Manufacturing method of semiconductor structure

By etching a specific trench structure on the semiconductor substrate and filling it with material, the problem of difficult control of gate and bit line positions in vertical transistors is solved, the integration level and unit characteristics of DRAM devices are improved, and the process steps are simplified.

CN118742033AActive Publication Date: 2024-10-01HANGZHOU HFC SEMICONDUCTOR CO
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202411204247.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2024-10-01
Estimated Expiration
2044-08-30

AI Technical Summary

Technical Problem

The existing method of forming vertical transistors is difficult to control the formation positions of gates and bit lines, and has many process steps, which affects the integration and cell characteristics of DRAM devices.

Method used

By forming a pad dielectric layer on a semiconductor substrate, etching to form a first trench and a second trench, depositing a pad layer, filling an isolation layer and a conductive material, and adjusting the trench depth and isolation layer height to control the gate position. and bitline gaps, precisely defining where conductive material is filled.

Benefits of technology

It achieves precise control of the gate formation position, reduces process steps, improves the isolation effect of bit lines and reduces parasitic capacitance, and improves the integration and cell characteristics of DRAM devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118742033A_ABST
    Figure CN118742033A_ABST
Patent Text Reader

Abstract

The invention provides a manufacturing method of a semiconductor structure, which comprises the following steps of: providing a substrate, and forming a pad dielectric layer on the substrate; the pad dielectric layer and the substrate are sequentially etched to form a first groove and a second groove, the first groove vertically and downwards extends into the substrate from the surface of the pad dielectric layer, the second groove downwards extends from the bottom of the first groove, and the groove width of the second groove gradually changes from the top to the bottom; depositing a liner layer on the inner surface of the first groove; filling the bottom of the second groove with an isolation layer; grooves are formed in the two sides of the second groove respectively; and filling the grooves with a conductive material. Therefore, the forming height of the liner layer and the forming positions of the bottom isolation layer and the groove can be accurately controlled without multiple steps, and the size of an air gap used for isolating conductive materials can be conveniently adjusted, so that the isolation effect and parasitic capacitance between bit lines reach a target balance point.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a method for manufacturing a semiconductor structure. Background Art

[0002] A DRAM cell transistor of a dynamic random access memory (DRAM) device may be electrically connected to a DRAM cell capacitor through a storage node contact plug, and the storage node contact plug is disposed between the source region of the DRAM cell transistor and the bottom electrode of the DRAM cell capacitor. In addition, the drain region of the DRAM cell transistor may be electrically connected to the bit line through a bit line contact plug, and the gate electrode of the DRAM cell transistor may be electrically connected to the word line. Therefore, the bit line and the word line for transmitting electrical signals may be disposed between the DRAM cell transistor and the DRAM cell capacitor. Therefore, due to the presence of the bit line and the word line, there may be certain restrictions on increasing the cell capacitance value. Moreover, most DRAM cell transistors may be formed to have a planar structure. In this case, if the width of the word line is reduced to increase the integration of the DRAM device, the resistance of the word line may be increased. As a result, the RC delay time of the word line may be increased and the performance of the DRAM device may be reduced. In addition, if the planar cell transistor is scaled down, the leakage current of the planar cell transistor may suddenly increase and reduce the cell characteristics of the DRAM device. Thus, it is proposed to solve or overcome the shortcomings of the planar transistor by a vertical transistor.

[0003] Figure 1 is a cross-sectional view showing a typical vertical transistor. Figure 1 As shown, the vertical transistor may be constructed to include a drain region 111 disposed in the lower side wall of the semiconductor substrate 110 and a source region 112 disposed in the upper side wall of the semiconductor substrate 110. A channel region 113 may be defined along the vertical direction between the drain region 111 and the source region 112, and a gate insulating layer 114 and a gate electrode 115 may be sequentially stacked on the side wall surface of the channel region 113. If the vertical transistor is used as a cell transistor of a DRAM device, the drain region 111 may be electrically connected to a bit line, and the source region 112 may be electrically connected to a storage node of a cell capacitor. In this case, the bit line may be buried in the lower portion of the semiconductor substrate 110. Therefore, the storage node may be freely disposed on the vertical transistor without the restriction of the bit line. That is, even if the integration of the DRAM device is increased, the use of the vertical transistor may prevent the cell capacitance value of the DRAM device from being reduced. In addition, since the bit line is buried in the semiconductor substrate 110, the parasitic capacitance value of the bit line may be reduced without reducing the quality of the cell capacitor, and the height of the storage node may also be reduced.

[0004] However, existing methods for forming vertical transistors have problems such as poor control of the positions of gate and bit lines, and often require many process steps to complete. Summary of the invention

[0005] An object of the present invention is to provide a method for manufacturing a semiconductor structure to solve one or more problems in the prior art.

[0006] In order to solve the above technical problems, the present invention provides a method for manufacturing a semiconductor structure, comprising: Providing a substrate and forming a pad dielectric layer on the substrate; The pad dielectric layer and the substrate are sequentially etched to form a first groove and a second groove, wherein the first groove vertically extends downward from the surface of the pad dielectric layer into the substrate, and the second groove extends downward from the bottom of the first groove, and the groove width of the second groove gradually changes from the top to the bottom; depositing a liner layer on an inner surface of the first trench; filling an isolation layer at the bottom of the second trench; forming grooves on both sides of the second groove respectively; and, Each of the grooves is filled with a conductive material.

[0007] Optionally, in the method for manufacturing the semiconductor structure, the second trench has a V-shaped longitudinal cross-section.

[0008] Optionally, in the method for manufacturing the semiconductor structure, the second trench has an inverted trapezoidal longitudinal cross-section.

[0009] Optionally, in the method for manufacturing the semiconductor structure, the second trench is obtained by etching using an anisotropic etching process.

[0010] Optionally, in the method for manufacturing the semiconductor structure, the etching solution used in the anisotropic etching process includes a potassium hydroxide solution or a tetramethylammonium hydroxide solution.

[0011] Optionally, in the method for manufacturing the semiconductor structure, the step of depositing the liner layer on the inner surface of the first trench includes: A liner layer is deposited on inner surfaces of the first trench and the second trench, and the liner layer on the inner surface of the second trench is removed.

[0012] Optionally, in the method for manufacturing the semiconductor structure, the step of filling the bottom of the second trench with an isolation layer includes: An isolation layer is filled in the first trench and the second trench, and the isolation layer is etched back so that the isolation layer is only filled in the bottom of the second trench.

[0013] Optionally, in the method for manufacturing a semiconductor structure, the conductive material is a metal silicide; The method of filling the two grooves with a conductive material comprises: Filling the first trench, the second trench and the two grooves in sequence with a metal material; Applying a heat treatment process to silicide the metal material in the groove to become metal silicide; The metal material in the first trench and the second trench is removed.

[0014] Optionally, in the method for manufacturing the semiconductor structure, a method for etching to form the first trench and the second trench includes: forming a hard mask layer, an anti-reflection layer and a photoresist layer in sequence on the pad dielectric layer; Patterning the photoresist layer, and sequentially etching the anti-reflection layer and the hard mask layer using the patterned photoresist layer as a mask to form an opening in the hard mask layer; Using the hard mask layer as a mask, sequentially etching the pad dielectric layer and the substrate along the opening to form the first trench and the second trench; and, The photoresist layer, the anti-reflective layer and the hard mask layer are removed.

[0015] Optionally, in the method for manufacturing the semiconductor structure, the pad dielectric layer includes a pad oxide layer and a pad nitride layer stacked in sequence from bottom to top.

[0016] In summary, the present invention provides a method for manufacturing a semiconductor structure, including: providing a substrate and forming a pad dielectric layer on the substrate; etching the pad dielectric layer and the substrate in sequence to form a first groove and a second groove, wherein the first groove extends vertically downward from the surface of the pad dielectric layer into the substrate, and the second groove extends downward from the bottom of the first groove, and the width of the second groove gradually changes from the top to the bottom; depositing a liner layer on the inner surface of the first groove; filling an isolation layer at the bottom of the second groove; forming grooves on both sides of the second groove respectively; and filling each of the grooves with a conductive material. By adopting the manufacturing method of the semiconductor structure provided by the present invention, the formation height of the liner layer can be accurately controlled by distinguishing the first groove and the second groove, so that the definition of the gate formation position can be completed without multiple steps, and the formation position of the bottom isolation layer and the groove for filling the conductive material can be accurately defined. In addition, by adopting the method provided by the present invention, it is convenient to adjust the depth of the second groove and / or the formation height of the bottom isolation layer to adjust the size of the air gap between the conductive materials (used as bit lines), so that the isolation effect and parasitic capacitance between the bit lines reach the target balance point. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1It is a schematic diagram of a part of the structure of a vertical transistor; Figure 2 A flowchart of the steps of the method for manufacturing the semiconductor structure provided by the present invention; Figure 3~Figure 12 for Figure 2 Schematic diagram of device structure corresponding to each step in the figure; The descriptions of the reference numerals are as follows: 110 - semiconductor substrate; 111 - drain region; 112 - source region; 113 - channel region; 114 - gate insulating layer; 115 - gate; 10-substrate; 20-pad dielectric layer; 30-hard mask layer; 40-antireflective layer; 50-photoresist layer; 60-liner layer; 70-isolation layer; 21- pad oxide layer; 22- pad nitride layer. DETAILED DESCRIPTION

[0018] The following is a further detailed description of the method for manufacturing the semiconductor structure provided by the present invention in conjunction with the accompanying drawings and specific embodiments. It should be noted that the drawings are all in a very simplified form and are all in an inaccurate scale, which is only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention. In addition, the structure shown in the drawings is often a part of the actual structure. In particular, the emphasis required to be shown in each drawing is different, and sometimes different scales are used. It should be recognized that relative terms such as "above", "below", "top", "bottom", "above" and "below" shown in the drawings can be used to describe the relationship between various elements. These relative terms are intended to cover different orientations of elements other than the orientations depicted in the drawings. For example, if the device is inverted relative to the view in the drawings, for example, an element described as "above" another element will now be below the element. It should also be understood that, unless otherwise specified or indicated, the terms "first", "second", "third" and the like in the specification are only used to distinguish between the various components, elements, steps, etc. in the specification, rather than to represent the logical relationship or sequential relationship between the various components, elements, steps, etc.

[0019] like Figure 2 As shown, an embodiment of the present invention provides a method for manufacturing a semiconductor structure, comprising the following steps: S1, providing a substrate, and forming a pad dielectric layer on the substrate; S2, sequentially etching the pad dielectric layer and the substrate to form a first groove and a second groove, wherein the first groove vertically extends downward from the surface of the pad dielectric layer into the substrate, and the second groove extends downward from the bottom of the first groove, and the groove width of the second groove gradually changes from the top to the bottom; S3, depositing a liner layer on the inner surface of the first groove; S4, filling an isolation layer at the bottom of the second trench; S5, laterally etching the substrate from the unfilled portion of the second trench to form grooves on both sides of the second trench; and S6, filling each of the grooves with a conductive material.

[0020] The following is combined with Figures 3 to 12 The method for manufacturing the semiconductor structure provided by the embodiment of the present invention is further described.

[0021] First, execute step S1, see Figure 3 and Figure 4 , a substrate 10 is provided, and a pad dielectric layer 20 is formed on the substrate 10 .

[0022] In this embodiment, the substrate 10 is a silicon substrate. In other embodiments, the material of the substrate 10 can also be other materials such as germanium, silicon germanium, silicon carbide, gallium arsenide or indium gallium, and the substrate 10 can also be other types of substrates 10 such as a silicon substrate 10 on an insulator or a germanium substrate 10 on an insulator. Optionally, the pad dielectric layer 20 includes a pad oxide layer (Pad Oxide) 21 and a pad nitride layer (Pad SiN) 22 stacked in sequence from bottom to top. The thickness of the pad oxide layer 21 and the pad nitride layer 22 can vary depending on the design of the structural process or the target trench depth, so as to protect the substrate and manufacture the desired pattern. In other embodiments, the pad dielectric layer 20 can be composed of oxides, nitrides, boron-containing oxides, polysilicon and combinations thereof.

[0023] Next, execute step S2, see Figure 5 and Figure 6 , the pad dielectric layer 20 and the substrate 10 are sequentially etched to form a first trench 101 and a second trench 102 .

[0024] The first trench 101 is a vertical trench extending vertically upward from the surface of the pad dielectric layer 20 into the substrate 10 , and the second trench 102 is a gradient trench extending downward from the bottom of the first trench 101 .

[0025] Optionally, a method for forming the first trench 101 and the second trench 102 includes: S21, such as Figure 3 As shown, a hard mask layer 30, an anti-reflection layer 40 and a patterned photoresist layer 50 are sequentially formed on the pad dielectric layer 20; S22, such as Figure 4As shown, the anti-reflection layer 40 and the hard mask layer 30 are sequentially etched using the patterned photoresist layer 50 as a mask to form an opening in the hard mask layer 30; S23, using the hard mask layer 30 as a mask, sequentially etching the pad dielectric layer 20 and the substrate 10 along the opening to form the first trench 101 and the second trench 102; and, S24 , removing the photoresist layer 50 , the anti-reflection layer 40 and the hard mask layer 30 .

[0026] The first groove 101 can be etched by an isotropic etching process, so that the first groove 101 is vertical. The isotropic etching process can be a dry etching process. For a silicon substrate, the dry etching process can include Cl 2 , HBr and SF 6 of mixed gases.

[0027] The second trench 102 is preferably obtained by etching using an anisotropic etching process. For the silicon substrate 10 , the etching solution used in the anisotropic etching process includes a potassium hydroxide (KOH) solution or a tetramethylammonium hydroxide (THAM) solution.

[0028] When the second trench 102 is formed by an anisotropic etching process, optionally, as Figure 5 As shown, the second groove 102 has a V-shaped longitudinal section, or, as shown Figure 6 As shown, the second trench 102 has an inverted trapezoidal longitudinal section, and can be etched along different crystal directions according to requirements so that the longitudinal section of the second trench 102 is V-shaped or inverted trapezoidal.

[0029] It should be noted that in the following description, for convenience, the relevant drawings illustrate that the second groove 102 has a V-shaped longitudinal section, but it should be understood that in all drawings, the longitudinal section of the second groove 102 is also an inverted trapezoidal shape.

[0030] Since the shapes of the second trench 102 and the first trench 101 are significantly different, and the second trench 102 and the first trench 101 have an obvious corner at their junction, the height of the liner layer subsequently formed on the inner surface of the first trench 101 can be accurately controlled, and when an isolation layer is subsequently formed at the bottom of the second trench and metal silicide is formed on both sides of the second trench, the formation positions of the isolation layer and the metal silicide can be accurately defined.

[0031] Next, execute step S3, see Figure 8 , depositing a liner layer 60 on the inner surface of the first trench 101; and performing step S4, see Fig.10 , an isolation layer 70 is filled at the bottom of the second trench 102 .

[0032] Specifically, the step of depositing the liner layer 60 on the inner surface of the first groove 101 includes: depositing the liner layer 60 on the inner surfaces of the first groove 101 and the second groove 102, and removing the liner layer 60 on the inner surface of the second groove 102, so that the liner layer 60 is only retained on the inner surface of the first groove 101. Since the longitudinal section of the second groove 102 is in an inverted trapezoidal or V-shaped shape, after the liner layer 60 is deposited on the inner surfaces of the first groove 101 and the second groove 102, the liner layer 60 on the inner surface of the second groove 102 can be removed. It can be seen that in the embodiment of the present invention, the distinction between the shapes of the second groove 102 and the first groove 101 is not only conducive to defining the subsequent formation positions of the isolation layer and the metal silicide, but also conducive to defining the formation position of the liner layer 60.

[0033] The liner layer 60 may be formed by a thermal oxidation process or a chemical vapor deposition process, and its material may be an oxide, such as silicon dioxide (SiO 2 ) and other materials. When the liner layer 60 is deposited on the inner surface of the first groove 101 and the second groove 102, the liner layer 60 may also extend to cover the surface of the pad dielectric layer 20. The liner layer 60 located on the surface of the pad dielectric layer 20 may be removed by a chemical mechanical polishing process, and the liner layer 60 deposited on the surface of the second groove 102 may be removed by a wet etching process.

[0034] The liner layer 60 is used as a gate insulating layer, and the formation height of the liner layer 60 is also the formation height of the subsequent gate. When forming the first trench 101 and the second trench 102 , the vertical etching depth can be determined according to the target height of the liner layer 60 .

[0035] Specifically, the step of filling the isolation layer 70 at the bottom of the second trench 102 includes: filling the isolation layer in the first trench 101 and the second trench 102 , and etching back the isolation layer 70 so that the isolation layer 70 is only filled at the bottom of the second trench 102 .

[0036] The liner layer 60 and the isolation layer 70 are made of different insulating materials. For example, in this embodiment, the liner layer 60 may be made of nitride, such as silicon nitride (SiN), and the isolation layer 70 may be made of oxide, such as silicon dioxide (SiO 2). When etching back the isolation layer 70, an etching gas having a higher etching rate for nitride than for nitride may be used for etching, so as to avoid etching the pad layer 60 during the etching back process. In some other embodiments, the pad layer 60 and the isolation layer 70 may also be made of other insulating materials. On this basis, an etching gas having a higher etching rate for the pad layer 60 than for the isolation layer 70 is selected to ensure that the pad layer 60 will not be etched during the etching back of the insulating material.

[0037] Since the first groove 101 and the second groove 102 have a corner at their junction, forming a distinct dividing line, the dividing line can be used as a reference when etching away the liner layer 60 on the inner surface of the second groove 102 and when etching back the isolation layer 70, thereby achieving precise control over the formation position of each layer.

[0038] The formation height of the liner layer 60 can be defined as needed. By controlling the height of the liner layer 60, the size of the remaining space of the second trench 102 can be controlled, and the remaining space of the second trench 102 is used as an air gap between subsequent isolation conductive materials (used as bit lines). By controlling the height of the liner layer 60, the size of the air gap is controlled so that the isolation effect and parasitic capacitance between the bit lines can reach a target balance point.

[0039] Then, execute step S5, see Fig.11 , forming grooves 103 on both sides of the second groove 102; and performing step S6, see Fig.12 , each of the grooves 103 is filled with a conductive material 70 .

[0040] The recess 103 is formed by laterally etching the portion of the second trench 102 that is not filled by the liner layer 60. The lateral etching may be performed by wet etching, and the reagent of the wet etching is, for example, phosphoric acid.

[0041] The conductive material 70 may be metal silicide, and the specific process of filling the conductive material 70 in each groove may be as follows: Filling metal material into the first trench 101 , the second trench 102 and the groove 103 ; Applying a heat treatment process to silicide the metal material in the groove 103 to become metal silicide; removing metal materials in the first groove 101 and the second groove 102; Specifically, the material of the metal material may be cobalt (Co), and correspondingly, the material of the metal silicide is (CoSi).

[0042] The metal silicide is used as a buried bit line. Since the metal silicide on both sides of the second trench 102 is isolated by the air in the second trench 102, the isolation effect can be improved and the parasitic capacitance can be reduced.

[0043] In addition, the manufacturing method of the semiconductor structure provided by the embodiment of the present invention may also include: forming a gate (not shown) in the second trench 102, and the gate can be formed by filling polysilicon material in the second trench 102; and forming a source region and a drain region (not shown) in the active region on both sides of the first trench 101 by ion implantation, the source region and the drain region are arranged in the active region with an upper and lower interval, the area between the source region and the drain region constitutes an active region, and the drain region is electrically connected to the metal silicide.

[0044] In summary, the manufacturing method of the semiconductor structure provided by an embodiment of the present invention includes: providing a substrate and forming a pad dielectric layer on the substrate; etching the pad dielectric layer and the substrate in sequence to form a first groove and a second groove, wherein the first groove extends vertically downward from the surface of the pad dielectric layer into the substrate, and the second groove extends downward from the bottom of the first groove, and the width of the second groove gradually changes from the top to the bottom; depositing a lining layer on the inner surface of the first groove; filling an isolation layer at the bottom of the second groove; forming grooves on both sides of the second groove respectively; and filling each of the grooves with a conductive material. By adopting the manufacturing method of the semiconductor structure provided by the embodiment of the present invention, the formation height of the liner layer can be accurately controlled by distinguishing the first trench and the second trench, so that the definition of the gate formation position can be completed without multiple steps, and the formation position of the bottom isolation layer and the groove for filling the conductive material can be accurately defined. In addition, by adopting the method provided by the present invention, it is convenient to adjust the depth of the second trench and / or the formation height of the bottom isolation layer to adjust the size of the air gap between the conductive materials (used as bit lines), so that the isolation effect and parasitic capacitance between the bit lines reach the target balance point.

[0045] In addition, it should be recognized that although the present invention has been disclosed as a preferred embodiment, the above embodiment is not intended to limit the present invention. For any technician familiar with the art, without departing from the scope of the technical solution of the present invention, the technical content disclosed above can be used to make many possible changes and modifications to the technical solution of the present invention, or modified into equivalent embodiments of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still belongs to the scope of protection of the technical solution of the present invention.

Claims

1. A method for manufacturing a semiconductor structure, characterized in that: include: Providing a substrate and forming a pad dielectric layer on the substrate; The pad dielectric layer and the substrate are sequentially etched to form a first groove and a second groove, wherein the first groove vertically extends downward from the surface of the pad dielectric layer into the substrate, and the second groove extends downward from the bottom of the first groove, and the groove width of the second groove gradually changes from the top to the bottom; depositing a liner layer on an inner surface of the first trench; filling an isolation layer at the bottom of the second trench; forming grooves on both sides of the second groove respectively; as well as, Each of the grooves is filled with a conductive material.

2. The method for manufacturing a semiconductor structure according to claim 1, wherein: The second groove has a V-shaped longitudinal section.

3. The method for manufacturing a semiconductor structure according to claim 1, wherein: The second groove has an inverted trapezoidal longitudinal section.

4. The method for manufacturing a semiconductor structure according to any one of claims 1 to 3, characterized in that: The second groove is etched by an anisotropic etching process.

5. The method for manufacturing a semiconductor structure according to claim 4, wherein: The etching solution used in the anisotropic etching process includes potassium hydroxide solution or tetramethylammonium hydroxide solution.

6. The method for manufacturing a semiconductor structure according to claim 1, wherein: The step of depositing the liner layer on the inner surface of the first trench comprises: A liner layer is deposited on inner surfaces of the first trench and the second trench, and the liner layer on the inner surface of the second trench is removed.

7. The method for manufacturing a semiconductor structure according to claim 1, wherein: The step of filling an isolation layer at the bottom of the second trench comprises: An isolation layer is filled in the first trench and the second trench, and the isolation layer is etched back so that the isolation layer is only filled in the bottom of the second trench.

8. The method for manufacturing a semiconductor structure according to claim 1, wherein: The conductive material is metal silicide; The method of filling the two grooves with a conductive material comprises: Filling the first trench, the second trench and the two grooves in sequence with a metal material; Applying a heat treatment process to silicide the metal material in the groove to become metal silicide; The metal material in the first trench and the second trench is removed.

9. The method for manufacturing a semiconductor structure according to claim 1, wherein: The method of etching to form the first trench and the second trench comprises: forming a hard mask layer, an anti-reflection layer and a photoresist layer in sequence on the pad dielectric layer; Patterning the photoresist layer, and sequentially etching the anti-reflection layer and the hard mask layer using the patterned photoresist layer as a mask to form an opening in the hard mask layer; Using the hard mask layer as a mask, sequentially etching the pad dielectric layer and the substrate along the opening to form the first trench and the second trench; and, The photoresist layer, the anti-reflective layer and the hard mask layer are removed.

10. The method for manufacturing a semiconductor structure according to claim 1, wherein: The pad dielectric layer includes a pad oxide layer and a pad nitride layer which are sequentially stacked from bottom to top.

Citation Information

Patent Citations

  • Method for forming buried bit line, semiconductor device having the same, and fabricating method thereof

    CN103165539A

  • A memory device and a method of manufacture that same

    CN109216359A

  • Forming method of semiconductor structure and semiconductor structure

    CN114068389A

  • Semiconductor device and forming method thereof

    CN115188708A

  • Vertical transistor and manufacturing method thereof

    CN115910784A