Semiconductor structure and forming method thereof
By introducing dipole dopants into CFETs and controlling their distribution in high k dielectric layer, the problems of uneven distribution of dipole dopants and threshold voltage regulation in semiconductor devices are solved, and the integrated density and performance of transistors are improved , realizes optimization of NFET and PFET work functions.
Patent Information
- Application Number
- CN202410929404.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-07-12
- Filing Date
- 2024-07-11
- Publication Date
- 2024-11-01
AI Technical Summary
With the reduction of the minimum feature size of semiconductor devices, the prior art is difficult to effectively solve the problems of uneven distribution of dipole dopant and threshold voltage regulation in gate dielectrics, affecting the performance and integration density of transistors.
By introducing dipole dopants into complementary field effect transistors (CFETs), the in-situ or ectopic doping of dipole dopants is controlled to form different dopants using a combination of high k dielectric layer and interface layer. Percentage of gate dielectric, sharing common gate electrodes to optimize the work function and threshold voltage of the transistor.
The effective work function adjustment of NFET and PFET is realized, the threshold voltage is reduced, the integrated density and performance stability of the transistor are improved, the damage of the high-k dielectric layer is avoided, and the manufacturing process is simplified.
Smart Images

Figure CN118888515A_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present application relate to semiconductor structures and methods of forming the same. Background Art
[0002] Semiconductor devices are used in a variety of electronic applications, such as, for example, personal computers, cell phones, digital cameras, and other electronic devices. Semiconductor devices are typically manufactured by sequentially depositing insulating or dielectric layers, conductive layers, and semiconductor material layers over a semiconductor substrate, and patterning the various material layers using photolithography to form circuit components and elements thereon.
[0003] The semiconductor industry continues to increase the integration density of various electronic components (such as transistors, diodes, resistors, capacitors, etc.) by continuously reducing the minimum feature size, thereby allowing more components to be integrated into a given area. However, as the minimum feature size decreases, other problems arise that need to be solved. Summary of the invention
[0004] Some embodiments of the present application provide a method for forming a semiconductor structure, comprising: forming a first semiconductor channel region and a second semiconductor channel region, wherein the second semiconductor channel region overlaps with the first semiconductor channel region; forming a first gate dielectric on the first semiconductor channel region; forming a second gate dielectric on the second semiconductor channel region; introducing a dipole dopant into the first gate dielectric of the first gate dielectric and the second gate dielectric to a higher atomic percentage, wherein the second gate dielectric of the first gate dielectric and the second gate dielectric has a lower atomic percentage of the dipole dopant; and forming a gate electrode on both the first gate dielectric and the second gate dielectric, wherein the gate electrode and the first gate dielectric form part of a first transistor, and the gate electrode and the second gate dielectric form part of a second transistor.
[0005] Some other embodiments of the present application further provide a semiconductor structure, the semiconductor structure comprising:
[0006] a lower transistor, the lower transistor comprising:
[0007] a first channel region;
[0008] a first gate dielectric overlying the first channel region, wherein the first gate dielectric has a first atomic percent of a dipole dopant; and
[0009] a first gate electrode on the first gate dielectric; and
[0010] an upper transistor, wherein the lower transistor and a first transistor of the upper transistor are n-type transistors, and wherein the lower transistor and a second transistor of the upper transistor are p-type transistors, and wherein the upper transistor comprises:
[0011] a second channel region overlapping the first channel region;
[0012] a second gate dielectric overlying the second channel region, wherein the second gate dielectric has a second atomic percentage of the dipole dopant, and wherein the second atomic percentage is different than the first atomic percentage; and
[0013] A second gate electrode is positioned on the second gate dielectric, wherein the first gate electrode and the second gate electrode are portions of a same continuous gate electrode.
[0014] Some other embodiments of the present application provide a semiconductor structure, which includes:
[0015] a lower transistor, the lower transistor comprising:
[0016] a first channel region;
[0017] a first gate dielectric on the first channel region, wherein the first gate dielectric comprises a high-k dielectric material; and
[0018] a first source / drain region connected to the first channel region; and
[0019] an upper transistor, the upper transistor comprising:
[0020] a second channel region overlapping the first channel region;
[0021] a second gate dielectric overlying the second channel region, wherein the second gate dielectric comprises the high-k dielectric material and a dipole dopant, wherein a first atomic percentage of the dipole dopant in the first gate dielectric is lower than a second atomic percentage of the dipole dopant in the second gate dielectric; and
[0022] A second source / drain region connected to the second channel region, wherein the second source / drain region overlaps the first source / drain region, and wherein the first source / drain region and the second source / drain region have opposite conductivity types.
[0023] The present application also relates to the introduction of volume-less dipole into a CFET with a common gate. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] When read in conjunction with the accompanying drawings, aspects of the present disclosure can be best understood from the following detailed description. It should be noted that, in accordance with standard practice in the industry, the various components are not drawn to scale. In fact, the dimensions of the various components may be arbitrarily increased or reduced for clarity of discussion.
[0025] Figure 1 A perspective view of an example complementary field effect transistor (CFET) is shown in accordance with some embodiments.
[0026] Figures 2 to 11 is a diagram of an intermediate stage in the fabrication of a CFET according to some embodiments.
[0027] Figure 12-1 to Figure 12-7 A diagram illustrating ex-situ dipole dopant doping in a gate stack forming a CFET, according to some embodiments.
[0028] Figure 13-1 to Figure 13-6 A diagram illustrating in-situ dipole dopant doping in a gate stack forming a CFET, according to some embodiments.
[0029] Figure 14-1 to Figure 14-6 A diagram illustrating ex-situ dipole dopant doping in a gate stack forming a CFET, according to some embodiments.
[0030] Figure 15-1 to Figure 15-6 A diagram illustrating in-situ dipole dopant doping in a gate stack forming a CFET, according to some embodiments.
[0031] Fig.16 Illustrative dipole dopant atomic percentages in the gate dielectric of a FET according to some embodiments are shown.
[0032] Fig.17 A flow chart for forming a CFET is shown in accordance with some embodiments. DETAILED DESCRIPTION
[0033] The following disclosure provides many different embodiments or examples for implementing the different components of the present application. Specific examples of components and arrangements are described below to simplify the present disclosure. Of course, these are merely examples and are not intended to be limiting. For example, in the following description, forming a first component above or on a second component may include an embodiment in which the first component and the second component are directly contacted, and may also include an additional component that can be formed between the first component and the second component, so that the first component and the second component may not be in direct contact. In addition, the present disclosure may repeat reference numerals and / or characters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself indicate the relationship between the various embodiments and / or configurations discussed.
[0034] Furthermore, for ease of description, spatially relative terms such as "below," "beneath," "lower," "above," "upper," etc. may be used herein to describe the relationship of one element or component to another (or additional) elements or components as shown in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein should be interpreted accordingly.
[0035] A complementary field effect transistor (CFET) structure and a method for forming the same are provided. Throughout the description, the terms "FET" and "transistor" are used interchangeably. According to some embodiments, the CFET structure includes an NFET and a PFET, which share a common metal gate (having a common work function material). When the common metal gate has a p-type work function layer, an n-type dipole dopant is doped into the high-k dielectric layer of the NFET. When the common metal gate has an n-type work function layer, a p-type dipole dopant is doped into the high-k dielectric layer of the PFET. Although full-all-around gate (GAA) transistors (such as nanostructure FETs) are discussed, the concepts of the present disclosure can also be applied to form other types of transistors, such as planar transistors, fin field effect transistors (FinFETs), and the like. In addition, in the example shown, the upper FET is a PFET and the lower FET is an NFET, while in other embodiments, the upper FET can also be an NFET and the lower FET can be a PFET.
[0036] Figure 1 An example of a CFET 10 (including FETs (transistors) 10U and 10L) according to some embodiments is shown. Figure 1 is a three-dimensional view in which some components of the CFET are omitted for clarity of illustration.
[0037] The CFET includes a plurality of vertically stacked FETs. For example, the CFET may include a lower nanostructure FET 10L of a first device type (e.g., n-type / p-type) and an upper nanostructure FET 10U of a second device type (e.g., p-type / n-type) opposite to the first device type. The nanostructure FETs 10U and 10L include a semiconductor nanostructure 26' (including a lower semiconductor nanostructure 26'L and an upper semiconductor nanostructure 26'U), wherein the semiconductor nanostructure 26' serves as a channel region of the nanostructure FET. The lower semiconductor nanostructure 26'L is used for the lower nanostructure FET 10L, and the upper semiconductor nanostructure 26'U is used for the upper nanostructure FET 10U.
[0038] The gate dielectric 78 surrounds the corresponding semiconductor nanostructure 26'. The gate electrode 80 (including the lower gate electrode 80L and the upper gate electrode 80U) is located above the gate dielectric 78. The source / drain region 62 (including the lower epitaxial source / drain region 62L and the upper epitaxial source / drain region 62U) is disposed on opposite sides of the gate dielectric 78 and the corresponding gate electrode 80. The source / drain region may refer to the source or drain individually or collectively depending on the context. An isolation member (not shown) may be formed to separate the desired source / drain region of the source / drain region 62 and / or the desired gate electrode of the gate electrode 80.
[0039] Figure 1 Reference cross sections used in subsequent figures are further illustrated. Cross section A-A' is a vertical cross section parallel to the longitudinal axis of the semiconductor nanostructure 26' of the CFET and in the direction of current flow, for example, between the source / drain regions 62 of the CFET. Cross section BB' is a vertical cross section perpendicular to cross section A-A' and along the longitudinal axis of the gate electrode 80 of the CFET. Cross section CC' is a vertical cross section parallel to cross section BB' and extending through the source / drain regions 62 of the CFET. For clarity, subsequent figures may refer to these reference cross sections.
[0040] Figures 2 to 11 The formation of a CFET (such as Figure 1 The corresponding process is also schematically shown in FIG. Fig.17 In the following discussion, unless otherwise indicated, the figures with the letter "A" after the number show the process flow 200 along the same Figure 1 The drawings with the letter "B" after the numbers show the vertical cross-section along the same plane as the vertical reference cross-section AA'. Figure 1 The drawings with the letter "C" after the numbers show the cross-sections along the vertical reference cross-section BB' in FIG. Figure 1 The vertical reference section C-C' in the figure is a vertical cross-sectional view of a similar section.
[0041] exist Figure 2In the present invention, a wafer 2 including a substrate 20 is provided. The substrate 20 may be a semiconductor substrate, such as a bulk semiconductor, a semiconductor on insulator (SOI) substrate, etc., which may be doped (e.g., with a p-type or n-type dopant) or undoped. The SOI substrate may include a semiconductor material layer formed on an insulator layer. The insulator layer may be, for example, a buried oxide (BOX) layer, a silicon oxide layer, etc. An insulator layer is provided on a substrate, such as on a silicon substrate or a glass substrate. Other substrates, such as multilayer substrates or gradient substrates may also be used. In some embodiments, the semiconductor material of the substrate 20 may include silicon, germanium, carbon-doped silicon, III-V compound semiconductors, etc., or a combination thereof.
[0042] A multilayer stack 22 is formed over the substrate 20. The corresponding process is shown as Fig.17 The process 202 in the process flow 200 is shown. The multilayer stack 22 includes alternating dummy semiconductor layers 24 (including dummy semiconductor layers 24A and dummy semiconductor layers 24B) and semiconductor layers 26 (including lower semiconductor layers 26L and upper semiconductor layers 26U). The lower semiconductor layers 26L and the upper semiconductor layers 26U are used to form lower FETs and upper FETs, respectively.
[0043] Appropriate wells (not separately shown) may be formed in the lower semiconductor layer 26L and the upper semiconductor layer 26U. For example, the semiconductor layers 26L and 26U may be in-situ doped (when epitaxially grown) and / or implanted to a desired conductivity type.
[0044] In the example shown, the multilayer stack 22 includes six dummy semiconductor layers 24 and six semiconductor layers 26. It should be understood that the multilayer stack 22 may include any number of dummy semiconductor layers 24 and semiconductor layers 26. Each layer of the multilayer stack 22 may be grown by a process such as vapor phase epitaxy (VPE) or molecular beam epitaxy (MBE), deposited by a process such as a chemical vapor deposition (CVD) process or an atomic layer deposition (ALD) process, etc.
[0045] The dummy semiconductor layer 24A is formed of a first semiconductor material, and the dummy semiconductor layer 24B is formed of a second semiconductor material different from the first semiconductor material. The first semiconductor material and the second semiconductor material can be selected from candidate semiconductor materials of the substrate 20. The first semiconductor material and the second semiconductor material have high etching selectivity relative to each other. In this way, in subsequent processes, the dummy semiconductor layer 24B can be removed at a faster rate than the dummy semiconductor layer 24A.
[0046] The semiconductor layer 26 (including the lower semiconductor layer 26L and the upper semiconductor layer 26U) is formed of one or more semiconductor materials. The semiconductor material can be selected from candidate semiconductor materials of the substrate 20. The lower semiconductor layer 26L and the upper semiconductor layer 26U can be formed of the same semiconductor material, or can be formed of different semiconductor materials.
[0047] In some embodiments, dummy semiconductor layer 24A is formed of or includes silicon germanium, semiconductor layer 26 is formed of silicon, and dummy semiconductor layer 24B may be formed of germanium or silicon germanium having a higher atomic percentage of germanium than in semiconductor layer 24A.
[0048] exist Figure 3 In the embodiment, the multilayer stack 22 and the substrate 20 are patterned to form semiconductor strips 28. The corresponding process is shown as Fig.17 Process 204 in the process flow 200 shown. Each semiconductor strip 28 includes a semiconductor strip 20' (part of the original substrate 20) and a multilayer stack 22', which is the remaining portion of the multilayer stack 22. The remaining portion 22' of the multilayer stack 22 is referred to as a nanostructure hereinafter, which is indicated by a "'" symbol after the corresponding reference numeral. Accordingly, the multilayer stack 22' includes a pseudo nanostructure 24'A, a pseudo nanostructure 24'B, a lower semiconductor nanostructure 26'L, an intermediate semiconductor nanostructure 26'M, and an upper semiconductor nanostructure 26'U. Etching can be performed by any acceptable etching process, such as reactive ion etching (RIE), neutral beam etching (NBE), etc. or a combination thereof. Etching can be anisotropic. The pseudo nanostructure 24'A and the pseudo nanostructure 24'B can also be collectively referred to as a pseudo nanostructure 24'. The lower semiconductor nanostructure 26'L and the upper semiconductor nanostructure 26'U can also be collectively referred to as a semiconductor nanostructure 26'.
[0049] The lower semiconductor nanostructure 26'L will serve as the channel region of the lower nanostructure FET of the CFET. The upper semiconductor nanostructure 26'U will serve as the channel region of the upper nanostructure FET of the CFET. The intermediate semiconductor nanostructure 26'M is a semiconductor nanostructure 26' that is immediately above / below (e.g., contacts the pseudo nanostructure 24'B) the pseudo nanostructure 24'B. The intermediate semiconductor nanostructure 26'M can be used for isolation and may or may not serve as the channel region of the CFET. The pseudo nanostructure 24'B will subsequently be replaced by an isolation structure. The isolation structure and the intermediate semiconductor nanostructure 26'M can define the boundaries of the lower nanostructure FET and the upper nanostructure FET.
[0050] The semiconductor fins and nanostructures may be patterned by any suitable method. For example, the patterning process may include one or more photolithography processes, including a double patterning process or a multiple patterning process. Typically, the double patterning process or the multiple patterning process combines a photolithography process with a self-aligned process, thereby allowing the creation of patterns having, for example, a smaller pitch than that obtainable using a single direct photolithography process. For example, in one embodiment, a sacrificial layer is formed over a substrate and the sacrificial layer is patterned using a photolithography process. Using a self-aligned process, spacers are formed next to the patterned sacrificial layer. The sacrificial layer is then removed, and the remaining spacers may then be used as an etch mask for the patterning process.
[0051] Isolation regions 32 are formed over substrate 20 and between adjacent semiconductor strips 28. The corresponding process is shown as follows Fig.17 Process 206 in the process flow 200 shown. The isolation region 32 may include a dielectric liner and a dielectric material above the dielectric liner. Each of the dielectric liner and the dielectric material may include an oxide such as silicon oxide, a nitride such as silicon nitride, or the like, or a combination thereof. The formation of the isolation region 32 may include depositing a dielectric layer, and performing a planarization process such as a chemical mechanical polishing (CMP) process, a mechanical polishing process, or the like to remove excess portions of the dielectric material. The deposition process may include ALD, high density plasma CVD (HDP-CVD), flowable CVD (FCVD), or the like, or a combination thereof. In some embodiments, the isolation region 32 includes silicon oxide formed by an FCVD process followed by an annealing process.
[0052] The isolation region 32 is then recessed. The corresponding process is shown as Fig.17 Process 206 of process flow 200 is shown. Some upper portions of semiconductor strips 28 (including multilayer stack 22 ′) protrude above remaining isolation regions 32 to form protruding fins 34 .
[0053] exist Figure 4 In the embodiment of the present invention, a dummy dielectric layer 36 is formed on the protruding fin 34. The dummy dielectric layer 36 may be formed of, for example, silicon oxide, silicon nitride, a combination thereof, or the like, or may include, for example, silicon oxide, silicon nitride, a combination thereof, or the like, and the dummy dielectric layer 36 may be deposited or thermally grown according to an acceptable technique. A dummy gate layer 38 is formed over the dummy dielectric layer 36. The dummy gate layer 38 may be deposited, for example, by physical vapor deposition (PVD), CVD, or other techniques, and then planarized by, for example, a CMP process. The material of the dummy gate layer 38 is conductive or non-conductive, and may be selected from a group including amorphous silicon, polycrystalline silicon (polysilicon), polycrystalline silicon germanium (poly-SiGe), or the like. A mask layer 40 is formed over the planarized dummy gate layer 38, and the mask layer 40 may include, for example, silicon nitride, silicon oxynitride, or the like.
[0054] Next, the mask layer 40 may be patterned by photolithography and etching processes to form a mask, which is then used to etch and pattern the dummy gate layer 38 and possibly the dummy dielectric layer 36 . Figure 5 The resulting structure is shown in Figure 5 2 shows a cross section along the longitudinal direction of the semiconductor strip 28. The mask layer 40, the dummy gate layer 38 and the remaining portion of the dummy dielectric layer 36 form a dummy gate stack 42. The corresponding process is shown as follows: Fig.17 Process 208 in process flow 200 is shown.
[0055] exist Figure 6 In the embodiment, gate spacers 44 are formed over the multilayer stack 22' and on the exposed sidewalls of the dummy gate stack 42. The corresponding process is shown as follows Fig.17 Process 210 in process flow 200 is shown. Gate spacers 44 may be formed by conformally forming one or more dielectric layers and then anisotropically etching the dielectric layers. Suitable dielectric materials may include silicon oxide, silicon nitride, silicon oxynitride, silicon carbon oxynitride, etc., which may be formed by deposition processes such as CVD, ALD, etc. Fin spacers are also formed.
[0056] Source / drain recesses 46 are formed in semiconductor strips 28. The corresponding process is shown as Fig.17 Process 210 in the process flow 200 shown. Source / drain recesses 46 are formed by etching, and the source / drain recesses 46 can extend through the multilayer stack 22' and into the semiconductor strip 20'. The bottom surface of the source / drain recess 46 can be located above, below, or flush with the top surface of the isolation region 32. During the etching process, the gate spacers 44 and the dummy gate stack 42 mask some portions of the semiconductor strip 28. The etching can include a single etching process or multiple etching processes. A timed etching process can be used to stop the etching of the source / drain recess 46 when the source / drain recess 46 reaches a desired depth.
[0057] exist Figure 7 In the embodiment, an internal spacer 54 and a dielectric isolation layer 56 are formed. The corresponding process is shown as follows Fig.17 The process 212 in the process flow 200 shown in FIG. 212 can include lateral etching of the pseudo nanostructure 24′A ( Figure 6 ) and an etching process for removing the pseudo nanostructure 24'B.
[0058] The etching process may be isotropic and may be selective to the material of the pseudo nanostructure 24'A, so that the pseudo nanostructure 24'A is etched at a faster rate than the semiconductor nanostructures 26'U and 26'L. The etching process may also be selective to the material of the pseudo nanostructure 24'B, so that the pseudo nanostructure 24'B is etched at a faster rate than the pseudo nanostructure 24'A. In this way, the pseudo nanostructure 24'B may be completely removed from between the lower semiconductor nanostructure 26'L (commonly) and the upper semiconductor nanostructure 26'U (commonly) without completely removing the pseudo nanostructure 24'A.
[0059] In some embodiments where the pseudo nanostructure 24'B is formed of germanium or silicon germanium with a high atomic percentage of germanium, the pseudo nanostructure 24'A is formed of silicon germanium with a low atomic percentage of germanium, and the semiconductor nanostructure 26' (including 26'M, 26'U, and 26'L) is formed of silicon without germanium, the etching process may include a dry etching process with or without plasma using chlorine gas. Because the pseudo gate stack 42 is wrapped around the semiconductor nanostructure 26' (see Figure 2 ), the dummy gate stack 42 can support the upper semiconductor nanostructure 26'U so that the upper semiconductor nanostructure 26'U does not collapse when the dummy nanostructure 24'B is removed. In addition, although the sidewall of the dummy nanostructure 24'A is shown as straight after etching, the sidewall can be concave or convex.
[0060] An internal spacer 54 is formed on the sidewall of the recessed pseudo nanostructure 24'A, and a dielectric isolation layer 56 is formed between the upper semiconductor nanostructure 26'U (collectively) and the lower semiconductor nanostructure 26'L (collectively). In the subsequent formation of the source / drain region, the internal spacer 54 can serve as an isolation component between the subsequently formed source / drain region and the subsequently formed gate structure. In addition, the internal spacer 54 can be used to prevent the subsequently formed source / drain region from being damaged by a subsequent etching process (such as an etching process for forming a gate structure). On the other hand, the dielectric isolation layer 56 is used to isolate the upper semiconductor nanostructure 26'U (collectively) from the lower semiconductor nanostructure 26'L (collectively). In addition, the intermediate semiconductor nanostructure 26'M and the dielectric isolation layer 56 can define the boundary of the lower nanostructure FET and the upper nanostructure FET.
[0061] The internal spacer 54 and the dielectric isolation layer 56 can be formed by conformally depositing an insulating material in the source / drain recess 46 and between the upper semiconductor nanostructure 26'U and the lower semiconductor nanostructure 26'L, and then etching the insulating material. The insulating material can be a non-low-k dielectric material, which can be a carbon-containing dielectric material such as silicon oxynitride, silicon oxycarbide, silicon oxynitride, etc. The insulating material can be formed by a deposition process such as ALD, CVD, etc. The etching of the insulating material can be anisotropic or isotropic. When etching the insulating material, the insulating material has a portion remaining in the sidewall of the pseudo nanostructure 24'A (thereby forming the internal spacer 54) and has a portion remaining between the upper semiconductor nanostructure 26'U and the lower semiconductor nanostructure 26'L (thereby forming the dielectric isolation layer 56).
[0062] Also like Figure 7 As shown, a lower epitaxial source / drain region 62L and an upper epitaxial source / drain region 62U are formed. The lower epitaxial source / drain region 62L is formed in the lower portion of the source / drain recess 46. The corresponding process is shown as follows: Fig.17 Process 222 of process flow 200 is shown. The lower epitaxial source / drain region 62L contacts the lower semiconductor nanostructure 26'L and does not contact the upper semiconductor nanostructure 26'U. The inner spacer 54 electrically insulates the lower epitaxial source / drain region 62L from the dummy nanostructure 24'A, which will be replaced by a replacement gate in a subsequent process.
[0063] The lower epitaxial source / drain region 62L is epitaxially grown and has a conductivity type suitable for the device type (p-type or n-type) of the lower nanostructure FET. When the lower epitaxial source / drain region 62L is an n-type source / drain region, the corresponding material may include silicon or carbon-doped silicon, which is doped with an n-type dopant such as phosphorus, arsenic, etc. When the lower epitaxial source / drain region 62L is a p-type source / drain region, the corresponding material may include silicon or silicon germanium, which is doped with a p-type dopant such as boron, indium, etc.
[0064] The lower epitaxial source / drain region 62L may be in-situ doped and may or may not be implanted with a corresponding p-type or n-type dopant. During epitaxy of the lower epitaxial source / drain region 62L, the upper semiconductor nanostructure 26'U may be masked to prevent undesired epitaxial growth on the upper semiconductor nanostructure 26'U. After growing the lower epitaxial source / drain region 62L, the mask on the upper semiconductor nanostructure 26'U may then be removed.
[0065] A first contact etch stop layer (CESL) 66 and a first interlayer dielectric (ILD) 68 are formed over the lower epitaxial source / drain regions 62L. The corresponding process is shown as follows Fig.17 Process 224 in the process flow 200 is shown. The first CESL 66 may be formed of a dielectric material having a high etch selectivity to the first ILD 68, such as silicon nitride, silicon oxide, silicon oxynitride, etc., and the first CESL 66 may be formed by any suitable deposition process, such as CVD, ALD, etc. The first ILD 68 may be formed of a dielectric material, and the first ILD 68 may be deposited by any suitable method, such as CVD, plasma enhanced CVD (PECVD), or FCVD. Suitable dielectric materials for the first ILD 68 may include phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), undoped silicate glass (USG), silicon oxide, etc.
[0066] The formation process may include depositing a conformal CESL layer, depositing a material for the first ILD 68, followed by a planarization process, and then an etch-back process. In some embodiments, the first ILD 68 is first etched, leaving the first CESL 66 unetched. An anisotropic etching process is then performed to remove the portion of the first CESL 66 that is above the recessed first ILD 68. After the recess, the sidewalls of the upper semiconductor nanostructure 26'U are exposed.
[0067] Then, an upper epitaxial source / drain region 62U is formed in the upper portion of the source / drain recess 46. The corresponding process is shown as follows: Fig.17 Process 226 in the illustrated process flow 200. An upper epitaxial source / drain region 62U may be epitaxially grown from the exposed surface of the upper semiconductor nanostructure 26'U. Depending on the desired conductivity type of the upper epitaxial source / drain region 62U, the material of the upper epitaxial source / drain region 62U may be selected from the same candidate group of materials used to form the lower source / drain region 62L.
[0068] The conductivity type of the upper epitaxial source / drain region 62U can be opposite to the conductivity type of the lower epitaxial source / drain region 62L. For example, the upper epitaxial source / drain region 62U can be doped opposite to the lower epitaxial source / drain region 62L. The upper epitaxial source / drain region 62U can be in-situ doped with and / or implanted with useful n-type or p-type dopants. Adjacent upper source / drain regions 62U can remain separated or can be merged after the epitaxial process.
[0069] After forming the epitaxial source / drain regions 62U, the second CESL 70 and the second ILD 72 are formed. The corresponding process is shown as follows: Fig.17Process 228 in process flow 200 is shown. The materials and formation methods may be similar to those of first CESL 66 and first ILD 68, respectively, and are not discussed in detail herein. The formation process may include depositing layers for CESL 70 and ILD 72, and performing a planarization process to remove excess portions of the respective layers. After the planarization process, the top surfaces of second ILD 72, gate spacers 44, and dummy gate stack 42 are coplanar (within process variations). The planarization process may remove mask 40, or leave hard mask 40 unremoved.
[0070] A replacement gate stack is then formed to replace the dummy gate stack. The dummy gate stack 42 is first removed in one or more etching processes to form a recess 74, such as Fig. 8A and Figure 8B The corresponding process is shown as Fig.17 Process 230 of process flow 200 is shown. Each recess 74 exposes a portion of multilayer stack 22' and / or is located over a portion of multilayer stack 22'.
[0071] The remaining portion of the pseudo nanostructure 24'A is then removed by etching, so that the groove 74 extends between the semiconductor nanostructures 26'. In the etching process, the pseudo nanostructure 24'A is etched at a faster rate than the semiconductor nanostructure 26', the dielectric isolation layer 56, and the internal spacer 54. The etching can be isotropic. For example, when the pseudo nanostructure 24'A is formed of silicon germanium and the semiconductor nanostructure 26' is formed of silicon, the etching process can include a wet etching process using tetramethylammonium hydroxide (TMAH), ammonium hydroxide (NH4OH), etc.
[0072] exist Fig.9A and Fig. 9B In FIG. 7 , the gate dielectric 78 is formed as part of a conformal liner located in the recess 74 and formed on the exposed semiconductor nanostructure 26 ′. The corresponding process is shown as Fig.17 Process 232 of process flow 200 is shown. A gate dielectric 78 is formed on the exposed surfaces of the exposed features including the semiconductor nanostructure 26' and the gate spacers 44. The gate dielectric 78 wraps around all (eg, four) sides of the semiconductor nanostructure 26'.
[0073] Figure 12-1 to Figure 12-7 , Figure 13-1 to Figure 13-6 , Figure 14-1 to Figure 14-6 and Figure 15-1 to Figure 15-6 Various embodiments of gate stacks forming CEFTS are shown, with the CEFTS sharing a common gate electrode 80 (including 80U and 80L). Figure 12-1 to Figure 12-7 The formation of a dipole dopant ex situ doped into the high-k dielectric layer of the lower FET is shown. Figure 12-1 , showing that Fig. 9B Region 86 is shown. In the example shown, the upper FET to be formed is a PFET and the lower FET to be formed is an NFET.
[0074] The gate dielectric 78 (including 78U and 78L) is formed to surround the nanostructures 26'U, 26'M and 26'L. Each gate dielectric 78 may include an interface layer 78IL, which may be formed of or include a group IV element, a group III element and / or a group V element. The interface layer 78IL may include an oxide such as silicon oxide or a metal oxide, a silicate such as a metal silicate, a combination thereof, a multilayer thereof, and the like. The interface layer 78IL may have a thickness in a range between about 0.5 nm and about 2 nm. The interface layer 78IL may be formed by a thermal oxidation process and / or a deposition process.
[0075] The gate dielectric 78 may also include a high-k dielectric layer 78HK (including 78HK-U and 78HK-L), and the high-k dielectric layer 78HK has a high dielectric constant (high-k) value greater than, for example, about 7.0, about 21 or more. The high-k dielectric layer 78HK may be formed by a metal oxide or silicate of a metal selected from hafnium, zirconium, barium, titanium, lead and a combination thereof, or the high-k dielectric layer 78HK may include a metal oxide or silicate of a metal selected from hafnium, zirconium, barium, titanium, lead and a combination thereof. The formation method of the high-k dielectric layer 78HK may be selected from molecular beam deposition (MBD), ALD, PECVD, etc. The high-k dielectric layer 78HK may have a thickness in a range between about 1nm and about 5nm. The gate dielectric 78 in the upper FET region and the lower FET region is formed in a common process. For clarity, the gate dielectric 78 is represented as 78U and 78L. When forming the gate dielectric 78 , the gate dielectric 78 may be free of an n-type dipole dopant as will be discussed later, or may include a small amount of a dipole dopant for adjusting a threshold voltage.
[0076] refer to Figure 12-2 , a dipole film 82 is deposited on the gate dielectric 78. The deposition process may include a conformal deposition process such as ALD, CVD, etc. The corresponding process is shown as Fig.17Process 234 in the process flow 200 shown. The dipole film 82 includes an n-type dipole dopant, which, when introduced into the gate dielectric of an n-type FET, can reduce the effective work function and thus reduce the threshold voltage of the corresponding n-type FET. When the n-type dipole dopant is introduced into the gate dielectric of a p-type FET, the n-type dipole dopant can reduce the effective work function and thus increase the threshold voltage of the corresponding p-type FET. According to some embodiments, the dipole film 82 may include one or more materials selected from oxides, nitrides and / or carbides of n-type dipole dopants (such as La, Sr, Y, Er, Sc, Mg, etc. or combinations thereof). The thickness of the dipole film 82 may be in a range between about 0.3 nm and about 1.5 nm.
[0077] refer to Figure 12-3 , forming a dummy filling region 84. The corresponding process is shown as Fig.17 The process 236 in the process flow 200 is shown. According to some embodiments, the dummy fill region 84 is formed by Fig.9A and Fig. 9B The exposed parts of the structure shown are formed of a material with high etch selectivity. For example, the dummy fill region 84 can be formed of SiN, SiOC, SiO, SiOCN, SiCN, AlO, AlN, CoN, etc. The formation process may include depositing a fill material to completely fill the groove 74 ( Fig. 9B ), performing a planarization process to flatten the top surface of the filling material, and etching back the filling material. The etching process is controlled so that the top surface of the dummy filling region 84 is at a level between the top surface level and the bottom surface level of the dielectric isolation layer 56, and the top surface may be slightly higher or lower. Within process variations, the dummy filling region 84 may have a flat top surface.
[0078] Next, an isotropic etching process is performed, such as Figure 12-4 The corresponding process is shown as Fig.17 Process 238 in the process flow 200 shown. The etching process can be a wet etching process or a dry etching process, and the etching process is isotropic. The etching chemical is selected to etch the dipole film 82 and stop on the high-k dielectric layer 78HK. Accordingly, the portion of the dipole film 82 located on the upper intermediate semiconductor nanostructure of the upper semiconductor nanostructure 26'U and the intermediate semiconductor nanostructure 26'M is removed. The portion of the dipole film 82 located on the lower intermediate semiconductor nanostructure of the lower semiconductor nanostructure 26'L and the intermediate semiconductor nanostructure 26'M is protected from being removed.
[0079] In the subsequent process, the dummy filling region 84 is removed. The corresponding process is shown as follows Fig.17The process 240 in the process flow 200 is shown. The resulting structure is as follows Figure 12-5 After the dummy filling region 84 is removed, the dipole film 82 in the lower FET region is exposed, while in the upper FET region, there is no dipole film.
[0080] Further references Figure 12-5 , an annealing process 88 is performed to drive the dipole dopant in the dipole film 82 into the corresponding underlying high-k dielectric layer 78HK-L. The resulting high-k dielectric layer with the introduced dipole dopant is referred to as the high-k dielectric layer 78HK'-L hereinafter. The corresponding process is shown as follows Fig.17 Process 242 in the process flow 200 shown. The annealing process 88 can be performed in a process gas such as N2, He, NH3, Ar, etc. or a mixture thereof. According to some embodiments, the annealing process 88 is performed by an immersion annealing process, a spike rapid thermal annealing process, etc. When the immersion annealing process is adopted, the annealing duration can be in the range between about 5 seconds to about 5 minutes. The annealing temperature can be in the range between about 500°C and about 850°C. When the spike rapid thermal annealing process is adopted, the annealing duration can be in the range between about 0.5 seconds to about 3.5 seconds. The annealing temperature can be in the range between about 700°C and about 850°C.
[0081] High-k dielectric layer 78HK'-L has a dipole dopant atomic percentage AP78-L greater than the dipole dopant atomic percentage AP78-U in high-k dielectric layer 78HK-U. High-k dielectric layer 78HK-U may or may not include a dipole dopant, depending on whether the deposited high-k dielectric layer 78HK-U includes a dipole dopant.
[0082] According to some embodiments, the difference in the dipole dopant atomic percentage (AP78-L-AP78-U) can be greater than about 0.5% and can be in a range between about 0.5% and about 10%. The desired dipole dopant atomic percentage AP78-L depends on the desired threshold voltage of the resulting NFET. The lower the threshold voltage of the desired NFET, the higher the dipole dopant atomic percentage AP78-L will be. The desired dipole dopant atomic percentage AP78-L is achieved by adjusting the thickness of the dipole film 82, and the greater the thickness, the higher the dipole dopant atomic percentage AP78-L.
[0083] The dipole film 82 is then removed in an isotropic etching process. The resulting structure is as follows Figure 12-6 As shown, the high-k dielectric layers 78HK-U and 78HK'-L are exposed.
[0084] Figure 12-7The formation of the gate electrode in the common process of the upper FET and the lower FET is shown. The corresponding process is shown as Fig.17 Process 244 in the process flow 200 shown. The gate dielectric 78 and the corresponding gate electrode 80 are collectively referred to as a gate stack 90, and the gate stack 90 includes an upper gate stack 90U and a lower gate stack 90L. The resulting upper FET 10U and lower FET 10L share a common gate electrode 80. The upper portion of the gate electrode 80 above the dielectric isolation layer 56 is referred to as the upper gate electrode 80U. The lower portion of the gate electrode below the dielectric isolation layer 56 is referred to as the lower gate electrode 80L.
[0085] The gate electrode 80 may include a plurality of layers including TiN, TaN, etc., and the gate electrode 80 may include one or more work function layers 80WF and a fill metal region 80FM. The thickness of each layer in the gate electrode 80 may be in a range between about 2 nm and about 5 nm. The fill metal region 80FM may include tungsten, ruthenium, cobalt, combinations thereof, multiple layers thereof, etc.
[0086] The work function layer 80WF surrounding each gate dielectric 78 may be physically separated from the work function layer 80WF surrounding other gate dielectrics 78. In this case, a fill metal region 80FM (such as tungsten, cobalt, etc.) may fill the space between the work function layers 80WF on adjacent gate dielectrics 78. Alternatively, the work function layer 80WF surrounding each gate dielectric 78 may be physically bonded to the work function layer 80WF surrounding other gate dielectrics 78.
[0087] According to some embodiments, the work function layer 80WF has a p-type work function higher than about 4.6 eV, and may be in a range between about 4.6 eV and about 5.2 eV. However, the n-type FET preferably has an n-type work function with a low work function value, such as less than about 4.5 eV, or between about 4.0 eV and about 4.5 eV. According to an embodiment of the present disclosure, as described above, this conflict is resolved by doping the high-k dielectric layer of the NFET with an n-type dipole dopant, thereby reducing the effective work function of the p-type work function layer in the NFET to the n-type work function range, such as in a range between about 4.0 eV and about 4.5 eV. On the other hand, the PFET is not doped with an n-type dipole dopant, and therefore its work function layer 80WF remains to have a p-type effective work function.
[0088] It should be understood that the dipole dopant diffuses from the dipole film 82, which is removed after the drive-in process. Accordingly, after removing the dipole film 82, the peak dipole dopant atomic percentage may occur at the outer surface of the high-k dielectric layer 78HK'-L that will contact the subsequently formed gate electrode 80. Fig.16Line 146 in illustratively shows the dipole dopant atomic percentage in the lower FET 10L as a function of position, where the dipole dopant distribution in the interface layer 78IL, the high-k dielectric layer 78HK, and the gate electrode 80 is shown. The peak dipole dopant atomic percentage may occur at the interface between the high-k dielectric layer 78 and the corresponding gate electrode 80, or may be slightly offset to the left or right, for example, by a distance less than about 1 nm. Moreover, the dipole dopant atomic percentage in the gate electrode 80 is steeper than the dipole dopant atomic percentage in the interface layer 78IL and the high-k dielectric layer 78HK.
[0089] Line 147 schematically shows the dipole dopant distribution in the upper FET 10U when the high-k dielectric layer 78HK (78HK-U) already includes n-type dipole dopants when it is deposited. Otherwise, line 147 will be located at the zero atomic percentage line. Line 147 can have a smooth top in the high-k dielectric layer 78HK (78HK-U), and the dips in the interface layer 78IL and the gate electrode 80 (80U) can have similar steepness.
[0090] Since the dipole film 82 is removed, there is no volume of the dipole film 82 in the resulting FET, and the dipole film 82 will not occupy the space between the nanostructures. By using the same material to form the gate electrodes of both the PFET and the NFET, it is no longer necessary to etch the gate electrode from the upper FET and then form the gate electrode of the upper FET again. The etching of the gate electrode may damage the high-k dielectric layer. Accordingly, according to the embodiments of the present disclosure, damage to the high-k dielectric layer is avoided due to the use of a common gate electrode.
[0091] Figure 13-1 to Figure 13-6 The formation of a CFET according to alternative embodiments is shown. These embodiments are similar to Figure 12-1 to Figure 12-7 The embodiment of the present invention is different from the embodiment of the present invention in that the dipole dopant is doped in situ (rather than ex situ) into the high-k dielectric layer 78HK. Unless otherwise specified, according to these embodiments (and Figure 14-1 to Figure 14-6 and Figure 15-1 to Figure 15-6 The materials, structure and formation process of the embodiment shown in FIG. Figure 12-1 to Figure 12-7 The embodiments shown are essentially the same and will not be repeated here.
[0092] refer to Figure 13-1, a gate dielectric 78 is formed in the upper FET region and the lower FET region. The formation of the gate dielectric 78 includes forming an interface layer 78IL, and depositing a high-k dielectric layer 78HK' (including 78HK'-U and 78HK'-L). The high-k dielectric layer 78HK' may include a high-k dielectric material such as hafnium, zirconium, barium, titanium, lead, or a combination thereof. During deposition, an n-type dipole dopant is in situ doped. For example, the n-type dipole dopant may include La, Sr, Y, Er, Sc, Mg, etc., or a combination thereof.
[0093] By introducing the n-type dipole dopant, the effective work function of the lower FET is inverted and falls within the range of n-type work functions. According to some embodiments, the atomic percentage of the dipole dopant in high-k dielectric layer 78HK' may be in a range between about 0.5% and about 10%.
[0094] refer to Figure 13-2 , forming a dummy fill region 84, and etch-back the dummy fill region 84 to mask the lower FET region while leaving the upper FET region unmasked. Figure 13-3 The high-k dielectric layer 78HK' in the upper FET region is shown removed by etching. Next, as Figure 13-4 As shown, a high-k dielectric layer 78HK-U is deposited in a conformal process. The high-k dielectric material in the high-k dielectric layer 78HK-U can be selected from the same candidate group as the material used to form the high-k dielectric layer 78HK'-L, and the high-k dielectric material in the high-k dielectric layer 78HK-U can be the same as or different from the high-k dielectric material in the high-k dielectric layer 78HK'-L. In addition, the high-k dielectric layer 78HK-U can be free of n-type dipole dopants, or optionally, in-situ doped with a small amount of n-type dopants. The total n-type dipole dopant atomic percentage in the high-k dielectric layer 78HK-U is lower than the total n-type dipole dopant atomic percentage in the high-k dielectric layer 78HK'-L. The n-type dipole dopant in the high-k dielectric layer 78HK-U (if in-situ doped) can be the same as or different from the n-type dipole dopant in the high-k dielectric layer 78HK'-L.
[0095] Figure 13-5 Removal of the dummy fill region 84 is shown, as well as removal of a portion of the high-k dielectric layer overlying the dummy fill region 84 .
[0096] Figure 13-6The formation of a common gate electrode 80 of a CFET is shown. The gate electrode 80 includes gate electrodes 80U and 80L formed in the same formation process. The resulting upper FET 10U is a PFET, and the lower FET 10L is an NFET. The effective work function of the lower FET 10L is reversed to have an n-type. The effective work function of the upper FET 10U is still of a p-type. Since the dipole dopant is in-situ doped, the dipole dopant can have a uniform atomic percentage when forming the high-k dielectric layer 78HK'-L. Figure 13-6 In the structure shown, the dipole dopant may have a peak atomic percentage in the corresponding high-k dielectric layer 78HK'-L (and possibly in the middle), similar to Fig.16 Line 147 in Figure 1. This peak may also be smoother than for diffused dipole dopants.
[0097] Figure 14-1 to Figure 14-2 The formation of a CFET according to yet another alternative embodiment is shown. These embodiments are similar to Figure 12-1 to Figure 12-7 , wherein the dipole dopant is ex situ doped. However, the dipole dopant is a p-type dopant and the work function layer of the resulting FET has an n-type work function, wherein the effective work function is adjusted by the dipole doping.
[0098] refer to Figure 14-1 , forming gate dielectric 78 (including 78U and 78L). High-k dielectric 78HK may be free of or substantially free of p-type dopants, as will be described in reference Figure 14-3 Next, Figure 14-2 As shown, a dummy fill region 84 is formed to mask the lower FET region while leaving the upper FET region open.
[0099] Then, a dipole film 82 is formed on the gate dielectric 78, such as Figure 14-3 As shown. The dipole film 82 includes a p-type dopant, which has the effect of increasing the effective work function of the resulting gate, and thus can increase the threshold voltage of the NFET and reduce the threshold voltage of the PFET. According to some embodiments, the p-type dipole dopant includes Al, Zn, Ga, etc. or a combination thereof. The atomic percentage of the p-type dipole dopant is sufficient to reverse the work function of the subsequently formed n-type work function layer and make the effective work function of the resulting gate PFET p-type.
[0100] refer to Figure 14-4, the dummy fill region 84 is removed, and the portion of the dipole film 82 on the dummy fill region 84 is also removed. An annealing process 88 is then performed to drive the dipole dopant into the corresponding underlying high-k dielectric layer, which is denoted as high-k dielectric layer 78HK'-U. The atomic percentage of the p-type dipole dopant in the high-k dielectric layer 78HK'-U may be in a range between about 0.5% and about 10%. On the other hand, the high-k dielectric layer 78HK-L has no dipole dopant diffused therein.
[0101] Figure 14-5 The dipole film 82 is shown removed by etching, thereby exposing the high-k dielectric layer 78HK'-U.
[0102] Figure 14-6 The formation of a common gate electrode 80 of a CFET is shown. The gate electrode 80 includes gate electrodes 80U and 80L formed in the same formation process. The resulting upper FET 10U is a PFET, and the lower FET 10L is an NFET. The work function layer 80WF has an n-type work function lower than about 4.5 eV, and may be in a range between about 4.0 eV and about 4.5 eV. The work function layer 80WF may include TiAl, TiAlN, AlN, etc. The effective work function of the upper FET 10U is inverted to have a p-type, and is higher than about 4.6 eV. The effective work function of the lower FET 10L still has an n-type.
[0103] Figure 15-1 to Figure 15-6 The formation of a CFET according to alternative embodiments is shown. These embodiments are similar to Figure 13-1 to Figure 13-6 The embodiment of FIG. 1 is different in that a p-type dipole dopant is in-situ doped instead of an n-type dopant. The work function layer of the resulting FET has an n-type work function.
[0104] refer to Figure 15-1 , a gate dielectric 78 is formed in the upper FET region and the lower FET region. The formation of the gate dielectric 78 includes forming an interface layer 78IL, and depositing a high-k dielectric layer 78HK (including 78HK-U and 78HK-L). The high-k dielectric layer 78HK may include a high-k dielectric material, such as hafnium, aluminum, zirconium, barium, titanium, lead, or a combination thereof. During deposition, no p-type dipole dopant is introduced in situ, or the p-type dipole dopant may be doped to a smaller atomic percentage. In the case where the high-k dielectric layer 78HK includes a p-type dopant, the atomic percentage of the p-type dopant is insufficient to invert the work function of the subsequently formed n-type work function layer to have a p-type effective work function.
[0105] refer to Figure 15-2 , forming a dummy fill region 84, and etch-back the dummy fill region 84 to mask the lower FET region while leaving the upper FET region unmasked. Figure 15-3The removal of the high-k dielectric layer 78HK in the upper FET region is shown. Next, as Figure 15-4 As shown, high-k dielectric layer 78HK'-U is deposited in a conformal process. The main high-k dielectric material in high-k dielectric layer 78HK'-U can be selected from the same candidate group as the material forming high-k dielectric layer 78HK-L, and can be the same as or different from the main high-k dielectric material in high-k dielectric layer 78HK-L. High-k dielectric layer 78HK'-U includes a p-type dipole dopant, and the p-type dipole dopant is in-situ doped during the deposition of high-k dielectric layer 78HK'-U. The total p-type dipole dopant atomic percentage in high-k dielectric layer 78HK'-U is higher than the total p-type dipole dopant atomic percentage in high-k dielectric layer 78HK-U, and can be in a range between about 0.5% and about 10%.
[0106] Figure 15-5 The removal of the dummy fill region 84 is shown, as well as the removal of the portion of the high-k dielectric layer 78HK′ on the dummy fill region 84 .
[0107] Figure 15-6 The formation of a common gate electrode 80 of a CFET is shown. The gate electrode 80 includes gate electrodes 80U and 80L formed in the same formation process. The resulting upper FET 10U is a PFET, and the lower FET 10L is an NFET. The effective work function of the upper FET 10U is reversed to have a p-type. The effective work function of the lower FET 10L still has an n-type. Since the p-type dipole dopant is in-situ doped, it can have a uniform atomic percentage when forming the high-k dielectric layer 78HK'-U. Figure 15-6 In the structure shown, the p-type dipole dopant may have Fig.16 The profile of line 147 in FIG. 14 is similar to the profile of line 147. The peak may also be smoother than for diffused dipole dopants.
[0108] Fig. 10A and Fig. 10B A cross-sectional view of an exemplary CFET formed in a previous process is shown. The common gate electrode 80 includes an upper electrode 80U and a lower electrode 80L, which are formed in the process and using the materials described above.
[0109] exist Fig. 10A and Fig. 10B In the embodiment of the present invention, a gate mask 92 is formed over the gate stack 90. The formation process may include recessing the gate stack 90, filling the resulting recess with a dielectric material such as silicon nitride, silicon carbonitride, silicon oxynitride, silicon carbon oxynitride, etc., and performing a planarization process to remove excess portions of the dielectric material over the second ILD 72.
[0110] Next, refer to Fig.11, silicide regions 94 and source / drain contact plugs 96U are formed to be electrically coupled to the source / drain regions 62U.
[0111] Embodiments of the present disclosure have some advantageous features. The same work function material (which may be a p-type work function material or an n-type work function material) is used to form both the PFET and the NFET in the same CFET structure. By doping a dipole dopant (such as an n-type dipole dopant or a p-type dopant) into the gate dielectric of one of the PFET and the NFET in situ or ex situ, the effective work function of one of the PFET and the NFET is inverted to have a desired value.
[0112] According to some embodiments, a method includes forming a first semiconductor channel region and a second semiconductor channel region, wherein the second semiconductor channel region overlaps the first semiconductor channel region; forming a first gate dielectric on the first semiconductor channel region; forming a second gate dielectric on the second semiconductor channel region; introducing a dipole dopant into a first gate dielectric of the first gate dielectric and the second gate dielectric to a higher atomic percentage, wherein the second gate dielectric of the first gate dielectric and the second gate dielectric has a lower atomic percentage of the dipole dopant; and forming a gate electrode on both the first gate dielectric and the second gate dielectric, wherein the gate electrode and the first gate dielectric form part of a first transistor, and the gate electrode and the second gate dielectric form part of a second transistor.
[0113] In an embodiment, introducing the dipole dopant comprises: depositing a dipole film on the first gate dielectric and the second gate dielectric; removing the dipole film from the second gate dielectric; driving the dipole dopant into the first gate dielectric; and removing the dipole film. In an embodiment, introducing the dipole dopant is performed in situ when depositing the first gate dielectric and the second gate dielectric.
[0114] In an embodiment, the first gate dielectric is deposited to have a lower atomic percentage of a dipole dopant, and the method further comprises replacing the second gate dielectric with another gate dielectric having a higher atomic percentage of a dipole dopant. In an embodiment, the first gate dielectric is deposited to have a higher atomic percentage of a dipole dopant, and the method further comprises replacing the second gate dielectric with another gate dielectric having a lower atomic percentage of a dipole dopant.
[0115] In an embodiment, the gate electrode comprises a p-type metal, and wherein the dipole dopant is an n-type dipole dopant. In an embodiment, the gate electrode comprises an n-type metal, and wherein the dipole dopant is a p-type dipole dopant. In an embodiment, the first transistor is an n-type transistor, and the second transistor is a p-type transistor. In an embodiment, the dipole dopant is an n-type dopant selected from the group consisting of La, Sr, Y, Er, Sc, Mg, and combinations thereof. In an embodiment, the dipole dopant is a p-type dopant selected from the group consisting of Al, Zn, Ga, and combinations thereof.
[0116] In accordance with some embodiments, a structure includes a lower transistor, the lower transistor including a first channel region; a first gate dielectric located on the first channel region, wherein the first gate dielectric has a first atomic percentage of a dipole dopant; and a first gate electrode located on the first gate dielectric; and an upper transistor, wherein a first transistor of the lower transistor and the upper transistor is an n-type transistor, and wherein a second transistor of the lower transistor and the upper transistor is a p-type transistor, and wherein the upper transistor includes a second channel region overlapping the first channel region; a second gate dielectric located on the second channel region, wherein the second gate dielectric has a second atomic percentage of a dipole dopant, and wherein the second atomic percentage is different from the first atomic percentage; and a second gate electrode located on the second gate dielectric, wherein the first gate electrode and the second gate electrode are portions of the same continuous gate electrode.
[0117] In an embodiment, the first transistor is an n-type transistor and the second transistor is a p-type transistor. In an embodiment, the dipole dopant is an n-type dopant selected from the group consisting of La, Sr, Y, Er, Sc, Mg and combinations thereof. In an embodiment, the dipole dopant is a p-type dopant selected from the group consisting of Al, Zn, Ga and combinations thereof. In an embodiment, the first gate dielectric and the second gate dielectric include the same high-k dielectric material. In an embodiment, the first gate dielectric and the second gate dielectric include different high-k dielectric materials.
[0118] In accordance with some embodiments, a structure includes a lower transistor comprising a first channel region; a first gate dielectric located on the first channel region, wherein the first gate dielectric includes a high-k dielectric material; and a first source / drain region connected to the first channel region; and an upper transistor comprising a second channel region overlapping the first channel region; a second gate dielectric located on the second channel region, wherein the second gate dielectric includes a high-k dielectric material and a dipole dopant, wherein a first atomic percentage of the dipole dopant in the first gate dielectric is lower than a second atomic percentage of the dipole dopant in the second gate dielectric; and a second source / drain region connected to the second channel region, wherein the second source / drain region overlaps the first source / drain region, and wherein the first source / drain region and the second source / drain region have opposite conductivity types.
[0119] In an embodiment, the dipole dopant is an n-type dopant selected from the group consisting of Sr, Y, Er, Sc, Mg and combinations thereof. In an embodiment, the structure further comprises a common gate electrode extending continuously from a first level below the first channel region to a second level above the second channel region, wherein the common gate electrode and the first source / drain region and the second source / drain region form a first transistor and a second transistor, respectively. In an embodiment, the high-k dielectric material comprises hafnium oxide.
[0120] The features of several embodiments are summarized above so that those skilled in the art can better understand aspects of the present disclosure. Those skilled in the art should understand that they can easily use the present disclosure as a basis to design or modify other processes and structures for implementing the same purpose and / or achieving the same advantages as the embodiments introduced herein. Those skilled in the art should also appreciate that such equivalent constructions do not deviate from the spirit and scope of the present disclosure, and that they can make various changes, substitutions, and modifications herein without departing from the spirit and scope of the present disclosure.
Claims
1. A method for forming a semiconductor structure, comprising: forming a first semiconductor channel region and a second semiconductor channel region, wherein the second semiconductor channel region overlaps the first semiconductor channel region; forming a first gate dielectric on the first semiconductor channel region; forming a second gate dielectric on the second semiconductor channel region; introducing a dipole dopant into a first gate dielectric of the first gate dielectric and the second gate dielectric to a higher atomic percentage, wherein a second gate dielectric of the first gate dielectric and the second gate dielectric has a lower atomic percentage of the dipole dopant; and A gate electrode is formed on both the first gate dielectric and the second gate dielectric, wherein the gate electrode and the first gate dielectric form part of a first transistor and the gate electrode and the second gate dielectric form part of a second transistor.
2. The method according to claim 1, wherein: The introducing the dipole dopant comprises: depositing a dipole film on the first gate dielectric and the second gate dielectric; removing the dipole film from the second gate dielectric; driving the dipole dopant into the first gate dielectric; and The dipole film is removed.
3. The method according to claim 1, wherein: The introducing the dipole dopant is performed in-situ during deposition of the first gate dielectric and the second gate dielectric.
4. The method according to claim 1, wherein: The first gate dielectric is deposited to have the lower atomic percentage of the dipole dopant, and the method further includes replacing the second gate dielectric with another gate dielectric having the higher atomic percentage of the dipole dopant.
5. The method according to claim 1, wherein: While depositing the first gate dielectric having the higher atomic percentage of the dipole dopant, the method further includes replacing the second gate dielectric with another gate dielectric having the lower atomic percentage of the dipole dopant.
6. The method according to claim 1, wherein: The gate electrode includes a p-type metal, and wherein the dipole dopant is an n-type dipole dopant.
7. The method according to claim 1, wherein: The gate electrode comprises an n-type metal, and wherein the dipole dopant is a p-type dipole dopant.
8. The method according to claim 1, wherein: The first transistor is an n-type transistor, and the second transistor is a p-type transistor.
9. A semiconductor structure comprising: a lower transistor, the lower transistor comprising: a first channel region; a first gate dielectric on the first channel region, wherein the first gate dielectric has a first atomic percent of a dipole dopant; and a first gate electrode disposed on the first gate dielectric; and an upper transistor, wherein the lower transistor and a first transistor of the upper transistor are n-type transistors, and wherein the lower transistor and a second transistor of the upper transistor are p-type transistors, and wherein the upper transistor comprises: a second channel region, overlapping the first channel region; a second gate dielectric on the second channel region, wherein the second gate dielectric has a second atomic percentage of the dipole dopant, and wherein the second atomic percentage is different from the first atomic percentage; and A second gate electrode is disposed on the second gate dielectric, wherein the first gate electrode and the second gate electrode are parts of a same continuous gate electrode.
10. A semiconductor structure comprising: a lower transistor, the lower transistor comprising: a first channel region; a first gate dielectric disposed on the first channel region, wherein the first gate dielectric comprises a high-k dielectric material; and a first source / drain region connected to the first channel region; and an upper transistor, the upper transistor comprising: a second channel region, overlapping the first channel region; a second gate dielectric located on the second channel region, wherein the second gate dielectric comprises the high-k dielectric material and a dipole dopant, wherein a first atomic percentage of the dipole dopant in the first gate dielectric is lower than a second atomic percentage of the dipole dopant in the second gate dielectric; and A second source / drain region is connected to the second channel region, wherein the second source / drain region overlaps the first source / drain region, and wherein the first source / drain region and the second source / drain region have opposite conductivity types.