Compressor shell and manufacturing method thereof

By setting internal chamfers and tapers on the lower shell seam of the compressor, assembly difficulties and impurity problems are solved, production efficiency and product quality are improved, and mold wear resistance and welding effects are enhanced through TD processing.

CN118745986APending Publication Date: 2024-10-08WUHU ABAUR MECHANICAL & ELECTRICAL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410630940.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-21
Publication Date
2024-10-08

AI Technical Summary

Technical Problem

The lower shell of the existing compressor has no chamfers and tapers at the seam, which makes assembly difficult, prone to flash and flanged impurities, and affects production efficiency and product quality.

Method used

Set an internal chamfer and/or taper at the joint of the lower housing of the compressor, and form it through the punching process and punch pressing. Ensure that the depth of the internal chamfer is not less than 2mm, the angle is not less than 5°, and it is processed by TD. Improve the wear resistance and position accuracy of the mold.

Benefits of technology

It improves the orientation of the assembly of the compressor upper casing, reduces the entry of impurities, improves production efficiency and product quality, extends the service life of the mold, and enhances the welding strength and aesthetics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118745986A_ABST
    Figure CN118745986A_ABST
Patent Text Reader

Abstract

The compressor shell comprises an upper shell body and a lower shell body which are connected with each other, the lower shell body is provided with a lower shell seam allowance, the upper edge of the inner circumference of the lower shell seam allowance is provided with an inner chamfer and / or taper, the depth of the inner chamfer is not smaller than 2 mm, and the angle of the inner chamfer is not smaller than 5 degrees. By means of the arrangement, an assembly guide can be formed, the problem that the compressor is difficult to assemble in the upper shell assembling process is solved, spigot burrs are turned off in a pressing mode, subsequent inner chamfer or taper machining is not needed, burrs and flashes at the lower shell spigot can be removed in the mode, the lower shell spigot does not need to be specially polished and cleaned, and the production efficiency is improved. The production efficiency is improved, burrs and turnups which are not cleaned at the seam allowance of the lower shell can be prevented from falling into the compressor in the assembling process, potential quality hazards caused by impurities and the like are reduced, and the product quality and reliability are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of compressor production, and in particular to a compressor housing and a manufacturing method thereof. Background Art

[0002] At present, during the production process of the lower shell of a reciprocating piston compressor, there is generally no taper angle or taper guide end at the stop. The shell is formed by stamping. When the stop is peeled or trimmed, flash and flange will be generated at the stop. At the same time, during the assembly of the compressor, it is necessary to use external force to knock the upper shell to make the upper shell assembled in place. When subjected to external force, the flash and flange of the stop are easy to fall into the shell, forming impurities and causing the compressor to be stuck and completely fail. The lower shell of the existing compressor has no chamfer and no taper at the stop, which makes it difficult to assemble the compressor during the assembly process of the upper shell. The compressor even gets stuck on the assembly production line. After troubleshooting the stuck fault, solid impurities were found. After analyzing the shape and spectrum of the impurities, it was confirmed that the impurities were flash impurities generated by the stop of the lower shell. The existing shell stamping method generates impurities and makes assembly difficult, which not only affects production efficiency, but also creates more serious quality risks. Summary of the invention

[0003] The purpose of the present invention is to provide a compressor housing and a manufacturing method thereof in view of the problems existing in the prior art, so as to achieve the purposes of improving production efficiency, reducing quality risks, etc.

[0004] To achieve the above object, the technical solution adopted by the present invention is: A compressor housing comprises an upper housing and a lower housing connected to each other, wherein the lower housing has a lower housing stop, and the inner circumferential upper edge of the lower housing stop is provided with an inner chamfer and / or a taper, the depth of the inner chamfer is not less than 2 mm, and the angle of the inner chamfer is not less than 5°.

[0005] Furthermore, the depth of the inner chamfer is 2 to 4 mm, and the angle of the inner chamfer is 7 to 18°.

[0006] A method for manufacturing a compressor housing, wherein the lower housing is manufactured by a punching process, including the steps of first stretching, second stretching, trimming and forming, wherein the inner chamfer is formed by pressing a forming punch in the forming step.

[0007] Furthermore, the stretching includes the following steps: according to the blanking area of ​​the lower shell, the sheet material is cut into the required flat sheet by the blanking knife; the flat sheet is moved to the spatial position of a stretching positioning plate through the robot clamping position, and the robot clamping position is released, and the flat sheet falls on the stretching positioning plate, and the stretching positioning plate is between a stretching punch and a stretching die, and the shape of the lower shell is initially stretched out by the stretching punch and the stretching die, and then demolded. After completing the stretching, the robot clamping position clamps the stretched lower shell and moves it to the next process.

[0008] Furthermore, the second stretching includes the following steps: moving the stretched lower shell to the spatial position of the second stretching positioning plate through the robot clamping position, and the robot clamping position is released, and the stretched lower shell falls on the second stretching positioning plate, and the second stretching positioning plate is between the second stretching punch and the second stretching die, and the shape of the lower shell is stretched out by the second stretching punch and the second stretching die, and then demolded. After completing the second stretching, the robot clamping position clamps the second stretched lower shell and moves it to the next process.

[0009] Furthermore, the trimming includes the following steps: the second stretched lower shell is moved to a support table by a robot clamping position, a cutter is provided on the top, and as the cutter moves downward, the excess part of the stop of the second stretched lower shell is cut off, the lower shell is always on the support table, the cutter moves upward, and the cutter is completely separated from the trimmed lower shell. After completing the trimming process, the robot clamping position clamps the trimmed lower shell and moves it to the next process.

[0010] Furthermore, the forming includes the following steps: the trimmed lower shell is moved to the spatial position of the forming positioning plate by the transfer machine robot clamping position, and the robot clamping position is released accordingly, and the trimmed lower shell falls on the forming positioning plate, and the forming positioning plate is between the forming punch and the forming die. As the forming die moves downward, the inner cavity of the trimmed lower shell gradually fits on the forming punch, and the outer cavity gradually fits into the forming die. The forming punch is provided with a stop transition outer chamfer. When the trimmed lower shell is completely fitted with the forming punch, the stop trimming of the lower shell is folded from a flanged state and a horizontal state to a vertical state under the downward force of the forming die, and the forming positioning plate and the forming die stop moving. Under the action of the stop transition outer chamfer, the lower shell presses out the inner chamfer in the stop of the lower shell, and then is demolded. The shell forming process is completed, and the lower shell formed by the robot clamping position moves to the next process.

[0011] Furthermore, the forming punch includes an upper forming punch and a lower connecting body, and a punch stop of the forming punch is arranged at the place where the upper forming punch and the lower connecting body are connected, and a stop transition outer chamfer is arranged at the place where the lower part of the punch stop is connected to the lower connecting body, the outward depth of the stop transition outer chamfer is the same as the depth of the inner chamfer, and the angle of the stop transition outer chamfer is the same as the angle of the inner chamfer.

[0012] Furthermore, the upper forming convex mold and the lower connecting body are an integrally formed structure, or the upper forming convex mold and the lower connecting body are a split structure and are fixed by screw connection.

[0013] In some embodiments, the material of the molding punch and the molding die are both DC53, and both are subjected to TD treatment after trial molding. The TD treatment process includes grinding, cleaning, preheating, TD, quenching, low-temperature tempering, cleaning and polishing, inspection and packaging; after the TD treatment, the molding punch and the molding die respectively have a TD layer with a thickness of 12-17 μm.

[0014] Compared with the prior art, the beneficial effects of the present invention are: 1. By setting the inner chamfer and / or taper at the stop of the lower shell of the compressor, an assembly guide can be formed to overcome the problem of difficulty in assembling the compressor during the assembly of the upper shell. The setting of the inner chamfer or taper is equivalent to removing the burrs and flanges of the stop by pressing, without the need to specially grind and clean the stop of the lower shell, thereby improving production efficiency and preventing the burrs and flanges that have not been cleaned at the stop of the lower shell from falling into the compressor during the assembly process, thereby reducing quality risks caused by impurities and the like, and improving product quality and reliability. 2. By setting the inner chamfer and / or taper at the stop of the lower shell Angle or (inner) taper, the upper and lower shells are equivalent to adding a molten pool in the airflow shielded welding or other methods such as laser welding. The molten welding fluid makes the weld full and uniform after solidification in the molten pool, and also reduces the overflow of the welding fluid to form welding slag, thereby improving the welding strength and making the weld beautiful; 3. By setting the material of the forming punch and the forming die to DC53, and performing TD treatment after the trial mold, through the TD process, the TD layer is firmly combined with the substrate, and the substrate material and the TD layer have high hardness, especially the TD layer hardness Vickers hardness is as high as 2800~3250, and the TD layer thickness is 12~17um. The wear resistance of the mold is greatly improved, which is conducive to the consistency and stability of the shell chamfer. The single service life of the mold is up to about 200,000 times, and the service life is long; 4. The upper forming punch and the lower connecting body are split structures and are fixed by screws, which does not affect the forming function of the entire forming punch. The upper forming punch can also be replaced separately as needed, so that the outer chamfer of the stop transition or the taper of the excessive outward can be adjusted or replaced; 5. Due to the presence of each guide column, it is ensured that the position relationship between the punch and the die of each process will not shift when moving downward, and the position is accurate; at the same time, due to the convex of each process The mold can also position the inner cavity of the lower shell by itself, further improving the position accuracy of the punch and the die, avoiding the influence of mold misalignment on the accuracy and size of the shell parts, and improving the overall physical quality of the shell; because the position relationship between the punch, die and positioning plate is accurate, the shell chamfer or taper is guaranteed to be uniform, further improving the assembly accuracy; 6. The compression spring must restore its elasticity after being compressed, and the positioning plate in each process can be lifted to lift the lower shell to complete the stretching forming work, and then the lower shell can be moved to the next process by using the clamping position of the manipulator. All processes are completed automatically and continuously, and the shell production efficiency is high. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a schematic diagram of the overall structure of a compressor housing of the present invention; Figure 2 It is a schematic diagram of the cross-sectional structure of a lower shell of a compressor shell of the present invention; Figure 3 It is a schematic diagram of multi-station stamping in the compressor housing manufacturing method of the present invention; Figure 4 This is a schematic diagram of the chamfering stamping of the lower shell of the present invention; Figure 5 It is a schematic diagram of stamping the lower shell in a stretching process of the present invention; Figure 6 It is a schematic diagram of stamping the lower shell in the second stretching process of the present invention; Figure 7 This is a schematic diagram of the cutting edge of the lower shell of the present invention; Figure 8 This is a schematic diagram of the positioning plate structure of the present invention; Fig. 9 For the present invention Figure 8 Schematic diagram of top view of the middle positioning plate; Fig.10 It is a schematic diagram of a chamfering punch for forming a shell stop according to the present invention; Fig.11 For the present invention Fig.10 Schematic diagram of the cross-section of the intermediate forming punch; Fig.12 It is a schematic diagram of assembling another forming punch of the present invention; In the figure: 1. upper shell; 2. lower shell; 201. lower shell during one stretching; 202. lower shell during two stretching; 3. lower shell stop; 4. inner chamfer; 5. forming die; 6. forming punch; 601. forming upper punch; 602. lower connecting body; 603. punch stop; 7. forming positioning plate; 8. transfer manipulator; 9. positioning plate guide column; 10. lower base; 11. forming die guide column; 12. manipulator clamping position; 13. support table; 14. lower shell during trimming; 15. cutter; 16. forming die compression spring; 17. positioning plate guide compression spring; 18. stop transition outer chamfer; 19. one stretching punch; 20. one stretching die; 21. two stretching punches; 22. two stretching die; 23. flanging; 24. supporting protrusion; 25. positioning contour; 26. forming punch assembly positioning surface; 27. screw. DETAILED DESCRIPTION

[0016] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0017] In the description of the present invention, it should be noted that the directions or positional relationships indicated by the terms "middle", "upper", "lower", "left", "right", "inner", "outer", etc. are based on the directions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.

[0018] like Figure 1 and Figure 2 As shown, a compressor housing comprises an upper housing 1 and a lower housing 2 which are connected to each other, wherein the lower housing 2 has a lower housing stop 3, and the inner circumferential upper edge of the lower housing stop 3 is provided with an inner chamfer 4 and / or a taper, wherein the depth of the inner chamfer 4 is not less than 2 mm, and the angle of the inner chamfer 4 is not less than 5°.

[0019] Preferably, the depth of the inner chamfer 4 is 2 to 4 mm, and the angle of the inner chamfer 4 is 7 to 18°.

[0020] By setting the inner chamfer 4 and / or taper at the stop of the lower shell 2 of the compressor, an assembly guide can be formed to overcome the problem of difficulty in assembling the compressor during the assembly of the upper shell. The setting of the inner chamfer or taper is equivalent to removing the burrs and flanges of the stop by pressing. That is to say, the inner chamfer and taper of the lower shell of the compressor are integrally formed during the pressing process, and there is no need for subsequent processing of the inner chamfer or taper. This method can also remove burrs and flash at the stop of the lower shell, and there is no need to specially grind and clean the stop of the lower shell, thereby improving production efficiency. It can also prevent the burrs and flanges that have not been cleaned at the stop of the lower shell from falling into the compressor during the assembly process, reducing quality risks caused by impurities, and improving product quality and reliability.

[0021] Combination Figure 3 to Figure 11 As shown, a method for manufacturing a compressor housing, the lower housing 2 is manufactured by a punching process, which sequentially includes the steps of first stretching, second stretching, trimming and forming, and the inner chamfer 4 is formed by pressing a forming punch 6 during the forming step.

[0022] First, the total required blanking area is calculated based on the three-dimensional drawing and engineering drawing of the lower shell and appropriate trimming allowance is added. According to the blanking area of ​​the lower shell 2, the required flat sheet is cut from the sheet material by a blanking knife.

[0023] The stretching comprises the following steps: the flat sheet material is moved to the spatial position of a stretching positioning plate through the manipulator clamping position of the manipulator, and the manipulator clamping position is released, and the flat sheet material falls on the stretching positioning plate, and the stretching positioning plate is between a stretching punch 19 and a stretching die 20, the stretching punch 19 is at the bottom, and the stretching die 20 is at the top, as the stretching die 20 moves downward, the shape of the lower shell is initially stretched out, and then demolded, the lower shell is always on a stretching positioning plate, a stretching die 20 moves upward, and the stretching positioning plate also moves upward under the action of elastic force, and the stretching convex and concave dies are completely separated. After completing a stretch, the manipulator clamping position clamps the stretched lower shell and moves it to the next process.

[0024] Furthermore, the second stretching includes the following steps: moving the stretched lower shell to the spatial position of the second stretching positioning plate through the robot clamping position, and the robot clamping position is released accordingly, and the stretched lower shell falls on the second stretching positioning plate, and the second stretching positioning plate is between the second stretching punch 21 and the second stretching die 22, the second stretching punch 21 is at the bottom, and the second stretching die 22 is at the top, as the second stretching die 22 moves downward, the shape of the lower shell is stretched out by the second stretching punch 21 and the second stretching die 22, and then demolding, the lower shell is always on the second stretching positioning plate, the second stretching die moves upward, and the second stretching positioning plate also moves upward under the action of elastic force, the second stretching convex and concave dies are completely separated, and after completing the second stretch, the robot clamping position clamps the second stretched lower shell and moves it to the next process.

[0025] Furthermore, the trimming includes the following steps: the second stretched lower shell is moved to the support platform 13 by the robot clamping position, and a cutter 15 is provided on the top. As the cutter 15 moves downward, the excess flange of the stop of the second stretched lower shell is cut off. The lower shell is always on the support platform 13, and the position relationship of the lower shell does not change. The cutter 15 moves upward, and the cutter 15 is completely separated from the trimmed lower shell. After completing the trimming process, the robot clamping position clamps the trimmed lower shell and moves it to the next process.

[0026] Furthermore, the molding comprises the following steps: the trimmed lower shell is moved to the spatial position of the molding positioning plate 7 by the manipulator clamping position 12 of the transfer manipulator 8, and the manipulator clamping position 12 is released accordingly, and the trimmed lower shell falls on the molding positioning plate 7, and the molding positioning plate 7 is between the molding convex mold 6 and the molding concave mold 5. As the molding concave mold 5 moves downward, the inner cavity of the trimmed lower shell gradually fits on the molding convex mold 6, and the outer cavity gradually fits into the molding concave mold 5, and the molding convex mold 6 A stop transition outer chamfer 18 is provided on it. When the lower shell body after trimming is completely fitted with the forming punch 6, the stop trimming of the lower shell body is folded from a flanged state and a horizontal state to a vertical state under the downward force of the forming die 5. The forming positioning plate 7 and the forming die 5 stop moving. Under the action of the stop transition outer chamfer 18, the lower shell body 2 presses out the inner chamfer 4 in the lower shell stop 3, and then is demolded. The shell molding process is completed, and the robot clamping position 12 clamps the formed lower shell body and moves it to the next process.

[0027] Furthermore, the forming punch 6 includes an upper forming punch 601 and a lower connecting body 602, and a punch stop 603 of the forming punch is arranged at the place where the upper forming punch 601 and the lower connecting body 602 are connected, and a stop transition outer chamfer 18 is arranged at the place where the lower part of the punch stop 603 is connected to the lower connecting body 602, the outward depth of the stop transition outer chamfer 18 is the same as the depth of the inner chamfer 4, and the angle of the stop transition outer chamfer 18 is the same as the angle of the inner chamfer 4, that is, the outward depth A of the stop transition outer chamfer 18 is 2~4mm, and the angle B of the stop transition outer chamfer 18 is 7~18°. Under the action of the stop transition outer chamfer 18, the lower shell 2 presses out an inner chamfer with a depth of 2~4mm and an angle of 7~18° in the stop of the lower shell.

[0028] Between the lower base and the die of each process punch of the above-mentioned first stretching, second stretching and forming process, there are positioning plate guide compression springs 17, compression springs (such as forming die compression springs 16), and guide columns (such as positioning plate guide columns 9, forming die guide columns 11). The guide columns are respectively arranged between the corresponding die and positioning plate and the lower base 10, and can move downward together with the die and positioning plate as a whole, wherein the compression spring is arranged on the guide column of the die and passes through the guide column of the die; the positioning plate compression spring is arranged on the guide column of the positioning plate and passes through the guide column of the positioning plate. The corresponding die is connected to the lower base of the supporting punch through the outer guide column, and the corresponding die can move downward along the outer guide column; the corresponding positioning plate and the lower base of each process punch are surrounded by 4 guide columns, and the positioning plate moves downward along the positioning plate guide columns. A fixedly connected punch is arranged at the center of each process punch, and each process punch is arranged on the lower base and does not change its positional relationship with the lower base.

[0029] The transfer robot 8 includes a pair of movable clamping arms, on which a plurality of robot clamping positions 12 are arranged at intervals, so that the shells on adjacent workstations can be clamped at the same time. For the compressor shell production line, the efficiency of material transfer can be improved.

[0030] The positioning plate (such as the molding positioning plate 7) is provided with a positioning profile in the middle, and a plurality of vertically arranged supporting protrusions are provided in the positioning profile. The lower shell is supported by the positioning plate during the entire molding process. The supporting protrusions provided on the positioning profile are conducive to supporting the lower shell to move upward when the die and the punch are demolded. At the same time, because the positioning plate and the molding punch are fixed in position, it is also conducive to the accurate positioning of the die and the punch as well as the lower shell.

[0031] Due to the existence of each guide column, the position relationship between the punch and the die in each process will not shift when they move downward, and the position is accurate. At the same time, since the punch in each process can also position the inner cavity of the lower shell, the position accuracy of the punch and the die is further improved, and the influence of the misalignment of the mold on the accuracy and size of the shell parts is avoided, and the overall physical quality of the shell is improved. At the same time, because the position relationship between the punch, the die and the positioning plate is accurate, the shell chamfer or taper is guaranteed to be uniform, and the assembly accuracy is further improved.

[0032] The compression spring needs to restore its elasticity after being compressed, so the positioning plate in each process can be lifted up to lift the lower shell, completing the stretching forming work, and then the lower shell is moved to the next process by the clamping position of the robot clamping position. All processes are completed automatically and continuously, and the shell production efficiency is high.

[0033] The shell is separated from the stop depth, ensuring that the lower shell will not be misaligned within the stop depth, ensuring that the upper and lower shells have high matching accuracy from the stop.

[0034] In some embodiments, during the forming process, the lower part of the stopper of the forming punch 6 where it meets the lower connecting body may be provided with a taper that is the same depth as the stopper or shallower than the stopper and transitions outwards, and the taper is 1-3°. The present production method provides a stop transition outer chamfer 18 or an outward taper at the place where the lower part of the stop of the forming punch 6 meets the lower connecting body, and during the press-forming process of the lower shell body, the inner chamfer 4 or inner taper of the stop of the lower shell is pressed out together with the main body, thereby avoiding subsequent chamfering or taper machining, and also dealing with burrs and flanging problems at the stop of the lower shell while forming the inner chamfer and taper, thereby avoiding subsequent grinding and cleaning work, thereby improving production efficiency as a whole.

[0035] The inner chamfer 4 or (inner) taper is provided at the stop 3 of the lower shell, and an accommodating space can be formed therein when it is assembled and connected with the upper shell 1. For example, the upper and lower shells are equivalent to adding a molten pool in airflow shielded welding or other methods such as laser welding. The molten welding fluid makes the weld full and uniform after solidification in the molten pool, and also reduces the overflow of the welding fluid to form welding slag, thereby improving the welding strength and making the weld beautiful.

[0036] Furthermore, the upper molding punch 601 and the lower connecting body 602 are an integrally molded structure.

[0037] Or, if Fig.12 As shown, the upper forming punch 601 and the lower connecting body 602 are split structures, which are connected and fixed by screws 27. The bottom of the lower connecting body 602 is provided with an internal countersunk hole, which is connected to the upper forming punch 601 above by screws 27. This does not affect the forming function of the entire forming punch. The upper forming punch can also be replaced separately as needed, so that the outer chamfer of the stop transition or the outward taper can be adjusted or replaced.

[0038] In some embodiments, the lower connecting body 602 (relative to the lower forming punch) includes the entire stop depth, and the plane formed from the stop depth is connected to the upper forming punch 601 by threads to ensure the precise position connection between the upper and lower forming punches. The lower forming punch includes a stop and a stop transition external chamfer.

[0039] The forming punch 6 is made into a movable connection, and a stop transition outer chamfer 18 is set on the forming lower punch. Since the stop transition outer chamfer 18 protrudes a little relative to the stop, during the shell forming process, this protruding stop transition outer chamfer collapses when it is squeezed and subjected to external force, and fails during the working cycle of the mold, causing the entire punch to be forced to be replaced, and the shell is detached from the stop depth to ensure that the lower shell will not be misaligned within the stop depth, and the upper and lower shells are ensured to have high precision in matching from the stop. Through the movable fastening connection, only the forming lower punch needs to be replaced and the production can be put into production immediately. At the same time, the depth and hardness of the TD wear-resistant coating are guaranteed to improve production efficiency and reduce costs, and further ensure the service life of the mold during the production cycle.

[0040] In some embodiments, the material of the molding punch and the molding die are both DC53, and both are subjected to TD treatment after trial molding. The TD treatment process includes grinding, cleaning, preheating, TD, quenching, low-temperature tempering, cleaning and polishing, inspection and packaging; after the TD treatment, the molding punch and the molding die respectively have a TD layer with a thickness of 12 to 17 μm.

[0041] By setting the material of the forming convex mold and the forming concave mold to DC53 and performing TD treatment after the mold trial, the TD layer is firmly combined with the substrate through the TD process, and the substrate material and the TD layer have high hardness, especially the TD layer has a Vickers hardness of up to 2800-3250, and the TD layer thickness is 12-17um. The wear resistance of the mold is greatly improved, which is conducive to the stability of the shell chamfer consistency. The single service life of the mold is up to about 200,000 times (200,000 lower shells can be stretched), and the service life is long.

[0042] Specifically, the preheating is to hang the mold workpiece (forming convex mold or forming concave mold) into a preheating furnace for preheating, the preheating temperature is 500-550°C, the preheating time is 35min-95min, and the preheating is to prevent the mold workpiece from deformation and cracking during TD.

[0043] The TD is to hang the mold workpiece into a molten salt composed of 99% pure aluminum, borax, and vanadium pentoxide, and continuously stir the molten salt for 30 to 60 minutes. At the same time, the mold workpiece is continuously and slightly shaken, the temperature of the molten salt is 1010°C to 1040°C, and the mold workpiece is hung into a TD furnace with a TD temperature of 980 to 1100°C and a TD time of 8 to 12 hours. Through the molten salt process, vanadium pentoxide penetrates into the matrix and combines with the carbon of the matrix. Through the action of TD temperature and time, vanadium pentoxide penetrates into the matrix and reacts with the matrix to form a TD layer of a certain thickness, and the thickness of the TD layer is 12 to 17um.

[0044] The quenching is to quench the substrate and TD coating of the mold workpiece after TD is completed, and the telescopic mold workpiece is hoisted into a quenching furnace for quenching. The quenching time is 20 to 35 minutes, and the quenching temperature is 510±10°C. After the quenching time is up, it is cooled to about 500°C and hoisted out, and naturally cooled to 50 to 70°C. The quenching process is completed. Quenching can increase the hardness of the substrate and the TD layer.

[0045] The low temperature tempering is as follows: confirming that the mold workpiece has cooled to 50-70°C, hoisting the mold workpiece into a low temperature tempering furnace for tempering, the tempering time is 4-8 hours, the tempering temperature is 170-210°C, after the tempering time is in place, hoisting the mold workpiece out, cooling it naturally or by air, and the working temperature is completed at room temperature, and through tempering, deformation or cracking of the mold workpiece is prevented after the quenching is completed.

[0046] The polishing process is: rough polishing and fine polishing of the mold workpiece after TD heat treatment, the rough polishing is to perform overall rough polishing on the surface of the mold workpiece after TD heat treatment, and mirror fine polishing is performed on the working surface of the workpiece after rough polishing.

[0047] The inspection process is: check whether the mold workpiece has cracks, scratches, and residues on the workpiece surface, and test the hardness. The HV Vickers hardness of the TD layer is 2800-3250, and the thickness of the TD layer is 12-16 um. Embodiment 1:

[0048] An inner chamfer is set at the stop of the lower shell, the inner chamfer depth A is 2.0mm, the inner chamfer angle B is 7°, the upper shell and the lower shell are matched normally, and the upper shell and the lower shell are assembled in place during the batch repeated assembly of the compressor. In the 1000-hour high-temperature life test of 8 compressors, the compressor passed the entire high-temperature life test without abnormalities such as stuck or high power, no leakage in the batch ring welding, and the appearance is full and uniform. Regularly check the forming mold, and there is no abnormality in the chamfer of the outer edge of the forming punch, and the chamfer is intact. Embodiment 2:

[0049] An inner chamfer is set at the stop of the lower shell, the inner chamfer depth A is 4.0mm, the inner chamfer angle B is 18°, the upper shell and the lower shell are matched normally, and the upper shell and the lower shell are assembled in place during the batch repeated assembly of the compressor. In the 1000-hour high-temperature life test of 8 compressors, the compressor passed the entire high-temperature life test without abnormalities such as stuck or high power, no leakage was found in the batch ring welding, and the appearance was full and uniform. Regularly check the forming mold, and there is no abnormality in the chamfer of the outer edge of the forming punch, and the chamfer is intact.

[0050] Comparative Example 1: An inner chamfer is set at the stop of the lower shell, the depth A of the inner chamfer is 0.5mm, and the angle B of the inner chamfer is 1°. During the transportation and actual assembly of the lower shell, the stop is bumped and bulges are generated. During the assembly on the production line, the assembly is difficult, and the upper shell needs to be assembled downward along the stop with a large external force. As a result, under the action of external force, the stop of the lower shell including the flash of the upper shell falls into the compressor. In the high-temperature life test of 8 compressors arranged for 1000 hours, when running to 515 hours, 600 hours, and 700 hours, 2 of the compressors were stuck, and the power of another compressor was obviously too high. After shell dissection analysis, it was found that the crankshaft motion pair was stuck in 2 units with metal impurities that blocked the long oil of the crankshaft motion pair, and the long axis of the crankshaft of another compressor was scratched. At the same time, the ring welding of 6000 compressors was tracked, and it was found that 15 compressors had protruding welding slag at the ring welding, which seriously affected the appearance of the whole machine. The main reason is that the weld pool formed by the chamfer is small, and the welding fluid overflows to form welding slag. Regular inspection of the mold revealed that the chamfer on the outer edge of the forming punch was damaged. The reason for the damage was that the outer chamfer of the stop transition on the forming punch was too small, and the outer chamfer of the stop transition and the forming punch body were pressed and cut during the downward pressure of the shell and the die, resulting in damage to the outer chamfer of the stop transition.

[0051] Comparative Example 2: An inner chamfer is set at the stop of the lower shell, the depth A of the inner chamfer is 1mm, and the angle B of the inner chamfer is 3°. During the transportation and actual assembly of the lower shell, the stop is bumped and bulges are generated. During the assembly on the production line, the assembly is difficult, and the upper shell needs to be assembled downward along the stop with a large external force. As a result, under the action of external force, the stop of the lower shell including the flash of the upper shell falls into the compressor. In the high-temperature life test of 8 compressors arranged for 1000 hours, when running to 650 hours, 700 hours, and 812 hours, one of the compressors was stuck, and the power of the other two compressors was obviously too high. After shell dissection analysis, it was found that the crankshaft motion pair was stuck in two units, and metal impurities blocked the long oil of the crankshaft motion pair, and the long axis of the crankshaft of another compressor was scratched. At the same time, the ring welding of 6000 compressors was tracked, and it was found that 12 compressors had protruding welding slag at the ring welding, which seriously affected the appearance of the whole machine. The main reason is that the weld pool formed by the chamfer is small, and the welding fluid overflows to form welding slag. Regular inspection of the mold revealed that the chamfer on the outer edge of the forming punch was damaged. The reason for the damage was that the outer chamfer of the stop transition on the forming punch was too small, and the outer chamfer of the stop transition and the forming punch body were pressed and cut during the downward pressure of the shell and the die, resulting in damage to the outer chamfer of the stop transition.

[0052] Comparative Example 3: An inner chamfer is set at the stop of the lower shell, the depth A of the inner chamfer is 2mm, and the angle B of the inner chamfer is 5°. During the transportation and actual assembly of the lower shell, the stop is bumped and bulges are generated. During the assembly on the production line, the assembly is difficult, and the upper shell needs to be assembled downward along the stop with a large external force. As a result, under the action of external force, the stop of the lower shell including the flash of the upper shell falls into the compressor. In the high-temperature life test of 8 compressors arranged for 1000 hours, when running to 800 hours, 815 hours, and 923 hours, one of the compressors was stuck, and the power of the other two compressors was obviously too high. After shell dissection analysis, it was found that the crankshaft motion pair was stuck in two units, and metal impurities blocked the long oil of the crankshaft motion pair, and the long axis of the crankshaft of another compressor was scratched. At the same time, the ring welding of 6500 compressors was tracked, and it was found that 10 compressors had protruding welding slag at the ring welding, which seriously affected the appearance of the whole machine. The main reason is that the weld pool formed by the chamfer is small, and the welding fluid overflows to form welding slag. Regular inspection of the mold revealed that the chamfer on the outer edge of the forming punch was damaged. The reason for the damage was that the outer chamfer of the stop transition on the forming punch was too small, and the outer chamfer of the stop transition and the forming punch body were pressed and cut during the downward pressure of the shell and the die, resulting in damage to the outer chamfer of the stop transition.

[0053] Comparative Example 4: An inner chamfer is set at the stop of the lower shell, the depth A of the inner chamfer is 4.3mm, the angle B of the inner chamfer is 20°, the upper shell and the lower shell are matched normally, but due to the large inner chamfer, the plane of the lower shell stop becomes thinner. During the installation process, it was found that the stop of the lower shell of 5 compressors collapsed. In the high-temperature life test of 8 compressors arranged for 1000 hours, when running to 700 hours and 860 hours, 2 of the compressors were stuck. After shell dissection analysis, it was found that the crankshaft motion pair was stuck and 2 of them had metal impurities that caused the crankshaft motion pair to be stuck. At the same time, tracking the ring welding of 5000 compressors, it was found that 8 compressors had ring welding leakage during water inspection and leak detection. The main reason is that the inner chamfer is large, the weld formed is large, and the flash of the upper shell is easy to fall to the bottom of the shell through the large weld. At the same time, due to the large weld pool formed by the inner chamfer, the welding fluid is uneven and full when flowing through the weld, resulting in ring welding leakage in 8 compressors.

[0054] Comparative Example 5: An inner chamfer is set at the stop of the lower shell, the depth A of the inner chamfer is 4.1mm, the angle B of the inner chamfer is 19°, the upper shell and the lower shell are matched normally, but due to the large inner chamfer, the plane of the lower shell stop becomes thinner. During the installation process, it was found that the stop of the lower shell of 2 compressors collapsed. In the high-temperature life test of 8 compressors arranged for 1000 hours, when running to 865 hours and 900 hours, 2 of the compressors had abnormally high power. After shell dissection analysis, it was found that the crankshaft motion pair was stuck and 2 of them had metal impurities that blocked the crankshaft motion pair. At the same time, tracking the ring welding of 5000 compressors, it was found that 4 compressors had ring welding leakage during water inspection and leak detection. The main reason is that the inner chamfer is large, the weld formed is large, and the flash of the upper shell is easy to fall to the bottom of the shell through the large weld. At the same time, due to the large weld pool formed by the inner chamfer, the welding fluid is uneven and full when flowing through the weld, resulting in ring welding leakage in 4 compressors.

[0055] Comparative Example 6: An inner chamfer is set at the stop of the lower shell, the depth A of the inner chamfer is 2mm, the angle B of the inner chamfer is 22°, the upper shell and the lower shell are matched normally, but due to the large inner chamfer, the plane of the lower shell stop becomes thinner. During the installation process, it was found that the stop of the lower shell of 2 compressors collapsed. In the high-temperature life test of 8 compressors arranged for 1000 hours, when running to 865 hours and 950 hours, 2 of the compressors had abnormally high power. After shell dissection analysis, it was found that the crankshaft motion pair was stuck and 2 of them had metal impurities that blocked the crankshaft motion pair. At the same time, tracking the ring welding of 5000 compressors, it was found that 6 compressors had ring welding leakage during water inspection and leak detection. The main reason is that the inner chamfer is large, the weld formed is large, and the flash of the upper shell is easy to fall to the bottom of the shell through the large weld. At the same time, due to the large weld pool formed by the inner chamfer, the welding fluid is uneven and full when flowing through the weld, resulting in ring welding leakage in 6 compressors.

[0056] It can be seen from the above embodiments and comparative examples that within the inner chamfer angle range and depth range specified in the present application, the compressor will not have obvious abnormal phenomena during assembly or operation, not only the assembly is smooth, but also there is no abnormality such as jamming or high power, no leakage is found in batch ring welding, the appearance is full and uniform, the stop transition outer chamfer on the forming punch is basically normal, the service life is long, and it has outstanding beneficial effects compared with the prior art. However, when the depth is too small or too large, the angle is too small or too large, the compressor is prone to abnormalities during assembly, and jamming, high power, weld leakage and other problems will occur in the subsequent operation process, and the stop transition outer chamfer on the forming punch is also easily damaged, and the service life is not long.

[0057] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A compressor housing, comprising an upper housing and a lower housing connected to each other, It is characterized in that The lower shell body has a lower shell stop, and the inner circumferential upper edge of the lower shell stop is provided with an inner chamfer and / or a taper, the depth of the inner chamfer is not less than 2 mm, and the angle of the inner chamfer is not less than 5°.

2. The compressor housing according to claim 1, It is characterized in that The depth of the inner chamfer is 2-4 mm, and the angle of the inner chamfer is 7-18°.

3. A method for manufacturing a compressor housing according to claim 1 or 2, It is characterized in that The lower shell is manufactured by a punching process, including the steps of first stretching, second stretching, trimming and forming. The inner chamfer is formed by pressing a forming punch during the forming step.

4. The method for manufacturing a compressor housing according to claim 3, It is characterized in that The stretching comprises the following steps: according to the blanking area of ​​the lower shell, the sheet material is cut into the required flat sheet material by a blanking knife; the flat sheet material is moved to the spatial position of a stretching positioning plate by a robot clamping position, and the robot clamping position is released accordingly, and the flat sheet material falls on the stretching positioning plate, and the stretching positioning plate is between a stretching punch and a stretching die, and the shape of the lower shell is initially stretched out by the stretching punch and the stretching die, and then demolded. After completing the stretching, the robot clamping position clamps the stretched lower shell and moves it to the next process.

5. The method for manufacturing a compressor housing according to claim 3, It is characterized in that The second stretching includes the following steps: the lower shell after stretching is moved to the spatial position of the second stretching positioning plate by the robot clamping position, and the robot clamping position is released accordingly, and the lower shell after stretching falls on the second stretching positioning plate, and the second stretching positioning plate is between the second stretching punch and the second stretching die, and the shape of the lower shell is stretched out by the second stretching punch and the second stretching die, and then demolded. After completing the second stretching, the robot clamping position clamps the lower shell after the second stretching and moves it to the next process.

6. The method for manufacturing a compressor housing according to claim 3, It is characterized in that The trimming includes the following steps: the second stretched lower shell is moved to a support table by a robot clamping position, a cutter is provided on the top, as the cutter moves downward, the excess part of the stop of the second stretched lower shell is cut off, the lower shell is always on the support table, the cutter moves upward, the cutter is completely separated from the trimmed lower shell, after completing the trimming process, the robot clamping position clamps the trimmed lower shell and moves it to the next process.

7. The method for manufacturing a compressor housing according to claim 3, It is characterized in that The forming includes the following steps: the trimmed lower shell is moved to the spatial position of the forming positioning plate by the transfer machine robot clamping position, and the robot clamping position is released, and the trimmed lower shell falls on the forming positioning plate, and the forming positioning plate is between the forming punch and the forming die. As the forming die moves downward, the inner cavity of the trimmed lower shell gradually fits on the forming punch, and the outer cavity gradually fits into the forming die. The forming punch is provided with a stop transition outer chamfer. When the trimmed lower shell is completely fitted with the forming punch, the stop trimming of the lower shell is folded from a flanging state and a horizontal state to a vertical state under the downward force of the forming die, and the forming positioning plate and the forming die stop moving. Under the action of the stop transition outer chamfer, the lower shell presses out the inner chamfer in the stop of the lower shell, and then is demolded. The shell molding process is completed, and the robot clamps the formed lower shell and moves to the next process.

8. The method for manufacturing a compressor housing according to claim 3, It is characterized in that The forming punch includes an upper forming punch and a lower connecting body, and a punch stop of the forming punch is arranged at the place where the upper forming punch and the lower connecting body are connected, and a stop transition outer chamfer is arranged at the place where the lower part of the punch stop is connected to the lower connecting body, the outward depth of the stop transition outer chamfer is the same as the depth of the inner chamfer, and the angle of the stop transition outer chamfer is the same as the angle of the inner chamfer.

9. The method for manufacturing a compressor housing according to claim 8, It is characterized in that The upper forming convex die and the lower connecting body are an integrally formed structure, or the upper forming convex die and the lower connecting body are a split structure and are fixed by screw connection.

10. The method for manufacturing a compressor housing according to claim 7, It is characterized in that The material of the forming punch and the forming die are both DC53, and both are subjected to TD treatment after trial molding. The TD treatment process includes grinding, cleaning, preheating, TD, quenching, low-temperature tempering, cleaning and polishing, inspection and packaging; after the TD treatment, the forming punch and the forming die respectively have a TD layer with a thickness of 12-17μm.