Battery shell bottom welding quality testing method

By cutting and bending the current collector plate and combining it with the battery case, the welding quality of the bottom of the cylindrical power battery case can be directly judged, which solves the problems of cumbersome and high-cost debugging of welding parameters in the existing technology, and improves the battery production yield. and security.

CN118808980APending Publication Date: 2024-10-22DONGGUAN CHAM BATTERY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410835816.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-26
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

In the current laser penetration welding process of the cylindrical power battery shell bottom, it is difficult to intuitively and comprehensively judge the welding penetration and welding quality, resulting in cumbersome debugging of welding parameters, high cost, low production yield, and prone to safety problems.

Method used

By cutting the battery case to retain the bottom, bending to form a stacked current collecting plate and combining it with the roll core, laser penetration welding is performed, and the welding track is observed by opening the main body and pulling the extension to directly judge the welding quality. , adjust the welding parameters to determine the best welding parameters.

Benefits of technology

It enables quick and intuitive judgment of the welding quality of the battery case bottom and the current collecting plate, improves the welding test speed, ensures the confirmation of the best welding parameters, improves the battery production yield and reduces safety risks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808980A_ABST
    Figure CN118808980A_ABST
Patent Text Reader

Abstract

The invention discloses a battery shell bottom welding quality testing method which comprises the steps that the number of stacked layers formed by bending of a collector plate is determined based on welding parameters, and the welding parameters comprise the shell bottom thickness, the preset welding fusion depth and the base material thickness of the collector plate; the battery shell is cut, the shell bottom of the battery shell is reserved, and a DOE shell bottom is obtained; the bent current collecting plate is attached to a full tab at one end of the roll core, the roll core is sleeved with the DOE shell bottom, the current collecting plate is attached to the bottom wall of the DOE shell bottom, and all layers of the current collecting plate are tightly attached; laser penetration welding is conducted from the outer side of the DOE shell bottom according to the preset welding penetration depth; and the DOE shell bottom and the collector plate are taken down, and the welding quality between the DOE shell bottom and the collector plate is judged. According to the method, the welding penetration condition of the battery shell bottom and the collector plate and whether the problems of insufficient welding and over-welding occur or not can be visually and comprehensively judged, the shell welding quality testing speed is increased, the optimal welding parameters can be quickly confirmed, the battery production yield can be increased, and the battery safety problem can be avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of batteries, and in particular to a method for testing the welding quality of a battery shell bottom. Background Art

[0002] As an important component of electric vehicles, cylindrical power batteries such as lithium-ion and sodium-ion are widely used in the field of electric vehicles due to their advantages such as small size, high energy density and green environmental protection. However, cylindrical power batteries still have the following common problems:

[0003] 1. In order to meet the needs of high-rate charging and discharging, increase production capacity and simplify the structure of cylindrical power batteries, some companies have begun to try laser penetration welding to weld the shell bottom and the current collecting plate. However, the laser penetration welding process must first be verified by DOE of the shell bottom laser penetration welding. It is necessary to continuously change different parameters to find the best parameters, and it is necessary to go through operations such as cutting sections, polishing and etching to measure the penetration depth. It is impossible to intuitively confirm the welding penetration depth and welding quality, and the DOE verification process is cumbersome, the test cycle is long, and the cost is high.

[0004] 2. The penetration welding of the bottom of the cylindrical power battery shell requires the use of high-power laser welding. When the welding parameters are not adjusted properly, it is easy to have large fluctuations in the depth of penetration or excessive laser energy locally, resulting in welding penetration. The conventional DOE sectioning test method can only randomly observe one surface and cannot confirm whether there is an over-welding problem in the entire welding trajectory, resulting in the inability to confirm the optimal welding parameters, which ultimately leads to low battery production yield and battery safety problems. Summary of the invention

[0005] The purpose of this application is to provide a battery shell bottom welding quality testing method, which can intuitively and comprehensively determine whether there are problems of cold welding or over welding between the battery shell bottom and the current collecting plate, thereby improving the speed of shell welding testing and facilitating the confirmation of optimal welding parameters.

[0006] In order to achieve the above objectives, the present application provides a battery shell bottom welding quality testing method, comprising:

[0007] Determining the number of stacked layers of the current collecting plate to be formed by bending based on welding parameters, wherein the welding parameters include: shell bottom thickness, preset welding penetration, and base material thickness of the current collecting plate;

[0008] Cutting the battery shell, retaining the shell bottom of the battery shell, and obtaining the DOE shell bottom;

[0009] The bent current collecting disk is attached to the full pole ear at one end of the winding core, and the DOE shell bottom is sleeved on the winding core, so that the current collecting disk is attached to the bottom wall of the DOE shell bottom and the layers of the current collecting disk are tightly attached;

[0010] Perform laser penetration welding from the outside of the bottom of the DOE shell according to the preset welding penetration depth;

[0011] Remove the bottom of the DOE shell and the current collector from the core, and judge the welding quality between the bottom of the DOE shell and the current collector.

[0012] Optionally, the welding parameters further include the fluctuation tolerance of the preset welding penetration depth.

[0013] Optionally, the side wall height of the bottom of the DOE shell is 1 mm to 7 mm.

[0014] Optionally, the current collector includes a main body portion and at least one extension portion extending and bent from the main body portion, and the extension portion is stacked on the main body portion;

[0015] The side of the main body portion facing away from the extension portion is attached to the full tab of the core, and the extension portion away from the main body portion is attached to the bottom wall of the bottom of the DOE shell.

[0016] Optionally, when the current collector is attached to the full tab of the core, the portion of the extension portion and the main body portion facing each other completely covers the through hole of the core.

[0017] Optionally, the attaching the current collector to the bottom wall of the bottom of the DOE shell and the layers of the current collector being closely attached includes:

[0018] Use a welding fixture to press against the core and pass through the through hole of the core to press against the current collector, so that the current collector is attached to the bottom wall of the bottom of the DOE shell and the layers of the current collector are closely attached.

[0019] Optionally, the value range of the preset welding penetration depth is T + 0.5t < t1 ≤ T + (n - 1), where T is the thickness of the bottom of the shell, and t is the substrate thickness of the current collector.

[0020] Optionally, the value range of the preset welding penetration depth is T + (n - 1.5)*t < t1 ≤ T + (n - 1)*t.

[0021] Optionally, the judging the welding quality between the bottom of the DOE shell and the current collector includes:

[0022] Perform an operation of lifting the main body portion;

[0023] If there is an adhesive force between the main body portion and the extension portion, it is confirmed that the welding track at least partially penetrates the extension portion;

[0024] If the main body is opened, the welding condition between the DOE shell bottom and the extension part can be determined by observing the adhesive residue of the main body and pulling the extension part circumferentially along the welding track.

[0025] Optionally, after determining the welding quality between the DOE shell bottom and the current collecting plate, the method further comprises:

[0026] Adjust the parameters of laser penetration welding according to the judgment results.

[0027] The battery shell welding quality test method provided in the present application first determines the number of layers of the current collecting disk after bending according to parameters such as the shell bottom thickness, preset welding penetration and the base material thickness of the current collecting disk, and then cuts the battery shell to obtain the DOE shell bottom. When welding, the bent current collecting disk is first placed on the winding core without welding and fixing, and then the pre-cut DOE shell bottom is placed on the winding core and the current collecting disk. When welding, the DOE shell bottom is tightly fitted with the extension of the upper layer of the current collecting disk, the layers of the current collecting disk, and the main body and the winding core, and the laser is penetrated from the outside of the DOE shell bottom. After welding, the welded DOE shell bottom and current collecting plate are removed. The cut DOE shell bottom can be conveniently observed by directly opening the main body, pulling the extension part, etc., to confirm the welding quality of the current collecting plate and the shell bottom. The present application does not need to cut the welded battery, and can intuitively and comprehensively judge the welding penetration of the battery shell bottom and the current collecting plate and whether there are problems of cold welding and over-welding. The speed of shell welding quality test is improved, which is conducive to quickly confirming the optimal welding parameters, thereby improving the battery production yield and reducing the probability of battery safety problems. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 This is a flow chart of a battery case bottom welding quality testing method according to an embodiment of the present application.

[0029] Figure 2 It is a schematic diagram of the three-dimensional structure of the current collecting plate before bending according to an embodiment of the present application.

[0030] Figure 3 This is a schematic diagram of a current collecting plate after bending according to an embodiment of the present application.

[0031] Figure 4 This is a schematic diagram of the current collecting plate after bending according to the second embodiment of the present application.

[0032] Figure 5 Schematic diagram of the bent current collecting plate of the third embodiment of the present application

[0033] Figure 6 This is a schematic diagram of the three-dimensional structure of the DOE shell bottom obtained after cutting according to the embodiment of the present application.

[0034] Figure 7It is a schematic diagram of the three-dimensional structure of the bent collecting plate placed on the winding core in the embodiment of the present application.

[0035] Figure 8 It is a schematic diagram and a partial enlarged diagram of the cross-sectional structure of the winding core, the collecting plate and the DOE shell bottom during welding in the embodiment of the present application.

[0036] Fig. 9 This is a schematic diagram of the three-dimensional structure of the embodiment of the present application when the DOE shell bottom and the current collecting plate are removed from the winding core and the main body is lifted up for observation. DETAILED DESCRIPTION

[0037] In order to explain the technical content, structural features and achieved effects of the present application in detail, the following is a detailed description in combination with the implementation methods and the accompanying drawings.

[0038] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present application, so the present application is not limited by the specific embodiments disclosed below.

[0039] See also Figure 1 , the present application discloses a battery shell bottom welding quality testing method, comprising:

[0040] S1, determining the number of stacked layers of the current collecting plate 1 that needs to be formed by bending based on welding parameters, the welding parameters including: shell bottom thickness, preset welding penetration and base material thickness of the current collecting plate 1.

[0041] It is understandable that when performing penetration welding on the bottom of the battery shell, changes in parameters such as welding current will cause fluctuations in penetration depth. If the welding parameters cannot be accurately controlled, damage to the core 3 may occur due to over-welding during the welding process. Therefore, the thickness of the current collecting plate can be adjusted based on the fluctuation in penetration depth.

[0042] The number of stacked layers formed after the current collecting disc 1 is bent can be determined based on the manufacturing process window. When the base material thickness of the current collecting disc 1 is t, the thickness of the current collecting disc after bending is t*n, where n is the number of layers of the current collecting disc 1 after bending.

[0043] It can be understood that the thickness of the current collecting plate after bending refers to the overall thickness of the current collecting plate 1 when its layers are tightly fitted together after bending.

[0044] Specifically, in the present application, the number of stacked layers n is at least two layers. In the present application, n is preferably 2 or 3. Of course, the present application does not limit the numerical selection of n.

[0045] In some embodiments, the collecting plate 1 includes a main body 11 and at least one extension portion 12 extending from the main body 11 and bent, and the extension portion 12 is stacked on the main body 11. Bending the collecting plate 1 may include: bending and stacking the extension portion 12 on the main body 11 based on a determined number of stacking layers.

[0046] In some embodiments, when n is 2, Figure 2 The extension portion 12 of the collecting plate 1 shown in the figure is bent toward the main body 11 along the connection between the main body 11 and the extension portion 12 and is superimposed on the main body 11. Figure 3 shown.

[0047] See also Figure 4 In some embodiments, when n is 3, the length of the extension portion 12 can be longer than when n is 2, so as to facilitate the double bending. The extension portion 12 is first bent toward the main body 11 along the connection between the main body 11 and the extension portion 12, and then the extension portion 12 is folded in half along its approximate middle to form a three-layer collector plate structure.

[0048] See also Figure 5 In some embodiments, when n is 3, the first extension portion 121 on one side of the main body 11 is first bent toward the main body 11 along the connection between the main body 11 and the extension portion 12 and stacked on the main body 11, and the second extension portion 122 on the other side is bent toward the main body 11 along the connection between the main body 11 and the extension portion 12 and stacked on the first extension portion 121.

[0049] Of course, the present application is not limited to the above three implementations, and the present application will not elaborate on other implementations in detail.

[0050] Specifically, the welding parameters also include a fluctuation tolerance of the preset welding penetration depth. Since errors in welding penetration depth are inevitable during the welding process, it is necessary to determine the fluctuation tolerance to facilitate controlling the welding penetration depth within a reasonable range.

[0051] Of course, welding parameters may also include relevant parameters of laser welding equipment, etc., which will not be elaborated in detail in this application.

[0052] S2, cutting the battery shell, retaining the shell bottom of the battery shell, and obtaining the DOE shell bottom 2.

[0053] See also Figure 6 It can be understood that when cutting the battery shell, the cutting position can be as close to the shell bottom as possible, under the premise of ensuring that the DOE shell bottom 2 can be sleeved on the winding core 3 during subsequent welding, so as to facilitate the subsequent removal of the welded DOE shell bottom 2 and the collecting plate 1 for observation of the welding condition.

[0054] Specifically, the side wall height H of the DOE bottom case 2 is preferably 1 mm to 7 mm. Of course, the value of the side wall height H of the DOE bottom case 2 in this application is not limited.

[0055] S3. Attach the bent current collector 1 to the full tab at one end of the winding core 3, and sleeved the DOE bottom case 2 on the winding core 3, so that the current collector 1 is attached to the bottom wall of the DOE bottom case 2 and each layer of the current collector 1 is closely attached.

[0056] It can be understood that in step S3, the current collector 1 is only attached to the full tab of the winding core 3, and is not welded and fixed.

[0057] Please refer to Figure 7 and Figure 8 , specifically, one side of the main body portion 11 facing away from the extension portion 12 is attached to the full tab of the winding core 3, and the extension portion 12 away from the main body portion 11 is attached to the bottom wall of the DOE bottom case 2.

[0058] Specifically, when the current collector 1 is attached to the full tab of the winding core 3, the portion of the extension portion 12 facing the main body portion 11 completely covers the through hole 31 of the winding core 3.

[0059] S4. Perform laser penetration welding from the outside of the DOE bottom case 2 according to a preset welding penetration depth.

[0060] In some embodiments, attaching the current collector 1 to the bottom wall of the DOE bottom case 2 and closely attaching each layer of the current collector 1 includes: using a welding fixture (not shown in the figure) to顶住 the winding core 3 and pass through the through hole 31 of the winding core 3 to顶住 the current collector 1, so that the current collector 1 is attached to the bottom wall of the DOE bottom case 2 and each layer of the current collector 1 is closely attached.

[0061] In some embodiments, the range of the t1 value of the preset welding penetration depth is T + 0.5t < t1 ≤ T + (n - 1)*t, where T is the thickness of the bottom case and t is the base material thickness of the current collector 1.

[0062] Specifically, the range of the value t1 of the preset welding penetration depth is preferably T + (n - 1.5)*t < t1 ≤ T + (n - 1)*t, n ≥ 2.

[0063] S5. Remove the DOE bottom case 2 and the current collector 1 from the winding core 3, and judge the welding quality between the DOE bottom case 2 and the current collector 1.

[0064] Please refer to Fig. 9 , specifically, judging the welding quality between the DOE bottom case 2 and the current collector 1 includes:

[0065] Perform the operation of lifting the main body portion 11;

[0066] It should be noted that there seems to be an incorrect expression "顶住" in the original text which is translated as "顶住" in the above translation. It might need to be corrected to a more appropriate word in the context.If there is bonding between the main body 11 and the extension 12, it is confirmed that the welding track at least partially penetrates the extension 12;

[0067] If the main body 11 is opened, the welding condition between the DOE shell bottom 2 and the extension part 12 can be determined by observing the adhesive residue of the main body and pulling the extension part 12 circumferentially along the welding track.

[0068] By observing and pulling, it can be determined whether there is a cold weld on the DOE shell bottom 2. According to the number of welded fixed layers, the penetration position can be determined. In addition, the welding trajectory can be observed to determine whether the welding energy is balanced. It can be understood that in the case where there is an adhesive force between the main body 11 and the extension 12, it can be determined whether to perform subsequent tests according to the settings. For example, if the adhesive force between the main body 11 and the extension 12 is large, making it difficult to open, it is not necessary to open and operate after opening. If there is an adhesive force between the main body 11 and the extension 12, but the effect on opening the main body 11 is small, the main body 11 can be opened and the welding condition between the DOE shell bottom 2 and the extension 12 can be determined by observing and pulling the extension 12. Of course, the welding trajectory may not penetrate the extension 12 at all, in which case the main body 11 can be opened normally.

[0069] Of course, it is not ruled out that when removing the DOE shell bottom 2 and the collecting plate 1, the DOE shell bottom 2 and the collecting plate 1 are not welded together and are directly separated, or the DOE shell bottom 2 and the collecting plate 1 cannot be smoothly removed from the winding core 3, which indicates that there is a large deviation in the welding situation.

[0070] After determining the welding quality between the DOE shell bottom 2 and the current collecting plate 1, the method further includes:

[0071] Adjust the parameters of laser penetration welding according to the judgment results.

[0072] Specifically, based on the welding quality result determined in step S5, the laser welding parameters can be adjusted to improve the penetration depth, the number of welding layers, and the energy consistency of the welding trajectory.

[0073] The battery shell welding quality test method provided in the present application first determines the number of layers of the current collecting disc 1 after bending according to parameters such as the shell bottom thickness, the preset welding penetration depth and the base material thickness of the current collecting disc 1, bends the current collecting disc 1, and then cuts the battery shell to obtain the DOE shell bottom 2. When welding, the bent current collecting disc 1 is first placed on the winding core 3 without welding and fixing, and then the pre-cut DOE shell bottom 2 is sleeved on the winding core 3 and the current collecting disc 1. When welding, the DOE shell bottom 2 is tightly fitted with the extension 12 of the upper layer of the current collecting disc 1, the layers of the current collecting disc 1, and the main body 11 and the winding core 3, and the DOE shell bottom 2 is welded. Laser penetration welding is performed on the outer side of the DOE shell, and finally the welded DOE shell bottom 2 and the current collecting plate 1 are removed. The cut DOE shell bottom 2 can be conveniently observed by directly opening the main body 11, pulling the extension part 12, etc., to confirm the welding quality of the current collecting plate 1 and the shell bottom. The present application does not need to cut the battery after welding, and can intuitively and comprehensively judge the welding penetration depth between the battery shell bottom and the current collecting plate 1 and whether there are problems of cold welding and over welding, which improves the speed of shell welding quality testing and is conducive to quickly confirming the optimal welding parameters, thereby improving the battery production yield and reducing the probability of battery safety problems.

[0074] The above disclosure is only a preferred example of the present application, and its role is to facilitate the technical personnel in this field to understand and implement it. Of course, it cannot be used to limit the scope of rights of the present application. Therefore, equivalent changes made according to the scope of the patent application of the present application still fall within the scope covered by the present application.

Claims

1. A battery shell bottom welding quality testing method, characterized in that: Including: Determining the number of stacked layers that the current collector plate needs to be formed by bending based on welding parameters, where the welding parameters include: the thickness of the battery bottom, the preset welding penetration depth, and the base material thickness of the current collector plate; Cutting the battery housing, retaining the battery bottom of the battery housing, to obtain a DOE battery bottom; Attaching the bent current collector plate to the full tab at one end of the winding core, sleeving the DOE battery bottom on the winding core, so that the current collector plate is attached to the bottom wall of the DOE battery bottom and the layers of the current collector plate are closely attached; Performing laser penetration welding from the outside of the DOE battery bottom according to the preset welding penetration depth; Removing the DOE battery bottom and the current collector plate from the winding core, and judging the welding quality between the DOE battery bottom and the current collector plate.

2. The battery case bottom welding quality testing method according to claim 1, characterized in that: The welding parameters further include the fluctuation tolerance of the preset welding penetration depth.

3. The battery case bottom welding quality testing method according to claim 1, characterized in that: The side wall height of the DOE battery bottom is 1 mm to 7 mm.

4. The battery case bottom welding quality testing method according to claim 1, characterized in that: The current collector plate includes a main body portion and at least one extension portion that extends from the main body portion and is bent, and the extension portion is stacked on the main body portion; The side of the main body portion facing away from the extension portion is attached to the full tab of the winding core, and the extension portion away from the main body portion is attached to the bottom wall of the DOE battery bottom.

5. The battery case bottom welding quality testing method according to claim 4, characterized in that: When the current collector plate is attached to the full tab of the winding core, the portion where the extension portion and the main body portion face each other completely covers the through hole of the winding core.

6. The battery case bottom welding quality testing method according to any one of claims 1 to 5, characterized in that: The making the current collector plate be attached to the bottom wall of the DOE battery bottom and the layers of the current collector plate be closely attached includes: Using a welding fixture to press against the winding core and pass through the through hole of the winding core to press against the current collector plate, so that the current collector plate is attached to the bottom wall of the DOE battery bottom and the layers of the current collector plate are closely attached.

7. The battery case bottom welding quality testing method according to claim 4, characterized in that: The value range of the preset welding penetration depth is T + 0.5t < t1 ≤ T + (n - 1)*t, where T is the thickness of the battery bottom and t is the base material thickness of the current collector plate.

8. The battery case bottom welding quality testing method according to claim 7, characterized in that: The value range of the preset welding penetration depth is T + (n - 1.5)*t < t1 ≤ T + (n - 1)*t.

9. The battery case bottom welding quality testing method according to claim 7, characterized in that: The performing the judgment on the welding quality between the DOE battery bottom and the current collector plate includes: Performing an operation of lifting the main body portion; If there is an adhesive force between the main body portion and the extension portion, it is confirmed that the welding track at least partially penetrates the extension portion; If the main body portion is lifted, the welding condition between the DOE battery bottom and the extension portion is judged by observing the adhesive residue of the main body portion and pulling the extension portion circumferentially along the welding track.

10. The battery case bottom welding quality testing method according to claim 9, characterized in that: After the performing the judgment on the welding quality between the DOE battery bottom and the current collector plate, the method further includes: Adjusting the parameters of the laser penetration welding according to the judgment result.