Safety film for prevention calibration and method for verifying prevention

By adopting hierarchical structures with different Young's modulus in the security film and embedding physical tag agents that are not identifiable with the human eye, combined with external stimulation and structural color display, the limitations of counterfeit confirmation and reuse problems in the existing technology are solved, achieving It achieves efficient counterfeiting verification and anti-counterfeiting effects.

CN118865801APending Publication Date: 2024-10-29NBST CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310641678.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-04-27
Filing Date
2023-06-01
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

Existing anti-counterfeiting and alteration technology has limitations in confirming whether it is counterfeit or not. It is especially difficult to apply on small-sized devices. Moreover, a single verification method cannot cope with the evolving counterfeiting and alteration technology, and cannot prevent the reuse of security films.

Method used

A security film made of flexible material, including a base material layer with high wrinkle areas and low wrinkle areas, a pattern layer and an upper layer with different Young's modulus, and a physical tag agent that is invisible to the eye embedded in the pattern layer, which can be passed through the outside Stimulus applied buckling is verified and images are visualized using structural color, while spurious alterations are confirmed by camera or microscopy identification of the taggant.

Benefits of technology

The buckling verification method is used to confirm whether it has been counterfeited or not, and the embedded physical tagging agent is identified to prevent the reuse of the security film, which improves the safety and effectiveness of anti-counterfeiting.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118865801A_ABST
    Figure CN118865801A_ABST
Patent Text Reader

Abstract

The present invention relates to a security film for preventing counterfeiting and alteration, and a method for verifying counterfeiting and alteration using the same, and more specifically, to prevent repeated use of the security film and to verify counterfeiting and alteration of a laminated security film by including a physical tagging agent which is not recognizable by eyes in a pattern layer when the adhesive surface and the base material layer of the film are to be detached. The invention relates to a security film and a pseudo-alteration verification method using the same, wherein whether the security film is counterfeited and altered or not is confirmed in a buckling mode through mechanical stimulation. The security film according to one embodiment of the present invention comprises: a substrate layer formed of a flexible material and including a high-fold region and a low-fold region; patterns are formed on the high-wrinkle area of the base material layer, and the Young modulus of the pattern layer is larger than that of the base material layer; and an upper layer which covers the low-wrinkle region of the base layer and the pattern layer, and which has a Young's modulus greater than that of the base layer and smaller than that of the pattern layer. The pattern layer is formed by embedding a physical tagging agent which cannot be recognized by naked eyes into the pattern layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a security film for preventing counterfeiting and alteration and a method for verifying counterfeiting and alteration using the same. More specifically, the present invention relates to a security film for preventing counterfeiting and alteration of a laminated security film. When the adhesive surface and the substrate layer of the film are to be separated, the security film is prevented from being reused because the pattern layer contains a physical labeling agent that cannot be identified by the naked eye. At the same time, the security film is confirmed to be counterfeit and altered in a bending manner through mechanical stimulation, and a method for verifying counterfeiting and alteration using the same. Background Art

[0002] In modern society, with the development of technology, various new products have been developed, and the developed products are traded very actively on the Internet. Unfortunately, copying technology has also made great progress, making it increasingly difficult to distinguish between genuine products and copies. For high-priced products, various anti-counterfeiting technologies can be used, but for slightly lower-priced products that are inevitably circulated in large quantities, it is still difficult to use such technologies. For example, food, medical drugs, cosmetics and other items are directly related to people's health and even life, so they need more attention from society.

[0003] For the anti-counterfeiting alteration system based on photonic crystal patterns, which is commonly used in anti-counterfeiting alteration technology, it is always visible when light is present and is not suitable for hiding information. Therefore, as an anti-counterfeiting alteration system, it has some limitations in application.

[0004] Therefore, a large number of new anti-counterfeiting devices that are fast-responsive to external stimuli (stretching, compression, bending, torsion, etc.) are being developed using reflective methods that can display structural colors.

[0005] For the anti-counterfeiting device that is responsive to external stimuli, a layer formed by a thin film stack with a predetermined rigidity on a flexible material is built into the device, and a load is applied by external stimulus verification methods such as stretching, compression, torsion, and bending to display structural colors and thus display images.

[0006] Here, the buckling verification method for confirming whether there is a false alteration by applying external stimulation to the above-mentioned device with a built-in layer formed by a thin film stack is to display an image of a certain size through structural color. The device itself needs to be formed with a thickness and area larger than that capable of displaying the corresponding image, so its application to very small devices will be limited.

[0007] Moreover, with the development of this verification method that can show structural colors, counterfeiting technology has also gradually evolved accordingly. Using only one anti-counterfeiting method may not be able to cope with the evolved counterfeiting technology. Therefore, in addition to the bending verification method, a small-size verification method is also required to improve security through multiple verification methods. Summary of the invention

[0008] Technical issues

[0009] The object of the present invention is to provide a security mold that can be used for anti-counterfeiting and alteration, and adopts an anti-counterfeiting and alteration means that can be verified by bending when an external stimulus is applied to layers with different Young's modulus. At the same time, when the pattern layer and the substrate layer forming the security film are separated, the pattern layer contains a physical labeling agent that is not recognizable by the naked eye, which prevents the security film from being reused, and an anti-counterfeiting and alteration device using the same.

[0010] Technical Solution

[0011] The safety film according to an embodiment of the present invention preferably comprises: a substrate layer formed of a flexible material and including a high wrinkle region and a low wrinkle region; a pattern layer having a pattern formed on the high wrinkle region of the substrate layer and a Young's modulus greater than that of the substrate layer; and an upper layer covering the low wrinkle region of the substrate layer and the pattern layer and having a Young's modulus greater than that of the substrate layer but less than that of the pattern layer. The pattern layer is formed by embedding a physical tag agent that is not recognizable by the naked eye.

[0012] According to an exemplary embodiment, the physical taggant is formed as microparticles of 1 to 300 μm.

[0013] According to an exemplary embodiment, the microparticles are formed at 1 weight percent or less relative to the pattern layer.

[0014] According to an exemplary embodiment, the microparticles are plastic particles containing a polymer substance and an organic dye and are formed with a specific image or specific text.

[0015] According to an exemplary embodiment, the polymer substance is formed of a thermoplastic resin composed of one or more selected from polyester, fluoropolymer, acrylate-methylmethacrylate copolymer or polymethylstyrene, or a thermosetting resin composed of one or more selected from polymethyl methacylate (PMMA), polybutylacrylate (PBA) or isocyanate resin.

[0016] According to an exemplary embodiment, the organic dye is formed of a color pigment or a fluorescent dye.

[0017] According to an exemplary embodiment, the substrate layer may be formed of one of EPU, polyurethane, copolyester (Ecoflex) and rubber series polymer substances.

[0018] According to an exemplary embodiment, the plastic particles formed with a specific image or specific text are formed at multiple positions within the pattern layer according to a certain rule, and the specific images formed according to the certain rule are combined to form another different image, or the specific texts are combined to form another different article.

[0019] According to an exemplary embodiment, the substrate layer, the pattern layer and the upper layer are wrinkled by one load selected from bending load, compression load, tensile load, shear load or torsional load, or a composite load of two or more, and a grating structure is generated by the wrinkles, thereby forming different structural colors and images through the structural colors.

[0020] According to an embodiment of the present invention, a method for verifying counterfeit tampering using a security film preferably includes: a step of confirming counterfeit tampering by means of structural color revealed due to external stimulation applied to the substrate layer, pattern layer and upper layer having different Young's moduli; and a step of confirming counterfeit tampering by identifying a physical tagging agent embedded in the pattern layer by means of a camera or a microscope.

[0021] Beneficial Effects

[0022] The beneficial effects of the present invention are:

[0023] As external stimuli are applied to the laminated layers with different Young's moduli, the forgery can be confirmed by buckling verification, and at the same time, the forgery can be confirmed by magnifying and identifying the corresponding information on the pattern layer where the physical tag agent containing microparticles that cannot be identified by the naked eye is embedded using a camera or a microscope, thereby improving the anti-counterfeiting effect;

[0024] Furthermore, in a film structure formed by multiple stacked layers, when the pattern layer and the upper layer adhered to the substrate layer are separated for the purpose of counterfeiting, the physical labeling agent is also separated and cannot be identified using a camera or a microscope. This can determine whether it is counterfeit or not, thereby preventing the repeated use of the film. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 A cross-sectional view showing a safety mold according to an embodiment of the present invention;

[0026] Figure 2 A diagram showing a state in which an image formed by structural color is confirmed by a buckling verification method in a safety mold according to an embodiment of the present invention;

[0027] Figure 3This is a diagram showing the state of microparticles displayed in a pattern when an image displayed by structural color is magnified with a normal camera in a safety film according to an embodiment of the present invention;

[0028] Figure 4 The diagram shows a state in which a plurality of images or texts in a pattern layer are combined to form another image or text in a security film according to an embodiment of the present invention.

[0029] Explanation of symbols:

[0030] 10: substrate layer;

[0031] 20: pattern layer;

[0032] 30: Upper layer. DETAILED DESCRIPTION

[0033] The following will describe in detail a specific embodiment of the present invention in conjunction with the drawings in the embodiments of the present invention, but the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, ordinary technicians in this field can still modify the technical solutions described in the aforementioned embodiments, or replace some of the technical features therein with equivalents; and these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

[0034] The embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0035] Figure 1 A cross-sectional view showing a safety membrane according to an embodiment of the present invention.

[0036] Figure 2 A diagram showing a state in which an image formed by structural color is confirmed by a buckling verification method in a safety mold according to an embodiment of the present invention;

[0037] Figure 3 This is a diagram showing the state of microparticles displayed in a pattern when an image displayed by structural color is magnified with a normal camera in a safety film according to an embodiment of the present invention;

[0038] The safety film disclosed in the present invention may have a structure formed by multiple stacked layers. It includes: a substrate layer 10 formed of a flexible material and including a high wrinkle area and a low wrinkle area; a pattern layer 20 having a pattern formed in the high wrinkle area of ​​the substrate layer 10 and having a Young's modulus greater than that of the substrate layer 10; and an upper layer 30 covering the low wrinkle area of ​​the substrate layer 10 and the pattern layer 20, and having a Young's modulus greater than that of the substrate layer 10 but less than that of the pattern layer 20. The interior of the pattern layer 20 may be embedded with a physical tag agent (T) that is not recognizable by the naked eye.

[0039] The base layer 10 is a base in a multi-layer structure that can be formed by stacking. The base layer 10 can be formed of a polymer material having a predetermined elasticity, and can be manufactured by the following method.

[0040] First, prepare a substrate made of polyethylene terephthalate (PET). Then, cure epoxy resin (EPU) on the substrate to form a substrate layer 10. In addition, it can also be formed of polypropylene or natural materials with outstanding flexibility, and preferably, it is formed of a flexible material containing a plasticizer to further improve flexibility. Specifically, the substrate layer 10 is preferably formed of one of EPU, polyurethane, polyurea, melamine resin, polydimethylsiloxane (PDMS), copolyester (Ecoflex) and rubber series polymer substances.

[0041] Here, the external stimulus that may be applied to the safety film may be one of the following loads, including a compression load, a tension load, a pressing load or a torsional load, or a composite load of two or more, and the compression deformation formed on the safety film may be a deformation caused by such a compression load, a tension load, a pressing load, a bending load or a torsional load.

[0042] In addition, the steps of forming the base material layer 10 include: removing bubbles after mixing the main material of the EPU and the curing agent in a ratio of 10:1; removing bubbles after mixing vinyl and platinum to improve the adhesion with the pattern layer 20 to be formed on the upper part to solve the problem of low adhesion of a single EPU due to the low surface energy of the EPU; pouring it on the above-mentioned substrate to solidify it. In addition, in order to strengthen the interface bonding with the pattern layer 20 formed on the upper part, preferably, it also includes a process of plasma treatment of the solidified base material layer 10, and the Young's modulus of the base material layer 10 formed in this way is preferably in the range of 10 to 20Mpa.

[0043] Then, a high-hardness material is printed on the high wrinkle area (FHW) on the substrate layer 10 to form a pattern layer 20. Here, the high-hardness material is a material with a hardness much higher than that of the base material, and therefore, preferably, a material with a large Young's modulus, such as a Young's modulus in the range of 60 GPa to 80 GPa, is used. A representative material that can be used as the high-hardness material is cellulose.

[0044] Here, the formation process of the pattern layer 20 is described. Specifically, the steps of forming the pattern layer 20 include: a step of mixing cellulose (Cellulose) powder and acetic acid (Acetic acid) in purified water (DIwater) to manufacture a high-hardness material; a step of plasma-treating the EPU before printing a hydrophilic cellulose solution on the hydrophobic surface, i.e., the upper surface of the EPU, to increase the contact area of ​​the cellulose droplets and improve the adhesion between the EPU and the cellulose; and a step of using an inkjet printer to print the high-hardness material according to the binary pattern generated on the substrate layer 10.

[0045] Then, an acrylic solution and a reinforcing material having at least one of yield strength, tensile strength, impact strength and shear strength greater than acrylic are mixed, so that a medium-hard material having a lower Young's modulus than the high-hard material but a roughly similar refractive index is impregnated onto the entire surface of the substrate layer 10, and then the upper layer 30 is formed entirely from the high wrinkle region (FHW) to the low wrinkle region (FLW) adjacent to the high wrinkle region (FHW). A representative material that can be used as the reinforcing material is cellulose. Furthermore, the reinforcing material can be the same as the high-hard material, and the use of the same material as the high-hard material can improve the adhesion between the pattern layer 20 and the upper layer 30.

[0046] The formation process of the upper layer 30 is described in detail as follows: after mixing a flexible material (low hardness material), namely acrylic acid, in purified water, the mixture is dissolved in hot water to form an acrylic acid aqueous solution. The prepared acrylic acid aqueous solution is then mixed with a reinforcing material (cellulose) to form a medium-hard material having a lower Young's modulus than the high-hardness material but a roughly similar refractive index; before impregnating the generated medium-hard material into the substrate layer 10 for forming the pattern layer 20, the substrate layer 20 is subjected to plasma treatment to improve the interfacial bonding force between the upper layer 30 and the pattern layer 20 and the substrate layer 10; and the generated medium-hard material is impregnated into the low-wrinkle region (FLW) from the high-wrinkle region (FHW) to the adjacent high-wrinkle region (FHW), or into the entire surface of the substrate layer 10. Here, the process of impregnating the medium-hard material can be performed by spin coating, scraping, spraying, or dipping.

[0047] As described above, a high-hardness material is printed on the high-wrinkle area (FHW) of the base material layer 10 generated on the substrate to form the pattern layer 20, and the medium-wrinkle material is completely impregnated from the high-wrinkle area (FHW) to the adjacent low-wrinkle area (FLW) to form the upper layer 30, and then the upper layer 30 is cured together with the pattern layer 20 to form a safety film.

[0048] As shown in the above-mentioned manufacturing method, when a safety film mixed with acrylic acid and a reinforcing material having at least one of yield strength, tensile strength, impact strength and shear strength greater than that of acrylic acid is used as a medium-hard material, it is advantageous in that durability can be improved.

[0049] When only acrylic is used as a hard material, if it is subjected to external stimulation caused by bending, plastic deformation occurs and cracks are easily generated in the upper layer 30. The cracks formed in this way will make the surface of the security film blurred, resulting in weakened durability and anti-counterfeiting function.

[0050] In contrast, when a safety film that is a mixture of acrylic acid and a reinforcing material having at least one of yield strength, tensile strength, impact strength and shear strength greater than that of acrylic acid is used as a medium-hard material, its advantage is that corresponding destructive stress and deformation rate can be generated in response to deformation under external stimulation, and at the same time, the transmittance between the two is similar, so the transmittance of light can also be maintained.

[0051] A safety membrane according to an embodiment of the present invention manufactured by the above-mentioned manufacturing method will be described below.

[0052] As described above, the present invention relates to a safety film in which the surface wrinkle structure of a structure formed by deformation under load is used as a grating structure for displaying structural color, and a grating structure is generated by arranging a plurality of wrinkles having different wavelengths due to the difference in Young's modulus, thereby making the plurality of grating structures form different structural colors and an image is formed by the structural color. The safety film may include a substrate layer 10 having the physical properties as described above, a pattern layer 20 and an upper layer 30, wherein the pattern layer 20 may be formed of a hard polymer material and may be embedded with a physical tag agent (T) that is not recognizable to the naked eye.

[0053] Here, the physical tag agent can be defined as a physical additive for anti-counterfeiting containing identification information, which can be formed in a tiny size that cannot be recognized by the naked eye. The form can also be diverse, and information such as a specific number or company name can be provided in a tiny size, and then it can be confirmed by a camera or a microscope to identify whether it is a counterfeit or not.

[0054] Here, the physical taggant (T) may be formed of microparticles of 1 to 300 μm.

[0055] The physical taggant is formed in a size that is not identifiable by naked eyes. As an embodiment, the taggant is formed in microparticles of 1 to 300 μm. Therefore, the taggant can only be identified by magnification with a camera or a microscope.

[0056] The table below shows the eye thresholds by focal length. At a focal distance of 10 cm, the smallest size that a person with 1.0 vision can see is about 29.1 μm, and at the threshold, the smallest size that a person can see is about 11.6 μm. Similarly, at a focal distance of 30 cm (smartphone), the smallest size that a person with 1.0 vision can see is about 87.3 μm, and at the threshold, the smallest size that a person can see is about 34.9 μm.

[0057] ■Eye threshold at different focal lengths

[0058]

[0059] Therefore, the size of the microparticles forming the physical tag agent embedded in the pattern layer 20 is 1 to 300 μm, preferably, 5 to 100 μm, so that ordinary people cannot recognize the microparticles with the naked eye. Even if some people with good eyesight can recognize the existence of the tag agent itself, it is impossible to recognize the image or text formed by the microparticles. Therefore, the microparticles can only be recognized by a camera or a microscope.

[0060] Furthermore, the microparticles may be formed at a weight percentage of less than 1% relative to the pattern layer 20. In order to limit the microparticles from being identifiable with the naked eye, in addition to the above-mentioned physical size, it is also possible to limit the microparticles to only a certain weight percentage relative to the total weight of the pattern layer 20, so that it is difficult to confirm whether the microparticles themselves are contained. As an embodiment, the microparticles are less than 1% by weight compared to the total weight of the pattern layer 20, so that it can only be known whether the microparticles are contained through a high-magnification camera or a microscope, thereby further improving safety.

[0061] In an exemplary embodiment, the microparticles are plastic particles containing a polymer substance and an organic dye and may be formed with a specific image or specific text.

[0062] The microparticles may be formed of plastic particles containing a polymer and an organic dye. The polymer constituting the microparticles may be formed in the same manner as the hard polymer constituting the pattern layer 20. In an exemplary embodiment, the polymer may be formed of a thermoplastic resin consisting of one or more selected from polyester, fluoropolymer, acrylate-methylmethacrylate copolymer, or polymethylstyrene, or a thermosetting resin consisting of one or more selected from polymethyl methacylate (PMMA), polybutylacrylate (PBA), or isocyanate resin.

[0063] The organic dye may be composed of a color pigment or a fluorescent dye. Here, the organic dye may be composed so that the color of the particles can be identified by the color pigment, or the presence of microparticles can be identified by the fluorescent dye through photoluminescence.

[0064] In this way, by limiting the size and even the content or substance and color of the microparticles forming the physical tag agent to form microparticles of various forms, safety can be improved.

[0065] Figure 4 The diagram illustrates a state in which a plurality of images or texts are combined in a pattern layer to form another different image or text in a security module according to an embodiment of the present invention.

[0066] According to an exemplary embodiment, the plastic particles consisting of the specific image or the specific text are formed according to a certain rule at multiple positions in the pattern layer 20, and the specific image formed according to the certain rule can be recombined to form another different image, or the specific text can be combined to form another different article.

[0067] The microparticles forming the physical tag agent or the plastic particles formed by the specific images or specific texts constituting the microparticles can be embedded in the pattern layer 20, and more specifically, can be embedded in a certain pattern layer 20 at multiple positions. As an embodiment, the multiple specific images constituting the plastic particles are formed by multiple pieces of images, and the images of the pieces can be combined to associate with another different image. Therefore, it is not only a method of confirming and identifying a single plastic particle by a camera or a microscope, but also by simultaneously confirming the overall plastic particle composed of multiple images, another different image formed by the combination of multiple specific images can be identified, thereby confirming whether it is a forgery or not.

[0068] Another embodiment is that the arrangement of the multiple specific texts constituting the plastic particles can have certain rules, which can be identified by whether a single text exists, but whether it is a forgery can also be confirmed by whether the multiple specific texts form another different article when combined.

[0069] For an exemplary embodiment, the substrate layer 10, the pattern layer 20 and the upper layer 30 are wrinkled by a load selected from a bending load, a compression load, a tensile load, a shear load or a torsional load, or a composite load of two or more, and a grating structure formed by the wrinkles is generated, thereby forming different structural colors and images through the structural colors.

[0070] The image formed by the structural color that appears by setting different types or directions of loads applied to the safety film can be formed differently to improve the safety effect, but in order to form a grating structure, external stimuli such as bending loads, compression loads, tensile loads, shear loads or torsional loads are applied to produce wrinkles, and then the image is formed by structural colors.

[0071] Here, the loads applied to the substrate layer 10, the pattern layer 20 and the upper layer 30 are composed of different types of loads selected from bending load, compressive load, tensile load, shearing load or twisting load, thereby forming different images.

[0072] From the perspective of the wrinkle formation principle of the grating structure, when external stimulation is applied to the flexible substrate layer 10, and then a bending load is applied in the direction of the upper layer 30 and the pattern layer 20, due to the mechanical and physical incompatibility between the thin and rigid upper layer 30 and the pattern layer 20 and the thicker and more flexible substrate layer 10 than the upper layer 30 and the pattern layer 20, the buckling-like instability in the upper layer 30 and the pattern layer 20 forms a wrinkle arrangement pattern with a periodic width.

[0073] Here, the periodicity λ of the wrinkle arrangement is determined as follows based on the thickness (h) and elastic modulus (Ef) of the upper layer 30 and the pattern layer 20 and the elastic modulus (Es) of the base layer 10 that can be predicted by the linear buckling theory.

[0074]

[0075] Here, is the plane deformation modulus, defined as E / (1-v 2 ). v is Poisson's ratio. This mathematical formula 1 expresses a model of surface periodic phenomena, which can predict the periodicity of the safety film. Specifically, the safety film formed by the lamination of the upper layer 30, the pattern layer 20 and the substrate layer 10 of the present invention is that the Young's modulus of the upper layer 30 and the pattern layer 20 is much higher than that of the substrate layer 10, so the upper layer 30 and the pattern layer 20 can be regarded as a rigid film layer, and the size (amplitude) of each wavelength of the wrinkles depends on the relative difference in Young's modulus (E) of the upper layer 30 and the pattern layer 20 and the substrate layer 10 and the relative difference in thickness (h).

[0076] Here, the Young's modulus (E) and thickness (h) of the base layer 10, the pattern layer 20, and the upper layer 30 are relatively different, so the wrinkle arrangement patterns are formed differently. Due to the difference, the wrinkle structure (micro unit) formed on the high wrinkle area of ​​the pattern layer 20 and the wrinkle structure (nano unit) formed on the low wrinkle area of ​​the upper layer 30 become different, so the chromaticity of the structural color and the image displayed become different.

[0077] According to an embodiment of the present invention, a method for verifying counterfeit tampering using a security mold may include: a step of confirming counterfeit tampering by using a structural color that appears due to external stimulation applied to the substrate layer 10, the pattern layer 20, and the upper layer 30 having different Young's moduli; and a step of confirming counterfeit tampering by identifying a physical tag agent embedded in the pattern layer 20 by using a camera or a microscope.

[0078] More specifically, the forgery verification method using the security mold disclosed in the present invention can simultaneously perform the bending verification method and the identification tag agent verification method to confirm whether it is forged or not. For example, by using the difference in Young's modulus of the substrate layer 10, the pattern layer 20 and the upper layer 30, for the image formed by the structural color that appears with the application of external stimulation, the forgery is confirmed by bending. For the physical tag agent formed by microparticles embedded in the pattern layer 20, it cannot be identified by the naked eye, but can be confirmed by a camera or a microscope, wherein the microparticles are different in size, content, material and color, so they can be identified in a variety of ways, and the forgery can be confirmed by identifying a specific image or a specific text by microparticles formed at multiple positions, thereby improving the anti-counterfeiting effect.

[0079] As described above, by embedding a physical taggant that cannot be recognized by the naked eye into the pattern layer, more precisely, by embedding a physical taggant into the pattern layer that shows structural color under external stimulation, the safety film formed can prevent the reuse of the film. Specifically, when separating the laminated layer from a thin film formed by multiple laminated layers for the purpose of pseudo-alteration, unlike ordinary thin films, the safety film disclosed in the present invention is embedded with a physical taggant that cannot be recognized by the naked eye, so the presence of the physical taggant can be confirmed by a camera or a microscope. For example, if it is a non-pseudo-altered film, the physical taggant still exists, so it can be identified by the same or a microscope, but if it has been pseudo-altered or another layer adhered to the film substrate layer is separated or a part of the adhesive surface is separated by attempting pseudo-alteration, the physical taggant formed by embedding in the pattern layer itself is separated and cannot be identified, so it can be confirmed whether it is pseudo-altered or not, thereby preventing the reuse of the film.

[0080] Even if there are effects not described in this specification, the invention can provide different effects through the above-mentioned structures. Through the organic combination relationship between the above-mentioned structures, new effects that are difficult to see in the prior art can be obtained.

[0081] In addition, the multiple embodiments illustrated in the figures can be modified and implemented in different forms, and these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions described in the embodiments of the present invention.

Claims

1. A safety film , It is characterized in that The invention comprises: a substrate layer formed of a flexible material and comprising a high-wrinkle area and a low-wrinkle area; A pattern is formed on the high wrinkle area of ​​the substrate layer, and the Young's modulus is greater than that of the pattern layer of the substrate layer; An upper layer covering the low wrinkle area of ​​the substrate layer and the pattern layer and having a Young's modulus greater than that of the substrate layer but less than that of the pattern layer; The pattern layer is formed by embedding a physical tag agent which is not discernible to the naked eye.

2. The safety film according to claim 1, It is characterized in that The physical taggant is formed in the form of microparticles of 1 to 300 μm.

3. The safety film according to claim 2, It is characterized in that The microparticles are formed at 1 weight percent or less relative to the pattern layer.

4. The safety film according to claim 2, It is characterized in that The microparticles are plastic particles containing a polymer substance or an organic dye and are formed in a specific image or specific text.

5. The safety film according to claim 4, It is characterized in that The polymer substance is formed of a thermoplastic resin composed of one or more selected from polyester, fluoropolymer, acrylate-methylmethacrylate copolymer or polymethylstyrene, or a thermosetting resin composed of one or more selected from polymethyl methacylate (PMMA), polybutylacrylate (PBA) or isocyanate resin.

6. The safety film according to claim 4, It is characterized in that The organic dye is formed of a color pigment or a fluorescent dye.

7. The safety film according to claim 1, It is characterized in that The base material layer is formed of one of EPU, polyurethane, polyurea, melamine resin, polydimethylsiloxane (PDMS) and rubber series polymer substances.

8. The safety film according to claim 4, It is characterized in that The plastic particles formed with the specific image or specific text are formed at multiple positions in the pattern layer according to a certain rule, and the specific images formed according to the certain rule are combined to form another different image, or the specific texts are combined to form another different article.

9. The safety film according to claim 1, It is characterized in that The substrate layer, pattern layer and upper layer are wrinkled by one load selected from bending load, compression load, tensile load, shear load or torsional load, or a composite load of two or more, and a grating structure is generated by the wrinkles, thereby forming different structural colors and images through the structural colors.

10. A method for verifying counterfeiting using a security film, It is characterized in that A method for verifying the counterfeiting of a security film as claimed in any one of claims 1 to 9, comprising: A step of confirming false alteration by using structural colors developed due to external stimulation applied to the base layer, the pattern layer, and the upper layer having different Young's moduli; The step of identifying the physical taggant formed in the pattern layer by a camera or a microscope to confirm the counterfeit alteration.

Citation Information

Patent Citations

  • Deformable heterogeneous surface complex and anti-counterfeiting alteration device using same

    CN113002205A

  • Manufacturing method of deformable heterogeneous surface complex and anti-counterfeiting alteration device using same