Butt-joint-free method for electroplating process clamp and heating device for butt-joint-free method

By heating the contact chuck on the heating plate, it is melted and contacted with the surface mask of the silicon wafer. This solves the problem that electroplating fixtures need to be repeatedly tested in the existing technology, improves the contact accuracy and fault tolerance, and is suitable for photovoltaic mass production application.

CN118910709APending Publication Date: 2024-11-08WUXI KINGENIOUS INTELLIGENT EQUIPMENT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411141545.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing electroplating fixtures need to be repeatedly tested when contacting the copper seed layer of the silicon wafer, and the docking accuracy is difficult to ensure, resulting in low usage efficiency.

Method used

The contact chuck is heated by a heating plate so that it can be made to contact with the surface mask of the silicon wafer after melting, so that the exposed area of ​​the grip points is not required to directly contact the copper seed layer, which improves contact accuracy and fault tolerance.

Benefits of technology

It realizes efficient conductivity without reserved clamp exposed areas, reduces the accuracy requirements of the clamp structure of the electroplating fixture, and improves the installation compactness and processing efficiency of silicon wafers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118910709A_ABST
    Figure CN118910709A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of photovoltaic cells, and particularly relates to a butt-joint-free method for an electroplating process clamp and a heating device used in the butt-joint-free method. According to the butt-joint-free method for the electroplating process clamp and the heating device for the butt-joint-free method, the contact chuck is heated through the heating plate, after the contact chuck is heated to a certain temperature, the heated contact chuck is used for melting a mask in the contact area of the contact chuck on a battery piece to be plated, and then the contact chuck is heated to a certain temperature; according to the method and the device, the contact chuck is in contact with the copper seed layer at the bottom of the mask on the surface of the to-be-electroplated battery piece in the corresponding area of the to-be-electroplated battery piece, so that the contact between the contact chuck and the copper seed layer of the silicon wafer does not need to reserve a pinch point exposed area; the contact chuck clamps the to-be-plated battery piece and melts the mask on the surface of the to-be-plated battery piece to conduct with the copper seed layer at the same time, the requirement for the precision of the clamping point structure of the electroplating clamp is low, the error-tolerant rate is high, silicon wafers are installed more compactly, and the number and efficiency of processed silicon wafers are higher.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of photovoltaic cells, and in particular relates to a docking-free method for an electroplating process fixture, and a heating device used in the method. Background Art

[0002] Electroplating is the process of plating a thin layer of other metals or alloys on certain metal surfaces using the principle of electrolysis. It is a process that uses electrolysis to attach a layer of metal film to the surface of metal or other material parts, thereby preventing metal oxidation (such as rust), improving wear resistance, conductivity, reflectivity, corrosion resistance (copper sulfate, etc.) and enhancing aesthetics. The general steps are as follows: assemble the electroplating tank, prepare the anode, prepare the electroplating solution, place the silicon wafer in the fixture, power on, and power off as needed. The fixture is a necessary device in this process, and the probe on the fixture is used to contact the copper seed layer on the silicon wafer to achieve conductivity.

[0003] The Chinese utility model patent with patent announcement number CN220189586U and announcement date 2023-12-15 discloses a sliding shaft type conductive clamping basket structure, which includes a first fixed plate, a second fixed plate, an electrode sheet, a connected spring sheet, a sliding shaft, a fixed shaft, a silicon sheet, a first clamping point, and a second clamping point.

[0004] The general structural principle of the sliding shaft type conductive clamping basket structure in this utility model patent is as follows: when in use, the sliding shaft is pushed by external force to move relative to the fixed shaft, so that the first clamping point on the sliding shaft and the second clamping point on the fixed shaft are separated, and then the silicon wafer is inserted. After the force is removed, the first clamping point is reset and closes to the second clamping point, so that the silicon wafer is positioned and clamped, and the first clamping point on the basket contacts the reserved clamping point exposed area on the silicon wafer, thereby conducting electricity.

[0005] However, the flower basket structure still has at least the following deficiencies in actual use, in other words, these are the technical problems to be solved by the present invention.

[0006] The first clamping point must be in contact with the exposed area of ​​the silicon wafer reserved for the clamping point to conduct electricity. Repeated attempts to align the points are required, and the final docking accuracy is difficult to guarantee.

[0007] Therefore, in summary, there is an urgent need for a docking-free method that uses a more efficient copper electroplating process and does not require repeated attempts to dock the clamp point with the silicon wafer. Summary of the invention

[0008] The present invention provides a docking-free method for an electroplating process fixture and a heating device for the method. The contact clamp is heated by a heating plate. After being heated to a certain temperature, the heated contact clamp is used to melt the mask on the battery cell to be plated in the contact area with the contact clamp, so that the contact clamp can contact the copper seed layer at the bottom of the mask on the surface of the battery cell to be plated in the corresponding area of ​​the battery cell to be plated. The method and device make the contact between the contact clamp and the copper seed layer of the silicon wafer without reserving a clamping point exposed area. The contact clamp clamps the battery cell to be plated and melts the mask on the surface of the battery cell to be plated to conduct electricity with the copper seed layer. The requirements for the precision of the clamping point structure of the electroplating fixture are low, the fault tolerance rate is high, the silicon wafer installation is more compact, and the number and efficiency of processing silicon wafers are higher.

[0009] The technical solution adopted by the present invention to solve the above-mentioned problem is: a docking-free method for electroplating process fixtures, separating two contact clamps; inserting a heating plate between the two contact clamps; closing the two contact clamps so that the contact clamps clamp the heating plate, and the heating plate heats the contact clamps; separating the two contact clamps again and removing the heating plate; inserting a battery cell to be plated between the two heated contact clamps; closing the two contact clamps so that when the contact clamps clamp the surface of the battery cell to be plated, the contact area between the contact clamps and the mask on the surface of the battery cell to be plated is first melted, and then contacts the copper seed layer.

[0010] A further preferred technical solution is that the heating plate is made of any one of aluminum alloy, stainless steel, ceramic, and carbon fiber materials.

[0011] A further preferred technical solution is that the material of the surface mask of the cell to be plated is any one of wax, photosensitive ink, photosensitive dry film, and hot melt adhesive, and the thickness of the surface mask of the cell to be plated is 5um-40um.

[0012] A further preferred technical solution is that when the contact clamp melts the mask on the surface of the cell to be plated, the temperature of the contact clamp is not less than 45°C.

[0013] A further preferred technical solution is that the time required for the heating plate to heat the contact clamp is 3S-15S.

[0014] A heating device for a docking-free method for an electroplating process fixture comprises the heating plate.

[0015] A further preferred technical solution is that it also includes a mounting plate arranged at the bottom of the heating plate.

[0016] A further preferred technical solution is that it also includes a limiting frame arranged on the mounting plate and used to clamp the heating plate.

[0017] A further preferred technical solution is that it also includes an integral bottom plate arranged at the lower end of the mounting plate.

[0018] A further preferred technical solution is that it also includes a mounting hole arranged on the mounting plate, and an adjustment hole arranged on the integral bottom plate and used to connect the mounting hole. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a stereogram of the present invention.

[0020] Figure 2 It is a schematic diagram of the state of the contact clamp heating the battery sheet to be plated in the present invention.

[0021] Figure 3 It is a three-dimensional picture of an existing battery cell with clamping points to be plated.

[0022] Figure 4 It is a three-dimensional diagram of the battery cell to be plated in the present invention.

[0023] Figure 5 It is a three-dimensional diagram of the heating plate in the present invention.

[0024] Figure 6 It is a partial enlarged view of A in the present invention.

[0025] Figure 7 It is a position structure diagram of the contact clamp in the present invention.

[0026] Figure 8 It is a partial cross-sectional view of the mask on the surface of the cell to be plated by the contact clamp in the present invention.

[0027] Fig. 9 This is a schematic diagram of the contact clamp melting the mask on the surface of the cell to be plated when the heating temperature is insufficient in the present invention.

[0028] Fig.10 This is a partial cross-sectional view of the contact clamp melting the surface mask of the battery cell to be plated when the surface mask material of the battery cell to be plated is other materials or the thickness is too large in the present invention.

[0029] Fig.11 It is a three-dimensional diagram of the connection of the flower basket in the present invention.

[0030] In the figure, the meanings of the symbols are as follows: A cell to be plated a, a surface mask a-1 of the cell to be plated, a copper seed layer a-2, a silicon wafer base layer a-3, and a reserved pinch point exposed area b; Contact chuck 11, flower basket 12; Heating plate 1, mounting plate 2, limiting frame 3, integral bottom plate 4, mounting hole 5, adjusting hole 6. DETAILED DESCRIPTION

[0031] The following descriptions are merely preferred embodiments of the present invention and are not intended to limit the scope of the present invention.

[0032] Embodiment 1 As attached Figure 1-11 As shown, a docking-free method for an electroplating process fixture comprises the following steps in sequence: S1, separate the two contact clamps 11; S2, inserting the heating plate 1 between the two contact clamps 11; S3, closing the two contact clamps 11, so that the contact clamps 11 clamp the heating plate 1, and the heating plate 1 performs a heating operation on the contact clamps 11; S4, separating the two contact clamps 11 again, and moving the heating plate 1 out; S5, inserting the cell a to be plated between the two heated contact clamps 11; S6. Close the two contact clamps 11 so that when the contact clamps 11 clamp the cell a to be plated, the contact area between the contact clamps 11 and the surface mask a-1 of the cell to be plated is melted first, and then contacts the copper seed layer a-2.

[0033] In this embodiment, in the related technology of preparing copper grid lines by copper electroplating process, it is necessary to first form a layer of copper seed layer a-2 on the surface of silicon wafer base layer a-3, then form the surface mask a-1 of the cell to be plated on the surface of copper seed layer, and then perform copper electroplating process with mask as protection to form copper grid lines on the surface of cell a to be plated. In the copper electroplating process, electroplating fixture is usually used to load the cell a to be plated and cathode current is passed to the cell to be plated area (i.e. non-mask area) through the electroplating fixture. As shown in the attached figure, Figure 3 As shown, in the prior art, for the cell a to be plated that has been masked, since the mask is made of insulating material, the reserved clamping point exposed area b (i.e., Pad clamping point area) on the mask is generally used to allow the conductive clamping points on the electroplating fixture to contact the reserved clamping point exposed area b and thus contact and conduct with the copper seed layer a-2 to achieve effective electrification of the cell area to be plated. Considering that in mass production in the photovoltaic industry, the basket clamp needs to be equipped with more clamping points to carry dozens or hundreds of silicon wafers for electroplating, in order to ensure that all the cell a to be plated can be stably energized during electroplating, this requires extremely high docking accuracy between the basket clamping points and the reserved clamping point exposed area b. In the prior art, the docking accuracy between the flower basket clamping point and the reserved clamping point exposed area b (Pad point) is generally improved by improving the processing accuracy of the flower basket clamping point or the area of ​​the reserved clamping point exposed area b. However, in actual production, it is difficult to control the processing accuracy of multiple clamping points in the flower basket clamp within an appropriate range, and increasing the area of ​​the Pad clamping point area will affect the appearance and efficiency of the final battery cell.

[0034] As attached Figure 4 and attached Figure 8 The present application heats the contact clamp by a heating plate, and after heating to a certain temperature, the heated contact clamp 11 is used to melt the surface mask a-1 of the cell to be plated in the contact area with the contact clamp on the cell to be plated a, so that the contact clamp 11 can contact the copper seed layer a-2 in the corresponding area of ​​the cell to be plated a, and realize stable conductivity of the cell to be plated area. The present application has low precision requirements on the clamping structure of the electroplating fixture, high fault tolerance, and a higher number and efficiency of processing silicon wafers, which is more suitable for photovoltaic mass production applications.

[0035] In addition, the specific steps of the docking-free method for the electroplating process fixture are: after separating the two contact clamps 11, place the heating plate 1 between the two contact clamps 11, and then close the two contact clamps 11 so that the contact clamps 11 clamp the heating plate 1, and the heating plate 1 heats the contact clamps 11. After heating to a certain temperature, separate the two contact clamps 11 again and remove the heating plate 1. To avoid the clamping point temperature from dropping, the battery cell a to be plated should be placed between the two heated contact clamps 11 within 30S of removing the heating plate 1, and close the two contact clamps 11 so that the contact clamps 11 melt the surface mask a-1 of the battery cell to be plated, and then contact the copper seed layer a-2.

[0036] The heating plate 1 in S2 is made of any one of aluminum alloy, stainless steel, ceramic, and carbon fiber materials.

[0037] In this embodiment, the heating plate 1 is made of a common heating plate material, such as aluminum alloy, stainless steel, ceramic or carbon fiber material, etc. The temperature of the heating plate 1 is between 60°C and 200°C to quickly conduct heat to the contact clamp 11.

[0038] The material of the surface mask a-1 of the cell to be plated in S6 is any one of wax, photosensitive ink, photosensitive dry film, and hot melt adhesive, and the thickness of the surface mask a-1 of the cell to be plated is 5um-40um.

[0039] In this embodiment, the material of the surface mask a-1 of the cell to be plated is wax, photosensitive ink, photosensitive dry film or hot melt adhesive, so that the heated contact clamp 11 can melt and contact the copper seed layer a-2 after contacting the surface mask a-1 of the cell to be plated. Since the temperature of the contact clamp 11 comes from the heating plate 1, in order to ensure that the contact clamp 11 can better melt the surface mask a-1 of the cell to be plated, in order to avoid the temperature of the contact clamp 11 from dropping, the cell a to be plated should be placed within 30 seconds after removing the heating plate 1. In addition, if the surface mask a-1 of the battery cell to be plated is too thick, it is difficult for the contact clamp 11 to melt the surface mask a-1 of the battery cell to be plated. If the surface mask a-1 of the battery cell to be plated is too thin, the high temperature of the contact clamp 11 may easily damage the battery cell a to be plated, and the surface mask a-1 of the battery cell to be plated may easily be scratched during transportation and installation, resulting in damage to the copper seed layer a-2. Therefore, the thickness of the surface mask a-1 of the battery cell to be plated is preferably between 5um and 40um.

[0040] When the contact clamp 11 melts the surface mask a-1 of the cell to be plated in S6, the temperature of the contact clamp 11 is not lower than 45°C.

[0041] In this embodiment, the contact clamp 11 should be no lower than 45°C. When the temperature is above 60°C and 80°C-90°C, the melting efficiency and product service life reach the optimal level; if the contact clamp 11 is lower than 45°C, the melting effect of the mask a-1 on the surface of the cell to be plated is poor, which affects the contact between the contact clamp 11 and the copper seed layer a-2, and further affects the electroplating effect.

[0042] The time required for the heating plate 1 to heat the contact clamp 11 is 3S-15S.

[0043] In this embodiment, the contact clamp 11 needs to melt the surface mask a-1 of the cell to be plated, and only after melting can it contact the copper seed layer a-2 of the bottom layer, so the temperature of the contact clamp 11 needs to reach the melting temperature of the surface mask a-1 of the cell to be plated, and the heating plate 1 needs to heat the contact clamp 11, and use the residual temperature of the contact clamp 11 after being heated to melt the surface mask a-1 of the cell to be plated. If the heating time of the heating plate 1 to heat the contact clamp 11 is too short, the residual temperature may not be able to completely melt the surface mask a-1 of the cell to be plated in contact with it, and the process stability is poor; if the heating time is too long, the high temperature of the contact clamp 11 will increase the temperature of the flower basket body and make the cell to be plated a as a whole in a higher temperature atmosphere, which will not only melt the mask in contact with it, but also damage the mask pattern, so the heating time is controlled to be 3S-15S for the best.

[0044] The heating device used in the docking-free method for the electroplating process fixture comprises the heating plate 1.

[0045] In this embodiment, the function of the heating plate 1 is to heat the contact clamp 11 so that the contact clamp 11 melts the mask a-1 on the surface of the cell to be plated. The temperature of the heating plate 1 is controlled between 60°C and 200°C. If the temperature is too low, the temperature of the heated contact clamp 11 is too low, and the mask cannot be melted stably. If the temperature is too high, it will have an adverse effect on the life of the fixture, energy consumption, wax morphology, etc. The heating time of the contact clamp 11 is reasonably adjusted according to the temperature of the heating plate 1 to ensure the process effect.

[0046] It also includes a mounting plate 2 arranged at the bottom of the heating plate 1 .

[0047] In this embodiment, the mounting plate 2 is arranged at the bottom of the heating plate 1, and each heating plate 1 is arranged as a whole, which is convenient for overall installation and disassembly.

[0048] It also includes a limiting frame 3 which is arranged on the mounting plate 2 and is used to clamp the heating plate 1 .

[0049] In this embodiment, the limiting frame 3 is arranged on the mounting plate 2 to clamp the heating plate 1. The heating plate 1 is located in a slot formed by two adjacent limiting frames 3. The two ends of the limiting frame 3 can well support the heating plate 1 to ensure the verticality and stability of the heating plate 1.

[0050] It also includes an integral bottom plate 4 arranged at the lower end of the mounting plate 2 .

[0051] In this embodiment, the integral bottom plate 4 is used to connect the mounting plate 2, and the other end of the integral bottom plate 4 can be connected to a power line to heat the heating plate 1. It also includes a mounting hole 5 arranged on the mounting plate 2 , and an adjustment hole 6 arranged on the integral bottom plate 4 and used for connecting the mounting hole 5 .

[0052] In this embodiment, the arrangement of the mounting holes 5 and the adjusting holes 6 enables the heating plate 1 arranged on the mounting plate 2 to move relative to the integral bottom plate 4, thereby heating the contact clamp 11 more flexibly.

[0053] Embodiment 2 Compared with the first embodiment, the difference lies in that when the surface mask a-1 of the cell to be plated is hot melt adhesive, the heating plate 1 heats the contact clamp 11 for 5 seconds, and the temperature of the contact clamp 11 is 60°C.

[0054] On the contrary, when the surface mask a-1 of the cell to be plated is a mask of inorganic materials, such as silicon nitride, silicon oxide, aluminum oxide, etc., due to the special material, the high temperature of the contact clamp 11 cannot melt the surface mask a-1 of the cell to be plated, so that the contact clamp 11 cannot contact the copper seed layer a-2.

[0055] Embodiment 3 Compared with the first embodiment, the difference lies in that the thickness of the mask a-1 on the surface of the cell to be plated is 10 um, the time for the heating plate 1 to heat the contact clamp 11 is 5 seconds, and the temperature of the contact clamp 11 is 80°C.

[0056] On the contrary, when the thickness of the mask a-1 on the surface of the cell to be plated is 50 um, Fig.10 As shown, when the temperature of the contact clamp 11 is 80° C., the contact clamp 11 has a poor effect in melting the mask a-1 on the surface of the cell to be plated, which makes it difficult for the contact clamp 11 to contact the copper seed layer a-2 and results in low melting efficiency.

[0057] Embodiment 4 Compared with the first embodiment, the difference is that the heating plate 1 is made of aluminum alloy. When its own temperature is 80°C, the temperature of the contact clamp 11 after heating is 79°C. The contact clamp 11 is not lower than 75°C, which can well melt the surface mask a-1 of the battery cell to be plated.

[0058] On the contrary, when the material of the heating plate 1 is a polymer material, due to its poor thermal conductivity, its own temperature is difficult to be higher than 40°C while ensuring the clamping ability. When it further heats the contact clamp 11, the temperature of the contact clamp 11 is difficult to be higher than 40°C, and it is impossible to melt the surface mask a-1 of the battery cell to be plated.

[0059] Embodiment 5 Compared with the first embodiment, the difference is that when the temperature of the temperature heating plate 1 is 90° C. and the material of the surface mask a-1 of the cell to be plated is wax, the temperature heating plate 1 heats the contact clamp 11 for 5S.

[0060] On the contrary, when the temperature of the heating plate 1 is 50°C and the material of the surface mask a-1 of the cell to be plated is wax, there is energy loss in the process of heating the contact clamp 11. The temperature of the contact clamp 11 when melting the surface mask a-1 of the cell to be plated is about 40°C. Fig. 9 As described above, due to the low temperature of the contact clamp 11, the melting effect of the mask a-1 on the surface of the cell to be plated is poor, and incomplete melting and residue are prone to occur, resulting in unstable contact between the contact clamp 11 and the copper seed layer a-2, affecting the conductive effect.

[0061] Embodiment 6 Compared with the first embodiment, the difference lies in that the temperature of the heating plate 1 is 90° C., the time required for the heating plate 1 to heat the contact clamp 11 is 3 seconds, and the temperature of the contact clamp 11 is 60° C.

[0062] On the contrary, when the time required for the heating plate 1 to heat the contact clamp 11 is 1S, the temperature of the contact clamp 11 is 50°C, and heat loss occurs during the process of placing the cell a to be plated, resulting in the temperature of the contact clamp 11 being lower than 45°C. The residual temperature of the contact clamp 11 cannot completely melt the surface mask a-1 of the cell to be plated that is in contact with it. Fig. 9 or attached Fig.10 As shown, the heating plate 1 does not heat the contact clamp 11 for an adequate time, causing the temperature of the contact clamp 11 to fail to meet the required melting temperature, resulting in poor melting effect of the surface mask a-1 of the cell to be plated and poor process stability.

[0063] The embodiments of the present invention are described in detail above in conjunction with the accompanying drawings, but the present invention is not limited to the above embodiments. Various modifications can be made within the knowledge of ordinary technicians in the technical field without departing from the purpose of the present invention. These are all non-creative modifications and are protected by patent law as long as they are within the scope of the claims of the present invention.

Claims

1. A docking-free method for electroplating process fixtures, characterized in that The following steps are included in sequence: S1, separate the two contact clamps (11); S2, extending the heating plate (1) between the two contact clamps (11); S3, closing the two contact clamps (11) so that the contact clamps (11) clamp the heating plate (1), and the heating plate (1) performs a heating operation on the contact clamps (11); S4, separating the two contact clamps (11) again, and removing the heating plate (1); S5, inserting the battery sheet (a) to be plated between the two heated contact clamps (11); S6. Close the two contact clamps (11) so that when the contact clamps (11) clamp the cell to be plated (a), the contact area between the contact clamps (11) and the surface mask (a-1) of the cell to be plated is first melted, and then contacts the copper seed layer (a-2).

2. The docking-free method for an electroplating process fixture according to claim 1, characterized in that: The heating plate (1) in S2 is made of any one of aluminum alloy, stainless steel, ceramic, and carbon fiber materials.

3. The docking-free method for an electroplating process fixture according to claim 1, characterized in that: The material of the surface mask (a-1) of the cell to be plated in S6 is any one of wax, photosensitive ink, photosensitive dry film, and hot melt adhesive, and the thickness of the surface mask (a-1) of the cell to be plated is 5um-40um.

4. The docking-free method for an electroplating process fixture according to claim 1, characterized in that: When the contact clamp (11) in S6 melts the surface mask (a-1) of the cell to be plated, the temperature of the contact clamp (11) is not less than 45°C.

5. The docking-free method for electroplating process fixture according to claim 1, characterized in that: The time required for the heating plate (1) to heat the contact clamp (11) is 3S-15S.

6. A heating device for a docking-free method for an electroplating process fixture according to any one of claims 1 to 5, characterized in that: The structure comprises the heating plate (1).

7. The heating device for the docking-free method for the electroplating process fixture according to claim 6, characterized in that: It also includes a mounting plate (2) arranged at the bottom of the heating plate (1).

8. The heating device for the docking-free method for the electroplating process fixture according to claim 7, characterized in that: It also includes a limiting frame (3) which is arranged on the mounting plate (2) and is used to clamp the heating plate (1).

9. The heating device for the docking-free method for the electroplating process fixture according to claim 7, characterized in that: It also includes an integral bottom plate (4) arranged at the lower end of the mounting plate (2).

10. The heating device for the docking-free method for the electroplating process fixture according to claim 9, characterized in that: It also includes a mounting hole (5) arranged on the mounting plate (2), and an adjustment hole (6) arranged on the integral bottom plate (4) and used to connect to the mounting hole (5).