Novel electromagnetic needle bar and processing technology thereof
By adopting the adhesive fixation of stainless steel rod body and zirconia ceramic rod and the design of guide sleeve in the electromagnetic needle needle rod, the problems of heating caused by friction and short life of the buffer gasket are solved, the service life is extended and the weaving quality is improved. quality.
Patent Information
- Application Number
- CN202411029625.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-10-11
AI Technical Summary
In the high-frequency reciprocating motion of the existing electromagnetic needle needle bar, the friction resistance between the guide sleeve and the needle bar is large, resulting in heat generation and a short life of the buffer gasket, which affects the service life and the quality of the fabric.
By bonding and fixing the stainless steel rod body with the zirconia ceramic rod in the electromagnetic needle rod, increasing the diameter of the iron core and the diameter of the buffer gasket, and installing small guide sleeves and auxiliary guide sleeves above and below the iron core to reduce friction. Enhance support.
The service life of the electromagnetic needle bar is extended, friction is reduced, the quality of the fabric is improved, and the frequency of maintenance is reduced.
Smart Images

Figure CN118756408A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of textile machinery and equipment, and specifically refers to a novel electromagnetic needle bar and a processing technology thereof. Background Art
[0002] The electromagnetic needle bar is a related structure of the weft storage device for water jet looms, which is used to control the release and blocking of weft yarn. In the prior art, the electromagnetic needle bar is provided with pure iron for magnetic attraction in the middle, and then the reciprocating motion of the pure iron is realized through the electromagnetic coils at both ends. The shortcomings of the prior art are: the high-frequency reciprocating motion of the electromagnetic needle bar, the large friction resistance between the guide sleeve and the needle bar causes the whole component to heat up, the life of the buffer gasket is shortened, which affects the service life of the electromagnetic needle bar, the yarn blocking is weak, long and short wefts appear, and the quality of weaving deteriorates.
[0003] In response to the above problems, the applicant applied for an invention patent for a manufacturing process of an electromagnetic needle bar (application number: CN202311489241.2) on November 9, 2023. In the manufacturing process, the electromagnetic needle bar is fixed at the upper and lower ends, and the middle guide sleeve is removed to reduce friction, increase the diameter of the pure iron, and make the needle bar more stable under magnetic force. After the diameter of the pure iron increases, the contact point with the buffer gasket increases, which can extend the life of the buffer gasket and ultimately extend the entire service life of the electromagnetic needle. In the above process, the applicant did not provide the corresponding dimensional data, and the applicant made further improvements based on the original application. Summary of the invention
[0004] In view of the above situation, in order to overcome the defects of the prior art, the present invention provides a new electromagnetic needle bar and a processing technology thereof, which are used to further improve the service life of the electromagnetic needle bar and adapt to the current production environment of water jet and air jet looms.
[0005] The technical solutions adopted in this application are as follows:
[0006] This solution provides a new electromagnetic needle bar, including:
[0007] Stainless steel rod body, needle rod and iron core;
[0008] The stainless steel rod body is fixedly connected to the needle rod, and the iron core is fixedly arranged between the stainless steel rod body and the needle rod.
[0009] In a preferred embodiment, the needle bar is a ceramic needle bar.
[0010] In a further embodiment, the needle rod is an inner arc rod with a diameter of 8.8 mm at both ends and a maximum diameter of 8 mm in the middle.
[0011] As a preferred solution, the stainless steel rod body is made of 304 stainless steel, the needle rod is made of 997 zirconia ceramic rod, and the stainless steel rod body and the needle rod are fixed with glue.
[0012] As a further elaboration of the scheme, this scheme provides a new type of electromagnetic needle bar processing technology, including:
[0013] S1: The stainless steel rod and the zirconia ceramic rod are bonded with glue to form a fixing part;
[0014] S2: Insert the iron core into the fixing part and then put it into the mold;
[0015] S3: using a plastic molding machine to inject a plastic preparation from the top of the stainless steel rod, and the plastic preparation forms an injection molding part;
[0016] S4: The injected plastic preparation flows out from the through hole of the stainless steel rod body and fills the inner hole of the iron core;
[0017] S5: Finally, the electromagnetic needle rod is obtained.
[0018] Furthermore, the diameter of the stainless steel rod is 3.5 mm, which is consistent with the inner diameter of the needle rod.
[0019] Furthermore, a return spring is installed at a position 2mm between the injection molded part and the stainless steel rod body.
[0020] Furthermore, the stainless steel rod body penetrates the main body of the electromagnetic needle rod and is combined with the upper injection molding part and the lower ceramic needle rod.
[0021] Furthermore, a small guide sleeve is installed at the lower position of the iron core, and an auxiliary guide sleeve is installed at the upper position of the iron core. The small guide sleeve, the auxiliary guide sleeve and the electromagnetic needle bar part are combined to form a guide body, which repositions the stroke position range of the needle bar structure, increases the supporting force, lengthens the force point position and reduces friction.
[0022] The beneficial effects achieved by the present invention using the above scheme are as follows:
[0023] 1. The diameter of the needle bar and the buffer washer is increased, which increases the service life of the buffer washer.
[0024] 2. The small guide sleeve, auxiliary guide sleeve and electromagnetic needle rod are combined to increase the supporting force, lengthen the force point position and reduce friction. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 A schematic diagram of the overall structure of a new electromagnetic needle rod provided in this solution;
[0026] The meanings of the numbers in the accompanying drawings are as follows:
[0027] 1. Stainless steel rod body, 2. Ceramic needle rod, 3. Iron core.
[0028] a is a small guide sleeve, b is an auxiliary guide sleeve. DETAILED DESCRIPTION
[0029] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the accompanying drawings in the embodiments of the present invention.
[0030] Example 1
[0031] Please refer to Figure 1 As shown, this embodiment provides a new electromagnetic needle bar, including: a stainless steel bar body, a needle bar and an iron core; the stainless steel bar body is fixedly connected to the needle bar, and the iron core is fixedly arranged between the stainless steel bar body and the needle bar.
[0032] In a preferred embodiment, the needle bar is a ceramic needle bar, the stainless steel rod body is made of 304 stainless steel, the needle bar is a 997 zirconia ceramic rod, and the stainless steel rod body and the needle bar are fixed with glue.
[0033] In a further embodiment, the needle rod is an inner arc rod with a diameter of 8.8 mm at both ends and a maximum diameter of 8 mm in the middle.
[0034] Example 2
[0035] This solution provides a new type of electromagnetic needle bar processing technology, including:
[0036] S1: The stainless steel rod and the zirconia ceramic rod are bonded with glue to form a fixing part;
[0037] S2: Insert the iron core into the fixing part and then put it into the mold;
[0038] S3: using a plastic molding machine to inject a plastic preparation from the top of the stainless steel rod, and the plastic preparation forms an injection molding part;
[0039] S4: The injected plastic preparation flows out from the through hole of the stainless steel rod body and fills the inner hole of the iron core;
[0040] S5: Finally, the electromagnetic needle rod is obtained.
[0041] The diameter of the stainless steel rod is 3.5 mm, which is consistent with the inner diameter of the needle rod. A reset spring is installed at a position 2 mm between the injection molding part and the stainless steel rod.
[0042] Furthermore, the stainless steel rod body penetrates the main body of the electromagnetic needle rod and is combined with the upper injection molding part and the lower ceramic needle rod.
[0043] Combination Figure 1As shown, a small guide sleeve is installed at the lower part of the iron core, and an auxiliary guide sleeve is installed at the upper part of the iron core. The small guide sleeve, the auxiliary guide sleeve and the electromagnetic needle bar part are combined to form a guide body, which repositions the travel position range of the needle bar structure, increases the supporting force, lengthens the force point position and reduces friction. The original large inner membrane sleeve with an outer diameter of 9.96mm, an inner diameter of 8.1mm and a length of 21mm is omitted.
[0044] In addition, the 8.4mm gaskets installed at the upper and lower positions of the iron core are changed to new 9.4mm gaskets, which increase the diameter of the needle bar and the buffer gasket by 1mm, thereby increasing the service life of the buffer gasket.
[0045] This product is used in the field of water looms:
[0046] (1) Increase the service life of vulnerable parts;
[0047] (2) Reduce the impact of carbonized powder produced by the wear of the original large guide sleeve on the white fabric surface;
[0048] (3) Reduce maintenance time of maintenance personnel, etc.
[0049] This product is used in the field of air jet looms:
[0050] (1) Increase the service life of vulnerable parts;
[0051] (2) It reduces the blockage of the electromagnetic needle by the cotton yarn hairiness and reduces the influence of the carbonized powder produced by the wear of the original large guide sleeve on the white fabric surface;
[0052] (3) Reduce maintenance time of maintenance personnel, etc.
[0053] This product is used in the field of plastic weaving water looms (heavy water looms):
[0054] (1) The use time of vulnerable parts is increased, and the increase in supporting force reduces the impact of thicker weft threads on the needle bar;
[0055] (2) It reduces the blocking time of the entire electromagnetic needle by the filling powder in the plastic weft;
[0056] (3) Reduce maintenance time of maintenance personnel, etc.
[0057] It should be noted that although the embodiments of the present invention have been shown and described, for ordinary technicians in this field, without departing from the purpose of the invention, structural methods and embodiments similar to the technical solution are designed without creativity and should all fall within the scope of protection of the present invention.
Claims
1. A new type of electromagnetic needle bar, characterized by: It comprises a stainless steel rod body, a needle rod and an iron core. The stainless steel rod body is fixedly connected to the needle rod, and the iron core is fixedly arranged between the stainless steel rod body and the needle rod.
2. The new electromagnetic needle bar according to claim 1, characterized in that: The needle bar is a ceramic needle bar.
3. The new electromagnetic needle bar according to claim 2, characterized in that: The stainless steel rod body is made of 304 stainless steel, the needle rod is made of 997 zirconium oxide ceramic rod, and the stainless steel rod body and the needle rod are fixed by glue.
4. The new electromagnetic needle bar according to claim 3 is characterized in that: The needle rod is an inner arc rod with a diameter of 8.8 mm at both ends and a maximum diameter of 8 mm in the middle.
5. A processing technology for a new electromagnetic needle bar according to any one of claims 1 to 4, characterized in that: include: S1: The stainless steel rod and the zirconia ceramic rod are bonded with glue to form a fixing part; S2: Insert the iron core into the fixing part and then put it into the mold; S3: using a plastic molding machine to inject a plastic preparation from the top of the stainless steel rod, and the plastic preparation forms an injection molding part; S4: The injected plastic preparation flows out from the through hole of the stainless steel rod body and fills the inner hole of the iron core; S5: Finally, the electromagnetic needle rod is obtained.
6. The processing technology of the new electromagnetic needle bar according to claim 5 is characterized in that: The diameter of the stainless steel rod is 3.5 mm, which is consistent with the inner diameter of the needle rod.
7. The processing technology of the new electromagnetic needle bar according to claim 5 is characterized in that: The injection molded part is combined with the stainless steel rod body and a return spring is installed at a position 2mm apart.
8. The processing technology of the new electromagnetic needle bar according to claim 5 is characterized in that: The stainless steel rod body penetrates the main body of the electromagnetic needle rod and is combined with the injection molding part at the upper part and the ceramic needle rod at the lower part.
9. The processing technology of the new electromagnetic needle bar according to claim 8 is characterized in that: A small guide sleeve is installed at the lower position of the iron core, and an auxiliary guide sleeve is installed at the upper position of the iron core. The small guide sleeve, the auxiliary guide sleeve and the electromagnetic needle rod part are combined to form a guide body, which repositions the stroke position range of the electromagnetic needle rod structure, increases the supporting force, lengthens the force point position and reduces friction.
Citation Information
Patent Citations
Permanent magnet electromagnetic needle
CN108462352A
Manufacturing process of electromagnetic needle core
CN117464913A
Restrict electronic weft feeder of flight
CN206266802U
Student's eyes nursing correction equipment