Battery formation method and jig thereof

By using inverted battery state and negative pressure formation technology, the problem of uneven electrolyte deposition during battery formation was solved, improving the uniformity of SEI film formation and battery performance, and reducing production costs.

CN118919894APending Publication Date: 2024-11-08REPT BATTERO ENERGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411298863.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-14
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

During battery formation, uneven electrolyte deposition leads to uneven SEI film formation, affecting battery capacity, cycle life, and rate performance.

Method used

By inverting the battery from its upright position to its inverted position for formation, and by draining and replenishing the electrolyte before and after formation, combined with negative pressure formation and confinement formation technologies, uniform distribution of electrolyte and effective removal of gas are ensured.

Benefits of technology

This method achieves uniform distribution of electrolyte during battery formation, improves the uniformity of SEI film formation, reduces gas generation, lowers electrolyte consumption and production costs, and extends battery life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919894A_ABST
    Figure CN118919894A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of battery production processes, and discloses a battery formation method and a jig thereof.The battery formation method comprises the steps that a battery is aged in a first state; the battery is formed in a second state, and the second state is an inverted state of the battery in the first state; the invention further discloses a battery formation jig which is suitable for the battery formation method in any one implementation mode in the first aspect, the battery formation jig comprises a box body, the box body comprises a containing cavity and an avoiding part, the upper portion of the containing cavity is provided with an opening, and the containing cavity is suitable for containing at least one battery; the avoiding part is arranged at the bottom of the box body and is suitable for connecting a liquid injection port and an electrode of a battery positioned in the accommodating cavity with equipment positioned outside the accommodating cavity. The battery formation method, the jig and the battery production line provided by the invention can solve or improve the problem that an SEI film generated in battery formation is not uniform.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of battery production technology, and in particular to a battery formation method and a jig thereof. Background Art

[0002] Battery formation refers to the process of charging and discharging the battery for the first time after the battery is injected with electrolyte. The main purpose of this process is to stimulate the active substances in the battery and make the lithium-ion battery enter an "activated" state. During this process, some additional reactions usually occur, that is, the electrolyte and lithium salt interact with each other at the negative electrode of the battery to form a SEI film (Solid Electrolyte Interface membrane). It can effectively prevent the continuous occurrence of side reactions, thereby reducing the loss of lithium in the battery. This is crucial to maintaining the overall capacity, cycle life and rate performance of the battery.

[0003] In the related art, the processes of the battery before formation are primary liquid injection and high-temperature aging. In both the primary liquid injection and high-temperature aging processes, the battery cells are placed upright. When the battery cells are placed upright, the electrolyte will preferentially deposit at the bottom of the battery cells due to gravity. Therefore, during the formation process, the battery formation will be uneven due to lack of liquid at the top of the battery cells. Summary of the invention

[0004] In view of this, the present application provides a battery formation method and a jig thereof to solve or improve the problem of uneven SEI film generation during battery formation.

[0005] In one aspect, the present application provides a battery formation method, comprising the steps of:

[0006] The battery is aged in a first state;

[0007] The battery is formed in a second state, wherein the second state is an inverted state of the battery in the first state.

[0008] In an optional embodiment, the battery formation method further comprises the steps of:

[0009] The battery, in the second state, discharges the electrolyte in the aged battery that is not absorbed by the battery core;

[0010] The battery after the electrolyte is discharged is formed in the second state.

[0011] In an optional embodiment, the liquid injection port on the battery opens upward in the first state; and opens downward in the second state.

[0012] In an optional embodiment, during the battery formation process, the battery is restrained; and / or the electrolyte injection amount of the battery before aging is 75% to 95%.

[0013] In an optional embodiment, the battery is formed under negative pressure during the formation process.

[0014] In an optional embodiment, the battery formation method further includes the steps of injecting electrolyte into the battery for the first time before aging the battery and inserting a pin into the injection port of the battery; after aging the battery, removing the pin and then performing formation.

[0015] In an optional embodiment, the battery formation method further comprises the step of replenishing the electrolyte of the battery for a second time after the battery is formed.

[0016] In the second aspect, the present application also provides a battery formation jig, which is suitable for the battery formation method in any one embodiment of the first aspect, comprising a box body, the box body comprising a accommodating cavity and an avoidance portion, the accommodating cavity is opened at the top, and the accommodating cavity is suitable for accommodating at least one battery; the avoidance portion is arranged at the bottom of the box body, and is suitable for connecting the liquid injection port and the electrode of the battery located in the accommodating cavity with the equipment located outside the accommodating cavity.

[0017] In an optional embodiment, the battery formation jig further includes a partition portion, a push plate portion and a pushing portion, wherein a plurality of partition portions are provided and movably arranged in the accommodating cavity, a plurality of batteries located in the accommodating cavity are arranged at intervals along the length direction of the accommodating cavity, and the partition portion is arranged between any two adjacent batteries; the push plate portion is located at one end of the plurality of batteries located in the accommodating cavity along the length direction of the accommodating cavity, and is located in the accommodating cavity; the pushing portion can push the push plate portion to restrain the plurality of batteries.

[0018] In an optional embodiment, the battery formation jig also includes a liquid collecting box, which is provided with a liquid inlet, and the liquid inlet is suitable for being fixedly and sealedly connected to the liquid filling port of the battery; and / or, the battery formation jig also includes a negative pressure tube, one end of the negative pressure tube is suitable for being connected to the liquid filling port of the battery, and the other end of the negative pressure tube is suitable for being connected to a negative pressure extraction device, an automatic telescopic clamping assembly is fixedly arranged in the negative pressure tube, an air-liquid channel is arranged between the automatic telescopic clamping assembly and the inner wall surface of the negative pressure tube, and the automatic telescopic clamping assembly is used to remove pins.

[0019] In a third aspect, the present application further provides a battery production line, which forms batteries using a battery formation method as in any one of the embodiments in the first aspect; and / or, includes a battery formation jig as in any one of the embodiments in the second aspect.

[0020] Beneficial effect: Because the battery production line adopts a battery formation method to form the battery; and / or includes a battery formation jig, it has the same effect as the battery formation method or the battery formation jig, which will not be described in detail here. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the related technologies, the drawings required for use in the specific implementation methods or the related technical descriptions will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0022] Figure 1 A flow chart of a battery formation method according to an embodiment of the present application;

[0023] Figure 2 is a schematic diagram of the axial side of the battery;

[0024] Figure 3 It is a schematic diagram of the axial side of the battery with the pin inserted;

[0025] Figure 4 It is an axial side view of a battery formation jig according to an embodiment of the present application;

[0026] Figure 5 An isometric view of a battery formation jig from another perspective according to an embodiment of the present application;

[0027] Figure 6 A schematic diagram of a process of loading a battery into a battery formation jig according to an embodiment of the present application;

[0028] Figure 7 A schematic diagram of a battery formation jig used for battery formation according to an embodiment of the present application;

[0029] Figure 8 This is a schematic diagram of the working of an automatic telescopic clamping assembly in a battery formation jig according to an embodiment of the present application;

[0030] Fig. 9 A schematic diagram of another moment when an automatic telescopic clamping assembly in a battery formation jig according to an embodiment of the present application is working;

[0031] Fig.10 A schematic diagram of an automatic telescopic clamping assembly in a battery formation jig according to an embodiment of the present application at another working moment;

[0032] Fig.11 This is a schematic structural diagram of a battery formation jig in an embodiment of the present application in which a liquid collecting box is installed on a battery;

[0033] Fig.12 This is a schematic diagram of removing a liquid collecting box from a battery in a battery formation jig according to an embodiment of the present application.

[0034] Description of reference numerals:

[0035] 1. Battery; 2. Pin; 3. Box; 4. Liquid collecting box; 5. Negative pressure tube; 6. Fixing bar; 7. Charging and discharging column;

[0036] 101. liquid injection port; 102. electrode;

[0037] 301, accommodating cavity; 302, avoidance portion; 303, partition portion; 304, push plate portion; 305, pushing portion;

[0038] 501, automatic telescopic gripping assembly;

[0039] 601. Bending portion. DETAILED DESCRIPTION

[0040] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present application.

[0041] In the relevant technology, battery formation refers to the process of charging and discharging the dry battery cell for the first time after the electrolyte is injected into it. The main purpose of this process is to stimulate the active substances in the battery and make the lithium-ion battery enter an "activated" state. During this process, a SEI film is usually generated, which can effectively prevent the continued occurrence of side reactions, thereby reducing the loss of lithium ions in the battery. This is crucial to maintaining the overall capacity, cycle life and rate performance of the battery.

[0042] The battery processes before formation are primary liquid injection and high-temperature aging. In both processes, the battery cells are placed upright. When the battery cells are placed upright, the electrolyte will preferentially deposit at the bottom of the battery cells due to gravity. Therefore, during the formation process, the battery formation will be uneven due to lack of liquid at the top of the battery cells.

[0043] In order to solve or improve the above problems, the present application provides a battery formation method, a fixture and a battery production line to improve the problem of uneven SEI film generation during battery formation.

[0044] Combine the following Figures 1 to 12 , describing an embodiment of the present application.

[0045] According to an embodiment of the present application, in a first aspect, a battery formation method is provided, such as Figure 1 As shown, the steps include:

[0046] The battery 1 is aged in a first state.

[0047] It is worth noting that the first state is a placement state of the battery 1, and is explained with reference to the liquid filling port 101 of the battery 1. The first state of the battery 1 can be placed with the liquid filling port 101 facing upward, or with the liquid filling port 101 facing downward, or with the liquid filling port 101 facing any horizontal direction.

[0048] It should be noted that the aging may be high temperature aging or aging with other parameters.

[0049] The battery 1 is formed in a second state, wherein the second state is an inverted state of the battery 1 in the first state.

[0050] It is worth noting that the second state is another placement state of the battery 1; wherein, the second state is an inverted state of the battery 1 in the first state, that is, the top and bottom of the battery 1 in the first state (at this time, the top of the battery 1 is located above the bottom of the battery 1), and in the second state, the top of the battery 1 in the first state is located below the bottom of the battery 1 in the first state; specifically, the liquid injection port 101 of the battery 1 is used as a reference for explanation. In the first state, the liquid injection port 101 of the battery 1 faces upward, and then, in the second state, the liquid injection port 101 of the battery 1 faces downward.

[0051] It should be noted that, in this embodiment, the aging process of the battery 1 and other formation processes of the battery 1 are not specifically limited and can be selected and set according to actual needs.

[0052] In this embodiment, the battery 1 is aged in the first state so that the electrolyte is preferentially deposited at the bottom of the battery cell in the battery 1, and then formed in the second state. Since the second state of the battery 1 is an inverted state of its first state, during the formation process of the battery 1, the electrolyte at the bottom of the battery cell before the battery 1 is inverted will flow to the top of the battery cell due to gravity after the inversion, thereby ensuring the electrolyte demand at the top of the battery cell during the formation process, avoiding the problem of lack of electrolyte at the top of the battery cell, and ensuring the uniformity of SEI film generated during the formation process of the battery cell.

[0053] In one embodiment, Figure 1 As shown, the battery formation method also includes the steps of:

[0054] In the second state, the battery 1 discharges the electrolyte that has not been absorbed by the battery cells in the aged battery 1 .

[0055] Specifically, there are many ways to discharge the electrolyte in the battery 1 that is not absorbed by the battery cell, such as connecting the negative pressure tube 5 to the injection port 101 of the battery 1 and inverting the battery 1 for extraction; another example is fixing a liquid collecting container in connection with the injection port 101, and then inverting the battery 1 and the liquid collecting container so that the electrolyte in the battery 1 is collected in the liquid collecting container under the action of gravity. Of course, other methods can also be adopted as long as the electrolyte in the battery 1 can be discharged. During the process of discharging the electrolyte from the battery 1, the free electrolyte in the battery 1 is concentrated on the top of the battery 1 due to gravity and infiltrates the top of the battery cell. When the top of the battery cell is fully infiltrated with the electrolyte, no more electrolyte is discharged from the battery 1. At this time, it can be judged that during the inversion process, the top electrode of the battery cell has been fully infiltrated, meeting the formation conditions.

[0056] The battery 1 from which the electrolyte has been discharged is formed in the second state.

[0057] In this embodiment, the electrolyte that is not absorbed by the battery cell in the battery 1 is discharged from the battery 1 before the battery 1 is formed, which not only reduces the amount of gas generated by the battery 1 during the formation process, but also allows the electrolyte to be recycled and reused to reduce the amount of electrolyte used, thereby reducing the production cost of the battery 1.

[0058] In one embodiment, the liquid injection port 101 on the battery 1 opens upward in the first state; Figure 7 As shown, the liquid injection port 101 opens downward in the second state. In this embodiment, the liquid injection port 101 on the battery 1 opens upward in the first state, which can facilitate the liquid injection operation into the battery 1, and the liquid injection port 101 opens downward in the second state. Since the battery cell assembly process of the battery 1 often adopts the process of welding the battery cell and the top cover, installing it in the aluminum shell of the battery 1, and then performing peripheral welding, this peripheral welding is prone to poor welding, and the liquid injection port 101 of the battery 1 is usually arranged on the top cover. The liquid injection port 101 opens downward in the second state, and the electrolyte will gather at the top of the battery 1, so as to detect the sealing of the welding point and find defective batteries 1.

[0059] In one embodiment, Figure 7 As shown, during the formation process of battery 1, battery 1 is restrained; and / or, the amount of electrolyte injected into battery 1 before aging is 75% to 95% of the remaining space inside battery 1, specifically, any one of 75%, 80%, 85%, 90% and 95%, preferably, the amount of electrolyte injected is 80% to 90%.

[0060] It should be noted that the “remaining space inside the battery 1 ” refers to the remaining space inside the battery 1 before the electrolyte is injected, excluding the space occupied by other components such as the battery cells.

[0061] In this embodiment, if Figure 7 As shown, during the formation process of the battery 1, the gap between the positive and negative electrodes in the battery cell can be reduced by constraining the formation of the battery 1, and the free electrolyte required for the formation can be reduced, thereby avoiding the gap between the positive and negative electrodes in the battery cell being too large, and requiring more electrolyte to be filled to achieve lithium ion transmission, thereby reducing the consumption of electrolyte and further reducing the battery formation cost; at the same time, the amount of electrolyte injected into the battery 1 before aging is 75% to 95% of the remaining space inside the battery 1, thereby maintaining the liquid retention coefficient of the battery 1 at 3.0g / Ah to 3.5g / Ah, and correspondingly, when the electrolyte injection amount is 80% to 90%, the liquid retention coefficient of the battery 1 can be maintained within a more optimal range, i.e., 3.1g / Ah to 3.3g / Ah, thereby reducing the waste of electrolyte and extending the service life of the battery 1.

[0062] In one embodiment, Figure 7 As shown, the battery 1 adopts negative pressure formation during the formation process. Specifically, the negative pressure tube 5 can be connected to the injection port 101 of the battery 1 to perform negative pressure formation on the battery 1. In this embodiment, the gas generated during the formation of the battery 1 can be removed in time by negative pressure formation, thereby ensuring the stability and consistency of the SEI film.

[0063] At the same time, since the battery 1 will produce reducing gas and oxidizing gas during the formation process, specifically, the reducing gases include hydrogen and methane with low density and strong reducing property, and carbon dioxide with high density and weak reducing property; the oxidizing gas is oxygen with low density, etc., when the liquid injection port 101 of the battery 1 is opened downward in the second state and is connected to the liquid injection port 101 through the negative pressure tube 5 for negative pressure formation, the gas with high density and weak reducing property (such as carbon dioxide) can be preferentially extracted, so that the gas with low density and strong reducing property (such as hydrogen and methane) and the oxidizing gas with low density (such as oxygen) are retained inside the battery 1 to participate in the redox reaction of generating the SEI film inside the battery 1, increase the stability of the SEI film, and thus improve the performance of the battery 1.

[0064] In one embodiment, Figure 1 As shown, the battery formation method also includes the steps of injecting electrolyte into the battery 1 for the first time before the battery 1 is aged, and inserting a pin 2 into the injection port 101 of the battery 1, such as Figure 2 and Figure 3 shown.

[0065] After the battery 1 is aged, the pin 2 is removed and then the battery is formed.

[0066] In this embodiment, the liquid injection port 101 of the battery 1 is blocked by the pin 2 during the aging process, and the blocking effect is good and easy to operate.

[0067] In one embodiment, after the battery 1 is formed, the electrolyte of the battery 1 is replenished for a second time so that there is enough electrolyte in the battery 1 to ensure the performance of the battery 1 .

[0068] Below is an example, combined with Figure 1 As shown, the above-mentioned battery formation method is comprehensively described as a whole; specifically, it includes the following steps:

[0069] The battery 1 is first injected with electrolyte, and the amount of electrolyte injected is 75% to 95% of the remaining space inside the battery 1. Preferably, the amount of electrolyte injected is 80% to 90%.

[0070] like Figure 2 and Figure 3 As shown, the pin 2 is inserted into the liquid filling port 101 of the battery 1.

[0071] The battery 1 is subjected to high-temperature aging in the first state.

[0072] Pull out the pin 2 on the aged battery 1.

[0073] In the second state, the battery 1 discharges the electrolyte that has not been absorbed by the battery cells in the aged battery 1 .

[0074] like Figure 7 As shown, the battery 1 is negatively pressurized in the second state and the battery 1 is restrained, wherein the second state is an inverted state of the battery 1 in the first state.

[0075] The formed battery 1 is subjected to secondary liquid injection and subsequent testing.

[0076] Preferably, Figure 2 As shown, the liquid injection port 101 on the battery 1 opens upward in the first state; Figure 6 and Figure 7 As shown, the liquid injection port 101 opens downward in the second state.

[0077] According to an embodiment of the present application, in a second aspect, a battery formation jig is provided, such as Figure 4 and Figure 5 As shown, the battery formation method applicable to the first aspect includes a box body 3, and the box body 3 includes a accommodating chamber 301 and an avoidance portion 302: the accommodating chamber 301 is opened at the top, and the accommodating chamber 301 is suitable for accommodating at least one battery 1; the avoidance portion 302 is arranged at the bottom of the box body 3, and is suitable for connecting the liquid injection port 101 and the electrode 102 of the battery 1 located in the accommodating chamber 301 with the equipment located outside the accommodating chamber 301.

[0078] Specifically, the box body 3 can be a box body 3 made of metal material, such as aluminum or steel; the shape of the avoidance portion 302 can be any shape such as square, circle, etc., as long as it can meet the requirements of the liquid injection port 101 and the motor being connected to external equipment through it for negative pressure formation.

[0079] In this embodiment, if Figure 4 As shown, by setting the upper opening of the accommodating cavity 301 and setting the avoidance portion 302 at the bottom, the battery 1 can be suitable for liquid injection and aging in the first state, and negative pressure formation in the second state.

[0080] In a specific embodiment, Figure 4 and Figure 5 As shown, the battery formation jig also includes a partition portion 303, a push plate portion 304 and a pushing portion 305. There are multiple partition portions 303, and they are movably arranged in the accommodating cavity 301. Multiple batteries 1 located in the accommodating cavity 301 are arranged at intervals along the length direction of the accommodating cavity 301, and a partition portion 303 is arranged between any two adjacent batteries 1; the push plate portion 304 is located at one end of the multiple batteries 1 located in the accommodating cavity 301 along the length direction of the accommodating cavity 301, and is located in the accommodating cavity 301; the pushing portion 305 can push the push plate portion 304 to restrain the multiple batteries 1.

[0081] Specifically, the partition portion 303 and the push plate portion 304 are made of steel plates, wooden plates and other non-metallic plates; the push portion 305 can be a lead screw that passes through the accommodating chamber 301 and is screwed to the accommodating chamber 301. One end of the lead screw is located in the accommodating chamber 301 and is pressed against the push plate portion 304, and the other end is used for manual drive or connection with a motor for drive; the push portion 305 can also be a cylinder with a telescopic function to push the push plate portion 304 to move to restrain the battery 1.

[0082] In this embodiment, a partition plate portion 303 and a push plate portion 304 are provided which can slide in the container cavity, and are driven by a push portion 305, so that the battery 1 can be restrained to achieve restrained formation.

[0083] In one embodiment, Fig.11 As shown, the battery formation jig also includes a liquid collecting box 4, on which a liquid inlet is provided, and the liquid inlet is suitable for being fixedly sealed and connected with the liquid injection port 101 of the battery 1; and / or, as Figures 8 to 10 As shown, it also includes a negative pressure tube 5, one end of the negative pressure tube 5 is suitable for being connected to the liquid injection port 101 of the battery 1, and the other end of the negative pressure tube 5 is suitable for being connected to the negative pressure extraction device, and an automatic telescopic clamping component 501 is fixedly arranged in the negative pressure tube 5, and an air-liquid channel is arranged between the automatic telescopic clamping component 501 and the inner wall surface of the negative pressure tube 5, and the automatic telescopic clamping component 501 is used to extract the pin 2.

[0084] Specifically, the liquid collecting box 4 is a box body made of plastic material, and its liquid inlet is sealed and connected with the liquid filling port 101 of the battery 1 by interference fit; at the same time, a fixing piece can also be set on the battery 1 to strengthen the fixing of the liquid collecting box 4. The specific solution is as follows: Fig.11 As shown, by fixing a fixing strip 6 on the battery 1, the fixing strip 6 is clamped on the side of the battery 1 through the bent portions 601 at both ends, and the liquid collecting box 4 is set between the two fixing parts by interference fit. Preferably, rubber pads are provided at the parts of the two fixing parts for contacting with the liquid collecting box 4 to increase friction and enhance the fixing effect of the liquid collecting box 4.

[0085] Specifically, the automatic telescopic clamping assembly 501 includes a one-way telescopic cylinder, a two-way telescopic cylinder and two rotating arms. The one-way telescopic cylinder is fixed to the inner arm of the negative pressure tube 5 by means of a clamping connection. Specifically, a clamping seat can be provided on the inner wall of the negative pressure tube 5, and a clamping head can be provided on the cylinder body of the one-way telescopic cylinder. The connection between the one-way telescopic cylinder and the negative pressure tube 5 is realized by the matching clamping connection between the clamping head and the clamping seat. The cylinder body of the two-way telescopic cylinder is connected to the telescopic end of the one-way telescopic cylinder by bolts. The two rotating arms are arranged in parallel, and brackets are provided on the middle parts of the two rotating arms. The two brackets are hinged by a rotating shaft. The ends of the telescopic cylinder are respectively hinged to the two ends of the bidirectional telescopic cylinder, and the ends of the two rotating arms away from the bidirectional telescopic cylinder are provided with clamping parts for clamping the pin 2. The bidirectional telescopic cylinder and the two rotating arms are driven by the unidirectional telescopic cylinder to move toward the liquid filling port 101 of the battery 1 (in this state, the liquid storage of the bidirectional telescopic cylinder is in a contracted state, and the clamping part is in an open state). When the clamping part reaches the position where the pin 2 can be clamped, the bidirectional telescopic cylinder extends in both directions and drives the two telescopic arms to rotate, so that the clamping part clamps the pin 2, and then the unidirectional telescopic cylinder contracts to pull out the pin 2.

[0086] The battery formation jig is described in detail below using an embodiment.

[0087] This embodiment provides a battery formation jig, such as Figure 4 and Figure 5As shown, the battery formation method applicable to the first aspect includes a box body 3, a partition portion 303, a push plate portion 304, a push portion 305, a liquid collecting box 4 and a negative pressure tube 5, the box body 3 includes a receiving chamber 301 and a avoiding portion 302; the receiving chamber 301 is opened at the top, and the receiving chamber 301 is suitable for receiving at least one battery 1; the avoiding portion 302 is arranged at the bottom of the box body 3, and is suitable for the injection port 101 and the electrode 102 of the battery 1 located in the receiving chamber 301 and the electrode 102 located outside the receiving chamber 301. Device connection; multiple partition parts 303 are provided, and are movably arranged in the accommodating chamber 301, multiple batteries 1 located in the accommodating chamber 301 are arranged at intervals along the length direction of the accommodating chamber 301, and a partition part 303 is provided between any two adjacent batteries 1; the push plate part 304 is located at one end of the multiple batteries 1 located in the accommodating chamber 301 along the length direction of the accommodating chamber 301, and is located in the accommodating chamber 301; the pushing part 305 can push the pushing plate part 304 to restrain the multiple batteries 1; Fig.11 As shown, the liquid collecting box 4 is provided with a liquid inlet, which is suitable for being fixedly and sealedly connected with the liquid filling port 101 of the battery 1; one end of the negative pressure tube 5 is suitable for being connected with the liquid filling port 101 of the battery 1, and the other end of the negative pressure tube 5 is suitable for being connected with the negative pressure extraction device, and an automatic telescopic clamping component 501 is fixedly provided in the negative pressure tube 5, and an air-liquid channel is provided between the automatic telescopic clamping component 501 and the inner wall surface of the negative pressure tube 5, and the automatic telescopic clamping component 501 is used to extract the pin 2.

[0088] According to an embodiment of the present application, on the other hand, a battery production line is provided, which uses the battery formation method in any one of the above embodiments to form a battery 1; and / or includes the battery formation jig in any one of the above embodiments.

[0089] Taking a battery production line as an example, the use of the above-mentioned battery formation method and battery formation jig is specifically explained below.

[0090] The electrolyte is first injected into the plurality of batteries 1 through the infusion device, and the electrolyte injection amount is 75% to 95% of the remaining space inside the battery 1. Preferably, the electrolyte injection amount is 80% to 90%.

[0091] A pin 2 is inserted into the liquid filling port 101 of each battery 1 by a robot to seal it.

[0092] The battery 1 is subjected to high temperature aging in the first state (eg, the liquid injection port 101 of the battery 1 faces upward).

[0093] ① The following are the steps for chemical formation using the negative pressure tube 5 with the automatic telescopic clamping assembly 501.

[0094] like Figure 6 As shown, a plurality of batteries 1 are inverted to a second state (with the liquid injection port 101 facing downward) using a manipulator and placed in the accommodating cavity 301;

[0095] like Figure 7 As shown, the negative pressure tube 5 is sealed and connected to the liquid injection port 101 through the avoidance portion 302 at the bottom of the accommodating chamber 301 , and the charge and discharge column 7 of the charge and discharge equipment is connected to the electrode 102 on the battery 1 through the avoidance portion 302 .

[0096] like Figures 8 to 10 As shown, the automatic telescopic clamping assembly 501 is actuated to pull out the pin 2 and perform negative pressure suction to extract the electrolyte in the battery 1 and recover it for reuse. At the same time, the charging and discharging equipment charges the battery 1, and the pushing part 305 pushes the pushing plate part 304 to restrain the battery 1, so that the battery 1 enters the formation stage.

[0097] After the formation of the battery 1 is completed, the charge and discharge column 7 and the negative pressure tube 5 are removed, and the pin 2 is removed from the negative pressure tube 5 to release the pressure of the push plate part 304 .

[0098] The robot takes the battery 1 out of the accommodating chamber 301 and performs the second test liquid injection and subsequent tests.

[0099] ② The following are steps for forming the battery 1 using the liquid collecting box 4 and the negative pressure tube 5 (the negative pressure tube 5 may or may not be provided with an automatic telescopic clamping assembly 501).

[0100] like Fig.11 As shown, a manipulator is used to pull out the pin 2 on each battery 1; and a liquid collecting box 4 is sealed and connected to the liquid filling port 101 of each battery 1;

[0101] like Figure 6 As shown, a plurality of batteries 1 are inverted to a second state (liquid injection port 101 facing downward) using a manipulator and placed in the accommodating cavity 301; the electrolyte in the battery 1 is collected in the liquid collecting box 4;

[0102] like Fig.12 As shown, the liquid collecting box 4 is removed, the negative pressure tube 5 is sealed and connected to the liquid filling port 101 through the avoidance portion 302 at the bottom of the accommodating chamber 301, and negative pressure suction is performed. The charging and discharging column 7 of the charging and discharging equipment is connected to the electrode 102 on the battery 1 through the avoidance portion 302, and the battery 1 is charged. The pushing portion 305 pushes the pushing plate portion 304 to restrain the battery 1, so that the battery 1 enters the formation stage.

[0103] After the battery 1 is formed, the charge-discharge column 7 and the negative pressure tube 5 are removed to release the pressure on the push plate portion 304 .

[0104] The robot takes the battery 1 out of the accommodating chamber 301 and performs the second test liquid injection and subsequent tests.

[0105] In this embodiment, because the battery production line adopts a battery formation method to form the battery 1; and / or includes a battery formation jig, it has the same effect as the battery formation method or the battery formation jig, which will not be described in detail here.

[0106] Although the embodiments of the present application are described in conjunction with the accompanying drawings, those skilled in the art may make various modifications and variations without departing from the spirit and scope of the present application, and such modifications and variations are all within the scope defined by the appended claims.

Claims

1. A battery formation method, characterized in that: Includes steps: The battery (1) is aged in a first state; The battery (1) is formed in a second state, wherein the second state is an inverted state of the battery (1) in the first state.

2. The battery formation method according to claim 1, characterized in that: Also includes the steps: The battery (1) discharges the electrolyte that has not been absorbed by the battery core in the aged battery (1) in the second state; The battery (1) after the electrolyte is discharged is formed in the second state.

3. The battery formation method according to claim 1, characterized in that: The liquid injection port (101) on the battery (1) opens upward in the first state; and opens downward in the second state.

4. The battery formation method according to any one of claims 1 to 3, characterized in that: During the formation process of the battery (1), the battery (1) is restrained; And / or, the electrolyte injection amount of the battery (1) before aging is 75% to 95%.

5. The battery formation method according to any one of claims 1 to 3, characterized in that: The battery (1) adopts negative pressure formation during the formation process.

6. The battery formation method according to any one of claims 1 to 3, characterized in that: Also includes the steps, Before the battery (1) is aged, the battery (1) is injected with electrolyte for the first time, and a pin (2) is inserted into the injection port (101) of the battery (1); After the battery (1) is aged, the pin (2) is removed and then the battery (1) is formed.

7. The battery formation method according to any one of claims 1 to 3, characterized in that: After the battery (1) is formed, the battery (1) is supplemented with electrolyte for a second time.

8. A battery formation jig, characterized in that: A battery (1) formation method suitable for use in any one of claims 1 to 7, comprising a housing (3), wherein the housing (3) comprises: a receiving cavity (301), the receiving cavity (301) being provided with an upper opening, and the receiving cavity (301) being suitable for receiving at least one battery (1); and The avoidance portion (302) is arranged at the bottom of the box body (3) and is suitable for connecting the injection port (101) and the electrode (102) of the battery (1) located in the accommodating cavity (301) with the equipment located outside the accommodating cavity (301).

9. The battery formation jig according to claim 8, characterized in that: Also includes: a partition part (303), wherein a plurality of the partition parts (303) are provided and are movably arranged in the accommodating cavity (301), a plurality of batteries (1) located in the accommodating cavity (301) are arranged at intervals along the length direction of the accommodating cavity (301), and the partition part (303) is provided between any two adjacent batteries (1); A push plate portion (304), the push plate portion (304) being located at one end of a plurality of batteries (1) located in the accommodating cavity (301) along the length direction of the accommodating cavity (301), and being located in the accommodating cavity (301); A pushing portion (305), wherein the pushing portion (305) can push the pushing plate portion (304) to restrain the plurality of batteries (1).

10. The battery formation jig according to claim 8 or 9, characterized in that: It also comprises a liquid collecting box (4), the liquid collecting box (4) being provided with a liquid inlet, the liquid inlet being adapted to be fixedly and sealedly connected to the liquid injection port (101) of the battery (1); And / or, it also includes a negative pressure tube (5), one end of the negative pressure tube (5) is suitable for communicating with the injection port (101) of the battery (1), and the other end of the negative pressure tube (5) is suitable for communicating with the negative pressure extraction device, an automatic telescopic clamping component (501) is fixedly arranged inside the negative pressure tube (5), a gas-liquid channel is arranged between the automatic telescopic clamping component (501) and the inner wall surface of the negative pressure tube (5), and the automatic telescopic clamping component (501) is used to extract the pin (2).