Aluminum profile injection bonding method

Through the aluminum profile injection bonding method, the problems of deformation and leakage caused by welding are solved, a stable bonding state is achieved, and the manufacturing cost and construction time are reduced.

CN118808599APending Publication Date: 2024-10-22金秉赞
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410091775.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-04-21
Filing Date
2024-01-23
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

Existing welding methods cause deformation in the manufacturing of aluminum profiles, difficulty in ensuring accuracy, high risk of leakage, and welding defects that are difficult to rework, resulting in product waste.

Method used

Using the aluminum profile injection bonding method, through product preparation, mold preparation, installation and injection filling steps, the injection material is filled into the aluminum profile contact part to form it into one body, eliminating multiple bonding components and improving bonding stability.

Benefits of technology

Significantly reduce manufacturing and construction costs, shorten construction time, avoid risks of deformation and leakage, and improve bonding accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808599A_ABST
    Figure CN118808599A_ABST
Patent Text Reader

Abstract

The invention discloses an aluminum profile injection bonding method. The aluminum profile injection bonding method according to an embodiment of the present invention comprises: a product preparation step of manufacturing a plurality of aluminum profiles to be bonded according to a product design; a mold preparation step of manufacturing a mold designed from the aluminum profile prepared in the first step; a mounting step of mounting the plurality of aluminum profiles to be bonded in the mold in a state of being in contact with each other; and an injection and filling step: filling the contact part of the aluminum profile with an injection material through the mold, so that the aluminum profiles to be bonded are formed into a whole. The present invention can provide an aluminum profile injection bonding method which can easily bond aluminum profiles having various cross-sectional structures and maintain a stable bonding state when manufacturing a battery case of an electric vehicle, and thus can omit a plurality of bonding members or coupling members, thereby significantly reducing the cost required for manufacturing and construction, and improving the production efficiency. Meanwhile, the construction time can be obviously shortened.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to an aluminum profile injection bonding method, and more specifically, to a profile injection bonding method for a battery shell of an electric vehicle. Background Art

[0002] The invention relates to a method for bonding a plurality of aluminum profiles constituting a battery shell of an electric vehicle, and is used to solve the problems existing in the bonding method by welding in the prior art.

[0003] In the prior art bonding method by welding, there is a problem of deformation of the aluminum profile after welding. Specifically, the aluminum profile has the characteristic of being deformed by heat of 500 to 600 degrees Celsius, so the aluminum profile is thermally deformed by the heat generated during welding.

[0004] For these reasons, in order to manufacture the desired structure by welding a plurality of aluminum profiles, a plurality of deformation prevention members and a plurality of additional processes after welding are required to prevent welding deformation. As a result, according to the bonding method using welding in the prior art, there is a problem that it is difficult to accurately align the tolerances of flatness, hole position, etc. In addition, the weld bead line is disturbed by the attached part and the weld bead needs to be removed by grinding work, so an additional process is required, it is difficult to align the flatness, and there is a problem that there is a high risk of leakage (leakage).

[0005] Furthermore, in the conventional bonding method by welding, it is difficult to rework after a welding defect is found, and thus there is a problem that the corresponding product has to be discarded.

[0006] Therefore, a technology is needed that can solve the above-mentioned problems according to the prior art, can simplify the process of the bonding method according to the prior art, does not cause deformation of the product, and can fundamentally eliminate the risk of leakage.

[0007] Prior art literature

[0008] Patent Literature

[0009] Patent Document 1 Korean Patent Gazette No. 10-1277453 (Grant Date: June 17, 2013) Summary of the invention

[0010] Technical issues

[0011] The object of the present invention is to provide an aluminum profile injection bonding method, which can easily bond aluminum profiles with various cross-sectional structures when manufacturing electric vehicle battery shells and can maintain a stable bonding state, so that multiple bonding components or combining components can be omitted, thereby significantly reducing the cost required for manufacturing and construction, and at the same time, significantly shortening the construction time.

[0012] Technical Solution

[0013] To achieve this purpose, the aluminum profile injection bonding method according to one aspect of the present invention may include: a product preparation step, manufacturing multiple aluminum profiles to be bonded according to product design; a mold preparation step, manufacturing a mold designed according to the aluminum profile prepared by the product preparation step; an installation step, installing the multiple aluminum profiles to be bonded in the mold in a state of contact with each other; and an injection filling step, filling the injection material into the contact part of the aluminum profile through the mold, so that the aluminum profiles to be bonded are formed into one body.

[0014] In one embodiment of the present invention, the mold preparation step may include: a mold gate forming step, forming a mold gate forming position according to a forming position of a filling hole of an aluminum profile, wherein the mold gate has a structure for discharging an injection material through the mold and leading it to the inside of a bonding portion of the aluminum profile.

[0015] In one embodiment of the present invention, the injection filling step may include: a side through hole forming step, in which a through hole is processed on the side of the aluminum profile to guide the injection material to be integrated with the aluminum profile.

[0016] In one embodiment of the present invention, the injection filling step may include: a pin inserting step of inserting a pin into the through hole formed by the side through hole forming step, so that the injection object and the aluminum profile are integrated into one.

[0017] In one embodiment of the present invention, the injection filling step may include: a block installation step of installing a block inside the aluminum profile so as to form a space adjacent to the bonding portion and having a specified volume inside the aluminum profile.

[0018] Beneficial Effects

[0019] As described above, according to the aluminum profile injection bonding method of the present invention, a method for injecting and bonding aluminum profiles can be provided, which has a product preparation step, a mold preparation step, an installation step and an injection filling step for performing a specific process. When manufacturing a battery casing of an electric vehicle, it is possible to easily bond aluminum profiles having various cross-sectional structures and maintain a stable bonding state. Therefore, a plurality of bonding components or combining components can be omitted, thereby significantly reducing the cost required for manufacturing and construction, and at the same time significantly shortening the construction time. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 is a photograph showing an aluminum profile bonding process according to the prior art.

[0021] Figure 2is a photograph showing the state of aluminum profiles bonded by a welding method of the related art.

[0022] Figure 3 is a flow chart showing an aluminum profile bonding method according to an embodiment of the present invention.

[0023] Figure 4 FIG. 4 is a flow chart showing an aluminum profile bonding method according to another embodiment of the present invention.

[0024] Figure 5 It is a perspective view showing a state in which two aluminum profiles to be bonded are in contact with each other to form a filling hole.

[0025] Figure 6 Is displayed Figure 5 The schematic plan view shows a state where a plurality of aluminum profiles in contact with each other are mounted on a mold.

[0026] Figure 7 Is to show the injection from Figure 6 The schematic plan view shows the state in which the mold is filled to the inside of the aluminum profile.

[0027] Figure 8 It is a schematic plan view showing a state where an injection material is filled from a mold into an aluminum profile in a state where a block is inserted into the aluminum profile.

[0028] Fig. 9 This is a perspective view showing a state where an ejector pin is inserted after a through hole is formed in an aluminum profile.

[0029] Reference numerals:

[0030] S100: Aluminum profile injection bonding method

[0031] S110: Product preparation steps

[0032] S120: Mold preparation step

[0033] S121: Mold gate formation

[0034] S130: Installation Steps

[0035] S140: Injection filling step

[0036] S141: Side through hole forming step

[0037] S142: Ejector Insertion Step

[0038] S143: Block installation steps

[0039] 10: Aluminum profile

[0040] 11: Filling holes

[0041] 12: Through hole

[0042] 20: Mold

[0043] 30: Ejector

[0044] 40: Block

[0045] 50: Injection DETAILED DESCRIPTION

[0046] The preferred embodiments of the present invention will be described in detail below with reference to the accompanying drawings. Prior to this, the terms or words used in this specification and claims should not be limited to the usual or dictionary meanings, but should be interpreted as the meanings and concepts that conform to the technical ideas of the present invention.

[0047] Throughout the specification, when a certain component is described as being "on" another component, it includes not only the case where the certain component is connected to the other component, but also the case where there is another component between the two components. Throughout the specification, unless otherwise clearly stated to the contrary, a part "comprising" a certain constituent element means that other constituent elements may also be included, rather than excluding other constituent elements.

[0048] Figure 3 A flow chart of an aluminum profile injection bonding method according to an embodiment of the present invention is shown.

[0049] Reference Figure 3 According to the aluminum profile injection bonding method S100 of the present embodiment, an aluminum profile injection bonding method can be provided. By having a product preparation step S110, a mold preparation step S120, an installation step S130 and an injection filling step S140 for performing a specific process, when manufacturing an electric vehicle battery shell, aluminum profiles with various cross-sectional structures can be easily bonded and a stable bonding state can be maintained. Therefore, multiple bonding components or combining components can be omitted, thereby significantly reducing the cost required for manufacturing and construction, and at the same time, significantly shortening the construction time.

[0050] Hereinafter, the components constituting the aluminum profile injection bonding method S100 according to the present embodiment will be described in detail with reference to the accompanying drawings.

[0051] Figure 4 A flow chart of an aluminum profile bonding method according to another embodiment of the present invention is shown. Figure 5 The perspective view shows a state where two aluminum profiles to be bonded are in contact with each other to form a filling hole. Figure 6 Shows the Figure 5 A schematic plan view of a state in which a plurality of aluminum profiles in contact with each other are mounted on a mold, Figure 7 The injection is shown Figure 6The schematic plan view of the state in which the mold is filled into the aluminum profile is shown. Figure 8 A schematic plan view of a state in which a block is inserted into the aluminum profile and an injection material is filled from a mold into the aluminum profile. Fig. 9 A perspective view showing a state where a through hole is formed in an aluminum profile and an ejector pin is inserted therein.

[0052] According to the product preparation step S110 of this embodiment, a process of manufacturing a plurality of aluminum profiles to be bonded according to the product design is performed.

[0053] According to the mold preparation step S120 of the present embodiment, a process of manufacturing a mold according to the aluminum profile manufacturing design prepared through the product preparation step S110 is performed.

[0054] Specifically, the mold preparation step S120 may include: a mold gate forming step S121 for performing a specific process, a side through hole forming step S141, an ejector pin inserting step S142, and a block installation step S143. The mold gate forming step S121 of the mold preparation step S120 performs a process of forming a mold gate forming position according to the forming position of the filling hole of the aluminum profile, wherein the mold gate has a structure that discharges the injection material through the mold and leads it to the inside of the bonding part of the aluminum profile. Figure 6 and Fig. 9 As shown, the side through hole forming step S141 performs a process of guiding the injection material to be integrated with the aluminum profile by machining a through hole 12 on the side of the aluminum profile. Fig. 9 As shown, the ejector pin insertion step S142 performs a process of inserting the ejector pin 30 into the through hole formed by the side through hole forming step S141 to integrate the injection molded product with the aluminum profile. Figure 8 As shown, the block installation step S143 is a process of installing the block 40 inside the aluminum profile so as to form a space adjacent to the bonding portion and having a specified volume inside the aluminum profile.

[0055] According to the installation step S130 of this embodiment, a process of installing a plurality of aluminum profiles to be bonded in a mold in a state of contacting each other is performed.

[0056] According to the injection filling step S140 of this embodiment, a process is performed in which the injection material is filled into the contact part of the aluminum profile through the mold to form the aluminum profile to be bonded into one body.

[0057] As described above, according to the aluminum profile injection bonding method of the present invention, an aluminum profile injection bonding method S100 can be provided, which has a product preparation step S110, a mold preparation step S120, an installation step S130 and an injection filling step S140 for performing a specific process. When manufacturing an electric vehicle battery shell, aluminum profiles with various cross-sectional structures can be easily bonded and a stable bonding state can be maintained. Therefore, multiple bonding components or combining components can be omitted, thereby significantly reducing the cost required for manufacturing and construction, and at the same time, significantly shortening the construction time.

[0058] In the above detailed description of the present invention, only relevant specific embodiments are described. However, it should be understood that the present invention is not limited to the specific forms mentioned in the detailed description, but should be understood to include all modifications, equivalents and substitutes within the spirit and scope of the present invention defined in the scope of the appended claims.

[0059] That is, the present invention is not limited to the above-mentioned specific embodiments and descriptions, and any technician in the field to which the present invention belongs can make various modifications without departing from the main purpose of the present invention as claimed in the claims, and these modifications all fall within the protection scope of the present invention.

Claims

1. A method for injection bonding of aluminum profiles, It is characterized in that include: A product preparation step (S110), manufacturing a plurality of aluminum profiles to be bonded according to the product design; A mold preparation step (S120) of manufacturing a mold designed according to the aluminum profile prepared in the product preparation step (S110); an installation step (S130), installing a plurality of aluminum profiles to be bonded in a mold in a state of contacting each other; as well as Injection filling step (S140), filling the injection material into the contact part of the aluminum profile through the mold, so that the aluminum profile to be bonded is formed into one body.

2. The aluminum profile injection bonding method according to claim 1, It is characterized in that The mold preparation step (S120) includes: A mold gate forming step (S121) forms a mold gate forming position according to a forming position of a filling hole of the aluminum profile, wherein the mold gate has a structure for discharging the injection material through the mold and leading it to the inside of the bonding portion of the aluminum profile.

3. The aluminum profile injection bonding method according to claim 1, It is characterized in that The injection filling step (S140) includes: The side through hole forming step (S141) is to process a through hole (12) on the side of the aluminum profile to guide the injection material to be integrated with the aluminum profile.

4. The aluminum profile injection bonding method according to claim 3, It is characterized in that The injection filling step (S140) includes: The ejector pin inserting step (S142) inserts the ejector pin (30) into the through hole formed by the side through hole forming step (S141) so that the injection object and the aluminum profile are integrated into one.

5. The aluminum profile injection bonding method according to claim 1, It is characterized in that The injection filling step (S140) includes: The block installation step (S143) is to install the block (40) inside the aluminum profile so as to form a space adjacent to the bonding portion and having a specified volume inside the aluminum profile.