in the drying chamber is too high and will cause a deflagration phenomenon. In order to remove the evaporated NMP gas in time, in this embodiment, a deflagration port 15 is also provided on the housing 1. The deflagration port 15 is opened in the housing 1 and communicates with the drying chamber. When a deflagration occurs in the drying chamber, the deflagration port 15 can be used to prevent damage to the operator in the event of an explosion.

[0060] In one embodiment of the present invention, please refer to Figure 1 During the drying process of the battery electrode 10, due to the large amount of evaporation of water and solvent in the slurry, the pressure inside the drying chamber will change significantly. In order to monitor the pressure difference between the inside and outside of the chamber 1, the drying equipment 100 also includes a pressure detector 8. The pressure detector 8 is fixedly installed in the chamber 1 and is used to detect the pressure inside the drying chamber in real time to ensure the safety of the drying process.

[0061] In one embodiment of the present invention, please refer to Figure 1 To prevent deflagration in the drying chamber, the drying equipment 100 also includes a gas concentration detector 9, which is fixedly installed in the housing 1 and used to detect the gas concentration in the drying chamber in real time. It can detect changes in the concentration of flammable gases such as NMP in a timely manner, prevent the concentration from being too high and causing deflagration, and improve the safety of battery production.

[0062] The above description is merely an exemplary embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural transformations made using the contents of the present invention specification and drawings under the technical concept of the present invention, or direct / indirect applications in other related technical fields, are included within the patent protection scope of the present invention.

Claims

1. A drying apparatus for drying a battery electrode sheet having a coated region, a thinned region, and a ceramic region, the thinned region being provided between the coated region and the ceramic region, characterized by, The drying equipment includes: The cabinet has an internal drying chamber. A transmission mechanism is used to transport the battery electrode sheet into the drying chamber. The housing is provided with opposite input and output ends. The transmission mechanism transports the battery electrode sheet into the drying chamber through the input end and outputs it through the output end. Heating mechanism, the heating mechanism comprising: A laser heater is disposed in the housing and above the transmission mechanism, and is used to emit laser light into the coating area. The laser heater has a first end away from the transmission mechanism and a second end close to the transmission mechanism, and is inclined from the first end to the second end toward the input end. A light-shielding component is disposed above the thinned area and the ceramic area to block the laser emitted by the laser heater from irradiating the thinned area and the ceramic area; and A first infrared heater is disposed on the side of the light-shielding assembly facing the thinned area and the ceramic area, and is used to emit infrared light to the thinned area and the ceramic area.

2. The drying equipment as described in claim 1, characterized in that, The light-shielding assembly includes a light-shielding cover, which is fixedly disposed on the housing and covers the thinned area and the ceramic area. The first infrared heater is disposed on the side of the light-shielding cover facing the thinned area and the ceramic area.

3. The drying equipment as described in claim 2, characterized in that, The light-shielding assembly further includes a first temperature detection element, which is fixedly disposed on the light-shielding cover and used to detect the temperature of the thinned area and the ceramic area in real time; and / or, The light shield is equipped with an air extraction port, which is connected to an external pneumatic device and used to extract the gas that evaporates inside the light shield.

4. The drying equipment as described in claim 1, characterized in that, The drying equipment also includes a second temperature detection element, which is fixedly installed in the housing and spaced apart from the laser heater, and is used to detect the temperature of the coating area in real time.

5. The drying equipment as described in claim 1, characterized in that, The drying equipment further includes a second infrared heater, which is disposed in the drying chamber and upstream of the heating mechanism, and is positioned above the transmission mechanism to pre-dry the battery electrode.

6. The drying equipment as described in claim 5, characterized in that, The drying equipment further includes a third infrared heater, which is disposed in the drying chamber and downstream of the heating mechanism, and is disposed above the transmission mechanism to perform post-drying of the battery electrode sheets.

7. The drying apparatus according to any one of claims 1 to 6, characterized in that, The housing is provided with an air inlet and an air outlet, both of which are connected to the drying chamber. The drying equipment also includes a blowing device, which is located in the housing and is used to provide airflow from the air inlet to the air outlet into the drying chamber.

8. The drying equipment as described in claim 7, characterized in that, The chamber is provided with an explosion vent, which is located in the chamber and communicates with the drying chamber.

9. The drying apparatus according to any one of claims 1 to 6, characterized in that, The drying equipment also includes a pressure detector, which is fixedly installed in the housing and used to monitor the pressure inside the drying chamber in real time; and / or, The drying equipment also includes a gas concentration detector, which is fixedly installed in the chamber and used to detect the gas concentration in the drying chamber in real time.

Citation Information

Patent Citations

  • Method for drying electrode

    CN106784601A

  • Drying device and coating drying method

    CN115780209A

  • Air control device of coating machine oven

    CN212702838U

  • Rolling mechanism

    CN218015203U