Preparation method of semiconductor structure and semiconductor structure

By creating an air gap in the semiconductor structure, the problem of decreased sensing margin caused by the increase in DRAM bit line capacitance is solved, and the effect of improving chip sensing margin and data transmission efficiency is achieved.

CN118785697AActive Publication Date: 2024-10-15CHANGXIN MEMORY TECH INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202310351043.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15
Estimated Expiration
2043-03-31

AI Technical Summary

Technical Problem

As DRAM bit lines shrink, the capacitance between the bit lines and node contacts increases, causing the chip's sensing margin to decrease.

Method used

By forming air gaps between multiple bit line structures and storage node contact structures in the semiconductor structure, the capacitance between the storage node contact structures and the bit line structures is reduced, and the sensing margin is improved. The specific method includes forming a bit line stack structure and an isolation spacer on a substrate, forming a storage node contact structure and a gap trench therebetween, and filling the isolation layer to create a second air gap.

Benefits of technology

It effectively reduces the capacitance of the bit line structure and improves the chip's sensing margin and data transmission efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118785697A_ABST
    Figure CN118785697A_ABST
Patent Text Reader

Abstract

The invention relates to a preparation method of a semiconductor structure and the semiconductor structure. The preparation method of the semiconductor structure comprises the steps of providing a substrate; a plurality of bit line structures are formed on the upper surface of the substrate, each bit line structure comprises a bit line lamination structure and an isolation side wall located on the side wall of the bit line lamination structure, and a first air gap is formed in each isolation side wall; forming a storage node contact structure material layer between adjacent bit line structures; the storage node contact structure material layer is etched to obtain a storage node contact structure and a first gap groove, and the first gap groove is located between the bit line structure and the storage node contact structure; forming a first isolation layer in the first gap groove, wherein a second air gap is formed in the first isolation layer; due to the existence of the first air gap and the second air gap, the capacitance between the storage node contact structure and the bit line structure can be reduced, so that the overall capacitance of the bit line structure can be reduced, and the sensing margin of the chip can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of semiconductor technology, and in particular to a method for preparing a semiconductor structure and a semiconductor structure. Background Art

[0002] With the development of dynamic random access memory (DRAM), the size of its bit line (BL) and word line (WL) is designed to be smaller and smaller, resulting in higher and higher capacitance of the bit line (C_BL). For example, the reduction of the bit line size may cause the capacitance (C_BL / NC) between the BL and the node contact (NC) to become higher, and usually C_BL / NC contributes about 40% to the capacitance of C_BL. Therefore, when C_BL / NC becomes higher, the overall capacitance of C_BL also becomes higher. Too high bit line capacitance will cause the sensing margin of the chip to decrease. Summary of the invention

[0003] Based on this, it is necessary to provide a method for preparing a semiconductor structure and a semiconductor structure to address the problem of reduced sensing margin of the above-mentioned chip.

[0004] In order to achieve the above objectives, on the one hand, the present disclosure provides a method for preparing a semiconductor structure, comprising:

[0005] providing a substrate;

[0006] forming a plurality of bit line structures on the upper surface of the substrate, wherein the bit line structures include a bit line stack structure and an isolation sidewall located on a sidewall of the bit line stack structure, wherein the isolation sidewall has a first air gap;

[0007] forming a storage node contact structure material layer between adjacent bit line structures;

[0008] Etching the storage node contact structure material layer to obtain a storage node contact structure and a first gap groove, wherein the first gap groove is located between the bit line structure and the storage node contact structure;

[0009] A first isolation layer is formed in the first gap groove, wherein the first isolation layer has a second air gap.

[0010] The method for preparing the semiconductor structure is as follows: a plurality of bit line structures are formed on the upper surface of the substrate, wherein the bit line structure includes a bit line stack structure and an isolation sidewall located on the sidewall of the bit line stack structure, wherein the isolation sidewall has a first air gap, a storage node contact structure material layer is formed between adjacent bit line structures, and the storage node contact structure material layer is etched to obtain a storage node contact structure and a first gap groove, wherein the first gap groove is located between the bit line structure and the storage node contact structure, and a first isolation layer is formed in the first gap groove, wherein the first isolation layer has a second air gap. Due to the presence of the first air gap and the second air gap, the capacitance between the storage node contact structure and the bit line structure can be reduced, thereby reducing the capacitance of the bit line structure as a whole, thereby improving the sensing margin of the chip.

[0011] In one embodiment, providing a substrate comprises:

[0012] providing a substrate;

[0013] forming a shallow trench isolation structure in the substrate, wherein the shallow trench isolation structure isolates a plurality of active areas arranged in an array at intervals in the substrate;

[0014] forming a first dielectric layer on the upper surface of the substrate;

[0015] A plurality of bit line contact holes are formed in the base and the first dielectric layer to form the substrate.

[0016] In one embodiment, a plurality of bit line structures are formed on the upper surface of the substrate, including:

[0017] Filling the bit line contact structure material layer in the bit line contact hole, and forming an initial bit line stack on the bit line contact structure material layer;

[0018] Patterning the initial bit line stack, the bit line contact structure material layer and the first dielectric layer to form a bit line stack structure, a bit line contact structure and second gap grooves located on both sides of the bit line contact structure, wherein the top of the bit line contact structure contacts the bottom of the bit line stack structure, and the bit line contact structure contacts the active area below the bit line contact hole;

[0019] A second isolation structure is formed in the second gap groove, a second dielectric layer is formed on the surface of the second isolation structure and the surface of the substrate, and an isolation sidewall is formed on the sidewall of the bit line stack structure.

[0020] In one embodiment, after forming a plurality of bit line structures on the upper surface of the substrate and before forming a storage node contact structure material layer between adjacent bit line structures, the method further includes:

[0021] The second dielectric layer and the substrate are etched to form a contact hole, wherein the contact hole exposes a portion of the active area; and the storage node contact structure material layer also fills the contact hole.

[0022] In one embodiment, the bit line stack structure includes a conductive layer and a passivation layer; the initial bit line stack is formed on the bit line contact structure material layer, including:

[0023] forming a conductive material layer on the upper surface of the bit line contact structure material layer;

[0024] forming a passivation material layer on the upper surface of the conductive material layer;

[0025] The patterning of the initial bit line stack comprises:

[0026] The passivation material layer and the conductive material layer are etched to obtain a plurality of the bit line stack structures arranged at intervals, the remaining passivation material layer is used as a passivation layer, and the remaining conductive material layer is used as a conductive layer.

[0027] In one embodiment, forming an isolation spacer on the sidewall of the bit line stack structure includes:

[0028] forming a first spacer on a sidewall of the bit line stack structure;

[0029] forming a first sacrificial layer on the surface of the first sidewall;

[0030] forming a second sidewall spacer on a surface of the first sidewall spacer and a surface of the first sacrificial layer;

[0031] The first sacrificial layer is removed to form the first air gap, and the first sidewall spacer, the first air gap and the second sidewall spacer constitute the isolation sidewall spacer.

[0032] In one embodiment, forming a first isolation layer in the first gap groove, wherein the first isolation layer has a second air gap, comprises:

[0033] The first isolation layer is formed in the first gap groove by a deposition process, and the first isolation layer has the second air gap therein.

[0034] In one embodiment, forming a first isolation layer in the first gap groove, wherein the first isolation layer has a second air gap, comprises:

[0035] forming a first sub-isolation layer on the sidewall and bottom of the first gap groove;

[0036] forming a second sacrificial layer on a surface of the first sub-isolation layer;

[0037] forming a second sub-isolation layer on the surface of the second sacrificial layer, wherein the first sub-isolation layer, the second sacrificial layer and the second sub-isolation layer together fill the first gap groove;

[0038] removing the second sacrificial layer to form a sacrificial gap;

[0039] A third sub-isolating layer is formed, wherein the third sub-isolating layer fills a portion of the sacrificial gap to form the second air gap.

[0040] On the other hand, the present disclosure further provides a semiconductor structure, the semiconductor structure comprising:

[0041] substrate;

[0042] A plurality of bit line structures are located on the upper surface of the substrate, wherein the bit line structures include a bit line stack structure and an isolation sidewall located on a sidewall of the bit line stack structure, and a first air gap is formed in the isolation sidewall;

[0043] A storage node contact structure located between the bit line structures;

[0044] The first isolation layer is located between the bit line structure and the storage node contact structure, and a second air gap is formed in the first isolation layer.

[0045] The semiconductor structure includes: a substrate, a plurality of bit line structures, a storage node contact structure and a first isolation layer. The plurality of bit line structures are located on the upper surface of the substrate, the bit line structure includes a bit line stack structure and an isolation sidewall located on the sidewall of the bit line stack structure, and the isolation sidewall has a first air gap. The storage node contact structure is located between the bit line structures. The first isolation layer is located between the bit line structure and the storage node contact structure, and the first isolation layer has a second air gap. Due to the existence of the first air gap and the second air gap, the capacitance between the storage node contact structure and the bit line structure can be reduced, thereby reducing the capacitance of the bit line structure as a whole, thereby improving the sensing margin of the chip.

[0046] In one embodiment, the substrate comprises:

[0047] A substrate, wherein the substrate has a shallow trench isolation structure, wherein the shallow trench isolation structure isolates a plurality of active areas arranged at intervals in the substrate;

[0048] A plurality of spaced-apart bit line contact holes are located in the substrate;

[0049] A second isolation trench is located in the bit line contact hole;

[0050] A dielectric layer, located on the upper surface of the substrate;

[0051] The semiconductor structure also includes a plurality of bit line contact structures located in the bit line contact holes, which are arranged one by one corresponding to the bit line contact holes, and the bit line contact structures penetrate the dielectric layer and the second isolation layer along the thickness direction, the top of the bit line contact structure contacts the bottom of the bit line stack structure, and the bit line contact structure contacts the active area below the bit line contact holes.

[0052] In one of the embodiments, the storage node contact structure also penetrates the dielectric layer along the thickness direction and extends into the substrate to contact the active area.

[0053] In one embodiment, the bit line stack structure includes a conductive layer and a passivation layer, and the storage node contact structure includes:

[0054] A contact structure located between conductive layers of adjacent bit line structures;

[0055] The contact pad is located between the upper surface of the contact structure and the passivation layer of the bit line structure and partially covers the top of the passivation layer.

[0056] In one embodiment, the first isolation layer is located between the contact pad and the bit line structure.

[0057] In one embodiment, a plurality of the bit line structures are arranged at intervals along a first direction and extend along a second direction, and a plurality of the storage node contact structures are arranged in an array along the first direction and the second direction; in two rows of the storage node contact structures arranged adjacent to each other along the second direction, a second air gap is provided between one row of the storage node contact structures and the bit line structures adjacent to the first side of the first direction, and a second air gap is provided between the other row of the storage node contact structures and the bit line structures adjacent to the second side of the first direction.

[0058] In one embodiment, in each of the first isolation layers, the number of the second air gaps is one or more. BRIEF DESCRIPTION OF THE DRAWINGS

[0059] In order to more clearly illustrate the technical solutions in the embodiments of the present disclosure or the conventional technology, the drawings required for use in the embodiments or the conventional technology descriptions will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present disclosure, and for ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0060] Figure 1 A schematic diagram of a process for preparing a semiconductor structure provided in an embodiment of the present disclosure;

[0061] Figure 2 A schematic flow chart of a step of providing a substrate in a method for preparing a semiconductor structure provided in an embodiment of the present disclosure;

[0062] Figure 3 A schematic diagram of a cross-sectional structure of a substrate provided in some embodiments of the present disclosure;

[0063] Figure 4 In some embodiments of the present disclosure, Figure 3 A schematic cross-sectional structure diagram of a shallow trench isolation structure formed in a substrate is shown;

[0064] Figure 5 In some embodiments of the present disclosure, Figure 4 A schematic cross-sectional structure diagram of a first dielectric layer formed on the structure shown;

[0065] Figure 6 In some embodiments of the present disclosure, Figure 5 A schematic cross-sectional view of a structure in which a plurality of bit line contact holes are formed in the structure shown;

[0066] Figure 7 A schematic flow chart of the steps of forming a plurality of bit line structures in a method for preparing a semiconductor structure provided in an embodiment of the present disclosure;

[0067] Figure 8 In some embodiments of the present disclosure, Figure 6 A schematic diagram of a cross-sectional structure of a bit line contact structure material layer formed in a bit line contact hole shown;

[0068] Fig. 9 A schematic flow chart of a step of forming an initial bit line stack in a method for preparing a semiconductor structure provided in an embodiment of the present disclosure;

[0069] Fig.10 In some embodiments of the present disclosure, Figure 8 A schematic cross-sectional structure diagram of a conductive material layer formed on the structure shown;

[0070] Fig.11 In some embodiments of the present disclosure, Fig.10 A schematic cross-sectional structure diagram of a passivation material layer formed on the structure shown;

[0071] Fig.12 The etching method provided in some embodiments of the present disclosure Fig.11 The structure shown is a schematic diagram of a cross-sectional structure of forming a bit line stack structure and a second gap groove;

[0072] Fig.13 A schematic diagram of a top view of a structure in which a second isolation structure, a second dielectric layer, and an isolation sidewall are formed in some embodiments of the present disclosure;

[0073] Fig.14 for Fig.13 Schematic diagram of the cross-sectional structure of the structure along the A-A' direction;

[0074] Fig.15 A schematic flow chart of a step of forming an isolation spacer in a method for preparing a semiconductor structure provided in an embodiment of the present disclosure;

[0075] Fig.16 In some embodiments of the present disclosure, Fig.12 A schematic cross-sectional structural diagram of a sidewall of a bit line stack structure in the structure shown forming a first spacer;

[0076] Fig.17 In some embodiments of the present disclosure, Fig.16 A schematic cross-sectional view of the structure in which the first sacrificial layer is formed;

[0077] Fig.18 In some embodiments of the present disclosure, Fig.17 A schematic diagram of a cross-sectional structure of a second side wall formed in the structure shown;

[0078] Fig.19 In some embodiments of the present disclosure, Fig.18 A schematic diagram of a cross-sectional structure after removing the first sacrificial layer from the structure shown;

[0079] Fig. 20 In some embodiments of the present disclosure, Fig.19 A schematic diagram of a cross-sectional structure of a contact hole formed in the structure shown;

[0080] Fig.21 In some embodiments of the present disclosure, Fig. 20 A schematic diagram of a cross-sectional structure of a material layer forming a storage node contact structure in the structure shown;

[0081] Fig. 22 In some embodiments of the present disclosure, Fig.21 A schematic diagram of a cross-sectional structure of a first gap groove formed in the structure shown;

[0082] Fig.23 A schematic diagram of a top view of a structure in which a first isolation layer and a second air gap are formed in some embodiments of the present disclosure;

[0083] Fig.24 for Fig.23 Schematic diagram of the cross-sectional structure of the structure along the A-A' direction;

[0084] Fig.25A schematic diagram of a top view of a structure in which a first isolation layer and a second air gap are formed by a deposition process in some other embodiments of the present disclosure;

[0085] Fig.26 for Fig.25 Schematic diagram of the cross-sectional structure of the structure along the A-A' direction;

[0086] Fig. 27 A schematic flow chart of the steps of forming a first isolation layer and a second air gap in a method for preparing a semiconductor structure provided in an embodiment of the present disclosure;

[0087] Fig.28 In some embodiments of the present disclosure, Fig. 20 A schematic cross-sectional structure diagram of forming a first sub-isolation layer in the structure shown;

[0088] Fig.29 In some embodiments of the present disclosure, Fig.26 A schematic cross-sectional view of the structure in which a second sacrificial layer is formed;

[0089] Fig.30 In some embodiments of the present disclosure, Fig. 27 A schematic cross-sectional structure diagram of forming a second sub-isolation layer in the structure shown;

[0090] Fig.31 In some embodiments of the present disclosure, Fig.28 A schematic cross-sectional view of the structure in which the second sacrificial layer is removed to form a sacrificial gap;

[0091] Fig.32 In some embodiments of the present disclosure, Fig.29 The schematic cross-sectional structure diagram shows a structure in which a third sub-isolation layer is formed in the structure to fill part of the sacrificial gap to form a second air gap.

[0092] Description of reference numerals: 10-substrate, 101-active region, 102-shallow trench isolation structure, 103-second gap groove, 104-second isolation structure, 20-dielectric layer, 201-first dielectric layer, 2011-bit line contact hole, 202-second dielectric layer, 203-contact hole, 30-bit line structure, 301-bit line contact structure, 301a-bit line contact structure material layer, 302-bit line stack structure, 302a-initial bit line stack, 3021-conductive layer, 3021a-conductive material layer, 302 2-passivation layer, 3022a-passivation material layer, 303-isolation side wall, 3031-first side wall, 3032-first sacrificial layer, 3033-second side wall, 3034-first air gap, 50-storage node contact structure, 501-storage node contact structure material layer, 60-first isolation layer, 601-first gap groove, 602-second air gap, 602a-sacrificial gap, 603-first sub-isolation layer, 604-second sacrificial layer, 605-second sub-isolation layer, 606-third sub-isolation layer. DETAILED DESCRIPTION

[0093] In order to facilitate understanding of the present disclosure, the present disclosure will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present disclosure are shown in the drawings. However, the present disclosure can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present disclosure more thorough and comprehensive.

[0094] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present disclosure. The terms used herein in the specification of the present disclosure are only for the purpose of describing specific embodiments and are not intended to limit the present disclosure.

[0095] It should be understood that when an element or layer is referred to as being "on, adjacent to, connected to or coupled to other elements or layers, it may be directly on, adjacent to, connected to or coupled to other elements or layers, or there may be intervening elements or layers. On the contrary, when an element is referred to as being "directly on, directly adjacent to, directly connected to or directly coupled to other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers, doping types and / or parts, these elements, components, regions, layers, doping types and / or parts should not be limited by these terms. These terms are merely used to distinguish one element, component, region, layer, doping type or part from another element, component, region, layer, doping type or part. Therefore, without departing from the teachings of the present disclosure, the first element, component, region, layer, doping type or portion discussed below may be represented as a second element, component, region, layer or portion; for example, the first doping type may be referred to as the second doping type, and similarly, the second doping type may be referred to as the first doping type; the first doping type and the second doping type are different doping types, for example, the first doping type may be P-type and the second doping type may be N-type, or the first doping type may be N-type and the second doping type may be P-type.

[0096] Spatially relative terms such as "under," "beneath," "below," "under," "above," "above," and the like may be used herein to describe the relationship of an element or feature shown in the figures to other elements or features. It should be understood that, in addition to the orientations shown in the figures, spatially relative terms also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is flipped, an element or feature described as "under other elements" or "under it" or "under it" will be oriented as being "above" the other elements or features. Thus, the exemplary terms "under" and "under" may include both upper and lower orientations. In addition, the device may also include additional orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptors used herein are interpreted accordingly.

[0097] When used herein, the singular forms "a", "an", and "said / the" may also include plural forms, unless the context clearly indicates otherwise. It should also be understood that when the terms "consisting of" and / or "comprising" are used in this specification, the presence of the features, integers, steps, operations, elements and / or parts can be determined, but the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups is not excluded. At the same time, when used herein, the term "and / or" includes any and all combinations of the relevant listed items.

[0098] Embodiments of the invention are described herein with reference to cross-sectional views which are schematic representations of ideal embodiments (and intermediate structures) of the present disclosure, such that variations in the shapes shown due to, for example, manufacturing techniques and / or tolerances are anticipated. Thus, embodiments of the present disclosure should not be limited to the particular shapes of the regions shown herein, but rather include deviations in shapes due to, for example, manufacturing techniques. For example, an implanted region shown as a rectangle typically has rounded or curved features and / or an implant concentration gradient at its edges rather than a binary change from an implanted region to a non-implanted region. Similarly, a buried region formed by implantation may result in some implantation in the region between the buried region and the surface through which the implantation is performed. Thus, the regions shown in the figures are schematic in nature, their shapes do not represent the actual shape of the region of the device, and do not limit the scope of the present disclosure.

[0099] like Figure 1 As shown, the present disclosure provides a method for preparing a semiconductor structure, and the method for preparing a semiconductor structure may include the following steps:

[0100] S101: providing a substrate;

[0101] S102: forming a plurality of bit line structures on the upper surface of the substrate, the bit line structures comprising a bit line stack structure and an isolation sidewall located on a sidewall of the bit line stack structure, wherein a first air gap is formed in the isolation sidewall;

[0102] S103: forming a storage node contact structure material layer between adjacent bit line structures 30;

[0103] S104: etching the storage node contact structure material layer to obtain a storage node contact structure and a first gap groove, wherein the first gap groove is located between the bit line structure and the storage node contact structure;

[0104] S105: forming a first isolation layer in the first gap groove, wherein the first isolation layer has a second air gap.

[0105] The method for preparing the semiconductor structure is as follows: a plurality of bit line structures are formed on the upper surface of the substrate, wherein the bit line structure includes a bit line stack structure and an isolation sidewall located on the sidewall of the bit line stack structure, wherein the isolation sidewall has a first air gap, a storage node contact structure material layer is formed between adjacent bit line structures, and the storage node contact structure material layer is etched to obtain a storage node contact structure and a first gap groove, wherein the first gap groove is located between the bit line structure and the storage node contact structure, and a first isolation layer is formed in the first gap groove, wherein the first isolation layer has a second air gap. Due to the presence of the first air gap and the second air gap, the capacitance between the storage node contact structure and the bit line structure and the capacitance between adjacent storage node contact structures 50 can be reduced, thereby reducing the capacitance of the entire bit line structure, thereby improving the sensing margin of the chip and improving the data transmission efficiency.

[0106] In step S101, refer to Figure 1 Step S101 in Figure 2-Figure 6 , providing a substrate.

[0107] In one embodiment, Figure 2 As shown, the above step S101 includes:

[0108] S1011: providing a substrate;

[0109] S1012: forming a shallow trench isolation structure in the substrate, wherein the shallow trench isolation structure isolates a plurality of active areas arranged in an array at intervals in the substrate;

[0110] S1013: forming a first dielectric layer on the upper surface of the substrate;

[0111] S1014: forming a plurality of bit line contact holes in the base and the first dielectric layer to form a substrate.

[0112] In step S1011, Figure 3 As shown, a substrate 10 is provided.

[0113] Among them, the material of the substrate 10 can be any suitable substrate material known in the art, for example, it can be at least one of the following materials: silicon (Si), germanium (Ge), red phosphorus, silicon germanium (SiGe), silicon carbide (SiC), carbon germanium silicon (SiGeC), indium arsenide (InAs), gallium arsenide (GaAs), indium phosphide (InP) or other III / V compound semiconductors, including multilayer structures composed of these semiconductors, or silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) and germanium on insulator (GeOI), or it can also be double-sided polished silicon wafers (Double Side Polished Wafers, DSP), or it can be a ceramic substrate such as alumina, a quartz or glass substrate, etc., and this embodiment is not limited here.

[0114] In step S1011, Figure 4 As shown, a shallow trench isolation structure 102 can be formed in the substrate 10 by combining processes such as photolithography, etching, and deposition. The shallow trench isolation structure 102 isolates a plurality of active areas 101 arranged in an array in the substrate 10. The formation process of the shallow trench isolation structure 102 and the active area 101 is relatively common and will not be repeated here.

[0115] Among them, the dielectric material filled in the shallow trench isolation (STI) structure can be any suitable dielectric material known in the art, for example, it can be a combination of one or more of silicon dioxide, fluorosilicate glass, undoped silicate glass (USG) or tetraethyl orthosilicate, and this embodiment is not limited here.

[0116] In step S1011, Figure 5 As shown, a first dielectric layer 201 can be formed on the upper surface of the substrate 10 by a deposition process, such as an atomic layer deposition (ALD) process, a physical vapor deposition (PVD) process, a chemical vapor deposition (CVD) process, etc., which is not limited in this embodiment.

[0117] The material of the first dielectric layer 201 may include at least one of silicon oxide, silicon oxynitride, silicon oxycarbide and silicon oxynitride and carbonitride.

[0118] In step S1011, Figure 6 As shown, photolithography, etching and other processes may be combined to form a plurality of bit line contact holes 2011 in the base 10 and the first dielectric layer 201 to form a substrate.

[0119] In step S102, refer to Figure 1 Step S101 in Figure 7-Figure 19 A plurality of bit line structures 30 are formed on the upper surface of the substrate. The bit line structure 30 includes a bit line stack structure 302 and an isolation spacer 303 located on the sidewall of the bit line stack structure 302 . The isolation spacer 303 has a first air gap 3034 therein.

[0120] In one embodiment, Figure 7 As shown, the above step S102 includes:

[0121] S1021: filling a bit line contact structure material layer in the bit line contact hole, and forming an initial bit line stack on the bit line contact structure material layer;

[0122] S1022: patterning the initial bit line stack, the bit line contact structure material layer and the first dielectric layer to form a bit line stack structure, a bit line contact structure and second gap grooves located on both sides of the bit line contact structure, wherein the top of the bit line contact structure contacts the bottom of the bit line stack structure, and the bit line contact structure contacts the active area below the bit line contact hole;

[0123] S1023: forming a second isolation structure in the second gap groove, forming a second dielectric layer on the surface of the second isolation structure and the surface of the substrate, and forming an isolation sidewall on the sidewall of the bit line stack structure.

[0124] In step S1021, if Figure 8 As shown, a deposition process can be used to fill the bit line contact structure material layer 301a in the bit line contact hole 2011. During the deposition process, part of the bit line contact structure material layer 301a will also cover the surface of the first dielectric layer 201. The material of the bit line contact structure material layer 301a can include polysilicon.

[0125] In one embodiment, the bit line stack structure includes a conductive layer and a passivation layer, such as Fig. 9 As shown, the step of forming an initial bit line stack on the bit line contact structure material layer in the above step S1021 includes:

[0126] S1021a: forming a conductive material layer on an upper surface of the bit line contact structure material layer;

[0127] S1021b: forming a passivation material layer on the upper surface of the conductive material layer.

[0128] In step S1021a, if Fig.10 As shown, a deposition process may be used to form a conductive material layer 3021a on the upper surface of the bit line contact structure material layer 301a. The material of the conductive material layer 3021a may include tungsten (W), cobalt (Co), molybdenum (Mo), ruthenium (Ru), copper (Cu), aluminum (Al), titanium (Ti), tantalum (Ta) or other metals.

[0129] In step S1021a, if Fig.11 As shown, a passivation material layer 3022a is formed on the upper surface of the conductive material layer 3021a. The material of the passivation material layer 3022a may include nitride, for example, silicon nitride (SiN).

[0130] In step S1022, if Fig.12 As shown, the initial bit line stack 302a, the bit line contact structure material layer 301a and the first dielectric layer 201 are patterned to form a bit line stack structure 302, a bit line contact structure 301 and second gap grooves 103 located on both sides of the bit line contact structure 301, the top of the bit line contact structure 301 contacts the bottom of the bit line stack structure 302, and the bit line contact structure 301 contacts the active area 101 below the bit line contact hole 2011.

[0131] The material of the second isolation structure 104 may include nitride, for example, silicon nitride (SiN). The material of the second dielectric layer 202 may include at least one of silicon oxide, silicon oxynitride, silicon oxycarbide, and silicon oxynitride and carbon oxynitride.

[0132] The step of patterning the initial bit line stack in the above step S1022 includes: etching the passivation material layer and the conductive material layer to obtain a plurality of bit line stack structures arranged at intervals.

[0133] like Figure 11-Figure 12 As shown, the passivation material layer 3022 a and the conductive material layer 3021 a are etched to obtain a plurality of spaced-apart bit line stack structures 302 , wherein the remaining passivation material layer 3022 a serves as the passivation layer 3022 , and the remaining conductive material layer 3021 a serves as the conductive layer 3021 .

[0134] In step S1023, if Fig.13 as well as Fig.14 As shown, a second isolation structure 104 is formed in the second gap groove 103 , a second dielectric layer 202 is formed on the surface of the second isolation structure 104 and the surface of the substrate, and an isolation spacer 303 is formed on the sidewall of the bit line stack structure 302 .

[0135] in, Fig.14 Can be regarded as Fig.13 The schematic diagram of the cross-sectional structure of the structure along the A-A' direction. In order to facilitate the understanding of this scheme, Fig.13 3 shows the positions of the first air gaps 3034 in the isolation sidewall 303 in the top view of the structure. However, it should be noted that, in fact, the first air gaps 3034 will not be exposed. Fig.13 This is only an example of the semiconductor structure of the present application, and the embodiments of the present disclosure should not be limited to such Fig.13 The specific shapes shown are intended to include deviations in shapes that result, for example, from manufacturing techniques.

[0136] In one embodiment, Fig.15 As shown, the step of forming an isolation spacer on the sidewall of the bit line stack structure in the above step S1023 includes:

[0137] S1023a: forming a first spacer on a sidewall of the bit line stack structure;

[0138] S1023b: forming a first sacrificial layer on the surface of the first sidewall;

[0139] S1023c: forming a second sidewall spacer on a surface of the first sidewall spacer and a surface of the first sacrificial layer;

[0140] S1023d: remove the first sacrificial layer to form a first air gap, and the first sidewall spacer, the first air gap and the second sidewall spacer constitute an isolation sidewall spacer.

[0141] In step S1023a, if Fig.16 As shown, a process combining deposition and etching can be used to form the first sidewall 3031 on the sidewall of the bitline stack structure 302. For example, a deposition process can be used to deposit the first sidewall 3031 material layer, and then an etching process (such as dry etching) can be used, thereby utilizing the anisotropic characteristics of the dry etching process to retain the first sidewall 3031 material layer located on the sidewall of the bitline stack structure 302, thereby forming the first sidewall 3031.

[0142] In step S1023b, if Fig.17 As shown, a first sacrificial layer 3032 is formed on the surface of the first sidewall spacer 3031 .

[0143] In step S1023b, if Fig.18 As shown, a second sidewall spacer 3033 is formed on the surface of the first sidewall spacer 3031 and the surface of the first sacrificial layer 3032 .

[0144] In step S1023b, if Fig.19 As shown, the first sacrificial layer 3032 is removed to form a first air gap 3034 , and the first spacer 3031 , the first air gap 3034 and the second spacer 3033 constitute the isolation spacer 303 .

[0145] The materials of the first sidewall 3031 and the second sidewall 3033 may be the same, and the material of the first sacrificial layer 3032 is different from the materials of the first sidewall 3031 and the second sidewall 3033 .

[0146] Optionally, a suitable removal process (such as a wet process) can be used to utilize the difference between the etching selectivity ratios of the first sacrificial layer 3032 and the first side wall 3031 and the second side wall 3033, so that the first sacrificial layer 3032 can be removed while retaining the first side wall 3031 and the second side wall 3033, thereby forming a first air gap 3034 located between the first side wall 3031 and the second side wall 3033, so that the first side wall 3031, the first air gap 3034 and the second side wall 3033 constitute an isolation side wall 303.

[0147] Optionally, the number of the first air gaps 3034 in the isolation sidewall 303 may be one or more. Further, when the number of the first air gaps 3034 in the isolation sidewall 303 is multiple, the multiple first air gaps 3034 may still be formed by removing the corresponding sacrificial layer to form the first air gaps 3034.

[0148] In one embodiment, after the above step S102 and before the above step S103, the method for preparing the semiconductor structure further includes: etching the second dielectric layer and the substrate to form a contact hole.

[0149] like Fig. 20 As shown, the contact hole 203 exposes a portion of the active area 101 ; the storage node contact structure material layer 501 also fills up the contact hole 203 .

[0150] In step S103, refer to Figure 1 Step S103 in Fig.21 A storage node contact structure material layer 501 may be formed between adjacent bit line structures using a suitable deposition process (eg, PVD, CVD, or ALD, etc.).

[0151] In step S104, refer to Figure 1 Step S104 in Fig. 22 , the storage node contact structure material layer is etched to obtain the storage node contact structure and the first gap groove 601, and the first gap groove 601 is located between the bit line structure and the storage node contact structure. In the process of forming the first gap groove 601 by etching, part of the isolation sidewall is also removed at the same time. The first gap groove 601 exposes the first air gap 3034 in the isolation sidewall, and the bottom surface of the first gap groove 601 is higher than the top surface of the conductive layer 3021, and the isolation sidewall of the sidewall of the conductive layer 3021 is retained to protect the conductive layer 3021.

[0152] In step S104, refer to Figure 1 Step S104 in Figure 23-Figure 32 , a first isolation layer 60 is formed in the first gap groove 601, and a second air gap 602 is provided in the first isolation layer 60. The first isolation layer 60 seals the exposed first air gap 3034 to prevent the etching liquid from entering the first air gap 3034 and damaging the first sidewall 3031 and the conductive layer 3021 when the second air gap 602 is formed. The bottom of the second air gap 602 formed finally is higher than the top surface of the conductive layer 3021, and the second air gap 602 is not connected to the first air gap 3034.

[0153] In some embodiments, the first sacrificial layer 3032 may not be removed before forming the first gap groove 601, but a portion of the isolation spacer 303 may be removed when forming the first gap groove 601, and then the exposed first sacrificial layer 3032 may be removed along the first gap groove 601 to form a first air gap 3034. The first spacer 3031, the first air gap 3034, and the second spacer 3032 constitute the isolation spacer 303. Therefore, the isolation spacer 303 does not need to be additionally processed to expose the first sacrificial layer 3032, which can improve process efficiency.

[0154] like Fig.23 as well as Fig.24 As shown, Fig.23 It can be a schematic diagram of a top view of a structure in which a second air gap 602 is formed in some embodiments. Fig.24 Can be Fig.23 Schematic diagram of the cross-sectional structure of the structure along the A-A' direction. Fig.23 In the embodiment, the second air gap 602 may be an annular gap in a top view, resulting in Fig.24 The cross section in FIG. 1 shows two second air gaps 602, and the bottoms of the two second air gaps 602 may be connected or disconnected. In addition, in order to facilitate understanding of this solution, Fig.23 Schematically illustrates the position of each second air gap 602 in the top view of the structure, but it should be noted that, in fact, the second air gap 602 will not be exposed.

[0155] Due to the existence of the first air gap 3034 and the second air gap 602, the dielectric constant of air is relatively low. Therefore, the use of the first air gap 3034 and the second air gap 602 can reduce the capacitance, thereby reducing the capacitance (C_BL / NC) between the storage node contact structure 50 and the bit line structure 30 and the capacitance between adjacent storage node contact structures 50, thereby reducing the overall capacitance (C_BL) of the bit line structure 30, thereby improving the sensing margin of the chip.

[0156] In addition, in each first isolation layer 60, the number of the second air gaps 602 may be one or more, and the number of the second air gaps 602 in each first isolation layer 60 may be controlled by selecting a suitable process. Fig.24 In the embodiment, the number of the second air gaps 602 is two, but according to specific process requirements, through some appropriate process steps, multiple second air gaps 602 can also be formed in the first isolation layer 60. This embodiment does not limit the number of the second air gaps 602.

[0157] In one embodiment, the step S104 includes: forming a first isolation layer in the first gap groove by a deposition process, wherein the first isolation layer has a second air gap.

[0158] like Fig.25 as well as Fig.26 As shown, Fig.25 It may be a schematic diagram of a top view of a structure in which a second air gap 602 is formed by a deposition process in some other embodiments. Fig.26 Can be Fig.25 The schematic diagram of the cross-sectional structure of the structure along the A-A' direction. In order to facilitate the understanding of this scheme, Fig.25Schematically illustrates the position of each second air gap 602 in the top view of the structure, but it should be noted that, in fact, the second air gap 602 will not be exposed.

[0159] When the first isolation layer 60 is formed in the first gap groove 601 by a deposition process, due to the characteristics of the deposition process, the first isolation layer 60 will first be deposited on the sidewalls and the bottom of the first gap groove 601, and then the first isolation layer 60 located on both sidewalls of the same first gap groove 601 will slowly close to the middle position in the first gap groove 601 as the deposition time increases. Generally, in order to ensure the integrity of the first isolation layer 60, the first isolation layer 60 on both sidewalls can usually be closed as much as possible by controlling the corresponding process parameters (such as controlling the deposition time, or changing the ratio of each deposition gas, etc.) to avoid the first isolation layer 60 from forming a void in the middle position of the first gap groove 601. In this embodiment, by controlling the above-mentioned corresponding process parameters, the void formed by the first isolation layer 60 in the middle position of the first gap groove 601 can be cleverly retained, so that the void formed in the middle position of the first gap groove 601 can be directly used as the second air gap 602, so that the first isolation layer 60 has the second air gap 602.

[0160] In one embodiment, Fig. 27 As shown, the above step S104 includes:

[0161] S1041: forming a first sub-isolation layer on the sidewall and bottom of the first gap groove;

[0162] S1042: forming a second sacrificial layer on a surface of the first sub-isolation layer;

[0163] S1043: forming a second sub-isolation layer on the surface of the second sacrificial layer, wherein the first sub-isolation layer, the second sacrificial layer and the second sub-isolation layer together fill the first gap groove;

[0164] S1044: removing the second sacrificial layer to form a sacrificial gap;

[0165] S1045: forming a third sub-isolation layer, wherein the third sub-isolation layer fills a portion of the sacrificial gap to form a second air gap.

[0166] In step S1041, if Fig.28 As shown, in order to facilitate the understanding of this scheme, Fig.28 Can be regarded as Fig.24 , a first sub-isolation layer 603 may be formed on the sidewall and bottom of the first gap groove 601 by a deposition process.

[0167] In step S1042, if Fig.29As shown, a second sacrificial layer 604 is formed on the surface of the first sub-isolation layer 603 .

[0168] In step S1043, if Fig.30 As shown, a second sub-isolation layer 605 is formed on the surface of the second sacrificial layer 604 , and the first sub-isolation layer 603 , the second sacrificial layer 604 , and the second sub-isolation layer 605 together fill up the first gap 601 .

[0169] In step S1044, if Fig.31 As shown, the second sacrificial layer 604 is removed to form a sacrificial gap 602a.

[0170] The material of the first sub-isolation layer 603 may be the same as the material of the second sub-isolation layer 605, and the material of the second sacrificial layer 604 is different from the materials of the first sub-isolation layer 603 and the second sub-isolation layer 605. Exemplarily, the material of the second sacrificial layer 604 may include a metal material, for example, tungsten (W).

[0171] Optionally, a suitable removal process (e.g., a wet process) can be used to utilize the difference in etching selectivity between the second sacrificial layer 604 and the first sub-isolation layer 603 and the second sub-isolation layer 605, thereby removing the first sacrificial layer 3032 while retaining the first sub-isolation layer 603 and the second sub-isolation layer 605, thereby forming a sacrificial gap located between the first sub-isolation layer 603 and the second sub-isolation layer 605.

[0172] Furthermore, the number of the second air gaps 602 may be one or more. When the number of the second air gaps 602 is multiple, multiple second air gaps 602 may be formed by removing the sacrificial layer in a similar manner to the above step or by combining the second air gap 602 with a deposition process.

[0173] In step S1045, if Fig.32 As shown, a third sub-isolation layer 606 is formed, and the third sub-isolation layer 606 fills a portion of the sacrificial gap 602 a to form a second air gap 602 .

[0174] It should be understood that, although each step in the flowchart of each embodiment is displayed in sequence according to the indication of the arrow, these steps are not necessarily executed in sequence according to the order indicated by the arrow. Unless there is a clear explanation in this article, the execution of these steps does not have a strict order restriction, and these steps can be executed in other orders. Moreover, at least a part of the steps in the flowchart of each embodiment may include multiple steps or multiple stages, and these steps or stages are not necessarily executed at the same time, but can be executed at different times, and the execution order of these steps or stages is not necessarily carried out in sequence, but can be executed in turn or alternately with other steps or at least a part of the steps or stages in other steps.

[0175] See also Fig. 22 The present disclosure also provides a semiconductor structure, including: a substrate, a plurality of bit line structures 30, a storage node contact structure 50, and a first isolation layer 60. The plurality of bit line structures 30 are located on the upper surface of the substrate, the bit line structure 30 includes a bit line stack structure 302 and an isolation sidewall 303 located on the sidewall of the bit line stack structure 302, and the isolation sidewall 303 has a first air gap 3034. The storage node contact structure 50 is located between the bit line structures 30. The first isolation layer 60 is located between the bit line structure 30 and the storage node contact structure 50, and the first isolation layer 60 has a second air gap 602.

[0176] like Fig. 22 As shown, due to the existence of the first air gap 3034 and the second air gap 602, the capacitance (C_BL / NC) between the storage node contact structure 50 and the bit line structure 30 can be reduced, thereby reducing the overall capacitance (C_BL) of the bit line structure 30, thereby improving the sensing margin of the chip.

[0177] The semiconductor structure includes: a substrate, a plurality of bit line structures 30, a storage node contact structure 50 and a first isolation layer 60. The plurality of bit line structures 30 are located on the upper surface of the substrate, the bit line structure 30 includes a bit line stack structure 302 and an isolation sidewall 303 located on the sidewall of the bit line stack structure 302, and a first air gap 3034 is provided in the isolation sidewall 303. The storage node contact structure 50 is located between the bit line structures 30. The first isolation layer 60 is located between the bit line structure 30 and the storage node contact structure 50, and a second air gap 602 is provided in the first isolation layer 60. Due to the existence of the first air gap 3034 and the second air gap 602, the capacitance between the storage node contact structure 50 and the bit line structure 30 can be reduced, thereby reducing the capacitance of the bit line structure 30 as a whole, and thus improving the sensing margin of the chip.

[0178] Optionally, there are one or more first air gaps 3034 in the isolation spacer 303. Further, when there are multiple first air gaps 3034 in the isolation spacer 303, multiple first air gaps 3034 can still be formed by removing corresponding sacrificial layers to form the first air gaps 3034.

[0179] In one embodiment, in each first isolation layer 60, the number of the second air gaps 602 is one or more. Fig.26 As shown, in each first isolation layer 60, the number of the second air gap 602 is one; or Fig.24 As shown, in each first isolation layer 60, there are two second air gaps 602. Of course, according to specific process requirements, the number of the second air gaps 602 can also be designed to be a suitable number, which is not limited in this embodiment.

[0180] In one embodiment, Fig.14 As shown, the substrate includes: a base 10, a plurality of spaced bit line contact holes 2011, a second isolation groove, and a dielectric layer 20. The base 10 has a shallow trench isolation structure 102, and the shallow trench isolation structure 102 isolates a plurality of spaced active areas 101 in the base 10. The plurality of spaced bit line contact holes 2011 are located in the base 10. The second isolation groove is located in the bit line contact hole 2011. The dielectric layer 20 is located on the upper surface of the base 10. The semiconductor structure also includes a plurality of bit line contact structures 301 located in the bit line contact holes 2011, which are arranged one by one corresponding to the bit line contact holes 2011, and the bit line contact structures 301 penetrate the dielectric layer 20 and the second isolation layer in the thickness direction, and the top of the bit line contact structure 301 contacts the bottom of the bit line stack structure 302, and the bit line contact structure 301 contacts the active area 101 below the bit line contact hole 2011.

[0181] Among them, the material of the substrate 10 can be any suitable substrate material known in the art, for example, it can be at least one of the following materials: silicon (Si), germanium (Ge), red phosphorus, silicon germanium (SiGe), silicon carbide (SiC), carbon germanium silicon (SiGeC), indium arsenide (InAs), gallium arsenide (GaAs), indium phosphide (InP) or other III / V compound semiconductors, including multilayer structures composed of these semiconductors, or silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) and germanium on insulator (GeOI), or it can also be double-sided polished silicon wafers (Double Side Polished Wafers, DSP), or it can be a ceramic substrate such as alumina, a quartz or glass substrate, etc., and this embodiment is not limited here.

[0182] Optional, such as Fig.14 As shown, the dielectric layer 20 may be composed of a first dielectric layer 201 and a second dielectric layer 202 located on the same layer. The first dielectric layer 201 and the second dielectric layer 202 may be made of the same material and both serve to insulate the bit line structure 30 from the active area 101 to prevent a short circuit between the bit line structure 30 and the active area 101.

[0183] In one embodiment, Fig.14 As shown, the storage node contact structure 50 also penetrates the dielectric layer 20 along the thickness direction and extends into the substrate 10 to contact the active area 101 .

[0184] In one embodiment, Fig.21 As shown, the bit line stack structure 302 includes a conductive layer 3021 and a passivation layer 3022, and the storage node contact structure 50 includes a contact structure (not shown) and a contact pad (not shown), wherein the contact structure is located between the conductive layers 3021 of adjacent bit line structures 30. The contact pad is located between the upper surface of the contact structure and the passivation layer 3022 of the bit line structure 30, and partially covers the top of the passivation layer 3022.

[0185] The material of the conductive layer 3021 may include tungsten (W), cobalt (Co), molybdenum (Mo), ruthenium (Ru), copper (Cu), aluminum (Al), titanium (Ti), tantalum (Ta) or other metals. The material of the passivation layer 3022 may include nitride, for example, silicon nitride (SiN).

[0186] In one embodiment, Fig. 22 As shown, the first isolation layer 60 is located between the contact pad and the bit line structure 30 .

[0187] In one embodiment, Fig.23 As shown, a plurality of bit line structures 30 are arranged at intervals along the first direction and extend along the second direction, and a plurality of storage node contact structures 50 are arranged in an array along the first direction and the second direction; in two rows of storage node contact structures 50 arranged adjacent to each other along the second direction, a second air gap 602 is provided between one row of storage node contact structures 50 and the bit line structures 30 adjacent to the first side in the first direction, and a second air gap 602 is provided between another row of storage node contact structures 50 and the bit line structures 30 adjacent to the second side in the first direction. The second air gap 602 may be a ring-shaped gap in a top view, resulting in Fig.24 The cross section in FIG. 4 shows two second air gaps 602 , and the bottoms of the two second air gaps 602 may be connected or disconnected.

[0188] The first direction may intersect with the second direction, and further, the first direction may be perpendicular to the second direction. Fig.23 The first direction can be Fig.23 The horizontal direction in the second direction can be Fig.23 In other suitable application scenarios, the first direction and the second direction may also be other suitable directions, which are not limited in this embodiment.

[0189] In one embodiment, the second air gap 602 may be a rectangular gap, a circular gap, or an irregular gap in a top view. Fig.25 Taking the structure shown as an example, the curvature of the sidewall close to the storage node contact structure 50 is greater than the curvature of the sidewall of the second air gap 602 close to the bit line structure 30 in the top view.

[0190] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features of the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0191] The above embodiments only express several implementation methods of the present disclosure, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the patent application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present disclosure, and these all belong to the protection scope of the present disclosure. Therefore, the protection scope of the patent of the present disclosure shall be subject to the attached claims.

Claims

1. A method for preparing a semiconductor structure, characterized in that: include: providing a substrate; forming a plurality of bit line structures on the upper surface of the substrate, wherein the bit line structures include a bit line stack structure and an isolation sidewall located on a sidewall of the bit line stack structure, wherein the isolation sidewall has a first air gap; forming a storage node contact structure material layer between adjacent bit line structures; Etching the storage node contact structure material layer to obtain a storage node contact structure and a first gap groove, wherein the first gap groove is located between the bit line structure and the storage node contact structure; A first isolation layer is formed in the first gap groove, wherein the first isolation layer has a second air gap.

2. The method for preparing a semiconductor structure according to claim 1, characterized in that: The providing of the substrate comprises: providing a substrate; forming a shallow trench isolation structure in the substrate, wherein the shallow trench isolation structure isolates a plurality of active areas arranged in an array at intervals in the substrate; forming a first dielectric layer on the upper surface of the substrate; A plurality of bit line contact holes are formed in the base and the first dielectric layer to form the substrate.

3. The method for preparing a semiconductor structure according to claim 2, characterized in that: A plurality of bit line structures are formed on the upper surface of the substrate, including: Filling the bit line contact structure material layer in the bit line contact hole, and forming an initial bit line stack on the bit line contact structure material layer; Patterning the initial bit line stack, the bit line contact structure material layer and the first dielectric layer to form a bit line stack structure, a bit line contact structure and second gap grooves located on both sides of the bit line contact structure, wherein the top of the bit line contact structure contacts the bottom of the bit line stack structure, and the bit line contact structure contacts the active area exposed by the bit line contact hole; A second isolation structure is formed in the second gap groove, a second dielectric layer is formed on the surface of the second isolation structure and the surface of the substrate, and an isolation sidewall is formed on the sidewall of the bit line stack structure.

4. The method for preparing a semiconductor structure according to claim 3, characterized in that: After forming a plurality of bit line structures on the upper surface of the substrate and before forming a storage node contact structure material layer between adjacent bit line structures, the method further includes: The second dielectric layer and the substrate are etched to form a contact hole, wherein the contact hole exposes a portion of the active area; and the storage node contact structure material layer also fills the contact hole.

5. The method for preparing a semiconductor structure according to claim 3, characterized in that: The bit line stack structure includes a conductive layer and a passivation layer; the initial bit line stack is formed on the bit line contact structure material layer, including: forming a conductive material layer on the upper surface of the bit line contact structure material layer; forming a passivation material layer on the upper surface of the conductive material layer; The patterning of the initial bit line stack comprises: The passivation material layer and the conductive material layer are etched to obtain a plurality of the bit line stack structures arranged at intervals, the remaining passivation material layer is used as a passivation layer, and the remaining conductive material layer is used as a conductive layer.

6. The method for preparing a semiconductor structure according to claim 3, characterized in that: The step of forming an isolation spacer on the sidewall of the bit line stack structure comprises: forming a first spacer on a sidewall of the bit line stack structure; forming a first sacrificial layer on the surface of the first sidewall; forming a second sidewall spacer on a surface of the first sidewall spacer and a surface of the first sacrificial layer; The first sacrificial layer is removed to form the first air gap, and the first sidewall spacer, the first air gap and the second sidewall spacer constitute the isolation sidewall spacer.

7. The method for preparing a semiconductor structure according to any one of claims 1 to 6, characterized in that: The first isolation layer is formed in the first gap groove, wherein the first isolation layer has a second air gap, comprising: The first isolation layer is formed in the first gap groove by a deposition process, and the first isolation layer has the second air gap therein.

8. The method for preparing a semiconductor structure according to any one of claims 1 to 6, characterized in that: The first isolation layer is formed in the first gap groove, wherein the first isolation layer has a second air gap, comprising: forming a first sub-isolation layer on the sidewall and bottom of the first gap groove; forming a second sacrificial layer on a surface of the first sub-isolation layer; forming a second sub-isolation layer on the surface of the second sacrificial layer, wherein the first sub-isolation layer, the second sacrificial layer and the second sub-isolation layer together fill the first gap groove; removing the second sacrificial layer to form a sacrificial gap; A third sub-isolating layer is formed, wherein the third sub-isolating layer fills a portion of the sacrificial gap to form the second air gap.

9. A semiconductor structure, characterized in that: include: substrate; A plurality of bit line structures are located on the upper surface of the substrate, wherein the bit line structures include a bit line stack structure and an isolation sidewall located on a sidewall of the bit line stack structure, and a first air gap is formed in the isolation sidewall; A storage node contact structure located between the bit line structures; The first isolation layer is located between the bit line structure and the storage node contact structure, and a second air gap is formed in the first isolation layer.

10. The semiconductor structure according to claim 9, characterized in that: The substrate comprises: A substrate, wherein the substrate has a shallow trench isolation structure, wherein the shallow trench isolation structure isolates a plurality of active areas arranged at intervals in the substrate; A plurality of spaced-apart bit line contact holes are located in the substrate; A second isolation trench is located in the bit line contact hole; A dielectric layer, located on the upper surface of the substrate; The semiconductor structure also includes a plurality of bit line contact structures located in the bit line contact holes, which are arranged one by one corresponding to the bit line contact holes, and the bit line contact structures penetrate the dielectric layer and the second isolation layer along the thickness direction, the top of the bit line contact structure contacts the bottom of the bit line stack structure, and the bit line contact structure contacts the active area below the bit line contact holes.

11. The semiconductor structure according to claim 10, characterized in that: The storage node contact structure also penetrates the dielectric layer along the thickness direction and extends into the substrate to contact the active area.

12. The semiconductor structure according to claim 9, characterized in that: The bit line stack structure includes a conductive layer and a passivation layer, and the storage node contact structure includes: A contact structure located between conductive layers of adjacent bit line structures; The contact pad is located between the upper surface of the contact structure and the passivation layer of the bit line structure and partially covers the top of the passivation layer.

13. The semiconductor structure according to claim 12, characterized in that: The first isolation layer is located between the contact pad and the bit line structure.

14. The semiconductor structure according to any one of claims 9 to 13, characterized in that: A plurality of the bit line structures are arranged in a first direction at intervals and extend in a second direction, and a plurality of the storage node contact structures are arranged in an array along the first direction and the second direction; In the two rows of storage node contact structures arranged adjacent to each other along the second direction, a second air gap is provided between one row of storage node contact structures and the bit line structure adjacent to the first side of the first direction, and a second air gap is provided between the other row of storage node contact structures and the bit line structure adjacent to the second side of the first direction.

15. The semiconductor structure according to any one of claims 9 to 13, characterized in that: In each of the first isolation layers, the number of the second air gaps is one or more.

Citation Information

Patent Citations

  • Semiconductor device with air gap and method for fabricating the same

    CN103456694A

  • Semiconductor device with self-aligned air gap and method for fabricating the same

    CN103915376A

  • Semiconductor structure and preparation method thereof

    CN113097148A

  • Method for manufacturing semiconductor device having spacer with air gap

    US20120276711A1

  • Method for manufacturing memory and same

    US20220093607A1