Enameled wire production coating equipment and process

By designing partitions in the enameled wire production equipment to divide the cleaning and coating rooms, and using motors and electric push rods to drive the coating barrel to rotate and sponge blocks to clean impurities, the problems of uneven coating and the influence of impurities are solved, and efficient Enameled wire surface coating.

CN118737583AActive Publication Date: 2024-10-01湖南聚石科技有限公司
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411085143.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-08
Publication Date
2024-10-01
Estimated Expiration
2044-08-08

AI Technical Summary

Technical Problem

In existing enameled wire coating equipment, since the coating groove is arc-shaped, it cannot wrap the entire outer surface of the wire body, resulting in uneven coating, and impurities on the surface of the wire body affect the coating effect.

Method used

Design an enameled wire production and coating equipment including a holding box, a partition, a motor and an electric push rod. The partition divides the cleaning room and the coating room. The motor is used to drive the coating barrel to rotate and the sponge block to clean impurities to ensure that the wire body Surface is evenly coated.

Benefits of technology

It achieves continuous cleaning and uniform coating of the wire surface, improves the coating effect and efficiency, and simplifies the operating process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737583A_ABST
    Figure CN118737583A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of varnished wire processing, particularly relates to varnished wire production coating equipment, and aims to solve the problems that a coating dead angle is formed above a wire body and coating cannot be performed due to the fact that a coating groove is arc-shaped and cannot wrap the whole outer surface of the wire body when the wire body is coated through a lubricating coating roller in the prior art, so that the coating is not uniform, and the production efficiency is high. In order to solve the problems that in the prior art, in the prior art, the surface of a wire body has impurities before being coated, and if the surface is not cleaned, the coating effect is influenced, the following scheme is provided: the device comprises a containing box, two partition plates are fixedly arranged in the containing box, and the containing box is divided into a cleaning room for cleaning and coating the wire body, a first coating room and a second coating room; according to the coating device, by starting the electric push rod and the motor, the electric push rod and the motor can drive the wire body to be immersed in the liquid, the liquid can be smeared through the coating brush in the coating barrel, the coating effect can be improved, the coating efficiency can be improved, and operation and use are easy and convenient.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of enameled wire processing, and in particular to an enameled wire production coating device and process. Background Art

[0002] Enameled wire is a main type of winding wire, consisting of a conductor and an insulating layer. The bare wire is annealed and softened, then painted and baked multiple times. The painting step requires the use of coating equipment for processing.

[0003] After searching, the invention with announcement number CN110223804A discloses an enameled wire surface lubrication coating device, which indirectly drives the second rotating shaft and the lubricating coating roller to rotate through a second rotating motor through a belt-driven pulley. At this time, the lubricating coating roller is in contact with the lubricating oil, and the coating groove on the surface is filled with lubricating oil. At this time, the enameled wire is coated through the coating groove, and then the anti-drip absorption felt absorbs excess lubricating oil to prevent excess lubricating oil from dripping.

[0004] The device also has the following disadvantages during use: the wire body is coated by a lubricating coating roller during use. Since the coating groove is arc-shaped, it cannot wrap the entire outer surface of the wire body, which makes the upper part of the wire body a coating dead corner, and coating cannot be performed, resulting in uneven coating. In addition, the wire body has impurities on the surface before coating, which will affect the coating effect if it is not cleaned. Summary of the invention

[0005] The purpose of the present invention is to solve the problems in the prior art that the wire body is coated by a lubricating coating roller. Since the coating groove is arc-shaped, it cannot wrap the entire outer surface of the wire body, which makes the upper part of the wire body a coating dead corner, and coating cannot be carried out, resulting in uneven coating, and the wire body has impurities on the surface before coating. If the impurities are not cleaned, the coating effect is affected. A kind of enameled wire production coating equipment and process is proposed.

[0006] In order to achieve the above object, the present invention adopts the following technical solutions:

[0007] An enameled wire production coating device comprises a containing box, wherein two partitions are fixedly provided inside the containing box, dividing the containing box into a cleaning room for cleaning and coating the wire body, a first coating room, and a second coating room;

[0008] A top plate, the top plate is lifted and arranged on the top of the containing box by a supporting member, two groups of first extension plates are fixedly arranged at the bottom of the top plate, a plurality of coating cylinders for coating the wire body are arranged between each group of the first extension plates, and after being lowered, the two groups of the first extension plates are respectively located in the first coating room and the second coating room;

[0009] A second extension plate, the second extension plate is fixedly arranged at the bottom of the top plate, a sponge block for cleaning the wire body is inserted at the bottom of the second extension plate, and a plurality of second guide wheels for guiding the wire body are fixedly arranged on both sides of the second extension plate;

[0010] A plurality of sets of first guide wheels, wherein the plurality of sets of the first guide wheels are respectively fixed on the containing box, the partition plate and the first extension plate, and are used to further guide the wire body;

[0011] A motor, which is arranged on the top plate and is used to drive the coating cylinder to rotate to improve the coating effect;

[0012] The electric push rod is fixed on the top plate and used in conjunction with the support member to provide lifting power for the support member.

[0013] In a possible design, the support member includes two groups of second fixed blocks fixed on both sides of the containing box, a first guide rod is slidably provided through the top of the second fixed block, a first fixed block is fixed on the top of the first guide rod, and the first fixed block is fixed on one side of the top plate to guide the lifting and lowering of the top plate.

[0014] In a possible design, a rotating rod is rotatably provided between the two first fixed blocks on the same side, and the outer walls of the two rotating rods are sleeved with the same sliding frame. Third fixed blocks are fixedly provided at the four corners of the bottom of the sliding frame, and a connecting rod is rotatably provided on the inner side of the third fixed block. The other end of the connecting rod is rotatably connected to the containing box, and the output end of the electric push rod is fixedly connected to the sliding frame.

[0015] In a possible design, a plug hole is provided at the bottom of the second extension plate, a plug strip is inserted into the plug hole, a connecting plate is fixed at the bottom of the plug strip, the sponge block is fixed at the bottom of the connecting plate, and a plurality of grooves for positioning the wire body are provided at the bottom of the sponge block.

[0016] In a possible design, a connecting frame is fixedly provided on the inner side of each group of the first extension plates, and a plurality of the coating cylinders are rotatably arranged between two connecting frames. A coating brush for coating the wire body is provided inside the coating cylinder, and a through hole for the wire body to pass through is provided at the bottom of the coating cylinder and the connecting frame.

[0017] In a possible design, a sliding plate is slidably provided between the two first extension plates, the bottom of the sliding plate is in contact with a plurality of coating brushes, two rectangular holes are provided on the top of the top plate, sliding bars are slidably provided in the rectangular holes, the bottom of the sliding bars is fixedly connected to the corresponding sliding plates, a first connecting bar is fixedly provided between the two sliding bars, a second connecting bar is fixedly provided on one side of the first connecting bar, the output end of the motor is fixedly connected to one of the rotating rods, and the second connecting bar is used in conjunction with the rotating rod to provide rotational power for the coating cylinder.

[0018] In a possible design, the outer wall fixed sleeve of the rotating rod is provided with a cam that interferes with the second connecting strip, the top of the top plate is fixed with a fourth fixed block, one side of the fourth fixed block is fixed with a second guide rod, the second guide rod is slidably connected with the first connecting strip, the outer wall sleeve of the second guide rod is provided with a spring, and the two ends of the spring are respectively fixedly connected to the first connecting strip and the side of the fourth fixed block close to each other.

[0019] A coating process for producing an enameled wire comprises the following steps:

[0020] S1. First, pass the wire body between the storage box and the top plate, then place it in the corresponding second guide wheel and the first guide wheel, and start the electric push rod to drive the top plate to move downward, so that the wire body is immersed in the cleaning liquid and the coating liquid;

[0021] S2, then start the pay-off and take-up rollers to drive the wire body to move, and during the movement, the impurities on the outer wall of the wire body are cleaned by the sponge block;

[0022] S3, the cleaned wire body is moved to the first coating room and the second coating room in turn, and the motor is started to drive the coating cylinder to rotate so that the coating liquid is evenly applied on the wire body;

[0023] S4. Finally, the fabric is dried in an external dryer and rolled up.

[0024] In the present application, first, the wire body is passed between the storage box and the top plate, and then placed in the corresponding second guide wheel, the groove and the first guide wheel. At the same time, the wire body is placed in the coating cylinder through the through hole, and the electric push rod is started to extend, which can drive the sliding frame to move on the two rotating rods. During the movement, the connecting rod can be driven to rotate through the third fixed block. During the rotation of the connecting rod, the top plate can be driven to move downward, so that the wire body is immersed in the cleaning liquid and the coating liquid;

[0025] Then start the pay-off and take-up rollers to drive the wire body to move. During the movement, the wire body starts in the groove, and the sponge block can be used to clean the impurities on the outer wall of the wire body to keep its surface clean;

[0026] Secondly, the cleaned wire body moves to the first coating room and the second coating room in turn, and the motor is started to drive the rotating rod to rotate. The rotation of the rotating rod can drive the cam to rotate. When the convex part of the cam contacts the second connecting strip, it can drive the second connecting strip to move, and drive the two sliding strips to move in the rectangular hole through the first connecting strip. During the movement, the sliding plate can be driven to move. The movement of the sliding plate can drive the coating barrel to rotate through the friction between the sliding plate and the coating barrel, and the coating liquid is evenly applied to the wire body through the coating brush. When the convex part of the cam is away from the second connecting strip, the first connecting strip can be reset and moved under the action of the spring, driving the sliding plate to reset and move, which can drive the coating barrel to rotate in the opposite direction, and coating is performed in turn.

[0027] Finally, it is dried in an external dryer and rolled.

[0028] Beneficial effects:

[0029] In the present invention, the enameled wire production coating equipment can divide the storage box into a cleaning room, a first coating room and a second coating room through two partitions, so that the wire body can be cleaned and coated continuously, which can improve the coating effect;

[0030] In the present invention, the enameled wire production coating equipment drives the top plate to move up and down by starting the electric push rod, so that the wire body can be immersed in the liquid, which can improve the cleaning and coating effects. After immersion, the wire body is curved, and its inclined portion guides the excess coating.

[0031] In the present invention, the enameled wire production coating equipment can drive the coating barrel to reciprocate by starting the motor, so that the surface of the wire body can be reciprocatedly coated, which can improve the coating effect and is easy to use;

[0032] In the present invention, by starting the electric push rod and the motor, the wire body can be driven to be immersed in the liquid, and the liquid can also be applied through the coating brush in the coating barrel, which can not only improve the coating effect, but also improve the coating efficiency, and the operation is simple and convenient. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 A three-dimensional structural schematic diagram of an enameled wire production coating device proposed by the present invention;

[0034] Figure 2 This is a schematic cross-sectional view of a containing box of an enameled wire production and coating equipment proposed by the present invention;

[0035] Figure 3 A schematic diagram of a top plate connection structure of an enameled wire production coating device proposed by the present invention;

[0036] Figure 4 for Figure 3 A schematic diagram of the enlarged structure of the middle part A;

[0037] Figure 5 This is a schematic diagram of the coating barrel connection structure of an enameled wire production coating equipment proposed by the present invention;

[0038] Figure 6 A schematic diagram of a connection structure of a connection frame of an enameled wire production and coating equipment proposed by the present invention;

[0039] Figure 7 for Figure 6 Enlarged schematic diagram of part A in the middle.

[0040] In the figure: 1, holding box; 2, first guide wheel; 3, top plate; 4, motor; 5, first extension plate; 6, coating cylinder; 7, second extension plate; 8, second guide wheel; 9, partition; 10, cleaning room; 11, first coating room; 12, second coating room; 13, first fixed block; 14, first guide rod; 15, second fixed block; 16, rotating rod; 17, sliding frame; 18, third fixed block; 19, connecting rod; 20, connecting frame; 21, jack; 22, insert strip; 23, connecting plate; 24, sponge block; 25, groove; 26, coating brush; 27, through hole; 28, sliding plate; 29, electric push rod; 30, rectangular hole; 31, sliding bar; 32, first connecting bar; 33, second connecting bar; 34, cam; 35, fourth fixed block; 36, second guide rod; 37, spring. DETAILED DESCRIPTION

[0041] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0042] Example 1

[0043] Reference Figure 1-Figure 7 , an enameled wire production coating equipment, which is used in the field of enameled wire processing, comprises: a containing box 1, two partitions 9 are fixedly provided inside the containing box 1, dividing it into a cleaning room 10 for cleaning and coating the wire body, a first coating room 11 and a second coating room 12;

[0044] A top plate 3, which is lifted and lowered on the top of the containing box 1 by a supporting member, and two groups of first extension plates 5 are fixedly provided at the bottom of the top plate 3, and a plurality of coating cylinders 6 for coating the wire body are provided between each group of first extension plates 5, and after being lowered, the two groups of first extension plates 5 are respectively located in the first coating room 11 and the second coating room 12;

[0045] A second extension plate 7, the second extension plate 7 is fixedly arranged at the bottom of the top plate 3, a sponge block 24 for cleaning the wire body is inserted at the bottom of the second extension plate 7, and a plurality of second guide wheels 8 for guiding the wire body are fixedly arranged on both sides of the second extension plate 7;

[0046] A plurality of sets of first guide wheels 2, the plurality of sets of first guide wheels 2 are respectively fixed on the containing box 1, the partition plate 9 and the first extension plate 5, and are used to further guide the wire body;

[0047] Motor 4, which is arranged on the top plate 3 and is used to drive the coating cylinder 6 to rotate to improve the coating effect;

[0048] The electric push rod 29 is fixed on the top plate 3 and used in conjunction with the support member to provide lifting power for the support member. By placing the wire body in the corresponding first guide wheel 2, second guide wheel 8 and coating cylinder 6, and starting the electric push rod 29 to drive the top plate 3 to move downward, the wire body can be immersed in the cleaning water and the coating liquid. While the wire body is moving, the motor 4 is started to drive the coating cylinder 6 to rotate, so that the coating liquid can be evenly applied to the wire body, making it simple to operate and convenient for threading.

[0049] The support member includes two groups of second fixed blocks 15 fixedly arranged on both sides of the containing box 1, a first guide rod 14 is slidably provided on the top of the second fixed block 15, a first fixed block 13 is fixedly arranged on the top of the first guide rod 14, and the first fixed block 13 is fixedly arranged on one side of the top plate 3 to guide the lifting of the top plate 3. The top plate 3 is guided by the first guide rod 14 and the second fixed block 15 so that it will not deviate during the movement, so that it can only be lifted and lowered.

[0050] A rotating rod 16 is rotatably provided between the two first fixed blocks 13 on the same side, and the outer walls of the two rotating rods 16 are sleeved with the same sliding frame 17. Third fixed blocks 18 are fixedly provided at the four corners of the bottom of the sliding frame 17. A connecting rod 19 is rotatably provided on the inner side of the third fixed block 18. The other end of the connecting rod 19 is rotatably connected to the containing box 1. The output end of the electric push rod 29 is fixedly connected to the sliding frame 17. The sliding frame 17 can be driven to move by starting the electric push rod 29 to extend. The movement of the sliding frame 17 can drive the connecting rod 19 to rotate on the containing box 1 through the third fixed block 18. During the rotation, the top plate 3 can be guided by the first guide rod 14 and the second fixed block 15 to move downward.

[0051] A plug hole 21 is provided at the bottom of the second extension plate 7, and an insertion strip 22 is inserted into the plug hole 21. A connecting plate 23 is fixedly provided at the bottom of the insertion strip 22. A sponge block 24 is fixedly provided at the bottom of the connecting plate 23. A plurality of grooves 25 for positioning the wire body are provided at the bottom of the sponge block 24. By arranging the sponge block 24 on the connecting plate 23, and inserting the connecting plate 23 into the second extension plate 7 through the insertion strip 22, it is convenient to replace the sponge block 24. In addition, a groove 25 is provided at the bottom of the sponge block 24 to position the wire body, so that the surface of the wire body can contact the sponge block 24, thereby reducing the cleaning dead angle.

[0052] A connecting frame 20 is fixedly provided on the inner side of each group of first extension plates 5, and a plurality of coating cylinders 6 are rotatably arranged between two connecting frames 20. A coating brush 26 for coating the wire body is arranged in the coating cylinder 6. A through hole 27 for the wire body to pass through is provided at the bottom of the coating cylinder 6 and the connecting frame 20. By rotatably placing the coating cylinder 6 on the two connecting frames 20, the coating cylinder 6 can be supported, and the wire body can move into the coating cylinder 6 through the through hole 27 and be coated by the coating brush 26, thereby improving the coating effect.

[0053] Example 2

[0054] refer to Figure 1-Figure 7 , an improvement on the basis of Example 1: a sliding plate 28 is slidably provided between the two first extension plates 5, and the bottom of the sliding plate 28 contacts with multiple coating brushes 26. Two rectangular holes 30 are provided on the top of the top plate 3, and a sliding bar 31 is slidably provided in the rectangular hole 30. The bottom of the sliding bar 31 is fixedly connected to the corresponding sliding plate 28, and a first connecting bar 32 is fixedly provided between the two sliding bars 31. A second connecting bar 33 is fixedly provided on one side of the first connecting bar 32. The output end of the motor 4 is fixedly connected to one of the rotating rods 16, and the second connecting bar 33 is used in conjunction with the rotating rod 16 to provide rotational power for the coating cylinder 6. By starting the motor 4, the rotating rod 16 can be driven to rotate, and the rotation of the rotating rod 16 can drive the second connecting bar 33 to move, so that the sliding plate 28 can be driven to move through the sliding bar 31. During the movement, the sliding plate 28 can drive the coating cylinder 6 to rotate through friction to perform coating work.

[0055] The outer wall fixed sleeve of the rotating rod 16 is provided with a cam 34 that conflicts with the second connecting strip 33, and a fourth fixed block 35 is fixedly provided on the top of the top plate 3, and a second guide rod 36 is fixedly provided on one side of the fourth fixed block 35. The second guide rod 36 is slidably connected with the first connecting strip 32, and the outer wall sleeve of the second guide rod 36 is provided with a spring 37. The two ends of the spring 37 are respectively fixedly connected to the first connecting strip 32 and the fourth fixed block 35 on the side close to each other. The rotation of the rotating rod 16 can drive the cam 34 to rotate. When the convex part of the cam 34 contacts the second connecting strip 33, it will drive the second connecting strip 33 to move, and drive the sliding plate 28 to move. When the convex part of the cam 34 is away from the second connecting strip 33, the first connecting strip 32 can be reset and moved under the action of the spring 37, so that it can reset and move the sliding plate 28, which is convenient for driving the coating cylinder 6 to rotate reciprocally.

[0056] A coating process for producing an enameled wire comprises the following steps:

[0057] S1. First, pass the wire body between the storage box 1 and the top plate 3, and then place it in the corresponding second guide wheel 8 and the first guide wheel 2, and start the electric push rod 29 to drive the top plate 3 to move downward, so that the wire body is immersed in the cleaning liquid and the coating liquid;

[0058] S2, then start the pay-off and take-up rollers to drive the wire body to move, and during the movement, the sponge block 24 cleans the impurities on the outer wall of the wire body;

[0059] S3, the cleaned wire body is moved to the first coating room 11 and the second coating room 12 in sequence, and the motor 4 is started to drive the coating cylinder 6 to rotate so that the coating liquid is evenly applied on the wire body;

[0060] S4. Finally, the fabric is dried in an external dryer and rolled up.

[0061] However, as is well known to those skilled in the art, the working principles and wiring methods of the motor 4 and the electric push rod 29 are commonplace, and are conventional means or common knowledge, and will not be elaborated here. Those skilled in the art may make any optional selections according to their needs or convenience.

[0062] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. An enameled wire production coating device, characterized in that: It comprises a storage box (1), wherein two partitions (9) are fixedly provided inside the storage box (1), dividing the storage box (1) into a cleaning room (10) for cleaning and coating the wire body, a first coating room (11) and a second coating room (12); A top plate (3), the top plate (3) being arranged on the top of the storage box (1) by means of a support member, two groups of first extension plates (5) being fixedly arranged at the bottom of the top plate (3), a plurality of coating cylinders (6) for coating the wire body being arranged between each group of the first extension plates (5), and after being lowered, the two groups of the first extension plates (5) are respectively located in the first coating room (11) and the second coating room (12); A second extension plate (7), the second extension plate (7) being fixedly arranged at the bottom of the top plate (3), a sponge block (24) for cleaning the wire body being inserted at the bottom of the second extension plate (7), and a plurality of second guide wheels (8) for guiding the wire body being fixedly arranged on both sides of the second extension plate (7); A plurality of groups of first guide wheels (2), wherein the plurality of groups of the first guide wheels (2) are respectively fixed on the containing box (1), the partition plate (9) and the first extension plate (5), and are used to further guide the wire body; A motor (4), wherein the motor (4) is arranged on the top plate (3) and is used to drive the coating cylinder (6) to rotate, thereby improving the coating effect; An electric push rod (29) is fixedly arranged on the top plate (3) and used in conjunction with the support member to provide lifting power for the support member.

2. The enameled wire production coating equipment according to claim 1, characterized in that: The support member comprises two groups of second fixed blocks (15) fixedly arranged on both sides of the storage box (1); a first guide rod (14) is slidably provided on the top of the second fixed block (15); a first fixed block (13) is fixedly arranged on the top of the first guide rod (14); the first fixed block (13) is fixedly arranged on one side of the top plate (3) to guide the lifting and lowering of the top plate (3).

3. The enameled wire production coating equipment according to claim 2, characterized in that: A rotating rod (16) is rotatably provided between the two first fixed blocks (13) on the same side, and the outer walls of the two rotating rods (16) are sleeved with a same sliding frame (17). A third fixed block (18) is fixedly provided at the four corners of the bottom of the sliding frame (17), and a connecting rod (19) is rotatably provided inside the third fixed block (18). The other end of the connecting rod (19) is rotatably connected to the storage box (1), and the output end of the electric push rod (29) is fixedly connected to the sliding frame (17).

4. The enameled wire production coating equipment according to claim 1, characterized in that: The bottom of the second extension plate (7) is provided with an insertion hole (21), an insertion strip (22) is inserted into the insertion hole (21), a connecting plate (23) is fixedly provided at the bottom of the insertion strip (22), the sponge block (24) is fixedly provided at the bottom of the connecting plate (23), and a plurality of grooves (25) for positioning the wire body are provided at the bottom of the sponge block (24).

5. The enameled wire production coating equipment according to claim 1, characterized in that: A connecting frame (20) is fixedly provided on the inner side of each group of the first extension plates (5), and a plurality of the coating cylinders (6) are rotatably arranged between two connecting frames (20). A coating brush (26) for coating the wire body is provided inside the coating cylinder (6), and a through hole (27) for the wire body to pass through is provided at the bottom of the coating cylinder (6) and the connecting frame (20).

6. The enameled wire production coating equipment according to claim 5, characterized in that: A sliding plate (28) is slidably provided between the two first extension plates (5), the bottom of the sliding plate (28) contacts with a plurality of coating brushes (26), two rectangular holes (30) are provided on the top of the top plate (3), a sliding bar (31) is slidably provided in the rectangular hole (30), the bottom of the sliding bar (31) is fixedly connected to the corresponding sliding plate (28), a first connecting bar (32) is fixedly provided between the two sliding bars (31), a second connecting bar (33) is fixedly provided on one side of the first connecting bar (32), an output end of the motor (4) is fixedly connected to one of the rotating rods (16), and the second connecting bar (33) is used in conjunction with the rotating rod (16) to provide rotational power for the coating cylinder (6).

7. The enameled wire production coating equipment according to claim 6, characterized in that: The outer wall of the rotating rod (16) is fixedly sleeved with a cam (34) that contacts the second connecting strip (33); the top of the top plate (3) is fixedly provided with a fourth fixing block (35); one side of the fourth fixing block (35) is fixedly provided with a second guide rod (36); the second guide rod (36) is slidably connected to the first connecting strip (32); the outer wall of the second guide rod (36) is sleeved with a spring (37); two ends of the spring (37) are respectively fixedly connected to the first connecting strip (32) and one side of the fourth fixing block (35) that are close to each other.

8. A coating process for producing enameled wire according to any one of claims 1 to 7, characterized in that: The following steps are involved: S1. First, the wire body is passed between the storage box (1) and the top plate (3), and then placed on the corresponding second guide wheel (8) and the first guide wheel (2), and the electric push rod (29) is started to drive the top plate (3) to move downward, so that the wire body is immersed in the cleaning liquid and the coating liquid; S2, then start the pay-off and take-up rollers to drive the wire body to move, and during the movement, the sponge block (24) is used to clean the impurities on the outer wall of the wire body; S3, the cleaned wire body is moved to the first coating room (11) and the second coating room (12) in turn, and the motor (4) is started to drive the coating cylinder (6) to rotate so that the coating liquid is evenly applied on the wire body; S4. Finally, the fabric is dried in an external dryer and rolled up.

Citation Information

Patent Citations

  • Enameled wire production coating device

    CN113245107A

  • Enameled wire production coating device and process

    CN117012466A

  • Reinforced coating mechanism for enameled wire processing

    CN211887602U

  • Enameled wire surface lubricant coating device

    CN216849472U

  • Enameled wire production coating device

    CN220004619U