Pressing-breaking device, method for manufacturing laminated electrode, and method for manufacturing laminated battery

By using a press-breaking device with a specific angle and gap length to cut off the stacked electrode sheets in the manufacturing of lithium secondary batteries, the problems of interlayer short circuit and cracks are solved, and the battery performance is improved and the accuracy of electrode separation is achieved.

CN118809734APending Publication Date: 2024-10-22TOYOTA JIDOSHA KK
6 Cites -1 Cited by

Patent Information

Application Number
CN202410443030.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-04-19
Filing Date
2024-04-12
Publication Date
2024-10-22

Smart Images

  • Figure CN118809734A_ABST
    Figure CN118809734A_ABST
Patent Text Reader

Abstract

The breaking device according to the present disclosure is provided with: a placement table on which a laminated electrode sheet is placed; a pressing mechanism that presses the laminated electrode sheet; and at least one cutting edge tool. By means of a cutting edge tool moving in a first direction with respect to a placement table, the breaking device of the present disclosure bends and breaks a portion of a protruding region of a laminated electrode sheet that is pressed by a pressing mechanism in a second direction orthogonal to the first direction, said protruding region protruding outward from the placement table and the pressing mechanism. The cutting edge portion of the cutting edge tool has an angle of 15 DEG to 30 DEG with respect to the second direction. The blade portion has an acute angle with respect to the first direction. A length in the second direction of a gap between the blade portion and an end of the placement table on the cutting blade tool side is 10% to 35% of a length in the first direction of the laminated electrode sheet.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a press-breaking device, a method for manufacturing a stacked electrode, and a method for manufacturing a stacked battery. Background Art

[0002] In recent years, the demand for high-output lithium secondary batteries as large energy sources such as electric vehicles has increased. Usually, in the process of manufacturing lithium secondary batteries, from the viewpoint of improving energy density, the area (for example, coating omission area, layer dislocation area, etc.) that does not play a role in power generation elements in the lithium secondary battery is cut off.

[0003] Japanese Patent Application Publication (JP-A) No. 2015-153538 discloses an electrode cutting device. The cutting device disclosed in JP-A No. 2015-153538 cuts a sheet electrode provided with an active material layer on a foil-like collector by a shearing operation based on the engagement of an upper blade and a lower blade which are linear blades and arranged to face each other, resulting from the movement of approaching and separating each other. At the upper blade, the outer corner portion formed by the side surface of the blade and the working contact surface of the upper blade is a cutting edge. The blade tip angle of the cutting edge is set to 90°. A specific rearward tilt surface is formed at the upper blade. Specifically, there is no gap between the lower blade and the upper blade.

[0004] The operation steps of the cutting device disclosed in JP-A No. 2015-153538 are as follows: FIG. 11A to FIG. 11C As shown in FIG. 11A to FIG. 11C , reference numeral 901 is a collector, reference numeral 902 is an active material layer, and reference numeral 903 is an active material layer.

[0005] In JP-A No. 2015-153538, an electrode substrate 900 is placed between an upper blade 910 and a lower blade 920 separated in the vertical direction. As the upper blade 910 descends, the electrode substrate 900 is separated into a first electrode 900A and a second electrode 900B. Specifically, when the upper blade 910 descends, as shown in FIG. Fig.11A As shown in FIG. , the upper blade 910 contacts the electrode substrate 900. Thereafter, as Fig. 11B As shown in FIG. 1 , the upper blade 910 pushes the electrode substrate 900 downward. Fig. 11C As shown in FIG. 1 , the cutting edge 911 of the upper blade 910 is engaged with the cutting edge 921 of the lower blade 920. At this time, the electrode 930 is cut out from the electrode substrate 900 due to the shearing action based on the engagement of the cutting edge 911 of the upper blade 910 with the cutting edge 921 of the lower blade 920.

[0006] However, in the process of cutting the electrode base material 900 by using the cutting device disclosed in JP-A No. 2015-153538, as Fig. 11Band Fig. 11C As shown in , there is a concern that the shear surface S900A of the first electrode 900A and the blade side surface S910 of the upper blade 910 may rub against each other. In addition, there is a concern that the shear surface S900A of the first electrode 900A and the shear surface S900B of the second electrode 900B may rub against each other. Therefore, there is a concern that the structural layers may be mixed at the surface of the shear surface S900A of the first electrode 900A, and a short circuit (hereinafter also referred to as "interlayer short circuit") may occur between the structural layers of the first electrode 900A. Summary of the invention

[0007] The present disclosure has been made in view of the above circumstances. The subject of the embodiments of the present disclosure is to provide a press-breaking device, a method for manufacturing a laminated electrode, and a method for manufacturing a laminated battery, which can separate laminated electrode sheets into desired sizes while suppressing the occurrence of interlayer short circuits and the generation of cracks.

[0008] The methods used to address the above topics include the following aspects:

[0009] <1> The first aspect of the present disclosure is a pressure-breaking device, comprising the following pressure-breaking device: a placing table on which the stacked electrode sheets are placed; A pressing mechanism that presses the stacked electrode sheet placed on the placement table; and at least one cutting edge tool, The breaking device is configured so that, by at least one cutting edge tool moving in a first direction relative to the placing table, the breaking device bends and breaks a portion of a protruding area of ​​the stacked electrode sheet pressed by the pressing mechanism in a second direction orthogonal to the first direction, which protrudes outward from the placing table and the pressing mechanism, wherein: The angle of the blade portion of the cutting edge tool relative to the second direction is 15° to 30°, The angle of the blade portion relative to the first direction is an acute angle, and The length of the gap between the blade portion and the end of the placement table on the cutting blade tool side in the second direction is 10% to 35% of the length of the laminated electrode sheet in the first direction.

[0010] The "laminated electrode sheet" includes at least a first active material sheet, a second active material sheet, and an insulating sheet that electrically insulates the first active material sheet from the second active material sheet. The insulating sheet is interposed between the first active material sheet and the second active material sheet in a first direction. The "cutting edge portion" is formed by the rake surface of the cutting edge tool and the relief surface of the cutting edge tool.

[0011] In the first aspect, when separating the stacked electrode sheet into at least two parts, the cutting edge tool moved along the first direction relative to the placement table contacts the protruding area of ​​the stacked electrode sheet pressed by the pressing mechanism, and bends the protruding area. In the state where the protruding area is bent, the blade portion of the cutting edge tool cuts into the surface of the protruding area. In addition, when the cutting edge tool moves along the first direction, a break is formed starting from the area in the protruding area cut by the blade portion of the cutting edge tool (hereinafter, this area is also referred to as the "cut-in line"), and a part of the protruding area is separated. As a result, a stacked electrode is obtained in which the end of the stacked electrode sheet on the cutting edge tool side (hereinafter referred to as the "edge material") is separated. In the first aspect, the angle of the blade portion of the cutting edge tool relative to the second direction (hereinafter also referred to as the "rake angle") is greater than or equal to 15°. As a result, the blade portion of the cutting edge tool is easier to cut into the protruding area than when the rake angle is less than 15°. Therefore, it is easy to form a break in the protruding area starting from the cutting line. In other words, when viewed from the first direction, the shape of the end of the obtained stacked electrode on the cutting edge tool side is unlikely to become a serrated shape. As a result, the first aspect's breaking device can separate the stacked electrode sheets into desired sizes. In the first aspect, the rake angle is less than or equal to 30°. As a result, it is more difficult for the blade portion of the cutting edge tool to cut into the protruding area compared to the case where the rake angle exceeds 30°. Therefore, it is difficult to perform a press-break of the protruding area by the sharp blade portion itself. That is, when a part of the protruding area is separated, it is difficult for the blade portion of the cutting edge tool and the separation surface of the protruding area to rub against each other. As a result, the press-break device of the first aspect can suppress the occurrence of interlayer short circuits. In the first aspect, the angle of the blade portion of the cutting edge tool relative to the first direction (hereinafter also referred to as the "back rake angle") is an acute angle. As a result, the separation surface of the obtained stacked electrode is less likely to rub against the cutting edge tool than when the back rake angle is not an acute angle. As a result, the first aspect of the press-breaking device can suppress the occurrence of interlayer short circuits. In the first aspect, the length of the gap between the blade portion and the end of the placement table on the cutting tool side in the second direction (hereinafter also referred to as "the length of the gap") is greater than or equal to 10% of the length of the stacked electrode sheet in the first direction. As a result, the protruding area is more easily bent by the moving cutting tool than in the case where the length of the gap is less than 10% of the length of the stacked electrode sheet in the first direction. Therefore, in the step of separating the edge material from the stacked electrode sheet, the separation surface of the stacked electrode is difficult to rub against the cutting tool and the edge material, respectively. As a result, the first aspect of the breaking device can suppress the occurrence of interlayer short circuits. In the first aspect, the length of the gap is less than or equal to 35% of the length of the stacked electrode sheet in the first direction. As a result, the bending moment (whose center is the area near the end on the cutting tool side of the placement table in the protruding area) is smaller than the case where the length of the gap exceeds 35% of the length of the stacked electrode sheet in the first direction. That is, when the moving cutting tool bends the protruding area, the stress tends not to be concentrated in the area near the end on the cutting tool side of the pressing mechanism in the stacked electrode sheet. Therefore, cracks tend not to form on the surface of the area near the end on the cutting tool side of the pressing mechanism in the stacked electrode sheet. If cracks appear in the stacked electrode, there is a concern that the stacked electrode will break during charging and discharging. Due to the above, the press-breaking device of the first aspect can separate the laminated electrode sheets into desired sizes while suppressing the occurrence of interlayer short circuits and the generation of cracks.

[0012] <2> The second aspect of the present disclosure is a pressure-breaking device according to <1> A pressure breaking device, wherein: The pressing mechanism has a contact member that contacts the stacked electrode sheet when the pressing mechanism presses the stacked electrode sheet, and In the second direction, the end of the contact member on the cutting tool side is at the same position as the end of the placement table on the cutting tool side, or is closer to the cutting tool side than the end of the placement table on the cutting tool side.

[0013] In the second aspect, when the moving cutting tool bends the protruding area, stress is less likely to be concentrated in the area near the end of the pressing mechanism on the cutting tool side of the stacked electrode sheet, compared to the position of the end of the contact member on the cutting tool side in the second direction being more toward the opposite side away from the cutting tool side than the position of the end of the placement table on the cutting tool side. As a result, the press-breaking device of the second aspect can separate the stacked electrode sheets while better suppressing the generation of cracks.

[0014] <3> The third aspect of the present disclosure is a pressure-breaking device according to <1> or <2> A pressure breaking device, wherein: The angle of the blade portion relative to the first direction is 5° to 15°.

[0015] In the third aspect, the stacked electrode obtained by separating the edge material therefrom is less likely to rub against the cutting edge tool than when the back rake angle is outside the range of 5° to 15°. As a result, the pressing device of the third aspect can separate the stacked electrode sheets while better suppressing the occurrence of interlayer short circuits.

[0016] <4> The fourth aspect of the present disclosure is a pressure-breaking device according to <1> to <3> The breaking device of any one of the above, wherein The length of the gap in the second direction is 20 μm to 50 μm.

[0017] The press-breaking device of the fourth aspect can separate the specific stacked electrode sheet into a desired size while suppressing the occurrence of interlayer short circuits and the generation of cracks more than the case where the length of the gap is outside the range of 20μm to 50μm. The specific stacked electrode sheet is formed by a first active material sheet, a solid electrolyte sheet, and a second active material sheet stacked in sequence along a first direction on both surfaces of a first collector sheet. The length (thickness) of the specific stacked electrode sheet in the first direction is, for example, 0.2mm.

[0018] <5> The fifth aspect of the present disclosure is a pressure-breaking device according to <1> to <4> The pressing device of any one of the above, further comprising a lower die holder and an upper die holder, wherein the upper die holder is arranged to face the lower die holder and is configured to move relative to the lower die holder in a first direction, wherein: The first direction is parallel to the direction of gravity, The cutting edge tool and the pressing mechanism are mounted on the upper die holder, and The placing table is installed at the lower mold holding member.

[0019] In the fifth aspect, since the stacked electrode sheet is placed between the cutting edge tool and the placement table spaced apart in the first direction, and the upper mold holder descends, the stacked electrode sheet is pressed and restrained by the pressing mechanism, so that a part of the protruding area of ​​the stacked electrode sheet can be separated. As a result, the pressing device of the fifth aspect can effectively separate the stacked electrode sheet with a simple structure.

[0020] <6> The pressure breaking device according to the sixth aspect of the present disclosure is based on <5> A breaking device, wherein The cutting edge tool includes an upper cutting edge, and The placement table includes a lower blade.

[0021] The press-breaking device of the sixth aspect can effectively separate the stacked electrode sheets.

[0022] <7> The method for manufacturing a stacked electrode according to a seventh aspect of the present disclosure is to use <1> to <6> A method for manufacturing a stacked electrode using a press-breaking device according to any one of the preceding claims, the method comprising: preparing a laminated electrode sheet; placing the stacked electrode sheet on a placement table so that a protruding region is formed; and At least one cutting edge tool is moved in a first direction to bend a portion of the protruding region and to break the laminated electrode sheets.

[0023] "Stacked electrode" refers to an electrode formed by a sheet-like first active material layer, a sheet-like insulating layer, a sheet-like second active material layer, and a second collector stacked in sequence along a first direction on both surfaces of a sheet-like first collector. The first collector sheet, the first active material sheet, the insulating sheet, and the second active material sheet included in the stacked electrode sheet are disconnected and become the first collector, the first active material layer, the insulating layer, and the second active material layer included in the stacked electrode. "Insulating layer" includes a solid electrolyte layer of a lithium secondary battery using a solid electrolyte and a separator of a lithium secondary battery using a non-aqueous electrolyte.

[0024] The method for manufacturing an electrode according to the seventh aspect can manufacture a laminated electrode sheet having a desired size while better suppressing the occurrence of interlayer short circuits and the generation of cracks.

[0025] <8> The method for manufacturing a stacked electrode according to an eighth aspect of the present disclosure is based on <7> A method for manufacturing an electrode, wherein: The laminated electrode sheet is formed by a first active material sheet, a solid electrolyte sheet, and a second active material sheet sequentially laminated in a first direction on both surfaces of a first collector sheet, and The method further includes laminating a second current collector on the second active material layer obtained from the second active material sheet as a result of performing the press-breaking.

[0026] The method for producing a laminated electrode according to the eighth aspect can produce a laminated electrode having a desired size while suppressing the occurrence of interlayer short circuits and the generation of cracks.

[0027] <9> A method for manufacturing a laminated battery, the method of the ninth aspect of the present disclosure is, comprising: <7> or <8> A method for manufacturing a stacked electrode and a method for manufacturing a stacked battery.

[0028] A "laminate cell" refers to a cell comprising at least one laminated electrode.

[0029] The method of manufacturing a laminate battery of the ninth aspect can manufacture a laminate battery having a laminate electrode in which the occurrence of interlayer short circuits and the generation of cracks are suppressed and which has a desired size.

[0030] According to the present disclosure, there are provided a press-breaking device, a method for manufacturing a laminated electrode, and a method for manufacturing a laminated battery, which are capable of separating laminated electrode sheets into desired sizes while suppressing the occurrence of interlayer short circuits and the generation of cracks. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Exemplary embodiments of the present invention will be described in detail based on the following drawings, in which: Figure 1 is a cross-sectional view of a crushing device related to an embodiment of the present disclosure; Figure 2is a cross-sectional view of an upper blade and a lower blade in an embodiment of the present disclosure; Figure 3 is a cross-sectional view of a crushing device related to an embodiment of the present disclosure; Figure 4 is a cross-sectional view of an upper blade and a lower blade in an embodiment of the present disclosure; Figure 5 is a cross-sectional view of an upper blade and a lower blade in an embodiment of the present disclosure; Figure 6 is a cross-sectional view of a crushing device related to an embodiment of the present disclosure; Figure 7 is a cross-sectional view of an upper blade and a lower blade in an embodiment of the present disclosure; Figure 8 is a cross-sectional view of a stacked electrode sheet in an embodiment of the present disclosure; Fig. 9 is a top view of a stacked electrode of a comparative example; Fig.10 is a top view of a stacked electrode of a comparative example; Fig.11A It is a diagram for explaining the operation steps of a conventional cutting device; Fig. 11B is a diagram for explaining the operation steps of a conventional cutting device; and Fig. 11C It is a figure for explaining the operation procedure of a conventional cutting device. DETAILED DESCRIPTION

[0032] In the present disclosure, a numerical range expressed as "to" means that the numerical values ​​listed before and after the "to" are included as the minimum value and the maximum value, respectively. In the numerical range expressed stepwise in the present disclosure, the upper limit value or the lower limit value listed in a given numerical range can be replaced by the upper limit value or the lower limit value of another numerical range expressed stepwise. In the present disclosure, a combination of two or more preferred aspects is a more preferred aspect. In the present disclosure, the term "step" is not only an independent step, but also includes a step in which the step cannot be clearly distinguished from other steps, as long as the intended goal of the step is achieved.

[0033] The embodiments of the press-breaking device, the method for manufacturing a laminated electrode, and the method for manufacturing a laminated battery disclosed in the present invention are described below with reference to the accompanying drawings. In the accompanying drawings, the same or corresponding parts are represented by the same reference numerals and will not be described in detail.

[0034] (1) Breaking device The breaking device 1 related to the embodiment of the present disclosure bends the stacked electrode sheet 4 and breaks the stacked electrode sheet 4. Thus, a stacked electrode precursor 40 is obtained. At the stacked electrode precursor 40, a region 41 (hereinafter also referred to as "edge material 41") that does not serve as a power generation element is removed from the stacked electrode sheet 4. The details of the stacked electrode sheet 4 will be described later.

[0035] like Figure 1 As shown in , the pressing device 1 has an upper die 2 and a lower die 3. The upper die 2 is arranged to face the lower die 3. The upper die 2 can move relatively along the gravity direction relative to the lower die 3. The upper die 2 has two linear upper blades 21, which are examples of at least one cutting edge tool.

[0036] In the present embodiment, the direction of gravity is defined as the lower side, and the opposite side thereof is defined as the upper side. The side of one of the two upper blades 21 is defined as the right side, and the opposite side thereof is defined as the left side. One side of the upper blade 21 in the longitudinal direction is defined as the front side, and the opposite side thereof is defined as the rear side. The vertical direction as an example of the first direction, the left-right direction as an example of the second direction, and the front-back direction are orthogonal to each other. It should be noted that these directions do not limit the directions of the crushing device disclosed herein when in use.

[0037] (1.1) Upper mold The upper die 2 has two upper blades 21, a pressing mechanism 22, a plurality of guide pins 23, and an upper die holder 24. The two upper blades 21, the pressing mechanism 22, and the plurality of guide pins 23 are installed at the upper die holder 24. The pressing mechanism 22 is located at the central portion of the upper die holder 24 in the left-right direction. The two upper blades 21 are located adjacent to both sides of the pressing mechanism 22 in the left-right direction. The plurality of guide pins 23 are located at the outer side of the pressing mechanism 22 in the left-right direction.

[0038] (1.1.1) Upper blade like Figure 2 As shown in , the upper blade 21 is a wedge-shaped object. The upper blade 21 has a blade portion 210 extending in the front-rear direction. A rake surface S210A and a rear rake surface S210B are formed at the upper blade 21. The blade portion 210 is formed by the rake surface S210A and the rear rake surface S210B.

[0039] The angle θA of the blade portion 210 of the upper blade 21 with respect to the left-right direction (hereinafter also referred to as “front rake angle θA”) is 15° to 30°.

[0040] The angle θB (hereinafter also referred to as "back rake angle θB") of the blade portion 210 of the upper blade 21 relative to the vertical direction is an acute angle. In the press-breaking device 1, the back rake angle θB is 5° to 15°.

[0041] The length of the upper blade 21 in the front-to-back direction is appropriately selected according to the size of the laminated electrode sheet 4, etc., and it may be longer than the length in the front-to-back direction of the laminated electrode sheet 4. The material of the upper blade 21 is not particularly limited, and it is appropriately selected according to the type of the laminated electrode sheet 4, etc. Examples thereof are steel, superhard metal, etc.

[0042] (1.1.2) Pressing mechanism The pressing mechanism 22 presses the laminated electrode sheet 4 disposed on the lower blade 31 included in the lower mold 3. The pressing mechanism 22 has a contact member 221 and an elastic member 222. The upper end of the elastic member 222 is fixed to the upper mold holder 24. The lower end of the elastic member 222 is fixed to the contact member 221.

[0043] When the pressing mechanism 22 presses the stacked electrode sheet 4, the contact member 221 contacts the stacked electrode sheet 4. The contact member 221 is a flat plate-shaped object. The length L1 of the contact member 221 in the left-right direction (see Figure 1 ) is shorter than the length L2 of the stacked electrode sheet 4 in the left-right direction (see Figure 1 ), and the length L1 is appropriately selected according to the length L2 of the laminated electrode sheet 4. The material of the contact member 221 is not particularly limited, and examples thereof are resin, metal, and the like.

[0044] When the pressing mechanism 22 presses the stacked electrode sheet 4, the elastic member 222 applies a force to the contact member 221. It is sufficient that the length of the elastic member 222 in the vertical direction is such a length that, in a state where the contact member 221 does not contact the stacked electrode sheet 4, the lower portion BS221 of the contact member 221 is positioned closer to the lower side than the position of the lower portion BS21 of the upper blade 21. It is sufficient that the elastic member 222 is a member that can extend and contract in the vertical direction, and an example thereof is a coil spring, etc. The material of the elastic member 222 is not particularly limited, and an example thereof is a resin, a metal, etc.

[0045] (1.1.3) Guide pin The guide pins 23 are used to control the direction in which the upper mold 2 moves relative to the lower mold 3 to be the vertical direction. A plurality of guide pins 23 extend downward from the lower surface S24 of the upper mold holder 24, respectively. It is sufficient to have at least two guide pins 23, and the number of guide pins 23 is appropriately selected according to the size of the stacked electrode sheet 4. The material of the guide pins 23 is not particularly limited, and examples thereof are resin, metal, etc.

[0046] (1.1.4) Upper die holder The upper mold holder 24 holds the two upper blades 21, the pressing mechanism 22 and the plurality of guide pins 23. The upper mold holder 24 is a plate-shaped object. The material of the upper mold holder 24 is appropriately selected according to the size of the laminated electrode sheet 4, etc. The material of the upper mold holder 24 is not particularly limited, and examples thereof are resin, metal, etc.

[0047] (1.2) Lower die The lower die 3 has a lower blade 31 as an example of a placement table, and a lower die holder 32. The lower blade 31 is installed at the lower die holder 32. The lower blade 31 is located at a central portion of the lower die holder 32 in the left-right direction.

[0048] (1.2.1) Lower blade The stacked electrode sheet 4 is placed on the lower blade 31. The lower blade 31 is a plate-like object. The lower blade 31 has a blade portion 310 that is linear and extends in the front-to-back direction. An end face S310A and a contact surface S310B that contacts the stacked electrode sheet 4 are formed at the lower blade 31. The blade portion 310 is formed by the end face S310A and the contact surface S310B. The angle θC formed by the end face S310A and the contact surface S310B is 90°. The length of the lower blade 31 in the front-to-back direction is appropriately selected according to the size of the stacked electrode sheet 4, etc., and it is sufficient that the length is longer than the length of the stacked electrode sheet 4 in the front-to-back direction. The material of the lower blade 31 is not particularly limited, and it is appropriately selected according to the type of the stacked electrode sheet 4, etc., and examples thereof are steel, superhard metal, etc.

[0049] (1.2.2) Lower die holder The lower die holder 32 holds the lower blade 31. The lower die holder 32 is a plate-shaped object. A plurality of guide holes H32 are formed in the lower die holder 32. The guide pins 23 of the upper die 2 are inserted into the guide holes H32. The guide holes H32 are formed in the vertical direction and pass through the lower die holder 32. The positions of the plurality of guide holes H32 correspond to the positions of the plurality of guide pins 23. The material of the lower die holder 32 is not particularly limited, and examples thereof are resin, metal, etc.

[0050] (1.3) Positional relationship The length L3 of the gap between the blade portion 210 of the upper blade 21 and the end of the lower blade 31 on the upper blade 21 side (i.e., the blade portion 310) in the left-right direction (see Figure 2 ) is the length L4 of the stacked electrode sheet 4 in the left-right direction (see Figure 2 In other words, at the press-breaking device 1, the length L3 of the gap is 20 μm to 50 μm.

[0051] In the left-right direction, the position of the end 2210 of the contact member 221 on the upper blade 21 side is in the same position as the position of the end of the lower blade 31 on the upper blade 21 side (ie, the blade portion 310 ).

[0052] (1.4) Driving device The press-breaking device 1 may or may not have a known driving device (such as a hydraulic cylinder, a driving motor, etc.). If the press-breaking device 1 has a driving device, the driving device can move the upper die 2 relative to the lower die 3. If the press-breaking device 1 does not have a driving device, the upper die 2 can be moved relative to the lower die 3 manually.

[0053] (1.5) Operation refer to Figures 1 to 7 The operation of the press-breaking device 1 will be described.

[0054] First, if Figure 1 As shown in FIG. 1 , the upper die 2 and the lower die 3 are set to be separated in the vertical direction, and the laminated electrode sheet 4 is placed on the lower blade 31 of the lower die 3 . Next, when the upper die 2 moves downward, the guide pins 23 of the upper die 2 are inserted into the guide holes H32 of the lower die 3 . When the upper mold 2 moves further downward, Figure 2 and Figure 3 As shown in FIG. 1 , the contact member 221 of the pressing mechanism 22 contacts the stacked electrode sheet 4. Thus, the contact member 221 of the pressing mechanism 22 presses and constrains the stacked electrode sheet 4 due to the force of the elastic member 222. Figure 2 As shown in FIG. 1 , both end portions R4 of the laminated electrode sheet 4 in the left-right direction (hereinafter also referred to as “protruding regions R4”) protrude outward from the contact member 221 of the pressing mechanism 22 and the lower blade 31 . At this time, the upper blade 21 does not contact the laminated electrode sheet 4 . Next, when the upper mold 2 moves further downward, the blade portion 210 of the upper blade 21 comes into contact with the protruding region R4 of the laminated electrode sheet 4 restrained by the pressing mechanism 22 . Next, when the upper mold 2 moves further downward, Figure 4 As shown in FIG. 1 , due to the push of the upper blade 21, the protruding region R4 follows the movement of the upper blade 21 and is bent downward. At this time, in the state where the protruding region R4 is bent, the blade portion 210 of the upper blade 21 cuts into the upper surface TS4 of the protruding region R4. Thus, a cutting line X1 is formed in the upper surface TS4 of the protruding region R4. The cutting line X1 extends linearly in the front-to-back direction from the end of the protruding region R4 on the front side to the end of the protruding region R4 on the rear side. Next, when the upper mold 2 moves further downward, Figure 5As shown in FIG. 1 , the crack X2 starting from the cut line X1 of the protruding region R4 reaches the bottom surface BS4 of the protruding region R4 . That is, the stacked electrode sheet 4 is disconnected starting from the cut line X1 . Then, if Figure 6 As shown in FIG. 2 , when the upper mold 2 moves further downward, the edge material 41 is separated from the laminated electrode sheet 4. Thus, the laminated electrode precursor 40 is obtained. When the edge material 41 is separated from the laminated electrode sheet 4, as shown in FIG. Figure 7 As shown in the figure, the region R40 of the stacked electrode precursor 40 protruding outward from the contact member 221 and the lower blade 31 (hereinafter also referred to as the "protruding region R40") is released from the push of the upper blade 21, and the stacked electrode sheet 4 is deformed to return to the state before being pushed by the upper blade 21.

[0055] (1.6) Laminated electrode sheets like Figure 8 As shown in FIG. 1 , at the stacked electrode sheet 4, a negative electrode active material sheet 43 as an example of a first active material sheet, a solid electrolyte sheet 44, and a positive electrode active material sheet 45 as an example of a second active material sheet are sequentially stacked in the vertical direction on both surfaces of a negative electrode collector sheet 42 as an example of a first collector sheet. The stacked electrode sheet 4 does not have a negative electrode collector sheet on the positive electrode active material sheet 45.

[0056] The stacked electrode sheet 4 has a region NR4 (hereinafter also referred to as "non-power generation region NR4") at both end portions thereof in the left-right direction that does not function as a power generation element. In the non-power generation region NR4, the negative electrode active material sheet 43 and the positive electrode active material sheet 45 do not face each other in the vertical direction via the solid electrolyte sheet 44.

[0057] The length L4 of the stacked electrode sheet 4 in the vertical direction is, for example, 0.2 mm. The length of the stacked electrode sheet 4 in the front-rear direction is, for example, 70 mm.

[0058] (1.6.1) Negative electrode collector Examples of the material of the negative electrode collector sheet 42 are stainless steel, aluminum, copper, nickel, iron, titanium, carbon, etc., and preferably copper. Examples of the form of the negative electrode collector sheet 42 are the form of a foil and the form of a mesh. The negative electrode collector sheet 42 may be a structure having a shock absorbing layer, an elastic layer, or a PTC (Positive Temperature Coefficient) thermistor layer provided on its surface.

[0059] (1.6.2) Negative electrode active material sheet The negative electrode active material sheet 43 contains a negative electrode active material. Examples of the negative electrode active material are Li-based active materials such as metallic lithium, carbon-based active materials such as graphite, oxide-based active materials such as lithium titanate, and Si-based active materials such as simple Si.

[0060] The negative electrode active material sheet 43 may contain at least one of a solid electrolyte for the negative electrode, a conductive aid, and a binder as needed. Examples of the solid electrolyte and binder for the negative electrode are the same as those contained in the solid electrolyte layer contained in the solid electrolyte sheet 44 described later.

[0061] Examples of conductive aids are carbon materials, metal materials, and conductive polymer materials. Examples of carbon materials are carbon black (e.g., acetylene black, furnace black, Ketjen black, etc.), fibrous carbon (e.g., vapor-grown carbon fibers, carbon nanotubes, carbon nanofibers, etc.), graphite, fluorocarbons, etc. Examples of metal materials are metal powders (e.g., aluminum powder, etc.), conductive whiskers (e.g., zinc oxide, potassium titanate, etc.), conductive metal oxides (e.g., titanium oxide, etc.), etc. Examples of conductive polymer materials are polyaniline, polypyrrole, polythiophene, etc. One type of conductive aid can be used alone, or two or more types of conductive aids can be mixed together for use.

[0062] (1.6.3) Solid electrolyte sheet The solid electrolyte sheet 44 preferably includes one selected from the group consisting of a sulfide solid electrolyte, an oxide solid electrolyte, and a halide solid electrolyte.

[0063] The sulfide solid electrolyte preferably contains sulfur (S) as a main component which is an anion element, and further preferably contains, for example, element Li and element A. Element A is at least one type selected from the group consisting of P, As, Sb, Si, Ge, Sn, B, Al, Ga and In. The sulfide solid electrolyte may also contain at least one of O and a halogen element. Examples of halogen elements (X) are F, Cl, Br, I, etc. The composition of the sulfide solid electrolyte is not particularly limited, and examples thereof are xLi2S·(100-x)P2S5(70≤x≤80) and yLiI·zLiBr·(100-yz)(xLi2S·(1-x)P2S5)(0.7≤x≤0.8,0≤y≤30,0≤z≤30). The sulfide solid electrolyte may have a composition as shown in the following general formula (1). Formula (1): Li 4-x Ge 1-x P x S4(0 < x < 1) In formula (1), at least a part of Ge can be replaced by at least one selected from the group consisting of Sb, Si, Sn, B, Al, Ga, In, Ti, Zr, V, and Nb. Further, at least a part of P can be replaced by at least one selected from the group consisting of Sb, Si, Sn, B, Al, Ga, In, Ti, Zr, V, and Nb. A part of Li can be replaced by at least one selected from the group consisting of Na, K, Mg, Ca, and Zn. A part of S can be replaced by a halogen. The halogen is at least one of F, Cl, Br, and I.

[0064] The oxide solid electrolyte preferably contains oxygen (O) as the main component of its anion element, and for example, it may contain Li, element Q (Q represents at least one of Nb, B, Al, Si, P, Ti, Zr, Mo, W, S), and O. Examples of the oxide solid electrolyte are garnet-type solid electrolytes, perovskite-type solid electrolytes, NASICON-type solid electrolytes, Li-P-O solid electrolytes, Li-B-O solid electrolytes, etc. Examples of the garnet-type solid electrolyte are Li7La3Zr2O 12 、Li 7-x La3(Zr 2-x Nb x )O 12 (0 ≤ x ≤ 2), Li5La3Nb2O 12 etc. Examples of the perovskite-type solid electrolyte are (Li,La)TiO3, (Li,La)NbO3, (Li,Sr)(Ta,Zr)O3, etc. Examples of the NASICON-type solid electrolyte are Li(Al,Ti)(PO4)3, Li(Al,Ga)(PO4)3, etc. Examples of the Li-P-O solid electrolyte are Li3PO4 and LiPON (a compound in which some O in Li3PO4 is replaced by N). Examples of the Li-B-O solid electrolyte are Li3BO3, a compound in which some O in Li3BO3 is replaced by C.

[0065] As the halide solid electrolyte, a solid electrolyte containing Li, M, and X (M represents at least one of Ti, Al, and Y, X represents F, Cl, or Br) is suitable. Specifically, preferably Li 6-3z Y z X6 (X represents Cl or Br, and z satisfies 0 < z < 2) and Li 6-(4-x)b (Ti 1-x Al x ) b F6 (0 < x < 1, 0 < b ≤ 1.5). In Li 6-3z Y zAmong X6, from the perspective of having excellent lithium ion conductivity, Li3YX6 (where X represents Cl or Br) is more preferred, and Li3YCl6 is even more preferred. Further, from the perspective of suppressing oxidative decomposition of sulfide solid electrolytes, etc., it is preferable to contain Li 6-(4-x)b (Ti 1-x Al x ) b F6 (0 < x < 1, 0 < b ≤ 1.5) together with a solid electrolyte such as a sulfide solid electrolyte.

[0066] The solid electrolyte sheet 44 can be a single-layer structure or a multi-layer structure of two or more layers.

[0067] The solid electrolyte sheet 44 can contain an adhesive or can also not contain an adhesive. Examples of adhesives that can be included in the solid electrolyte sheet 44 are vinyl halide resins, rubbers, polyolefin resins, etc. Examples of vinyl halide resins are polyvinylidene fluoride (PVdF), copolymers of polyvinylidene fluoride and hexafluoropropylene (PVdF-HFP), etc. Examples of polyolefin resins are butadiene rubber (BR), acrylate-butadiene rubber (ABR), styrene-butadiene rubber (SBR), acrylonitrile-butadiene rubber (NBR), butyl rubber (isobutene-isoprene rubber), etc. Examples of polyolefin resins are polyethylene, polypropylene, etc. The adhesive can be a diene rubber containing a double bond in the main chain, such as a butadiene rubber in which butadiene accounts for 30 mol% or more of the total amount.

[0068] (1.6.4) Positive electrode active material sheet The positive electrode active material sheet 45 contains a positive electrode active material. Optionally, the positive electrode active material sheet 45 can contain at least one of a solid electrolyte for the positive electrode, a conductive additive, and an adhesive.

[0069] Preferably, a lithium composite oxide is included as the positive electrode active material. The lithium composite oxide can contain at least one type selected from the group consisting of F, Cl, N, S, Br, and I. In addition, the lithium composite oxide can have a crystal structure belonging to at least one space group selected from the space groups R-3m, Immm, and P63-mmc (also referred to as P63mc, P6 / mmc). In the lithium composite oxide, the main sequence of transition metal, oxygen, and lithium can be an O2-type structure.

[0070] Examples of lithium composite oxides having a crystal structure belonging to R-3m are compounds represented by the following: Li x Me y O α X β(Me represents at least one type selected from the group consisting of Mn, Co, Ni, Fe, Al, Cu, V, Nb, Mo, Ti, Cr, Zr, Zn, Na, K, Ca, Mg, Pt, Au, Ag, Ru, W, B, Si and P, and X represents at least one type selected from the group consisting of F, Cl, N, S, Br and I, and satisfies 0.5≤x≤1.5, 0.5≤y≤1.0, 1≤α<2, 0<β≤1).

[0071] An example of a lithium composite oxide having a crystal structure belonging to Immm is a composite oxide represented by: Li x1 M 1 A 1 2(satisfying 1.5≤x1≤2.3, M 1 including at least one type selected from the group consisting of Ni, Co, Mn, Cu and Fe, A 1 At least oxygen, and A 1 The proportion of oxygen contained in is greater than or equal to 85 atomic %) (a specific example is Li2NiO2), and the composite oxide represented by: Li x1 M 1A 1-x2 M 1B x2 O 2-y A 2 y (0≤x2≤0.5 and 0≤y≤0.3, at least one of x2 and y is not 0, M 1A represents at least one type selected from the group consisting of Ni, Co, Mn, Cu and Fe, M 1B represents at least one type selected from the group consisting of Al, Mg, Sc, Ti, Cr, V, Zn, Ga, Zr, Mo, Nb, Ta and W, and A 2 represents at least one type selected from the group consisting of F, Cl, Br, S and P).

[0072] An example of a lithium composite oxide having a crystal structure belonging to P63-mmc is a composite oxide represented by: M1 x M2 y O2 (M1 represents an alkali metal (preferably at least one of Na and K), M2 represents a transition metal (preferably at least one type selected from the group consisting of Mn, Ni, Co and Fe), and x+y satisfies 0 <x+y≤2)。

[0073] An example of a lithium composite oxide having an O2 type structure is a composite oxide represented by: Li x [Li α (Mn a Co bM c ) 1-α O2 (where 0.5 < x < 1.1, 0.1 < α < 0.33, 0.17 < a < 0.93, 0.03 < b < 0.50, 0.04 < c < 0.33, and M represents at least one type selected from the group consisting of Ni, Mg, Ti, Fe, Sn, Zr, Nb, Mo, W, and Bi). Specific examples are Li 0.744 [Li 0.145 Mn 0.625 Co 0.115 Ni 0.115 O2 and the like.

[0074] The solid electrolyte for the positive electrode preferably includes one selected from the group consisting of a sulfide solid electrolyte, an oxide solid electrolyte, and a halide solid electrolyte. Examples of the sulfide solid electrolyte are the same as those of the sulfide solid electrolyte included in the solid electrolyte. Examples of the oxide solid electrolyte are the same as those of the oxide solid electrolyte included in the solid electrolyte. Examples of the halide solid electrolyte are the same as those of the halide solid electrolyte included in the solid electrolyte.

[0075] Examples of the binder are the same as those of the binder included in the solid electrolyte layer.

[0076] (1.7) Operations and effects As Figures 1 to 7 shown in, the breaking device 1 has a lower blade 31, a pressing mechanism 22, and two upper blades 21. At the breaking device 1, a part of the protruding region R4 of the laminated electrode sheet 4 pressed by the pressing mechanism 22 is bent and broken by the two upper blades 21 moving in the vertical direction relative to the lower blade 31. The front inclination angle θA is 15° to 30°. The rear inclination angle θB is an acute angle. The length L3 of the gap is 10% to 35% of the length L4 of the laminated electrode sheet 4. Thus, the breaking device 1 can separate the laminated electrode sheet 4 into a desired size while suppressing the occurrence of interlayer short circuits and the generation of cracks.

[0077] The present inventor cut the laminated electrode sheet 4 by using a device similar to the breaking device 1, except that the front inclination angle θA was changed to less than 15° (specifically, 0°, 5°, 10°). Fig. 9 A top view of the cutting area of the cut laminated electrode sheet 4 is shown in. As Fig. 9As shown in , it can be seen that the shape D1 of the end of the cut-off area of ​​the stacked electrode is sawtooth-shaped. In the left-right direction, the distance L5 between the peak of the convex part and the bottom of the concave part of the shape D1 of the end of the cut-off area of ​​the stacked electrode is not less than 100μm. It is speculated that this is due to the following reasons. That is, if the forward tilt angle θA is less than 15°, it is difficult for the blade portion 210 of the upper blade 21 to cut into the protruding area R4, and it is difficult to stably form a linear cutting line X1. As a result, a disconnection starting from the cutting line X1 cannot be generated. It is speculated that the shape D1 of the end of the cut-off area of ​​the stacked electrode is therefore sawtooth-shaped. As a result, it can be seen from experiments that if the forward tilt angle θA is less than 15°, it is difficult to separate the stacked electrode sheet 4 into the desired size.

[0078] The inventors cut the stacked electrode sheet 4 by using a device similar to the pressing device 1, except that the forward tilt angle θA is changed to more than 30° (specifically, 45°, 60°). When the cut cross section of the cut stacked electrode sheet 4 is observed with the naked eye, the boundaries between the layers constituting the stacked electrode sheet 4 cannot be clearly distinguished. It is speculated that this is due to the following reasons. That is, it is speculated that the pressing of the protruding area R4 is performed by the blade portion 210 of the upper blade 21, and at this time, the blade portion 210 of the upper blade 21 and the separation surface S40 of the stacked electrode precursor 40 rub against each other. As a result, it can be seen from experiments that if the forward tilt angle θA exceeds 30°, it is difficult to separate the stacked electrode sheet 4 while suppressing the occurrence of interlayer short circuits.

[0079] The inventors cut the stacked electrode sheet 4 by using a device similar to the press-breaking device 1, except that the back tilt angle is changed to 0°. When the cut cross section of the cut stacked electrode sheet 4 is observed with the naked eye, the boundaries between the layers constituting the stacked electrode sheet 4 cannot be clearly distinguished. In addition, powder of the material produced from the stacked electrode sheet 4 is scattered on the floor near the device. It is speculated that this is because, after the edge material 41 is separated from the stacked electrode sheet 4, the blade portion 210 of the upper blade 21 rubs against the separation surface S40 of the stacked electrode precursor 40. As a result, it can be seen from the experiment that if the back tilt angle is not an acute angle, it is difficult to separate the stacked electrode sheet 4 while suppressing the occurrence of interlayer short circuits.

[0080] The inventors cut the stacked electrode sheet 4 by using a device similar to the pressing device 1, except that the length L3 of the gap is made less than 10% of the length L4 of the stacked electrode sheet 4. When the cut cross section of the cut stacked electrode sheet 4 is observed with the naked eye, the boundaries between the layers constituting the stacked electrode sheet 4 cannot be clearly distinguished. It is speculated that this is because the protruding area R4 is cut without being bent by the upper blade 21, and the separation surface S40 of the stacked electrode precursor 40 rubs against the upper blade 21 and the edge material 41. As a result, it can be seen from the experiment that if the length L3 of the gap is made less than 10% of the length L4 of the stacked electrode sheet 4, it is difficult to separate the stacked electrode sheet 4 while suppressing the occurrence of interlayer short circuits.

[0081] The present inventors cut the laminated electrode sheet 4 by using a device similar to the press-breaking device 1 , except that the length L3 of the gap is made to exceed 35% of the length L4 of the laminated electrode sheet 4 . Fig.10 FIG. 4 shows a top view of a cut region of a cut stacked electrode sheet 4. Fig.10 As shown in , a crack D2 is confirmed at a position at a distance L6 (about 70 μm) from the end of the cut area of ​​the surface of the stacked electrode sheet 4 toward the center side in the left-right direction. The crack D2 extends straightly in the front-to-back direction. It is speculated that this is because when the moving upper blade 21 bends the protruding area R4, the stress is concentrated in the stacked electrode sheet 4 at the area CR4 near the end 2210 of the pressing mechanism 22 on the upper blade 21 side. As a result, it is known through experiments that if the length L3 of the gap exceeds 35% of the length L4 of the stacked electrode sheet 4, it is difficult to separate the stacked electrode sheet 4 while suppressing the generation of cracks.

[0082] like Figures 1 to 7 As shown in FIG. 1 , at the press-breaking device 1, the pressing mechanism 22 has a contact member 221. In the left-right direction, the position of the end 2210 of the contact member 221 on the upper blade 21 side is at the same position as the end of the lower blade 31 on the upper blade 21 side (i.e., the blade portion 310). Thus, when the moving upper blade 21 bends the protruding region R4, stress is less likely to concentrate in the region CR4 near the end 2210 of the pressing mechanism 22 on the upper blade 21 side of the stacked electrode sheet 4. As a result, the pressing device 1 can separate the stacked electrode sheet 4 while better suppressing the occurrence of cracks.

[0083] like Figures 1 to 7 As shown in , at the breaking device 1, the rearward inclination angle is 5° to 15°. Thus, the laminated electrode precursor 40 obtained by separating the scrap 41 is less likely to rub against the upper blade 21. As a result, the press-breaking device 1 can separate the laminated electrode sheet 4 while better suppressing the occurrence of interlayer short circuits.

[0084] like Figures 1 to 7As shown in FIG. 1 , at the press-breaking device 1 , the length L3 of the gap is 20 μm to 50 μm. Thus, the press-breaking device 1 can separate the laminated electrode sheet 4 into desired sizes while suppressing the occurrence of interlayer short circuits and cracks. The length L4 of the laminated electrode sheet 4 in the vertical direction is, for example, 0.2 mm.

[0085] like Figures 1 to 7 As shown in , the pressing device 1 further includes a lower die holder 32 and an upper die holder 24. The upper blade 21 and the pressing mechanism 22 are mounted on the upper die holder 24. The lower blade 31 is mounted on the lower die holder 32. Thus, the press-breaking device 1 can effectively separate the stacked electrode sheets 4 with a simple structure.

[0086] like Figures 1 to 7 As shown in FIG. 1 , the breaking device 1 has an upper blade 21 and a lower blade 31 . Thus, the press-breaking device 1 can effectively separate the stacked electrode sheets 4 .

[0087] (2) Method for manufacturing laminated electrodes The method for manufacturing a stacked electrode related to the present embodiment manufactures a stacked electrode by using a press-breaking device 1. The method for manufacturing a stacked electrode related to the present embodiment includes a preparation step, a placement step, a press-breaking step, and a stacking step. The preparation step, the placement step, the press-breaking step, and the stacking step are performed in this order.

[0088] (2.1) Laminated battery The laminated battery is formed by a negative electrode active material layer, a solid electrolyte layer, a positive electrode active material layer and a positive electrode collector layer stacked in sequence in a vertical direction on both surfaces of the negative electrode collector. In other words, the laminated battery has a laminated electrode precursor 40, and two positive electrode collectors stacked on two positive electrode active material layers of the laminated electrode precursor 40. The first collector sheet, the first active material sheet, the insulating sheet and the second active material sheet included in the laminated electrode sheet are disconnected, and play the role of the first collector, the first active material layer, the insulating layer and the second active material layer. The negative electrode collector sheet 42, the negative electrode active material sheet 43, the solid electrolyte sheet 44 and the positive electrode active material sheet 45 contained in the laminated electrode sheet are disconnected, and become the negative electrode collector, the negative electrode active material layer, the solid electrolyte layer and the negative electrode active material layer included in the laminated electrode.

[0089] Examples of the positive electrode collector are stainless steel, aluminum, copper, nickel, iron, titanium, carbon, etc., and preferably aluminum alloy foil or aluminum foil. The aluminum alloy foil or aluminum foil can be made of powder. The form of the positive electrode collector is, for example, in the form of a foil or a mesh. The positive electrode collector may have a positive electrode collector tab. The positive electrode collector tab is electrically connected to the positive terminal of the laminated electrode described later. The positive electrode collector tab may extend from a region corresponding to one end of the positive active material layer of the positive electrode collector in the left-right direction toward one side in the left-right direction. The positive electrode collector may be a structure having a shock absorbing layer, an elastic layer or a PTC (Positive Temperature Coefficient) thermistor layer disposed on the surface thereof.

[0090] (2.2) Preparation steps In the preparation step, the laminated electrode sheet 4 is prepared. The method of preparing the laminated electrode sheet 4 is not particularly limited, and it suffices that the method is a known method.

[0091] (2.3) Placement steps In the placing step, the laminated electrode sheet 4 is placed on the lower blade 31 so as to form the protruding region R4 of the laminated electrode sheet 4. The method of placing the laminated electrode sheet 4 on the lower blade 31 is not particularly limited, and it suffices that the method is a known method.

[0092] (2.4) Breaking steps In the pressing step, the upper mold 2 including two upper blades 21 is moved downward to bend and break the portion of the protruding area R4 of the stacked electrode sheet 4. In the present embodiment, the portion of the protruding area R4 is bent and broken only by moving the upper mold 2 downward. Thus, a stacked electrode precursor 40 is obtained in which the edge material 41 is separated from the stacked electrode sheet 4. The method for moving the upper mold 2 is not particularly limited, and it is sufficient that the method is a known method. If the pressing device 1 has the above-mentioned driving device, the upper mold 2 can be moved by the driving device. If the pressing device 1 does not have the above-mentioned driving device, the upper mold 2 can be moved manually. The speed at which the upper mold 2 moves is not particularly limited, and it is, for example, 30 mm / second.

[0093] (2.5) Lamination steps In the lamination step, the positive electrode collector is laminated on the positive electrode active material layer obtained from the positive electrode active material sheet 45 by performing the press-breaking step (i.e., the two positive electrode active material layers of the laminated electrode precursor 40). Thus, a laminated battery is obtained. The method of laminating the positive electrode collector on the positive electrode active material layer is not particularly limited, and it is sufficient that the method is a known method.

[0094] (2.6) Operation and Effect The method for manufacturing a laminated electrode related to the present embodiment manufactures a laminated electrode by using the press-breaking device 1. The method for manufacturing a laminated electrode related to the present embodiment includes a preparation step, a placement step, and a press-breaking step. The method for manufacturing an electrode of this embodiment can manufacture a laminated electrode sheet having a desired size while suppressing the occurrence of interlayer short circuits and the generation of cracks.

[0095] In the method for manufacturing a laminated electrode related to the present embodiment, the laminated electrode sheet 4 is formed by a negative electrode active material sheet 43, a solid electrolyte sheet 44, and a positive electrode active material sheet 45 sequentially laminated in a first direction on both surfaces of a negative electrode collector sheet 42. The method for manufacturing a laminated electrode related to the present embodiment further includes a lamination step. Thus, a laminated electrode having a desired size can be manufactured while better suppressing the occurrence of interlayer short circuits and the generation of cracks.

[0096] (3) Method for manufacturing a laminated battery The method of manufacturing a laminate battery related to the present embodiment includes manufacturing a laminate electrode by the method of manufacturing a laminate electrode related to the present embodiment (hereinafter also referred to as an "electrode manufacturing step").

[0097] (3.1) Laminated electrodes The stacked electrode has at least one stacked electrode, a positive terminal, a negative terminal and an outer casing. The positive terminal is electrically connected to a positive electrode collector included in the stacked electrode. The negative terminal is electrically connected to a negative electrode collector included in the stacked electrode. The outer casing accommodates the at least one stacked electrode, the positive terminal and the negative terminal so that the positive terminal and the negative terminal are electrically connected to the outside.

[0098] The number of stacked electrodes is appropriately selected depending on the intended use of the stacked electrodes, etc. In the case of a plurality of stacked electrodes, the plurality of stacked electrodes may be stacked in a vertical direction, for example.

[0099] The shape and size of the positive and negative terminals are appropriately selected according to the intended use of the laminated electrode, etc. Examples of the material of the positive and negative terminals are metals (eg, stainless steel (SUS) etc.) and the like.

[0100] The outer package is not particularly limited, and examples thereof include a laminated outer package, a metal can (eg, square, cylindrical, etc.), etc. The shape and size of the outer package are appropriately selected depending on the intended use of the laminated electrode, etc.

[0101] (3.2) Electrode manufacturing steps The method for manufacturing a stacked battery related to the present embodiment includes an electrode manufacturing step.

[0102] In the electrode manufacturing step, a laminated electrode is manufactured by the method of manufacturing a laminated electrode related to the present embodiment.

[0103] (3.3) Other steps The method for manufacturing a laminated battery associated with the present embodiment may include other steps. These other steps include general steps for manufacturing a battery. Examples of these other steps are: a step of stacking a plurality of laminated electrodes to prepare an electrode laminate, a step of accommodating the electrode laminate in an outer body (e.g., a laminate film, a can, etc.), a step of electrically connecting a plurality of negative electrode collectors contained in the electrode laminate to at least one negative terminal, a step of electrically connecting a plurality of positive electrode collectors contained in the electrode laminate to at least one positive terminal, etc.

[0104] (3.4) Operation and Effect The method for manufacturing a stacked battery related to the present embodiment includes an electrode manufacturing step. Thus, the method of manufacturing a laminate battery related to the present embodiment can manufacture a laminate battery having laminate electrodes in which the occurrence of interlayer short circuits and the generation of cracks are suppressed and which have a desired size.

[0105] (4) Deformation example In this embodiment, the position of the end 2210 of the contact member 221 on the upper blade 21 side is at the same position as the position of the end of the lower blade 31 on the upper blade 21 side (i.e., the blade portion 310), but may be a position closer to the upper blade 21 side than the position of the end of the lower blade 31 on the upper blade 21 side (i.e., the blade portion 310).

[0106] In the present embodiment, the rearward inclination angle θB is 5° to 15°, but the rearward inclination angle θB may not be 5° to 15° as long as it is an acute angle.

[0107] In the present embodiment, the length L3 of the gap is 20 μm to 50 μm. However, if the length L3 is 10% to 35% of the length L4 of the laminated electrode sheet 4 in the left-right direction, the length L3 may be outside the range of 20 μm to 50 μm.

[0108] In the present embodiment, the press-breaking device 1 includes the upper die holder 24 and the lower die holder 32 , but does not necessarily need to include at least one of the upper die holder 24 and the lower die holder 32 .

[0109] In the present embodiment, the press-breaking device 1 has the lower blade 31. However, if the press-breaking device 1 has a placement table on which the laminated electrode sheet 4 is placed, the press-breaking device 1 does not necessarily have the lower blade 31.

[0110] The method of manufacturing a laminated electrode of the present embodiment includes a laminate step, but does not necessarily need to include the laminate step.

[0111] In the present embodiment, the stacked electrode sheet 4 is formed by a negative electrode active material sheet 43, a solid electrolyte sheet 44, and a positive electrode active material sheet 45 stacked in sequence in a vertical direction on both surfaces of the negative electrode collector sheet 42. However, the present disclosure is not limited thereto. The stacked electrode sheet may be formed by a positive electrode active material sheet 45, a solid electrolyte sheet 44, and a negative electrode active material sheet 43 stacked in sequence in a vertical direction on both surfaces of the positive electrode collector sheet. In the present disclosure, a separator of a lithium secondary battery using a non-aqueous electrolyte may be used instead of the solid electrolyte sheet 44.

[0112] In this embodiment, the laminated battery cell is a battery cell in a lithium secondary battery using a solid electrolyte, but may also be a battery cell used in a secondary battery (such as a nickel-hydrogen battery).

[0113] In the present embodiment, the angle θC formed by the end surface S310A of the lower blade 31 and the contact surface S310B is 90°, but may be smaller than 90°.

Claims

1. Breaking device, including: a placing table on which the stacked electrode sheets are placed; A pressing mechanism for pressing the stacked electrode sheet placed on the placement table; as well as at least one cutting edge tool, The pressing device is configured so that, by the at least one cutting edge tool moving in a first direction relative to the placing table, the pressing device bends and breaks a portion of the protruding area of ​​the stacked electrode sheet pressed by the pressing mechanism in a second direction orthogonal to the first direction, which protrudes outward from the placing table and the pressing mechanism, wherein: The angle of the blade portion of the cutting tool relative to the second direction is 15° to 30°, The angle of the blade portion relative to the first direction is an acute angle, and The length of the gap between the blade portion and the end of the placement table on the cutting blade tool side in the second direction is 10% to 35% of the length of the laminated electrode sheet in the first direction.

2. The crushing device according to claim 1, wherein: The pressing mechanism has a contact member that contacts the stacked electrode sheet when the pressing mechanism presses the stacked electrode sheet, and In the second direction, the position of the end of the contact member on the cutting tool side is at the same position as the position of the end of the placement table on the cutting tool side, or is at a position closer to the cutting tool side than the position of the end of the placement table on the cutting tool side.

3. The crushing device according to claim 1, wherein: The angle of the blade portion relative to the first direction is 5° to 15°.

4. The crushing device according to claim 1, wherein: The length of the gap in the second direction is 20 μm to 50 μm.

5. The crushing device according to claim 1, further comprising a lower die holder and an upper die holder, wherein the upper die holder is arranged to face the lower die holder and is configured to move relative to the lower die holder along the first direction, wherein: The first direction is parallel to the direction of gravity, The blade and the pressing mechanism are mounted on the upper die holder, and The placement table is installed at the lower mold holding member.

6. The crushing device according to claim 5, wherein: The cutting edge tool comprises an upper cutting edge, and The placement table includes a lower blade.

7. A method for manufacturing a laminated electrode by using the press-breaking device according to any one of claims 1 to 6, the method comprising: preparing the stacked electrode sheet; placing the stacked electrode sheet on the placement table so as to form the protruding area; as well as The at least one cutting edge tool is moved in the first direction to bend a portion of the protruding region and to break the laminated electrode sheet.

8. The method for manufacturing a laminated electrode according to claim 7, wherein: The stacked electrode sheet is formed by a first active material sheet, a solid electrolyte sheet, and a second active material sheet stacked in sequence along the first direction on both surfaces of the first collector sheet, and The method further includes laminating a second current collector on a second active material layer obtained from the second active material sheet as a result of performing the press-breaking.

9. A method for manufacturing a stacked battery, the method comprising: A laminated electrode is manufactured by the method for manufacturing a laminated electrode according to claim 7.

Citation Information

Patent Citations

  • Breaking device for electrode

    JP2015153538A

  • Manufacture of non-aqueous secondary battery

    JP2000315525A

  • Method for processing fiber-reinforced composite material

    JP2013099817A

  • Die assembly and method of manufacturiing die assembly

    US20010023607A1

  • Apparatus and method for cutting sheet materials

    US20030131699A1