Method of forming charge layer using gas phase and liquid phase coating
By using gas- and liquid phase coating and dopant diffusion treatment on semiconductor substrates, an efficient charge layer is formed, which solves the problem of reduced efficiency caused by high-temperature treatment, and achieves efficient charge manipulation capabilities and quantum efficiency improvements. It is suitable for Large aspect ratio structure.
Patent Information
- Application Number
- CN202380026767.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-22
- Filing Date
- 2023-03-14
- Publication Date
- 2024-11-01
AI Technical Summary
High temperature treatment can damage the surrounding devices and form a large charge gradient area during the block processing of the semiconductor substrate, resulting in reduced efficiency.
The non-solid-phase doped layer and oxide layer containing dopants are formed at a temperature less than 450°C by gas-phase and liquid phase coating. The work function of the substrate structure is adjusted by dopant diffusion treatment to form a steep junction profile. and charge layer, a controllable oxide layer is formed using a dry oxidation treatment, and an etching process is performed in the later stage process to improve charge manipulation capability.
It significantly improves the charge manipulation capability of the structural surface, increases quantum efficiency, avoids crystal damage and thermal budget limitations, is compatible with high-deep aspect ratio structures greater than 50:1, and is not sensitive to the surface state.
Smart Images

Figure CN118891699A_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present invention generally relate to semiconductor processing of semiconductor substrates. Background Art
[0002] Structures such as trenches are often formed on substrates as part of building semiconductor devices. Bulk processing and elevated temperatures are often used to change the work function of the structure. However, the inventors have discovered that during such processing, elevated temperatures can damage surrounding devices and also cause large charge gradient regions to be formed in the structure, reducing the area available for other device layers, resulting in a substantial reduction in performance.
[0003] Thus, the inventors have provided an improved process for forming a charge layer that substantially increases the performance and quantum efficiency of the structure without requiring surface modification prior to performing such a process. Summary of the invention
[0004] Provided herein are methods and structures for modified charge layers using vapor and liquid phase coating.
[0005] In some embodiments, a method for adjusting the work function of a structure on a substrate may include coating a surface of the structure to form a non-solid phase doping layer containing dopants on the surface of the structure, and performing a dopant diffusion process using an oxidation process to drive the dopants through the surface of the structure and bury the dopants in the structure to adjust the work function of the structure near the surface to form a steep junction profile and form an oxide layer on the surface of the structure.
[0006] In some embodiments, the method may further include wherein the oxidation treatment is a dry oxidation treatment, wherein the oxidation treatment is a wet oxidation treatment, the method is performed without prior modification of the crystal formation of the surface of the structure, wherein the surface of the structure is coated using vapor phase coating, wherein the surface of the structure is coated using liquid phase coating, the method is performed at a temperature of less than 450° C., wherein the dopant diffusion treatment produces up to positive or negative about 1e16 / cm in the surface of the structure. 3 to about 1e20 / cm 3 A method of forming a doped layer on a substrate comprising: forming a sacrificial oxide layer on a surface of the structure using a dry oxide process at a temperature of less than about 450° C., the sacrificial oxide layer having a controllable oxide thickness of about 1 nm to about 15 nm, and selectively removing the sacrificial oxide layer from the surface of the structure before coating the surface of the structure to form a doped layer, wherein the dry oxide process is performed in a plasma oxidation chamber, and / or etching the structure into the substrate to a high aspect ratio of greater than about 75:1.
[0007] In some embodiments, a method for adjusting the work function of a structure on a substrate may include coating a surface of the structure with a plasma-based process to form a gas-phase doping layer containing dopants on the surface of the structure, and performing a dopant diffusion process using a dry oxidation process to drive the dopants through the surface of the structure and bury the dopants in the structure to adjust the work function of the structure near the surface and form an oxide layer on the surface of the structure, wherein the dopant diffusion process is performed at less than approximately 450° C. and a charge layer having a steep junction profile is formed.
[0008] In some embodiments, the method may further include wherein the dopant diffusion process produces up to positive or negative about 1e16 / cm in the surface of the structure. 3 to about 1e20 / cm 3 A method of forming a structure having a charge of 0.05 W, wherein the dopant is P-type or N-type, the method being performed in a back-end-of-line (BEOL) process, the method being performed without modifying the crystal formation of the surface of the structure, and / or forming the structure using an etching process, forming a sacrificial oxide layer on the surface of the structure using a dry oxide process at a temperature of less than about 450° C., the sacrificial oxide layer having a controllable oxide thickness of about 1 nm to about 15 nm, and selectively removing the sacrificial oxide layer from the surface of the structure before coating the surface of the structure to form a vapor phase doping layer.
[0009] In some embodiments, a non-transitory computer-readable medium has instructions stored thereon that, when executed, cause a method for adjusting the work function of a structure in a substrate to be performed, the method may include coating a surface of the structure to form a non-solid doping layer containing dopants on the surface of the structure, and performing a dopant diffusion process using an oxidation process to drive the dopants through the surface of the structure to bury the dopants in the structure to adjust the work function of the structure near the surface to form a steep junction profile and form an oxide layer on the surface of the structure.
[0010] In some embodiments, the non-transitory computer readable medium may cause the method to further include wherein the dopant diffusion process produces up to positive or negative about 1e16 / cm in the surface of the structure. 3 to about 1e20 / cm 3 The invention relates to a method for coating a surface of a structure by applying a vapor coating or a liquid coating to the structure.
[0011] Other and further embodiments are disclosed hereinafter. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Embodiments of the invention briefly summarized above and discussed in more detail below may be understood by reference to the exemplary embodiments of the invention depicted in the accompanying drawings. However, the drawings depict only typical embodiments of the invention and are therefore not to be considered limiting in scope, as the invention may admit to other equally effective embodiments.
[0013] Figure 1 A method of adjusting a charge layer of a surface of a structure in a substrate according to some embodiments of the present invention.
[0014] Figure 2A Depicted is a cross-sectional view of a structure after an etching process according to some embodiments of the present invention.
[0015] Figure 2B Depicted is a cross-sectional view of a structure after an optional dry oxide treatment according to some embodiments of the present invention.
[0016] Figure 2C Depicted is a cross-sectional view of a structure after an optional selective oxide removal process according to some embodiments of the present invention.
[0017] Figure 2D Depicted is a cross-sectional view of a structure after forming a coating or doping layer according to some embodiments of the present invention.
[0018] Figure 2E Depicted is a cross-sectional view of a structure after oxidation according to some embodiments of the present invention.
[0019] Figure 2F Depicted is a cross-sectional view of a structure after formation of an oxide layer according to some embodiments of the present invention.
[0020] Figure 3 An integration tool according to some embodiments of the present invention is depicted.
[0021] To facilitate understanding, identical reference numerals have been used wherever possible to refer to identical components shared among the figures. The illustrations are not drawn to scale and may be simplified for clarity. Components and features of one embodiment may be beneficially incorporated into other embodiments without further clarification. DETAILED DESCRIPTION
[0022] The present method provides a high-efficiency charge layer formation scheme that significantly increases the charge manipulation capabilities in the surface of a structure. The method provides innovative dopant and junction formation with precise profile control using vapor and liquid phase processing without the thermal budget and surface state limitations found in traditional processing. The present technology enables the formation of steep junctions with extremely high activation doping close to the surface without crystal damage. In addition, the technology allows for use in back-end of line (BEOL) processing without thermal damage to existing structures on the substrate. The method is also compatible with the surfaces of high aspect ratio structures greater than 50:1. The technology of the present invention is capable of low to high activation doping levels while maintaining a low thermal budget of less than 450°C and while being insensitive to surface states. In addition, vapor phase processing allows for high conformality in high aspect ratio structures.
[0023] Although grooves are used as "structures" in the examples that follow for simplicity, other structures may benefit from the methods of the present invention, and thus the use of grooves in the examples is not intended to be limiting. For example, the techniques of the present invention may also be used for planar structures. Figure 1 1 is a method 100 of adjusting the work function of a charge layer or structure 204 in a substrate 202 according to some embodiments. In block 102, in some embodiments, for example, an etching process forms the structure 204 into the substrate 202, such as Figure 2A 200A of FIG. 100. The etching process typically uses a hard mask layer 212 that protects areas from the etching process. In some embodiments, the aspect ratio of the structure 204 is at least about 50:1. In some embodiments, the aspect ratio of the structure 204 is at least about 75:1. In some embodiments, the aspect ratio of the structure 204 is at least about 100:1. As a side effect of the etching process, damage 208 occurs on the surface 206 of the structure 204. The damage 208 may include crystalline damage to the substrate material, contaminants or residues from the etching process, and / or dangling bonds and the like of the substrate material. The hard mask layer 212 is removed after the etching process is completed. The method of the present invention has the advantage and ability to be performed directly on a damaged or unclean surface of the structure 204 (performing block 102 and proceeding directly to block 108 of method 100). However, for completeness, the method may also be performed on an undamaged and clean surface, as described in optional blocks 104 and 106.
[0024] In optional block 104, to further prepare structure 204, in some embodiments, a dry oxidation process is used to form an oxide layer 216 on substrate 202 as a sacrificial layer. Figure 2BAs depicted in view 200B of , a field 214 or top surface of the substrate 202 and a surface 206 of the structure 204 undergo a dry oxidation process to form an oxide layer 216 that partially consumes material of the substrate 202 including damaged portions. The dry oxidation process can be performed at a temperature of less than 450° C. and produces less contamination and residue than a wet oxidation process. In addition, the dry oxidation process can be used with substantially higher aspect ratio structures (e.g., greater than 100:1 aspect ratio) than wet oxidation (e.g., less than 50:1 aspect ratio). In some embodiments, the dry oxidation process is performed in a plasma oxidation chamber with or without a remote plasma source. The dry oxidation process facilitates burying oxygen into the surface 206 of the substrate 204 to repair damage to the surface 206 and to reduce stress induced leakage current (SILC) and interface trap density (D it ).
[0025] The dry oxidation process can also be controlled to provide oxide layer 216 of varying thickness. Parameters such as exposure time, plasma density, temperature, and the like can help determine the oxidation rate. The thickness is then controlled by the duration of the dry oxidation process. In conventional methods such as wet oxidation, the oxidation process is self-limiting (wet oxidation processes are self-terminating) and the oxide layer thickness cannot be adjusted. Wet oxidation typically stops at a saturation point (self-limiting) at a thickness of 1 nm to 2 nm. Dry oxidation does not have a saturation point and is not self-limiting, allowing any degree of thickness to be obtained. In some embodiments, the dry oxidation process can achieve greater than 95% conformality in structure 204 for structures having aspect ratios greater than 100:1, enabling the use of the present invention to shrink isolation structures.
[0026] In optional block 106, in some embodiments, oxide layer 216 is selectively removed from surface 206 of structure 204 and field 214 of substrate 202, such as Figure 2C 200C. In some embodiments, a plasma-based chamber can be used to selectively remove the oxide layer 216 at a selectivity ratio of, for example, greater than 50:1 (e.g., oxide to Si or SiGe). The selective removal of the oxide layer 216 removes all of the oxide layer 216 without damaging any underlying material of the substrate 202 or creating contaminants / residues, leaving an undamaged and clean surface of the structure 204. In block 108, the surface 206 of the structure 204 is coated using a gas phase or liquid phase process to form a doped layer 210 having a dopant 222 on the surface of the structure 204, such as Figure 2D As previously described, this coating and treatment is not sensitive to surface conditions and can be applied to damaged or unclean surfaces of structure 204 (e.g., Figure 2Asurface 206) and an undamaged and clean surface of structure 204 (e.g., Figure 2C surface 206).
[0027] The surface insensitivity of this process enables great flexibility without adding complexity to the process when it is not needed. In some embodiments, a gas phase process can be performed to deposit dopants 222 on the surface 206 of the structure 204 by using a plasma-based process and a process gas. The gas phase dopant deployment on the surface 206 is limited by the subsequent dry oxidation process used to diffuse the dopant 222 into the surface 206. The gas phase dopant deployment provides a higher conformality on the surface 206, especially in high aspect ratio structures. The pressure can be adjusted to allow the gas phase dopant to be formed on the surface with higher conformality when the pressure is increased. In some embodiments, a liquid phase process produces a wet layer of dopant 222 on the surface 206 of the structure 204. The liquid phase dopant deployment on the surface 206 is compatible with the subsequent dry oxidation process and wet oxidation process used to diffuse the dopant 222 into the surface 206. The coating or doping layer 210 of the surface 206 may have a thickness 232 of less than 1 nanometer and down to an atomic layer thickness.
[0028] The species of dopant 222 (illustrated as a P-type species but not intended to be limited thereto) may be incorporated to form a positive or negative charge on substrate 202 (e.g., doping silicon with boron, gallium, phosphorus, arsenic, etc.). The density of dopant 222 and / or the type of dopant 222 may be adjusted to provide a given positive or negative charge level required for structure 204. In block 110, structure 204 is oxidized to diffuse dopant 222 into surface 206 to adjust the work function of structure 204 and form an oxide layer. The work function of structure 204 is adjusted by varying the dopant density, dopant type, and dopant depth. The density of dopant 222 and / or the type of dopant 222 may be adjusted to provide a given positive or negative charge level and a given work function required for structure 204. A higher work function close to the surface may promote or increase carrier mobility within adjacent structures such as pixel structures and reduce susceptibility to surface recombination. The top technology allows substantial flexibility in work function engineering through adjustment of dopant depth, density, and type, while increasing adjacent structure area by using steep junction profiles.
[0029] After deposition of the dopant using a vapor or liquid phase process, a dopant diffusion process 224 is performed on the structure 204, such as Figure 2E200E. In some embodiments, the dopant diffusion process 224 can be a dry oxidation process performed in a plasma oxidation chamber and the like. The dry oxidation process is compatible with both gas phase and liquid phase processes for diffusing dopants into the surface 206 of the substrate 204. In some embodiments, the dopant diffusion process 224 can be a wet oxidation process that is compatible with liquid phase processes for diffusing dopants into the surface 206 of the substrate 204. In practice, without an annealing process, the doped layer 210 produces the liner layer 230 and the buried charge layer 226, as shown in FIG. Figure 2F As depicted in view 200F.
[0030] In contrast to conventional techniques that form a graded charge region that requires more area adjacent to a structure to be used, thereby reducing the effectiveness of adjacent structures, the dopant diffusion process 224 produces a steep charge boundary or a steep junction profile or a steep composition transition in the material of the substrate 202 that increases the effective area of adjacent structures (e.g., pixel structure areas, etc.). As used herein, by definition, a steep junction is a junction where the dopant concentration changes at a very small distance from the surface compared to the spatial extent to which the dopant can be diffused. In some embodiments, the charge layer 226 may have a charge formation of up to about 1e16 / cm2, positive or negative. 3 to about 1e20 / cm 3 , depending on the allowed temperature and pressure. The charge layer 226 of the present invention can achieve the treated activation level without any post-activation treatment. In the optional area 112, additional back-end of line (BEOL) compatible thermal treatment or annealing treatment can be performed after oxidation. In some embodiments, the above treatment can be performed without air break to avoid surface impurities, contaminants, and / or particle generation.
[0031] The methods described herein may be performed in individual process chambers, which may be provided as stand-alone configurations or as part of a cluster tool, for example, as described hereinafter with reference to Figure 3 The integrated tool 300 (i.e., cluster tool) is described. An advantage of using the integrated tool 300 is that there is no vacuum break and therefore no need to degas and pre-clean the substrate prior to processing in the chamber. For example, in some embodiments, the inventive method described above can be advantageously performed in an integrated tool so that there is limited or no vacuum break between processing, limiting or avoiding contamination of the substrate. The integrated tool 300 includes a vacuum-enclosed processing platform 301, a factory interface 304, and a system controller 302. The processing platform 301 includes a plurality of processing chambers, such as 314A, 313B, 314C, 314D, 314E, and 314F, operatively coupled to a vacuum substrate transfer chamber (transfer chambers 303A, 303B). The factory interface 304 is coupled to the processing platform 301 via one or more load lock chambers (two load lock chambers, such as Figure 3 306A and 306B) are operatively coupled to transfer chamber 303A.
[0032] In some embodiments, the factory interface 304 includes at least one docking station 307 and at least one factory interface robot 338 to facilitate the transfer of semiconductor substrates. The docking station 307 is configured to receive one or more front opening wafer transport boxes (FOUPs). Four FOUPs, such as 305A, 305B, 305C, and 305D are shown in FIG. Figure 3 In an embodiment of the present invention, the factory interface robot 338 is configured to transfer substrates from the factory interface 304 through the load lock chambers (such as 306A and 306B) to the processing platform 301. Each of the load lock chambers 306A and 306B has a first port coupled to the factory interface 304 and a second port coupled to the transfer chamber 303A. The load lock chambers 306A and 306B are coupled to a pressure control system (not shown) that pumps back and evacuates the load lock chambers 306A and 306B to facilitate the transfer of substrates between the vacuum environment of the transfer chamber 303A and the substantially ambient (e.g., atmospheric pressure) environment of the factory interface 304. The transfer chambers 303A, 303B have vacuum robots 342A, 342B disposed in the respective transfer chambers 303A, 303B. The vacuum robot 342A can transfer the substrate 321 between the load lock chambers 306A, 306B, the processing chambers 314A and 314F, and the cooling station 340 or the pre-cleaning station 342. The vacuum robot 342B can transfer the substrate 321 between the cooling station 340 or the pre-cleaning station 342 and the processing chambers 314B, 314C, 314D, and 314E.
[0033] In some embodiments, processing chambers 314A, 314B, 314C, 314D, 314E, and 314F are coupled to transfer chambers 303A, 303B. Processing chambers 314A, 314B, 314C, 314D, 314E, and 314F may include, for example, atomic layer deposition (ALD) processing chambers, physical vapor deposition (PVD) processing chambers, chemical vapor deposition (CVD) chambers, annealing chambers, or the like. The chambers may include any chamber suitable for performing all or part of the methods described herein, such as dry oxide removal chambers or pre-clean chambers and etch and deposition chambers, as described above. In some embodiments, one or more optional service chambers (illustrated as 316A and 316B) may be coupled to transfer chamber 303A. Service chambers 316A and 316B may be configured to perform other substrate processing, such as degassing, orientation, substrate measurement, cooling, and the like.
[0034] The system controller 302 controls the operation of the tool 300, either by directly controlling the processing chambers 314A, 314B, 314C, 314D, 314E, and 314F, or by controlling a computer (or controller) associated with the processing chambers 314A, 314B, 314C, 314D, 314E, and 314F and the tool 300. In operation, the system controller 302 is capable of collecting data and feedback from the respective chambers and systems to optimize the performance of the tool 300. The system controller 302 generally includes a central processing unit (CPU) 330, a memory 334, and support circuits 332. The CPU 330 may be any form of general purpose computer processor that may be used in an industrial setting. The support circuits 332 are conventionally coupled to the CPU 330 and may include cache, clock circuits, input / output subsystems, power supplies, and the like. Software routines, such as the methods described above, may be stored in memory 334 and, when executed by CPU 330, transform CPU 330 into a special purpose computer (system controller) 302. Software routines may also be stored and / or executed by a second controller (not shown) that is remote from tool 300.
[0035] Embodiments according to the present invention may be implemented in hardware, firmware, software, or any combination of the foregoing. Embodiments may also be implemented as instructions stored using one or more computer-readable media, which may be read and implemented by one or more processors. Computer-readable media may include any mechanism for storing or transmitting information in a machine-readable form (e.g., a computing platform or a "virtual machine" running on one or more computing platforms). For example, a computer-readable medium may include any suitable form of volatile or non-volatile memory. In some embodiments, a computer-readable medium may include a non-transient computer-readable medium.
[0036] While the foregoing is directed to embodiments of the present invention, other and further embodiments of the invention may be devised without departing from the basic scope of the invention.
Claims
1. A method for adjusting the work function of a structure on a substrate, comprising the following steps: coating a surface of the structure to form a non-solid phase doping layer containing a dopant on the surface of the structure, wherein the structure has an aspect ratio of at least 50:1; and An oxidation process is used to perform a dopant diffusion process to drive the dopant through the surface of the structure and bury the dopant in the structure to adjust the work function of the structure near the surface to form a steep junction profile and an oxide layer on the surface of the structure.
2. The method of claim 1, wherein the oxidation treatment is a dry oxidation treatment.
3. The method of claim 1, wherein the oxidation treatment is a wet oxidation treatment.
4. The method of claim 1, performed without previously modifying the crystal formation of the surface of the structure.
5. The method of claim 1, wherein vapor coating is used to coat the surface of the structure.
6. The method of claim 1, wherein the surface of the structure is coated using liquid phase coating.
7. The method of claim 1, performed at a temperature less than 450°C.
8. The method of claim 1, wherein the dopant diffusion process produces up to positive or negative about 1e16 / cm in the surface of the structure. 3 to about 1e20 / cm 3 of charge.
9. The method of claim 1, further comprising the steps of: forming the structure using an etching process; forming a sacrificial oxide layer on the surface of the structure at a temperature less than about 450° C. using a dry oxide process, the sacrificial oxide layer having a controllable oxide thickness of about 1 nm to about 15 nm; and The sacrificial oxide layer is selectively removed from the surface of the structure before coating the surface of the structure to form the doped layer.
10. The method of claim 9, wherein the dry oxide treatment is performed in a plasma oxidation chamber.
11. The method of claim 9, further comprising the steps of: The structure is etched into the substrate to a high aspect ratio of greater than about 75:
1.
12. A method for adjusting the work function of a structure on a substrate, comprising the steps of: coating a surface of the structure with a plasma-based process to form a vapor-phase doped layer containing a dopant on the surface of the structure; and A dopant diffusion process is performed using a dry oxidation process to drive the dopants through the surface of the structure and bury the dopants in the structure to adjust the work function of the structure close to the surface and form an oxide layer on the surface of the structure, wherein the dopant diffusion process is performed at less than approximately 450° C. and forms a charge layer with a steep junction profile.
13. The method of claim 12, wherein the dopant diffusion process produces a dopant diffusion in the surface of the structure of up to positive or negative about 1e16 / cm 3 to about 1e20 / cm 3 of charge. The method of claim 12 , wherein the dopant is P-type or N-type.
15. The method of claim 12, performed in a back-end-of-line (BEOL) process.
16. The method of claim 12, performed without previously modifying the crystal formation of the surface of the structure.
17. The method of claim 12, further comprising the steps of: forming the structure using an etching process; forming a sacrificial oxide layer on the surface of the structure at a temperature less than about 450° C. using a dry oxide process, the sacrificial oxide layer having a controllable oxide thickness of about 1 nm to about 15 nm; and The sacrificial oxide layer is selectively removed from the surface of the structure before coating the surface of the structure to form the vapor phase doping layer.
18. A non-transitory computer readable medium having instructions stored thereon, said instructions when executed causing a method of adjusting a work function of a structure in a substrate to be performed, said method comprising the steps of: coating the surface of the structure to form a non-solid phase doping layer containing dopants on the surface of the structure; and An oxidation process is used to perform a dopant diffusion process to drive the dopant through the surface of the structure and bury the dopant in the structure to adjust the work function of the structure near the surface to form a steep junction profile and an oxide layer on the surface of the structure.
19. The non-transitory computer readable medium of claim 18, wherein the dopant diffusion process produces a dopant diffusion process in the surface of the structure of up to positive or negative about 1e16 / cm 3 to about 1e20 / cm 3 of charge and forms the steep junction profile.
20. The non-transitory computer readable medium of claim 18, wherein the surface of the structure is coated using vapor coating or liquid coating.