Laser adjusting cutting method for metal stamping part

By adjusting laser cutting parameters in real time, the problem of insufficient adjustment of cutting parameters in laser cutting of three-dimensional metal parts is solved, the cutting effect and energy utilization are improved, thermal damage and defects are reduced, and a more efficient cutting process is achieved.

CN118808945APending Publication Date: 2024-10-22TIANJIN UNIV OF TECH & EDUCATION (TEACHER DEV CENT OF CHINA VOCATIONAL TRAINING & GUIDANCE)

Patent Information

Application Number
CN202410926065.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-11
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

During the laser cutting process of three-dimensional metal parts, it is difficult to effectively adjust the laser power, cutting speed and cutting posture with the existing technology, resulting in a large heat-affected zone when cutting to the thinned area, incomplete cutting of the thickened area, and the inability to adapt to complex structures. This leads to defects such as hardening of the cut tissue, reduced material performance, and rough cut surfaces.

Method used

By obtaining the thickness distribution and normal distribution of the cutting path of the cut part, the laser power, cutting speed and cutting attitude are adjusted in real time, and the laser power adjustment module, cutting speed adjustment module and attitude adjustment module are established to realize dynamic adjustment of cutting parameters.

Benefits of technology

It improves the energy utilization rate and cutting effect of the laser cutting process, reduces thermal damage and defects, and improves the consistency of the kerf width and the smoothness of the cutting surface.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808945A_ABST
    Figure CN118808945A_ABST
Patent Text Reader

Abstract

The invention relates to a laser adjusting cutting method for a metal stamping part, which comprises the following steps of: analyzing and measuring the thickness and the normal direction of a cutting path of a cut part to obtain the thickness distribution and the normal distribution of the cutting path, and adjusting laser cutting parameters in the cutting process according to the thickness distribution and the normal distribution. And real-time adjustment of laser cutting parameters in the cutting process is completed. The cutting method can adapt to three-dimensional cutting, the cutting effect and the energy utilization rate in the laser cutting process can be improved, and the heat influence and defects on the cut part in the laser cutting process are reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of metal parts cutting, and in particular to a laser adjustment cutting method for metal stamping parts. Background Art

[0002] With the rapid development of advanced manufacturing technology, laser cutting technology has been widely used in aerospace, shipbuilding, automobile manufacturing, medical equipment and other fields due to its high automation, high adaptability and non-contact characteristics. The application scenarios have expanded from two-dimensional plane cutting to three-dimensional cutting. However, three-dimensional parts have diverse shapes and complex structures. Under the current production and manufacturing level, the parts produced must have thinning areas and thickening areas, especially stamping parts, which can reach a maximum thinning rate of about 20% compared with the original sheet. If such parts are still kept at a constant laser power and constant cutting speed during the laser cutting process, it will inevitably lead to a large heat-affected zone when cutting to the thinning area, causing hardening of the tissue at the cut of the cut part and reduced material properties; when cutting to the thickening area, incomplete cutting will occur, resulting in defects such as slag hanging and rough cut surface; and when three-dimensional cutting is cut to a steep vertical surface or a surface with a large curvature change, if the cutting posture is not adjusted in time, it will also cause the above defects.

[0003] For example, the US patent with application number US202218066362 discloses a laser cutting method for irregular parts based on machine vision, including: (a) obtaining the vertices of all parts on the layout diagram and numbering them; planning the part vertex set and the empty cutting path vertex set; obtaining the shortest empty cutting path and the empty cutting path vertex set with the shortest empty cutting path; (d) cutting the parts one by one according to the order obtained by the CPLEX algorithm. However, the energy utilization rate of this cutting method is low and the cutting effect is not good.

[0004] Another example is the Chinese invention patent with the authorization announcement number CN 112222631 B, which discloses a method for laser cutting of amorphous parts, including: fixing the amorphous alloy material to be processed on a photosensitive glass substrate; using a femtosecond laser to process the amorphous alloy material to be processed, and completing the processing when the photosensitive glass substrate emits continuous fluorescence. The invention adopts the method of sticking and fixing the amorphous alloy material on a photosensitive glass substrate, without the need for a special clamping tool, and can complete the laser cutting of the contour of the amorphous alloy material at one time, and it is easy to remove the processed parts from the photosensitive glass substrate; and the laser removal threshold of the glass substrate is extremely high, and the damage is very small during the laser cutting process, which can avoid the contamination of the amorphous amorphous alloy material. At the same time, the invention uses a photosensitive glass substrate doped with fluorescent substances, which will emit fluorescence after contacting the laser, and can efficiently judge the processing progress. The femtosecond laser method with extremely small thermal effect effectively avoids the oxidation of crystallization of amorphous alloy materials. However, this cutting method is only applicable to amorphous parts, and the thickness of the parts cannot be judged, and the cutting effect is poor. Summary of the invention

[0005] In order to solve the above-mentioned technical defects existing in the prior art, the purpose of the present invention is to provide a laser adjustment cutting method for metal stamping parts, which adjusts the laser power, cutting speed and cutting posture in real time by obtaining the thickness distribution on the cutting path of the cut parts, thereby improving the energy utilization rate and cutting effect in the laser cutting process, reducing the thermal damage and defects of the cut parts in the laser cutting process, and improving the consistency of the cutting width and the smoothness of the cutting surface.

[0006] In order to solve the above technical problems, the solution adopted by the present invention is as follows:

[0007] The present invention provides a laser adjustment and cutting method for metal stamping parts, comprising:

[0008] Step 1: Obtain the thickness distribution and normal distribution of the cutting path on the metal to be cut;

[0009] Step 2: Determine the cutting origin, obtain the initial value of laser power, initial value of cutting speed, and initial value of posture feature;

[0010] Step 3: Establish a laser power adjustment module and a cutting speed adjustment module according to the material characteristics; establish a posture adjustment module according to the robot arm posture adjustment characteristics;

[0011] Step 4: Output the laser power change value and cutting speed change value according to the thickness distribution; output the posture feature change value according to the normal distribution;

[0012] Step 5: Adjust the laser power, cutting speed and cutting posture during the cutting process according to the changed values.

[0013] The laser adjustment cutting method for metal stamping parts of the present invention obtains the thickness distribution and normal distribution of the cutting path by analyzing and measuring the thickness and normal direction of the cutting path of the cut piece, adjusts the laser cutting parameters during the cutting process according to the thickness distribution and normal distribution, and completes the real-time adjustment of the laser cutting parameters during the cutting process. The cutting method of the present invention can adapt to three-dimensional cutting, can improve the cutting effect and energy utilization rate during the laser cutting process, and reduce the thermal impact and defects of the laser cutting process on the cut piece.

[0014] Preferably, all parameter adjustments in the step one are based on a determined cutting path, and the cutting path needs to be determined first; when adjusting the laser power, cutting speed and cutting posture, the thickness distribution and normal distribution on the cutting path need to be obtained first; before the part is formed, grid points are printed on the material cutting path range, and after the part is formed, the part is photographed from multiple angles, and the grid points printed on the part cutting path are reverse modeled through an image recognition algorithm combined with the volume invariance theory of plastic deformation of metal materials, and a sheet model of the part and the cutting path is output; further data analysis is performed on the sheet model of the part and the cutting path to obtain the thickness distribution and normal distribution of the cutting path.

[0015] In any of the above schemes, it is preferred that in step 2, a point with a thickness equal to the initial thickness of the part sheet and a relatively stable normal direction is selected as the cutting origin, and the laser power, cutting speed and posture characteristics that achieve the optimal effect at the cutting origin are set as the initial values ​​of the cutting parameters, and subsequent cutting parameters are all based on changes in the initial values.

[0016] In any of the above schemes, it is preferred that in step three, the relationship between material thickness, laser power and cutting speed is determined according to the material reflectivity and thermal conductivity, an optimal solution calculation model is formed, and a laser power adjustment module and a cutting speed adjustment module are established; a posture adjustment module is established according to the robot arm adjustment speed and adjustment range.

[0017] In any of the above schemes, it is preferred that in step five, the laser emitting unit continuously adjusts the cutting process according to the model's continuous output laser power change value, cutting speed change value and posture feature change value.

[0018] In any of the above schemes, preferably, the steps one to four further include establishing a first power adjustment threshold and a first speed adjustment threshold.

[0019] In summary, the laser adjustment cutting method for metal stamping parts of the present invention has the following advantages: by analyzing and measuring the thickness and normal direction of the cutting path of the cut workpiece, the thickness distribution and normal distribution of the cutting path are obtained, and the laser cutting parameters are adjusted during the cutting process according to the thickness distribution and normal distribution, thereby completing the real-time adjustment of the laser cutting parameters during the cutting process; the cutting method of the present invention can adapt to three-dimensional cutting, can improve the cutting effect and energy utilization rate during the laser cutting process, and reduce the thermal impact and defects of the laser cutting process on the cut workpiece. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 The present invention is a flow chart of a preferred embodiment of the laser adjustment cutting method for metal stamping parts according to the present invention. DETAILED DESCRIPTION

[0021] The following description is merely exemplary in nature and is not intended to limit the disclosure, application or use of the present invention. The specific implementation of the laser adjustment cutting method for metal stamping parts of the present invention is further described below in conjunction with the accompanying drawings.

[0022] Embodiment 1:

[0023] like Figure 1 As shown, a flow chart of a preferred embodiment of the metal stamping part laser adjustment cutting method according to the present invention. The metal stamping part laser adjustment cutting method of the present invention comprises:

[0024] Step 1: Obtain the thickness distribution and normal distribution of the cutting path on the metal to be cut;

[0025] Step 2: Determine the cutting origin, obtain the initial value of laser power, initial value of cutting speed, and initial value of posture feature;

[0026] Step 3: Establish a laser power adjustment module and a cutting speed adjustment module according to the material characteristics; establish a posture adjustment module according to the robot arm posture adjustment characteristics;

[0027] Step 4: Output the laser power change value and cutting speed change value according to the thickness distribution; output the posture feature change value according to the normal distribution;

[0028] Step 5: Adjust the laser power, cutting speed and cutting posture during the cutting process according to the changed values.

[0029] The laser adjustment cutting method for metal stamping parts of the present invention obtains the thickness distribution and normal distribution of the cutting path by analyzing and measuring the thickness and normal direction of the cutting path of the cut piece, adjusts the laser cutting parameters during the cutting process according to the thickness distribution and normal distribution, and completes the real-time adjustment of the laser cutting parameters during the cutting process. The cutting method of the present invention can adapt to three-dimensional cutting, can improve the cutting effect and energy utilization rate during the laser cutting process, and reduce the thermal impact and defects of the laser cutting process on the cut piece.

[0030] In this embodiment, all parameter adjustments in the step one are based on a determined cutting path, and the cutting path needs to be determined first; when adjusting the laser power, cutting speed and cutting posture, the thickness distribution and normal distribution on the cutting path need to be obtained first; before the part is formed, grid points are printed on the material cutting path range, and after the part is formed, the part is photographed from multiple angles, and the grid points printed on the part cutting path are reverse modeled through an image recognition algorithm combined with the volume invariance theory of plastic deformation of metal materials, and a sheet model of the part and the cutting path is output; further data analysis is performed on the sheet model of the part and the cutting path to obtain the thickness distribution and normal distribution of the cutting path.

[0031] In this embodiment, in step 2, a point whose thickness is the initial thickness of the part sheet and whose normal direction is relatively stable is selected as the cutting origin, and the laser power, cutting speed and posture characteristics that achieve the optimal effect at the cutting origin are set as the initial values ​​of the cutting parameters, and subsequent cutting parameters are all based on the changes in the initial values.

[0032] In this embodiment, in step three, the relationship between material thickness, laser power and cutting speed is determined based on the material reflectivity and thermal conductivity, an optimal solution calculation model is formed, and a laser power adjustment module and a cutting speed adjustment module are established; a posture adjustment module is established based on the robot arm adjustment speed and adjustment range.

[0033] In this embodiment, in step five, the laser emitting unit continuously adjusts the cutting process according to the model's continuous output laser power change value, cutting speed change value and posture feature change value.

[0034] The laser adjustment cutting method for metal stamping parts of the present invention obtains the thickness of the cutting path sheet model and the distribution in the normal direction through reverse engineering technology or by adding an ultrasonic thickness gauge and a linear array camera to the laser cutting equipment. Before the cutting process, a robotic arm is used to obtain data according to the movement of the cutting path or to measure the thickness and normal of the cut parts, so as to obtain the thickness distribution and normal distribution on the cutting path of the parts. The cutting origin is obtained according to the thickness distribution and the normal distribution, and the initial value of the laser power, the initial value of the cutting power, and the initial value of the posture feature are determined according to the thickness parameter of the cutting origin and the normal direction.

[0035] The present invention establishes a laser power adjustment module and a cutting speed adjustment module based on thickness distribution according to the characteristics of metal materials and cutting effects. During the cutting process, the laser power adjustment module and the cutting speed adjustment module output laser power change values ​​and cutting speed change values ​​according to the thickness distribution; a posture adjustment module is established according to the posture adjustment characteristics of the robot arm, and during the cutting process, the posture feature change value is output according to the normal distribution.

[0036] Embodiment 1 has the following beneficial effects: by obtaining the thickness distribution on the cutting path of the cut part, the laser power, cutting speed and cutting posture are adjusted in real time, which improves the energy utilization and cutting effect during the laser cutting process, reduces the thermal damage and defects of the cut part during the laser cutting process, and improves the consistency of the cutting width and the smoothness of the cutting surface.

[0037] In this embodiment, the use of reverse engineering technology to obtain the thickness and normal direction of the sheet model is to print grid points on the material cutting path range before the part is formed, photograph the part from multiple angles after the part is formed, and reverse model the grid points printed on the part cutting path through an image recognition algorithm combined with the volume invariance theory of plastic deformation of metal materials to output the sheet model of the part and the cutting path; further data analysis is performed on the sheet model of the part and the cutting path to obtain the thickness distribution and normal distribution of the cutting path.

[0038] In this embodiment, the thickness and normal direction of the parts after cutting are measured by measuring the thickness and angle of the cut surface of the parts in the same batch after cutting. The thickness distribution and normal direction on the cutting path are obtained. An ultrasonic thickness gauge and a linear array camera are installed on the laser cutting equipment, and the robot moves along the cutting path to obtain data before cutting. The robot arm is used to measure the thickness and normal direction of the parts according to the planned cutting path, and the thickness distribution and normal direction on the cutting path of the parts are obtained by ultrasonic thickness measurement and linear array cameras.

[0039] In this embodiment, the thickness distribution and the normal distribution respectively describe the thickness variation and the normal direction variation on the part cutting path.

[0040] In this embodiment, the cutting origin is the cutting starting point, and generally a point whose thickness is the median of the thickness of the part material or the thickness of the cutting path and whose posture characteristic value is zero is selected as the cutting origin.

[0041] In this embodiment, the initial value of the laser power and the initial value of the cutting power need to meet the laser cutting requirements of the part cutting zero point, and the cutting effect must be guaranteed; the initial value of the posture feature can be determined according to the cutting posture at the beginning of cutting, and is used to measure the cutting angle of the laser on the cutting plane at the waypoint on the path. During the cutting process, it is necessary to ensure that the laser is directly shot at the waypoint on the cutting path at 90° to achieve the best cutting effect.

[0042] In this embodiment, the laser power adjustment module and cutting speed adjustment module based on thickness are established according to the metal material characteristics and cutting effect. Different materials have large differences in the same power laser cutting efficiency and cutting effect. When establishing the laser power adjustment module and cutting speed adjustment module based on thickness, the influence of material characteristics must be fully considered. The laser power adjustment module and the cutting speed adjustment module calculate the laser power and cutting speed accordingly based on the characteristics of different materials and the comprehensive thickness change, output the laser power change value and the cutting speed change value, and adjust the laser power and cutting speed in real time according to the thickness distribution.

[0043] In this embodiment, a posture adjustment module is established according to the posture adjustment characteristics of the robot arm, and corresponding calculations are performed based on the posture characteristic values ​​of the points along the cutting path according to the adjustment rate and adjustment angle of the robot arm to output a posture characteristic change value.

[0044] In this embodiment, the posture feature value expresses the laser incident angle of the waypoint on the cutting path on its cutting plane, and the entire cutting process is completed by comprehensive cutting path planning.

[0045] In this embodiment, the characteristic data includes: thickness distribution, normal distribution, laser power initial value, cutting power initial value, posture characteristic initial value, laser power change value, cutting speed change value, posture characteristic change value.

[0046] Embodiment 2:

[0047] The laser adjustment cutting method for metal stamping parts of the present invention further includes establishing a first power adjustment threshold and a first speed adjustment threshold based on steps one to four.

[0048] It is not difficult for a person skilled in the art to understand that the metal stamping parts laser adjustment cutting method of the present invention includes any combination of the parts in this specification. Due to the limited space and to make the specification concise, these combinations are not introduced in detail one by one here, but after reading this specification, the scope of the present invention constituted by any combination of the parts constituting this specification is self-evident.

Claims

1. A laser adjustment and cutting method for metal stamping parts, Features include, Step 1: Obtain the thickness distribution and normal distribution of the cutting path on the metal to be cut; Step 2: Determine the cutting origin, obtain the initial value of laser power, initial value of cutting speed, and initial value of posture feature; Step 3: Establish a laser power adjustment module and a cutting speed adjustment module according to the material characteristics; establish a posture adjustment module according to the robot arm posture adjustment characteristics; Step 4: Output the laser power change value and cutting speed change value according to the thickness distribution; output the posture feature change value according to the normal distribution; Step 5: Adjust the laser power, cutting speed and cutting posture during the cutting process according to the changed values.

2. The detection method of the laser adjustment cutting method of metal stamping parts according to claim 1, Features: All parameter adjustments in the step one are based on the determined cutting path, and the cutting path needs to be determined first; when adjusting the laser power, cutting speed and cutting posture, the thickness distribution and normal distribution on the cutting path need to be obtained first; before the part is formed, grid points are printed on the material cutting path range, and after the part is formed, the part is photographed from multiple angles, and the grid points printed on the part cutting path are reverse modeled through the image recognition algorithm combined with the volume invariance theory of plastic deformation of metal materials, and the sheet model of the part and the cutting path is output; further data analysis is performed on the sheet model of the part and the cutting path to obtain the thickness distribution and normal distribution of the cutting path.

3. The detection method of the laser adjustment cutting method of metal stamping parts according to claim 1, Features: In the step 2, a point with a thickness equal to the initial thickness of the part sheet and a relatively stable normal direction is selected as the cutting origin, and the laser power, cutting speed and posture characteristics that achieve the optimal effect at the cutting origin are set as the initial values ​​of the cutting parameters, and subsequent cutting parameters are all based on the changes in the initial values.

4. The detection method of the laser adjustment cutting method of metal stamping parts according to claim 1, Features: In the step three, the relationship between material thickness, laser power and cutting speed is determined according to the material reflectivity and thermal conductivity, an optimal solution calculation model is formed, and a laser power adjustment module and a cutting speed adjustment module are established; a posture adjustment module is established according to the robot arm adjustment speed and adjustment range.

5. The detection method of the laser adjustment cutting method of metal stamping parts according to claim 1, Features: In the step 5, the laser emitting unit continuously adjusts the cutting process according to the model's continuous output laser power change value, cutting speed change value and posture feature change value.

6. The detection method of the laser adjustment cutting method of metal stamping parts according to claim 1, Features: Based on the steps 1 to 4, the method further includes establishing a first threshold for power adjustment and a first threshold for speed adjustment.

Citation Information

Patent Citations

  • A laser cutting method for amorphous parts

    CN112222631B

  • Laser cutting method and system for irregular parts based on machine vision

    US20230136158A1

  • Laser cutting method

    CN102000916A

  • Laser cutting method and laser cutting platform

    CN112975164A

  • Laser cutting device and cutting method for profiled bar

    CN113084365A

Cited By

  • Die casting forming method and device

    CN119426785A

  • Pole piece processing system and method, pole piece processing production line and battery processing production line

    CN120734563A