Environment-tensile loading coupling test device and method for testing overlapping performance of thermoplastic FRP (Fiber Reinforced Plastic) rib

By designing an environment-tensile load-bearing coupling test device for thermoplastic FRP bars, the problem that existing devices are difficult to provide long-term stable load-bearing and stress adjustment is solved, and effective testing and precise stress control of the lap joint performance of thermoplastic FRP bars are achieved. control.

CN118777035AInactive Publication Date: 2024-10-15HARBIN INST OF TECH
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
CN202410920855.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-10
Publication Date
2024-10-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

It is difficult for the existing device to provide long-term stable and clear load-carrying path at the overlapping position of thermoplastic FRP bars, and it is impossible to timely adjust the stress relaxation of composite bars during the load-holding process.

Method used

An environment-tensile load-bearing coupling test device is designed, including an anchor assembly, a detachable fixed plate assembly and a load-bearing reaction device. Through the anchoring of the anchor assembly and the concrete test block, the load-bearing reaction device is used to provide a reliable Adjust the tensile load, monitor the stretching situation through a displacement meter and a hollow tension sensor, and dynamically adjust the load-bearing spring to maintain a stable display of the mechanical calculation and analysis system.

Benefits of technology

It achieves effective testing of the overlapping performance of thermoplastic FRP bars, provides a clear load path, and the load application path is precise and controllable. It is suitable for FRP bars with different stress levels and diameters, and can adjust stress relaxation in a timely manner, reducing test costs. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118777035A_ABST
    Figure CN118777035A_ABST
Patent Text Reader

Abstract

The invention provides an environment-tensile loading coupling test device and method for testing the lap joint performance of thermoplastic FRP (Fiber Reinforced Plastic) ribs, and belongs to the field of composite material rib testing. The problem that due to the fact that joints at the lap joint positions of the thermoplastic FRP ribs are weak, a traditional carrying device is difficult to provide long-term stable carrying with a clear application path is solved. The invention discloses an environment-tensile loading coupling test device for testing the overlapping performance of a thermoplastic FRP (Fiber Reinforced Plastic) rib. The environment-tensile loading coupling test device comprises a loading device and an environment box, the holding and loading device comprises anchorage device assemblies which are arranged at the end parts of a force application side and a force bearing side for stretching and holding and loading of the thermoplastic FRP lap joint rib; the detachable fixing plate assembly comprises an upper fixing plate, a lower fixing plate and a limiting assembly, wherein the upper fixing plate and the lower fixing plate are arranged at intervals, and the limiting assembly is used for relatively fixing the upper fixing plate and the lower fixing plate. And the holding counterforce device is used for providing long-term stable and adjustable tensile holding for the thermoplastic FRP lap joint rib. The device is mainly used for testing the overlapping performance of the thermoplastic FRP rib under the long-term corrosion environment-tensile loading coupling effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of composite material reinforcement testing, and in particular relates to an environment-tensile load-bearing coupling test device and method for testing the lap performance of thermoplastic FRP reinforcement. Background Art

[0002] Marine engineering construction, operation and maintenance are the foundation for building a strong maritime nation. Under the strong corrosion environment of the ocean, marine engineering infrastructure based on traditional reinforced concrete structures faces prominent durability issues. Continuous fiber reinforced polymer (FRP) has excellent properties such as light weight, high strength, corrosion resistance and fatigue resistance. Replacing steel bars in marine engineering construction is one of the effective ways to effectively solve the problems of short service life and reduced durability of marine engineering infrastructure.

[0003] At present, thermosetting resin-based FRP bars are widely used in reinforced concrete structures due to their low viscosity during the molding process, excellent mechanical properties and chemical corrosion resistance, and relatively low cost. However, due to the fact that they cannot be bent and recycled after one-time molding, thermosetting resin-based FRP bars are usually connected in the form of binding overlap, mechanical connection, etc., and the interlocking structure formed by the mechanical interlocking of the overlapped bars and concrete is used to achieve effective bonding between the bars and concrete. However, the damage to the continuous fibers caused by mechanical connection affects the overall performance of the composite product, thereby limiting its connection efficiency. Thermoplastic resins make up for the deficiency that thermosetting resins cannot be processed secondary after curing. Through thermal processing, thermoplastic resin-based FRP bars can change their shape without changing their properties, making adhesive connection an efficient overlap method for transmitting uniform stress. The molten bonding of the resin matrix under hot melt treatment effectively improves the bearing capacity of the overlap node.

[0004] Affected by harsh factors such as wind, waves, salt spray, and seawater solutions, FRP bars in reinforced concrete structures are subjected to external loads and erosion from extremely harsh environments for a long time. At present, researchers at home and abroad often study the long-term performance evolution of fiber-reinforced composite material load-bearing components under natural atmospheric corrosion or working loads by adding environmental simulation devices that simulate environmental factors such as temperature, humidity, or media to large-scale fatigue testing equipment. Such test equipment has significant advantages in simulating the tensile-bending-fatigue coupling and bending-environmental coupling of thermosetting resin-based FRP straight bars. However, there is no load-environment coupling test device suitable for thermoplastic FRP lap bars, and the existing devices are limited by design components, making it difficult to adjust the stress relaxation of composite bars in a timely manner during the loading process. Summary of the invention

[0005] In view of this, the present invention aims to propose an environmental-tensile loading coupling test device and method for testing the lap performance of thermoplastic FRP bars, so as to solve the problem that traditional loading devices are difficult to provide long-term stable loading with clear application paths due to weak nodes at the lap positions of thermoplastic FRP bars.

[0006] To achieve the above object, the present invention adopts the following technical scheme. According to one aspect of the present invention, an environmental-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars is provided, comprising: a loading device and an environmental box for providing a constant temperature and a corrosive environmental solution for the tensile loading test; the loading device comprises:

[0007] Anchorage components are arranged at the ends of the force-applying side and the load-bearing side of the thermoplastic FRP lap reinforcement for tensile loading, and are used to provide a fixed end for stable tensile loading, wherein the thermoplastic FRP lap reinforcement is connected to the concrete test block;

[0008] The detachable fixing plate assembly comprises an upper fixing plate and a lower fixing plate arranged at intervals, and a limiting assembly for fixing the upper fixing plate and the lower fixing plate relative to each other, the concrete test block is arranged between the upper fixing plate and the lower fixing plate, and the anchor assembly on the load-bearing side is pushed against the corresponding side end surface of the concrete test block;

[0009] The load reaction device is arranged between the anchor assembly on the force-applying side and the concrete test block, and is used to provide an adjustable tensile load for the thermoplastic FRP lap reinforcement. A displacement meter and a hollow tension sensor are arranged on the force-applying side of the thermoplastic FRP lap reinforcement, and the mechanical calculation and analysis system configured with the displacement meter is used to monitor the changes in displacement and tension of the thermoplastic FRP lap reinforcement during the tensile loading process.

[0010] Furthermore, the limiting assembly is four control slide rails distributed in parallel at the four corners of the detachable fixed plate assembly, and the upper fixed plate and the lower fixed plate are connected to all the control slide rails.

[0011] Furthermore, the anchor assembly includes an anchor clip and an anchor sleeve, and the length-to-diameter ratio of the anchor sleeve is greater than the length-to-diameter ratio of the anchor clip, so that the anchor clip and the end of the thermoplastic FRP lap reinforcement are pressed into the anchor sleeve and clamped.

[0012] Furthermore, the load-bearing reaction device includes a reaction plate clamped between the concrete test block and the lower fixed plate, a screw rod symmetrically arranged relative to the thermoplastic FRP lap ribs and connected to the reaction plate at one end, a load-bearing spring sleeved on each screw rod and connected to the reaction plate at one end, a support plate connected to the other end of all the load-bearing springs, and a nut connected to the other end of each screw rod and connected to the end face of the support plate away from the load-bearing spring, and the load-bearing spring is used to dynamically adjust the size of the tensile load.

[0013] Furthermore, the upper fixing plate, the lower fixing plate, the reaction plate and the support plate are all arranged perpendicular to the thermoplastic FRP lap ribs and are all provided with channels for the thermoplastic FRP lap ribs to pass through.

[0014] Furthermore, the thermoplastic FRP lap reinforcement and two opposite surfaces of the concrete test block are kept perpendicular.

[0015] Furthermore, the environmental box is a closed device that controls a constant temperature and contains a corrosive solution environment, and is used to place the holding device after the upper fixing plate, the lower fixing plate and the limiting assembly are removed in a corrosive solution environment at a constant temperature.

[0016] Furthermore, the diameter of the thermoplastic FRP lap rib does not exceed 25 mm.

[0017] Furthermore, the surfaces of the load-bearing reaction force device and the anchor assembly are subjected to rust-proof treatment before entering the environmental chamber.

[0018] According to another aspect of the present invention, there is provided a test method using the above-mentioned environment-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars, comprising the following steps:

[0019] S1. Pass the thermoplastic FRP lap reinforcement across a concrete test mold of standard size, pour fresh concrete into the concrete test mold, and form a concrete test block after demoulding to complete the preparation of the lap reinforcement-concrete bonding specimen;

[0020] S2. Install an upper fixing plate and a lower fixing plate at the upper and lower ends of the concrete test block, and fix the upper fixing plate and the lower fixing plate relatively by means of a limit assembly;

[0021] S3. Clamp the anchor clips at both ends of the thermoplastic FRP lap reinforcement, adjust the anchor clips on the upper fixing plate side to be close to the concrete test block, and keep a certain free section length between the anchor clips on the lower fixing plate and the lower fixing plate. Use a press to pre-press the anchor clips at both ends into the anchor sleeve to complete the anchoring;

[0022] S4. Install a load-bearing reaction device, a displacement meter, and a hollow tension sensor on the surface of the thermoplastic FRP lap reinforcement between the anchor clip on the lower fixing plate side and the lower fixing plate in sequence, and connect the hollow tension sensor to the mechanical calculation and analysis system;

[0023] S5. The tensile load is provided by adjusting the load spring, and the load is transmitted to the support plate through the screw. When the reading of the mechanical calculation and analysis system connected to the hollow tension sensor reaches the preset value, the support plate is fixed by connecting the nut to the screw to stabilize the tensile load acting on the end of the thermoplastic FRP lap rib;

[0024] S6. Place the holding device after removing the control slide rail and the upper fixed plate in a constant temperature corrosive solution in an environmental chamber for a certain period of time. Use a displacement meter and a hollow tension sensor to monitor the tensile load size and displacement changes of the thermoplastic FRP lap ribs. Dynamically adjust the holding spring to keep the reading of the mechanical calculation and analysis system constant. After a certain period of time, observe and record the performance of the thermoplastic FRP lap ribs. The test is completed.

[0025] Compared with the prior art, the present invention has the following beneficial effects:

[0026] 1. The present invention adopts its own structural design, so that after the concrete test block and the thermoplastic FRP lap reinforcement are connected, the connected test sample is well fixed through the cooperation of the anchor assembly, the upper fixing plate and the lower fixing plate. Through the load-holding reaction force device, a load holding path with a clear path can be provided, and the load application path is clear, which has the advantages of simple design and processing and simple operation;

[0027] 2. The present invention has a simple structure, a clear load path, and a precisely controllable load level. It can adapt to the tensile load of thermoplastic FRP lap bars under different stress levels. The operation process is simple and convenient, and the test cost is relatively low.

[0028] 3. The present invention can be used to carry out load-bearing tests on thermoplastic FRP lap bars of different diameters, and has strong versatility and stable performance;

[0029] 4. The present invention can timely adjust stress relaxation during the test by adjusting the load-holding spring, and is suitable for conducting lap performance tests on thermoplastic FRP lap bars of various diameters and different surface morphologies. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings:

[0031] Figure 1 It is a structural schematic diagram of an environment-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars according to the present invention;

[0032] Figure 2 It is a schematic diagram of the three-dimensional structure of the carrying device of the present invention;

[0033] Figure 3 It is a front structural schematic diagram of the carrying device of the present invention;

[0034] Figure 4 It is a top view of the concrete test block and the anchor assembly after being anchored according to the present invention.

[0035] Anchor assembly 1; anchor clip 101; anchor sleeve 102; control slide rail 2; detachable fixing plate assembly 3; upper fixing plate 301; lower fixing plate 302; concrete test block 4; thermoplastic FRP lap rib 5; load-bearing reaction device 6; reaction plate 601; load-bearing spring 602; screw 603; support plate 604; nut 605; gasket 606; displacement meter 7; hollow tension sensor 8; mechanical calculation and analysis system 9; environmental chamber 10. DETAILED DESCRIPTION

[0036] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely explain the technical solutions in the embodiments of the present invention. It should be noted that the embodiments of the present invention and the features in the embodiments can be combined with each other without conflict, and the described embodiments are only part of the embodiments of the present invention, not all of the embodiments.

[0037] It should be noted that the descriptions of the present invention regarding directions such as "left", "right", "left side", "right side", "upper", "lower", "top", "bottom", etc. are all defined based on the relationship between the orientations or positions shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the structure described must be constructed and operated in a specific orientation, and therefore, cannot be understood as a limitation on the present invention. In the description of the present invention, the meaning of "multiple" is more than two, unless otherwise clearly and specifically defined.

[0038] In the description of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0039] Referring to the accompanying drawings, this embodiment is described. According to one aspect of the present invention, there is provided an environment-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars, comprising: a loading device and an environmental box 10 for providing a constant temperature and a corrosive environment solution for the tensile loading test; the loading device comprises:

[0040] The anchor assembly 1 is arranged at the end of the force-applying side and the load-bearing side of the thermoplastic FRP lap bar 5 for tensile support, and is used to provide a fixed end for stable tensile support. The thermoplastic FRP lap bar 5 is connected to the concrete test block 4; the anchor assembly 1 is used to anchor the two ends of the thermoplastic FRP lap bar 5, and the anchoring process is completed by a press after the anchor assembly 1 is installed in place. The overlapping part of the thermoplastic FRP lap bar 5 is set on the concrete test block 4, and the concrete test block 4 is a standard-sized concrete test mold that is made in a prefabricated form and has holes reserved for accommodating the thermoplastic FRP lap bar 5. After the thermoplastic FRP lap bar 5 is inserted, fresh concrete is poured into the hole, and the mold is removed at room temperature for 24 hours, and standard curing is performed to the specified age.

[0041] The detachable fixing plate assembly 3 includes an upper fixing plate 301 and a lower fixing plate 302 arranged at intervals, and a limit assembly for fixing the upper fixing plate 301 and the lower fixing plate 302 relatively. The concrete test block 4 is arranged between the upper fixing plate 301 and the lower fixing plate 302, and the anchor assembly 1 on the load-bearing side is pushed against the corresponding side end surface of the concrete test block 4; the upper fixing plate 301 and the lower fixing plate 302 are used to cooperate with the anchor assembly 1 to complete the fixation of the concrete test block 4, and at the same time provide certain support for the lower fixing plate 302 to the load-bearing reaction device 6, so that the load of the load-bearing reaction device 6 can be loaded on the concrete test block 4, thereby applying a torque to the thermoplastic FRP lap rib 5.

[0042] The load reaction device 6 is arranged between the anchor assembly 1 on the force-applying side and the concrete test block 4, and is used to provide an adjustable tensile load for the thermoplastic FRP lap reinforcement 5. A displacement meter 7 and a hollow tension sensor 8 are arranged on the force-applying side of the thermoplastic FRP lap reinforcement 5, and a mechanical calculation and analysis system 9 configured with the displacement meter 7 is used to monitor the displacement and tension changes of the thermoplastic FRP lap reinforcement 5 during the tensile loading process. The strain gauge 7 and the hollow tension sensor 8 are used to measure the corresponding torque data to prepare data for subsequent displacement and other data analysis; the hollow tension sensor 8 is used to collect the load force in real time, and the actual load size of the hollow tension and pressure sensor should not exceed 80% of the sensor range.

[0043] In this embodiment, the position limiting assembly is four control rails 2 parallelly distributed at the four corners of the detachable fixed plate assembly 3, and the upper fixed plate 301 and the lower fixed plate 302 are connected to all the control rails 2. The upper fixed plate 301 and the lower fixed plate 302 are provided with buckles or other fixing structures that cooperate with the control rails 2, which can help the upper fixed plate 301 or the lower fixed plate 302 to slide and adjust with the control rails 2 and then fix to the corresponding position.

[0044] In this embodiment, the anchor assembly 1 includes an anchor clip 101 and an anchor sleeve 102, and the length-to-diameter ratio of the anchor sleeve 102 is greater than the length-to-diameter ratio of the anchor clip 101, so that the anchor clip 101 and the end of the thermoplastic FRP lap rib 5 are pressed into the anchor sleeve 102 and clamped. The anchoring process specifically presses the anchor sleeve 102 by a press machine, so that the anchor clip 101 and the anchor sleeve 102 complete the anchoring of the thermoplastic FRP lap rib 5 at the corresponding end. The diameter range of the thermoplastic FRP lap rib 5 does not exceed 25 mm.

[0045] In this embodiment, the load-bearing reaction device 6 includes a reaction plate 601 clamped between the concrete test block 4 and the lower fixed plate 302, a screw 603 symmetrically arranged relative to the thermoplastic FRP lap rib 5 and connected to the reaction plate 601 at one end, a load-bearing spring 602 sleeved on each screw 603 and connected to the reaction plate 601 at one end, a support plate 604 connected to the other end of all the load-bearing springs 602, and a nut 605 and a gasket 606 connected to the other end of each screw 603 and connected to the end face of the support plate 604 away from the load-bearing spring 602. The load-bearing spring 602 is used to dynamically adjust the size of the tensile load. By compressing the load-bearing spring 602 and fixing it with the nut 605 and the gasket 606, the support plate 604 can form a reaction force on the load-bearing spring 602, so that the torque finally reacts on the concrete test block 4. The entire transmission direction of the torque is carried out in the vertical direction of the screw 603. The torque path is clear and easy to observe and record during the experiment.

[0046] In this embodiment, the upper fixing plate 301, the lower fixing plate 302, the reaction plate 601 and the support plate 604 are arranged perpendicular to the thermoplastic FRP lap ribs 5 and are provided with channels for the thermoplastic FRP lap ribs 5 to pass through. It is convenient to install and disassemble the thermoplastic FRP lap ribs 5 and other parts, and the convenience is improved. As for the aperture of the channel, it is sufficient to ensure that the anchor assembly 1 passes through smoothly. The materials of the upper fixing plate 301, the lower fixing plate 302, the reaction plate 601 and the support plate 604 can be selected according to the needs of the actual test and the corrosion resistance characteristics.

[0047] In this embodiment, the thermoplastic FRP lap ribs 5 are kept perpendicular to the two opposite surfaces of the concrete test block 4. This arrangement is to cooperate with the load-bearing reaction force device 6 to form a load with a clear load path to act on the sample.

[0048] In this embodiment, the environmental box 10 is a closed device for controlling a constant temperature and containing a corrosive solution environment, and is used to place the holding device after the upper fixing plate 301, the lower fixing plate 302 and the limit assembly are removed in a constant temperature corrosive solution environment. The closed device is a constant temperature water tank, and an existing corrosion-resistant constant temperature water tank can be used. At the same time, gloves that can be integrated for internal operations are required to adjust the nut 605 and the gasket 606 to stabilize the reading of the mechanical calculation and analysis system 9 during the test phase. The constant temperature corrosive solution can be seawater.

[0049] In this embodiment, the surfaces of the load-bearing reaction device 6 and the anchor assembly 1 are subjected to rust prevention treatment before entering the environmental chamber 10 to prevent the corrosive solution from affecting the normal progress of the test.

[0050] According to another aspect of the present invention, there is provided a test method using an environmental-tensile loading coupling test apparatus as described above for testing the lap properties of thermoplastic FRP bars, comprising the following steps:

[0051] S1, passing the thermoplastic FRP lap reinforcement 5 across a concrete test mold of standard size, pouring fresh concrete into the concrete test mold, and forming a concrete test block 4 after demoulding, thereby completing the preparation of the lap reinforcement-concrete bonding specimen;

[0052] S2, install the upper fixing plate 301 and the lower fixing plate 302 at the upper and lower ends of the concrete test block 4, and fix the upper fixing plate 301 and the lower fixing plate 302 relatively by a limiting assembly;

[0053] S3, respectively clamp the anchor clips 101 at both ends of the thermoplastic FRP lap rib 5, adjust the anchor clips 101 on the upper fixing plate 301 side to be close to the concrete test block 4, and keep a certain free section length between the anchor clips 101 on the lower fixing plate 302 and the lower fixing plate 302, and use a press to pre-press the anchor clips 101 at both ends into the anchor sleeve 102 to complete the anchoring;

[0054] S4, sequentially install the load-bearing reaction device 6, the displacement meter 7, and the hollow tension sensor 8 on the surface of the thermoplastic FRP lap rib 5 between the anchor clip 101 on the lower fixing plate 302 and the lower fixing plate 302, and connect the hollow tension sensor 8 to the mechanical calculation and analysis system 9;

[0055] S5. The tensile load is provided by adjusting the load spring 602. The load is transmitted to the support plate 604 through the screw rod 603. When the reading of the mechanical calculation and analysis system 9 connected to the hollow tension sensor 8 reaches the preset value, the support plate 604 is fixed by connecting the screw rod 603 through the nut 605 and the gasket 606, so that the tensile load acting on the end of the thermoplastic FRP lap rib 5 is stable.

[0056] S6. After removing the control slide rail 2 and the upper fixed plate 301, place the holding device in the constant temperature corrosive solution of the environmental box 10 for a certain period of time. The displacement meter 7 and the hollow tension sensor 8 monitor the tensile load size and displacement change of the thermoplastic FRP lap rib 5. The holding spring 602 is dynamically adjusted to make the indication of the mechanical calculation and analysis system 9 constant. After a certain period of time, the performance of the thermoplastic FRP lap rib 5 is observed and recorded, and the test is completed.

[0057] For the thermoplastic FRP lap ribs 5, the resin matrix includes but is not limited to polypropylene, nylon 6 or nylon 66, etc., and the reinforcing fibers include glass fibers, basalt fibers or carbon fibers. The surface morphology of the thermoplastic FRP lap ribs 5 includes but is not limited to plain round ribs, threaded ribs and sand-bonded ribs, and the diameter range does not exceed 25 mm. For the concrete test block 4, it includes cement concrete, seawater sand concrete and building mortar. Strain gauges can be replaced by displacement sensors. For the surface of the load reaction device 6 and the anchor assembly 1, anti-rust measures such as applying an isolation agent should be taken before the tension and compression load-environment coupling test.

[0058] For thermoplastic FRP lap reinforcement 5, the melting lap method is:

[0059] In the first step, two thermoplastic FRP bars with the same diameter and surface morphology are selected, and the ends of the thermoplastic FRP bars are heated to a molten state using a hot melt glue gun;

[0060] In the second step, the thermoplastic fiber reinforced composite material reinforcement that is heated and melted is fastened by the sleeve;

[0061] The third step is to cool and shape the ends of the reinforcement at the overlapped position and remove the sleeve.

[0062] According to the above disclosure, two sets of actual test processes and corresponding parameters are provided:

[0063] Test 1:

[0064] During the preparation stage of the thermoplastic FRP lap ribs, first, two glass fiber reinforced polypropylene threaded ribs with a diameter of 10 mm were selected, and the ends of the thermoplastic composite ribs were heated to a molten state using a hot melt glue gun; then, the heated and molten thermoplastic fiber reinforced composite ribs were fastened by a sleeve; finally, the ends of the ribs at the lap position were cooled and shaped, and the sleeve was removed.

[0065] In the test phase of tension-compression load-environment coupling, first, the melt-jointed thermoplastic FRP bars are passed through a 100mm×100mm×100mm concrete steel test mold, fresh concrete is poured into the test mold, and the mold is demolded at room temperature for 24 hours. After standard curing for 28 days, the thermoplastic FRP lap bar-concrete bonding specimen is prepared; then, fixed plates are installed at the upper and lower ends of the concrete specimen to be tested, and the upper fixed plate 301 and the lower fixed plate 302 are fixed by four parallel control slide rails 2. The anchor clip 101 is clamped at the end of the thermoplastic FRP lap bar-concrete bonding specimen, and the anchor clip 101 on the upper fixed plate 301 side is adjusted to be close to the concrete specimen, and the anchor clip 101 on the lower fixed plate side retains a certain free section length. The two are pre-pressed into the anchor sleeve by a press to complete the anchoring; then, the reinforcement surface on the free end side of the thermoplastic FRP lap bar-concrete bonding specimen is installed in sequence. The load-bearing reaction force device 6, the strain gauge 7, the hollow tension and pressure sensor 8, and the hollow tension and pressure sensor 8 are connected to the mechanical calculation and analysis system 9; then, the load-bearing spring 602 is adjusted to a stress level of 10% σu, and the load is transmitted to the support plate 604 through the screws 603 on both sides. When the reading of the mechanical calculation and analysis system 10 connected to the hollow tension and pressure sensor 8 reaches 10% σu, the screw 603 is fixed by the nut 605 and the gasket 606 at the connection of the support plate 604, so that the tension and compression load acting on the end of the bonding sample is stable; finally, the control slide rail 2 and the upper fixed plate 301 are removed, and the tension and compression load-environment coupling device with the sample to be tested is placed in an environmental box 10 prepared with a salt solution, and the constant temperature of the environmental box 10 is set to 60°C. During the test, the tension and compression load and displacement changes monitored by the hollow tension and pressure sensor 8 and the strain gauge 7 are checked every day, and the load-bearing spring is dynamically adjusted to make the reading of the mechanical calculation and analysis system 9 constant.

[0066] Test 2:

[0067] The carbon fiber reinforced nylon 6 rebar was subjected to a tensile and compressive load-simulated seawater environment coupling test. The specific implementation method is as follows:

[0068] During the preparation stage of the lap joint reinforcement, first, two carbon fiber reinforced nylon 6 sand-bonded reinforcements with a diameter of 12 mm are selected, and the ends of the carbon fiber reinforced nylon 6 reinforcements are heated to a molten state using a hot melt glue gun; then, the heated and molten thermoplastic fiber reinforced composite reinforcement is fastened by a sleeve; finally, the ends of the reinforcement at the lap joint position are cooled and shaped, and the sleeve is taken out.

[0069] In the test phase of tension and compression load-environment coupling, first, the melt-jointed thermoplastic FRP bars are passed through a concrete test block 4 of standard size, fresh concrete is poured into the test mold, demolded at room temperature for 24 hours, and standardly cured to the specified age to prepare the thermoplastic FRP lap bar-concrete bonding specimen; then, fixed plates are installed at the upper and lower ends of the concrete test block to be tested, and the fixed plates are fixed by four parallel control slide rails 2, and the anchor clips 101 are clamped at the ends of the thermoplastic FRP lap bar-concrete bonding specimen, and the anchor clips on the upper fixed plate side are adjusted to be close to the concrete test block 4, and the anchor clips 101 on the lower fixed plate side retain a certain free section length, and the two are pre-pressed into the anchor sleeve by a press to complete the anchoring; then, the load reaction device 6, the strain gauge 7, and the hollow tension and pressure sensor 8 are installed in sequence on the surface of the reinforcement material on the free end side of the thermoplastic FRP lap bar-concrete bonding specimen, and the hollow tension and pressure sensor 8 is connected to the mechanical The calculation and analysis system 9 is connected; then, the load spring 602 is adjusted to a stress level of 10% σu, and the load is transmitted to the support plate 604 through the screws 603 on both sides. When the reading of the mechanical calculation and analysis system connected to the hollow tension and pressure sensor reaches 10% σu, the screw 603 is fixed by the nut 605 and the gasket 606 at the connection of the support plate to stabilize the tension and compression load acting on the end of the bonding sample; finally, the control slide rail 2 and the upper fixed plate 301 are removed, and the tension and compression load-environment coupling device with the sample to be tested is placed in an environmental box 10 prepared with a simulated seawater solution, and the constant temperature of the environmental box 10 is set to 60°C. The stress level is adjusted to 10% σu, 20% σu, 30% σu and 40% σu at 7d, 14d, 21d and 28d respectively. During the test, the tension and compression load and displacement changes monitored by the hollow tension and pressure sensor and the strain gauge are checked every 1d, and the load spring is dynamically adjusted to keep the reading of the mechanical calculation and analysis system constant.

[0070] The sensors, controllers and control programs that may be involved in the above description are all existing technologies and will not be described in detail here.

[0071] The embodiments of the present invention disclosed above are only used to help illustrate the present invention. The embodiments do not describe all the details in detail, nor do they limit the invention to the specific implementation methods described. According to the content of this specification, many modifications and changes can be made. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well.

Claims

1. An environmental-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars. It is characterized in that include: A loading device and an environmental chamber (10) for providing a constant temperature and a corrosive environmental solution for a tensile loading test; The holding device includes: An anchor assembly (1) is arranged at the end of the force-applying side and the load-bearing side of the thermoplastic FRP lap reinforcement (5) for tensile loading, and is used to provide a fixed end for stable tensile loading, wherein the thermoplastic FRP lap reinforcement (5) is connected to the concrete test block (4); The detachable fixing plate assembly (3) comprises an upper fixing plate (301) and a lower fixing plate (302) arranged at intervals, and a limiting assembly for fixing the upper fixing plate (301) and the lower fixing plate (302) relatively, wherein the concrete test block (4) is arranged between the upper fixing plate (301) and the lower fixing plate (302), and the anchor assembly (1) on the load-bearing side is pushed against the corresponding side end surface of the concrete test block (4); A load-holding reaction force device (6) is arranged between the anchor assembly (1) on the force-applying side and the concrete test block (4) and is used to provide an adjustable tensile load for the thermoplastic FRP lap reinforcement (5). A displacement meter (7) and a hollow tension sensor (8) are arranged on the force-applying side of the thermoplastic FRP lap reinforcement (5), and a mechanical calculation and analysis system (9) configured with the displacement meter (7) is used to monitor the displacement and tension changes of the thermoplastic FRP lap reinforcement (5) during the tensile loading process.

2. An environmental-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars according to claim 1, Features: The limiting assembly is four control slide rails (2) distributed in parallel at the four corners of the detachable fixed plate assembly (3), and the upper fixed plate (301) and the lower fixed plate (302) are connected to all the control slide rails (2).

3. The environment-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars according to claim 1, Features: The anchor assembly (1) comprises an anchor clip (101) and an anchor sleeve (102), wherein the length-to-diameter ratio of the anchor sleeve (102) is greater than the length-to-diameter ratio of the anchor clip (101), so that the anchor clip (101) and the end of the thermoplastic FRP lap rib (5) are pressed into the anchor sleeve (102) and clamped.

4. The environment-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars according to claim 1, Features: The load-bearing reaction force device (6) comprises a reaction force plate (601) sandwiched between a concrete test block (4) and a lower fixed plate (302), a screw rod (603) symmetrically arranged relative to the thermoplastic FRP lap rib (5) and connected at one end to the reaction force plate (601), a load-bearing spring (602) sleeved on each screw rod (603) and connected at one end to the reaction force plate (601), a support plate (604) connected to the other end of all the load-bearing springs (602), and a nut (605) and a gasket (606) connected to the other end of each screw rod (603) and connected to the end face of the support plate (604) away from the load-bearing spring (602), wherein the load-bearing spring (602) is used to dynamically adjust the tensile load size.

5. The environment-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars according to claim 1, Features: The upper fixing plate (301), the lower fixing plate (302), the reaction plate (601) and the support plate (604) are all arranged perpendicular to the thermoplastic FRP lap ribs (5) and are all provided with channels for the thermoplastic FRP lap ribs (5) to pass through.

6. An environmental-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars according to claim 5, Features: The two opposite surfaces of the thermoplastic FRP lap reinforcement (5) and the concrete test block (4) are kept perpendicular.

7. The environment-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars according to claim 1, Features: The environmental box (10) is a closed device for controlling a constant temperature and containing a corrosive solution environment, and is used to contain the holding device after the upper fixing plate (301), the lower fixing plate (302) and the limit assembly are removed in a corrosive solution environment at a constant temperature.

8. The environment-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars according to claim 1, Features: The diameter of the thermoplastic FRP lap rib (5) does not exceed 25 mm.

9. The environment-tensile loading coupling test device for testing the lap performance of thermoplastic FRP bars according to claim 1, Features: The surfaces of the load-bearing reaction force device (6) and the anchor assembly (1) are subjected to rust prevention treatment before entering the environmental chamber (10).

10. A test method using the environment-tensile loading coupling test device for testing the lap properties of thermoplastic FRP bars as claimed in claim 4, It is characterized in that The following steps are involved: S1, passing the thermoplastic FRP lap reinforcement (5) across a concrete test mold of standard size, pouring fresh concrete into the concrete test mold, and forming a concrete test block (4) after demoulding, thereby completing the preparation of the lap reinforcement-concrete bonding specimen; S2, installing an upper fixing plate (301) and a lower fixing plate (302) at the upper and lower ends of the concrete test block (4), and fixing the upper fixing plate (301) and the lower fixing plate (302) relatively by means of a limiting assembly; S3, respectively clamping the anchor clips (101) at both ends of the thermoplastic FRP lap rib (5), adjusting the anchor clips (101) on the upper fixing plate (301) to be close to the concrete test block (4), retaining a certain free section length between the anchor clips (101) on the lower fixing plate (302) and the lower fixing plate (302), and using a press to pre-press the anchor clips (101) at both ends into the anchor sleeve (102) to complete the anchoring; S4, sequentially installing a load-bearing reaction device (6), a displacement meter (7), and a hollow tension sensor (8) on the surface of the thermoplastic FRP lap rib (5) between the anchor clip (101) on the lower fixing plate (302) and the lower fixing plate (302), and connecting the hollow tension sensor (8) to the mechanical calculation and analysis system (9); S5. A tensile load is provided by adjusting the load spring (602). The load is transmitted to the support plate (604) through the screw rod (603). When the reading of the mechanical calculation analysis system (9) connected to the hollow tension sensor (8) reaches a preset value, a nut (605) and a gasket (606) are connected to the screw rod (603) and the support plate (604) is fixed to stabilize the tensile load acting on the end of the thermoplastic FRP lap rib (5). S6. After removing the control slide rail (2) and the upper fixed plate (301), the holding device is placed in a constant temperature corrosive solution in an environmental box (10) for a certain period of time. The displacement meter (7) and the hollow tension sensor (8) monitor the tensile load size and displacement change of the thermoplastic FRP lap rib (5). The holding spring (602) is dynamically adjusted to make the reading of the mechanical calculation and analysis system (9) constant. After a certain period of time, the performance of the thermoplastic FRP lap rib (5) is observed and recorded, and the test is completed.

Citation Information

Patent Citations

  • Constant-temperature stress corrosion testing device and method for FRP (fiber reinforced polymer) tendon

    CN103376222A

  • Testing method and device for measuring FRP (fiber reinforced polymer) and concrete adhesion performance under impact load action

    CN107036915A

  • Method for connecting fiber reinforce plastic ribs

    CN109955488A

  • Composite material tensile fixture with load and environment coupling effect and using method thereof

    CN111795889A

  • Mechanical property test method under long-term coupling of corrosion and tensile stress