Lithium precipitation detection method and device, electronic equipment and computer readable storage medium
By analyzing the voltage-capacity curve, differential curve and voltage-time curve of lithium-ion batteries, combined with the charge-resistance curve, the lithium-ion battery performance of non-destructive detection is achieved, and the existing destructive detection method is solved The problem has improved the accuracy and safety of detection.
Patent Information
- Application Number
- CN202411130626.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-16
- Publication Date
- 2024-11-08
AI Technical Summary
The existing lithium-ion detection method is a destructive detection method based on disassembly, and cannot effectively detect the lithium-ion evolution of lithium-ion batteries, affecting the safety of the battery.
By obtaining the first voltage-capacity curve and the second voltage-capacity curve of the lithium-ion battery, combining the differential curve to analyze the difference in characteristic peak positions, combining the voltage-time curve and the state-of-charge-resistance curve, the lossless analysis based on electrical data is achieved. Lithium detection.
Non-destructive testing of lithium-ion battery lithium-ion battery is achieved, the accuracy and reliability of battery safety detection is improved, and damage caused by battery disassembly is avoided.
Smart Images

Figure CN118914883A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to lithium plating detection, and in particular to a lithium plating detection method, device, electronic device and computer-readable storage medium. Background Art
[0002] Lithium-ion batteries are widely used in both consumer and power fields. In particular, the development of the new energy vehicle industry and the growing demand in the power field have directly driven the expansion and growth of upstream battery and material companies. Lithium plasmosis is a common phenomenon in the use of lithium-ion batteries. Lithium plasmosis refers to the phenomenon that during the charging process of lithium-ion batteries, lithium ions are released from the positive electrode and cannot be normally embedded in the negative electrode, and electrons are obtained on the surface of the negative electrode to form metallic lithium. Lithium plasmosis will seriously affect the safety of lithium-ion batteries. However, the current lithium plasmosis detection method is a destructive detection method based on disassembly. Therefore, it is urgent to provide a non-destructive lithium plasmosis detection method to detect lithium plasmosis in lithium-ion batteries. Summary of the invention
[0003] The embodiments of the present application provide a lithium plating detection method, device, electronic device, and computer-readable storage medium, which can non-destructively detect the lithium plating of a lithium-ion battery.
[0004] In a first aspect, the present application provides a lithium deposition detection method, comprising:
[0005] Discharging the battery to be detected after first charging it at a first charging rate, and obtaining a first voltage-capacity curve of the battery to be detected during the discharge process;
[0006] Performing cyclic charge-discharge aging on the battery to be tested at a second charge rate; the second charge rate is greater than the first charge rate;
[0007] charging and then discharging the battery to be detected after cyclic charge and discharge aging at the first charging rate, and obtaining a second voltage-capacity curve of the battery to be detected during the discharge process;
[0008] A first lithium plating detection result of the battery to be detected is obtained according to the first voltage-capacity curve and the second voltage-capacity curve.
[0009] In one embodiment, obtaining a first lithium deposition detection result of the battery to be detected according to the first voltage-capacity curve and the second voltage-capacity curve includes:
[0010] Differentiating the first voltage-capacity curve to obtain a first dV / dQ-Q curve, and differentiating the second voltage-capacity curve to obtain a second dV / dQ-Q curve;
[0011] When the distance between the position of the characteristic peak of the first dV / dQ-Q curve and the position of the characteristic peak of the second dV / dQ-Q curve is greater than a preset distance, it is determined that the first lithium deposition detection result of the battery to be detected is that lithium deposition exists.
[0012] In one embodiment, it also includes:
[0013] The control battery is charged for the first time at a first charge rate and then discharged, and a third voltage-capacity curve of the control battery is obtained during the discharge process; the control battery and the battery to be tested are batteries from the same batch;
[0014] Performing cyclic charge-discharge aging on the control battery at a third charge rate;
[0015] charging and then discharging the control battery after cyclic charge-discharge aging at the first charge rate, and obtaining a fourth voltage-capacity curve of the battery to be tested during the discharge process;
[0016] Differentiating the third voltage-capacity curve to obtain a third dV / dQ-Q curve, and differentiating the fourth voltage-capacity curve to obtain a fourth dV / dQ-Q curve;
[0017] The distance between the position of the characteristic peak of the third dV / dQ-Q curve and the position of the characteristic peak of the fourth dV / dQ-Q curve is determined as the preset distance.
[0018] In one embodiment, it also includes:
[0019] charging the battery to be detected after cyclic charge-discharge aging at the second charging rate and then letting it stand, and obtaining a voltage-time curve of the battery to be detected during the standing process;
[0020] A second lithium deposition detection result of the battery to be detected is obtained according to the voltage-time curve.
[0021] In one embodiment, obtaining a second lithium deposition detection result of the battery to be detected according to the voltage-time curve includes:
[0022] Differentiating the voltage-time curve to obtain a dV / dt-t curve;
[0023] When the dV / dt-t curve has a platform, it is determined that the second lithium deposition test result of the battery to be tested is that lithium deposition exists.
[0024] In one embodiment, before the battery to be tested is subjected to cyclic charge-discharge aging at a second charge rate, the method further comprises:
[0025] Performing constant current charging on the battery to be detected at the second charging rate, and obtaining a state of charge-resistance curve of the battery to be detected during the constant current charging process;
[0026] A third lithium plating detection result of the battery to be detected is obtained according to the state of charge-resistance curve.
[0027] In one embodiment, the step of obtaining a third lithium deposition detection result of the battery to be detected according to the state of charge-resistance curve includes:
[0028] When there is no minimum value in the state of charge-resistance curve, it is determined that the third lithium deposition detection result of the battery to be detected is that lithium deposition exists.
[0029] In one embodiment, it also includes:
[0030] When the first lithium deposition test result, the second lithium deposition test result and the third lithium deposition test result all indicate that lithium deposition exists, it is determined that lithium deposition exists in the battery to be tested.
[0031] In one embodiment, there are multiple batteries to be tested, and the second charging rates of the multiple batteries to be tested are different. The method further includes:
[0032] Performing a first charge and discharge operation on a control battery at a first charge rate, and obtaining a third voltage-capacity curve of the control battery during the discharge process; the control battery and the battery to be tested are batteries from the same batch;
[0033] Wherein, when the first voltage-capacity curve and the third voltage-capacity curve are consistent, the step of performing cyclic charge-discharge aging on the battery to be tested at a second charge rate is performed.
[0034] In a second aspect, the present application provides a lithium deposition detection device, comprising:
[0035] A first voltage-capacity curve acquisition module, used to charge and discharge the battery to be detected for the first time at a first charging rate, and acquire a first voltage-capacity curve of the battery to be detected during the discharge process;
[0036] A first aging control module, used for performing cyclic charge-discharge aging on the battery to be tested at a second charging rate; the second charging rate is greater than the first charging rate;
[0037] A second voltage-capacity curve acquisition module is used to charge and then discharge the battery to be detected after cyclic charge-discharge aging at the first charging rate, and obtain a second voltage-capacity curve of the battery to be detected during the discharge process;
[0038] The first result acquisition module is used to acquire a first lithium plating detection result of the battery to be detected according to the first voltage-capacity curve and the second voltage-capacity curve.
[0039] In a third aspect, the present application provides an electronic device, including a memory and a processor, wherein the memory stores a computer program, and when the computer program is executed by the processor, the processor executes the steps of the lithium plating detection method as described above.
[0040] In a fourth aspect, the present application provides a computer-readable storage medium having a computer program stored thereon, wherein the computer program implements the steps of the above method when executed by a processor.
[0041] In a fifth aspect, the present application provides a computer program product, including a computer program, which implements the steps of the above method when executed by a processor.
[0042] The above-mentioned lithium plating detection method, device, electronic device, and computer-readable storage medium can determine the initial state of the battery to be detected by obtaining the data of the first charge and discharge cycle of the battery to be detected. After the aging process of cyclic charge and discharge aging, by using the same charging parameters as the first charge and discharge cycle to perform a charge and discharge cycle on the battery to be detected again, it is possible to analyze whether the second charging rate used in the cyclic charge and discharge aging process will cause lithium plating in the battery based on the voltage-capacity curve of the charge and discharge cycle before and after aging, thereby realizing a non-destructive lithium plating detection method based on electrical property data. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0044] Figure 1 This is one of the flow charts of a lithium deposition detection method according to an embodiment;
[0045] Figure 2 is a sub-flow chart of step 104 of an embodiment;
[0046] Figure 3 A first dV / dQ-Q curve of each battery in an embodiment;
[0047] Figure 4 A second dV / dQ-Q curve of each battery of an embodiment;
[0048] Figure 5This is a second flow chart of a lithium deposition detection method according to an embodiment;
[0049] Figure 6 dV / dt-t curves of each battery in an embodiment;
[0050] Figure 7 is a state of charge-resistance curve of each battery of an embodiment;
[0051] Figure 8 The negative electrode interface diagram obtained by disassembling the control battery and the battery to be tested;
[0052] Fig. 9 Schematic diagram of the structure of a lithium deposition detection device according to an embodiment. DETAILED DESCRIPTION
[0053] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0054] In the related art, whether lithium plating occurs in the battery is mainly confirmed by disassembling the fully charged battery and observing the morphology of the negative electrode. However, the disassembly process necessarily requires the destruction of the battery, so it is a destructive test. Therefore, it is urgent to provide a non-destructive lithium plating detection method. The lithium plating detection method of the embodiment of the present application can be applied to lithium-ion batteries whose positive electrode materials are any one of lithium cobalt oxide (LCO), lithium manganese oxide (LMO), lithium nickel oxide (LNO), and lithium iron phosphate (LFP). In addition, the negative electrode material of the lithium-ion battery can be, but is not limited to, any one of graphite, lithium metal, silicon carbon, oxide, etc., and this application does not limit it.
[0055] Figure 1 This is one of the flow charts of a lithium deposition detection method according to an embodiment, referring to Figure 1 In one embodiment, the lithium plating detection method includes steps 101 to 104.
[0056] Step 101 , charging a battery to be tested for the first time at a first charging rate and then discharging the battery to be tested, and obtaining a first voltage-capacity curve of the battery to be tested during the discharging process.
[0057] Among them, the first charging rate can be understood as a charging rate that is not easy to cause lithium precipitation in the battery. Specifically, the first charging rate can be a lower charging rate. Under low-rate charging conditions, due to the small current, the number of lithium ions reaching the negative electrode per unit time is small, which allows the negative electrode to have enough time and space to accommodate these lithium ions, and the charge transfer and diffusion process is relatively slow, which also helps the lithium ions to be more smoothly embedded in the negative electrode material, thereby reducing the occurrence of lithium precipitation. Exemplarily, the first charging rate can be 0.05C, 0.1C, etc. After the battery is discharged to empty after charging, it can be considered that a charge and discharge cycle is completed. In this embodiment, by obtaining the data of the first charge and discharge cycle of the battery to be detected, the initial state of the battery to be detected can be determined, so as to facilitate the analysis of the lithium precipitation of the battery in combination with subsequent detection data. Further, before the battery to be detected is charged for the first time at the first charging rate, the battery to be detected can be discharged at a preset rate to ensure that the state of the battery before the first charging is stable and controllable. Among them, the emptying rate can be 0.05C, for example.
[0058] Step 102, performing cyclic charge-discharge aging on the battery to be tested at a second charge rate.
[0059] Among them, the second charging rate is greater than the first charging rate, and the second charging rate may be a charging rate that may cause lithium deposition in the battery. Specifically, the second charging rate may be greater than 1.5C, such as 1.5C, 1.6C, 2C, 2.5C, etc. Cyclic charge and discharge aging refers to performing multiple charge and discharge cycles on the battery continuously. The number of charge and discharge cycles can be determined according to the needs of the electronic equipment using the battery, such as 30 cycles, 100 cycles, 300 cycles, etc. Specifically, since lithium deposition is a phenomenon that occurs during the charging process of the battery, the parameters of each discharge process of the battery to be tested can be controlled to be the same to reduce the variables in the detection process, thereby improving the accuracy of the detection results. Exemplarily, discharge can be performed at a rate of 0.05C in each charge and discharge cycle.
[0060] Step 103 , charging and then discharging the battery to be detected after cyclic charge and discharge aging at a first charging rate, and obtaining a second voltage-capacity curve of the battery to be detected during the discharge process.
[0061] The parameter selection in the charge-discharge cycle of this step is the same as that in step 101, for example, the battery to be tested is charged to full at a first charge rate of 0.05C by constant current charging, and then the battery to be tested is discharged to empty at a rate of 0.05C. Based on the above method, the difference between the second voltage-capacity curve and the first voltage-capacity curve can reflect the lithium deposition of the battery to be tested during the cyclic charge-discharge aging process.
[0062] Step 104: Obtain a first lithium plating detection result of the battery to be detected according to the first voltage-capacity curve and the second voltage-capacity curve.
[0063] Among them, the first lithium deposition test result is one of the presence of lithium deposition and the absence of lithium deposition in the battery to be tested. It can be understood that if the first voltage-capacity curve and the second voltage-capacity curve match, it means that there is no performance change or very little change in the battery to be tested during the cyclic charge and discharge aging process, that is, it can be considered that lithium deposition has not occurred in the battery to be tested. If the first voltage-capacity curve and the second voltage-capacity curve match, it means that there is a performance change in the battery to be tested during the cyclic charge and discharge aging process, but it should be noted that the above performance changes may not be caused by lithium deposition, so it is necessary to conduct a more specific analysis of the voltage-capacity curve, or combine other data for comprehensive judgment, so as to improve the accuracy of lithium deposition detection.
[0064] In the embodiment of the application, the initial state of the battery to be detected can be determined by obtaining the data of the first charge and discharge cycle of the battery to be detected. After the aging process of cyclic charge and discharge aging, the battery to be detected is subjected to a charge and discharge cycle again using the same charging parameters as the first charge and discharge cycle. Based on the voltage-capacity curve of the charge and discharge cycle before and after aging, it can be analyzed whether the second charging rate used in the cyclic charge and discharge aging process will cause lithium deposition in the battery, thereby realizing a non-destructive lithium deposition detection method based on electrical property data.
[0065] In one embodiment, there are multiple batteries to be tested, and the second charging rates of the multiple batteries to be tested are different. Among them, the multiple batteries to be tested are batteries from the same batch. That is, the structures and preparation conditions of the multiple batteries to be tested are the same, so that the difference in the test results can better reflect the impact of different second charging rates on lithium precipitation. Exemplarily, the different second charging rates can be 1.6C and 2.5C, for example. By performing cyclic charge and discharge aging on the corresponding batteries to be tested at different second charging rates, multiple second voltage-capacity curves can be obtained. Therefore, when obtaining the first lithium precipitation test result, it is necessary to compare the first voltage-capacity curve and the second voltage-capacity curve of the same battery to be tested to obtain the lithium precipitation conditions under each second charging rate.
[0066] In one embodiment, the method further includes charging and discharging the control battery for the first time at a first charging rate, and obtaining a third voltage-capacity curve of the control battery during the discharge process. Wherein, the control battery and the battery to be tested are batteries from the same batch. That is, the structure and preparation conditions of the battery to be tested and the control battery are the same. Similar to the battery to be tested, before the control battery is charged for the first time at the first charging rate, the control battery can be discharged at a preset rate to ensure that the state of the battery before the first charging is stable and controllable. Further, when the first voltage-capacity curve and the third voltage-capacity curve are consistent, the step of cyclic charge and discharge aging of the battery to be tested at the second charging rate is performed. It can be understood that if the first voltage-capacity curve and the third voltage-capacity curve are consistent, it means that the consistency of the initial state of the battery to be tested and the control battery is good. Therefore, on the one hand, it can be shown that the battery to be tested is a battery that meets the design requirements, and its lithium plating test results can reflect the characteristics of each battery in the same batch. On the other hand, the experimental data of the control battery can be introduced in the result analysis to provide more complete data support for the lithium plating test results. Furthermore, if the first voltage-capacity curve does not match the third voltage-capacity curve, other batteries in the same batch may be replaced to continue testing.
[0067] Figure 2 is a sub-flow chart of step 104 of an embodiment, refer to Figure 2 In one embodiment, the above step 104 includes steps 201 to 202.
[0068] Step 201 : Differentiate a first voltage-capacity curve to obtain a first dV / dQ-Q curve, and differentiate a second voltage-capacity curve to obtain a second dV / dQ-Q curve.
[0069] Step 202: When the distance between the position of the characteristic peak of the first dV / dQ-Q curve and the position of the characteristic peak of the second dV / dQ-Q curve is greater than a preset distance, it is determined that the first lithium deposition detection result of the battery to be detected is that lithium deposition exists.
[0070] Among them, the characteristic peaks of the dV / dQ-Q curve represent specific electrochemical reactions inside the battery. These reactions appear as obvious peaks on the curve, which helps to understand the behavior of the battery at different charge and discharge stages. Therefore, the position and / or shape changes of these characteristic peaks can be used to analyze the reactions inside lithium-ion batteries, especially the loss of active lithium. Two batteries to be tested are used for illustration here, and the second charging rates of the two batteries to be tested are 1.6C and 2.5C, respectively. In order to make the subsequent description clear, the batteries to be tested are provided with the above-mentioned two second charging rates in the subsequent embodiments, and the battery to be tested after aging at the second charging rate of 1.6C is referred to as battery A to be tested, and the battery to be tested after aging at the second charging rate of 2.5C is referred to as battery B to be tested. Figure 3 is a first dV / dQ-Q curve of each battery in an embodiment, referring to Figure 3 , the first dV / dQ-Q curve has three characteristic peaks, Q1, Q2, and Q3 from left to right. Moreover, the positions of the three characteristic peaks of each battery are the same, so it can be considered that the initial state of each battery has a high consistency and meets the detection requirements. Figure 4 The second dV / dQ-Q curve of each battery in an embodiment is compared with the first dV / dQ-Q curve. The change in the characteristic peak Q1 before and after aging of the same battery to be detected generally indicates the loss of active lithium in the battery, and the change in Q2+Q3 indicates the loss of active materials in the battery. Therefore, it is possible to infer whether the battery has lithium deposition based on the change in Q1. It is understandable that during the cyclic charge and discharge aging process, there may be some other phenomena that will have some slight effects on the position of the characteristic peak Q1. Therefore, a preset distance for the movement of a characteristic peak position can be determined based on the degree of influence of other phenomena. Only when the position of the characteristic peak Q1 moves beyond the preset distance, the first lithium deposition detection result is determined to be the presence of lithium deposition, thereby avoiding incorrect judgments on lithium deposition. Reference Figure 4 , the characteristic peak Q1 of the battery A to be tested does not change significantly, so it can be considered that the first test result of the battery to be tested is that there is no lithium deposition. However, the dV / dQ-Q curve of the battery B to be tested has obvious lateral compression, and the Q1 change is obvious, so it can be considered that the first test result of the battery to be tested is that there is lithium deposition.
[0071] Figure 5 This is a second flow chart of a lithium deposition detection method according to an embodiment, referring to Figure 5 In one embodiment, the lithium deposition detection method includes steps 501 to 510. Compared with the above embodiment, the lithium deposition detection method of this embodiment further includes steps 502, 504, and 506 to 508.
[0072] Step 501 : charging a battery to be tested for the first time at a first charging rate and then discharging the battery to be tested, and obtaining a first voltage-capacity curve of the battery to be tested during the discharging process.
[0073] Step 502 , performing an initial charge and then discharge on a control battery at a first charge rate, and obtaining a third voltage-capacity curve of the control battery during the discharge process.
[0074] Step 503: Cyclic charge and discharge aging of the battery to be tested at a second charging rate
[0075] Step 504, performing cyclic charge-discharge aging on the control battery at a third charge rate.
[0076] The third charging rate is less than the second charging rate, and the third charging rate can be understood as a charging rate that will not cause lithium deposition in the control battery. Exemplarily, the third charging rate is 0.5C.
[0077] Step 505 , charging and then discharging the battery to be detected after cyclic charge and discharge aging at a first charging rate, and obtaining a second voltage-capacity curve of the battery to be detected during the discharge process.
[0078] Step 506, charging and then discharging the control battery after cyclic charge and discharge aging at the first charging rate, and obtaining a fourth voltage-capacity curve of the battery to be tested during the discharge process.
[0079] Among them, step 501 and step 502 can be executed synchronously, step 503 and step 504 can be executed synchronously, and step 505 and step 506 can be executed synchronously to improve the efficiency of lithium precipitation detection.
[0080] Step 507: Differentiate the third voltage-capacity curve to obtain a third dV / dQ-Q curve, and differentiate the fourth voltage-capacity curve to obtain a fourth dV / dQ-Q curve.
[0081] Step 508, determining the distance between the position of the characteristic peak of the third dV / dQ-Q curve and the position of the characteristic peak of the fourth dV / dQ-Q curve as a preset distance;
[0082] Specifically, the distance between the position of the first characteristic peak Q1 of the third dV / dQ-Q curve and the position of the first characteristic peak Q1 of the fourth dV / dQ-Q curve is the preset distance. It can be understood that since the third charging rate does not cause lithium deposition in the control battery, the above preset distance must be caused by other factors that cause the loss of lithium ions.
[0083] The inventors have found that the irreversible growth of the solid electrolyte interface (SEI) will also cause the position of the first characteristic peak of the dV / dQ-Q curve to move. Among them, SEI is a passivation layer covering the surface of the electrode material formed by the reaction between the electrode material and the electrolyte at the solid-liquid interface during the first charge and discharge process of the lithium-ion battery. Part of the active lithium ions will be consumed during the formation of SEI, which leads to a decrease in the reversible capacity of the battery. As the number of cycles increases, the continuous consumption of active lithium will reduce the amount of lithium embedded in the negative electrode, which is reflected in the change in the position of the characteristic peak on the dV / dQ curve. It can be understood that the irreversible growth of SEI is not inevitable, so the preset distance can be zero or other values greater than zero.
[0084] Step 509 : Differentiate the first voltage-capacity curve to obtain a first dV / dQ-Q curve, and differentiate the second voltage-capacity curve to obtain a second dV / dQ-Q curve.
[0085] Step 510: When the distance between the position of the characteristic peak of the first dV / dQ-Q curve and the position of the characteristic peak of the second dV / dQ-Q curve is greater than a preset distance, it is determined that the first lithium deposition detection result of the battery to be detected is that lithium deposition exists.
[0086] Combined with reference Figure 3 and Figure 4 , the position movement of the characteristic peak of the battery B to be tested is greater than the preset distance, so it can be determined that lithium deposition exists in the battery after the battery B to be tested is subjected to cyclic charge and discharge aging. In the embodiment of the application, by obtaining the position movement amount of the characteristic peak of the control battery before and after cyclic charge and discharge aging at the third charging rate, a more accurate preset distance can be provided to eliminate the influence of other force majeure factors other than lithium deposition on the movement of the characteristic peak Q1, thereby improving the accuracy of lithium deposition detection.
[0087] In one embodiment, the lithium plating detection method further includes: charging the battery to be detected after cyclic charge and discharge aging at a second charging rate and then standing, and obtaining the voltage-time curve of the battery to be detected during the standing process; obtaining the second lithium plating detection result of the battery to be detected according to the voltage-time curve. Specifically, the battery to be detected can be charged to a fully charged state and then left to stand, and the standing time can be 2h, 3h, 4h, etc., which is not limited here. Further, the battery voltage value can be recorded once every 1s during the standing process to obtain the voltage-time curve. When the battery is fully charged, if there is a lithium plating phenomenon, the precipitated metallic lithium may gradually be re-embedded in the negative electrode material during the standing period. This process can restore the effective capacity of the battery and cause the open circuit voltage of the battery to rise slowly over time. Therefore, the behavior of the metallic lithium after lithium plating being re-embedded in the negative electrode can be indirectly observed by monitoring the voltage change during the standing period, thereby evaluating the degree of lithium plating and the impact on battery performance.
[0088] In one embodiment, obtaining the second lithium deposition test result of the battery to be tested according to the voltage-time curve includes: differentiating the voltage-time curve to obtain a dV / dt-t curve; when there is a platform in the dV / dt-t curve, determining that the second lithium deposition test result of the battery to be tested is the presence of lithium deposition. Specifically, the appearance of the platform reflects the uniform embedding process of lithium ions in the negative electrode material, so the platform of the dV / dt-t curve is a direct reflection of the lithium deposition characteristics. Figure 6 The dV / dt-t curves of the batteries in one embodiment are shown in FIG. Figure 6 , the voltage relaxation curves of the control battery and the battery A to be tested do not show a platform, so it can be determined that the second lithium deposition test results of the above two batteries do not have lithium deposition. However, the voltage relaxation curve of the battery B to be tested shows a platform, so it can be determined that the second lithium deposition test result of the battery to be tested does have lithium deposition.
[0089] In one embodiment, before the battery to be tested is subjected to cyclic charge and discharge aging at a second charging rate, it also includes: constant current charging of the battery to be tested at a second charging rate, obtaining the state of charge-resistance curve of the battery to be tested during the constant current charging process, and obtaining the third lithium precipitation detection result of the battery to be tested according to the state of charge-resistance curve. Specifically, the cut-off voltage of the constant current charging is 2.5V to 3.65V, for example, it can be 2.5V, 3V, 3.65V. During the constant current charging process, the charging can be stopped after a certain length of time, and the voltage change value in a very short time after the moment of stopping charging is obtained, and the resistance of the battery to be tested is obtained according to the change value. Exemplarily, the charging can be stopped for 1s every 30s, and the voltage value can be recorded every 0.1s in this 1s to ensure that the voltage change value within a very short time (for example, 0.1s) after the moment of stopping charging can be collected. Among them, the resistance of the battery to be tested is the voltage change value within 0.1s after the moment of stopping charging / the current value of constant current charging. The state of charge SOC is the charging capacity / total charging capacity*100%. It is understandable that the longer the waiting time after stopping charging, the greater the impact of factors such as ambient temperature and battery aging on the voltage reading may have. Therefore, in the embodiment of the application, by measuring the voltage change value at the moment when charging stops, the impact of environmental factors on the measurement results can be minimized. Moreover, at the moment when the current is suddenly interrupted, the instantaneous change value of the voltage can more truly reflect the electrochemical reaction state and electrode interface characteristics inside the battery, thereby providing a more accurate impedance measurement result, thereby improving the accuracy of the third lithium precipitation detection result.
[0090] In one of the embodiments, obtaining a third lithium deposition detection result of the battery to be detected according to the state of charge-resistance curve includes: when there is no minimum value in the state of charge-resistance curve, determining that the third lithium deposition detection result of the battery to be detected is the presence of lithium deposition. Specifically, in an ideal case where there is no lithium deposition, the state of charge-resistance curve of the battery usually decreases gradually with the increase of the battery charge state, because the impedance inside the battery decreases with the increase of the amount of electricity. When the state of charge is close to full charge, the curve may rise slightly, because when the battery is close to full charge, the chemical reaction rate inside it slows down, resulting in a slight increase in internal resistance. However, if there is lithium deposition, the irregular deposition of metallic lithium will cause uneven current distribution inside the battery, thereby hindering charge transfer in certain areas, which will appear as abnormal fluctuations on the state of charge-resistance curve or not conform to the normal downward and upward trends. Figure 7 The state of charge-resistance curve of each battery in an embodiment is shown in FIG. Figure 7As the SOC increases, the resistance of the control battery decreases first during the charging process, and then increases slightly. The resistance of the test battery A decreases first during the charging process, and then tends to stabilize. The resistance of the test battery B decreases first during the charging process, and then stabilizes. When a certain SOC is reached, the resistance value drops suddenly. Therefore, it can be determined that the third lithium deposition test results of the two test batteries are both lithium deposition.
[0091] In one of the embodiments, the lithium deposition detection method further includes: when the first lithium deposition detection result, the second lithium deposition detection result and the third lithium deposition detection result are all the results of lithium deposition, determining that lithium deposition exists in the battery to be detected. It is understandable that if the lithium deposition detection method includes only one of the second lithium deposition detection result and the third lithium deposition detection result in addition to the first lithium deposition detection result, then the battery to be detected can be determined to have lithium deposition when both the first lithium deposition detection result and the second lithium deposition detection result are the results of lithium deposition, or when both the first lithium deposition detection result and the third lithium deposition detection result are the results of lithium deposition. That is, as long as all the lithium deposition detection results involved in the determination are the results of lithium deposition, the battery to be detected is determined to have lithium deposition, otherwise it is determined that lithium deposition does not exist in the battery to be detected. In the embodiment of the application, multiple methods are used for joint detection and joint determination, and lithium deposition is determined to have occurred when and only when all the multiple methods meet the lithium deposition standard, which can greatly reduce the occurrence of misjudgments, thereby improving the accuracy of determination. Combined with reference Figure 3 to Figure 4 , Figure 6 to Figure 7 The data can be used to determine that the control battery and the test battery A do not have lithium deposition, while the test battery B has lithium deposition. In order to verify the accuracy of the lithium deposition detection method of this application, the control battery and the test batteries A and B were disassembled and observed for verification. Figure 8 As shown, the observed results are consistent with the results of the lithium precipitation detection method using this embodiment, proving the high feasibility and accuracy of this method.
[0092] It should be understood that, although the steps in the flowcharts involved in the above embodiments are displayed in sequence according to the indication of the arrows, these steps are not necessarily executed in sequence according to the order indicated by the arrows. Unless there is a clear explanation in this article, the execution of these steps is not strictly limited in order, and these steps can be executed in other orders. Moreover, at least a part of the steps in the flowcharts involved in the above embodiments may include multiple steps or multiple stages, and these steps or stages are not necessarily executed at the same time, but can be executed at different times, and the execution order of these steps or stages is not necessarily carried out in sequence, but can be executed in turn or alternately with other steps or at least a part of the steps or stages in other steps.
[0093] Based on the same inventive concept, the embodiment of the present application also provides a lithium deposition detection device for implementing the above-mentioned lithium deposition detection method. The implementation scheme for solving the problem provided by the device is similar to the implementation scheme recorded in the above-mentioned method, so the specific limitations in one or more lithium deposition detection device embodiments provided below can refer to the limitations of the lithium deposition detection method above, and will not be repeated here.
[0094] Fig. 9 is a schematic diagram of the structure of a lithium deposition detection device according to an embodiment, referring to Fig. 9 The lithium plating detection device includes a first voltage-capacity curve acquisition module, a first aging control module, a second voltage-capacity curve acquisition module and a first result acquisition module. Among them, the first voltage-capacity curve acquisition module is used to charge and discharge the battery to be detected for the first time at a first charging rate, and obtain the first voltage-capacity curve of the battery to be detected during the discharge process. The first aging control module is used to perform cyclic charge and discharge aging on the battery to be detected at a second charging rate; the second charging rate is greater than the first charging rate. The second voltage-capacity curve acquisition module is used to charge and discharge the battery to be detected after cyclic charge and discharge aging at the first charging rate, and obtain the second voltage-capacity curve of the battery to be detected during the discharge process. The first result acquisition module is used to obtain the first lithium plating detection result of the battery to be detected according to the first voltage-capacity curve and the second voltage-capacity curve.
[0095] In one embodiment, the first result acquisition module includes a first differential unit and a first determination unit. The first differential unit is used to differentiate the first voltage-capacity curve to obtain a first dV / dQ-Q curve, and to differentiate the second voltage-capacity curve to obtain a second dV / dQ-Q curve. The first determination unit is used to determine that the first lithium deposition detection result of the battery to be detected is the presence of lithium deposition when the distance between the position of the characteristic peak of the first dV / dQ-Q curve and the position of the characteristic peak of the second dV / dQ-Q curve is greater than a preset distance.
[0096] In one embodiment, the lithium deposition detection device further includes a third voltage-capacity curve acquisition module, a second aging control module, a fourth voltage-capacity curve acquisition module and a distance acquisition module. Among them, the third voltage-capacity curve acquisition module is used to discharge the control battery after the first charge at the first charging rate, and obtain the third voltage-capacity curve of the control battery during the discharge process; the control battery and the battery to be detected are batteries of the same batch. The second aging control module is used to perform cyclic charge and discharge aging on the control battery at the third charging rate. The fourth voltage-capacity curve acquisition module is used to discharge the control battery after cyclic charge and discharge aging at the first charging rate, and obtain the fourth voltage-capacity curve of the battery to be detected during the discharge process. The distance acquisition module is used to differentiate the third voltage-capacity curve to obtain a third dV / dQ-Q curve, and differentiate the fourth voltage-capacity curve to obtain a fourth dV / dQ-Q curve; determine that the distance between the position of the characteristic peak of the third dV / dQ-Q curve and the position of the characteristic peak of the fourth dV / dQ-Q curve is a preset distance.
[0097] In one embodiment, the lithium deposition detection device further includes a voltage-time curve acquisition module and a second result acquisition module. The voltage-time curve acquisition module is used to charge the battery to be detected after cyclic charge-discharge aging at a second charging rate and then let it stand, and obtain the voltage-time curve of the battery to be detected during the standing process. The second result acquisition module is used to obtain a second lithium deposition detection result of the battery to be detected according to the voltage-time curve.
[0098] In one embodiment, the second result acquisition module includes a second differential unit and a second determination unit. The second differential unit is used to differentiate the voltage-time curve to obtain a dV / dt-t curve. The second determination unit is used to determine that the second lithium deposition test result of the battery to be tested is the presence of lithium deposition when there is a platform in the dV / dt-t curve.
[0099] In one embodiment, the lithium deposition detection device further includes a state of charge-resistance curve module and a third result acquisition module. The state of charge-resistance curve module is used to perform constant current charging on the battery to be detected at a second charging rate, and obtain the state of charge-resistance curve of the battery to be detected during the constant current charging process. The third result acquisition module is used to obtain a third lithium deposition detection result of the battery to be detected according to the state of charge-resistance curve.
[0100] In one of the embodiments, the third result acquisition module is used to determine that the third lithium deposition detection result of the battery to be detected is the presence of lithium deposition when there is no minimum value in the state of charge-resistance curve.
[0101] In one embodiment, the lithium deposition detection device further comprises a comprehensive determination module, which is used to determine whether lithium deposition exists in the battery to be detected when the first lithium deposition detection result, the second lithium deposition detection result and the third lithium deposition detection result all indicate the presence of lithium deposition.
[0102] In one embodiment, there are multiple batteries to be tested, and the second charging rates of the multiple batteries to be tested are different. The lithium plating detection device also includes an initial detection module. The initial detection module is used to perform the first charge and discharge of the control battery at the first charging rate, and obtain the third voltage-capacity curve of the control battery during the discharge process; the control battery and the battery to be tested are batteries from the same batch. Wherein, when the first voltage-capacity curve and the third voltage-capacity curve are consistent, the step of performing cyclic charge and discharge aging on the battery to be tested at the second charging rate is performed.
[0103] Each module in the above lithium deposition detection device can be implemented in whole or in part by software, hardware, or a combination thereof. Each module can be embedded in or independent of a processor in an electronic device in the form of hardware, or can be stored in a memory in an electronic device in the form of software, so that the processor can call and execute operations corresponding to each module.
[0104] The embodiment of the present application also provides a computer-readable storage medium. One or more non-volatile computer-readable storage media containing computer-executable instructions, when the computer-executable instructions are executed by one or more processors, the processors execute the steps of the lithium deposition detection method.
[0105] An embodiment of the present application also provides a computer program product comprising instructions, which, when executed on a computer, enables the computer to execute a lithium deposition detection method.
[0106] Those skilled in the art can understand that all or part of the processes in the above-mentioned embodiments can be completed by instructing the relevant hardware through a computer program, and the computer program can be stored in a non-volatile computer-readable storage medium. When the computer program is executed, it can include the processes of the embodiments of the above-mentioned methods. Among them, any reference to the memory, database or other medium used in the embodiments provided in this application can include at least one of non-volatile and volatile memory. Non-volatile memory can include read-only memory (ROM), magnetic tape, floppy disk, flash memory, optical memory, high-density embedded non-volatile memory, resistive random access memory (ReRAM), magnetoresistive random access memory (MRAM), ferroelectric random access memory (FRAM), phase change memory (PCM), graphene memory, etc. Volatile memory can include random access memory (RAM) or external cache memory, etc. As an illustration and not limitation, RAM can be in various forms, such as static random access memory (SRAM) or dynamic random access memory (DRAM). The database involved in each embodiment provided in this application may include at least one of a relational database and a non-relational database. Non-relational databases may include distributed databases based on blockchains, etc., but are not limited to this. The processor involved in each embodiment provided in this application may be a general-purpose processor, a central processing unit, a graphics processor, a digital signal processor, a programmable logic device, a data processing logic device based on quantum computing, etc., but are not limited to this.
[0107] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0108] The above embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the present application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the present application shall be subject to the attached claims.
Claims
1. A lithium precipitation detection method, characterized in that: include: Discharging the battery to be detected after first charging it at a first charging rate, and obtaining a first voltage-capacity curve of the battery to be detected during the discharge process; Performing cyclic charge-discharge aging on the battery to be tested at a second charge rate; The second charging rate is greater than the first charging rate; charging and then discharging the battery to be detected after cyclic charge and discharge aging at the first charging rate, and obtaining a second voltage-capacity curve of the battery to be detected during the discharge process; A first lithium plating detection result of the battery to be detected is obtained according to the first voltage-capacity curve and the second voltage-capacity curve.
2. The lithium precipitation detection method according to claim 1, characterized in that: The obtaining a first lithium deposition detection result of the battery to be detected according to the first voltage-capacity curve and the second voltage-capacity curve includes: Differentiating the first voltage-capacity curve to obtain a first dV / dQ-Q curve, and differentiating the second voltage-capacity curve to obtain a second dV / dQ-Q curve; When the distance between the position of the characteristic peak of the first dV / dQ-Q curve and the position of the characteristic peak of the second dV / dQ-Q curve is greater than a preset distance, it is determined that the first lithium deposition detection result of the battery to be detected is that lithium deposition exists.
3. The lithium precipitation detection method according to claim 2, characterized in that: Also includes: Discharging a control battery after first charging at a first charging rate, and obtaining a third voltage-capacity curve of the control battery during the discharge process; The control battery and the battery to be tested are batteries from the same batch; Performing cyclic charge-discharge aging on the control battery at a third charge rate; charging and then discharging the control battery after cyclic charge-discharge aging at the first charge rate, and obtaining a fourth voltage-capacity curve of the battery to be tested during the discharge process; Differentiating the third voltage-capacity curve to obtain a third dV / dQ-Q curve, and differentiating the fourth voltage-capacity curve to obtain a fourth dV / dQ-Q curve; The distance between the position of the characteristic peak of the third dV / dQ-Q curve and the position of the characteristic peak of the fourth dV / dQ-Q curve is determined as the preset distance.
4. The lithium precipitation detection method according to claim 1, characterized in that: Also includes: charging the battery to be detected after cyclic charge-discharge aging at the second charging rate and then letting it stand, and obtaining a voltage-time curve of the battery to be detected during the standing process; A second lithium deposition detection result of the battery to be detected is obtained according to the voltage-time curve.
5. The lithium precipitation detection method according to claim 4, characterized in that: The step of obtaining a second lithium deposition detection result of the battery to be detected according to the voltage-time curve includes: Differentiating the voltage-time curve to obtain a dV / dt-t curve; When the dV / dt-t curve has a platform, it is determined that the second lithium deposition test result of the battery to be tested is that lithium deposition exists.
6. The lithium precipitation detection method according to claim 1, characterized in that: Before the battery to be tested is subjected to cyclic charge-discharge aging at a second charge rate, the method further comprises: Performing constant current charging on the battery to be detected at the second charging rate, and obtaining a state of charge-resistance curve of the battery to be detected during the constant current charging process; A third lithium plating detection result of the battery to be detected is obtained according to the state of charge-resistance curve.
7. The lithium precipitation detection method according to claim 6, characterized in that: The step of obtaining a third lithium deposition detection result of the battery to be detected according to the state of charge-resistance curve includes: When there is no minimum value in the state of charge-resistance curve, it is determined that the third lithium deposition detection result of the battery to be detected is that lithium deposition exists.
8. The lithium precipitation detection method according to any one of claims 4 to 7, characterized in that: Also includes: When the first lithium deposition test result, the second lithium deposition test result and the third lithium deposition test result all indicate that lithium deposition exists, it is determined that lithium deposition exists in the battery to be tested.
9. The lithium precipitation detection method according to claim 1, characterized in that: There are multiple batteries to be tested, and the second charging rates of the multiple batteries to be tested are different. The method further includes: Performing a first charge and discharge operation on a control battery at a first charge rate, and obtaining a third voltage-capacity curve of the control battery during the discharge process; the control battery and the battery to be tested are batteries from the same batch; Wherein, when the first voltage-capacity curve and the third voltage-capacity curve are consistent, the step of performing cyclic charge-discharge aging on the battery to be tested at a second charge rate is performed.
10. A lithium deposition detection device, characterized in that: include: A first voltage-capacity curve acquisition module, used to charge and discharge the battery to be detected for the first time at a first charging rate, and acquire a first voltage-capacity curve of the battery to be detected during the discharge process; A first aging control module, used for performing cyclic charge-discharge aging on the battery to be tested at a second charging rate; the second charging rate is greater than the first charging rate; A second voltage-capacity curve acquisition module is used to charge and then discharge the battery to be detected after cyclic charge-discharge aging at the first charging rate, and obtain a second voltage-capacity curve of the battery to be detected during the discharge process; The first result acquisition module is used to acquire a first lithium plating detection result of the battery to be detected according to the first voltage-capacity curve and the second voltage-capacity curve.
11. An electronic device comprising a memory and a processor, wherein a computer program is stored in the memory, wherein: When the computer program is executed by the processor, the processor performs the steps of the lithium precipitation detection method according to any one of claims 1 to 9.
12. A computer-readable storage medium having a computer program stored thereon, characterized in that: When the computer program is executed by a processor, the steps of the method according to any one of claims 1 to 9 are implemented.
13. A computer program product, comprising a computer program, characterized in that When the computer program is executed by a processor, the steps of the method according to any one of claims 1 to 9 are implemented.