Screening method and manufacturing method of nickel-cobalt-manganese active material for positive electrode

Through thermal mass analysis screening and particle structure optimization of nickel-cobalt-manganese active materials, the problem of reduced storage characteristics of non-aqueous electrolyte secondary batteries caused by high nickel ratios was solved, and better battery gas control and storage performance were achieved.

CN118788620APending Publication Date: 2024-10-18PRIME PLANET ENERGY & SOLUTIONS INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410419295.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-04-11
Filing Date
2024-04-09
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

In non-aqueous electrolyte secondary batteries, the use of a nickel-cobalt-manganese active material with a high nickel ratio leads to a decrease in storage characteristics.

Method used

Screen the nickel-cobalt-manganese active material through thermal mass analysis to ensure that its mass reduction rate at 100 to 600°C is less than 1.10%/minute, and that it contains more than 70 mol% nickel, and that single-crystal particles are given priority to reduce battery costs. The amount of gas produced in the charging state.

Benefits of technology

The storage characteristics of non-aqueous electrolyte secondary batteries are improved, the amount of gas generated by the battery under high temperature conditions is reduced, and the storage life of the battery is extended.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118788620A_ABST
    Figure CN118788620A_ABST
Patent Text Reader

Abstract

The invention relates to a screening method and a manufacturing method of a nickel-cobalt-manganese active material for a positive electrode. This method for screening a nickel-cobalt-manganese-based active material for positive electrodes comprises: a thermal mass analysis step in which the mass reduction rate (mass% / minute) of the nickel-cobalt-manganese-based active material at a temperature of 100-600 DEG C and a temperature increase rate of 5 DEG C / minute is obtained by thermal mass analysis; and a determination step for determining whether or not the nickel-cobalt-manganese-based active material satisfies the following formula (1): (1) Wd < = 1.10. According to the present disclosure, provided are: a method for screening and manufacturing a nickel-cobalt-manganese-based active material for a positive electrode capable of improving the storage characteristics of a non-aqueous electrolyte secondary battery; a nickel-cobalt-manganese-based active material for a positive electrode; a mixture containing the same; a positive electrode plate;
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field The present disclosure relates to a method for screening and a method for producing a nickel-cobalt-manganese-based active material for a positive electrode, and also relates to a nickel-cobalt-manganese-based active material for a positive electrode, a mixture containing the same, a positive electrode plate, and a non-aqueous electrolyte secondary battery. Background Art International Publication No. 2020 / 174794 proposes a non-aqueous electrolyte secondary battery that increases the capacity while suppressing an increase in resistance and the occurrence of an internal short circuit by increasing the nickel ratio in a nickel-containing lithium composite oxide. Summary of the invention In a non-aqueous electrolyte secondary battery, when a nickel-cobalt-manganese-based active material having a high nickel ratio (for example, 70 mol % or more) is used, the storage characteristics of the non-aqueous electrolyte secondary battery may be deteriorated. The present disclosure aims to provide a method for screening and a method for producing a nickel-cobalt-manganese-based active material for a positive electrode that can improve the storage characteristics of a non-aqueous electrolyte secondary battery, a nickel-cobalt-manganese-based active material for a positive electrode, a mixture containing the same, a positive electrode plate, and a non-aqueous electrolyte secondary battery. The present disclosure provides the following method for screening and manufacturing a nickel-cobalt-manganese-based active material for a positive electrode, a nickel-cobalt-manganese-based active material for a positive electrode, a mixture containing the same, a positive electrode plate, and a non-aqueous electrolyte secondary battery.

[0001] A method for screening a nickel-cobalt-manganese active material for a positive electrode, comprising: a thermal mass analysis step, wherein the mass reduction rate (mass % / minute) of the nickel-cobalt-manganese active material at a temperature of 100 to 600° C. and a heating rate of 5° C. / minute is determined by thermal mass analysis; and a determination step, wherein when the mass reduction rate (mass % / minute) is set as Wd, it is determined whether the nickel-cobalt-manganese active material satisfies the following formula: (1)Wd≤1.10.

[0002] The method for screening a nickel-cobalt-manganese-based active material for a positive electrode according to [1], wherein the thermal mass analysis step includes a sampling step of taking out the nickel-cobalt-manganese-based active material for thermal mass analysis from a battery in a charged state.

[0003] The method for screening a nickel-cobalt-manganese-based active material for a positive electrode according to [1] or [2], wherein the nickel content of the nickel-cobalt-manganese-based active material is 70 mol % or more.

[0004] The method for screening a nickel-cobalt-manganese-based active material for a positive electrode according to any one of [1] to [3], wherein the nickel-cobalt-manganese-based active material comprises single crystal particles.

[0005] A method for producing a nickel-cobalt-manganese-based active material for a positive electrode, comprising a screening step of performing the method for screening a nickel-cobalt-manganese-based active material for a positive electrode according to any one of [1] to [4].

[0006] A nickel-cobalt-manganese-based active material for a positive electrode, wherein the mass reduction rate per minute in a thermal mass analysis at 100 to 600° C. and a heating rate of 5° C. / min is 1.10 mass % / min or less.

[0007] The nickel-cobalt-manganese-based active material for a positive electrode according to [6], wherein the nickel content is 70% or more.

[0008] The nickel-cobalt-manganese-based active material for a positive electrode according to [6] or [7], comprising single crystal particles.

[0009] A nickel-cobalt-manganese-based active material mixture for a positive electrode, comprising the nickel-cobalt-manganese-based active material for a positive electrode according to any one of [6] to [8] and a nickel-cobalt-manganese-based active material different from the nickel-cobalt-manganese-based active material for a positive electrode.

[0010] The nickel-cobalt-manganese based active material mixture for a positive electrode according to [9], wherein the nickel-cobalt-manganese based active material for a positive electrode comprises single crystal particles, and the nickel-cobalt-manganese based active material different from the nickel-cobalt-manganese based active material for a positive electrode comprises polycrystalline particles.

[0011] A positive electrode plate having a positive electrode active material layer containing the nickel-cobalt-manganese-based active material for a positive electrode according to any one of [6] to [8].

[0012] A non-aqueous electrolyte secondary battery comprising the positive electrode plate according to

[11] . The foregoing and other objects, features, aspects and advantages of the present invention will become more apparent from the following detailed description of the present invention when read in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 This is a schematic flowchart of the method for screening the nickel-cobalt-manganese-based active material for the positive electrode in this embodiment. Figure 2 This is a schematic flow chart of a method for producing a nickel-cobalt-manganese-based active material for a positive electrode in this embodiment. Figure 3 This is a schematic diagram showing an example of the structure of the positive electrode plate in this embodiment. Figure 4 This is a schematic flowchart showing a method for manufacturing a positive electrode plate in this embodiment. Figure 5 This is a schematic diagram showing an example of the configuration of a battery in this embodiment. Figure 6 This is a schematic diagram showing an example of the structure of the electrode body in this embodiment. DETAILED DESCRIPTION The following describes the embodiments of the present disclosure with reference to the accompanying drawings, but the present disclosure is not limited to the following embodiments. In all the following drawings, in order to facilitate the understanding of each component, the scale is appropriately adjusted to represent it, and the proportion of each component shown in the drawings is not necessarily consistent with the proportion of the actual component. It should be noted that, in this specification, elements expressed in the singular also include the plural unless otherwise specified. For example, "particle" refers not only to "one particle" but also to "an aggregate of particles (powder, powder, particle group)". <Method for screening nickel-cobalt-manganese based active materials for positive electrodes> The screening method (hereinafter also referred to as screening method) of the positive electrode nickel-cobalt-manganese active material (hereinafter also referred to as positive electrode NCM active material) in this embodiment is as follows: Figure 1 As shown, it includes: a thermal mass analysis step A, wherein the mass reduction rate (mass % / minute) (hereinafter also referred to as the mass reduction rate) of the nickel-cobalt-manganese active material (hereinafter also referred to as the NCM active material) at a temperature of 100 to 600°C and a heating rate of 5°C / minute is determined by thermal mass analysis; and a determination step B, wherein it is determined whether the NCM active material satisfies formula (1). The positive electrode NCM active material can be used for the positive electrode of a non-aqueous electrolyte secondary battery (hereinafter also referred to as a battery). The details of the battery will be described later. In the thermal mass analysis step A, the mass reduction rate can be obtained by thermal mass analysis. The thermal mass analysis can be performed according to the following steps. 20 mg of NCM active material for thermal mass analysis is measured in a dish for thermal mass analysis, and after being installed in the thermal mass analysis measurement device, the mass reduction amount of 100°C to 600°C when heated at a heating rate of 5°C / min and an upper temperature limit of 600°C under Ar atmosphere is measured, and the mass reduction rate per minute is calculated. The thermal mass analysis can be performed according to the method described in the column of the embodiment described later. In the determination step B, a thermal mass analysis is performed to determine whether the NCM active material satisfies formula (1). By using the NCM active material determined to satisfy formula (1) in the determination step B as the positive electrode NCM active material for the positive electrode active material layer, the amount of gas generated when the battery is stored at a high temperature in a charged state (hereinafter also referred to as the amount of stored gas) can be reduced, thereby improving the storage characteristics. Considering that the stored gas is usually generated by the side reaction of the NCM active material contained in the electrolyte and the positive electrode, it is surprising that a correlation between the mass reduction rate and the stored gas was found, rather than a correlation between the composition, average particle size and specific surface area of ​​the NCM active material and the stored gas. From the viewpoint of storage characteristics, the right side of formula (1) is preferably 1.00 or less, more preferably 0.45 or less, and further preferably 0.40 or less. The left side of formula (1) is usually 0 or more, for example, 0.0001 or more, 0.001 or more, 0.01 or more, or 0.1 or more. The thermal mass analysis step A may include: a sampling step of taking out the NCM active material for thermal mass analysis from the battery set to a charged state. The battery has a positive electrode plate, and the positive electrode plate includes a positive electrode active material layer containing the NCM active material. The battery can be measured by 0.2 mA / cm at a temperature of 25°C. 2 The current density was charged at a constant current of 4.35 V, and then the constant voltage was charged at 4.35 V until the current density reached 0.04 mA / cm 2 Thus, it becomes a charged state. The positive electrode plate can be taken out from the battery in the charged state, and the NCM active material for thermal mass analysis can be taken out (taken) from the positive electrode active material layer of the positive electrode plate. The test cell (test cell) can be, for example, a stacked type or a wound type. More specific methods for making a test cell, charging a test cell, and taking out the NCM active material for thermal mass analysis from a test cell in a charged state will be described in the column of the embodiments described later. The NCM active material contains one or more compounds containing nickel, cobalt and manganese. The compound containing nickel, cobalt and manganese can be a single crystal particle or a polycrystalline particle described later. The nickel content ratio relative to the metal element other than lithium in the NCM active material can be, for example, 70 mol% or more, preferably 75 mol% or more, more preferably 80 mol% or more, further preferably 85 mol% or more, and particularly preferably 90 mol% or more. The compound containing nickel, cobalt and manganese preferably includes a nickel-cobalt-manganese composite hydroxide, and more preferably includes a lithium-nickel-cobalt-manganese composite oxide. The nickel-cobalt-manganese composite hydroxide can be obtained, for example, by a coprecipitation method (coprecipitation method). The nickel-cobalt-manganese composite hydroxide can be, for example, a general formula: Ni x Co y Mn z (OH) 2 (wherein x+y+z=1) The molar ratio of lithium to nickel, cobalt and manganese in the lithium nickel cobalt manganese composite oxide Li:(Ni+Co+Mn) can be, for example, 1.0 to 1.2:1.0. The NCM active material may include, for example, a first layered metal oxide. The first layered metal oxide is represented by formula (i): Li 1-a1 Ni x1 Me 1 1-x1 O 2 (i). In formula (i), "a1" satisfies the relationship "-0.3≤a1≤0.3". "x1" satisfies the relationship "0.1≤x1≤0.95". 1 ” represents at least one selected from Co, Mn, Al, Zr, Ti, V, Cr, Fe, Cu, Zn, Mo, Sn, Ge, Nb and W. The NCM active material may include, for example, a LiNi 0.7 Co 0.2 Mn 0.1 O 2 、LiNi 0.7 Co 0.1 Mn 0.2 O 2 、LiNi 0.75 Co 0.15 Mn 0.1 O 2 、LiNi 0.75 Co 0.1 Mn 0.15 O 2 and LiNi 0.8 Co 0.1 Mn 0.1 O 2 At least one of the following. The NCM active material can be basically selected from, for example, LiNi 0.7 Co 0.2 Mn 0.1 O 2 、LiNi 0.7 Co 0.1 Mn 0.2 O 2 LiNi 0.75 Co 0.15 Mn 0.1 O 2 、LiNi 0.75 Co 0.1 Mn 0.15 O 2 and LiNi 0.8 Co 0.1 Mn 0.1 O 2 At least one of the components. The NCM active material may include, for example, single crystal particles, may include polycrystalline particles, and may include both single crystal particles and polycrystalline particles. Single crystal particles and polycrystalline particles may be, for example, one particle, or may be, for example, an aggregate consisting of 2 to 10 primary particles. Primary particles refer to particles whose grain boundaries cannot be confirmed in the SEM image of the particles. Single crystal particles and polycrystalline particles may be, for example, spherical, columnar, blocky, etc. The NCM active material preferably includes single crystal particles, more preferably single crystal particles. Single crystal particles and polycrystalline particles can have any size. The average particle size D50 of single crystal particles can be, for example, 1 μm or more and 20 μm or less, preferably 1 μm or more and 10 μm or less, and more preferably 1 μm or more and 5 μm or less. The average particle size D50 of polycrystalline particles can be, for example, 1 μm or more and 40 μm or less, preferably 1 μm or more and 30 μm or less, and more preferably 1 μm or more and 20 μm or less. The average particle size D50 represents the particle size at which the cumulative particle volume from the small particle size side in the volume-based particle size distribution becomes 50% of the total particle volume. The average particle size can be measured by laser diffraction and scattering method. A single crystal particle may have, for example, 0.4 m 2 / g or more and 5.0m 2 / g or less. The polycrystalline particles may have, for example, a BET specific surface area of ​​0.1 m 2 / g or more and 5.0m 2 In this specification, the BET specific surface area is measured by the BET multipoint method. <Method for producing NCM active material for positive electrode> The method for producing the positive electrode NCM active material in this embodiment includes a screening step of performing the above-mentioned method for screening the positive electrode NCM active material. By including the screening step in the method for producing the positive electrode NCM active material, a positive electrode NCM active material that can reduce the amount of storage gas in the battery and improve the storage characteristics can be provided. The method for producing the positive electrode NCM active material can further include a preparation step of preparing the NCM active material. For example, the method for producing the positive electrode NCM active material is as follows Figure 2 As shown, it includes a preparation step C and a screening step D. For the NCM active material prepared in the preparation step C, the above description is applicable. In the preparation step C, an NCM active material can be prepared. When the NCM active material is a lithium nickel cobalt manganese composite oxide, for example, the NCM active material can be prepared by mixing a lithium source such as lithium hydroxide and a nickel cobalt manganese composite hydroxide, calcining to obtain a lithium nickel cobalt manganese composite oxide having an aggregate structure (agglomerated structure), adding a metal oxide thereto, and performing a heat treatment. In the screening step D, when it is determined that the NCM active material satisfies the above formula (1), the NCM active material can be screened as a positive electrode NCM active material. If the screened positive electrode NCM active material has not been surface treated, it can be surface treated in the subsequent surface treatment step. <NCM active material for positive electrode> The mass reduction rate of the positive electrode NCM active material in this embodiment is less than 1.10 mass% / minute. For the mass reduction rate, the above description applies. The positive electrode NCM active material has the above mass reduction rate, which can reduce the amount of gas stored in the battery and improve the storage characteristics. The positive electrode NCM active material can be obtained by the above-mentioned method for manufacturing the positive electrode NCM active material. From the perspective of reducing the amount of storage gas, the mass reduction rate of the NCM active material for the positive electrode is preferably less than 1.00, more preferably less than 0.45, further preferably less than 0.40, and usually greater than 0, for example, greater than 0.0001 or greater than 0.001 or greater than 0.01 or greater than 0.1. For the positive electrode NCM active material, the above description of the NCM active material applies except for the mass reduction rate. The nickel content ratio of the positive electrode NCM active material relative to the metal element other than lithium can be, for example, 70 mol% or more, preferably 75 mol% or more, more preferably 80 mol% or more, further preferably 85 mol% or more, and particularly preferably 90 mol% or more. The positive electrode NCM active material preferably contains single crystal particles, more preferably single crystal particles. <NCM active material mixture for positive electrode> The positive electrode NCM active material mixture in this embodiment includes the above-mentioned positive electrode NCM-based active material (hereinafter also referred to as a first NCM active material) and an NCM-based active material different from the positive electrode NCM active material (hereinafter also referred to as a second NCM active material). The second NCM active material includes one or more compounds containing nickel, cobalt and manganese. The nickel content ratio relative to the metal elements other than lithium in the second NCM active material can be, for example, 70 mol% or more, preferably 75 mol% or more, more preferably 80 mol% or more, further preferably 85 mol% or more, and particularly preferably 90 mol% or more. The compound containing nickel, cobalt and manganese preferably includes a nickel-cobalt-manganese composite hydroxide, and more preferably includes a lithium-nickel-cobalt-manganese composite oxide. The nickel-cobalt-manganese composite hydroxide can be obtained, for example, by a coprecipitation method. The nickel-cobalt-manganese composite hydroxide can, for example, be a general formula: Ni x Co y Mn z (OH) 2 (wherein x+y+z=1) The molar ratio of lithium to nickel, cobalt and manganese in the lithium nickel cobalt manganese composite oxide Li:(Ni+Co+Mn) can be, for example, 1.0 to 1.2:1.0. The second NCM active material may include, for example, a second layered metal oxide. The second layered metal oxide is represented by formula (ii): Li 1-a1 Ni x1 Me2 1-x1 O 2 (ii). In formula (ii), "a1" satisfies the relationship "-0.3≤a1≤0.3". "x1" satisfies the relationship "0.1≤x1≤0.95". 2 ” represents at least one selected from Co, Mn, Al, Zr, Ti, V, Cr, Fe, Cu, Zn, Mo, Sn, Ge, Nb and W. The second NCM active material may include, for example, a material selected from LiNi 0.7 Co 0.2 Mn 0.1 O 2 、LiNi 0.7 Co 0.1 Mn 0.2 O 2 、LiNi 0.75 Co 0.15 Mn 0.1 O 2 、LiNi 0.75 Co 0.1 Mn 0.15 O 2 and LiNi 0.8 Co 0.1 Mn 0.1 O 2 The second NCM active material may be substantially composed of, for example, LiNi 0.7 Co 0.2 Mn 0.1 O 2 、LiNi 0.7 Co 0.1 Mn 0.2 O 2 、LiNi 0.75 Co 0.15 Mn 0.1 O 2 、LiNi 0.75 Co 0.1 Mn 0.15 O 2 and LiNi 0.8 Co 0.1 Mn 0.1 O 2 At least one of the components. The second NCM active material may include, for example, single crystal particles, polycrystalline particles, or both. The second NCM active material preferably includes polycrystalline particles, more preferably polycrystalline particles. The above description applies to the description of single crystal particles and polycrystalline particles. The first NCM active material of the NCM active material mixture for the positive electrode comprises single crystal particles, and the second NCM active material comprises polycrystalline particles. More preferably, the first NCM active material is single crystal particles, and the second NCM active material is polycrystalline particles. <Positive electrode plate> Figure 3 This is a schematic diagram showing an example of the structure of the positive electrode plate in the present embodiment. The positive electrode plate 10 includes, for example, a positive electrode substrate 11 and a positive electrode active material layer 12. The positive electrode substrate 11 is a conductive sheet. The positive electrode substrate 11 may be, for example, an aluminum alloy foil. The positive electrode substrate 11 may have a thickness of, for example, 10 μm to 30 μm. The thickness of the positive electrode substrate 11 may be measured using a constant pressure thickness measuring device (thickness gauge). The positive electrode active material layer 12 may be arranged on the surface of the positive electrode substrate 11. The positive electrode active material layer 12 may be arranged on a single surface or both surfaces of the positive electrode substrate 11. The positive electrode active material layer 12 may have a thickness of, for example, 10 μm to 200 μm. The thickness of the positive electrode active material layer 12 is measured in a cross-sectional SEM image of the positive electrode active material layer 12. The observation surface may be parallel to the thickness direction of the positive electrode active material layer 12. The thickness of the positive electrode active material layer 12 is measured at more than 5 locations. The thickness of the positive electrode active material layer 12 is defined as the arithmetic average of the thicknesses at more than 5 locations. The density of the positive electrode active material layer 12 may be, for example, 3.0 to 3.8 g / cm 3 . The positive electrode active material layer 12 includes active material particles 23. The active material particles 23 include the above-mentioned positive electrode NCM active material, preferably the above-mentioned positive electrode NCM active material. Figure 3 As shown, the positive electrode active material layer 12 may further include active material particles 24. When the positive electrode active material layer 12 includes active material particles 24, the active material particles 23 may be the first NCM active material, and the active material particles 24 may be the second NCM active material. Although not shown, the positive electrode active material layer 12 can include a binder and a conductive aid. As the binder, for example, polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), polyimide (PI), polyamide (PA), polyamideimide (PAI), butadiene rubber (BR), styrene butadiene rubber (SBR), nitrile-butadiene rubber (NBR), styrene-ethylene-butylene-styrene block copolymer (SEBS), carboxymethyl cellulose (CMC), or a combination thereof. As for the content of the binder in the positive electrode active material layer 12, based on the total solid content of the positive electrode active material layer 12 as 100wt%, for example, it can be 0.5 to 10wt%, preferably 1.0 to 5wt%. The conductive aid may include carbon black such as acetylene black, other carbon materials (such as graphite), carbon nanotubes, etc. The content of the conductive aid in the positive electrode active material layer 12 may be, for example, 0.05 to 2.0 wt %, preferably 0.10 to 1.0 wt %, based on 100 wt % of the total solid content of the positive electrode active material layer 12. like Figure 4 As shown, the manufacturing method of the positive electrode plate 10 includes: preparation of positive electrode slurry (E), coating (F), drying (G) and compression (H). In the preparation of the positive electrode slurry (E), a positive electrode slurry containing active material particles is prepared. The positive electrode slurry is prepared by dispersing the active material particles in a dispersion medium. The organic solvent may, for example, contain at least one selected from N-methyl-2-pyrrolidone (NMP), tetrahydrofuran (THF), dimethylformamide (DMF), methyl ethyl ketone (MEK) and dimethyl sulfoxide (DMSO). The amount of the organic solvent used is arbitrary. The positive electrode slurry may have an arbitrary solid content concentration (mass fraction of the solid content). The slurry may have a solid content concentration of, for example, 40% to 80%. Any stirring device, mixing device, or dispersing device may be used for mixing. The coating (F) may include coating the positive electrode slurry on the surface of the substrate to form a coating film. In this embodiment, the positive electrode slurry may be coated on the surface of the substrate using any coating device. Drying (G) may include, for example, heating the coating film to dry it using a hot air dryer to form a dry coating film. Compression (H) may include compressing the dry coating film using any compression device to form a positive electrode active material layer 12. The dried coating film is compressed to form a positive electrode active material layer 12 to complete the positive electrode plate 10. The positive electrode plate 10 can be cut (cut) into a specified plane size according to the specifications of the battery. The positive electrode plate 10 can be cut in a manner such as a strip-shaped plane shape. The positive electrode plate 10 can be cut in a manner such as a rectangular plane shape. <Battery> The battery in this embodiment can be a lithium ion battery. Figure 5 This is a schematic diagram showing an example of a battery in this embodiment. Figure 5 The battery 100 shown may be a lithium ion battery used, for example, as a main power source or a power auxiliary power source for an electric vehicle. The battery 100 includes an outer package 90. The outer package 90 contains an electrode body 50 and a non-aqueous electrolyte (not shown). The electrode body 50 is connected to a positive terminal 91 using a positive electrode current collecting member 81. The electrode body 50 is connected to a negative terminal 92 using a negative electrode current collecting member 82. Figure 6Schematic diagram showing an example of an electrode body in this embodiment. The electrode body 50 is a wound type. The electrode body 50 includes a positive electrode plate 10, a separator (separator) 70 and a negative electrode plate 60. That is, the battery 100 includes a positive electrode plate 10. The positive electrode plate 10 includes a positive electrode active material layer 12 and a positive electrode substrate 11. The negative electrode plate 60 includes a negative electrode active material layer 62 and a negative electrode substrate 61. Example The present disclosure will be described in more detail below using examples. "%" and "parts" in the examples are mass % and mass parts unless otherwise specified. <Evaluation method of storage characteristics> [Method for manufacturing positive electrode plate] The first positive electrode active material and the second positive electrode active material [composed of LiOH and Ni 0.83 Co 0.09 Mn 0.08 (OH) 2 Synthesized transition metal compound. Particle size: 15-18 μm, average particle size: 16 μm, specific surface area: 0.20 m 2 / g of polycrystalline particles] 97.5 parts by mass of a mixture mixed in a mass ratio of 5:5, 1.5 parts by mass of carbon black as a conductive aid, and 1.0 parts by mass of polyvinylidene fluoride (PVdF) as a binder were mixed, and then an appropriate amount of N-methyl-2-pyrrolidone (NMP) was added to prepare a positive electrode slurry. The positive electrode slurry was applied to a collector composed of aluminum foil to form a positive electrode active material layer. Then, it was dried and rolled using a calendering roller to a density of 3.55 g / cm 3 , cut into specified size, install aluminum pole piece, and make positive electrode plate. [Method for manufacturing negative electrode plate] The negative electrode active material, carboxymethyl cellulose (CMC) as a thickener, and styrene butadiene rubber (SBR) as a binder are weighed so that the mass ratio of each is 98:1:1, and they are dispersed in water to prepare a negative electrode slurry. The negative electrode slurry is applied to a collector composed of copper foil to form a negative electrode active material layer. Then, it is dried, rolled using a rolling roller to a specified thickness, cut into a specified size, and a nickel electrode sheet is installed to make a negative electrode. [Method for preparing non-aqueous electrolyte] Ethylene carbonate (EC), dimethyl carbonate (DMC) and ethyl methyl carbonate (EMC) were mixed in a volume ratio of 30:30:40. Lithium hexafluorophosphate (LiPF 6 ) to a concentration of 1.15 mol / L. Furthermore, vinylene carbonate (VC) was added at an addition rate of 1.0 mass % relative to the total mass of the mixed solvent to prepare a non-aqueous electrolyte. [Method for manufacturing a test battery cell] The positive electrode plate and the negative electrode plate were stacked via a polyolefin separator to produce a stacked electrode body, which was housed in an outer package made of an aluminum laminate sheet, injected with the nonaqueous electrolyte, and then the opening of the outer package was sealed to obtain a test battery cell. [Evaluation of the amount of stored gas] The gas volume of the test battery cell in the above-discharged state was taken as the gas volume before storage. Then, the gas volume was measured at 0.2 mA / cm2 at a temperature of 25°C. 2 The current density was charged at a constant current until it reached 4.25 V, and then charged at a constant voltage of 4.25 V until the current density reached 0.04 mA / cm 2 After that, it was stored in a 60°C constant temperature bath for 60 days. 2 After the battery was discharged at a constant current density of 1.500 cc to 3.0 V, the amount of gas was measured to obtain the amount of gas generated after storage. The amount of gas stored was measured by removing (subtracting) the gas before storage from the gas after storage. When the amount of gas stored was less than 0.60 cc, the storage characteristics were judged to be good. <Thermal Mass Analysis> [Method for manufacturing positive electrode plate] 97.5 parts by mass of the first positive electrode active material, 1.5 parts by mass of carbon black as a conductive material, and 1.0 parts by mass of polyvinylidene fluoride (PVdF) as a binding material were mixed, and then an appropriate amount of N-methyl-2-pyrrolidone (NMP) was added to prepare a positive electrode slurry. The positive electrode slurry was applied to a collector composed of aluminum foil to form a positive electrode composite layer. Then, it was dried, rolled using a calendering roller to a specified thickness, cut into a specified size, and an aluminum pole piece was installed to make a positive electrode plate. [Method for preparing non-aqueous electrolyte] Ethylene carbonate (EC), dimethyl carbonate (DMC) and ethyl methyl carbonate (EMC) were mixed in a volume ratio of 30:30:40. Lithium hexafluorophosphate (LiPF6) was added to the mixed solvent to a concentration of 1.15 mol / L. Furthermore, vinylene carbonate (VC) was added in an addition rate of 1.0 mass % relative to the total mass of the mixed solvent to prepare a non-aqueous electrolyte. [Method for manufacturing a test battery cell] The positive electrode plate and the metal lithium sheet were wound through a polyolefin separator to produce a wound electrode body, which was placed in an outer package made of an aluminum laminate, injected with the nonaqueous electrolyte, and then the opening of the outer package was sealed to obtain a test battery cell. [Sampling method for thermal mass analysis] For the test battery cell, at a temperature of 25°C and a flow rate of 0.2 mA / cm 2 The current density was charged at a constant current until it reached 4.35 V, and then charged at a constant voltage of 4.35 V until the current density reached 0.04 mA / cm 2 The charged battery was disassembled in a glove box, the positive electrode plate was taken out, washed with DMC, and vacuum dried. The positive electrode mixture layer was scraped off from the core of the positive electrode plate to prepare a sample for thermal mass analysis. [Calculation method of mass reduction rate] 20 mg of the sample was weighed on a TG pan and installed in a thermal analysis measuring device (DTG-60AH manufactured by Shimadzu). The measurement was performed under Ar atmosphere at a heating rate of 5°C / min and a temperature upper limit of 600°C. The mass reduction from 100°C to 600°C and the mass reduction rate per minute were calculated. <Example 1> For LiOH and Ni 0.83 Co 0.09 Mn 0.08 (OH) 2 The single crystal particles composed of the synthesized transition metal compound were subjected to the above-mentioned thermal mass analysis, and the mass reduction rate at a temperature of 100-600°C and a heating rate of 5°C / min was 0.99% / min. The single crystal particles were used as the first positive electrode active material, and the storage gas volume was measured according to the above-mentioned storage characteristic evaluation method. The results are shown in Table 1 together with the average particle size (D50) and specific surface area of ​​the single crystal particles. <Examples 2 and 3 and Comparative Examples 1 to 4> Single crystal particles [composed of LiOH and Ni] having the average particle size (D50) and specific surface area shown in Table 1 were prepared. 0.83 Co 0.09 Mn 0.08 (OH) 2 The mass reduction rate was measured for the single crystal particles composed of the synthesized transition metal compound. The storage gas amount was measured for these single crystal particles in the same manner as in Example 1. The results are shown in Table 1.

Table 1

Claims

1. A method for screening nickel-cobalt-manganese active materials for positive electrodes, comprising: A thermal mass analysis step, wherein the mass reduction rate (mass % / minute) of the nickel-cobalt-manganese active material at a temperature of 100 to 600° C. and a heating rate of 5° C. / minute is determined by thermal mass analysis; and A determination step, wherein when the mass reduction rate (mass % / minute) is defined as Wd, it is determined whether the nickel-cobalt-manganese based active material satisfies the following formula: (1) Wd≤1.

10.

2. The method for screening a nickel-cobalt-manganese-based active material for a positive electrode according to claim 1, wherein: The thermal mass analysis step includes a sampling step of taking out a nickel-cobalt-manganese-based active material for thermal mass analysis from a battery in a charged state.

3. The method for screening a nickel-cobalt-manganese-based active material for a positive electrode according to claim 1, wherein: The nickel content of the nickel-cobalt-manganese based active material is 70 mol % or more.

4. The method for screening a nickel-cobalt-manganese-based active material for a positive electrode according to claim 1, wherein: The nickel-cobalt-manganese based active material includes single crystal particles. 5 . A method for producing a nickel-cobalt-manganese based active material for a positive electrode, comprising a screening step of performing the method for screening a nickel-cobalt-manganese based active material for a positive electrode according to claim 1 .

6. Nickel-cobalt-manganese active material for positive electrode, wherein: The mass reduction rate per minute in a thermal mass analysis at 100 to 600° C. and a heating rate of 5° C. / min was 1.10 mass % / min or less.

7. The nickel-cobalt-manganese based active material for a positive electrode according to claim 6, wherein: The nickel content is 70% or more. 8 . The nickel-cobalt-manganese-based active material for a positive electrode according to claim 6 , comprising single crystal particles. 9 . A nickel-cobalt-manganese based active material mixture for a positive electrode, comprising the nickel-cobalt-manganese based active material for a positive electrode according to claim 6 and a nickel-cobalt-manganese based active material different from the nickel-cobalt-manganese based active material for a positive electrode.

10. The nickel-cobalt-manganese active material mixture for positive electrode according to claim 9, wherein: The nickel-cobalt-manganese based active material for a positive electrode includes single crystal particles, and a nickel-cobalt-manganese based active material different from the nickel-cobalt-manganese based active material for a positive electrode includes polycrystalline particles. 11 . A positive electrode plate comprising a positive electrode active material layer comprising the nickel-cobalt-manganese based active material for a positive electrode according to claim 6 . 12 . A non-aqueous electrolyte secondary battery comprising the positive electrode plate according to claim 11 .