Souvenir made of remains

By combining the deceased's personal belongings with quartz and other materials, and burning, crushing and sintering processes to make relics and souvenirs, this solves the limitations of existing technology that rely on ashes and realizes the function of making relics and souvenirs under any conditions, supporting Promotion of green memorial services and environmentally friendly memorial services.

CN118754607APending Publication Date: 2024-10-11赵玮
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410571770.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-10
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

The existing technology for making relics and souvenirs mainly relies on human ashes, which cannot meet the needs of people who do not have ashes to make relics and souvenirs, and limits the way to commemorate the deceased's relatives.

Method used

The personal belongings of the deceased are burned, crushed, ground, mixed with quartz, quartz products, silicate and other materials, and dried and sintered to make crystal and beautiful souvenirs, which expands the scope of use.

Benefits of technology

It realizes the production of noble and elegant relic souvenirs under any conditions, meets the memorial and commemorative needs of different groups of people, and supports the country's promotion of green memorial and environmentally friendly memorial methods.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a souvenir made of remains, which comprises quartz, quartz products, silicate, aluminosilicate, phosphate, aluminoferrite, five-color colored glaze and remains before the deceased, and a preparation method of the souvenir comprises the following steps: fully burning the remains before the deceased before the deceased is born, crushing, and weighing 20-65% of the powder according to the weight ratio to obtain a raw material A; grinding quartz, a quartz product, silicate, aluminosilicate, phosphate, aluminoferrite and five-color colored glaze, and weighing 8-35% by weight to obtain a raw material B; after the mixture of the raw material A and the raw material B is fully and uniformly mixed, 20-55% of water is added, the mixture is kneaded and aged, the aged mixture is made into a remain wet blank through a remain mold, and the remain wet blank is dried, dehydrated and sintered at the temperature of 1000-1300 DEG C for molding. Compared with the prior art, the method has the advantages that the limitation that an original remain product only uses human body bone ash is broken through, personal articles of people can be expanded, the application range is expanded, and people can make souvenirs to memorize relatives of the departed regardless of whether bone ash exists or not.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of relic making, in particular to a souvenir made from relics. Background Art

[0002] In order to implement the country's green memorial service and scientific memorial service, reverse backward and bad behaviors such as burial and cenotaph, create a humanistic, scientific and environmentally friendly memorial service method, and use unique scientific and technological methods to transform the deceased's relics into noble and elegant souvenirs to commemorate the deceased relatives.

[0003] The previous patent for making relics and souvenirs only used human ashes to commemorate the deceased, which has certain limitations. In fact, our lives are changing. Some people have ashes and some do not. Then the basic conditions for owning relics and souvenirs are lost, and the relatives of the deceased cannot remember the deceased by owning relics and souvenirs. This is really regrettable. Our new invention is to use people's personal belongings to make crystal clear and beautiful relics and souvenirs to make up for this shortcoming. The deceased's belongings can be used to make noble and elegant relics and souvenirs, which can be used to commemorate and remember the deceased under any conditions. It truly realizes the national advocacy of not repairing tombs and occupying land, science and technology, and green memorial planning for the deceased. Summary of the invention

[0004] In order to solve the above technical problems, the technical solution provided by the present invention is: a souvenir made of relics, including quartz, quartz products, silicate, aluminosilicate, phosphate, ferroaluminate, five-color glaze and relics of the deceased, and the preparation method thereof comprises the following steps:

[0005] S1. Fully burn the deceased's belongings and then crush them, and weigh 20-65% of the powder of the raw materials according to the weight ratio to obtain raw material A;

[0006] S2, grinding quartz, quartz products, silicate, aluminosilicate, phosphate, aluminoferrite, and five-color glaze, weighing 8-35% by weight to obtain raw material B;

[0007] S3, after the mixture of raw material A and raw material B is fully mixed, 20-55% of water is added, kneaded and aged, and made into a relic wet blank through a relic mold, and then dried and dehydrated;

[0008] S4. Preheat and dry it in a drying furnace at 100-150℃, then use a high-temperature furnace to heat and dehydrate it at 200-500℃, then preheat it in a sintering furnace at 500-1000℃, sinter it at 1000-1300℃, and set it at 1300℃ for 10 minutes. Then cool it down gradually and slowly until it reaches room temperature, and you can get a relic souvenir.

[0009] As an improvement, the crushing fineness in S1 is 200 mesh.

[0010] As an improvement, the grinding fineness in S2 is 200 mesh.

[0011] As an improvement, the deceased's belongings include ashes.

[0012] As an improvement, the cooling method in S4 is to cool down gradually and slowly, reducing the temperature by 100°C every quarter of an hour, first slowly, then speeding up the cooling to 800°C, and increasing it to 200°C every quarter of an hour until it reaches room temperature.

[0013] Compared with the prior art, the invention has the advantages of breaking through the limitation that the original relic products only use human ashes, and can be expanded to include people's personal belongings, thus expanding the scope of use. People can make relic souvenirs to commemorate their deceased relatives regardless of whether they have ashes or not. DETAILED DESCRIPTION

[0014] The embodiments described in the present invention are only a part of the embodiments of the present invention, rather than all the embodiments; based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0015] Example 1

[0016] A souvenir made of relics, including quartz, quartz products, silicate, aluminosilicate, phosphate, ferroaluminate, five-color glaze and relics of the deceased, wherein the relics of the deceased include clothes and daily necessities, and the preparation method thereof comprises the following steps:

[0017] S1. The deceased's belongings are fully burned and then crushed into 200 meshes, and 65% of the powder of the raw materials is weighed according to the weight ratio to obtain raw material A;

[0018] S2, grinding quartz, quartz products, silicate, aluminosilicate, phosphate, aluminoferrite, and five-color glaze to 200 mesh and weighing 35% by weight to obtain raw material B;

[0019] S3, after the mixture of raw material A and raw material B is fully mixed, 55% of water is added, kneaded and aged, and made into a relic wet blank through a relic mold, and then dried and dehydrated;

[0020] S4. Preheat and dry it in a drying furnace at 100℃, then use a high-temperature furnace to heat and dehydrate it at 200℃, then preheat it in a sintering furnace at 1000℃, sinter it at 1300℃, and keep it at 1300℃ for 10 minutes to fix it. Then cool it down slowly by 100℃ every moment, first slowly, then speed up the cooling at 800℃, and increase it to 200℃ every moment until it reaches room temperature. Then you can get a relic souvenir.

[0021] Example 2

[0022] A souvenir made of relics, including quartz, quartz products, silicate, aluminosilicate, phosphate, ferroaluminate, five-color glaze and relics of the deceased, the relics of the deceased including ashes, clothes and daily necessities, and the preparation method thereof comprises the following steps:

[0023] S1. The deceased's belongings are fully burned and then crushed into 200 meshes, and 20% of the powder of the raw materials is weighed according to the weight ratio to obtain raw material A;

[0024] S2, grinding quartz products, silicate, aluminosilicate, phosphate, aluminoferrite, and five-color glaze to 200 mesh and weighing 8% by weight to obtain raw material B;

[0025] S3, after the mixture of raw material A and raw material B is fully mixed, 20% of water is added, kneaded and aged, and made into a relic wet blank through a relic mold, and then dried and dehydrated;

[0026] S4. Preheat and dry it in a drying furnace at 10℃, then use a high-temperature furnace to heat and dehydrate it at 200℃, then preheat it in a sintering furnace at 500℃, sinter it at 1000℃, and set it at 1300℃ for 10 minutes. Then cool it down slowly, by 100℃ every moment, first slowly, then speed up the cooling at 800℃, and increase it to 200℃ every moment, until it reaches room temperature, and it can be a relic souvenir.

[0027] Example 3

[0028] A souvenir made of relics, including quartz, quartz products, silicate, aluminosilicate, phosphate, ferroaluminate, five-color glaze and relics of the deceased, the relics of the deceased including ashes, clothes and daily necessities, and the preparation method thereof comprises the following steps:

[0029] S1. The deceased's belongings are fully burned and then crushed into 200 meshes, and 65% of the powder of the raw materials is weighed according to the weight ratio to obtain raw material A;

[0030] S2, grinding quartz, quartz products, silicate, aluminosilicate, phosphate, aluminoferrite, and five-color glaze to 200 mesh and weighing 35% by weight to obtain raw material B;

[0031] S3, after the mixture of raw material A and raw material B is fully mixed, 55% of water is added, kneaded and aged, and made into a relic wet blank through a relic mold, and then dried and dehydrated;

[0032] S4. Preheat and dry it in a drying furnace at 150℃, then use a high-temperature furnace to heat and dehydrate it at 500℃, then preheat it in a sintering furnace at 1000℃, sinter it at 1300℃, and keep it at 1300℃ for 10 minutes to set it. Then cool it down slowly by 100℃ every moment, first slowly, then speed up the cooling at 800℃, and increase it to 200℃ every moment, until it reaches room temperature, and you can get the relic souvenir.

[0033] The present invention uses people's personal belongings to obtain powder through sanitation inspection, dehumidification and drying, combustion oxidation, crushing and grinding, and mixes with quartz, quartz products, silicate, aluminum silicate, phosphate, ferroaluminate, color glaze and other raw materials in proportion, then adds water to fully mix, stirs to form, dries and preheats, and sintered at high temperature to obtain a crystal clear and beautiful relic souvenir. The whole process belongs to the protection scope.

[0034] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0035] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

[0036] The present invention and its implementation methods are described above, and such description is not restrictive. In short, if a person skilled in the art is inspired by it and, without departing from the purpose of the invention, designs structures and embodiments similar to the technical solution without creativity, they should all fall within the protection scope of the present invention.

Claims

1. A souvenir made from relics, characterized by: The invention comprises quartz, quartz products, silicate, aluminosilicate, phosphate, ferroaluminate, five-color glaze and relics of the deceased, and the preparation method thereof comprises the following steps: S1. Fully burn the deceased's belongings and then crush them, and weigh 20-65% of the powder of the raw materials according to the weight ratio to obtain raw material A; S2, grinding quartz, quartz products, silicate, aluminosilicate, phosphate, aluminoferrite, and five-color glaze, weighing 8-35% by weight to obtain raw material B; S3, after the mixture of raw material A and raw material B is fully mixed, 20-55% of water is added, kneaded and aged, and made into a relic wet blank through a relic mold, and then dried and dehydrated; S4. Preheat and dry it in a drying furnace at 100-150℃, then use a high-temperature furnace to heat and dehydrate it at 200-500℃, then preheat it in a sintering furnace at 500-1000℃, sinter it at 1000-1300℃, and set it at 1300℃ for 10 minutes. Then cool it down gradually and slowly until it reaches room temperature, and you can get a relic souvenir.

2. A souvenir made from relics according to claim 1, characterized in that: The grinding fineness in S1 is 200 mesh.

3. A souvenir made from relics according to claim 1, characterized in that: The grinding fineness in S2 is 200 mesh.

4. A souvenir made from relics according to claim 1, characterized in that: The deceased's belongings include ashes.

5. A souvenir made from relics according to claim 1, characterized in that: The cooling method in S4 is to cool down gradually and slowly, cooling down by 100°C every moment, first slowly, then accelerating the cooling to 800°C, and then increasing the cooling to 200°C every moment until it reaches room temperature.

Citation Information

Patent Citations

  • Preparation method of Buddhist bone relic product

    CN101617909A

  • Cabbage collection unit with loading device

    KR102603772B1