Preparation method of N-methylaniline

Through the combination of multi-step preparation method and iridium catalyst, the problem of high by-product content in traditional N-methylaniline synthesis was solved, and the preparation of N-methylaniline with high purity and high yield was achieved, and the by-product was changed to Environmentally friendly water.

CN118878423APending Publication Date: 2024-11-01HEBEI JINDONG THERMAL MEDIA NEW MATERIALS CO LTD

Patent Information

Application Number
CN202411106140.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-11-01

Smart Images

  • Figure CN118878423A_ABST
    Figure CN118878423A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method of N-methylaniline, which comprises the steps of N-methylation reaction, atmospheric distillation, reduced pressure distillation and the like, and the method provided by the invention has the advantages that the yield is high, the purity is high, and the yield is not lower than 92%; the byproduct with the purity not lower than 99.9% is water, so that the method is green and environment-friendly. # imgabs0 #
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of organic chemical synthesis, and in particular to a method for preparing N-methylaniline. Background Art

[0002] N-methylaniline, chemical formula is C 7 H 9 N, with the structural formula as follows, is a colorless to reddish brown oily liquid with a boiling point of 196°C; slightly soluble in water, soluble in ethanol, ether and chloroform, mainly used as an intermediate, acid absorbent and solvent for organic synthesis. In the dye industry, it is used for the production of Cationic Brilliant Red 5GN, Cationic Pink FG, Cationic Pink B, Reactive Yellow Brown KGR, Reactive Yellow Brown KGR, Reactive Brilliant Blue X-BR, Reaction Orange K-2RL, Acid Blue BR, etc.

[0003]

[0004] The traditional N-methylaniline synthesis method uses aniline as raw material, methanol as alkylating agent, sulfuric acid as catalyst, and liquid phase synthesis to obtain a crude product under a pressure of 3.0 MPa, and then distills to obtain a finished product. The disadvantage of this method is that the impurity content in the product is relatively high, mainly the by-product N, N-dimethylaniline. The boiling point of N, N-dimethylaniline is 193°C-194°C, which is close to the boiling point of the target product N-methylaniline of 196°C, and it is difficult to remove it by conventional distillation methods. Summary of the invention

[0005] The object of the present invention is to provide a method for preparing high-purity N-methylaniline. The N-methylaniline obtained by the method of the present invention has a by-product N,N-dimethylaniline content of less than 0.1%, preferably less than 0.05%, and more preferably less than 0.01%.

[0006] The present invention provides a method for preparing N-methylaniline, comprising the following steps:

[0007] (1) N-methylation reaction: Aniline, methanol and water are added to a reaction tank, a catalyst is added, the temperature is controlled at 110-120°C, the pressure is 1.7-2.0 atm, and the reaction is carried out for 9-12 hours to obtain a crude product 1 of N-methylaniline; (2) Atmospheric pressure distillation: heat the crude N-methylaniline 1 to 60-120°C, collect the fraction at this temperature and discard it; obtain the crude N-methylaniline 2; (3) Vacuum distillation: The crude N-methylaniline product 2 is heated to above 135°C, the system pressure is controlled to be 8-10 mmHg, and vacuum distillation is performed to collect the fraction at 138-139°C, which is N-methylaniline; (4) Optionally, using the product obtained in step (3) as a raw material, repeat steps (2) and (3) 1-2 times.

[0008] Furthermore, in step (1), the catalyst is composed of A1 iridium catalyst and A2 iridium catalyst in a weight ratio of (1.5-2.5):1, preferably 2:1.

[0009]

[0010] Furthermore, in step (1), the molar ratio of aniline to methanol is 1:(1-1.3), preferably 1:1.2.

[0011] Furthermore, in step (1), the weight ratio of aniline to catalyst is 1:0.05-0.08, preferably 1:0.064.

[0012] Furthermore, in the step (1), the weight ratio of aniline to water is 1:(3-5).

[0013] Furthermore, the step (2) can be distilled in stages, specifically: heating the crude N-methylaniline 1 to 60-85°C, collecting the fraction at this temperature, and sending it to a methanol recovery system; continuing to heat the mixture to 85-105°C, collecting the fraction at this temperature, and discarding it.

[0014] In step (2), the distillation temperature is 60-85°C, and the fraction is mainly methanol, which is sent to the methanol recovery system to recover methanol; the temperature is raised to 85-105°C, and the main component is water.

[0015] In the present invention, the catalyst is a water-soluble catalyst and the reaction solvent is water. Since the raw materials used can make the reaction system weakly alkaline, the catalyst has no special requirements on the pH value and there is no need to add additional inorganic base to adjust the pH value of the reaction system.

[0016] In the present invention, the byproduct is mainly water, which is green and environmentally friendly.

[0017] Compared with the prior art, the present invention has the following beneficial effects: (1) High yield and purity. The yield is not less than 92% and the purity is not less than 99.9%. (2) The by-product is water, which is green and environmentally friendly. DETAILED DESCRIPTION

[0018] The invention discloses a method for making N-methylaniline. Those skilled in the art can learn from the content of the present invention, combine the relevant principles of organic chemistry, and appropriately improve the process parameters to achieve. It is particularly important to point out that all similar replacements and modifications are obvious to those skilled in the art, and they are all considered to be included within the scope of the invention. The application of the present invention has been described by preferred embodiments, and relevant personnel can obviously change or appropriately change and combine the methods and applications described herein without departing from the content, spirit and scope of the present invention, to achieve and apply the technology of the present invention.

[0019] In order to better understand the present invention but not to limit the scope of the present invention, all the numbers expressing the amount, percentage, and other numerical values ​​used in this application should be understood to be modified by the word "about" in all cases. Each numerical parameter should at least be considered to be obtained based on the reported significant figures and by conventional rounding methods.

[0020] All components used in the present invention can be purchased commercially.

[0021] The present invention is further described below by way of examples, but the examples do not limit the present invention in any way.

[0022] Example 1: Preparation method of N-methylaniline (1) N-methylation reaction: 466 g (5 mol) of aniline, 192 g (6 mol) of methanol, and 2 L of water were added to a reaction tank, and 30 g of a catalyst composed of A1 and A2 in a ratio of 2:1 was added. The temperature was controlled at 110-120° C. and the pressure was 1.8-1.9 atm. The reaction was carried out for 10 hours to obtain a crude product 1 of N-methylaniline. (2) Atmospheric pressure distillation: The crude N-methylaniline product 1 is heated to 60-85°C, the fraction at this temperature is collected and sent to a methanol recovery system; the temperature is further raised to 85-105°C, the fraction at this temperature is collected and discarded; and the crude N-methylaniline product 2 is obtained; (3) Vacuum distillation: The crude N-methylaniline product 2 is heated to above 135°C, the system pressure is controlled to be 8-10 mmHg, and vacuum distillation is performed to collect the fraction at 138-139°C, which is N-methylaniline; 517.5 g (4.83 mol) of N-methylaniline was obtained with a yield of 96.6%, a purity of 99.92%, an N,N-dimethylaniline content of 0.07%, and a methanol content of 0.01%.

[0023] Example 2: Preparation method of N-methylaniline (1) N-methylation reaction: 466 g (5 mol) of aniline, 192 g (6 mol) of methanol, and 2 L of water were added to a reaction tank, and 30 g of a catalyst composed of A1 and A2 in a ratio of 2:1 was added. The temperature was controlled at 110-120° C. and the pressure was 1.8-1.9 atm. The reaction was carried out for 10 hours to obtain a crude product 1 of N-methylaniline. (2) Atmospheric pressure distillation: heat the crude N-methylaniline 1 to 60-120°C, collect the fraction at this temperature and discard it; obtain the crude N-methylaniline 2; (3) Vacuum distillation: The crude N-methylaniline product 2 is heated to above 135°C, the system pressure is controlled to be 8-10 mmHg, and vacuum distillation is performed to collect the fraction at 138-139°C, which is N-methylaniline; (4) Using the product obtained in step (3) as raw material, repeat steps (2) and (3) once.

[0024] 509.0 g (4.75 mol) of N-methylaniline was obtained with a yield of 95.0%, a purity of 99.96% and a content of 0.04% of N,N-dimethylaniline. Example 3: Preparation method of N-methylaniline Steps (1) to (3) are the same as in Example 1; (4) Using the product obtained in step (3) as raw material, repeat steps (2) and (3) twice.

[0025] 500.9 g (4.675 mol) of N-methylaniline was obtained with a yield of 95.0% and a purity of 100.0% without N,N-dimethylaniline.

[0026] Example 4: Preparation method of N-methylaniline (1) N-methylation reaction: 466 g (5 mol) of aniline, 208 g (6.5 mol) of methanol, and 2.2 L of water were added to a reaction tank, and 30.8 g of a catalyst composed of A1 and A2 in a ratio of 1.8:1 was added. The temperature was controlled at 110-120° C. and the pressure was 1.8-1.9 atm. The reaction was carried out for 9 hours to obtain a crude product 1 of N-methylaniline. (2) Atmospheric pressure distillation: heat the crude N-methylaniline 1 to 60-120°C, collect the fraction at this temperature and discard it; obtain the crude N-methylaniline 2; (3) Vacuum distillation: The crude N-methylaniline product 2 is heated to above 135°C, the system pressure is controlled to be 8-10 mmHg, and vacuum distillation is performed to collect the fraction at 138-139°C, which is N-methylaniline; (4) Using the product obtained in step (3) as raw material, repeat steps (2) and (3) once.

[0027] 504.1 g (4.705 mol) of N-methylaniline was obtained with a yield of 94.1%, a purity of 99.93% and an N,N-dimethylaniline content of 0.07%.

[0028] Example 5: Preparation of N-methylaniline (1) N-methylation reaction: 466 g (5 mol) of aniline, 185.6 g (5.8 mol) of methanol, and 1.8 L of water were added to a reaction tank, and 32 g of a catalyst composed of A1 and A2 in a ratio of 2.2:1 was added. The temperature was controlled at 110-120° C. and the pressure was 1.8-1.9 atm. The reaction was carried out for 11 hours to obtain a crude product 1 of N-methylaniline. (2) Atmospheric pressure distillation: heat the crude N-methylaniline 1 to 60-120°C, collect the fraction at this temperature and discard it; obtain the crude N-methylaniline 2; (3) Vacuum distillation: The crude N-methylaniline product 2 is heated to above 135°C, the system pressure is controlled to be 8-10 mmHg, and vacuum distillation is performed to collect the fraction at 138-139°C, which is N-methylaniline; (4) Using the product obtained in step (3) as raw material, repeat steps (2) and (3) once.

[0029] 492.18 g (4.64 mol) of N-methylaniline was obtained with a yield of 92.8%, a purity of 99.94% and an N,N-dimethylaniline content of 0.06%.

[0030] Comparative Example 1: Preparation of N-methylaniline: (1) N-methylation reaction: 466 g (5 mol) of aniline, 192 g (6 mol) of methanol, and 2 L of water were added to a reaction tank, and 30 g of A1 catalyst was added. The temperature was controlled at 110-120° C. and the pressure was 1.8-1.9 atm. The reaction was carried out for 10 hours to obtain a crude product 1 of N-methylaniline. Steps (2) to (4) are the same as in Example 2.

[0031] 456.5 g (4.26 mol) of N-methylaniline was obtained with a yield of 85.2%, a purity of 99.6% and an N,N-dimethylaniline content of 0.4%.

[0032] Comparative Example 2: Preparation of N-methylaniline (1) N-methylation reaction: 466 g (5 mol) of aniline, 192 g (6 mol) of methanol, and 2 L of water were added to a reaction tank, and 30 g of a catalyst composed of A1 and A2 in a ratio of 1:1 was added. The temperature was controlled at 110-120° C. and the pressure was 1.8-1.9 atm. The reaction was carried out for 10 hours to obtain a crude product 1 of N-methylaniline. Steps (2) to (4) are the same as in Example 2.

[0033] 476.3 g (4.45 mol) of N-methylaniline was obtained with a yield of 88.9%, a purity of 99.0% and an N,N-dimethylaniline content of 1.0%.

[0034] Comparative analysis of Examples 1-5 and Comparative Examples 1-2 shows that the catalyst affects the reaction yield and purity. (1) Using a composite catalyst composed of A1 iridium catalyst and A2 iridium catalyst in a weight ratio of (1.5-2.5):1, as shown in Examples 1-5, the yield is not less than 92% and the purity is not less than 99.9%.

[0035] (2) Using a single A1 catalyst, as shown in Comparative Example 1, the yield was 85.2% and the purity of N-methylaniline was 99.6%. Both the yield and the purity were significantly worse than those of Examples 1-5.

[0036] (3) Using a composite catalyst composed of A1 iridium catalyst and A2 iridium catalyst in other weight ratios, such as the composite catalyst composed of A1 iridium catalyst and A2 iridium catalyst in a ratio of 1:1 in Comparative Example 2, the yield was 88.9% and the purity was 99.0%; both the yield and purity were significantly worse than those of Examples 1-5.

[0037] Comparative Example 3: Preparation method of N-methylaniline Steps (1)-(2) and (4) are the same as in Example 2; step (3) is as follows: (3) Vacuum distillation: The crude N-methylaniline product 2 is heated to above 140°C, the system pressure is controlled to be 12-14 mmHg, and vacuum distillation is performed to collect the fraction at 141-142°C, which is N-methylaniline; 510.0 g (4.76 mol) of N-methylaniline was obtained with a yield of 95.2%, a purity of 99.70%, an N,N-dimethylaniline content of 0.26%, and other impurities of 0.04%.

[0038] Comparative analysis of Example 2 and Comparative Example 3 shows that the pressure during vacuum distillation affects the purity of the reactants. (1) When the system pressure is 8-10 mmHg during vacuum distillation, the purity is 99.96%.

[0039] (2) When the system pressure during vacuum distillation was 12-14 mmHg, the purity was 99.70%, the N,N-dimethylaniline content was 0.26%, and the other impurities were 0.04%. Comparative Example 3 was significantly worse than Example 2.

[0040] Comparative Example 4: Preparation of N-methylaniline according to Example 1 of CN112409186A Preparation method: the method of Example 1 of CN112409186A.

[0041] The yield is 90.2%, the purity of N-methylaniline is 99.32%, the content of N,N-dimethylaniline is 0.45%, and other impurities are 0.23%.

Claims

1. A method for preparing N-methylaniline, comprising the steps of: (1) N-methylation reaction: Aniline, methanol and water are added to a reaction tank, a catalyst is added, the temperature is controlled at 110-120°C, the pressure is 1.7-2.0 atm, and the reaction is carried out for 9-12 hours to obtain a crude product 1 of N-methylaniline; (2) Atmospheric pressure distillation: heat the crude N-methylaniline 1 to 60-120°C, collect the fraction at this temperature and discard it; obtain the crude N-methylaniline 2; (3) Vacuum distillation: The crude N-methylaniline product 2 is heated to above 135°C, the system pressure is controlled to be 8-10 mmHg, and vacuum distillation is performed to collect the fraction at 138-139°C, which is N-methylaniline; (4) Optionally, using the product obtained in step (3) as a raw material, repeat steps (2) and (3) 1-2 times; In step (1), the catalyst is composed of A1 iridium catalyst and A2 iridium catalyst in a weight ratio of (1.5-2.5):1; .

2. The preparation method according to claim 1, characterized in that The molar ratio of aniline to methanol is 1:(1-1.3).

3. The preparation method according to claim 1, characterized in that: The molar ratio of aniline to methanol is 1:1.

2.

4. The preparation method according to claim 1, characterized in that: The weight ratio of aniline to catalyst is 1:(0.05-0.08).

5. The preparation method according to claim 1, characterized in that: The weight ratio of aniline to catalyst is 1:0.

064.

6. The preparation method according to claim 1, characterized in that: The weight ratio of aniline to water is 1:(3-5).

Citation Information

Patent Citations

  • Method for realizing selective N-methylation of primary amine

    CN103172523A

  • Metal iridium catalyst with 2, 2'-bis-benzimidazole ligand and method for synthesizing N-methylated primary amine

    CN109420525A

  • Method for catalysis of N-methylation of amines by using iridium complex with methanol as carbon source

    CN110372517A

  • Method for synthesizing N-methylaniline in water

    CN112409186A

Cited By

  • A nitrogen-doped carbon supported Cu-Zn-Bi composite metal catalyst, a preparation method and application thereof

    CN122806530A