Semiconductor structure and preparation method thereof

By forming an intermediate barrier layer in the semiconductor memory, the problem of short circuit in the bit line contact structure is solved, the yield rate and film quality of the memory are improved, and the short circuit phenomenon in the preparation process is avoided.

CN118742011AActive Publication Date: 2024-10-01CHANGXIN MEMORY TECH INC
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202310304252.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-24
Publication Date
2024-10-01
Estimated Expiration
2043-03-24

AI Technical Summary

Technical Problem

As the feature size of semiconductor structures shrinks, the bit line contact structure in the memory is prone to short circuit. It is difficult for the existing technology to effectively avoid the short circuit phenomenon caused by poor manufacturing process, which affects the yield of the memory.

Method used

By forming an initial barrier layer on the outer wall of the conductive pillar and introducing a preset process gas to turn it into an intermediate barrier layer, impurities and reaction by-products are reduced, the wet etching rate is reduced, and the target barrier layer thickness is ensured to be within the preset range. Avoid short circuits.

Benefits of technology

It effectively improves the film quality and yield of the bit line contact structure, reduces the product rework rate, avoids short circuits and damage to electronic components, and improves the quality of semiconductor products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118742011A_ABST
    Figure CN118742011A_ABST
Patent Text Reader

Abstract

The invention relates to a semiconductor structure and a preparation method thereof, and the method comprises the steps: providing a substrate, and forming conductive columns which are arranged at intervals in a first direction on the substrate; introducing a reaction precursor into a gap between the adjacent conductive columns to form an initial barrier layer; preset process gas is introduced into the gap, so that the initial barrier layer becomes a middle barrier layer; wherein under the same wet etching condition, the etching rate of the middle barrier layer is smaller than the etching rate of the initial barrier layer, and under the same dry etching condition, the etching rate of the middle barrier layer is equal to the etching rate of the initial barrier layer; and removing the substrate between the adjacent conductive columns and a part of the middle barrier layer, the remaining middle barrier layer forming a target barrier layer, and the thickness of the target barrier layer being within a preset thickness range. The preparation method not only can improve the film quality of the target barrier layer, but also can improve the short circuit phenomenon in the bit line contact structure, thereby improving the yield of semiconductor products.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of semiconductor manufacturing technology, and in particular to a semiconductor structure and a preparation method thereof. Background Art

[0002] In integrated circuit manufacturing, DRAM (Dynamic Random Access Memory) has the advantages of high integration, low power consumption, and low price, so it is widely used in large-capacity storage. With the continuous increase in integration in semiconductor manufacturing processes, improving the integration density of memory has become a trend.

[0003] However, as the characteristic size of semiconductor structures continues to shrink, the bit line contact structure in the memory is prone to short circuit. Therefore, it is urgent to provide a semiconductor structure and a preparation method thereof to avoid the short circuit phenomenon caused by the poor preparation process of the bit line contact and improve the film quality in the bit line contact structure, thereby improving the yield of the memory. Summary of the invention

[0004] The present disclosure provides a semiconductor structure and a preparation method thereof, so as to optimize the preparation process of a bit line contact structure in a dynamic memory, avoid or improve the short circuit phenomenon of the memory structure caused by a poor preparation process and improve the film quality in the bit line contact structure, thereby reducing the product rework rate and improving the yield of the dynamic memory.

[0005] According to some embodiments, one aspect of the present disclosure provides a method for preparing a semiconductor structure, including: providing a substrate, on which conductive pillars arranged at intervals along a first direction are formed; introducing a reaction precursor into a gap between adjacent conductive pillars to form an initial barrier layer on the outer wall of the conductive pillars; introducing a preset process gas into the gap to change the initial barrier layer into an intermediate barrier layer; wherein, under the same wet etching conditions, the etching rate of the intermediate barrier layer is less than the etching rate of the initial barrier layer, and under the same dry etching conditions, the etching rate of the intermediate barrier layer is equal to the etching rate of the initial barrier layer; removing the substrate and part of the intermediate barrier layer between adjacent conductive pillars, the remaining intermediate barrier layer constitutes a target barrier layer, and the thickness of the target barrier layer is within a preset thickness range.

[0006] In the method for preparing the semiconductor structure described in the above embodiment, the initial barrier layer is first formed by reacting different reaction precursors under certain process conditions. Since the reaction precursors contain multiple elements and the deposition process introduces impurities into the film, the initial barrier layer contains more impurities in addition to the main material, and there are more reaction by-products in the reaction chamber, which will affect the yield of the subsequent etching and deposition process. If the initial barrier layer is directly retained as a barrier layer structure, when the excess material at the bottom of the gap is etched before the gap is filled, the initial barrier layer containing impurities will be partially etched away, and the initial barrier layer containing impurities has a faster etching rate in wet etching, and will be etched away in large quantities, thereby exposing the conductive pillars, causing the formed memory structure to short-circuit. Therefore, after forming the initial barrier layer, the present invention introduces a preset process gas into the gap so that the initial barrier layer becomes an intermediate barrier layer, thereby reducing impurities in the initial barrier layer to reduce its wet etching rate, and the preset process gas can also remove the reaction byproducts remaining in the reaction chamber. In the subsequent wet etching process, the etching rate of the intermediate barrier layer slows down, and a certain film thickness can be retained, and the conductive pillars will not be exposed or the blocking effect will be deteriorated. The intermediate barrier layer remaining after etching constitutes the target barrier layer. Due to the improvement of the preparation process disclosed in the present invention, the thickness of the target barrier layer can be guaranteed to be within the preset thickness range. When the gap is filled later, the target barrier layer can well block the filling material so that it does not contact the material in the conductive pillar, thereby avoiding or improving the short circuit phenomenon in the semiconductor structure, avoiding the generation of large currents, and avoiding mechanical damage to electronic components or even devices, thereby improving the quality of semiconductor products.

[0007] In some of the embodiments, a preset process gas is introduced into the gap to change the initial barrier layer into an intermediate barrier layer, including: introducing a preset process gas into the gap, the preset process gas reacting with impurity ions in the initial barrier layer to at least remove a portion of the impurity ions in the initial barrier layer to change the initial barrier layer into an intermediate barrier layer.

[0008] In some of the embodiments, the predetermined process gas reacts with the impurity ions in the initial barrier layer to generate the target gas.

[0009] In some embodiments, the impurity ions include chloride ions, the preset process gas includes diborane, and the target gas includes boron trichloride gas and hydrogen chloride gas.

[0010] In some embodiments, the preset supply flow rate of the process gas is 0.7 slm to 0.9 slm.

[0011] In some embodiments, the preset supply time of the process gas is 1 second to 3 seconds.

[0012] In some embodiments, the material of the initial barrier layer includes one or more of silicon nitride, silicon oxynitride, and silicon carbide nitride.

[0013] In some embodiments, the material of the intermediate barrier layer includes one or more of silicon nitride, silicon oxynitride and silicon carbide nitride.

[0014] In some embodiments, the material of the target barrier layer includes one or more of silicon nitride, silicon oxynitride, and silicon carbide nitride.

[0015] In some of the embodiments, the process of forming the initial barrier layer includes an atomic layer deposition process.

[0016] In some of these embodiments, the reactive precursor includes a silicon-containing precursor and a nitrogen-containing precursor.

[0017] In some embodiments, the silicon-containing precursor includes dichlorosilane, and the nitrogen-containing precursor includes ammonia.

[0018] In some of the embodiments, the temperature of the atomic layer deposition process is 620° C. to 640° C.

[0019] In some embodiments, the supply flow rate of dichlorosilane is 0.7 slm to 0.9 slm, and the supply flow rate of ammonia is 9 slm to 11 slm.

[0020] In some of the embodiments, the pressure valve state of the atomic layer deposition process is fully open.

[0021] In some of the embodiments, after introducing the reaction precursor into the gap between adjacent conductive pillars and before introducing the preset process gas into the gap, it also includes: introducing a cleaning gas into the reaction chamber and simultaneously pumping the cleaning gas to remove reaction byproducts near the surface of the initial barrier layer.

[0022] In some embodiments, the cleaning gas includes nitrogen.

[0023] In some embodiments, the cleaning gas is supplied for a time period of 1 second to 3 seconds.

[0024] In some of these embodiments, the reaction byproduct includes ammonium chloride.

[0025] According to some embodiments, the present disclosure further provides a semiconductor structure comprising a preparation method described in any one of the embodiments of the present disclosure, comprising a substrate and a target barrier layer. The substrate is provided with conductive pillars arranged at intervals along a first direction; the target barrier layer is located on the outer side wall of the conductive pillar, and the thickness of the target barrier layer is within a preset thickness range.

[0026] In the semiconductor structure described in the above embodiments, the target blocking layer is located on the outer wall of the conductive column and its thickness is within a preset thickness range, which can ensure that the filling material between adjacent conductive columns does not contact the material in the conductive column, and prevent the grains of the filling material from entering the conductive column to cause a short circuit. In addition, the film quality and uniformity of the target blocking layer are improved to improve the yield of the semiconductor structure and reduce the product rework rate.

[0027] In some of these embodiments, the conductive pillar comprises a bit line pillar.

[0028] In some embodiments, the bit line pillar includes a bit line contact plug, a bit line conductive layer, and a bit line protection layer which are sequentially stacked in a direction away from the substrate.

[0029] In some embodiments, the material of the bit line contact plug includes polysilicon and / or doped polysilicon.

[0030] In some embodiments, the material of the bit line conductive layer includes one or more of titanium, tungsten, cobalt, nickel, tantalum, tantalum titanium, tungsten silicide and tungsten nitride.

[0031] In some embodiments, the material of the bit line protection layer includes one or more of silicon nitride, silicon oxynitride and silicon carbide nitride. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] In order to more clearly illustrate the technical solutions of the embodiments of the present disclosure, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present disclosure. For ordinary technicians in this field, drawings of other embodiments can be obtained based on these drawings without creative work.

[0033] Figure 1 A schematic diagram of a process for preparing a semiconductor structure provided in an embodiment of the present disclosure;

[0034] Figure 2-Figure 4 It is a schematic structural cross-sectional diagram of each step of a method for preparing a semiconductor structure provided in an embodiment of the present disclosure;

[0035] Figure 5 A schematic flow chart of a method for preparing a semiconductor structure provided in another embodiment of the present disclosure;

[0036] Figure 6-Figure 7 A schematic diagram of the relationship between the supply flow rate of different gases and time in a method for preparing a semiconductor structure provided in different embodiments of the present disclosure;

[0037] Figure 8-Figure 13A schematic diagram of a chemical reaction process of particles in each step of a method for preparing a semiconductor structure provided in different embodiments of the present disclosure;

[0038] Fig.14 A schematic cross-sectional view of a semiconductor structure provided in one embodiment of the present disclosure;

[0039] Fig.15 A schematic diagram of the etching rate of a barrier layer in a different semiconductor structure provided in an embodiment of the present disclosure.

[0040] Description of reference numerals:

[0041] 10. Substrate; 11. Conductive pillar; 111. Bit line contact plug; 112. Bit line conductive layer; 113. Bit line protection layer; 12. Initial barrier layer; 13. Intermediate barrier layer; 14. Target substrate; 15. Target barrier layer. DETAILED DESCRIPTION

[0042] In order to facilitate the understanding of the present disclosure, the present disclosure will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present disclosure are given in the drawings. However, the present disclosure can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the present disclosure more thorough and comprehensive.

[0043] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present disclosure. The terms used herein in the specification of the present disclosure are only for the purpose of describing specific embodiments and are not intended to limit the present disclosure. The term "and / or" used herein includes any and all combinations of one or more related listed items.

[0044] In the case of using “including”, “having”, and “comprising” described herein, another component may be added unless a clear limiting term such as “only”, “consisting of”, etc. is used. Unless mentioned otherwise, a term in the singular form may include a plural form and should not be construed as being one in number.

[0045] Memory is a memory component used to store programs and various data information. According to the type of memory used, it can be divided into ROM (Read-Only Memory) and RAM (Random Access Memory). According to the working principle of the storage unit, random access memory is divided into SRAM (Static RAM) and DRAM. DRAM is a semiconductor memory. Its main working principle is to use the amount of charge stored in the capacitor to represent whether a binary bit is 1 or 0. Compared with SRAM, the advantage of DRAM is its simple structure - each bit of data only needs one capacitor and one transistor to process. In contrast, one bit on SRAM usually requires six transistors. Therefore, DRAM has a very high density and a higher capacity per unit volume. Compared with SRAM, DRAM has the advantages of high integration, low power consumption, and low price, so it is widely used in large-capacity memory. With the integration and reduction in size of memories such as DRAM, the density of the circuit structure inside the memory is gradually increasing. The increase in density will cause the line width of the metal wires forming the circuit structure and the spacing between two adjacent metal wires to gradually decrease. When the size of the semiconductor is reduced, although the degree of integration is better and the performance is stronger, the defects of the small-sized semiconductor structure produced during the manufacturing process, even if they are very small, will have a significant impact on the performance of the semiconductor.

[0046] In the structure of a dynamic memory, it usually includes a capacitor and a transistor connected to the capacitor. The capacitor is used to store charges representing the stored information, and the transistor is a switch that controls the inflow and release of charges in the capacitor. When writing data, the word line gives a high level, the transistor is turned on, and the bit line charges the capacitor. When reading, the word line also gives a high level, the transistor is turned on, the capacitor is discharged, and the bit line obtains a read signal. As the characteristic size of the semiconductor structure continues to shrink, the silicon nitride film in the traditional technology is used as a barrier layer for the bit line structure. It is used as an etching barrier material when the gap filling material between adjacent bit line contact structures is used to prevent the gap filling material from penetrating into the bit line contact structure and causing a short circuit. Therefore, it is necessary to ensure that the barrier layer has sufficient thickness. However, in the process of preparing the traditional barrier layer, the barrier layer formed contains more impurities and has poor film uniformity. Before the subsequent gap filling material is deposited between adjacent bit line structures, the excess substrate material and barrier layer material at the bottom of the gap need to be wet-etched. At this time, the barrier layer located on the side wall surface of the conductive column is exposed in the gap and contacts the wet-etched material. Due to the large amount of impurities in the barrier layer, the insufficient proportion of silicon nitride material and the loose film structure, the wet etching will etch away a large part of the barrier layer, so that the barrier layer becomes thinner and even exposes the surface of the bit line structure, or the thickness of the barrier layer is not enough to achieve the blocking effect. Therefore, when filling the gap material, the gap material is easy to contact the bit line structure through the barrier layer after deposition, resulting in a short circuit, which reduces the yield of the dynamic memory.

[0047] Based on the above technical problems, the present disclosure provides a semiconductor structure and a preparation method thereof to optimize the preparation process of the bit line contact structure in the dynamic memory, prevent the defect of the bit line contact structure short-circuited due to excessive etching of the barrier layer, avoid or improve the device damage caused by the short circuit phenomenon in the memory structure, and improve the quality of the film in the bit line contact structure, thereby reducing the product rework rate and improving the yield of the dynamic memory.

[0048] As an example, see Figure 1 One aspect of the present disclosure provides a method for preparing a semiconductor structure, comprising:

[0049] Step S2: providing a substrate, on which conductive columns are formed and arranged at intervals along a first direction;

[0050] Step S4: introducing a reaction precursor into the gap between adjacent conductive pillars to form an initial barrier layer on the outer sidewalls of the conductive pillars;

[0051] Step S6: introducing a preset process gas into the gap so that the initial barrier layer becomes an intermediate barrier layer; wherein, under the same wet etching conditions, the etching rate of the intermediate barrier layer is less than the etching rate of the initial barrier layer, and under the same dry etching conditions, the etching rate of the intermediate barrier layer is equal to the etching rate of the initial barrier layer;

[0052] Step S8: removing the substrate and part of the intermediate barrier layer between adjacent conductive pillars, and the remaining intermediate barrier layer constitutes a target barrier layer, and the thickness of the target barrier layer is within a preset thickness range.

[0053] As an example, the first direction may be the ox direction, and the second direction may be the oy direction. In other embodiments, the first direction may also be the oy direction, and the second direction may also be the ox direction.

[0054] In step S2, see Figure 1 Step S2 and Figure 2 The conductive pillar 11 may include a bit line pillar, and the bit line pillar may include a bit line contact plug 111 , a bit line conductive layer 112 , and a bit line protection layer 113 sequentially stacked in a direction away from the substrate 10 .

[0055] As an example, in step S2, conductive pillars 11 arranged at intervals along a first direction (eg, ox direction) are formed on the substrate 10, wherein the conductive pillars 11 may be bit line pillars, and the following steps may be included:

[0056] Step S21: forming a plurality of discrete bit line contact plugs on the top of the substrate, wherein the bit line contact plugs are in contact with the substrate thereunder (such as the active region directly thereunder), and the bottom surface of the bit line contact plugs may be lower than the top surface of the substrate;

[0057] Step S22: forming a bit line conductive layer and a bit line protection layer in sequence on the top of the bit line contact plug, and the stacked bit line contact plug, the bit line conductive layer and the bit line protection layer together constitute a bit line pillar.

[0058] As an example, the material of the bit line contact plug 111 includes polysilicon and / or doped polysilicon. The bit line contact plug 111 is used to connect the active area in the substrate 10 and the bit line conductive layer 112, and its filling material can be the same as the filling material of the gap between adjacent bit line pillars.

[0059] As an example, the material of the bit line conductive layer 112 includes one or more of titanium, tungsten, cobalt, nickel, tantalum, tantalum titanium, tungsten silicide and tungsten nitride. Specifically, the material of the bit line conductive layer 112 can be a low resistance material such as tungsten or ruthenium to reduce resistance and increase the operating speed of the device.

[0060] As an example, the material of the bit line protection layer 113 includes one or more of silicon nitride, silicon oxynitride and silicon carbide. The preparation method of each part of the bit line pillar is common knowledge to those skilled in the art and will not be described in detail here.

[0061] As an example, the substrate 10 can be made of semiconductor material, insulating material, conductor material or any combination thereof. The substrate 10 can be a single-layer structure or a multi-layer structure. For example, the substrate 10 can be a III / V semiconductor substrate or a II / VI semiconductor substrate such as a silicon (Si) substrate, a silicon germanium (SiGe) substrate, a silicon germanium carbon (SiGeC) substrate, a silicon carbide (SiC) substrate, a gallium arsenide (GaAs) substrate, an indium arsenide (InAs) substrate, an indium phosphide (InP) substrate or other. Or, for example, the substrate 10 can be a layered substrate including Si / SiGe, Si / SiC, silicon on insulator (SOI) or silicon germanium on insulator. Those skilled in the art can select the type of substrate 10 according to the type of transistor formed on the substrate 10, so the type of substrate 10 should not limit the scope of protection of the present disclosure.

[0062] As an example, in an embodiment where the substrate 10 includes a P-type substrate, an active region may be formed by implanting N-type ions; correspondingly, in an embodiment where the substrate 10 includes an N-type substrate, an active region may be formed by implanting P-type ions. Accordingly, the active region may be a P-type active region or an N-type active region. The P-type active region may form an N-type metal oxide semiconductor (Negative channel Metal Oxide Semiconductor, referred to as NMOS) device, and the N-type active region may form a P-type metal oxide semiconductor (Positive channel Metal Oxide Semiconductor, referred to as PMOS) device.

[0063] As an example, P-type ions may include but are not limited to any one or more of boron (B) ions, gallium (Ga) ions, boron fluoride (BF2) ions, and indium (In) ions, and N-type impurity ions may include but are not limited to any one or more of phosphorus (P) ions, arsenic (As) ions, and antimony (Sb) ions.

[0064] In step S4, see Figure 1 Step S4 and Figure 2, a reaction precursor is introduced into the gap between adjacent conductive pillars 11 to form an initial barrier layer 12 on the outer sidewall of the conductive pillar 11, the initial barrier layer 12 extends along the second direction (for example, the oy direction) on the outer sidewall of the conductive pillar 11, and the initial barrier layer 12 is formed not only on the outer sidewall of the conductive pillar 11, but also on the bottom of the gap between adjacent conductive pillars 11, covering the top surface of the substrate 10. The initial barrier layer 12 generated in this step contains more impurities, so its wet etching rate is faster, it is easy to be etched too thin, the thickness is insufficient, and the barrier effect is poor.

[0065] In step S6, refer to Figure 1 Step S6 and Figure 3 , a preset process gas is introduced into the gap so that the initial barrier layer 12 is transformed into the intermediate barrier layer 13; wherein, under the same wet etching conditions, the etching rate of the intermediate barrier layer 13 is less than the etching rate of the initial barrier layer 12, and under the same dry etching conditions, the etching rate of the intermediate barrier layer 13 is equal to the etching rate of the initial barrier layer 12, so as to ensure the film thickness after the gap is subsequently wet-etched.

[0066] In step S8, refer to Figure 1 Step S8 and Figure 4 , the substrate 10 and part of the intermediate barrier layer 13 between adjacent conductive pillars 11 are removed, and the remaining intermediate barrier layer 13 constitutes a target barrier layer 15, and the thickness of the target barrier layer 15 is within a preset thickness range. Since the wet etching rate of the intermediate barrier layer 13 is reduced, when the rate of wet etching of the substrate at the bottom of the gap remains unchanged, the etching rate of the intermediate barrier layer 13 on the sidewall of the gap is reduced; after the wet etching is completed, the thickness of the target barrier layer 15 is within a preset thickness range, so as to serve as a barrier structure for the bit line contact plug 111, ensuring that the particles of the gap filling material penetrate into the inside of the bit line pillar, thereby improving the short circuit phenomenon of the bit line structure.

[0067] As an example, the etching material used for wet etching may include hydrofluoric acid (HF), which can react with the material of the intermediate barrier layer 13 at the bottom of the gap and the material of the substrate 10, thereby removing excess material at the bottom of the gap to facilitate subsequent filling of a new gap material layer. However, during the etching process, the etching material will contact the intermediate barrier layer 13 on the side wall of the gap, causing part of its volume to be etched away. Since the wet etching rate of the intermediate barrier layer 13 is relatively low, it can still maintain a certain thickness after wet etching, that is, the thickness of the target barrier layer 15 is within a preset thickness range, so as to ensure an effective blocking effect on the conductive pillars 11 and improve the operating rate of the semiconductor structure and the electrical performance of the semiconductor structure.

[0068] As an example, after forming the target barrier layer 15, a gap material layer can be filled in the gap between adjacent conductive pillars 11. The gap material layer at least fills the gap between adjacent conductive pillars 11. The gap material layer contacts the target barrier layer 15 to prevent it from penetrating into the interior of the conductive pillars 11 and causing a short circuit.

[0069] In the method for preparing the semiconductor structure described in the above embodiment, the initial barrier layer 12 is first formed by reacting different reaction precursors under certain process conditions. Due to the fact that the reaction precursors contain multiple elements and the deposition process introduces impurities into the film, the initial barrier layer 12 contains more impurities in addition to the main material, and there are more reaction byproducts in the reaction chamber, which will affect the yield of the subsequent process. If the initial barrier layer 12 is directly retained as a barrier layer structure, when the excess material at the bottom of the gap is etched before the gap is filled later, the initial barrier layer 12 containing impurities will be partially etched away, and the initial barrier layer 12 containing impurities has a faster etching rate in wet etching, and will be etched away in large quantities, thereby exposing the conductive pillars 11, causing the formed structure to short-circuit. Therefore, after the initial barrier layer 12 is formed, the present disclosure introduces a preset process gas into the gap so that the initial barrier layer 12 becomes an intermediate barrier layer 13, thereby reducing the impurities in the initial barrier layer 12 to reduce its wet etching rate, and can remove the residual reaction byproducts in the reaction chamber. In the subsequent wet etching process, the etching rate of the intermediate barrier layer 13 is slowed down, and a certain film thickness can be retained without exposing the conductive pillars 11. The intermediate barrier layer 13 remaining after etching constitutes the target barrier layer 15. Due to the improvement of the preparation process disclosed in the present invention, the thickness of the target barrier layer 15 can be ensured to be within a preset thickness range. When the gap is subsequently filled, the target barrier layer 15 can well block the filling material from contacting the material in the conductive pillars 11, thereby avoiding or improving the short circuit phenomenon in the semiconductor structure, avoiding the generation of large currents, and avoiding mechanical damage to electronic components or even devices, thereby improving the operating rate of the semiconductor structure and the electrical performance of the semiconductor structure, thereby improving the quality of semiconductor products.

[0070] As an example, see Figure 5 , introducing a preset process gas into the gap so that the initial barrier layer becomes an intermediate barrier layer, including:

[0071] Step S61: introducing a preset process gas into the gap, wherein the preset process gas reacts with the impurity ions in the initial barrier layer to remove at least a portion of the impurity ions in the initial barrier layer, so that the initial barrier layer becomes an intermediate barrier layer.

[0072] In step S61, refer to Figure 5In step S61, since the preset process gas can remove the residual reaction byproducts in the reaction chamber and the impurities in the initial barrier layer 12, the film quality of the intermediate barrier layer 13 is better than the film quality of the initial barrier layer 12, and the wet etching rate of the film is reduced.

[0073] As an example, the preset process gas reacts with the impurity ions in the initial barrier layer 12 to generate the target gas. The target gas can remove the impurity ions from the initial barrier layer 12, so that the impurity content in the intermediate barrier layer 13 is less than the impurity content in the initial barrier layer 12, thereby increasing the proportion of the main material in the intermediate barrier layer 13, improving the film quality, and reducing its wet etching rate.

[0074] As an example, the impurity ions include chlorine (Cl) ions, the preset process gas includes diborane (B2H6), and the target gas includes boron trichloride (BCl3) gas and hydrogen chloride (HCl) gas.

[0075] As an example, the preset supply flow rate of the process gas is 0.7 slm to 0.9 slm. Specifically, the preset supply flow rate of the process gas may be 0.7 slm, 0.75 slm, 0.8 slm, 0.85 slm or 0.9 slm, etc.

[0076] As an example, the preset supply time of the process gas is 1 s to 3 s. Specifically, the preset supply time of the process gas may be 1 s, 1.5 s, 2 s, 2.5 s or 3 s, etc.

[0077] As an example, the material of the initial barrier layer 12 includes one or more of silicon nitride, silicon oxynitride and silicon carbide nitride. The material of the initial barrier layer 12 also includes impurity ions such as chloride ions.

[0078] As an example, the material of the intermediate barrier layer 13 includes one or more of silicon nitride, silicon oxynitride and silicon carbide nitride. The content of impurity ions in the intermediate barrier layer 13 is less than the content of impurity ions in the initial barrier layer 12.

[0079] As an example, the material of the target barrier layer 15 includes one or more of silicon nitride, silicon oxynitride and silicon carbide nitride. The target barrier layer 15 has a thickness less than that of the intermediate barrier layer 13 and is within a preset thickness range to ensure its blocking effect on the bit line pillars.

[0080] As an example, the process of forming the initial barrier layer 12 includes an atomic layer deposition (ALD) process and the like. The ALD process can make the thickness of the initial barrier layer 12 obtained more uniform.

[0081] As an example, the reactive precursor includes a silicon-containing precursor and a nitrogen-containing precursor. The silicon-containing precursor provides silicon elements for chemical reaction, and the nitrogen-containing precursor provides nitrogen elements for chemical reaction to form the initial barrier layer 12 whose main material is silicon nitride.

[0082] As an example, the silicon-containing precursor includes dichlorosilane (SiH2Cl2), and the nitrogen-containing precursor includes ammonia (NH3). Since the silicon-containing precursor provides chloride ions for the reaction, and the chloride ions are located inside the initial barrier layer 12, the generation of impurity ions affects the quality of the silicon nitride film and the wet etching rate.

[0083] As an example, the temperature of the atomic layer deposition process is 620° C. to 640° C. Specifically, the temperature of the atomic layer deposition process can be 620° C., 625° C., 630° C., 635° C. or 640° C., etc., so that the atomic layer deposited thin film is more uniform and has better film quality.

[0084] As an example, the supply flow rate of dichlorosilane is 0.7slm to 0.9slm, and the supply flow rate of ammonia is 9slm to 11slm. Specifically, the supply flow rate of dichlorosilane can be 0.7slm, 0.75slm, 0.8slm, 0.85slm or 0.9slm, etc., and the supply flow rate of ammonia can be 9slm, 9.5slm, 10slm, 10.5slm or 11slm, etc. The chemical reaction formula of the reaction precursor in the gap is 3SiH2Cl2+10NH3→Si3N4+6NH4Cl+6H2.

[0085] By way of example, reaction byproducts include ammonium chloride (NH 4 Cl), hydrogen (H 2 ), and the like.

[0086] As an example, the pressure valve state of the atomic layer deposition process is fully open to release the pressure generated during the chemical reaction.

[0087] As an example, after the reaction precursor is introduced into the gap between adjacent conductive pillars 11 and before the preset process gas is introduced into the gap, the method further includes:

[0088] Step S5: introducing a cleaning gas into the reaction chamber and simultaneously pumping the cleaning gas to remove reaction byproducts near the surface of the initial barrier layer.

[0089] As an example, the cleaning gas includes nitrogen (N2). By introducing nitrogen into the reaction chamber and extracting the nitrogen using an air pump, the nitrogen can clean the relevant reaction by-products in the reaction chamber to ensure the normal progress of subsequent reaction processes.

[0090] As an example, the supply time of the cleaning gas is 1s to 3s. Specifically, the supply time of the cleaning gas can be 1s, 1.5s, 2s, 2.5s or 3s, etc. The cleaning gas is supplied in the gaps where the reaction precursors are circulated successively to clean up the reaction by-products.

[0091] As an example, see Figure 6 In the conventional process, during the process of forming a barrier layer on the side wall of the bit line pillar by atomic layer deposition, the silicon-containing precursor used for atomic layer deposition of silicon nitride film is dichlorosilane. The presence of chlorine in the silicon nitride film makes the film quality of the silicon nitride film poor, so that the etching rate is too high during the wet etching process, and the thickness of the film is thin, which leads to short-circuit defects of the bit line contact. First, during the time 0-t1, dichlorosilane is introduced to provide silicon elements and introduce chloride ion impurities. Then, during the time t1-t2, nitrogen is introduced to purge the excess dichlorosilane. During the time t2-t3, ammonia is continued to be introduced to provide nitrogen elements and form a silicon nitride film on the surface of the bit line pillar. During the time t3-t4, nitrogen is continued to be introduced to purge the excess reaction precursors and reaction by-products; and the steps 0-t4 are repeated until the deposition of the silicon nitride film is completed. The silicon nitride film formed under this deposition process contains more impurities and the film quality is poor.

[0092] As an example, see Figure 7 In the preparation method provided by the present disclosure, during the process of forming the target barrier layer 15 on the sidewall of the bit line pillar by atomic layer deposition, the temperature of the atomic layer deposition process is 620° C. to 640° C. Specifically, the temperature of the atomic layer deposition process can be 620° C., 625° C., 630° C., 635° C. or 640° C., etc., the reaction precursors can be dichlorosilane and ammonia, and the preset process gas can be diborane gas.

[0093] During the time 0-t1', see Figure 7 and Figure 8 First, dichlorosilane is introduced into the gap between adjacent bit line pillars to provide silicon elements, but chloride ion impurities are also introduced in this step. The supply flow rate of dichlorosilane is 0.7slm to 0.9slm. Specifically, the supply flow rate of dichlorosilane can be 0.7slm, 0.75slm, 0.8slm, 0.85slm or 0.9slm, etc.

[0094] During the time t1'-t2', see Figure 7 and Fig. 9 Then, nitrogen gas is introduced to purge the excess dichlorosilane to ensure that no excess dichlorosilane gas remains in the gap and only the dichlorosilane gas on the surface of the gap sidewall is retained.

[0095] During the time period t2'-t3', please continue to refer to Figure 7 , Fig. 9 and Fig.10 , continue to introduce ammonia gas to provide nitrogen elements, and deposit a silicon nitride film on the surface of the conductive pillar 11 to form an initial barrier layer 12, wherein the main material of the initial barrier layer 12 is silicon nitride, but the silicon nitride film contains more chloride ion impurities. The supply flow rate of ammonia gas is 9slm to 11slm, specifically, the supply flow rate of ammonia gas can be 9slm, 9.5slm, 10slm, 10.5slm or 11slm, etc.

[0096] In the above steps, the chemical reaction formula of the reaction precursor in the gap is 3SiH2Cl2+10NH3→Si3N4+6NH4Cl+6H2, and the excess reaction by-products and ammonia exist in the reaction chamber in the form of gas.

[0097] During the time period t3'-t4', see Figure 7 and Fig.11 , and then continue to introduce nitrogen, the supply time of nitrogen is 1s to 3s; specifically, the supply time of nitrogen can be 1s, 1.5s, 2s, 2.5s or 3s, etc., and at the same time, the nitrogen is sucked by an air pump to form an airflow in the reaction chamber to purge excess reaction precursors and reaction by-products such as NH4Cl, and remove reaction by-products on the surface of the initial barrier layer 12 to avoid reaction with the subsequently introduced diborane gas to cause gas loss, so as to enhance the effect of the subsequently introduced diborane gas.

[0098] During the period t4'-t5', see Figure 7 and Fig.12 , diborane gas is introduced, which reacts with the chloride ions in the initial barrier layer 12 to generate a target gas, thereby forming an intermediate barrier layer 13, wherein the chloride ion content in the intermediate barrier layer 13 is less than the chloride ion content in the initial barrier layer 12, wherein the target gas can be boron trichloride (BCl3) gas and hydrogen chloride (HCl) gas.

[0099] During the time period t5'-t6', see Figure 7 and Fig.13 , nitrogen gas is introduced to remove the target gas and excess diborane gas, which can effectively reduce the chloride ion content in the silicon nitride film to optimize the film quality, so that the initial barrier layer 12 gradually changes into the intermediate barrier layer 13, thereby reducing the wet etching rate and avoiding the short circuit defect of the bit line contact plug 111.

[0100] After the steps 0 to t6' are completed, the steps 0 to t6' are continuously repeated until the deposition of the silicon nitride film is completed. At this time, the impurity content in the intermediate barrier layer 13 is reduced, the film quality is better, and the wet etching rate is lower.

[0101] It should be understood that, although the various steps in the flowchart of the present disclosure are displayed in sequence according to the indication of the arrows, these steps are not necessarily executed in sequence according to the order indicated by the arrows. Unless there is a clear description in this article, there is no strict order restriction on the execution of these steps, and these steps can be executed in other orders. Moreover, although at least a part of the steps in the present disclosure may include multiple steps or multiple stages, these steps or stages are not necessarily executed at the same time, but can be executed at different times, and the execution order of these steps or stages is not necessarily to be carried out in sequence, but can be executed in turn or alternately with other steps or at least a part of the steps or stages in other steps.

[0102] As an example, see Fig.14 The present disclosure also provides a semiconductor structure including any one of the preparation methods described in the embodiments of the present disclosure, including a substrate 10 and a target barrier layer 15. The substrate 10 is provided with conductive pillars 11 arranged at intervals along a first direction; the target barrier layer 15 is located on the outer side wall of the conductive pillars 11, and the thickness of the target barrier layer 15 is within a preset thickness range.

[0103] In the semiconductor structure described in the above embodiment, the target barrier layer 15 is located on the outer wall of the conductive column 11 and its thickness is within a preset thickness range, which can ensure that the filling material between adjacent conductive columns 11 does not contact the material in the conductive column 11, and prevent the grains of the filling material from entering the conductive column 11 to cause a short circuit. In addition, the film quality and uniformity of the target barrier layer 15 are improved to improve the yield of the semiconductor structure and reduce the product rework rate.

[0104] As an example, the conductive pillar 11 may include a bit line pillar.

[0105] As an example, the bit line pillar may include a bit line contact plug 11 bit line pillar; 111, a bit line conductive layer 112 and a bit line protection layer 113 sequentially stacked in a direction away from the substrate 10. The bit line contact plug 11 bit line pillar; 111 is in contact with the substrate 10 below it (such as the active area directly below it), and the bottom surface of the bit line contact plug 11 bit line pillar; 111 may also be lower than the top surface of the substrate 10. The bit line contact plug 111 is used to connect the active area in the substrate 10 and the bit line conductive layer 112, and its filling material may be the same as the filling material of the gap between adjacent bit line pillars.

[0106] As an example, the material of the bit line contact plug 111 includes polysilicon and / or doped polysilicon.

[0107] As an example, the material of the bit line conductive layer 112 includes one or more of titanium, tungsten, cobalt, nickel, tantalum, tantalum titanium, tungsten silicide and tungsten nitride. Specifically, the material of the bit line conductive layer 112 can be a low resistance material such as tungsten or ruthenium to reduce resistance and increase the operating speed of the device.

[0108] As an example, the material of the bit line protection layer 113 includes one or more of silicon nitride, silicon oxynitride, and silicon nitride carbide.

[0109] As an example, see Fig.15 , the first group is the etching rate of the initial barrier layer 12, the wet etching rate is 12.25nm / min, the dry etching rate is 34.51nm / min, and the second group is the etching rate of the intermediate barrier layer 13, the wet etching rate is 11.44nm / min, and the dry etching rate is 34.45nm / min. It can be seen that after reducing the content of chloride ion impurities in the intermediate barrier layer 13, the wet etching rate of the intermediate barrier layer 13 is significantly reduced, while the dry etching rate is almost unchanged. Therefore, when the intermediate barrier layer 13 is wet-etched, the etching rate is reduced, and the etched volume is reduced, thereby ensuring that the thickness of the target barrier layer 15 obtained is within the preset thickness range, so as to serve as a barrier layer for the sidewall of the bit line pillar, thereby avoiding short circuit of the bit line contact plug 111, so as to improve the yield of the memory device, reduce the rework rate, and thus reduce the preparation cost of the semiconductor structure and improve its preparation efficiency.

[0110] In the semiconductor structure and preparation method thereof in the above-mentioned embodiment, an initial barrier layer containing impurity ions is first formed between adjacent conductive pillars, and then a preset process gas is introduced to remove the impurity ions in the initial barrier layer to form an intermediate barrier layer with a lower wet etching rate, so as to ensure that when the gap bottom material between adjacent conductive pillars is wet-etched, the etching rate of the intermediate barrier layer is low and the etched volume is small, thereby forming a target barrier layer with a thickness within a preset thickness range, which can prevent the gap material layer from penetrating into the interior of the conductive pillar, thereby avoiding short circuit of the conductive pillar, thereby improving the preparation yield of the semiconductor structure, avoiding the generation of large current to avoid mechanical damage to electronic components or even devices, thereby improving the operating rate of the semiconductor structure and the electrical performance of the semiconductor structure, and further improving the quality of semiconductor products.

[0111] Please note that the above embodiments are for illustrative purposes only and are not meant to limit the present disclosure.

[0112] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.

[0113] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0114] The above-mentioned embodiments only express several implementation methods of the present disclosure, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the disclosed patent. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present disclosure, and these all belong to the protection scope of the present disclosure. Therefore, the protection scope of the disclosed patent shall be subject to the attached claims.

Claims

1. A method for preparing a semiconductor structure, characterized in that: include: Providing a substrate, on which conductive columns are formed and arranged at intervals along a first direction; Introducing a reaction precursor into the gap between adjacent conductive pillars to form an initial barrier layer on the outer sidewalls of the conductive pillars; A preset process gas is introduced into the gap so that the initial barrier layer becomes an intermediate barrier layer; wherein, under the same wet etching conditions, the etching rate of the intermediate barrier layer is less than the etching rate of the initial barrier layer, and under the same dry etching conditions, the etching rate of the intermediate barrier layer is equal to the etching rate of the initial barrier layer; The substrate and part of the intermediate barrier layer between adjacent conductive pillars are removed, and the remaining intermediate barrier layer constitutes a target barrier layer, and the thickness of the target barrier layer is within a preset thickness range.

2. The method for preparing a semiconductor structure according to claim 1, characterized in that: Introducing a preset process gas into the gap so that the initial barrier layer becomes an intermediate barrier layer, comprising: A preset process gas is introduced into the gap, and the preset process gas reacts with the impurity ions in the initial barrier layer to remove at least a portion of the impurity ions in the initial barrier layer, so that the initial barrier layer becomes an intermediate barrier layer.

3. The method for preparing a semiconductor structure according to claim 2, characterized in that: The preset process gas reacts with the impurity ions in the initial barrier layer to generate a target gas.

4. The method for preparing a semiconductor structure according to claim 3, characterized in that: The impurity ions include chloride ions, the preset process gas includes diborane, and the target gas includes boron trichloride gas and hydrogen chloride gas.

5. The method for preparing a semiconductor structure according to claim 4, characterized in that: The preset supply flow rate of the process gas is 0.7slm to 0.9slm; and / or The preset supply time of the process gas is 1s to 3s.

6. The method for preparing a semiconductor structure according to any one of claims 1 to 5, characterized in that: Includes at least one of the following features: The material of the initial barrier layer includes one or more of silicon nitride, silicon oxynitride and silicon carbide nitride; The material of the intermediate barrier layer includes one or more of silicon nitride, silicon oxynitride and silicon carbide nitride; The material of the target barrier layer includes one or more of silicon nitride, silicon oxynitride and silicon carbide nitride.

7. The method for preparing a semiconductor structure according to any one of claims 1 to 5, characterized in that: Includes at least one of the following features: The process of forming the initial barrier layer includes an atomic layer deposition process; The reaction precursors include a silicon-containing precursor and a nitrogen-containing precursor.

8. The method for preparing a semiconductor structure according to claim 7, characterized in that: The silicon-containing precursor includes dichlorosilane, and the nitrogen-containing precursor includes ammonia.

9. The method for preparing a semiconductor structure according to claim 8, characterized in that: Includes at least one of the following features: The temperature of the atomic layer deposition process is 620°C to 640°C; The supply flow rate of the dichlorosilane is 0.7slm to 0.9slm, and the supply flow rate of the ammonia is 9slm to 11slm; The pressure valve state of the atomic layer deposition process is fully open.

10. The method for preparing a semiconductor structure according to claim 9, characterized in that: After the reaction precursor is introduced into the gap between the adjacent conductive pillars and before the preset process gas is introduced into the gap, the method further includes: A cleaning gas is introduced into the reaction chamber and the cleaning gas is simultaneously pumped to remove reaction byproducts near the surface of the initial barrier layer.

11. The method for preparing a semiconductor structure according to claim 10, characterized in that: Includes at least one of the following features: The cleaning gas includes nitrogen; The supply time of the cleaning gas is 1s to 3s; The reaction byproducts include ammonium chloride.

12. A semiconductor structure comprising the preparation method according to any one of claims 1 to 11, characterized in that: include: A substrate, on which conductive columns are formed and arranged at intervals along a first direction; The target blocking layer is located on the outer side wall of the conductive column, and the thickness of the target blocking layer is within a preset thickness range.

13. The semiconductor structure according to claim 12, characterized in that: The conductive pillars include bit line pillars.

14. The semiconductor structure according to claim 13, characterized in that: The bit line pillar comprises a bit line contact plug, a bit line conductive layer and a bit line protection layer which are sequentially stacked in a direction away from the substrate.

15. The semiconductor structure according to claim 14, characterized in that: Includes at least one of the following features: The material of the bit line contact plug includes polysilicon and / or doped polysilicon; The material of the bit line conductive layer includes one or more of titanium, tungsten, cobalt, nickel, tantalum, tantalum titanium, tungsten silicide and tungsten nitride; The material of the bit line protection layer includes one or more of silicon nitride, silicon oxynitride and silicon carbide nitride.

Citation Information

Patent Citations

  • Manufacturing method of semiconductor memory

    CN112563207A

  • Semiconductor structure and manufacturing method thereof

    CN112864087A

  • Bit line structure manufacturing method, semiconductor structure manufacturing method and semiconductor structure

    CN114078775A

  • Method of forming bit-line in a semiconductor device

    KR1020070078183A

  • Semiconductor device and method of fabricating the same

    KR1020160025278A