A nano powder morphology and particle size optimization device and method
By using a combination technology of the evaporation chamber, cooling air conveying channel and countercurrent blowing air supply channel during the preparation of nano powder, the problems of particle size and sphericality of nano powder are solved, and the particle size is below 50nm and sphericality is achieved. High nanometal powder preparation meets the needs of 3D printing technology.
Patent Information
- Application Number
- CN202411012693.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-07-26
AI Technical Summary
The existing nano powder preparation methods are difficult to control the particle size below 50nm, and the spherical requirements are high, which cannot meet the needs of 3D printing technology.
An optimized equipment for nano powder form and particle size is designed, using the combination of the evaporation chamber, the cooling air conveying channel and the countercurrent blowing air channel, by adjusting the position of the cooling air conveying channel and the setting of the countercurrent blowing air channel. Control the formation and diffusion of nanometal powders to ensure that the particle size is below 50 nm and the spherical degree is high.
The particle size of nanometal powder is controlled below 50nm, with a high spherical shape, reducing the formation of special-shaped bodies, improving the quality of nano powder, and meeting the requirements of 3D printing technology.
Smart Images

Figure CN118543827B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of metal powder manufacturing, and more specifically, to a device and method for optimizing the morphology and particle size of nano powder. Background Art
[0002] Nanopowder refers to ultrafine particles with a size of 1nm to 100nm, which is between single atoms, molecules and macroscopic objects, and is a typical mesoscopic system. Because nanopowder has unique mechanical, magnetic, electrical, thermal and optical properties, it has shown great potential for application in many fields such as national defense science and technology, biomedicine, electronics industry, and new energy. For example, nanopowder can be used as a raw material for 3D printing technology and is suitable for the development of complex structure metal products.
[0003] The current mainstream preparation method for nanopowders is the arc method, which heats the metal raw material through the high-energy plasma generated by the arc, causing the metal raw material to evaporate and condense in the cooling gas to form nanometal particles. For example, patent number CN116765410A is a nanopowder production method. Although this method has produced nanopowders with an average particle size of 65 to 90 nm, 3D printing technology requires the particle size of nanopowders to be less than 50 nm and has high requirements for sphericity. Therefore, the production process of nanopowders still needs to be optimized. Summary of the invention
[0004] In order to optimize the morphology of nanopowders and control the particle size of nanopowders to be below 50 nm, the present application provides a device and method for optimizing the morphology and particle size of nanopowders.
[0005] In the first aspect, the present application provides an optimization device for the morphology and particle size of nanopowders, which adopts the following technical solution:
[0006] A device for optimizing the morphology and particle size of nanopowders, comprising an evaporation chamber, wherein a cooling air delivery channel and a first countercurrent blowing air channel are provided in the evaporation chamber; the position of the air outlet of the cooling air delivery channel in the evaporation chamber is adjustable; the first countercurrent blowing air channel is arranged opposite to the cooling air delivery channel, and the axis of the first countercurrent blowing air channel is located below the axis of the cooling air delivery channel, and the first countercurrent blowing air channel and the air suction port in the evaporation chamber are located on the same side.
[0007] By adopting the above technical solution, since the cooling air volume is relatively fixed, the longer the blowing distance of the cooling air, the gradually attenuated cooling effect of the cooling air. Therefore, the cooling air delivery channel of the present application can slide in the evaporation chamber to control the distance between the cooling air delivery channel and the molten pool, thereby ensuring that the cooling air can be delivered to the metal evaporation area in the evaporation chamber; in the metal evaporation area, the atomic metal vapor and the cooling air collide and cool down quickly, forming a large supersaturation, and quickly homogeneously nucleate to form "nano-atomic clusters". The "nano-atomic clusters" have a fast condensation speed, which inhibits excessive collision of the initial nano-metal powder, and the nano-metal powder is more likely to form granules with high sphericity, and the initial particle size of the nano-metal powder is small;
[0008] The initial nano-metal powder is carried by the cooling wind to the second half of the evaporation chamber. The nano-metal powder flows toward the cold wall under the action of the thermophoretic force. If the nano-metal powder contacts the cold wall, it is easy to deposit and collide with the new powder that is constantly flowing to grow into a large-size irregular body. Therefore, under the action of the first countercurrent blowing air, the nano-metal powder is lifted by the first countercurrent blowing air before approaching the cold wall and mixed into the cooling air; under the suction action of the air intake port, the first countercurrent blowing air and the cooling air are mixed, and the volume of the second half of the evaporation chamber is used to reduce the concentration of the nano-metal powder, reduce the possibility of nano-metal powder accumulation to form low-density agglomerates, and inhibit the further growth of the nano-metal powder and the formation of irregular bodies. At the same time, the possibility of nano-metal powder deposition on the low-temperature wall of the evaporation chamber is reduced. Finally, nano-metal powders with high sphericity and a particle size of less than 50nm can be obtained.
[0009] Furthermore, a second countercurrent blowing air channel is provided in the evaporation chamber, the second countercurrent blowing air channel is located on the same side of the first countercurrent blowing air channel, and the axis of the second countercurrent blowing air channel is located above the evaporation chamber.
[0010] Furthermore, the second countercurrent blowing air channel is inclined, and the inclination angle tanθ=L / D, where L is the length of the evaporation chamber and D is the diameter of the evaporation chamber.
[0011] By adopting the above technical solution, since the cooling air is lifted by the first countercurrent air flow, the air flow containing the nano-metal powder is easy to rise, so the second countercurrent blowing air channel can prevent the rising nano-metal powder from condensing on the upper inner wall of the evaporation chamber, thereby reducing the possibility of the nano-metal powder generating irregular particles;
[0012] Secondly, the second countercurrent blowing air channel can be mixed with the cooling air and the first countercurrent blowing air under the suction effect of the suction port, further reducing the concentration of the nano-metal powder. The volume utilization rate of the second half of the evaporation chamber is high, the nano-metal powder can be fully diffused, and the growth of the nano-metal powder is delayed.
[0013] Furthermore, the first countercurrent blowing air channel and the second countercurrent blowing air channel are both arc-shaped openings.
[0014] By adopting the above technical solution, the arc-shaped opening fits the shape of the inner wall of the evaporation chamber more closely, and the arc-shaped opening can ensure that the first countercurrent blowing air and the second countercurrent blowing air can achieve a greater coverage of the inner wall of the evaporation chamber with a smaller air volume, thereby reducing the possibility of nano-metal powders adhering to the low-temperature wall surface.
[0015] Furthermore, the curvature of the first countercurrent blowing air channel and the second countercurrent blowing air channel are both 60° to 90°.
[0016] By adopting the above technical solution, within this arc range, the first countercurrent blowing air and the second countercurrent blowing air can basically cover the inner wall surface of the evaporation chamber.
[0017] Furthermore, a plurality of the first countercurrent blowing air channels and a plurality of the second countercurrent blowing air channels are provided, and each of the first countercurrent blowing air channels and each of the second countercurrent blowing air channels are distributed in equal arcs.
[0018] By adopting the above technical scheme, since there are certain requirements for the wind speed of the countercurrent blowing air, when the arc length of the countercurrent blowing air channel is longer, in order to control the air supply area of the countercurrent blowing air channel, the arc height will be reduced, thereby increasing the difficulty of processing the countercurrent blowing air channel; therefore, while ensuring that the air supply area of the countercurrent blowing air channel is constant, the countercurrent blowing air channel is divided into sections, and multiple sections of countercurrent blowing air are connected to ensure uniform coverage of the inner wall of the evaporation chamber.
[0019] Furthermore, the wind speed at the outlet of the first countercurrent blowing air channel is the same as the wind speed at the outlet of the cooling air delivery channel.
[0020] Furthermore, the air inlet is located at 1 / 2 to 1 / 4 of the height of the evaporation chamber.
[0021] By adopting the above technical solution, the mixed air containing nano-metal powder can be better sucked into the subsequent powder collection and classification device within this height range; at the same time, the nano-metal powder entrained by the cooling air can be evenly distributed in the second half of the evaporation chamber under the suction force of the extraction port.
[0022] In a second aspect, the present application provides a method for optimizing the morphology and particle size of nanopowders, using the following technical solution:
[0023] A method for optimizing the morphology and particle size of nanopowders is implemented in the aforementioned equipment for optimizing the morphology and particle size of nanopowders, comprising the following steps:
[0024] Opening the air inlet of the cooling air delivery channel and adjusting the length of the cooling air delivery channel extending into the evaporation chamber;
[0025] Starting the first countercurrent blowing air channel;
[0026] Collecting nano-metal powders.
[0027] By adopting the above technical solution, the method has simple implementation steps and is easy to produce. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 This is a schematic diagram of the cross-sectional structure of an optimization device for the morphology and particle size of nanopowders disclosed in Example 1.
[0029] Figure 2 for Figure 1 View from the center AA direction.
[0030] Figure 3 This is a scanning electron microscope photograph of the nano-metal powder produced in Example 1.
[0031] Markings in the accompanying drawings:
[0032] 1. Evaporation chamber; 2. Cooling air delivery channel; 3. First countercurrent blowing air channel; 4. Second countercurrent blowing air channel; 5. Air suction port; 6. Arc generator; 7. Crucible. DETAILED DESCRIPTION
[0033] Example 1
[0034] Figure 1 This is a schematic cross-sectional structure diagram of an optimization device for the morphology and particle size of a nanopowder disclosed in Example 1. Figure 1 , an optimization device for the morphology and particle size of nano powders, comprising an evaporation chamber 1, a crucible 7 is arranged in the evaporation chamber 1, the crucible 7 is used as a molten pool, and a metal raw material is placed inside. An arc generator 6 is installed on the crucible 7, and the tip of the arc generator 6 discharges, and the metal raw material evaporates to form atomic metal vapor.
[0035] See also Figure 1A cooling air delivery channel 2 is provided on one side of the evaporation chamber 1. The distance of the air outlet of the cooling air delivery channel 2 in the evaporation chamber 1 can be adjusted in various ways. For example, one end of the cooling air delivery channel 2 located in the evaporation chamber 1 is a telescopic end, and the distance between the air outlet and the crucible 7 can be adjusted by telescopic means; or, a slide rail is installed at the bottom of the cooling air delivery channel 2, so that the cooling air delivery channel 2 slides and adjusts the distance it extends into the evaporation chamber 1. The cooling air volume is negatively correlated with the extension length of the cooling air delivery channel 2 in the evaporation chamber 1, that is, the smaller the cooling air volume, the longer the extension length of the cooling air channel in the evaporation chamber 1, so as to ensure that the cooling air can cover the high-temperature evaporation area.
[0036] The metal vapor contacts the cooling air, collides rapidly and cools down, forming a large supersaturation, and the atomic metal rapidly homogeneously nucleates to form "nano-atomic clusters". The "nano-atomic clusters" grow up to form nano-metal powders through condensation or collision in the later stage. Since the metal vapor condenses rapidly in the initial state, the excessive collision of the initial nano-metal powders is suppressed, forming nano-metal powders with small initial particle size and high sphericity. The initial nano-metal powders are entrained by the cooling air and transported to the second half of the evaporation chamber 1. At the same time, the air volume of the cooling air delivery channel 2 has little effect on the arc area and the arc input power distribution, which is almost negligible.
[0037] Figure 2 for Figure 1 View from the center AA direction. Figure 1 and Figure 2 , the other side of the evaporation chamber 1 is provided with a first countercurrent blowing air channel 3, an air suction port 5 and a second countercurrent blowing air channel 4 in sequence from low to high. The first countercurrent blowing air channel 3 is arranged opposite to the cooling air delivery channel 2, and the axis of the first countercurrent blowing air channel 3 is lower than the axis of the cooling air delivery channel 2. The air volume at the outlet of the first countercurrent blowing air channel 3 is positively correlated with the air volume of the cooling air, the wind speed at the outlet of the first countercurrent blowing air is the same as the wind speed at the outlet of the cooling air delivery channel 2, and the wind speed of the first countercurrent blowing air is controlled at 2 to 5 m / s to ensure that the first countercurrent blowing air can be blown to the vicinity of the metal evaporation zone. The first countercurrent blowing air can carry the cooling air upward, and the first countercurrent blowing air is mixed with the cooling air, which can reduce the concentration of nano-metal powders in the mixed air body and reduce the collision probability of nano-metal powders in the later growth process. At the same time, the first countercurrent blowing air is also cold air, which can inhibit the growth of nano-metal powders.
[0038] See also Figure 2, the opening of the first countercurrent blowing air channel 3 is arc-shaped. According to the proportion of input molten pool energy, the air volume of the first countercurrent blowing air is 30% to 100% of the cooling air volume. The outlet area of the first countercurrent blowing air channel 3 is constant. In order to reduce the processing difficulty of the first countercurrent blowing air channel 3, the first countercurrent blowing air channel 3 is provided with a plurality of first countercurrent blowing air channels 3, and the plurality of first countercurrent blowing air channels 3 form an arc with an arc of 60° to 90°, and the plurality of first countercurrent blowing air channels 3 are evenly distributed in arcs; the degree of the arc is the angle between the central axes of the two first countercurrent blowing air channels 3 that are farthest apart.
[0039] Based on this setting, it can be ensured that the height of each first countercurrent blowing air channel 3 is above 1 mm. In the present embodiment, three first countercurrent blowing air channels 3 are provided, and the angle between the central axes of two adjacent first countercurrent blowing air channels 3 is 45°. The three first countercurrent blowing air channels 3 form an arc of 90°.
[0040] See also Figure 1 and Figure 2 , the first countercurrent blowing air channel 3 is close to the bottom of the evaporation chamber 1, and the wind formed by the first countercurrent blowing air channel 3 is connected to each other, covering the inner wall of the bottom of the evaporation chamber 1. When the nano-metal powder moves toward the cold wall surface of the evaporation chamber 1 under the action of thermophoretic force, the first countercurrent blowing wind lifts the nano-metal powder upward to reduce the possibility of the nano-metal powder contacting the cold wall surface and causing deposition. At the same time, the temperature at the air inlet 5 is reduced to below 600K, reducing the probability of collision between nano-metal powders due to Brownian motion.
[0041] See also Figure 1 and Figure 2 The air inlet 5 is located at 1 / 2 to 1 / 4 of the height of the evaporation chamber 1. The air inlet 5 is connected to an external suction device (not shown in the figure). Under the suction effect of the suction device, the mixed wind containing the initial nano-metal powder can be fully diffused into the rear half of the evaporation chamber 1 and quickly discharged from the air inlet 5. The cooling air delivery channel 2, the first countercurrent blowing air channel 3 and the second countercurrent blowing air channel 4 are all air supply ports. The area of the air inlet 5 is larger than the sum of the areas of the air supply ports, so that the nano-metal powder is quickly cooled and discharged from the evaporation chamber 1 to reduce the possibility of collision and growth of the nano-metal powder during the subsequent condensation process. The final particle size of the nano-metal powder is small and the sphericity is high.
[0042] See also Figure 1 and Figure 2The second countercurrent blowing air channel 4 is tilted, and the tilt angle tanθ=L / D, where L is the length of the evaporation chamber 1 and D is the diameter of the evaporation chamber 1. The jet at the outlet of the second countercurrent blowing air channel 4 reaches the vicinity of the center of the evaporation chamber 1, or the jet reaches the half height of the arc generator 6. The tilted setting can not only make the second countercurrent blowing air cover the inner wall at the top of the evaporation chamber 1, but also prevent part of the nano-metal powder in the mixed air body from rising and adhering to the top wall of the evaporation chamber 1, further improving the sphericity of the nano-metal powder.
[0043] Secondly, since the second countercurrent blowing air can be mixed with the cooling air under the suction effect of the air suction port 5, the concentration of the nano-metal powder in the mixed air is further reduced, and the latter half volume of the evaporation chamber 1 is fully utilized.
[0044] The specific working method of this embodiment is as follows:
[0045] Place an appropriate amount of raw metal ingots into the crucible 7 and adjust the arc generator 6 to a set height;
[0046] Start the vacuum pump group and reduce the pressure of evaporation chamber 1 to 10 -4 Pa(A), and then sufficient argon gas is injected to restore the pressure to 0.06MPa(A), and this is repeated three times to ensure that the evaporation chamber 1 is in a reliable inert atmosphere;
[0047] Start the process air circulation system, and open the cooling air delivery channel 2 and the first countercurrent blowing air channel 3 by 20%;
[0048] Start the power supply of the arc generator 6, establish an arc between the arc generator 6 and the raw metal ingot, gradually increase the single-circuit arc current to 200A, and move the arc generator 6 to maintain the position near the set voltage;
[0049] According to the input power, the air volume and moving distance of the cooling air delivery channel 2 are adjusted, and the air volume of the first countercurrent blowing air channel 3 is adjusted according to the temperature at the air suction port 5. The nano-metal particles generated by the high-temperature evaporation of the arc encounter the cooling delivery air and quickly form "nano-atomic clusters". When the cooling delivery air migrates to the air suction port 5, it meets and mixes with the first countercurrent blowing air and the second countercurrent blowing air. The nano-metal powder diffuses to the latter half of the evaporation chamber 1, and the concentration of the nano-metal powder is further reduced. It is discharged under the suction effect of the air suction port 5 and enters the cooling collection system.
[0050] Among them, the opening radius of the cooling air delivery channel 2 is 12mm, and the flow rate is 350SLPM; the opening heights of the first countercurrent blowing air and the second countercurrent blowing air are both 2mm, and the flow rate is set to 150SLPM, so that the average temperature at the suction port 5 is maintained below 600K.
[0051] Figure 3 This is a scanning electron microscope photo of the nano-metal powder produced in Example 1. Figure 3 It can be seen from the figure that the particle size of the nano-metal powder is controlled below 50nm, and it can be seen from the figure that most of the nano-metal powders are spherical particles, and the particles are relatively uniform, and the sphericity of the nano-metal powders is high.
[0052] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0053] Moreover, the above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the invention patent. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be based on the attached claims.
Claims
1. A device for optimizing the morphology and particle size of nanopowders, comprising an evaporation chamber (1), characterized in that: The evaporation chamber (1) is provided with a cooling air delivery channel (2) and a first countercurrent blowing air channel (3); the position of the air outlet of the cooling air delivery channel (2) in the evaporation chamber (1) is adjustable; the first countercurrent blowing air channel (3) is arranged opposite to the cooling air delivery channel (2), and the axis of the first countercurrent blowing air channel (3) is located below the axis of the cooling air delivery channel (2), and the first countercurrent blowing air channel (3) and the air intake port (5) in the evaporation chamber (1) are located on the same side; the evaporation chamber (1) is also provided with a second countercurrent blowing air channel (4), the second countercurrent blowing air channel (4) is located on the same side of the first countercurrent blowing air channel (3), and the axis of the second countercurrent blowing air channel (4) is located above the evaporation chamber (1).
2. The device for optimizing the morphology and particle size of nanopowders according to claim 1, characterized in that: The second countercurrent blowing air channel (4) is arranged to be inclined, and the inclination angle tanθ=L / D, where L is the length of the evaporation chamber (1) and D is the diameter of the evaporation chamber (1).
3. The device for optimizing the morphology and particle size of nanopowders according to claim 1, characterized in that: The first countercurrent blowing air channel (3) and the second countercurrent blowing air channel (4) are both arc-shaped openings.
4. The device for optimizing the morphology and particle size of nanopowders according to claim 3, characterized in that: The curvature of the first countercurrent blowing air channel (3) and the curvature of the second countercurrent blowing air channel (4) are both 60° to 90°.
5. The device for optimizing the morphology and particle size of nanopowders according to claim 3, characterized in that: A plurality of the first countercurrent blowing air channels (3) and the second countercurrent blowing air channels (4) are provided, and each of the first countercurrent blowing air channels (3) and each of the second countercurrent blowing air channels (4) are distributed in equal arcs.
6. The device for optimizing the morphology and particle size of nanopowders according to claim 5, characterized in that: The wind speed at the outlet of the first countercurrent blowing air channel (3) is the same as the wind speed at the outlet of the cooling air delivery channel (2).
7. The device for optimizing the morphology and particle size of nanopowders according to claim 6, characterized in that: The air inlet (5) is located at 1 / 2 to 1 / 4 of the height of the evaporation chamber (1).
8. A method for optimizing the morphology and particle size of nanopowders, characterized in that: The method is implemented in the nano powder morphology and particle size optimization equipment according to any one of claims 1 to 7, comprising the following steps: Opening the air inlet of the cooling air delivery channel (2), and adjusting the length of the cooling air delivery channel (2) extending into the evaporation chamber (1); Starting the first countercurrent blowing air channel (3); Collecting nano-metal powders.
Citation Information
Patent Citations
Nanopowder production method
CN116765410A
Ultra-fine powder particle gathering and cooling tank type structure and ultra-fine powder particle forming method
CN112915919A
A equipment of plasma arc for NANO powder materials
KR1020050104256A
Arc apparatus for producing ultrafine particles
US4732369A
Method of making nanostructured materials
US5460701A