A method and system for identifying defects of double sealing rings of top cover

By measuring the difference in the pole height and airtightness data of the top cover, and identifying and eliminating the double sealing ring defects, the problem of difficult to identify the appearance of the top cover is solved, ensuring the safety of the lithium-ion battery pack.

CN118649907BActive Publication Date: 2024-12-06JIANGSU ZENIO NEW ENERGY BATTERY TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411081548.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-08
Publication Date
2024-12-06
Estimated Expiration
2044-08-08

AI Technical Summary

Technical Problem

Since the appearance of the existing battery cover is no different from that of the normal cover, it is difficult to accurately identify the defects of the double-layer sealing ring superposition, resulting in safety hazards of lithium-ion battery packs.

Method used

By measuring the height difference between the initial pole height of the top cover and the height of the pole height after heating, if it exceeds the preset threshold, it is determined to be a double sealing ring defect; at the same time, the difference between the initial and updated airtightness data is measured, if it exceeds the threshold value, it is determined to be a double sealing ring defect; at the same time, the difference between the initial and updated airtightness data is measured, if it exceeds the threshold value. , further confirm the defect.

Benefits of technology

It realizes the rapid and accurate identification of the defects of the double seal ring on the roof, and timely screening and eliminating them, avoiding subsequent safety hazards, and improving the safety of the lithium-ion battery pack.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118649907B_ABST
    Figure CN118649907B_ABST
Patent Text Reader

Abstract

The present invention discloses a method and system for identifying double sealing ring defects of a top cover. The method obtains multiple top covers to be identified and measures the initial pole heights respectively; heats each top cover to be identified according to a preset temperature and time condition to obtain an intermediate top cover; measures the updated pole height of each intermediate top cover; if the height difference between the initial pole height and the updated pole height is greater than a preset defect threshold, it is determined that the intermediate top cover to which the updated pole height belongs has a double sealing ring defect. Thus, by the change of the pole height before and after heating, it is possible to quickly and accurately identify whether the top cover to which the pole belongs has a double sealing ring defect, and timely screen and remove the top cover, effectively avoiding subsequent safety hazards.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of defect recognition, and in particular to a method and system for identifying defects of a double sealing ring of a top cover. Background Art

[0002] With the continuous development and growth of the lithium battery industry, the safety and reliability of battery cells have also become issues of great concern. Among them, power batteries, as the power source of new energy vehicles, their use affects the overall safety performance of the vehicle.

[0003] At present, new energy vehicles usually use lithium-ion batteries as power batteries. They charge and discharge by relying on the movement of lithium ions between the positive and negative electrodes. When the reaction principle is fixed, the battery structure has a decisive influence on the safety of battery use.

[0004] In the structure of lithium-ion batteries, the top cover, as one of the sealing components, has the function of preventing leakage of electrolyte inside the battery. However, some top covers may have defects such as overlapping double-layer sealing rings due to manufacturing reasons. Since their appearance is no different from that of normal top covers, it is difficult to accurately identify the defects of overlapping double-layer sealing rings, which can easily lead to safety hazards after subsequent production of lithium-ion battery packs. Summary of the invention

[0005] The present invention provides a method and system for identifying defects of double sealing rings on a top cover, which solves the technical problem that the existing battery top cover has no difference in appearance from a normal top cover, making it difficult to accurately identify the overlapping defects of the double sealing rings, which easily leads to safety hazards after subsequent production of a lithium-ion battery pack.

[0006] The present invention provides a method for identifying defects of a top cover double sealing ring, comprising:

[0007] Obtain multiple top covers to be identified, and measure the initial pole heights respectively;

[0008] Heating each of the top covers to be identified according to preset temperature and time conditions to obtain an intermediate top cover;

[0009] Measuring the height of the updated pole of each intermediate top cover;

[0010] If the height difference between the initial pole height and the updated pole height is greater than a preset defect threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated pole height belongs.

[0011] Optionally, the method further comprises:

[0012] Measuring the initial air tightness data of each of the top covers to be identified;

[0013] Measuring updated air tightness data corresponding to the middle top cover whose height difference is not greater than the defect threshold;

[0014] If the airtightness difference between the initial airtightness data and the updated airtightness data is greater than a preset airtightness threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated airtightness data belongs.

[0015] Optionally, the measuring of the initial airtightness data of each of the top covers to be identified includes:

[0016] Place each of the top covers to be identified into the breathing cavity and connect them to a breathing trachea;

[0017] Vacuuming the breathing cavity;

[0018] Injecting inert gas into the breathing cavity through the breathing trachea until the air pressure in the breathing cavity reaches a preset air pressure threshold and is maintained for a preset time;

[0019] The gas concentration of the inert gas outside the breathing cavity is detected as initial airtightness data.

[0020] Optionally, the preset air pressure threshold is 0.09 MPa.

[0021] Optionally, the acquiring of a plurality of top covers to be identified and measuring the initial pole heights respectively includes:

[0022] Obtain multiple caps to be identified;

[0023] A height gauge is used to measure the initial pole height corresponding to each of the top covers to be identified.

[0024] Optionally, the temperature-duration condition includes a temperature interval and a storage duration interval;

[0025] The temperature range is 110° C.-130° C., and the storage time range is 400h-500h.

[0026] Optionally, the method further comprises:

[0027] If the height difference is not greater than the preset defect threshold, and the airtightness difference is not greater than the preset airtightness threshold, it is determined that the intermediate top cover to which the updated pole height belongs does not have a double sealing ring defect.

[0028] The present invention also provides a top cover double sealing ring defect identification system, comprising a grasping mechanism, a first measuring mechanism, a temperature box, a second measuring mechanism and a control center;

[0029] Grab at least one top cover to be identified by the grabbing mechanism and transfer it to the conveyor belt and then to the first measuring mechanism to measure the initial pole height of the top cover to be identified and upload it to the control center;

[0030] The top covers to be identified are transported into the temperature box via the conveyor belt, so as to heat each of the top covers to be identified according to a preset temperature and time condition to obtain an intermediate top cover;

[0031] The intermediate top cover is transported to the second measuring mechanism via the conveyor belt to measure the updated pole height of the intermediate top cover and upload it to the control center;

[0032] The control center calculates the height difference between the initial pole height and the updated pole height in real time, and if the height difference is greater than a preset defect threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated pole height belongs.

[0033] Optionally, the system further comprises a breathing cavity, and the breathing cavity is externally connected to a breathing trachea;

[0034] Before the conveyor belt transports the top cover to be identified to the first measuring mechanism, the top cover is transported to the breathing cavity to measure the initial air tightness data of the top cover to be identified and upload it to the control center;

[0035] The intermediate top cover whose height difference is not greater than the defect threshold is transported to the breathing cavity by the conveyor belt to measure the updated air tightness data of the intermediate top cover and upload it to the control center;

[0036] The control center calculates the airtightness difference between the initial airtightness data and the updated airtightness data in real time. If the difference is greater than a preset airtightness threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated airtightness data belongs.

[0037] Optionally, when the control center determines that the intermediate top cover to which the updated pole height belongs and / or the intermediate top cover to which the updated air tightness data belongs has a double sealing ring defect, the control center sends a rejection instruction to the gripping mechanism;

[0038] The gripping mechanism responds to the rejection instruction to reject the middle top cover having the double sealing ring defect.

[0039] It can be seen from the above technical solutions that the present invention has the following advantages:

[0040] The present invention obtains multiple top covers to be identified and measures the initial pole heights respectively; heats each top cover to be identified according to a preset temperature and duration condition to obtain an intermediate top cover; measures the updated pole height of each intermediate top cover; if the height difference between the initial pole height and the updated pole height is greater than a preset defect threshold, it is determined that the intermediate top cover to which the updated pole height belongs has a double sealing ring defect. Thus, through the change of the pole height before and after heating, it is possible to quickly and accurately identify whether the top cover to which the pole belongs has a double sealing ring defect, and timely screen and remove the top cover, effectively avoiding subsequent safety hazards. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0042] Figure 1 A flowchart of a method for identifying defects of a double sealing ring of a top cover provided by an embodiment of the present invention;

[0043] Figure 2 A schematic cross-sectional view of a normal top cover provided by an embodiment of the present invention;

[0044] Figure 3 A normal state schematic diagram of a top cover with a double sealing ring defect provided by an embodiment of the present invention;

[0045] Figure 4 A schematic diagram of a top cover with a double sealing ring defect after heating provided by an embodiment of the present invention;

[0046] Figure 5 A schematic diagram of air tightness detection provided by an embodiment of the present invention;

[0047] Figure 6 A schematic structural diagram of a top cover double sealing ring defect identification system provided in an embodiment of the present invention. DETAILED DESCRIPTION

[0048] The embodiment of the present invention provides a method and system for identifying defects in double sealing rings on a top cover, which is used to solve the technical problem that the existing battery top cover has no difference in appearance from a normal top cover, making it difficult to accurately identify the overlapping defects of the double-layer sealing rings, which easily leads to safety hazards after subsequent production of lithium-ion battery packs.

[0049] In order to make the purpose, features and advantages of the present invention more obvious and easy to understand, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the embodiments described below are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0050] See also Figure 1 , Figure 1 A flowchart of the steps of a method for identifying defects of a top cover double sealing ring provided in an embodiment of the present invention.

[0051] The present invention provides a method for identifying defects of a top cover double sealing ring, comprising:

[0052] Step 101, obtaining a plurality of top covers 2 to be identified, and measuring the initial pole heights respectively;

[0053] like Figure 2 As shown, the top cover 2 to be identified in the embodiment of the present invention includes a pole 11, an injection molding block 12, a top cover sheet 13 and a sealing ring 14, the pole 11 is sleeved with a sealing ring 14, the top cover sheet 13 covers the sealing ring 14 and is sealed and connected to the pole 11 through the injection molding block 12. The types of the top cover 2 to be identified may include a positive pole top cover and a negative pole top cover, and the heights of the poles 11 of the two are different. Due to the influence of unexpected factors in the manufacturing process, the top cover 2 to be identified may have a double sealing ring defect.

[0054] The double sealing ring defect refers to a product defect that causes two or more sealing rings to be superimposed on the volume at the location where there was originally one sealing ring under the pole 11.

[0055] It should be noted that, taking the top cover used for 166Ah battery as an example, the cross-sectional view of a normal top cover is as follows: Figure 2 As shown in the figure, the internal structure of the normal top cover is intact, the force is evenly distributed and there is no deformation. The cross-sectional view of the defective top cover is as follows: Figure 3 As shown, since the sealing ring 14 is subjected to excessive backlog, the rebound force it generates causes the aluminum sheet covering it to bounce upward, but without the influence of other external factors, the injection block 12 in the defective top cover, such as PPS-polyphenylene sulfide, will not break and cause the pole to sink. Therefore, the defective top cover is no different from the normal top cover in appearance and is not easy to be identified.

[0056] Since it is impossible to directly determine whether the top cover has a double seal ring defect from the appearance, it is necessary to identify the double seal ring defect of the top cover material. In this embodiment, after obtaining multiple top covers 2 to be identified, the initial pole height corresponding to each top cover 2 to be identified is measured respectively as the data basis for subsequent comparison.

[0057] In an example of the present invention, step 101 may include the following sub-steps:

[0058] Obtain multiple top covers 2 to be identified;

[0059] A height gauge is used to measure the initial pole heights corresponding to each of the top covers 2 to be identified.

[0060] In an embodiment, a plurality of top covers 2 to be identified may be obtained by conveying on a conveyor belt and transported to a designated location, at which the initial pole height of each top cover 2 to be identified is measured in turn by a height gauge.

[0061] There may be a plurality of accommodating slots on the conveyor belt, in each of which a single top cover 2 to be identified is placed, and the height gauge at the designated position is used to measure the initial pole height at the point where the pole 11 is located. The height gauge may be a vernier height gauge, a gauge height gauge, a liquid crystal height gauge, a magnetic height gauge, a linear height gauge, or a two-dimensional measuring instrument, which transmits the image of the product to the control center through an imaging system, and then measures the size of the product through relevant measurement software.

[0062] Step 102, heating each of the top covers 2 to be identified according to a preset temperature and time condition to obtain an intermediate top cover;

[0063] After the initial pole height is obtained, a certain number of top covers 2 to be identified are sent to the temperature box to heat and store each top cover 2 to be identified according to the preset temperature and time conditions to obtain an intermediate top cover after being heated at a certain temperature for a certain period of time.

[0064] Specifically, under the preset temperature and time conditions, if the top cover 2 to be identified has a double sealing ring defect, the injection molded block 12 is subjected to the upward tensile force of the sealing ring 14 on the injection molded block 12, resulting in a decrease in the toughness of the injection molded block 12 during the heating process. The higher the temperature, the lower the strength of the injection molded block 12 in the tensile state, and the injection molded block 12 is prone to breakage at the weak tensile point. During the temperature rise process, the injection molded block 12 of the single-sealing-ring top cover is not subjected to the upward stretching force of the sealing ring 14, so the injection molded block 12 is heated more evenly at this temperature, and there is no weak point of the injection molded block 12 of the double-sealing-ring top cover under the stretching state. Therefore, the heat resistance of the injection molded block 12 of the single-sealing-ring top cover is much better than that of the injection molded block 12 of the double-sealing-ring top cover, so that after being stored at a certain temperature for a certain period of time, the injection molded block 12 in the top cover with the double sealing ring defect is prone to breakage, while the injection molded block 12 of the single-sealing-ring top cover is not subjected to the corresponding force and therefore will not break.

[0065] like Figure 4As shown, the injection block 12 is squeezed by the double sealing ring 14 and has weak points. After high-temperature aging, the tensile strength is reduced. The double sealing ring 14 generates an upward squeezing force to squeeze the top cover sheet 13 such as an aluminum sheet. The injection block 12 is affected by the external temperature and the upward squeezing force from the aluminum sheet. After a certain period of time, the injection block 12 breaks under the influence of multiple factors, and then moves upward to wrap the pole 11. Therefore, after heating and storage, the appearance is that the pole is sunken.

[0066] The temperature-time condition includes a temperature interval and a storage time interval. The temperature interval can be 110°C-130°C, and the storage time interval can be 400h-500h. The specific temperature interval and storage time interval are adjusted according to the type, material or size of the battery top cover. The specific adjustment method can be increased according to a certain gradient. The interval in the embodiment of the present invention is the interval required for double sealing ring defect identification of the top cover used for the 166Ah battery.

[0067] Step 103, measuring the updated pole height of each intermediate top cover;

[0068] After heating and storing each to-be-identified top cover 2 for a certain period of time, an intermediate top cover is obtained, which can be transported to a designated location by a conveyor belt or other means to update the pole height measurement. The measurement method can refer to the measurement method of the initial pole height, and the embodiment of the present invention will not be repeated here.

[0069] Step 104: If the height difference between the initial pole height and the updated pole height is greater than a preset defect threshold, it is determined that a double sealing ring defect occurs in the middle top cover of the updated pole height.

[0070] After measuring the initial pole height and the updated pole height, the height difference or the absolute value of the height difference between the two is calculated, and the height difference is compared with the preset defect threshold to determine whether the intermediate top cover has a double sealing ring defect. Since the existence of a double sealing ring defect will cause the pole to sink, if the height difference is greater than the preset defect threshold, it can be determined that the intermediate top cover to which the updated pole height belongs has a double sealing ring defect, and a mechanism can be further used to remove it to avoid safety problems caused by subsequent use.

[0071] In another example of the present invention, the method further includes the following steps S11-S13:

[0072] S11, measuring the initial air tightness data of each of the top covers 2 to be identified;

[0073] In this embodiment, in addition to the double-layer sealing ring, the defects that may occur in the top cover during the production and transportation process may include unqualified sealing and gaps at the pole 11. If the above problems occur, air leakage will occur at the pole. Before measuring the initial pole height of the top cover 2 to be identified, the first airtightness test can be performed to obtain the initial airtightness data corresponding to each top cover 2 to be identified, and the leaking top covers can be preliminarily eliminated.

[0074] In an example of the present invention, S11 may include the following sub-steps:

[0075] Place each of the top covers 2 to be identified into the breathing cavity and connect them to the breathing trachea 1;

[0076] Vacuuming the breathing cavity;

[0077] Injecting a specific gas into the breathing cavity through the breathing trachea 1 until the air pressure in the breathing cavity reaches a preset air pressure threshold and is maintained for a preset time;

[0078] The gas concentration of the specific gas outside the breathing cavity is detected as initial airtightness data.

[0079] See also Figure 5 In this embodiment, each top cover 2 to be identified is transported into the breathing cavity by a conveyor belt or other means, and a breathing trachea 1 is connected outside the breathing cavity to facilitate gas suction. The breathing cavity is vacuumed through the breathing trachea 1 to discharge the air therein, and then a specific gas is injected into the breathing cavity through the breathing trachea 1 until the air pressure in the breathing cavity reaches a preset air pressure threshold. At this time, the breathing trachea 1 is closed to maintain the air pressure in the breathing cavity for a preset time, and then the gas concentration of the specific gas outside the breathing cavity is detected to obtain initial air tightness data for measuring the air tightness of the top cover 2 to be identified. Among them, the initial air tightness data can be the gas leakage rate, gas concentration or other data for measuring air tightness of the specific gas.

[0080] In addition, the breathing tube 1 can be connected to a vacuum pump or an air tightness detector to simultaneously achieve the requirements of vacuuming and inert gas output. The preset time can be 1 hour or a time adjusted according to the size or material of the top cover 2 to be identified.

[0081] Among them, the preset air pressure threshold is 0.09 MPa, and the type of the specific gas is inert gas.

[0082] In this embodiment, the specific gas type used for measuring the air tightness data may be an inert gas, such as helium, nitrogen or dry clean air, etc., and its pressure threshold is 0.09 MPa, or adjusted according to the size or material of the top cover 2 to be identified. The helium concentration is generally less than .

[0083] S12, measuring the updated air tightness data corresponding to the middle top cover whose height difference is not greater than the defect threshold;

[0084] In this embodiment, after the top cover 2 to be identified is heated and stored to obtain the intermediate top cover, it is transported to the designated location before measuring the updated pole height of the intermediate top cover, and the air tightness test is performed again through the above-mentioned breathing cavity and the breathing trachea 1 to measure the updated air tightness data corresponding to each intermediate top cover. The measurement process can refer to the process of the above-mentioned initial air tightness data, which will not be repeated here.

[0085] S13: If the airtightness difference between the initial airtightness data and the updated airtightness data is greater than a preset airtightness threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated airtightness data belongs.

[0086] To ensure the accuracy of the detection and avoid missed detection, after completing the measurement of the updated pole height, if the height difference between the updated pole height and the initial pole height is not greater than the preset defect threshold, a second airtightness test can be performed on the intermediate top cover that does not exceed the defect threshold to obtain updated airtightness data. If the airtightness difference between the initial airtightness data and the updated airtightness data is greater than the preset airtightness threshold, it means that the intermediate top cover has leaked after heated storage, and the intermediate top cover can be discarded.

[0087] In one example of the present invention, a normal top cover will not cause changes in its pole height or airtightness data due to the heating storage operation. Therefore, if the height difference is not greater than the preset defect threshold and the airtightness difference is not greater than the preset airtightness threshold, it is determined that the intermediate top cover to which the updated pole height belongs does not have a double sealing ring defect.

[0088] See Table 1 below for the air tightness data and pole height data of different types of top covers before and after heating:

[0089] Table 1

[0090]

[0091] It can be seen from the above table that when the top cover has a double seal ring defect in the positive pole column or a double seal ring defect in the negative pole column, the difference in air tightness and the height of the positive and negative pole columns before heating is not much between the top cover and the normal top cover. However, after high-temperature baking such as 110 ℃ ≤ X ≤ 130 ℃, it can be seen that the air tightness of the top cover with double seal ring defects has significantly deteriorated, while the air tightness of the normal top cover is not affected by temperature. At the same time, after high temperature, the top cover with double seal ring defects has a significant decrease in height of both the positive pole column and the negative pole column, while the height of the normal battery cell pole remains unchanged. Among them, the positive pole double seal ring 14 pole column decreased by about 16%, and the negative pole double seal ring 14 pole column decreased by about 70%, and the negative pole double seal ring 14 pole column decreased more significantly than the positive pole double seal ring 14 pole column. The pole column of the top cover with double seal ring defect 1 of the negative pole column directly fell off at high temperature, indicating that the negative pole column is more susceptible to high temperature. It can be seen that after the above-mentioned heating and storage for a certain period of time, the top cover with double sealing ring defects can be accurately identified.

[0092] In a specific implementation, considering that the proportion of double sealing ring defects in a whole batch of top covers is extremely small, in order to reduce the identification cost of double sealing ring defects, all top covers 2 to be identified can be divided into multiple sets according to a predetermined number without measuring the pole height, and airtightness detection, heating storage, re-airtightness detection and calculation of airtightness difference are carried out in sequence in sets. If it is detected that the airtightness difference of any set is greater than the preset airtightness threshold, a single pole height detection can be performed on the set. Since the pole sinks during the heating process, and the whole batch of top covers usually has a uniform pole height, the top covers with double sealing ring defects can be determined through a single pole height detection. This greatly reduces the number of pole height detections and airtightness detections, and effectively reduces the identification cost.

[0093] In the embodiment of the present invention, multiple top covers to be identified are obtained, and the initial pole heights are measured respectively; each top cover to be identified is heated according to the preset temperature and time conditions to obtain an intermediate top cover; the updated pole height of each intermediate top cover is measured; if the height difference between the initial pole height and the updated pole height is greater than the preset defect threshold, it is determined that the intermediate top cover to which the updated pole height belongs has a double sealing ring defect. Therefore, through the change of the pole height before and after heating, it is possible to quickly and accurately identify whether the top cover to which the pole belongs has a double sealing ring defect, and timely screen and eliminate the top cover, effectively avoiding subsequent safety hazards.

[0094] See also Figure 6 , Figure 6 A schematic structural diagram of a top cover double sealing ring defect recognition system according to an embodiment of the present invention is shown.

[0095] The embodiment of the present invention further provides a top cover double sealing ring defect identification system, comprising a gripping mechanism 501, a first measuring mechanism 502, a temperature box, a second measuring mechanism 504 and a control center;

[0096] Grab at least one top cover 2 to be identified by the grabbing mechanism 501 and transfer it to the conveyor belt 506 and then to the first measuring mechanism 502 to measure the initial pole height of the top cover 2 to be identified and upload it to the control center;

[0097] The top covers 2 to be identified are transported to the temperature box via the conveyor belt 506, so as to heat each top cover 2 to be identified according to a preset temperature and time condition to obtain an intermediate top cover;

[0098] The intermediate top cover is transported to the second measuring mechanism 504 via the conveyor belt 506 to measure the updated pole height of the intermediate top cover and upload it to the control center;

[0099] The control center calculates the height difference between the initial pole height and the updated pole height in real time, and if the height difference is greater than a preset defect threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated pole height belongs.

[0100] In this embodiment, the top cover is usually produced and processed in batches. To ensure that the top cover is defect-free, the same defect identification process needs to be performed on each top cover, which is repeated many times and the action is simple. Therefore, a top cover double sealing ring defect identification system can be constructed to identify the top cover double sealing ring defects in an automated manner, thereby improving the identification efficiency while ensuring the identification accuracy. Among them, the control center communicates with the grasping mechanism 501, the first measuring mechanism 502, the temperature box 1, 2...n and the second measuring mechanism 504 and sends corresponding instructions to drive the mechanism or adjust the temperature and time conditions. Each mechanism can be arranged sequentially along the conveying direction of the conveyor belt, and the number of them is at least one.

[0101] Specifically, when the top cover is incoming, the control center sends a command to the grasping mechanism 501, and the grasping mechanism 501 grasps at least one top cover 2 to be identified and places it on the conveyor belt 506. In order to improve the grasping efficiency, the grasping mechanism 501 can grasp multiple top covers 2 to be identified by selecting a mold of a specific specification and shake it, so that the top covers 2 to be identified that are not embedded in the mold fall off, and the entire mold is placed on the conveyor belt 506; at least one top cover 2 to be identified is transported to the location of the first measuring mechanism 502 via the conveyor belt 506, and the initial pole height of the top cover 2 to be identified is measured by the first measuring mechanism 502 and uploaded to the control center. The top cover 2 to be identified can be provided with a unique identification code, and the control center constructs a key-value pair with the unique identification code and the initial pole height for storage; after completing the measurement of the initial pole height, the top cover 2 to be identified is transported to the incubator via the conveyor belt 506, so that each top cover 2 to be identified is heated by the incubator according to the temperature and time conditions set by the control center. An intermediate top cover is obtained. Since the heating time of the top cover 2 to be identified may be longer, n temperature boxes can be set up at the same time; after a batch of top covers 2 to be identified are sent to the temperature box 1, the heated intermediate top cover can be grabbed from another temperature box 2 onto the conveyor belt 506 by the grabbing mechanism 501, and the intermediate top cover is transported to the second measuring mechanism 504 via the conveyor belt 506 to measure the updated pole height of the intermediate top cover and upload it to the control center. The updated pole height can be added according to the stored key-value pair to store the initial pole height and the updated pole height of the same unique identification code in correspondence; after receiving the initial pole height and the updated pole height, the control center calculates the height difference between the initial pole height and the updated pole height in real time, and compares the height difference with the preset defect threshold. If the height difference is greater than the preset defect threshold, it is determined that the intermediate top cover to which the updated pole height belongs has a double sealing ring defect, thereby completing the identification of whether the top cover has a double sealing ring defect.

[0102] In one example of the present invention, the system further comprises a breathing cavity 505, and the breathing cavity 505 is externally connected to a breathing trachea 1;

[0103] Before the conveyor belt 506 transports the top cover 2 to be identified to the first measuring mechanism 502, it is transported to the breathing cavity 505 to measure the initial air tightness data of the top cover 2 to be identified and upload it to the control center;

[0104] The intermediate top cover whose height difference is not greater than the defect threshold is transported to the breathing cavity 505 by the conveyor belt 506 to measure the updated air tightness data of the intermediate top cover and upload it to the control center;

[0105] The control center calculates the airtightness difference between the initial airtightness data and the updated airtightness data in real time. If the difference is greater than a preset airtightness threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated airtightness data belongs.

[0106] In this embodiment, the system may further be provided with a plurality of additional breathing cavities 505 along the transport direction of the conveyor belt 506 , and the breathing cavities 505 are externally connected to the breathing air tubes 1 to provide a mechanism for performing airtightness detection on the top cover.

[0107] Specifically, before the conveyor belt 506 transports the top cover 2 to be identified to the first measuring mechanism 502, it can be first transported to the breathing cavity 505 by the conveyor belt 506, the breathing cavity 505 is sealed and the breathing cavity 505 is evacuated through the breathing trachea 1, and then filled with inert gas to maintain a certain pressure for a certain time, and the leakage rate of the inert gas is measured as the initial airtightness data of the top cover 2 to be identified and uploaded to the control center, so as to facilitate the elimination of some top covers 2 to be identified with airtightness defects. The control center can construct a key-value pair with it and the above-mentioned unique identification code, and the subsequent initial pole height is also stored in the key-value pair, and then the top cover 2 to be identified is transported to the first measuring mechanism 502 for measurement of the initial pole height. After the top cover 2 to be identified is heated and stored in any temperature box to obtain the intermediate top cover, the intermediate top cover is then transported to the second measuring mechanism 504 to measure the updated pole height to determine whether the pole height of the top cover 2 to be identified changes before and after heating, and then the conveyor belt 506 transports the intermediate top cover to the breathing cavity 505 to measure the updated air tightness data of the intermediate top cover and upload it to the control center, which stores the updated air tightness data and the initial air tightness data in a unified manner. The control center then calculates the air tightness difference between the initial air tightness data and the updated air tightness data in real time, and compares the air tightness difference with the preset air tightness threshold. If the air tightness difference is greater than the preset air tightness threshold, it is determined that the intermediate top cover may have an air tightness defect during the heating process, and the air tightness defect may be caused by a double sealing ring defect. It can be determined that the intermediate top cover to which the updated air tightness data belongs has a double sealing ring defect, thereby effectively avoiding missed detection through two air tightness tests and two pole height measurements, and improving the accuracy of top cover defect identification.

[0108] It should be noted that the conveyor belt 506 may include multiple branches that are interconnected, and each measuring mechanism, temperature box, gripping mechanism 501 or breathing chamber 505 may be distributed near each branch to facilitate the transportation of the conveyor belt 506 and complete the detection or measurement operations of different items of the top cover.

[0109] In addition, if the height difference is not greater than the preset defect threshold, and the airtightness difference is not greater than the preset airtightness threshold, it is determined that the intermediate top cover to which the updated pole height belongs does not have a double sealing ring defect.

[0110] Further, when the control center determines that the intermediate top cover to which the updated pole height belongs and / or the intermediate top cover to which the updated air tightness data belongs has a double sealing ring defect, the control center sends a rejection instruction to the gripping mechanism 501;

[0111] The gripping mechanism 501 responds to the rejection instruction to reject the middle top cover having the double sealing ring defect.

[0112] In an embodiment of the present invention, if the control center determines that the intermediate top cover to which the updated pole height belongs and / or the intermediate top cover to which the updated airtightness data belongs has a double sealing ring defect, the intermediate top cover to which the corresponding unique identification code belongs can be located at this time, so as to generate a removal instruction and send it to the grasping mechanism 501 to control the grasping mechanism 501 to remove the intermediate top cover, thereby avoiding safety hazards in subsequent battery assembly.

[0113] In an embodiment of the present invention, a top cover double sealing ring defect identification system is provided, specifically, at least one top cover to be identified is grabbed by a grabbing mechanism and transported to a conveyor belt to a first measuring mechanism, so as to measure the initial pole height of the top cover to be identified and upload it to a control center; the top cover to be identified is transported to an incubator via a conveyor belt, so as to heat each top cover to be identified according to a preset temperature and time condition to obtain an intermediate top cover; the intermediate top cover is transported to a second measuring mechanism via a conveyor belt, so as to measure the updated pole height of the intermediate top cover and upload it to the control center; the control center calculates the height difference between the initial pole height and the updated pole height in real time, and if the height difference is greater than a preset defect threshold, it is determined that the intermediate top cover to which the updated pole height belongs has a double sealing ring defect, thereby improving the identification efficiency on the basis of accurately identifying the double sealing ring defect of the top cover, thereby effectively avoiding safety hazards in subsequent batteries.

[0114] Those skilled in the art can clearly understand that, for the convenience and brevity of description, the specific working process of the above-described system and mechanism can refer to the corresponding process in the aforementioned method embodiment, and will not be repeated here.

[0115] In the several embodiments provided by the present invention, it should be understood that the disclosed systems and methods can be implemented in other ways. For example, the system embodiments described above are only schematic. For example, the division of the modules is only a logical function division. There may be other division methods in actual implementation, such as multiple modules or components can be combined or integrated into another system, or some features can be ignored or not executed. Another point is that the mutual coupling or direct coupling or communication connection shown or discussed can be through some interfaces, indirect coupling or communication connection of systems or modules, which can be electrical, mechanical or other forms.

[0116] As described above, the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features thereof may be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for identifying defects of double sealing rings of top cover, It is characterized in that include: Obtain multiple top covers to be identified, and measure the initial pole heights respectively; Heating each of the top covers to be identified according to preset temperature and time conditions to obtain an intermediate top cover; Measuring the height of the updated pole of each intermediate top cover; If the height difference between the initial pole height and the updated pole height is greater than a preset defect threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated pole height belongs; The method further comprises: Before measuring the initial pole heights respectively, measuring the initial air tightness data of each of the top covers to be identified; Measuring updated air tightness data corresponding to the middle top cover whose height difference is not greater than the defect threshold; If the airtightness difference between the initial airtightness data and the updated airtightness data is greater than a preset airtightness threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated airtightness data belongs.

2. The method according to claim 1, It is characterized in that The measuring of the initial air tightness data of each of the top covers to be identified comprises: Place each of the top covers to be identified into the breathing cavity and connect them to a breathing trachea; Vacuuming the breathing cavity; Injecting inert gas into the breathing cavity through the breathing trachea until the air pressure in the breathing cavity reaches a preset air pressure threshold and is maintained for a preset time; The gas concentration of the inert gas outside the breathing cavity is detected as initial airtightness data.

3. The method according to claim 2, It is characterized in that The preset air pressure threshold is 0.09 MPa.

4. The method according to claim 1, It is characterized in that The step of obtaining a plurality of top covers to be identified and measuring the initial pole heights respectively includes: Obtain multiple caps to be identified; A height gauge is used to measure the initial pole height corresponding to each of the top covers to be identified.

5. The method according to claim 1, It is characterized in that The temperature-time condition includes a temperature interval and a storage time interval; The temperature range is 110° C.-130° C., and the storage time range is 400h-500h.

6. The method according to claim 1, It is characterized in that The method further comprises: If the height difference is not greater than the preset defect threshold, and the airtightness difference is not greater than the preset airtightness threshold, it is determined that the intermediate top cover to which the updated pole height belongs does not have a double sealing ring defect.

7. A top cover double sealing ring defect recognition system, It is characterized in that It includes a grasping mechanism, a first measuring mechanism, a temperature box, a second measuring mechanism and a control center; Grab at least one top cover to be identified by the grabbing mechanism and transfer it to the conveyor belt and then to the first measuring mechanism to measure the initial pole height of the top cover to be identified and upload it to the control center; The top covers to be identified are transported into the temperature box via the conveyor belt, so as to heat each of the top covers to be identified according to a preset temperature and time condition to obtain an intermediate top cover; The intermediate top cover is transported to the second measuring mechanism via the conveyor belt to measure the updated pole height of the intermediate top cover and upload it to the control center; The control center calculates the height difference between the initial pole height and the updated pole height in real time, and if the height difference is greater than a preset defect threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated pole height belongs; The system also includes a breathing cavity, and the breathing cavity is externally connected to a breathing trachea; Before the conveyor belt transports the top cover to be identified to the first measuring mechanism, the top cover is transported to the breathing cavity to measure the initial air tightness data of the top cover to be identified and upload it to the control center; The intermediate top cover whose height difference is not greater than the defect threshold is transported to the breathing cavity by the conveyor belt to measure the updated air tightness data of the intermediate top cover and upload it to the control center; The control center calculates the airtightness difference between the initial airtightness data and the updated airtightness data in real time. If the difference is greater than a preset airtightness threshold, it is determined that a double sealing ring defect occurs in the middle top cover to which the updated airtightness data belongs.

8. The top cover double sealing ring defect identification system according to claim 7, It is characterized in that When the control center determines that the intermediate top cover to which the updated pole height belongs and / or the intermediate top cover to which the updated air tightness data belongs has a double sealing ring defect, the control center sends a rejection instruction to the gripping mechanism; The gripping mechanism responds to the rejection instruction to reject the middle top cover having the double sealing ring defect.

Citation Information

Patent Citations

  • Method and system

    CN106457652A

  • Air tightness detection method for automobile battery

    CN113074878A