Method for graded conversion and high-value utilization of lignite

By mildly oxidizing lignite in an alkaline aqueous solution and using alkaline electrolysis, the problem of CO2 generation and alkali consumption caused by high-temperature and high-pressure oxidation is solved, low-carbon conversion and high-value utilization of lignite are achieved, and high yields of fulvic acid are obtained and high-purity hydrogen, improving the utilization efficiency and electrolysis efficiency of lignite.

CN118756154AActive Publication Date: 2024-10-11ANHUI UNIVERSITY OF TECHNOLOGY

Patent Information

Application Number
CN202410914996.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-09
Publication Date
2024-10-11
Estimated Expiration
2044-07-09

AI Technical Summary

Technical Problem

In the existing technology, the high-temperature and high-pressure oxidation of lignite to prepare water-soluble organic acids has the problems of large amount of CO2 generation, high alkali consumption, and low yield of the target product. Moreover, the insolubility of solid coal used in coal-water slurry electrolysis for hydrogen production restricts the electrolysis kinetics. process and failed to achieve industrial application.

Method used

Alkaline-soluble products are prepared by mildly oxidizing lignite depolymerization in an alkaline aqueous solution, and electrolysis in an alkaline system is used to obtain fulvic acid and small molecule carboxylic acids, and at the same time, hydrogen is co-produced. Transition metal-loaded nickel foam is used as the anode to reduce the cost of the anode. overpotential and improve electrolysis efficiency.

Benefits of technology

It achieves low-carbon conversion and high-value utilization of lignite, with mild reaction conditions and low CO2 emissions. It improves lignite utilization and electrolysis efficiency, obtains high-purity hydrogen and high-yield fulvic acid, and avoids the problems in traditional methods. Base consumption and CO2 production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118756154A_ABST
    Figure CN118756154A_ABST
Patent Text Reader

Abstract

The invention discloses a method for graded conversion and high-value utilization of lignite, and belongs to the technical field of lignite resource utilization and fine chemical engineering. The method comprises the following steps: oxidizing lignite in an alkaline aqueous solution to obtain an alkali-soluble depolymer, electrolyzing the depolymer through an alkaline system to obtain water-soluble fulvic acid and small-molecular carboxylic acid, and co-producing hydrogen. According to the method, oxygen is used for oxidizing lignite in the alkaline aqueous solution for depolymerization, the reaction condition is mild, the lignite conversion rate is high, and the alkali consumption and CO2 generation amount are low. The oxidative depolymerization product is subjected to solid-liquid separation, and the obtained alkali-soluble depolymerization product can be directly used for electrolysis without acid-base neutralization and refining. The method comprises the following steps of: performing constant-potential electrolysis at 60-80 DEG C by taking fulvic acid as a raw material and transition metal loaded nickel as an anode to obtain a conversion product mainly comprising the fulvic acid, and simultaneously co-producing high-purity hydrogen at a cathode. Compared with a traditional chemical oxidation method, the method has the technical remarkable advantages of being high in lignite utilization rate, safe, clean, low in carbon and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of comprehensive energy utilization, lignite resource utilization and fine chemical technology. Specifically, it relates to a lignite graded conversion and high-value utilization method, which uses lignite in an alkaline system to mildly oxidize and depolymerize to prepare humic acid, then electrolyzes the humic acid to obtain fulvic acid and small molecule carboxylic acids, and co-produces hydrogen. Background Art

[0002] Lignite is a cheap, low-metamorphic coal resource with high oxygen content and moisture content, low calorific value, and easy to spontaneously combust. my country is rich in lignite resources, which are mainly used in traditional energy production methods such as combustion for power generation, with low utilization efficiency and high carbon emissions. However, lignite has a high H / C ratio and is relatively chemically active. Selective oxidation and depolymerization of lignite under mild conditions to prepare oxygen-containing chemicals has significant structural advantages. In particular, the oxidation of lignite in aqueous media can avoid high-energy consumption processes such as dehydration and deoxygenation, and obtain oxygen-containing chemical raw materials such as coal-based humic acid, fulvic acid, aromatic carboxylic acids and small molecule fatty carboxylic acids, which are widely used in the preparation of fine chemicals and advanced carbon materials, ecological restoration and environmental governance, and related fields such as agriculture and medicine. Achieve clean conversion and high-value utilization of lignite. Therefore, for CC((CH 2 ) n ) and CO (ether bond) and other cross-linked aromatic ring macromolecules as well as the structural characteristics of lignite rich in oxygen-containing functional groups such as phenolic hydroxyl and carboxyl groups. Efficient oxidative depolymerization under mild conditions to prepare oxygen-containing chemicals can achieve low-carbon conversion and high-value utilization of lignite, make up for the shortage of petroleum resources, and has important development and utilization prospects.

[0003] Selective oxidation of lignite in water has always been one of the important research areas of coal conversion. The preparation of coal-based humic acid by nitric acid oxidation is one of the main production processes of commercial humic acid. However, the high cost and NO x Pollution, process safety and nitration side reactions have not been effectively resolved. Hydrogen peroxide is a clean and efficient oxidant, and the use of hydrogen peroxide to oxidize lignite to prepare oxygen-containing chemicals has also attracted much attention. Although the use of hydrogen peroxide to oxidize lignite can produce chemicals such as benzoic acid and small molecule fatty acids, the poor safety of hydrogen peroxide oxidation has restricted its large-scale production and application. 2 The cost of coal "alkali-oxygen" oxidation using air as the oxidant is low, but it needs to be carried out in a concentrated alkaline solution, which consumes a lot of alkali. In particular, if the goal is to prepare benzene carboxylic acid and water-soluble organic acids, it is necessary to deeply oxidize and crack the macromolecular structure of coal at high temperature. 2 The amount of production is large and the yield of the target product is low. For example, at 200-300°C and an alkali / coal weight ratio of 2.5, using an initial pressure of 5-6 MPa of O 2The alkali-oxygen oxidation of coal can produce water-soluble acid with a mass yield of up to 54.9% (Journal of Fuel Chemistry, 1997, 25: 373). However, in conventional alkali-oxygen oxidation of lignite to produce water-soluble organic carboxylic acids, more than 50% of the carbon is oxidized to CO. 2 (Fuel2020, 280: 118652; Energy Fuels 1997, 11(1): 227), lignite utilization efficiency is low. Based on the study of lignite structure and oxidative reactivity, the applicant proposed a new method for preparing coal-based humic acid by mild oxidative depolymerization of lignite (Fuel2022, 308: 122043; 315: 123277). Through selective oxidative cleavage of cross-linked structures such as CC and CO, a coal-based humic acid yield of more than 80% was obtained at below 100°C and in a dilute alkaline solution (alkaline coal mass ratio 1 / 3), and no CO was detected. 2 The generation of lignite provides a new conversion technology for low-carbon and efficient utilization of lignite.

[0004] Coal-based humic acid is the main source of commercial humic acid and has been widely used in industry, agriculture, medicine, environmental protection and other fields. In recent years, with the good application potential in the field of carbon-based new materials and bulk chemical preparation, humic acid, as a potential organic resource being developed and utilized, has attracted more and more attention from the world. At present, coal-based humic acid is mainly produced by alkali extraction or nitric acid oxidation of lignite and weathered coal, with low humic acid yield, large acid and alkali consumption and high cost. Although oxidative depolymerization under mild conditions can significantly reduce the amount of alkali, increase the humic acid yield, and be used in the production of bulk fine chemicals such as high-efficiency concrete water reducer and water-coal slurry dispersant (ZL 202010259004.7; 202011523968.4; 202110767465.X). However, the humic acid obtained by mild oxidation is mainly alkali-soluble black humic acid, and its application range is limited. In order to obtain fulvic acid with higher utilization value, or even water-soluble organic acids such as benzene polycarboxylic acid, it is necessary to increase the oxidation reaction temperature and the amount of alkali, which will lead to a large amount of CO 2 Generate (Green Chem 2020, 22: 7233).

[0005] In recent years, the use of renewable electricity such as wind power and solar energy to produce hydrogen by electrolysis of water is considered to be the most promising "green hydrogen" production technology for development and application, which can solve the storage and transportation problems of distributed energy. Among them, the use of biomass oxidation coupled with water electrolysis to produce hydrogen can simultaneously obtain value-added chemicals, which has become a research hotspot in the field of hydrogen energy and biomass conversion (AdvEnergy Mater 2021,11:2102292.). Its technical advantage lies in the use of biomass selective oxidation to obtain value-added chemicals instead of the complete oxidation product CO 2, can achieve low overpotential electrolysis hydrogen production, improve current efficiency, and achieve product value-added. Compared with biomass, coal has a high energy density, and auxiliary water electrolysis hydrogen production has the advantage of large-scale low-cost hydrogen production (J Power Sources 2021, 483: 229175). However, the main product of traditional coal-assisted water electrolysis is H 2 and CO 2 , which does not meet the properties of "green hydrogen". At the same time, the poor solubility of solid coal seriously restricts the electrolysis kinetics process. Therefore, water-coal slurry electrolysis to produce hydrogen has not been industrially applied. Summary of the invention

[0006] In view of the energy conversion advantages and value-added effect of biomass-assisted water electrolysis in alkaline media, the present invention proposes a technical idea of ​​preparing alkaline-soluble products by depolymerizing lignite under mild conditions, which are directly used to assist water electrolysis in hydrogen production. The chemical energy and electrical energy in the lignite oxidation process are coupled and converted into clean hydrogen energy by electrochemical oxidation, and oxygen-containing chemicals such as fulvic acid and small molecule water-soluble organic acids are obtained at the same time, realizing the low-carbon conversion and high-value utilization of lignite.

[0007] The present invention is achieved through the following technical solutions.

[0008] The present invention provides a method for graded conversion and high-value utilization of lignite, which comprises the following steps: mildly oxidatively depolymerizing lignite in an alkaline aqueous solution to obtain an alkali-soluble depolymerized product, and then electrolyzing the product in an alkaline system to obtain water-soluble fulvic acid and small molecule carboxylic acids.

[0009] (1) Oxidative depolymerization of lignite: lignite: alkali: water = 1:0.3 to 1:30 mass ratio is added into a high pressure reactor in sequence, heated to 60 to 100 °C in a water bath under stirring conditions, and O 2 To 0-3MPa, and react at constant temperature for 0.5-5h. After the reaction is completed, the solid coal residue is separated by centrifugation to obtain a soluble depolymerized alkaline solution.

[0010] (2) Preparation of electrolyte: Add KOH and deionized water to the soluble depolymerized alkaline solution obtained in (1), adjust the pH to 13-14, and add 5-15 g / L humic acid to prepare the electrolyte.

[0011] (3) Electrolysis: Add the electrolyte prepared in step (2) to the anode chamber of the H-type electrolytic cell. At the same time, add an equal volume and concentration of alkaline solution to the cathode. Select transition metal-loaded nickel foam as the anode, platinum sheet as the cathode, and an anion exchange membrane as the diaphragm. Perform constant potential electrolysis at a temperature of 60 to 80°C and an anode potential of 0.3 to 1V (vs Ag / AgCl), and collect the gases produced at the cathode and cathode, respectively. Perform electrolysis for 1 to 5 hours, terminate the reaction and cool to room temperature.

[0012] (4) Product separation: The product solution obtained in (3) was acidified to pH = 1 with 5 mol / L sulfuric acid, and allowed to settle for 12 h. The insoluble humic acid was separated by centrifugation, washed with deionized water, dried, and weighed to obtain black humic acid + brown humic acid. The liquid product obtained after acid precipitation was extracted with butanone to obtain the product fulvic acid. The butanone extract was neutralized to neutrality with alkali and used for TOC analysis to determine the total organic carbon content of small molecular products such as soluble carboxylic acids.

[0013] As an optimization, the lignite in step (1) is low-metamorphosis lignite with a dry ash-free carbon content of 50-70%, preferably one of Xilin Gol lignite, Xiaolongtan lignite and Zhaotong lignite; the alkali is KOH or NaOH, preferably KOH; the oxidative depolymerization conditions are: lignite: alkali: water = 1: 0.3-1: 30 (mass ratio), 60-100°C, O 2 Pressure 0~3MPa.

[0014] In the step (2), the base is KOH or NaOH, preferably KOH; and the pH is preferably 13.7.

[0015] In the step (3), the anode is a transition metal loaded nickel foam, and the transition metal is preferably Co, Ni, Cu, Cr and a combination thereof, prepared by electrochemical deposition. The electrolysis conditions are a temperature of 60 to 80° C., an anode potential of 0.3 to 1 V (vs Ag / AgCl), and constant potential electrolysis.

[0016] The present invention provides a method for obtaining humic acid by mild oxidative depolymerization of lignite in an alkaline aqueous solution, and then obtaining water-soluble fulvic acid and small molecule carboxylic acid by electrolysis in an alkaline system, which has the following innovative features:

[0017] (1) Based on the fact that lignite has a weak covalent cross-linked structure such as methylene and ether bonds that are easily oxidized, selective depolymerization of lignite can be achieved through oxidation and alkali dissolution under mild conditions to obtain alkali-soluble depolymerization products. At the same time, overoxidation at high temperatures to produce CO 2 , and significantly reduce the amount of alkali used.

[0018] (2) Using the alkaline depolymerization product of lignite to replace the insoluble lignite can significantly improve the kinetic process of anodic oxidation and increase the efficiency of anode-assisted cathode hydrogen evolution. At the same time, electrochemical oxidation replaces chemical oxidation to improve energy utilization efficiency.

[0019] (3) Using transition metal-loaded nickel foam to replace traditional precious metal electrodes such as Pt can improve the anode electrocatalytic oxidation activity, reduce the anode overpotential, inhibit anode oxygen evolution and overoxidation, and achieve anode product value-added.

[0020] Compared with the prior art, the present invention has the following technical effects:

[0021] 1. The present invention realizes the selective oxidation of lignite to prepare chemical raw materials such as fulvic acid and small molecule carboxylic acid, and co-produces hydrogen, with mild reaction conditions and low CO 2 Low emissions. Compared with the traditional chemical oxidation method, the present invention has significant technical advantages such as high utilization rate of lignite, safety, cleanliness and low carbon.

[0022] 2. The present invention provides a method for obtaining humic acid by mild oxidative depolymerization of lignite in an alkaline aqueous solution, wherein the reaction conditions are mild, the yield of humic acid is high, and CO 2 When the reaction conditions were 80°C and the mass ratio of lignite: KOH: water was 1:1:30, the humic acid yield reached 61.15%, and no CO was detected. 2 generate.

[0023] 3. The present invention provides a method for preparing fulvic acid by electrochemical oxidation to improve the quality of humic acid. The method has the advantages of no need for external oxidant, mild reaction conditions, high humic acid utilization rate, simple operation, and co-production of hydrogen. When the electrolysis temperature = 80 ° C, pH = 13.7, humic acid 10g / L, anode potential 0.7V (vs Ag / AgCl), the humic acid conversion rate reached 89.11% after 2h of electrolysis, and the anode CO 2 The amount of production is less than 0.5%, and the cathode product H 2 (Purity>99.9%) with a Faradaic efficiency of 98.8%. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 The present invention provides a technical route for a method for graded conversion and high-value utilization of lignite.

[0025] Figure 2 The ESI FT-ICR MS spectrum of the electrolysis product fulvic acid in Example 1 of the present invention and its analysis results.

[0026] Figure 3 This is the MALD-TOF / MS spectrum of the electrolysis products humic acid + palmitic acid in Example 1 of the present invention. DETAILED DESCRIPTION

[0027] The present invention is described in detail below with reference to the accompanying drawings and embodiments, but the present invention is not limited to the following embodiments.

[0028] By the attached Figure 1It can be seen that the technical route of the present invention includes: (1) converting solid coal into alkali-soluble products through oxidative depolymerization in an alkaline medium, and then using them for electrolysis under alkaline conditions, converting the solid (coal particles)-liquid (electrolyte)-solid (electrode catalyst) multiphase reaction of traditional water-coal slurry into a liquid (electrolyte + alkali-soluble products)-solid (electrode catalyst) two-phase reaction, significantly improving the electrolysis kinetics process and improving the electrolysis efficiency. (2) Using transition metal catalysts, the selective oxidation of alkali-soluble products of lignite oxidative depolymerization is achieved under optimized electrolysis conditions to obtain high-value products such as small molecular carboxylic acids and fulvic acid, which is lower than the anode product CO of traditional water-coal slurry electrolysis. 2 (3) Through electrolysis, distributed renewable electricity is coupled with the chemical energy of lignite oxidation to produce coal-based chemicals to achieve hydrogen production, with high energy conversion efficiency and clean process.

[0029] Example 1

[0030] (1) Oxidative depolymerization of lignite: Zhaotong lignite: KOH: water = 1:1:30 mass ratio was added into a high pressure reactor, heated to 80°C under stirring conditions, and reacted at normal pressure for 5 hours. After the reaction was completed, the solid residual coal was removed by centrifugation to obtain a soluble depolymerized alkaline solution.

[0031] (2) Preparation of electrolyte: Add KOH and deionized water to the soluble depolymerized alkaline solution obtained in (1), adjust the pH to 14, and add 10 g / L humic acid to prepare the electrolyte.

[0032] (3) Electrolysis: Add the electrolyte prepared in step (2) to the anode chamber of an H-type electrolytic cell. At the same time, add an equal volume of KOH solution with a pH of 14 to the cathode. Select Co loaded on nickel foam as the anode, platinum sheet as the cathode, and Fumasep FAB-PK-130 anion exchange membrane as the diaphragm. Perform constant potential electrolysis at a temperature of 80°C and an anode potential of 0.5V (vs Ag / AgCl), and collect the gases produced at the cathode and cathode, respectively. Perform electrolysis for 2 hours, terminate the reaction and cool to room temperature.

[0033] (4) Product separation: The product solution obtained in (3) was acidified to pH = 1 with 5 mol / L sulfuric acid, and allowed to settle for 12 h. The insoluble humic acid was separated by centrifugation, washed with deionized water, dried, and weighed to obtain black humic acid + yellow humic acid. The liquid product obtained after acid precipitation was extracted with butanone to obtain the product yellow humic acid. The butanone extract was neutralized to neutral with alkali and used for TOC analysis to determine the total organic carbon content of small molecular products such as soluble carboxylic acids.

[0034] By the attached Figure 2 It can be seen that the main component of the electrolysis product fulvic acid is organic polycarboxylic acid, mainly including aromatic polycarboxylic acid and fatty polycarboxylic acid containing aromatic nucleus, which has the structural characteristics of fulvic acid.

[0035] By the attached Figure 3 It can be seen that the molecular weight of the electrolysis products, humic acid + humic acid, is mainly concentrated in the range of 500-2000 amu, which is significantly lower than the alkali-soluble products obtained by oxidative depolymerization of lignite.

[0036] Example 2

[0037] (1) Lignite oxidative depolymerization: Zhaotong lignite: KOH: water = 1:0.3:30 mass ratio was added into a high pressure reactor, the temperature was raised to 80 °C under stirring, and O 2 After the reaction is completed, the solid coal residue is removed by centrifugation to obtain a soluble depolymerized alkaline solution.

[0038] (2) Preparation of electrolyte: KOH and deionized water were added to the soluble depolymerized alkaline solution obtained in (1), pH was adjusted to 13.7, humic acid was added to 10 g / L, and the electrolyte was prepared.

[0039] (3) Electrolysis: Add the electrolyte prepared in step (2) to the anode chamber of the H-type electrolytic cell. At the same time, add an equal volume of KOH solution with a pH of 13.7 to the cathode. Select CoNi loaded on nickel foam as the anode, platinum sheet as the cathode, and Fumasep FAB-PK-130 anion exchange membrane as the diaphragm. Perform constant potential electrolysis at a temperature of 80°C and an anode potential of 0.3V (vs Ag / AgCl), and collect the gases produced at the cathode and cathode, respectively. Electrolyze for 2 hours, terminate the reaction and cool to room temperature.

[0040] (4) Product separation: Same as Example 1.

[0041] Example 3

[0042] (1) Lignite oxidative depolymerization: Zhaotong lignite: KOH: water = 1:1:30 mass ratio was added into a high pressure reactor, the temperature was raised to 60 °C under stirring, and O 2 The pressure was raised to 0.1 MPa and the reaction was continued at a constant temperature for 5 hours. After the reaction was completed, the solid coal residue was removed by centrifugation to obtain a soluble depolymerized alkaline solution.

[0043] (2) Preparation of electrolyte: KOH and deionized water were added to the soluble depolymerized alkaline solution obtained in (1), pH was adjusted to 13, humic acid was added to 10 g / L, and the electrolyte was prepared.

[0044] (3) Electrolysis: Add the electrolyte prepared in step (2) to the anode chamber of the H-type electrolytic cell. At the same time, add an equal volume of KOH solution with a pH of 13 to the cathode. Select CoNi loaded on nickel foam as the anode, platinum sheet as the cathode, and Fumasep FAB-PK-130 anion exchange membrane as the diaphragm. Perform constant potential electrolysis at a temperature of 80°C and an anode potential of 1.0V (vs Ag / AgCl), and collect the gases produced at the cathode and cathode respectively. Electrolyze for 1 hour, terminate the reaction and cool to room temperature.

[0045] (4) Product separation: Same as Example 1.

[0046] Example 4

[0047] (1) Oxidative depolymerization of lignite: Zhaotong lignite: KOH: water = 1:0.5:30 mass ratio was added into a high pressure reactor in sequence, the temperature was raised to 100 °C under stirring, and O 2 The pressure was raised to 1.0 MPa and the reaction was continued at a constant temperature for 0.5 h. After the reaction was completed, the solid coal residue was removed by centrifugation to obtain a soluble depolymerized alkaline solution.

[0048] (2) Preparation of electrolyte: Add KOH and deionized water to the soluble depolymerized alkaline solution obtained in (1), adjust the pH to 14, and add 15 g / L humic acid to prepare the electrolyte.

[0049] (3) Electrolysis: Add the electrolyte prepared in step (2) to the anode chamber of the H-type electrolytic cell. At the same time, add an equal volume of KOH solution with a pH of 14 to the cathode. Select CoNi loaded on nickel foam as the anode, platinum sheet as the cathode, and Fumasep FAB-PK-130 anion exchange membrane as the diaphragm. Perform constant potential electrolysis at a temperature of 60°C and an anode potential of 0.3V (vs Ag / AgCl), and collect the gases produced at the cathode and cathode, respectively. Perform electrolysis for 5 hours, terminate the reaction and cool to room temperature.

[0050] (4) Product separation: Same as Example 1.

[0051] Example 5

[0052] (1) Oxidative depolymerization of lignite: Zhaotong lignite: NaOH: water = 1:0.6:30 mass ratio was added into a high pressure reactor, the temperature was raised to 80 °C under stirring, and O 2 After the reaction, the solid coal residue was removed by centrifugation to obtain a soluble depolymerized alkaline solution.

[0053] (2) Preparation of electrolyte: Add KOH and deionized water to the soluble depolymerized alkaline solution obtained in (1), adjust the pH to 13.5, and add 5 g / L humic acid to prepare the electrolyte.

[0054] (3) Electrolysis: Add the electrolyte prepared in step (2) to the anode chamber of an H-type electrolytic cell. At the same time, add an equal volume of NaOH solution with a pH of 13.5 to the cathode. Select Co loaded on nickel foam as the anode, platinum sheet as the cathode, and Fumasep FAB-PK-130 anion exchange membrane as the diaphragm. Perform constant potential electrolysis at a temperature of 60°C and an anode potential of 0.7V (vs Ag / AgCl), and collect the gases produced at the cathode and cathode, respectively. Perform electrolysis for 2 hours, terminate the reaction and cool to room temperature.

[0055] (4) Product separation: Same as Example 1.

[0056] Example 6

[0057] (1) Oxidative depolymerization of lignite: Xiaolongtan lignite: KOH: water = 1:1:30 mass ratio was added into a high pressure reactor, the temperature was raised to 80°C under stirring, and O 2 After the reaction is completed, the solid coal residue is removed by centrifugation to obtain a soluble depolymerized alkaline solution.

[0058] (2) Preparation of electrolyte: Add KOH and deionized water to the soluble depolymerized alkaline solution obtained in (1), adjust the pH to 14, and add 10 g / L humic acid to prepare the electrolyte.

[0059] (3) Electrolysis: Add the electrolyte prepared in step (2) to the anode chamber of an H-type electrolytic cell. At the same time, add an equal volume of KOH solution with a pH of 14 to the cathode. Select CoCu loaded on nickel foam as the anode, platinum sheet as the cathode, and Fumasep FAB-PK-130 anion exchange membrane as the diaphragm. Perform constant potential electrolysis at a temperature of 80°C and an anode potential of 0.3V (vs Ag / AgCl), and collect the gases produced at the cathode and cathode, respectively. Perform electrolysis for 2 hours, terminate the reaction and cool to room temperature.

[0060] (4) Product separation: Same as Example 1.

[0061] Example 7

[0062] (1) Oxidative depolymerization of lignite: The lignite was added into a high-pressure reactor in the mass ratio of Xiaolongtan lignite: KOH: water = 1:0.6:30, and the temperature was raised to 100°C under stirring. O 2 After the reaction, the solid coal residue was removed by centrifugation to obtain a soluble depolymerized alkaline solution.

[0063] (2) Preparation of electrolyte: Add KOH and deionized water to the soluble depolymerized alkaline solution obtained in (1), adjust the pH to 14, and add 10 g / L humic acid to prepare the electrolyte.

[0064] (3) Electrolysis: Add the electrolyte prepared in step (2) to the anode chamber of the H-type electrolytic cell. At the same time, add an equal volume of KOH solution with a pH of 14 to the cathode. Select CuCr loaded on nickel foam as the anode, platinum sheet as the cathode, and Fumasep FAB-PK-130 anion exchange membrane as the diaphragm. Perform constant potential electrolysis at a temperature of 80°C and an anode potential of 0.5V (vs Ag / AgCl), and collect the gases produced at the cathode and cathode, respectively. Perform electrolysis for 3 hours, terminate the reaction and cool to room temperature.

[0065] (4) Product separation: Same as Example 1.

[0066] Example 8

[0067] (1) Lignite oxidative depolymerization: The lignite was added into a high pressure reactor in a mass ratio of Xilin Gol lignite: NaOH: water = 1:1:30, and the temperature was raised to 100 °C under stirring. O 2 After the reaction, the solid coal residue was removed by centrifugation to obtain a soluble depolymerized alkaline solution.

[0068] (2) Preparation of electrolyte: NaOH and deionized water were added to the soluble depolymerized alkaline solution obtained in (1), and the pH was adjusted to 14 and 10 g / L humic acid to prepare the electrolyte.

[0069] (3) Electrolysis: Add the electrolyte prepared in step (2) to the anode chamber of the H-type electrolytic cell. At the same time, add an equal volume of NaOH solution with a pH of 14 to the cathode. Select CoNi loaded on nickel foam as the anode, platinum sheet as the cathode, and Fumasep FAB-PK-130 anion exchange membrane as the diaphragm. Perform constant potential electrolysis at a temperature of 80°C and an anode potential of 0.3V (vs Ag / AgCl), and collect the gases produced at the cathode and cathode, respectively. Perform electrolysis for 2 hours, terminate the reaction and cool to room temperature.

[0070] (4) Product separation: Same as Example 1.

[0071] The results of Examples 1 to 8 are shown in Tables 1 to 3.

[0072] Table 1 Results of oxidative depolymerization of lignite in the present invention

[0073]

[0074]

[0075] Table 2 Results of electrolysis of alkali-soluble depolymers of the present invention

[0076]

[0077] Table 3 Composition distribution of lignite conversion products of the present invention

[0078]

[0079] *Indicates the carbon mass yield of soluble small molecular organic matter determined by TOC.

Claims

1. A method for graded conversion and high-value utilization of lignite, characterized in that The steps include: (1) Oxidative depolymerization of lignite: lignite: alkali: water = 1:0.3 to 1:30 by mass ratio are added to a high-pressure reactor in sequence, heated to 60 to 100°C in a water bath under stirring conditions, and O2 is introduced to 0 to 3 MPa, and the reaction is carried out at a constant temperature for 0.5 to 5 hours; after the reaction is completed, the solid residual coal is separated by centrifugation to obtain a soluble depolymerized alkali solution; (2) electrolyte preparation: adding KOH and deionized water to the soluble depolymerized alkaline solution obtained in step (1), adjusting the pH to 13-14 and the humic acid to 5-15 g / L, to prepare an electrolyte; (3) electrolysis: adding the electrolyte prepared in step (2) to the anode chamber of an H-type electrolytic cell; adding an equal volume of an alkaline solution of equal concentration to the cathode; selecting transition metal-loaded nickel foam as the anode, platinum sheet as the cathode, and an anion exchange membrane as the diaphragm; performing constant potential electrolysis at a temperature of 60 to 80° C. and an anode potential of 0.3 to 1 V, and collecting the gases generated at the cathode and cathode respectively; performing electrolysis for 1 to 5 hours, terminating the reaction, and cooling to room temperature; (4) Product separation: The product solution obtained in step (3) is acidified to pH = 1 using 5 mol / L sulfuric acid, and the mixture is allowed to stand for 12 h. The insoluble humic acid is separated by centrifugation, and then washed with deionized water, dried, and weighed to obtain black humic acid + palmitic acid. The liquid product obtained after acid precipitation is extracted with butanone to obtain the product fulvic acid.

2. The method for graded conversion and high-value utilization of lignite according to claim 1, characterized in that: The lignite in step (1) is low-metamorphosis lignite with a dry ash-free carbon content of 50-70% and a particle size of 80-200 meshes.

3. The method for graded conversion and high-value utilization of lignite according to claim 1, characterized in that: The base in steps (1) to (3) is KOH or NaOH.

4. The method for graded conversion and high-value utilization of lignite as claimed in claim 3, characterized in that: The base in steps (1) to (3) is KOH.

5. The method for graded conversion and high-value utilization of lignite as claimed in claim 1, characterized in that: In the step (2), pH=13.

7.

6. The method for graded conversion and high-value utilization of lignite according to claim 1, characterized in that: The electrolysis device in step (3) is an H-type diaphragm electrolytic cell, the anode is transition metal loaded nickel foam, the cathode is a platinum sheet electrode, and the diaphragm is an anion exchange membrane.

7. The method for graded conversion and high-value utilization of lignite as claimed in claim 6, characterized in that: The transition metal in the transition metal-loaded nickel foam is one or more of Co, Ni, Cu and Cr.

Citation Information

Patent Citations

  • Method for preparing anode-catalyzed electrode for electrolyzing slurry coal

    CN101717950A

  • Method for preparing organics by strengthening electrolysis of coal slurry under alkaline system

    CN102732910A

  • Method for preparing humic acid through lignite electrochemical oxidation

    CN102747381A

  • Coupling process for efficiently utilizing electric energy to perform coal oxidation and carbon dioxide reduction

    CN112725823A

  • Method for preparing solid humic acid by mechanically activating weathered coal and application

    CN117964913A

Cited By

  • Flotation-electrolysis combined quality-based resource utilization method for raw coal

    CN119465186A

  • A method for resource utilization of raw coal by flotation-electrolysis

    CN119465186B