Stretch blow-molded plastic container having integrated handle region and method for producing plastic container

Through the hollow handle area and laser welding technology, the problems of transparency and mechanical strength in existing plastic container manufacturing are solved, efficient and low-cost plastic container manufacturing is achieved, and the stability and operability of the container are ensured.

CN118790599APending Publication Date: 2024-10-18ALPLA WERKE ALWIN LEHNER
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
CN202411173345.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2016-06-06
Filing Date
2017-05-15
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

It is difficult to produce an integrated handle area that is transparent and has sufficient mechanical strength during the manufacturing process of existing plastic containers, and the traditional stretch blow molding method has problems of unstable operation and high cost.

Method used

The hollow handle area is connected to the container body, manufactured by stretch blow molding, and laser welding technology is used to form welds to ensure the strength and transparency of the handle area while simplifying the manufacturing process.

Benefits of technology

It achieves reliable grasping and transportation of plastic containers, improves mechanical strength and drop resistance, reduces manufacturing costs, and simplifies the process flow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118790599A_ABST
    Figure CN118790599A_ABST
Patent Text Reader

Abstract

The invention relates to a stretch-blow-molded plastic container, for example, a preferably transparent plastic bottle, comprising a container body (12) which surrounds a filling volume and which has a container bottom (19), a container neck (11) which is connected to opposite ends of the container body (12), and an integrated handle region (18) which is connected to the container neck (11), the container neck has a container opening. The handle region (18) is hollow and is connected to a filling volume surrounded by the container body (12). A grip opening (17) is formed between the handle region (18) and the container body (12), said grip opening being covered over the entire circumference thereof by wall parts of the container body (12) and of the handle region (18), said wall parts being welded to one another.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of an application with an international application date of May 15, 2017, a national application number of 201780035000.7 (international application number of PCT / EP2017 / 061602), and an invention name of "Plastic container made by stretch blow molding with an integrated handle area and a manufacturing method for a plastic container". Technical Field

[0002] The invention relates to a stretch blow molded plastic container, such as a preferably transparent plastic bottle, with an integrally formed handle region according to the preamble of claim 1. The invention also relates to a method for producing such a plastic container according to the independent method claim. Background Art

[0003] Containers made of tinplate or non-ferrous metal, glass or even ceramics, which were commonly used in the past, are increasingly being replaced by containers made of plastic. Plastic containers are mainly used, in particular, for the packaging of liquid substances in household, agricultural, industrial and commercial applications. Low weight and lower costs certainly play an important role in this replacement. The use of recyclable plastic materials and the overall more favorable total energy balance in their production also help to promote the acceptance of plastic containers by consumers.

[0004] Different methods are known for manufacturing plastic containers, especially plastic bottles, and their application is not only related to the plastic used. Plastic containers are mostly made by blow molding, in which containers, such as plastic bottles, are blown into their final shape by overpressure in the blow mold. Different method technologies are distinguished in blow molding, among which extrusion blow molding, injection blow molding and injection stretch blow molding are mentioned in particular. In extrusion blow molding, a single-layer or multi-layer plastic tube is hot extruded, introduced into a blow mold and blown into a plastic container via a blow mandrel inserted into the mold cavity. Injection blow molding is a combination of injection molding and blow molding. Here, a preform is first manufactured in an injection mold by injection molding. The preform is demoulded from the injection mold, pretreated if necessary and introduced into the mold cavity of the blow mold, in which the preform is finally blown with overpressure according to the shape preset by the mold cavity. In injection stretch blow molding, the preform introduced into the mold cavity is additionally stretched with a stretching mandrel during the blow molding process. The blow molding of the preform can be carried out directly after its production by injection molding. In alternative production methods, the further processing of the preform can also be carried out separately from the production of the preform in terms of time and / or space. Finally, it should also be mentioned that the preform can also be produced by extrusion or also by extrusion blow molding.

[0005] The first plastic container with an integrated handle area is made of polyethylene (PE) by an extrusion blow molding method. Polyethylene can be processed well as a whole and allows the integrated handle area to be manufactured by deformation and welding. However, the disadvantage is that the plastic container composed of PE is opaque. Therefore, PE was soon replaced by polyvinyl chloride (PVC) as a raw material, which was used to manufacture transparent plastic containers with integrated handle areas. Although PVC has good weldability, it is relatively difficult to process in different blow molding methods. Ecological reasons also oppose the use of PVC as a raw material for transparent plastic containers in large quantities. Many alternative plastics, although with the desired transparency, are excluded as materials for plastic containers with integrated handle areas due to their relatively difficult processability and due to, for example, too low mechanical strength in a drop test for price reasons.

[0006] The raw material most often used for the production of transparent plastic containers in the stretch blow molding process is polyethylene terephthalate (PET). Due to the large stretching that can be achieved in the stretch blow molding process, PET has very good mechanical strength values. For example, in the stretch blow molding process of PET, a total stretch factor of up to 20 is achieved. This is in contrast to the total stretch factors of less than 5, for example, in polyolefins such as polyethylene (PE) or polypropylene (PP), which are usually processed by extrusion blow molding. Due to the higher total stretch factor compared to plastic containers produced by extrusion blow molding, plastic containers produced by stretch blow molding, especially made of PET, have significantly higher mechanical strength values. This and the low-cost method solution, especially with PET and similar plastics, such as PEF, make the stretch blow molding process very attractive, especially for the production of plastic containers with integrated handle areas.

[0007] JP 61 043535 A discloses a stretch blow molding method in which a handle region is formed by deformation inside a blow mold. Here, after the container body has been stretch blow molded into its final shape, mutually opposing wall regions on the container body are pressed together by a push rod that can be inserted into the blow mold. The handle region formed in this way forms a handle recess on both sides of the plastic container. However, it has been shown that such bottles with a handle region formed as a handle recess cannot always be handled reliably. Therefore, bottles made of PET with a handle recess have not yet been generally accepted on the market. Summary of the invention

[0008] The object of the present invention is therefore to remedy these disadvantages and shortcomings of the plastic containers of the prior art. A plastic container, such as a plastic bottle, with an integrally formed handle region should be provided, which can be reliably gripped and transported by means of the integrated handle region. In this case, the plastic container should be producible using a largely standardized stretch blow molding method. Expensive modifications of the method concept should be avoided. The production method should allow short cycle times and be cost-effective to carry out.

[0009] The solution to this and other objects is a stretch-blow-molded plastic container with an integrally formed handle region, which has the features listed in claim 1. The associated production method for the plastic container according to the invention has the features listed in the independent method claim. Improvements and / or advantageous embodiment variants of the invention are the subject matter of the corresponding dependent device claims or method claims.

[0010] The invention provides a stretch blow molded plastic container, which has a container body surrounding a filling volume, a container neck connected to opposite longitudinal ends of the container body, and an integrally formed handle region, the container body having a container bottom, and the container neck having a container opening. The handle region is hollow and connected to the filling volume surrounded by the container body. A gripping opening is provided between the handle region and the container body, and the gripping opening is surrounded by wall parts of the container body and the handle region welded to each other over its entire circumference.

[0011] The handle area of ​​the plastic container is designed to be hollow and connected to the filling volume. As a result, the filling substance can also expand into the handle area. The hollow handle area thus contributes to the filling volume. Here, the size of the area bounded by the inner wall of the handle area is about 5 mm. 2 Up to about 400mm 2The handle area is given sufficient strength at the narrowest position of the handle. Here, the handle area can have any geometric shape. Geometric embodiments that are rounded, for example elliptical or oval, at least in the area of ​​the handle have been proven to be comfortable for the user to grip. The empty gripping opening makes it easy to grip and hold the plastic container. As a result, the plastic container can also have a volume of about 0.5 liters to about 20 liters and can be better gripped and safely held and handled. Plastic containers are manufactured from tubular preforms in a largely traditional stretch blow molding method, which were previously usually made by injection molding. The manufacture of plastic containers from traditional preforms in a stretch blow molding method results in a large stretching of the plastic material used and can provide very good mechanical strength values, for example in terms of upset strength and resistance to falling. The manufacturing method consisting of preforms in a stretch blow molding method can be understood as on the finished blow-molded plastic container. For example, the injection point of the preform can be seen on the bottom of the container. The container neck provided with the container opening also generally has a greater wall thickness and cannot be stretched in the stretch blow moulding process because it lies outside the blow mould cavity.

[0012] In one embodiment variant of the plastic container, the wall parts which surround the gripping opening and are welded to one another can form a weld seam which has a width of 100 μm to 5 mm.

[0013] Another embodiment variant of the plastic container can provide that the wall parts welded to each other are connected to each other with a laser penetration welding method. In such a traditional laser welding method, the weld seam can usually reach a width of 3mm to 5mm.

[0014] In an alternative embodiment variant of a plastic container, a clear welding method (Klar-Klar-Schweissverfahren) can be used as a laser welding method for welding wall parts that edge the gripping opening. In this case, the wall parts have a total elongation coefficient greater than 3. On the finished plastic container, this can be understood with the help of a very narrow weld width of 100 μm to 3 mm. Here, the weld can have a very small fluctuation width of only 10 μm. Clear welding laser welding allows very accurate welding of plastic materials that are transparent to the laser radiation used without adding additives. Therefore, the wall areas that edge the gripping opening can be welded to each other. In conventional laser welding, the upper joint fitting is laser-melted and heat is only generated in the lower joint fitting located below it, while in clear welding, heat is introduced into the entire laser-melted body. Since the injected laser is accurately focused on the welding plane, the material of the two joint fittings melts. Here, heat input can be achieved by exciting the water molecules in the plastic to oscillate. Therefore, additives for converting the injected energy into heat can be discarded. As a result, the laser welding process can be simplified and accelerated.

[0015] In an embodiment variant of the plastic container according to the invention, the container body can have a filling volume of 0.5 to 20 liters, preferably 0.7 to 10 liters and particularly preferably 0.9 to 3 liters. Plastic containers with such a volume are also desirable in the food sector, for example for edible oils, and for storing household cleaners and care products, detergents or also mineral oils and the like.

[0016] Another embodiment variant of the plastic container can provide that the container body is formed as a single layer or multilayer and has a mass proportion of at least 80% consisting of a plastic main component, which consists of the following group, which consists of polyethylene terephthalate, polyethylene naphthalate, polylactic acid, polyethylene furanoate, polypropylene furanoate, their copolymers and mixtures of the plastics. In the literature, polypropylene furanoate is often also referred to as polytrimethylene furanoate. In this case, the glass transition temperature of the plastics listed is less than 150° C. and greater than 54° C. The plastics listed have great similarities in their processability. The plastics allow a large degree of stretching and can be processed into transparent plastic containers with high strength values. The plastics are usually stretched so that when heated to a temperature greater than 150° C., they shrink by more than 20%. This can be measured in that a 10 mm wide tie rod consisting of the contour to be welded is prepared and heated to above 150° C. for 20 seconds. Furthermore, the plastics listed can also be reliably combined with the laser welding methods listed in order to be able to produce an integrated handle region with a grip opening.

[0017] In another embodiment, the container body of the plastic container can be at least partially transparent. The transparent embodiment of the container body enables direct control of the filling level.

[0018] According to another design example of the present invention, the edge delimiting the gripping opening is configured as a burr-free rounded bulge. After welding the wall portion, the wall segments delimited by the weld seam and substantially close to each other are removed to form the gripping opening. This can be achieved with the aid of a CO2 laser, which can thermally separate the unnecessary wall segments in one working step and can produce a burr-free rounded bulge on the cut edge. This makes it comfortable for the user to grip through the gripping opening. The wall part can also be separated in such a way that at least one protrusion is formed on its edge in the gripping opening produced, and the protrusion is designed to accommodate an insert in the gripping opening. The insert can be configured, for example, as a metering cup, with the aid of which the contents of the container can be removed in a metered manner.

[0019] In a method for producing a plastic container according to an embodiment variant of the invention, a preform of tubular construction is stretched axially and radially in a blow mold to form a plastic container by a stretch blow molding method. During the stretching, two mutually opposite wall regions of the container body are brought closer together by means of a push rod that can be removed from the blow mold to prepare for an integrated handle region. The stretch blow molded plastic container is then demolded and transported to a welding station, where the mutually adjacent wall regions are welded together to form a weld seam. The wall segment surrounded by the weld seam is then separated from the container body and removed to form a gripping opening.

[0020] In the method according to the present invention, the wall areas of the container body that are opposite to each other can be close to each other during the stretching of the preform used. Here, the pre-blown parts produced in the initial stage of the stretch blow molding method can be deformed. It can be ensured that the plastic material is stretched in the desired circumferential manner. Afterwards, the pre-blown parts are blow-molded according to the blow mold cavity that is reduced around the push rod that is moved out. It is possible to have a very uniform material distribution so that the plastic container that has been blown has a relatively uniform wall thickness distribution in the area where the wall areas that are opposite to each other are close to each other. If necessary, the plunger can still move toward each other during the main blow molding process in order to further change the outer contour of the container body. The wall areas that are close to each other and opposite to each other form a handle groove on the plastic container that has been blown, and the handle groove forms a preparatory stage for the integrated handle area. After the plastic container is demoulded, the plastic container is transported to the welding station. There, the wall areas that are close to each other in the blow mold are flatly attached to each other and welded to each other along the closed line that wraps the handle groove. Then, the wall section surrounded by the weld seam formed in this way can be separated and removed to form a gripping mouth. In one embodiment variant, adjacent wall regions can be welded around each other without removing the wall sections that are edged by the weld seam. This allows regions to be created inside the container body that are not filled with the container contents. This can create visual effects, especially if the container contents are colored.

[0021] Although not absolutely necessary, in one method variant it can be provided that the adjacent wall regions already lie flat against each other in the blow mold. As a result, the region of the container body formed in the handle recess can achieve maximum stretching. The adjacent wall regions can also already have a certain adhesion to each other, which can facilitate the subsequent welding process.

[0022] In another method variant, the adjacent wall regions can be connected to each other in a materially bonded manner by laser welding after the plastic container has been demoulded. The laser welding can be carried out separately from the stretch blow molding process in time and / or space. This should mean that the adjacent wall regions do not have to be welded to each other immediately after demoulding in the welding station. It can also be provided that the finished plastic containers are first temporarily stored before they are transported further to the welding station.

[0023] In another method variant, the wall areas close to each other can be connected to each other with a material fit using a clear welding method. Laser clear welding allows very accurate welding of plastic materials that are transparent to the laser radiation used without the need to add additives. In conventional laser welding, the upper joint fitting is melted through by the laser and heat is only generated in the lower joint fitting located below it, while in clear welding, heat is introduced into the entire laser-melted body. Since the injected laser is accurately focused on the welding surface, the materials of the two joint fittings melt. Here, heat input can be achieved by exciting the water molecules in the plastic to oscillate. Therefore, additives for converting the injected energy into heat can be discarded, so that mixing of additives that absorb relative to the laser used can not occur in the plastic. This can simplify and accelerate the laser welding process.

[0024] A method variant of laser welding can provide that the wall areas that are close to each other are pressed together by means of two plungers that are opposite to each other, wherein at least one of the two plungers is transparent to the laser radiation used for laser welding. Even if the two wall areas that are close to each other are already in contact or are already more or less well attached to each other after the stretch blow molding method, the pressing of the wall parts against each other provides a defined position of the wall parts. Thus, the two plungers fix the two wall areas and can also prevent shrinkage and deformation of the area to be welded, especially during the welding process. The plunger can also cool the area to be welded so that the weld is stable, that is, it does not shrink or break during or after the welding process. As a result, the weld can be made accurately and reproducibly from container to container. In this case, a weld can be achieved that is within a tolerance of 10 μm relative to a preset weld line.

[0025] In another method variant, the plunger for pressing the wall areas to be welded to each other comprises at least one plunger, which can be made of a material transparent to the laser radiation used, such as glass, quartz glass or organic glass. The laser energy is then injected into the joint partner through this plunger. When using the clear welding method, the two plungers can also be made of a material that is transparent to the laser used.

[0026] In another method variant, which can alternatively or additionally be used to press the wall areas to be welded together, the wall areas that are close to each other can be kept in planar contact with each other by a negative pressure generated in the container body. The negative pressure can be generated via the container opening in that the suction head is placed on the container opening.

[0027] The welding of the wall regions close to each other can be carried out in conventional laser welding methods and in clear welding of the sides opposite each other. When using plungers to compress the wall regions in the welding station, the two plungers are transparent to the introduced laser radiation and can be composed of glass, quartz glass or organic glass.

[0028] Another method variant can provide that the weld seam which surrounds the grip opening over its entire circumference is deburred and / or rounded.

[0029] Deburring or rounding may be necessary in order to increase the gripping comfort of the plastic container for the user.

[0030] Deburring and / or rounding can be performed simultaneously or immediately after the removal of the wall section surrounded by the weld seam. For example, a CO2 laser can be used for this purpose, which separates the wall section and simultaneously forms a burr-free, rounded weld bead on the edge that delimits the gripping opening. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Further advantages and features emerge from the following description of exemplary embodiments of the invention with reference to schematic drawings which are not true to scale.

[0032] Figure 1 A blow mold cavity with a preform used is shown;

[0033] Figure 2 Show according to Figure 1 A cross section of the blow mold cavity along section line II-II;

[0034] Figure 3 shows a cross section of a blow mold cavity having a pre-blown piece formed by stretch blow molding of a preform;

[0035] Figure 4 A cross section showing a blow mold cavity and a pre-blow piece with deformed side walls;

[0036] Figure 5 A cross section showing a blow mold cavity and a fully blow molded plastic container;

[0037] Figure 6 A cross section of a plastic container is shown in a welding station;

[0038] Figure 7 shows a cross section of a plastic container during laser welding;

[0039] Figure 8 shows a cross section of a plastic container with a wall part cut away;

[0040] Fig. 9 showing an enlarged cross section through an edge bounding a grip opening; and

[0041] Fig.10 A perspective view showing a plastic container stretch blow molded according to the method of the present invention.

[0042] In the schematic drawings, identical components or elements are respectively provided with the same reference numerals. DETAILED DESCRIPTION

[0043] Figure 1 The axial section of the preform 20 used in the blow mold cavity 2 of the blow mold 1 is shown. The section extends along the separation plane of the two blow mold halves of the blow mold 1. The tubular preform 20 having a preform neck 21 with an opening and a preform body 22 closed by a preform bottom 23 is made of thermoplastic. For example, at least the preform body 22 is formed as a single layer or multilayer and has a mass proportion of at least 80%, which is composed of a plastic main component, which is composed of the following group, which is composed of polyethylene terephthalate, polylactic acid, polyethylene naphthalate, polyethylene furanoate, polypropylene furanoate, copolymers thereof and mixtures of the plastics. The preform 20 is usually made by injection molding. However, the preform can also be made by extrusion or extrusion blow molding. The blow mold 1 is a component of a stretch blow molding device, in which the preform 20 is blown into a plastic container according to the mold cavity 2. The preform neck 21 is located outside the mold cavity 2 and is usually not changed any more during the stretch blow molding process.

[0044] The preform 20 is supported on the mouth 5 of the blow mold cavity 2 and extends axially toward the bottom 6 of the blow mold cavity 2. The blow mold cavity 2 is bounded by the blow mold wall 3 and the blow mold bottom 6. In the section near the edge of the blow mold wall 3, the wall section 4 extends into the interior of the blow mold cavity 2. The inner contour of the blow mold cavity 2 essentially predetermines the later configuration of the plastic container to be manufactured by the stretch blow molding method. Here, the preform body 22 is deformed into the container body of the plastic container by blowing and axial stretching by means of a stretch blow molding mandrel that is moved through the opening in the preform 21. The preform neck 21 remains virtually unchanged during the stretch blow molding method and forms the container neck of the plastic container.

[0045] Figure 2The cross-sectional view in FIG. 1 shows, for example, a preform 20 that is rotationally symmetrically configured inside the blow mold cavity 2 of the blow mold 1 before the start of the blow molding and stretching process. The blow mold cavity 2 has, for example, two opposite wall sections 4 that protrude relative to the blow mold wall 3. The two wall sections 4 each have a central region that is configured as a movable push rod 7. By moving the push rod 7 into the blow mold cavity 2, its inner contour can be changed. The protruding wall section 4 is stretched out from the axial middle region of the blow mold cavity 2 and leaves a central, essentially cylindrical section free for stretching the blow mold core rod.

[0046] Figure 3 The pre-blown part B produced from a preform 20 , in particular a preform body 21 , in a so-called pre-blowing process is shown. The pre-blown part B largely follows the inner contour of the blow mold cavity 2 with the tappet 7 in the starting position.

[0047] Figure 4 The blow mold cavity 2 of the blow mold 1 is shown at the end of the pre-blowing process. The push rod 7 in the central region of the mutually opposite wall regions 4 is moved into the interior of the blow mold cavity 2 to the desired extent. In the process, the pre-blown part B is deformed and the plastic material is stretched. The deformation of the side wall of the pre-blown part B is provided in the region where the integrated handle region is to be formed.

[0048] Figure 5 1 shows a cross section of a blow mold cavity 2 and a finished stretch blow molded plastic container before it is demoulded. The figure shows in particular a cross section of a container body 12 with wall regions 13, 14 close to each other. The wall regions 13, 14 correspond to the deformations ( Figure 4 ) and is arranged in the area near the edge of the container body 12 and forms a handle groove. The wall areas 13, 14 forming the handle groove follow the contour of the section 4 protruding relative to the blow mold wall 3 and the contour of the push rod 7 inserted into the blow mold cavity 2. The feed movement of the push rod 7 can be defined, for example, so that the wall areas 13, 14 that are close to each other still have a distance from each other. In an alternative method scheme, the push rod 7 inserted into the mold cavity 2 of the blow mold 1 is also fed toward each other, so that the wall areas 13, 14 are clamped between the push rods 7 and reach abutment against each other. Here, the wall parts 13, 14 can be at least partially bonded to each other at the contact point when the pre-blow piece is still hot.

[0049] Figure 6 A schematic cross-sectional view of a container body 12 of a stretch-blow-molded plastic container removed from a blow mold is shown. In the welding station, the wall areas 13, 14 that are brought close to each other by the stretch-blow-molding method are pressed together by means of two mutually opposite plungers 31, 32 that can be fed toward each other. Figure 6The state is shown shortly before the compressed wall regions 13, 14 lie flat against one another. Alternatively or additionally, it is also possible to place the adjacent wall regions 13, 14 flat against one another in the welding station by generating a negative pressure inside the container body 12. For example, a suction head can be placed on the opening in the container neck for this purpose. Even in the case of plastic containers whose wall regions 13, 14 already lie flat against one another during the stretch blow molding method, the compression of the wall regions is achieved in the welding station by means of plungers 31, 32. This ensures flat contact and the wall regions can be brought into a defined and reproducible position relative to one another in any case.

[0050] Figure 7 A container body 12 is shown with wall regions 13, 14 compressed by means of plungers 31, 32. The mutual compression of the wall regions 13, 14 by means of the plungers 31, 32 causes the wall regions 13, 14 to be welded to remain stable and not twisted or deformed during welding. In addition, the plungers 31, 32 cool and promote the process of not twisting the wall regions 13, 14 to be welded. The wall regions 13, 14 are stretched in such a way that they shrink by more than 20% when heated to more than 150° C. for 20 seconds. The wall parts 13, 14, which are placed flatly next to each other, are then welded to each other along the edges of their abutment surfaces. A closed weld seam 16 is produced here, which surrounds the wall segment 15 formed by the two wall regions 13, 14. In a further processing step, the wall segment 15 surrounded by the weld seam 16 is then separated and removed in order to produce a gripping opening 17.

[0051] The welding of the wall regions 13, 14 placed close to each other can be achieved by conventional laser penetration welding. The weld seam 16 produced here can have a width of 3mm to 5mm. In a method variant, the compressed wall regions 13, 14 can be connected to each other in a form-fitting manner by a clear welding method. In this laser welding variant, the introduced heat is precisely focused on the welding plane and the mating parts to be joined to each other can be melted in a targeted manner in the welding plane. Here, heat input can be achieved by exciting the water molecules in the plastic to oscillate. Additives for converting the injected energy into heat in this welding method can be discarded.

[0052] At least one of the two plungers 32, 32 is transparent to the laser radiation L used for laser welding, so that the laser radiation L can be focused on the welding plane by the plunger, wherein the wall areas 13, 14 are pressed by means of the plunger. In an alternative method, laser welding can also be performed from both sides of the pressed wall areas 13, 14. It should be understood that in this case, the two plungers 31, 32 are composed of a material that is transparent to the introduced laser radiation. For example, at least one or both plungers 31, 32 are composed of glass, quartz glass or organic glass.

[0053] exist Figure 8 Schematically shows the separation and removal of the wall section 15 surrounded by the weld seam 16. The separation and removal of the wall section 15 produces a gripping opening 17. The weld seam 16, which edges the gripping opening 17 over its entire circumference, can also be deburred and / or rounded. Deburring and / or rounding can be carried out simultaneously with or immediately after the removal of the wall section 15 surrounded by the weld seam 16. For example, an infrared radiator adapted to the radius of the handle area can be used for this purpose.

[0054] Fig. 9 An enlarged cross section through the edge delimiting the gripping opening 17 is shown. In this exemplary embodiment, the wall segment 15 is thermally separated by means of a CO2 laser. The separation of the wall segment 15 is carried out in a manner spaced apart from the weld seam 16 in order to keep the thermal load of the weld seam 16 as low as possible by the thermal separation. The formation of the burr-free bulge 24 on the edge is carried out simultaneously with the separation. When forming the bulge 24, a portion of the material is squeezed out over each of the corresponding wall regions 13, 14 and a subregion 25 is formed. Each subregion 25 is formed with a radius R of approximately 0.25 mm at its edge. The burr-free bulge 24, which is wider than the material thickness of the two wall regions 13, 14, provides a comfortable feeling for the user's hand gripping through the gripping opening 17 during operation in combination with the rounding of the subregion 25.

[0055] at last, Fig.10 A perspective view of a plastic container 10 with an integrated handle region 18, which has been stretch blow molded according to the method of the invention, is shown. The plastic container 10 has a container neck 11 with a container opening, which corresponds essentially to the preform neck of the preform from which the plastic container 10 has been stretch blow molded. A container body 12, which is closed by a container bottom 19 and has an integrated handle region 18, is connected to the container neck 11. The handle region 18 surrounds a grip opening 17, which is surrounded by a weld seam 16 over its entire circumference and is opened by removing a wall section 15 ( Figure 7 and Figure 8 ) is produced.

[0056] The handle region 18 of the plastic container 10 is designed to be hollow and is connected to the remaining filling volume surrounded by the container body 12. As a result, the filling substance can also spread into the handle region 18. The hollow handle region 18 thus contributes to the filling volume. Here, it has an approximately 5 mm opening limited by the inner wall of the handle region. 2 Up to about 400mm 2 The size of the area gives the handle area sufficient strength. The handle area comprises approximately 60 mm at its narrowest point. 2The open gripping opening 17 makes it easier to grip and hold the plastic container 10. As a result, the plastic container can also have a larger volume of 2 to 10 liters and can be better gripped and safely held and handled. The plastic container 10 is preferably designed to be transparent, which allows direct control of the filling level. The plastic container 10 is produced by a largely conventional stretch blow molding method from a tubular preform, which was previously usually produced by injection molding. Production by injection molding leads to a large stretching of the plastic material used and allows the production of a plastic container 10 with very good mechanical strength values, for example in terms of upset strength and fall resistance.

Claims

1. A stretch-blow-moulded plastic container having a container body (12) enclosing a filling volume and a container neck (11) connected to the opposite end of the container body (12) and having an integrally formed handle area (18), the container body having a container bottom (19), the container neck having a container opening, It is characterized in that The handle region (18) is hollow and connected to a filling volume enclosed by the container body (12), and a gripping opening (17) is left between the handle region (18) and the container body (12), the gripping opening (17) being surrounded over its entire circumference by wall parts (13, 14) of the container body and the handle region (18) that are welded to one another.

2. The plastic container according to claim 1, It is characterized in that The wall parts (13, 14) welded to one another form a weld seam (16) having a width of 100 μm to 5 mm.

3. The plastic container according to claim 1 or 2, It is characterized in that The wall parts (13, 14) welded to each other are materially connected to each other by a laser welding method.

4. The plastic container according to claim 3, It is characterized in that The laser welding method is a clear welding method.

5. The plastic container according to any one of the preceding claims, It is characterized in that The container body (12) has a filling volume of 0.5 liter to 20 liters, preferably 0.7 liter to 10 liters and particularly preferably 0.9 liter to 3 liters.

6. The plastic container according to any one of the preceding claims, It is characterized in that The container body (12) is constructed as a single layer or multiple layers and has a mass proportion of at least 80%, which is composed of a plastic main component, and the plastic main component is composed of the following group, which is composed of polyethylene terephthalate, polylactic acid, polyethylene naphthalate, polyethylene furanoate, polypropylene furanoate, their copolymers and mixtures of the above plastics.

7. The plastic container according to any one of the preceding claims, It is characterized in that The container body (12) is at least partially transparent.

8. Plastic container according to any one of the preceding claims, It is characterized in that The edge delimiting the gripping opening is designed as a burr-free, rounded elevation.

9. A method for producing a plastic container according to any one of claims 1 to 8, It is characterized in that A tubular preform (20) is stretched axially and radially into a plastic container (20) in a blow mold (1) by a stretch blow molding method, wherein during the stretching, two mutually opposite wall areas (13, 14) of the container body (12) are brought closer to each other by means of a push rod (7) that can be extended from the blow mold (1) to prepare for an integrated handle area (18), and then the stretch blow molded plastic container (10) is demoulded and transported to a welding station, in which the mutually adjacent wall areas (13, 14) are welded to each other to form a weld seam (16), and the wall section (15) surrounded by the weld seam (16) is separated from the container body (12) and removed to form a gripping opening (17).

10. The method according to claim 9, It is characterized in that The wall regions (13, 14) lying adjacent to one another lie flat against one another in the blow mold (1).

11. The method according to claim 9 or 10, It is characterized in that The wall regions (13, 14) that lie adjacent to one another are materially connected to one another by laser welding.

12. The method according to claim 11, It is characterized in that The wall regions (13, 14) that lie adjacent to one another are materially connected to one another by a clean welding method.

13. The method according to claim 12, It is characterized in that In the welding station, the wall regions (13, 14) are pressed against one another by means of two oppositely disposed plungers (31, 32), wherein at least one of the two plungers is transparent to the laser radiation (L) used for laser welding.

14. The method according to claim 13, It is characterized in that The plunger, which is transparent at least with respect to the laser radiation (L) used, consists of glass, quartz glass or organic glass.

15. The method according to any one of claims 12 to 14, It is characterized in that The wall regions (13, 14) which are adjacent to one another are held in planar contact with one another by the negative pressure generated in the container body (12).

16. The method according to any one of claims 11 to 15, It is characterized in that The wall parts (13, 14) adjacent to each other are connected to each other in a materially bonded manner by laser welding from the sides facing each other.

17. The method according to any one of claims 9 to 16, It is characterized in that The weld seam (16) which surrounds the grip opening (17) over its entire circumference is deburred and / or rounded.

18. The method according to claim 17, It is characterized in that The deburring and / or rounding of the weld seam (16) is carried out simultaneously with or immediately after the removal of the wall section (15) surrounded by the weld seam (16).

Citation Information

Patent Citations

  • Method for manufacturing containers containing handle parts through blowing

    CN101115607A

  • Process for the manufacture of containers which have an integral handle, and containers manufactured thereby

    CN101115608A

  • Plastic container with through hole, and production method thereof

    CN105480541A

  • Plastics container with integral handle

    CN1452544A

  • Arrangement and method for manufacturing PET bottle with handle formed at body part by injection blow molding, and PET bottle manufactured by them