LNG low-temperature flexible pipeline framework layer steel wire machining mechanical behavior analysis method
By constructing various mechanical models of steel wires, the wire processing process of LNG low-temperature flexible pipelines is analyzed based on the theory of elastic-plastic mechanics, the problem of failure to consider processing stress in the existing technology is solved, and the rapid calculation and prediction of the mechanical behavior of the pipeline is achieved. Reduced design costs.
Patent Information
- Application Number
- CN202411031817.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-01
AI Technical Summary
The prior art fails to fully consider the stress during the processing process when studying the mechanical properties of low-temperature composite flexible pipelines, which makes it difficult to accurately calculate the deformation information of the pipeline during the processing process, affecting structural performance.
Using the method based on elastic-plastic mechanics theory, the cross-section stress model, bending moment model, axial strain model and tension model of the steel wire are solved by spiral winding angle and wire parameters, and the cross-section stress and tension of the steel wire are calculated. Bending moment provides a rapid analysis of the mechanical behavior of steel wires in the skeleton layer of LNG low-temperature flexible pipeline.
It realizes rapid calculation and prediction of the mechanical behavior of the inner and outer spiral frame steel wire processing process of LNG low-temperature flexible pipelines, makes up for the disadvantages of high cost of manual trial and error in the prior art, and provides a reference for the processing and design of marine flexible pipelines.
Smart Images

Figure CN118886148A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of natural gas pipelines, and in particular to a method for analyzing mechanical behavior of steel wire processing in a skeleton layer of an LNG low-temperature flexible pipeline. Background Art
[0002] Natural gas is a green, clean and efficient energy source, playing an increasingly important role in the global energy sector. Due to its low density, natural gas is usually transported and stored in liquid form to reduce its volume, called liquefied natural gas (LNG). Floating liquefied natural gas (FLNG) is a floating production unit used for offshore natural gas field development. Marine LNG cryogenic flexible pipelines are one of the key core preparations of the offshore LNG transmission system and are known as the "blood vessels" of the marine LNG extraction system.
[0003] So far, many scholars have conducted extensive research on the mechanical properties, failure modes, and structural optimization design of low-temperature composite flexible pipes. However, they mainly focus on exploring the mechanical properties of pipeline structures under different load conditions and do not consider the stress generated by the processing process. In the study of similar structures, it was found that the influence of processing stress on the structural performance of the pipeline cannot be ignored. The pipeline processing and forming process mainly involves the winding forming theory, which is characterized by deformation exceeding the elastic range, with the purpose of producing a permanent effect, so it involves elastic-plastic deformation. How to accurately calculate the deformation information of the pipeline during the processing process is crucial to the study of pipeline performance. Solving the problem of complex load conditions, high nonlinearity and large deformation in pipeline processing is still a challenge.
[0004] Therefore, the present invention provides a method for analyzing the mechanical behavior of steel wire processing in a skeleton layer of an LNG low-temperature flexible pipeline. Summary of the invention
[0005] According to the above-mentioned deficiencies, a method for analyzing the mechanical behavior of steel wire processing in the skeleton layer of LNG low-temperature flexible pipeline is provided. The present invention mainly constructs a steel wire cross-sectional stress model, a steel wire bending moment model, an axial strain model of the inner skeleton steel wire, an axial strain model of the outer skeleton steel wire, a tension model of the inner skeleton steel wire and a tension model of the outer skeleton steel wire based on the pipeline processing process, and quickly analyzes and evaluates the stress state of the steel wire based on the elastic-plastic mechanics theory.
[0006] The technical means adopted by the present invention are as follows:
[0007] The present invention provides a method for analyzing mechanical behavior of a skeleton layer steel wire of an LNG cryogenic flexible pipeline. The skeleton layer steel wire of the LNG cryogenic flexible pipeline comprises an inner skeleton steel wire and an outer skeleton steel wire, including:
[0008] Constructing a steel wire cross-sectional stress model, a steel wire bending moment model, an axial strain model of the inner skeleton steel wire, an axial strain model of the outer skeleton steel wire, a tension model of the inner skeleton steel wire, and a tension model of the outer skeleton steel wire;
[0009] Obtain the spiral winding angle, the parameters of the inner skeleton steel wire and the parameters of the outer skeleton steel wire, solve the axial strain model of the inner skeleton steel wire and the tension model of the inner skeleton steel wire according to the spiral winding angle and the parameters of the inner skeleton steel wire, obtain the axial stress distribution of the inner skeleton steel wire and the tension of the inner skeleton steel wire, solve the steel wire cross-sectional stress model and the steel wire bending moment model according to the tension of the inner skeleton steel wire, and obtain the cross-sectional stress distribution of the inner skeleton steel wire and the bending moment of the inner skeleton steel wire; solve the axial strain model and the tension model of the outer skeleton steel wire according to the spiral winding angle and the parameters of the outer skeleton steel wire, obtain the axial stress distribution of the outer skeleton steel wire and the tension of the outer skeleton steel wire, solve the steel wire cross-sectional stress model and the steel wire bending moment model according to the tension of the outer skeleton steel wire, and obtain the cross-sectional stress distribution of the outer skeleton steel wire and the bending moment of the outer skeleton steel wire.
[0010] Preferably, the wire cross-section stress model is calculated in the following manner:
[0011]
[0012] Among them, F t is the section tension along the tangent direction, A is the cross-sectional area of the wire, σ s is the yield strength of the steel wire, y is the distance from a point on the steel wire cross section to the neutral axis, σ p R is the maximum stress on the wire section after rolling. s_in is the radius of the inner skeleton steel wire, σ0 is the internal stress of the steel wire after rolling, and d E is the height of the elastic zone of the cross section after rolling, P in is the extrusion pressure between the mandrel and the steel wire, P out is the external pressure on the steel wire, M t is the moment along the tangent direction, I t is the polar moment of inertia, α is the spiral winding angle, R is the radius of the liner core mold, G is the shear modulus of the steel wire, is the cross-sectional stress along the tangent direction, σ n is the normal stress, σ b is the stress in the binormal direction, R m1 It is the sum of the wire radius and the drum radius.
[0013] Preferably, the wire bending moment model is calculated in the following manner:
[0014]
[0015] Among them, P in is the extrusion pressure between the mandrel and the steel wire, P out is the external pressure on the steel wire, α is the spiral winding angle, M b is the moment along the binormal direction, E is the elastic modulus of the steel wire, I t is the polar moment of inertia, R s_in is the radius of the inner skeleton wire, F t p is the tension of the inner skeleton steel wire, R m1 It is the sum of the radius of the inner skeleton wire and the radius of the drum, and ν is the Poisson's ratio.
[0016] Preferably, the axial strain model of the inner skeleton steel wire is calculated in the following manner:
[0017]
[0018] Among them, ε t is the total strain along the axial direction of the inner skeleton steel wire, H is the horizontal projection length of the front edge of the steel wire winding, α is the spiral winding angle, y is the distance from a point on the steel wire cross section to the neutral axis, R m1 is the sum of the radius of the inner skeleton wire and the radius of the drum, ΔH is the change in the horizontal projection length before and after the wire is wound, It is the change in torsion angle after the wire is wound.
[0019] Preferably, the axial strain model of the exoskeleton steel wire is calculated in the following manner:
[0020]
[0021] Among them, ε t ′ is the total strain along the axial direction of the exoskeleton steel wire, H is the horizontal projection length of the front edge of the steel wire winding, α is the spiral winding angle, y is the distance from a point on the steel wire cross section to the neutral axis, R m2 is the sum of the radius of the outer skeleton steel wire, the thickness of the composite material layer and the radius of the drum. ΔH is the change in the horizontal projection length before and after the steel wire is wound. It is the change in torsion angle after the wire is wound.
[0022] Preferably, the tension model of the inner skeleton steel wire is calculated in the following manner:
[0023]
[0024] Among them, F t pis the tension of the inner skeleton steel wire, α is the spiral winding angle, E is the elastic modulus of the steel wire, A is the cross-sectional area of the steel wire, and R s_in is the radius of the inner skeleton steel wire, H is the horizontal projection length of the front edge of the steel wire winding, is the change in torsion angle after the wire is wound, R m1 E is the sum of the radius of the inner skeleton wire and the radius of the drum. p is the tangent modulus of the steel wire in the plastic deformation stage, Θ1 is the first constant term, ΔH is the change in the projection length of the steel wire in the horizontal direction before and after winding, and ν is the Poisson's ratio.
[0025] Preferably, the tension model of the exoskeleton steel wire is calculated in the following manner:
[0026]
[0027] Among them, F t p ' is the tension of the inner skeleton steel wire, α is the spiral winding angle, E is the elastic modulus of the steel wire, A is the cross-sectional area of the steel wire, R s_out is the radius of the outer skeleton steel wire, is the change in torsion angle after the wire is wound, R m2 E is the sum of the radius of the outer skeleton steel wire, the thickness of the composite material layer and the radius of the drum. p is the tangent modulus of the steel wire in the plastic deformation stage, Θ2 is the second constant term, ΔH is the change in the projection length of the steel wire in the horizontal direction before and after winding, and ν is the Poisson's ratio.
[0028] Preferably, the internal stress of the steel wire after rolling is determined according to the residual stress in the steel wire during the steel wire rolling forming process, and the residual stress in the steel wire is calculated by a residual stress model in the steel wire during the steel wire rolling forming process;
[0029] The residual stress model in the steel wire is calculated in the following way:
[0030]
[0031] Among them, σ a is the maximum stress on the wire cross section during the wire rolling process, σ s is the yield strength of the steel wire, y is the distance from a point on the steel wire cross section to the neutral axis, σ max is the maximum stress caused by the unloading bending moment, d e is the height of the elastic zone of the cross section during the wire rolling process, R s_in is the radius of the inner skeleton steel wire.
[0032] Compared with the prior art, the present invention has the following advantages:
[0033] 1. The mechanical behavior analysis method for the steel wire processing of the skeleton layer of the LNG cryogenic flexible pipeline provided by the present invention can quickly calculate and predict the mechanical behavior of the inner and outer spiral skeleton steel wire processing process of the LNG cryogenic flexible pipeline. At the same time, this method is not limited to the pipeline type and the cross-sectional shape of the steel wire. When performing the calculation, it is only necessary to perform equivalent substitution on the relevant variables.
[0034] 2. The mechanical behavior analysis method for the steel wire processing of the skeleton layer of the LNG cryogenic flexible pipeline provided by the present invention is solved based on the principles of elastic-plastic mechanics, which is closer to the actual situation than the current research method based on elastic assumptions for winding mechanical behavior.
[0035] 3. The mechanical behavior analysis method for processing steel wires in the skeleton layer of LNG cryogenic flexible pipelines provided by the present invention makes up for the shortcoming of high cost of manual trial and error in the current pipeline processing process, and provides a reference for the processing and design of marine flexible pipelines. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0037] Figure 1 This is a structural schematic diagram of LNG cryogenic flexible pipeline.
[0038] Figure 2 This is a processing schematic diagram of LNG cryogenic flexible pipeline.
[0039] Figure 3 A schematic diagram of a rolling process.
[0040] Figure 4 Schematic diagram of a steel wire constitutive model.
[0041] Figure 5 A schematic diagram of stress distribution in a wire-wrapped cross section.
[0042] Figure 6 Schematic diagram of stress distribution caused by unloading bending moment.
[0043] Figure 7 A schematic diagram of residual stress in a steel wire.
[0044] Figure 8 It is a mechanical analysis model for the inner skeleton wire winding process.
[0045] Fig. 9 This is a schematic diagram of the relationship between tension and contact in a wire winding process.
[0046] Fig.10 A schematic diagram of stress distribution of a steel wire cross section.
[0047] Fig.11 This is a schematic diagram of the force on a steel wire.
[0048] Fig.12 It is a mechanical analysis model for the exoskeleton wire winding process.
[0049] In the figure: 1. Inner skeleton steel wire; 2. Sealing layer; 3. Braided layer; 4. Outer skeleton steel wire; 5. Composite layer. DETAILED DESCRIPTION
[0050] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.
[0051] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.
[0052] Combination Figure 1 , Figure 2 , Figure 1 This is a structural diagram of a LNG cryogenic flexible pipeline. Figure 2 The following is a schematic diagram of processing a LNG cryogenic flexible pipeline to illustrate a specific embodiment of the mechanical behavior analysis method for processing a steel wire of a skeleton layer of a LNG cryogenic flexible pipeline provided by the present invention, including:
[0053] Constructing a wire cross-sectional stress model, a wire bending moment model, an axial strain model of an inner skeleton wire, an axial strain model of an outer skeleton wire, a tension model of an inner skeleton wire, and a tension model of an outer skeleton wire;
[0054] The spiral winding angle, the parameters of the inner skeleton steel wire and the parameters of the outer skeleton steel wire are obtained, and the axial strain model and the tension model of the inner skeleton steel wire are solved according to the spiral winding angle and the parameters of the inner skeleton steel wire to obtain the axial stress distribution of the inner skeleton steel wire and the tension of the inner skeleton steel wire, and the wire cross-sectional stress model and the wire bending moment model are solved according to the tension of the inner skeleton steel wire to obtain the cross-sectional stress distribution of the inner skeleton steel wire and the bending moment of the inner skeleton steel wire; the axial strain model and the tension model of the outer skeleton steel wire are solved according to the spiral winding angle and the parameters of the outer skeleton steel wire to obtain the axial stress distribution of the outer skeleton steel wire and the tension of the outer skeleton steel wire, and the wire cross-sectional stress model and the wire bending moment model are solved according to the tension of the outer skeleton steel wire to obtain the cross-sectional stress distribution of the outer skeleton steel wire and the bending moment of the outer skeleton steel wire.
[0055] It is understandable that common marine LNG cryogenic flexible pipeline structures such as Figure 1 As shown; the inner and outer parts are skeleton steel wires spirally wound at nearly 90 degrees, which are used to improve the resistance of the LNG composite ultra-low temperature resistant flexible pipeline structure to internal and external pressures. The inner skeleton steel wire 1 and the outer skeleton steel wire 4 are offset to fix the sealing layer 2 in the middle of the two layers of springs. The pressure acting on the sealing layer 2 provides radial sealing pressure, which is beneficial to the sealing of the pipeline. The composite layer 5 is mainly composed of a sealing layer 2 and a braided layer 3. The sealing layer 2 placed on the inner layer is used to prevent liquid leakage, and the braided layer 3 laid on the outer layer withstands the axial deformation of the pipeline and provides axial rigidity, and finally forms a wave-like structure, which is beneficial to the bending of the low-temperature composite flexible pipeline and has good flexibility. According to the structural characteristics of the LNG low-temperature flexible pipeline, the processing order is the winding of the inner skeleton steel wire 1, the winding of the sealing layer 2, the winding of the braided layer 3, the winding of the outer skeleton steel wire 4, and the assembly of the end connection joints, and finally forms a sample pipe for testing and verification.
[0056] The processing of the inner and outer spiral skeleton layers includes two processes. Figure 2 The first step is to pre-deform the steel wire through a three-wheel rolling bending mechanism, and the second step is to wind the deformed steel wire around the lining core mold.
[0057] Therefore, when modeling and analyzing the mechanical behavior of skeleton layer steel wire processing, the deformation and stress process of the steel wire during these two processing processes are considered, and the following assumptions are made:
[0058] The friction between the inner and outer skeleton wires, drums and rollers is ignored;
[0059] The inner and outer skeleton steel wires are in a stress-free state before rolling;
[0060] The stress-strain curves of the inner and outer skeleton steel wire materials are simplified into a linear strengthening constitutive model;
[0061] The drum and roller are set as rigid bodies;
[0062] The rolling and winding process of the inner and outer skeleton steel wires is regarded as a quasi-static loading process;
[0063] The sealing layer and the braided layer are equivalent to a homogeneous cylindrical shell.
[0064] Furthermore, the wire cross-section stress model, wire bending moment model, axial strain model of inner skeleton wire, axial strain model of outer skeleton wire, tension model of inner skeleton wire and tension model of outer skeleton wire are constructed. According to the model, the mechanical behavior of the inner and outer spiral skeleton wires of LNG cryogenic flexible pipelines can be quickly calculated and predicted during processing. At the same time, this method is not limited to pipeline types and wire cross-section shapes. When calculating, only relevant variables need to be equivalently replaced. The solution based on the principle of elastic-plastic mechanics is closer to the actual situation than the current research method based on elastic assumptions for winding mechanical behavior, which makes up for the high cost of manual trial and error in the current pipeline processing process and provides a reference for the processing and design of marine flexible pipelines.
[0065] In some optional embodiments, referring to Figure 3 , Figure 4 , Figure 5 , Figure 6 and Figure 7 , Figure 3 A schematic diagram of a rolling process. Figure 4 is a schematic diagram of a steel wire constitutive model. Figure 5 A schematic diagram of stress distribution in a wire winding section. Figure 6 A schematic diagram of stress distribution caused by unloading bending moment. Figure 7 This is a schematic diagram of residual stress in a steel wire, and an analysis of the steel wire during the rolling process is performed. Figure 3 , the contact points of the upper roller, lower left roller, and lower right roller with the steel wire are A and B respectively. The curvature of the steel wire is 0 before passing through point A. After reaching point A, the curvature and bending moment increase rapidly. After reaching point B, the curvature reaches the maximum, and the bending moment also reaches the maximum at this time. After reaching point C, the bending moment decreases, and the steel wire rebounds to a certain extent. When unloading, the stress change caused by the change in bending moment is calculated according to the elastic law. In this process, the friction between the steel wire and the roller is ignored, and the stress-strain curve of the steel wire material is simplified to a linear hardening constitutive model, such as Figure 4 As shown in the figure. Due to the elastic-plastic deformation of the steel wire, its cross section is divided into an elastic region and a plastic region. The stress distribution diagram is shown in the figure. Figure 5 shown.
[0066] The height of the elastic zone of the cross section during the wire rolling process is calculated as follows:
[0067]
[0068] Among them, d eis the height of the cross-section elastic zone during the wire rolling process, R3 is the radius of the upper roller, and R s_in is the radius of the inner skeleton wire, σ s is the yield strength of the steel wire, and E is the elastic modulus of the steel wire.
[0069] According to the stress distribution of the steel wire cross section, the theoretical stress expression can be written as follows:
[0070]
[0071] Among them, σ a It is the maximum stress on the cross section of the steel wire during the steel wire rolling process.
[0072] The strain of the steel wire at point B can be expressed as follows:
[0073]
[0074] Among them, ε B is the strain of the wire at point B.
[0075] According to the strain at point B and the constitutive model, ε can be solved by B The stress at point B is approximated by the formula:
[0076]
[0077] Among them, E p is the tangent modulus of the steel wire during the plastic deformation stage.
[0078] After the steel wire passes through point C, the cross-sectional stress will be released to a certain extent. During unloading, the stress change caused by the change in bending moment is calculated according to the elastic law below.
[0079]
[0080] Among them, y is the distance from a point on the wire cross section to the neutral axis, ΔM is the unloading bending moment, and Δσ is the change in stress caused by the change in bending moment.
[0081] The stress distribution caused by the unloading bending moment is as follows Figure 6 As shown:
[0082]
[0083] Among them, σ max is the maximum stress caused by the unloading bending moment.
[0084] Reference Figure 7 , the residual stress model in the steel wire is calculated as follows:
[0085]
[0086] Among them, σ a is the maximum stress on the wire cross section during the wire rolling process, σ s is the yield strength of the steel wire, y is the distance from a point on the steel wire cross section to the neutral axis, σ max is the maximum stress caused by the unloading bending moment, d e is the height of the elastic zone of the cross section during the wire rolling process, R s_in is the radius of the inner skeleton wire.
[0087] In some optional embodiments, referring to Figure 8 , Figure 8 This is a mechanical analysis model for the inner skeleton wire winding process, which analyzes the inner spiral skeleton wire winding forming process:
[0088] After the steel wire passes through the rolling section, there will be stress inside. This part of stress is superimposed as the initial stress on the stress state during the winding process. The length of the steel wire is s. Assuming that the angle between the steel wire and the horizontal direction before winding is α, the spiral winding structure formed after processing has a spiral angle of α'. Assuming that the steel wire is continuously wound along the tangent direction of the initial placement angle, that is, α = α', the length of the steel wire changes by Δs after winding. The stress-strain curve of the steel wire material is simplified to a linear strengthening constitutive model. The mechanical model is as follows: Figure 8 As shown in the figure, in this process, the axial strain model of the inner skeleton wire is calculated as follows:
[0089]
[0090] Among them, ε t is the total strain along the axial direction of the inner skeleton wire, H is the horizontal projection length of the wire winding front, α is the spiral winding angle, y is the distance from a point on the wire cross section to the neutral axis, R m1 is the sum of the radius of the inner skeleton wire and the radius of the drum, ΔH is the change in the horizontal projection length before and after the wire is wound, is the change in torsion angle after wire winding, and R is the radius of the liner core mold.
[0091] In some optional embodiments, referring to Fig. 9 , Fig. 9 This is a schematic diagram of the relationship between tension and contact in a steel wire winding process. After the steel wire enters the elastic-plastic state, the cross section will show an interval distribution between the elastic region and the plastic region. Due to the combined effect of tension and bending moment in this direction, the neutral axis will be offset to a certain extent. The offset distance is h. The stress distribution of the steel wire cross section is as follows: Fig. 9 shown.
[0092] The height of the elastic zone of the cross section after rolling is d E , can be calculated as follows:
[0093]
[0094] Among them, σ s is the yield strength of the steel wire, and E is the elastic modulus of the steel wire.
[0095] Therefore, the wire cross-section stress model is calculated as follows:
[0096]
[0097] Among them, F t is the section tension along the tangent direction, A is the cross-sectional area of the wire, σ s is the yield strength of the steel wire, y is the distance from a point on the steel wire cross section to the neutral axis, σ p R is the maximum stress on the wire section after rolling. s_in is the radius of the inner skeleton wire, σ0 is the internal stress of the wire after rolling, d E is the height of the elastic zone of the cross section after rolling, P in is the extrusion pressure between the mandrel and the steel wire, P out is the external pressure on the steel wire, M t is the moment along the tangent direction, I t is the polar moment of inertia, α is the spiral winding angle, R is the radius of the inner liner core mold, G is the shear modulus of the steel wire, is the cross-sectional stress along the tangent direction, σ n is the normal stress, σ b is the stress in the binormal direction, R m1 It is the sum of the wire radius and the drum radius.
[0098] It should be noted that P in is the extrusion force between the mandrel and the steel wire, and its value has a certain relationship with the steel wire tension. Fig. 9 The internal stress σ0 of the steel wire after rolling is calculated based on the residual stress σ r (y) determines the residual stress σ in the steel wire r (y) is calculated by the residual stress model of the steel wire during the steel wire rolling process. out is the external pressure on the steel wire, and P can be used in subsequent solutions. out =0.
[0099] Specifically, the cross-sectional force F along the tangent direction is t , calculated as follows:
[0100]
[0101] Here, β is the helix angle.
[0102] In some optional embodiments, the wire balance equation is calculated as follows:
[0103]
[0104] Among them, F b , F t p , M b , M t are the section forces and moments along the normal, binormal and tangent directions, respectively, f n is the cross-sectional distributed force along the normal direction, κ n is the normal curvature, κ t is the tangential curvature.
[0105] Section moment M n , M b , M t It can be calculated as follows:
[0106]
[0107] Where h is the offset distance of the neutral axis under tension and bending moment, I t is the polar moment of inertia.
[0108] The constitutive equation of the steel wire is calculated as follows:
[0109]
[0110] in, is the tangential strain, is the normal strain, is the strain in the binormal direction, F t p is the tension along the tangent direction of the cross section.
[0111] By making the axial strain model of the inner skeleton steel wire equal to the constitutive equation of the steel wire, the tension model of the inner skeleton steel wire can be derived and calculated as follows:
[0112]
[0113] Θ1=2E p Gνycosαsinα+2sinα 2 Y p -E p P e R m1 ν-2ER m1 σ p +2ER m1 σ s -2E p R m1 σ s
[0114] Among them, F t p is the tension of the inner skeleton wire, α is the spiral winding angle, E is the elastic modulus of the wire, A is the cross-sectional area of the wire, R s_in is the radius of the inner skeleton wire, H is the horizontal projection length of the wire winding front, is the change in torsion angle after the wire is wound, R m1 is the sum of the wire radius and the drum radius, E p is the tangent modulus of the steel wire in the plastic deformation stage, Θ1 is the first constant term, ΔH is the change in the projection length of the steel wire in the horizontal direction before and after winding, and ν is the Poisson's ratio.
[0115] In some optional embodiments, referring to Fig.10 , Fig.10 A schematic diagram of the stress distribution of a steel wire cross section, with the cross-sectional distribution force f along the normal direction n It can also be calculated as follows:
[0116] f n =(P out -P in )·2R s_in
[0117] Among them, P in is the extrusion pressure between the mandrel and the steel wire, P out is the external pressure on the steel wire, R s_in is the radius of the inner skeleton wire.
[0118] Make n =(P out -P in )·2R s_in With f n =κ t (κ n M t -κ t M b )-κ n F t The wire bending moment model can be derived and calculated as follows:
[0119]
[0120] Among them, P in is the extrusion pressure between the mandrel and the steel wire, P out is the external pressure on the wire, α is the spiral winding angle, M b is the moment along the binormal direction, E is the elastic modulus of the steel wire, I t is the polar moment of inertia, R s_in is the radius of the inner skeleton wire, F tp is the tension of the inner skeleton wire, R m1 is the sum of the wire radius and the drum radius, and ν is the Poisson's ratio.
[0121] In some optional embodiments, the mechanical analysis of the inner skeleton steel wire processing process is performed according to the model, including:
[0122] The Poisson effect of the wire along the cross-sectional direction is not considered, that is, ε n =0 can be deduced:
[0123]
[0124] Where G is the shear modulus of the steel wire.
[0125] The force of skeleton steel wire is Fig.10 As shown in the figure, the actual contact position between the steel wire and the core mold is at point B due to the relaxation effect during winding. The relaxation offset distance d is defined as the distance between the extension line of the steel wire tension F and the core axis. The force on the steel wire is decomposed in the xoy plane to obtain the following relationship:
[0126]
[0127] Among them, θ is the relaxation angle, and d is the shortest distance between the wire tension action line and the outer radius of the liner core mold, which is positively correlated with the relaxation angle θ.
[0128] Given the spiral winding angle α and the parameters of the inner skeleton wire, let F BT =F t p , M B =M b , the following formulas can be combined to solve:
[0129]
[0130] Get the inner skeleton wire and
[0131] Substitute it into the axial strain model of the inner skeleton steel wire to obtain the axial stress distribution of the inner skeleton steel wire, substitute it into the tension model of the inner skeleton steel wire to obtain the tension of the inner skeleton steel wire, substitute the tension of the inner skeleton steel wire into the steel wire cross-sectional stress model to obtain the cross-sectional stress distribution of the inner skeleton steel wire, substitute the tension of the inner skeleton steel wire into the steel wire bending moment model to obtain the bending moment of the inner skeleton steel wire.
[0132] In some optional embodiments, referring to Fig.11 and Fig.12 , Fig.11 A schematic diagram of the force on a steel wire. Fig.12It is a mechanical analysis model for exoskeleton steel wire winding processing. The mechanical analysis model for exoskeleton steel wire winding is shown in Figure 11. The strain tension derivation of the exoskeleton steel wire is based on the linear strengthening assumption.
[0133] Because the outer skeleton steel wire needs to exert pressure on the middle composite material layer during the process of winding it around the inner liner core mold to compress it inward to form a corrugated shape, the solution for the axial strain and tension of the outer skeleton steel wire is the same as that of the inner skeleton steel wire, but the variable R in the above formula needs to be m1 Replace with R m2 , R s_in Replace with R s_out .
[0134] Therefore, the axial strain model of the exoskeleton steel wire is calculated as follows:
[0135]
[0136] Among them, ε t ′ is the total strain along the axial direction of the exoskeleton wire, H is the horizontal projection length of the wire winding front, α is the spiral winding angle, y is the distance from a point on the wire cross section to the neutral axis, R m2 is the sum of the radius of the outer skeleton steel wire, the thickness of the composite material layer and the radius of the drum. ΔH is the change in the horizontal projection length before and after the steel wire is wound. It is the change in torsion angle after the wire is wound.
[0137] Specifically, R m2 It is calculated as follows:
[0138] R m2 =R+R s_out +t
[0139] Wherein, t is the thickness of the middle composite material layer after compaction.
[0140] In some optional embodiments, continue to refer to Fig.11 and Fig.12 The idea of establishing the tension model of the outer skeleton steel wire is the same as that of the inner skeleton steel wire. Therefore, the tension model of the outer skeleton steel wire is calculated as follows:
[0141]
[0142] Among them, F t p ′ is the tension of the inner skeleton wire, α is the spiral winding angle, E is the elastic modulus of the wire, A is the cross-sectional area of the wire, R s_out is the radius of the outer skeleton wire, is the change in torsion angle after the wire is wound, R m2E is the sum of the radius of the outer skeleton steel wire, the thickness of the composite material layer and the radius of the drum. p is the tangent modulus of the steel wire in the plastic deformation stage, Θ2 is the second constant term, ΔH is the change in the projection length of the steel wire in the horizontal direction before and after winding, and ν is the Poisson's ratio.
[0143] Specifically, Θ2 is calculated as follows:
[0144] Θ2=2E p Gνycosαsinα+2sinα 2 Y p -E p P e R m2 ν+2ER m2 (σ s -σ p )-2E p R m2 σ s .
[0145] In some optional embodiments, mechanical analysis of the exoskeleton steel wire processing process is performed according to the model, including:
[0146] Given the spiral winding angle α and the parameters of the outer skeleton wire, substitute them into the following formula:
[0147]
[0148]
[0149] Get the outer skeleton wire and
[0150] Substitute it into the axial strain model of the exoskeleton steel wire to obtain the axial stress distribution of the exoskeleton steel wire, substitute it into the tension model of the exoskeleton steel wire to obtain the tension of the exoskeleton steel wire, substitute the tension of the exoskeleton steel wire into the steel wire cross-sectional stress model to obtain the cross-sectional stress distribution of the exoskeleton steel wire, substitute the tension of the exoskeleton steel wire into the steel wire bending moment model to obtain the bending moment of the exoskeleton steel wire.
[0151] In some optional embodiments, the present invention is further described by taking a certain project using a low-temperature composite flexible pipe as an example and combining with a specific embodiment, with reference to Table 1:
[0152] Table 1. Steel wire parameters
[0153]
[0154] Step 1: Substitute the parameters of the inner and outer skeleton steel wires into the formula to calculate the residual stress in the rolling stage;
[0155] Step 2: Solve the strain, stress distribution, tension and bending moment of the inner skeleton wire
[0156] Let the winding relaxation angle be 16.5° and calculate the inner skeleton wire and
[0157] The result is introduced into the axial strain model of the inner skeleton steel wire to calculate the axial stress distribution of the inner skeleton steel wire;
[0158] The result is brought into the tension model of the inner skeleton steel wire to calculate the tension of the inner skeleton steel wire;
[0159] The tension of the inner skeleton steel wire is introduced into the steel wire cross-sectional stress model to calculate the cross-sectional stress distribution of the inner skeleton steel wire;
[0160] The tension of the inner skeleton steel wire is brought into the steel wire bending moment model to calculate the bending moment of the inner skeleton steel wire.
[0161] Step 3: Solve the strain, stress distribution, tension and bending moment of the exoskeleton steel wire
[0162] Let the winding relaxation angle be 16.5° and calculate the outer skeleton wire and
[0163] The result is introduced into the axial strain model of the exoskeleton steel wire to calculate the axial stress distribution of the exoskeleton steel wire;
[0164] Substitute this result into the tension model of the exoskeleton steel wire to calculate the tension of the exoskeleton steel wire;
[0165] The tension of the exoskeleton steel wire is brought into the steel wire cross-sectional stress model to calculate the cross-sectional stress distribution of the exoskeleton steel wire;
[0166] The tension of the exoskeleton steel wire is brought into the steel wire bending moment model to obtain the bending moment of the exoskeleton steel wire.
[0167] Step 4: Arrange the results. The mechanical behavior analysis results of the inner and outer skeleton steel wires are shown in Table 2:
[0168] Table 2. Summary of inner and outer skeleton wire winding results
[0169]
[0170] It can be seen from the above that the mechanical behavior analysis method for LNG cryogenic flexible pipeline skeleton layer steel wire processing provided by the present invention can quickly calculate and predict the mechanical behavior of the inner and outer spiral skeleton steel wire processing process of LNG cryogenic flexible pipeline.
[0171] The serial numbers of the above embodiments of the present invention are only for description and do not represent the advantages or disadvantages of the embodiments.
[0172] In the above embodiments of the present invention, the description of each embodiment has its own emphasis. For parts that are not described in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.
[0173] The technical solution of the present invention, in essence, or the part that contributes to the prior art, or the whole or part of the technical solution can be embodied in the form of a software product, which is stored in a storage medium and includes several instructions for enabling a computer device (which can be a personal computer, a server or a network device, etc.) to perform all or part of the steps of the method described in each embodiment of the present invention. The aforementioned storage medium includes: U disk, read-only memory (ROM, Read-Only Memory), random access memory (RAM, Random Access Memory), mobile hard disk, magnetic disk or optical disk, etc., various media that can store program codes.
[0174] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for analyzing mechanical behavior of steel wire processing for skeleton layer of LNG cryogenic flexible pipeline, wherein the steel wire for skeleton layer of LNG cryogenic flexible pipeline comprises inner skeleton steel wire and outer skeleton steel wire, characterized in that: include: Constructing a steel wire cross-sectional stress model, a steel wire bending moment model, an axial strain model of the inner skeleton steel wire, an axial strain model of the outer skeleton steel wire, a tension model of the inner skeleton steel wire, and a tension model of the outer skeleton steel wire; Obtain the spiral winding angle, the parameters of the inner skeleton steel wire and the parameters of the outer skeleton steel wire, solve the axial strain model of the inner skeleton steel wire and the tension model of the inner skeleton steel wire according to the spiral winding angle and the parameters of the inner skeleton steel wire, obtain the axial stress distribution of the inner skeleton steel wire and the tension of the inner skeleton steel wire, solve the steel wire cross-sectional stress model and the steel wire bending moment model according to the tension of the inner skeleton steel wire, and obtain the cross-sectional stress distribution of the inner skeleton steel wire and the bending moment of the inner skeleton steel wire; solve the axial strain model and the tension model of the outer skeleton steel wire according to the spiral winding angle and the parameters of the outer skeleton steel wire, obtain the axial stress distribution of the outer skeleton steel wire and the tension of the outer skeleton steel wire, solve the steel wire cross-sectional stress model and the steel wire bending moment model according to the tension of the outer skeleton steel wire, and obtain the cross-sectional stress distribution of the outer skeleton steel wire and the bending moment of the outer skeleton steel wire.
2. The mechanical behavior analysis method for processing steel wire of the skeleton layer of LNG cryogenic flexible pipeline according to claim 1 is characterized in that: The wire cross-section stress model is calculated in the following manner: Among them, F t is the section tension along the tangent direction, A is the cross-sectional area of the wire, σ s is the yield strength of the steel wire, y is the distance from a point on the steel wire cross section to the neutral axis, σ p R is the maximum stress on the wire section after rolling. s_in is the radius of the inner skeleton steel wire, σ0 is the internal stress of the steel wire after rolling, and d E is the height of the elastic zone of the cross section after rolling, P in is the extrusion pressure between the mandrel and the steel wire, P out is the external pressure on the steel wire, M t is the moment along the tangent direction, I t is the polar moment of inertia, α is the spiral winding angle, R is the radius of the liner core mold, G is the shear modulus of the steel wire, is the cross-sectional stress along the tangent direction, σ n is the normal stress, σ b is the stress in the binormal direction, R m1 It is the sum of the wire radius and the drum radius.
3. The mechanical behavior analysis method for processing steel wire of LNG cryogenic flexible pipeline skeleton layer according to claim 1 is characterized in that: The wire bending moment model is calculated as follows: Among them, P in is the extrusion pressure between the mandrel and the steel wire, P out is the external pressure on the wire, α is the spiral winding angle, M b is the moment along the binormal direction, E is the elastic modulus of the steel wire, I t is the polar moment of inertia, R s_in is the radius of the inner skeleton wire, F t p is the tension of the inner skeleton wire, R m1 It is the sum of the radius of the inner skeleton wire and the radius of the drum, and ν is the Poisson's ratio.
4. The mechanical behavior analysis method for processing steel wire of skeleton layer of LNG cryogenic flexible pipeline according to claim 1 is characterized in that: The axial strain model of the inner skeleton steel wire is calculated as follows: Among them, ε t is the total strain along the axial direction of the inner skeleton steel wire, H is the horizontal projection length of the front edge of the steel wire winding, α is the spiral winding angle, y is the distance from a point on the steel wire cross section to the neutral axis, R m1 is the sum of the radius of the inner skeleton wire and the radius of the drum, ΔH is the change in the horizontal projection length before and after the wire is wound, It is the change in torsion angle after the wire is wound.
5. The mechanical behavior analysis method for processing steel wire of skeleton layer of LNG cryogenic flexible pipeline according to claim 1 is characterized in that: The axial strain model of the exoskeleton steel wire is calculated as follows: Among them, ε t ′ is the total strain along the axial direction of the exoskeleton steel wire, H is the horizontal projection length of the front edge of the steel wire winding, α is the spiral winding angle, y is the distance from a point on the steel wire cross section to the neutral axis, R m2 is the sum of the radius of the outer skeleton steel wire, the thickness of the composite material layer and the radius of the drum. ΔH is the change in the horizontal projection length before and after the steel wire is wound. It is the change in torsion angle after the wire is wound.
6. The mechanical behavior analysis method for processing steel wire of skeleton layer of LNG cryogenic flexible pipeline according to claim 1 is characterized in that: The tension model of the inner skeleton steel wire is calculated as follows: Among them, F t p is the tension of the inner skeleton steel wire, α is the spiral winding angle, E is the elastic modulus of the steel wire, A is the cross-sectional area of the steel wire, and R s_in is the radius of the inner skeleton steel wire, H is the horizontal projection length of the front edge of the steel wire winding, is the change in torsion angle after the wire is wound, R m1 is the sum of the wire radius and the drum radius, E p is the tangent modulus of the steel wire in the plastic deformation stage, Θ1 is the first constant term, ΔH is the change in the projection length of the steel wire in the horizontal direction before and after winding, and ν is the Poisson's ratio.
7. The mechanical behavior analysis method for processing steel wire of skeleton layer of LNG cryogenic flexible pipeline according to claim 1 is characterized in that: The tension model of the exoskeleton steel wire is calculated as follows: Among them, F t p ' is the tension of the inner skeleton steel wire, α is the spiral winding angle, E is the elastic modulus of the steel wire, A is the cross-sectional area of the steel wire, R s_out is the radius of the outer skeleton steel wire, is the change in torsion angle after the wire is wound, R m2 E is the sum of the radius of the outer skeleton steel wire, the thickness of the composite material layer and the radius of the drum. p is the tangent modulus of the steel wire in the plastic deformation stage, Θ2 is the second constant term, ΔH is the change in the projection length of the steel wire in the horizontal direction before and after winding, and ν is the Poisson's ratio.
8. The mechanical behavior analysis method for processing steel wire of skeleton layer of LNG cryogenic flexible pipeline according to claim 2 is characterized in that: The internal stress of the steel wire after rolling is determined according to the residual stress in the steel wire during the steel wire rolling forming process, and the residual stress in the steel wire is calculated by a residual stress model in the steel wire during the steel wire rolling forming process; The residual stress model in the steel wire is calculated in the following way: Among them, σ a is the maximum stress on the wire cross section during the wire rolling process, σ s is the yield strength of the steel wire, y is the distance from a point on the steel wire cross section to the neutral axis, σ max is the maximum stress caused by the unloading bending moment, d e is the height of the elastic zone of the cross section during the wire rolling process, R s_in is the radius of the inner skeleton steel wire.