MEMS device with reduced Z-axis static friction and manufacturing process

By selectively etching the surface of the single crystal semiconductor inspection mass and polysilicon electrode of the MEMS device to form a rough surface, and using a high-temperature eutectic sealing ring bonding structure, the static friction problem in the MEMS device is solved, and the feasibility of manufacturing and operation is improved. And protects the inertial converter components.

CN118929559APending Publication Date: 2024-11-12STMICROELECTRONICS INT NV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410564621.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-09
Filing Date
2024-05-08
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Existing MEMS devices are prone to static friction problems in Z-axis accelerometers, which lead to difficulties in manufacturing and operation. In particular, the contact surface between the single-crystal silicon inspection mass and the polysilicon electrode is high, and the anti-static friction coating may interfere with the gyroscope test. eutectic bonding process of instrument.

Method used

By selective etching on the contact surfaces of the single crystal semiconductor inspection mass and the polysilicon electrode, a rough surface is formed to reduce static friction, and a vacuum environment is formed using a high-temperature eutectic sealing ring bonding structure in the MEMS inertial converter element to protect the inertial transformation instrument components.

Benefits of technology

It effectively reduces the Z-axis static friction in the MEMS device, improves the feasibility of manufacturing and operation, and avoids the impact of anti-static friction coating on the gyroscope tester, achieving efficient protection of inertial converter components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118929559A_ABST
    Figure CN118929559A_ABST
Patent Text Reader

Abstract

A method and apparatus for fabricating a high aspect ratio MEMS sensor device having an inertial transducer element formed in a multi-layer semiconductor structure is described, wherein the first inertial transducer element comprises a first single crystal semiconductor proof mass element and a second conductive electrode element separated from each other by an air sensing gap, and wherein at least the first sensing gap surface of the first single crystal semiconductor proof mass element is a first rough surface that has been selectively etched to reduce static friction between the first single crystal semiconductor proof mass element and the second conductive electrode element.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates generally to the field of semiconductor devices. In one aspect, the present disclosure relates to MEMS devices and methods for fabricating MEMS devices. Background Art

[0002] Micro-electromechanical systems (MEMS) technology is increasingly used to integrate mechanical elements, sensors, actuators, and electronic devices on a common silicon substrate through microfabrication techniques. For example, inertial sensors can be formed on an integrated circuit wafer substrate using MEMS devices to form various applications, such as accelerometers for measuring linear acceleration, gyroscopes for measuring angular velocity, optical devices, pressure sensors, switches, and the like. Conventional MEMS devices typically include a movable element, such as a proof mass, a diaphragm, a mirror, etc., which is flexible or movable and attached to the rest of the device. The relative motion between this movable element and the rest of the device is driven by an actuator and / or sensed by a sensor in various ways, depending on the device design. It has been observed that Z-axis accelerometer devices are more prone to stiction when accelerated with existing semiconductor processing technology. One of the reasons is that there is a higher probability of stiction between the extremely smooth contact surface of the single crystal silicon proof mass and the extremely smooth contact surface of the polycrystalline silicon electrode surface. Although anti-stiction coatings have been proposed for forming accelerometer sensors, such coatings may interfere with the eutectic bonding process used to form gyroscope tester sensors. As a result, the current design, operation and manufacturability of integrated circuit MEMS sensors is extremely difficult to implement on a practical level. Summary of the invention

[0003] A MEMS sensor device and an associated method for manufacturing the MEMS sensor device have been provided herein. The disclosed MEMS sensor device includes a first inertial transducer element formed in a multi-layer semiconductor structure. In selected embodiments, the first inertial transducer element is a z-axis accelerometer sensor. The disclosed MEMS sensor device also includes a cap device bonded to the multi-layer semiconductor structure to protect the first inertial transducer element from ambient environmental conditions. In selected embodiments, the cap device is bonded to the multi-layer semiconductor structure using a high temperature eutectic seal ring bonding structure to form a vacuum in a first sensor cavity that accommodates the first inertial transducer element. As disclosed, the first inertial transducer element includes a first single crystal semiconductor proof mass element and a second conductive electrode element separated from each other by an air sensing gap. In selected embodiments, the first single crystal semiconductor proof mass element is a cantilevered single crystal silicon crossbar anchored to the multi-layer semiconductor structure. In addition, the second conductive electrode element may include a conductive layer (e.g., a conductive polycrystalline layer) formed in the multi-layer semiconductor structure, the conductive layer being positioned to align with but separate from the cantilevered single crystal silicon crossbar. In the disclosed first inertial transducer element, a first sensing gap surface of at least a first single crystal semiconductor proof mass element is a first roughened surface that has been selectively etched to reduce stiction between the first single crystal semiconductor proof mass element and a second conductive electrode element. In selected embodiments, a second sensing gap surface of at least a second conductive electrode element is a second roughened surface that has been selectively etched to reduce stiction between the first single crystal semiconductor proof mass element and the second conductive electrode element. In other selected embodiments, the first sensing gap surface of at least the first single crystal semiconductor proof mass element comprises a non-uniform deposited polymer layer that has been selectively etched to form a first roughened surface on at least the first sensing gap surface. In other selected embodiments, the second sensing gap surface of at least the second conductive electrode element comprises a non-uniform deposited polymer layer that has been selectively etched to form a second roughened surface on at least the second sensing gap surface.

[0004] In another form, a transducer and an associated method for manufacturing the transducer are provided. In the disclosed method, a MEMS wafer structure is provided, including a first semiconductor electrode and a first semiconductor layer formed on the first semiconductor electrode. In selected embodiments, the first semiconductor electrode is formed as a polysilicon electrode and the first semiconductor layer is formed as a first single crystalline semiconductor layer. In other embodiments, the first semiconductor electrode is formed as a polysilicon electrode and the first semiconductor layer is formed as a first polycrystalline semiconductor layer. The disclosed method also includes selectively etching the first semiconductor layer to form a first MEMS inertial transducer element and a surrounding frame support element. In selected embodiments, the first semiconductor layer is selectively etched by etching the first semiconductor layer with a deep reactive ion etching process to form the first MEMS inertial transducer element as a high aspect ratio proof mass transducer element (e.g., a z-axis accelerometer sensor). In addition, the disclosed method includes applying a structural release etching process to release the first MEMS inertial transducer element and expose a first sensing gap surface of the first MEMS inertial transducer element and a second sensing gap surface of the first semiconductor electrode. In selected embodiments, a structure release etching process may be applied using vapor release etching to remove a sacrificial dielectric layer formed between the semiconductor electrode and the first semiconductor layer. The disclosed method also includes applying a surface wear etching process to roughen one or both of the first sensing gap surface of the first MEMS inertial transducer element or the second sensing gap surface of the first semiconductor electrode, thereby reducing the static friction between the first MEMS inertial transducer element and the first semiconductor electrode. In selected embodiments, a surface wear etching process may be applied using inhomogeneous plasma etching, which etches the crystal grain boundary region in the first MEMS inertial transducer element or the first semiconductor electrode faster than the non-boundary region in either one or both of the first MEMS inertial transducer element or the first semiconductor electrode. In other selected embodiments, a surface wear etching process may be applied by: depositing an inhomogeneous polymer layer on at least the first sensing gap surface and the second sensing gap surface; and applying a semiconductor etching process, which roughens the first sensing gap surface and the second sensing gap surface by selectively etching the first MEMS inertial transducer element and the first semiconductor electrode that are not protected by the inhomogeneous polymer layer. In addition, the disclosed method includes attaching the first cap wafer structure to the MEMS wafer structure using a first bonding process. In selected embodiments, the first cap wafer structure may be attached to the MEMS wafer structure by bonding the first cap wafer structure to the MEMS wafer structure using a high temperature eutectic sealing ring bonding structure to form a vacuum in a first sensor cavity of the cap wafer structure housing a first MEMS inertial transducer element.

[0005] In yet another form, a high aspect ratio transducer and a method for manufacturing a high aspect ratio transducer are provided. The disclosed transducer includes a first cap structure including a substrate, a plurality of first metal interconnect bonding spacer structures, and a high vacuum cavity formed in the substrate to define a first inertial transducer space. The disclosed transducer also includes a first semiconductor substrate structure attached to the plurality of first metal interconnect bonding spacer structures, wherein the first semiconductor substrate structure includes: a first surface, a second patterned metal layer formed on the first surface and the second patterned metal layer bonded to the plurality of first metal interconnect bonding spacer structures, a first high aspect ratio proof mass element aligned with the first inertial transducer space, and a second surface, a plurality of spacer structures formed on the second surface to define an out-of-plane semiconductor sensing electrode space. In addition, the disclosed transducer includes a second semiconductor substrate structure attached to the plurality of spacer structures and including an out-of-plane semiconductor sensing electrode aligned with the first high aspect ratio proof mass element. In the disclosed transducer, at least a first sense gap surface of a first high aspect ratio proof mass element is a first roughened surface that has been selectively etched to reduce stiction between the first high aspect ratio proof mass element and an out-of-plane semiconductor sense electrode. In selected embodiments, the first high aspect ratio proof mass element is a cantilevered single crystal silicon crossbar anchored to a first semiconductor substrate structure, and the out-of-plane semiconductor sense electrode is a polysilicon electrode layer formed in a second semiconductor substrate structure. In other selected embodiments, at least a second sense gap surface of the out-of-plane semiconductor sense electrode is a second roughened surface that has been selectively etched to reduce stiction between the first high aspect ratio proof mass element and the out-of-plane semiconductor sense electrode. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] The present disclosure and its numerous objects, features and advantages achieved will be understood when the following detailed description of the preferred embodiments is considered in conjunction with the following drawings.

[0007] Figure 1 is a simplified cross-sectional view of a Z-axis stiction-reduced MEMS sensor device including a MEMS transducer element in accordance with selected embodiments of the present disclosure.

[0008] Figure 2-Figure 9 is a method for manufacturing a selected embodiment of the present disclosure Figure 1 Simplified cross-sectional views of various exemplary fabrication steps for the MEMS sensor device shown in FIG.

[0009] Fig.10 Depicted is a simplified flow chart showing processing steps for fabricating a Z-axis stiction-reduced MEMS sensor device in accordance with selected embodiments of the present disclosure. DETAILED DESCRIPTION

[0010] A method and apparatus for fabricating a high aspect ratio transducer (i.e., "inertial transducer element") in a MEMS device wafer assembly is described by applying one or more inhomogeneous etching and / or deposition process steps to roughen at least one of the contact surfaces of a single crystal silicon proof mass and / or a polycrystalline silicon electrode, thereby reducing Z-axis stiction for the MEMS device. By forming at least one roughened surface, the effective contact area of ​​the proof mass when contacting the bottom electrode is significantly reduced, thereby reducing adhesion and contact stiction. In selected embodiments, a MEMS device wafer having a deposited polycrystalline electrode layer and a single crystal substrate or proof mass layer undergoes a first patterned transducer etching process of the single crystal substrate or proof mass layer to form one or more single crystal proof mass elements, the single crystal proof mass elements comprising a movable sensor proof mass for a MEMS sensor (e.g., a gyroscope sensor mass), and the MEMS device wafer is subsequently subjected to an inhomogeneous etching step that non-uniformly etches the surfaces of the single crystal proof mass elements and the polycrystalline silicon electrode layer. By selecting a heterogeneous etching process that etches the grain boundaries and nearby regions of the polysilicon electrode layer faster than the rest of the polysilicon electrode layer, valleys are formed in the grain boundary regions and peaks are formed in the non-boundary regions. Thus, the surface roughness of the polysilicon electrode layer is increased. In other selected embodiments, a MEMS device wafer having one or more patterned single crystal proof mass elements undergoes an extremely thin and non-uniform polymer deposition step and a subsequent silicon etching step. By depositing a suitable non-uniform polymer, the subsequent silicon etching step will non-uniformly etch the patterned single crystal proof mass element, thereby producing peaks and valleys in the patterned single crystal proof mass element. This method can increase the surface roughness in both the single crystal silicon surface of the patterned single crystal proof mass element and the polysilicon electrode layer. As should be appreciated, additional processing can be used to form one or more sensor electrodes, driver electrodes, and / or interconnect wiring in the MEMS device.

[0011] Reference now Figure 1, shows a simplified cross-sectional view of a Z-axis stiction-reduced MEMS sensor device wafer assembly 1, according to selected embodiments of the present disclosure, comprising a cap wafer structure (i.e., a "cap device") 200 attached or attached to a MEMS wafer device 100, wherein the MEMS wafer device 100 comprises one or more of a MEMS transducer sensor element (i.e., a "MEMS inertial element") formed in a multi-layer semiconductor structure. Generally speaking, the MEMS wafer device 100 is formed on a single crystalline semiconductor film wafer substrate 101 (i.e., a "first substrate") by selectively forming anchor elements 102 / 104A-E / 106, which include a polycrystalline silicon layer 104D (i.e., a polycrystalline sensing electrode layer 104D) deposited on the single crystalline film wafer substrate 101, along with a planarized dielectric layer 108 and a patterned bonding anchor element 116. A worn or roughened surface layer (collectively referred to as worn or roughened surface layer 114) is formed at exposed sense gap surfaces 114A-F (i.e., "first sense gap surfaces") at single crystal proof mass elements 101A-F (i.e., "first single crystal semiconductor proof mass elements") and polycrystalline sense electrode layers 104D / 115E (i.e., "second conductive electrode elements"). In addition, a cap wafer structure 200 (i.e., "cap device") is formed on single crystal semiconductor wafer 201 by selectively forming defined insulator layers 202, 206 and patterned conductor layer 204, selectively etching single crystal semiconductor wafer 201 to form etched cap cavity 207, and then selectively forming metal bonding anchor elements 208 / 210 / 212.

[0012] In the depicted MEMS wafer device 100, the MEMS transducer sensor element may be a gyroscopic sensor formed of a high aspect ratio single crystal semiconductor proof mass element single crystal 101D including a worn surface 114D (i.e., a "first rough surface") and one or more out-of-plane polycrystalline sensing electrodes 104D / 115E integrated with the MEMS wafer device 100, which is attached or bonded to the cap wafer structure 200 using a metal compression bonding technique. As used herein, and in some embodiments, "worn" or "roughened surface" means a surface having a roughness average (RA) between about 150 angstroms and about 500 angstroms. In other embodiments, the RA of the roughened or worn surface may be between about 100 and about 1,000 angstroms, although other higher or lower RA values ​​may be used. Additionally or in the alternative, a "worn" or "roughened surface" may refer to a polycrystalline semiconductor layer having peaks and / or valleys formed on the surface of a polycrystalline semiconductor layer, such as etched or recessed valleys at polycrystalline grain boundaries and nearby regions and / or peaks at non-boundary surface regions. Additionally or in the alternative, a "worn" or "roughened surface" may refer to a single crystalline semiconductor layer having peaks and valleys on the surface of the single crystalline semiconductor layer, the peaks and valleys being formed by depositing a non-uniform polymer layer on the surface of the single crystalline semiconductor layer followed by an etching process that removes the non-uniform polymer layer to form the peaks and valleys on the surface of the single crystalline semiconductor layer. As should be appreciated, the MEMS transducer sensor element may represent any type of MEMS sensor (e.g., accelerometer, gyroscope, etc.), and any number of MEMS sensor devices may be formed in either or both of the MEMS wafer device 100 and the cap wafer structure 200.

[0013] As formed, the MEMS transducer sensor element may include a single crystal semiconductor proof mass element 101D formed below a high vacuum cavity 207 in a cap wafer structure 200 and suspended within a single crystal semiconductor film wafer substrate 101 by, for example, one or more suspension springs (not shown). In other embodiments, the single crystal semiconductor proof mass element 101D may be formed as a cantilevered single crystal silicon crossbar anchored to a multi-layer semiconductor structure. As disclosed herein and indicated by cross-hatching, roughened or worn surfaces 114A-F are formed on at least the single crystal MEMS proof mass 101D (and, if not, on one or more structural connecting elements 101A-C, 101E-F) by applying one or more inhomogeneous etching and / or deposition process steps. The MEMS transducer sensor element may also include one or more polycrystalline sensing electrodes 104D / 115E positioned to detect vibrational movement of the single crystal MEMS proof mass 101D / 114D. In addition, the MEMS transducer sensor element includes one or more structural connection elements 101A-C, 101E-F formed in the single crystal semiconductor film wafer layer 101, which are coupled to the cap wafer structure 200 (via metal bonding anchor elements (208 / 210 / 212 / 116) and the single crystal handle wafer substrate layer 110 (via bonding anchor elements 102 / 104 / 106 / 108) in a fixed manner. In addition to serving as a mechanical anchor of the proof mass 101D / 114D to the surrounding frame, the structural connection elements (e.g., 101C, 101E) can also serve as a sealing ring structure to seal the high vacuum chamber 200 when the first MEMS wafer device 100 and the first cap wafer structure 200 are bonded together, such as by using a eutectic bonding process. 7 provides a vacuum seal. Additionally or alternatively, the structural connection elements (e.g., 101A, 101F) may also serve as a bonding ring structure formed to couple the first MEMS wafer device 100 to the first cap wafer structure 200 in a fixed manner across the metal bonding anchor elements (208 / 210 / 212 / 116) and to the single crystal handle wafer substrate layer 110 in a fixed manner (via the bonding anchor elements 106 / 104 / 102). Additionally or alternatively, the structural connection elements (e.g., 101B, 101E) may also serve as an electrical interconnect structure that provides an electrical connection between one portion of a circuit in the first MEMS wafer device 100 and another circuit in the first cap wafer structure 200.

[0014] Although shown in simplified cross-sectional views, it should be understood that the MEMS sensor device wafer assembly 1 may also include one or more not shown mobile electrodes and one or more not shown fixed electrodes. The mobile electrodes may form part of the suspended sensor structure 101D / 114D, and the fixed electrodes may be coupled to the single crystal membrane wafer layer 101 and / or the single crystal handle wafer layer 110 in a fixed manner. The specific structure and configuration of the MEMS sensor may vary. In addition, a description of the specific structure and configuration of the MEMS sensor is not required to implement or fully describe the present disclosure, and therefore the specific structure and configuration of the MEMS sensor will not be further described in more detail.

[0015] Having described the embodiment of the MEMS sensor device wafer assembly 1 from a structural perspective, reference will now be made to Figure 2-Figure 9 Describing an example process sequence for manufacturing a MEMS sensor device wafer assembly 1, Figure 2-Figure 9 Simplified cross-sectional diagrams depicting various exemplary manufacturing steps for manufacturing a MEMS sensor device according to selected embodiments of the present disclosure. Although the process sequence depicted is with reference to the manufacturing Figure 1 The method is provided with a MEMS sensor device wafer assembly 1 as shown, but it should be understood that the process is applicable to any of many other MEMS devices and that there are additional process steps not described because they can be formed using any of many processes now known or developed in the future. In addition, although the method is described using a particular order of steps for convenience, portions of the method may be performed in a different order or using different types of steps than those described below.

[0016] First reference Figure 2 , a partial cross-sectional view of a handling wafer structure 2 is shown, the handling wafer structure 2 includes a first substrate 101 and a plurality of defined insulator layers 102, 106, 108 and a conductor layer 104 formed above the first single crystal film wafer substrate 101. Depending on the type of device being manufactured, the first substrate 101 may be formed of: a highly doped (e.g., n-type) single crystal film wafer substrate material, such as a bulk insulator substrate, a bulk metal substrate, a bulk silicon substrate, (doped or undoped) single crystal silicon, a semiconductor on insulator (SOI) substrate; a multi-layer composite thin film wafer substrate or any semiconductor material, including, for example, Si, SiC, SiGe, SiGeC, Ge, GaAs, InAs, InP, and other III-IV compound semiconductors; or any combination thereof. Although not shown, one or more alignment marks may be formed in the first substrate 101 to assist in pattern etching using any desired marking process.

[0017] On a first or top surface of the first substrate 101, a first insulator layer 102 is formed (e.g., grown or deposited). In selected embodiments, the surface of the first substrate 101 is cleaned and a thinner (e.g., 2 microns) oxide layer is thermally grown to passivate the first substrate 101 and provide an etch stop layer for future structural silicon etching processes (described below). Additionally or in the alternative, a field oxide layer, a local oxidation of silicon (LOCOS), or an oxide-nitride-oxide (ONO) layer may be formed. Thus, the insulator layer 102 may be implemented as silicon dioxide or some low-k dielectric material, but may include other materials, such as phosphosilicate glass (PSG) oxide, fluorinated silicon glass (FSG) oxide, silicon nitride, and / or other types of dielectrics, including low-K dielectric materials with higher thermal conductivity for cooling.

[0018] If desired, the first insulator layer 102 may be patterned and etched to form one or more openings, thereby exposing the first substrate 101. Alternatively, a partial etch may be applied to form patterned recessed openings in the first insulator layer 102. Although not shown, a patterned mask layer may be formed over the insulator layer 102, and any desired etching technique may be used to form (recess) openings in the insulator layer 102. The defined openings in the insulator layer 102 may provide an electrical interconnection path to the substrate 101 or otherwise define a ground contact area to the first substrate 101 for a subsequently formed bonding ring structure.

[0019] After forming the patterned insulator layer 102, the first conductive layer 104 may be formed, for example, by depositing a polycrystalline layer 104 that may be doped or implanted to form the first conductive layer 104. In other embodiments, an epitaxial growth process may be used to form the depicted interconnect substrate contacts 104A-E from the exposed portion of the first substrate 101, followed by an optional patterned etching process and / or planarization or polishing step for forming the interconnect substrate contacts 104A-E. When formed with a doped polysilicon layer, the patterned first conductive layer 104 forms various mechanical and electrical functional structures on the first MEMS wafer device 100, such as vertical stop layers, vertical sensing electrodes, electrical interconnects, and bonding ring structures. In selected embodiments, a first conductive layer 104 is formed on the patterned insulator layer 102 and the exposed first substrate 101 using any desired epitaxial growth, deposition, or sputtering process, such as chemical vapor deposition (CVD), plasma enhanced chemical vapor deposition (PECVD), physical vapor deposition (PVD), atomic layer deposition (ALD), molecular beam deposition (MBD), or any combination thereof. A suitable material for the first conductive layer 104 is a doped polysilicon layer deposited to a predetermined thickness of less than 5 microns (e.g., 0.2-1 microns), although other conductive materials with different thicknesses may also be used. However, having formed the first conductive layer 104, a patterned resist or mask layer (not shown) may be formed on the first conductive layer 104 to protect predetermined portions of the first conductive layer 104, and the exposed portions of the first conductive layer 104 may be selectively etched and removed, thereby retaining portions of the first conductive layer 104 in the movable mass or proof mass region, including the interconnect conductors 104A, the interconnect substrate contacts 104B, 104E to the substrate 101, the structural connection elements 104C, and the sensor electrode structures 104D. The pattern transfer and etching of the first conductive layer 104 may remove the unprotected portions of the first conductive layer 104 using one or more etching steps, including: a dry etching process, such as reactive ion etching, ion beam etching, plasma etching, or laser etching; a wet etching process, in which a chemical etchant is employed; or any combination thereof. Although not shown, it should be understood that one or more additional insulators and / or conductive layers may also be formed over the first conductive layer 104 using additional deposition, patterning, and etching processing steps.

[0020] In embodiments where the first conductive layer 104 is formed by depositing a doped polysilicon layer, it will be appreciated that the bottom surface of the first conductive layer 104 is relatively smooth when the first conductive layer 104 is formed on an underlying thermal oxide or insulator layer 102 having a relatively smooth upper surface. However, it will also be appreciated that the upper or top surface of the first conductive layer 104 is relatively rough due to the nature of the polycrystalline structure produced by the polycrystalline deposition process.

[0021] After forming the patterned first conductive layer 104, a second insulator layer 106 may be formed, for example, by depositing a field nitride or aluminum oxide (Al2O3) layer over the semiconductor wafer structure 2 to cover the patterned first conductive layer 104, followed by an optional selective patterning and etching process to selectively form the defined insulator layer 106. Subsequently, a planarization dielectric or insulator layer 108 may be formed over the defined insulator layer 106 to cover the semiconductor wafer structure 2.

[0022] Reference Figure 3 , showing a partial cross-sectional view of the handled wafer structure 3 after forming a planarized dielectric layer 108. In selected embodiments, the planarized dielectric layer 108 may be formed by depositing and planarizing a tetraethyl orthosilicate (TEOS) or silane-based oxide layer over the semiconductor wafer structure 3 to cover the second insulator layer 106 and the first conductive layer 104 and the patterned openings therein. Additionally, a chemical mechanical polishing process or other planarization step may be applied to planarize the planarized dielectric layer 108.

[0023] Reference Figure 4 , showing a partial cross-sectional view of the handling wafer structure 4 after the single crystal film wafer structure 101 is flipped, attached to the handling wafer structure 110 and thinned. In the selected embodiment, the handling wafer structure 110 is a single crystal silicon wafer with good surface smoothness, and provides mechanical support for the subsequent processing of the single crystal film wafer structure 101. Before attaching the handling wafer structure 110 and the film wafer structure 101, a suitable cleaning step is performed to prepare the handling wafer structure 110 for subsequent fusion bonding. After melting the single crystal film wafer structure 101 and the handling wafer structure 110, the single crystal silicon layer 101 can be thinned to a suitable or target thickness to form the final MEMS device layer. For example, a recessing or polishing process can be applied to thin the deposited film wafer substrate layer 101 to a predetermined thickness (e.g., about 25 microns), but other thicknesses may also be required. Although not shown, a germanium (Ge) layer can also be deposited and patterned on the top surface of the single crystal film wafer structure 101 to prepare for eutectic bonding with a cap wafer later.

[0024] Reference Figure 5, shows a partial cross-sectional view of the disposed wafer structure 5 after applying a patterned etching process 111 to the membrane wafer substrate layer 101 to form openings 111A-E, which expose the underlying first insulator layer 102 and define patterned single crystal membrane wafer structure elements 101A-F. In selected embodiments, one or more selective etching processes are applied to form interconnects, bonding and sealing ring structures, and MEMS transducer elements, such as any mechanical elements in a MEMS sensor (e.g., a gyroscope sensor). For example, any suitable photolithography and deep reactive ion etching (DRIE) processes may be applied to fabricate MEMS device structures using a single crystal silicon layer from the membrane wafer substrate 101. Selective etching of the membrane wafer substrate layer 101 forms openings 111A that will expose bonding pad areas in the final formed MEMS device wafer assembly, and also forms openings 111B-E that define patterned single crystal membrane wafer structure elements 101B-F. Although a DRIE process may be used to structurally etch the membrane wafer substrate layer 101 to define the active layer elements 101A-F, it should be appreciated that any desired patterning and etching process may be used, including applying and patterning photoresist directly on the membrane wafer structural layer 101. In selected embodiments, a structural etching process suitable for forming high aspect ratio features is selected.

[0025] Reference Figure 6 , shows a partial cross-sectional view of the handling wafer structure 6 after applying one or more MEMS structure release etching processes 112, wherein the release etching process 112 is used to selectively remove the exposed portion of the first insulator layer 102 and form electrode openings 112A-D, thereby defining all the components of the MEMS sensor device. These components include structural connection elements (e.g., 101B) and bonding ring structures (e.g., 101A, 101F) coupled to the handling wafer substrate 110 in a fixed manner. The components also include sealing ring structures (e.g., 101C, 101E) coupled to the handling wafer substrate 110 in a fixed manner to surround the polycrystalline MEMS proof mass 101D. Finally, the components include mechanical elements 101D of the MEMS sensor device, such as one or more proof mass structures, plates, flexures, frames, and hinges (not shown). In selected embodiments, the release etching process 112 may include a vapor release etch (VPE) applied to remove the thermal oxide layer 102 from under the MEMS proof mass 101D, thereby releasing these components. For example, a single vapor hydrofluoric acid (vHF) etch step may be used to release the MEMS mechanical element 101D by etching away the exposed portion of the first insulator layer 102. The release etch process 112 also removes a portion of the first insulator layer 102 as part of an opening that exposes the bond pad area 111A in the final MEMS device wafer assembly.

[0026] Reference Figure 7 , shows a partial cross-sectional view of the treated wafer structure 7 after applying one or more processing steps 113 to roughen or abrade the sensing gap surfaces of the patterned membrane wafer substrate layers 101A-F and / or the polycrystalline electrode layer 104D, thereby forming roughened or abraded surface layers 114A-F, 115E. In selected embodiments, the one or more processing steps 113 may include applying a heterogeneous etching step that may be controlled to non-uniformly etch the exposed surface 115E of the patterned polycrystalline electrode layer 104D. For example, the heterogeneous etching process 113 may employ plasma etching using sulfur hexafluoride (SF6) and oxygen (O2) chemistry or carbon fluorine chemistry, which etches at least the polycrystalline grain boundaries and nearby regions more rapidly on the upper sensing gap surface 115E of the polycrystalline electrode layer 104D, thereby forming valleys in the grain boundary regions and peaks in the non-boundary regions. Therefore, the surface roughness of the roughened or worn patterned polycrystalline electrode layer 104D at the sensing gap surface 115E increases.

[0027] In other selected embodiments, the processing step 113 may include an extremely thin and non-uniform polymer deposition step, followed by a silicon etching step that etches the formed surface layer and removes the non-uniform polymer layer in the etching process. By the polymer deposition step, the sensing gap surfaces at the bottom of the patterned membrane wafer substrate layers 101A-F and at the top of the sensing polycrystalline gate electrode 104D are coated with non-uniform polymer. Of course, all exposed surfaces of the layers 101A-F, 104D will be coated with the polymer layer, but the relevant area of ​​interest is the sensing gap surface. In an example embodiment, the non-uniform polymer deposition step may use a carbon fluorine chemistry to deposit the extremely thin and non-uniform polymer layers 114A-F, 115E. Due to the nature of the non-uniform polymer layers 114, 115, the subsequent silicon etching step results in non-uniform etching of the sensing gap surface because the removal of the non-uniform polymer layers 114, 115 protects the underlying surface (but not the exposed surface) from etching, thereby creating peaks and valleys in the sensing gap surface 114 at the bottom of the patterned membrane wafer substrate layers 101A-F and the sensing gap surface 115 at the top of the sensing electrode 104D. In selected embodiments, a suitable etching process may be a fluorine or chlorine etching chemistry. As a result, the surface roughness of the roughened or worn patterned polycrystalline layers 114A-F and the sensing electrode surfaces 104D / 115E at the sensing gap surface increases.

[0028] Reference Figure 8, shows a partial cross-sectional view of the handled wafer structure 8 after patterned bonding anchor elements 116A-C, 116E-F are formed on the top surface of the semiconductor wafer structure 8. In selected embodiments, the patterned bonding anchor elements 116A-C, 116E-F are formed as patterned germanium anchor elements by depositing a germanium layer 116 on the semiconductor wafer structure 8. To this end, the top surface of the semiconductor wafer structure 8 may be cleaned, and then the germanium layer may be formed, which is then patterned and etched using a patterned resist or mask layer (not shown) to define the germanium interconnect structures 116A-C, 116E-F in the interconnect, bonding ring, and seal ring areas. If formed prior to etching the membrane wafer substrate layer 101, the deposited germanium layer 116 may be covered by a patterned hard mask layer (e.g., TEOS) that is used to etch the germanium layer 116 and protect the resulting patterned germanium bonding anchor elements 116A-C, 116E-F during subsequent etching of the membrane wafer substrate layer 101.

[0029] Reference Fig. 9 , showing a partial cross section of the cap wafer structure 200 attached to the membrane wafer substrate structure 100 Fig. 9 As depicted, the cap wafer structure 200 includes a second substrate 201 and a plurality of defined insulator layers 202, 206, 208, 210 and conductor layers 204, 212 formed and patterned over the second substrate 201. Depending on the type of device being manufactured, the second substrate 201 may be implemented with: a single crystalline semiconductor material, such as a bulk insulator substrate, a bulk metal substrate, a bulk silicon substrate, (doped or undoped) single crystal silicon, a semiconductor on insulator (SO1) substrate; a multilayer composite thin film wafer substrate or any semiconductor material, including, for example, Si, SiC, SiGe, SiGeC, Ge, GaAs, InAs, InP, and other Group III-IV compound semiconductors; or any combination thereof. On the back side of the second substrate 201, a protective insulator layer 201A may be formed, for example, by thermally growing an oxide layer 201a (e.g., silicon oxide) to a predetermined thickness.

[0030] To manufacture the top cover wafer structure 200, a first insulator layer 202 is formed (e.g., grown or deposited) on a first or top surface of a second substrate 201, for example by cleaning the surface of the second substrate 201, followed by thermal growth of a thinner (e.g., 2 microns) layer of passivation oxide or other insulator material, such as PSG oxide, FSG oxide, silicon nitride and / or other types of dielectrics, including low-K dielectric materials with higher thermal conductivity for cooling.

[0031] Additionally, the first insulator layer 202 may be patterned and selectively etched to form one or more openings, thereby exposing the second substrate 201. For example, a patterned mask layer (not shown) may be formed over the insulator layer 202, and a selective etching process may be applied to form openings in the insulator layer 202 that expose the second substrate 201, the openings providing electrical interconnection paths to conductive lines or paths (not shown) in the substrate 201.

[0032] After forming the insulator layer 202, a first conductive layer 204 may be formed by depositing a metal or conductive polysilicon layer on the cap wafer structure 200 using any desired deposition or sputtering process (e.g., CVD, PECVD, PVD, ALD, MBD, or any combination thereof). In a selected embodiment, the first conductive layer may be a deposited aluminum layer. Once deposited, the first conductive layer 204 may be patterned and etched to define electrodes, interconnects, and bonding ring structures on the first cap wafer structure 200. For example, a patterned resist or mask layer (not shown) may be formed to protect a predetermined portion of the first conductive layer 204, and the exposed portion of the first conductive layer 204 may be selectively etched and removed, thereby retaining portions of the first conductive layer 204 (including the interconnect conductor 204A and the interconnect substrate contact 204B to the substrate 201), but other patterned conductive layers (e.g., interconnect structures and sensor electrode structures) may also be formed. The pattern transfer and etching of the first conductive layer 204 may use one or more etching steps to remove unprotected portions of the first conductive layer 204, wherein the etching steps include: a dry etching process, such as reactive ion etching, ion beam etching, plasma etching, or laser etching; a wet etching process, in which a chemical etchant is used; or any combination thereof.

[0033] In selected embodiments, a patterned first conductive layer 204 is used to bond the cap wafer structure 200 to the membrane wafer substrate structure 100. For example, the patterned aluminum first conductive layer 204 can serve the dual purpose of conductive interconnection and Al-Ge bonding with the patterned bonding anchor elements 116A-C, 116E-F, thereby eliminating the need to form separate raised portion structures 206, 208, 210, 212, as described below.

[0034] However, in other embodiments, a separate standoff structure is formed on the patterned first conductive layer 204 by forming a second insulator layer 206 on the cap wafer structure 200, for example, by depositing one or more interlayer dielectric (ILD) layers to a predetermined thickness over the cap wafer structure 200. In selected embodiments, the second insulator layer 206 may be formed by depositing and planarizing a first cap oxide layer 206 over the cap wafer structure 200 to cover the first conductive layer 204 and the patterned openings therein. Subsequently, a cap etch stop layer 208 (e.g., silicon nitride) and a second cap oxide layer 210 are sequentially deposited, patterned, and etched to form patterned standoff elements 208 / 210 that are positioned to align with the patterned bonding anchor elements 116A-C, 116E-F during bonding. Additionally, one or more patterned etching processes may be applied to selectively etch the first cap oxide layer 206 and expose the underlying first conductive layer 204 at predetermined via openings.

[0035] In preparation for bonding, a patterned cap metal bonding anchor element 212 is formed on the cap wafer structure 200. For example, when forming the metal bonding anchor element 212 with patterned aluminum, the aluminum layer can be deposited or sputtered to a predetermined thickness (e.g., 1-2 microns), although other deposition processes, materials, and thicknesses can also be used. Once deposited, a photolithographic mask and etching process are applied to define the aluminum bonding anchor element 212 located in the bonding pad area and used to align with the patterned bonding anchor elements 116A-C, 116E-F from the first MEMS wafer device 100. Although Fig. 9 Two patterned interconnect layers 210 , 212 are shown formed on the cap wafer structure 200 , but those skilled in the art will appreciate that the cap wafer structure 200 may also be formed with additional (three or more) or fewer (one) electrical interconnect layers.

[0036] Before or after forming the patterned cap metal bonding anchor element 216, a cap cavity 207 may be formed in the second substrate 201 by patterning and etching the cap wafer structure 200. For example, a patterned cap resist or mask layer (not shown) may be formed to expose and remove the cap oxide layer 206 above a given cap cavity 207, followed by selectively removing the exposed portion of the second substrate 201 to form a cap cavity 207 of a predetermined depth and width, the cap cavity 207 being positioned for alignment with the patterned polycrystalline MEMS proof mass 101D from the MEMS wafer device 100. The pattern transfer and etching of the second substrate 201 may use one or more silicon etching steps, including: a dry etching process, such as reactive ion etching, ion beam etching, plasma etching, or laser etching; a wet etching process, in which a chemical etchant is employed; or any combination thereof.

[0037] like Fig. 9 , the top cover wafer structure 200 has been turned upside down in preparation for bonding the attachment 300 to the top of the fusion bonded membrane / handling wafer structure 100. In preparation for bonding, the handling wafer structure 100 and the top cover wafer structure 200 can be cleaned separately, for example, by using a non-oxidative ash chemistry or a solvent-based wet removal process that does not oxidize the underlying metal layer. In selected embodiments, the MEMS handling wafer structure 100 and the top cover wafer structure 200 are bonded together using metal compression bonding techniques, such as a combination of heat and pressure bonding. For example, AlGe bonding techniques can be used to provide both a hermetic seal to the cavity (e.g., 207) to enclose the released MEMS structure, and an electrical connection between the MEMS structure and the top cover wafer structure 200.

[0038] The above-mentioned metal thermocompression bonding technique provides an airtight barrier between the MEMS transducer structure 101D (formed by the MEMS handling wafer structure 100) and the surrounding environment, which is superior to the sealing performance provided by the oxide or glass sealing technology. However, it is expected that other bonding techniques can be used to obtain additional sealing protection. For example, instead of using thermocompression bonding technology to bond the aligned aluminum bonding anchor elements 212 and 116A-C, 116E-F, the bonding anchor elements 116A-C, 116E-F are replaced with patterned germanium anchor elements 116A-C, 116E-F, so that an aluminum-germanium eutectic bond can be formed to bond the MEMS handling wafer structure 100 and the top cover wafer structure 200 together. To this end, the protective top cover wafer structure 200 and the MEMS handling wafer structure 100 are bonded together using aluminum-germanium eutectic bonding under vacuum conditions. Therefore, the high aspect ratio polycrystalline MEMS proof mass structure 110D formed by the MEMS handling wafer structure 100 can be hermetically sealed.

[0039] In other embodiments where the bonding anchor elements 212 and 116A-C, 116E-F are formed of patterned aluminum, the aluminum layers can be bonded together using thermocompression bonding, where the anchor elements are aligned in contact while heat and compression are applied to bond the aligned anchor elements to each other. In selected example embodiments, thermocompression bonding can be performed by applying a pressure at or above a predetermined threshold (e.g., 30 MPa) in combination with a relatively low temperature heat treatment (e.g., at or below 500 degrees Celsius). For example, aluminum thermocompression bonding can be performed by aligning and compressing the first MEMS handle wafer structure 100 and the cap wafer structure 200 with a force of 70-90 kilonewtons while heating the wafer structures 100, 200 to 400-500 degrees Celsius for about 30-50 minutes. By attaching the MEMS handle wafer structure 100 to the first cap wafer structure 200 using metal-to-metal bonding techniques, the MEMS transducer structure formed by the MEMS handle wafer structure 100 may be hermetically sealed by the bonding and sealing ring structures 208 / 210 / 212 / 116 / 110 / 106 / 104 .

[0040] As will be appreciated, additional or different processing steps may be used to complete the fabrication of the depicted MEMS device wafer assembly into a functional device. In addition to various front-end processing steps (e.g., sacrificial oxide formation, stripping, isolation region formation, implantation, spacer formation, annealing, silicide formation, and polishing steps), additional back-end processing steps may also be performed, such as forming contact plugs and multi-level interconnects for connecting device components in a desired manner to achieve the desired functions. Therefore, depending on process and / or design requirements, the specific sequence of steps for completing the manufacture of device components may vary. It should be understood that the terms so used are interchangeable where appropriate, such that the embodiments of the invention described herein are, for example, capable of operating in other orientations than those shown or otherwise described herein.

[0041] In order to provide additional details to improve the contextual understanding of selected embodiments of the present disclosure, reference is now made to Fig.10 , Fig.10 Depicts a simplified flow chart showing process steps 1000-1009 for fabricating a Z-axis stiction-reduced MEMS sensor device Fig.10 After processing begins at step 1000, a membrane wafer having a polycrystalline electrode layer and a single crystal proof mass layer is fabricated (step 1001). As will be appreciated, the membrane wafer 101 may be fabricated on a first crystalline silicon wafer substrate using a series of processing steps to deposit, pattern, and etch an insulator layer and a conductive polycrystalline sensing electrode layer, thereby defining a MEMS wafer interconnect layer and a sensing electrode layer. For example, Figure 3A semiconductor wafer structure 3 is shown having a single crystalline proof mass layer 101 , a plurality of insulator layers 102 , 106 , 108 , a conductive polycrystalline electrode layer 104 , and one or more covering insulator layers 106 , 108 .

[0042] At step 1002, a handle wafer 110 is fabricated. As should be appreciated, the handle wafer may be fabricated with a second crystalline silicon wafer substrate.

[0043] At step 1003, the membrane wafer 101 is bonded to a handle wafer. In this way, the handle wafer provides mechanical support for subsequent processing of the membrane wafer. For example, Figure 4 A handle wafer structure 4 is shown with a handle wafer 110 bonded to a planarized dielectric layer 108 on a membrane wafer 101. After bonding the membrane wafer to the handle wafer, the single crystal proof mass layer 101 of the membrane wafer 101 may be thinned to a target thickness to form the final MEMS device layer.

[0044] At step 1004, a cap wafer is fabricated. As will be appreciated, the cap wafer may be fabricated using a third crystalline silicon wafer substrate that is processed using a series of processing steps to deposit, pattern, and etch the insulator layer and the conductive layer, respectively. For example, the cap wafer may be processed using a deep reactive ion etching (DRIE) process 111 to form a through silicon via (TSV) array to selectively etch the third crystalline silicon wafer substrate, followed by a polysilicon deposition process and a chemical mechanical polishing step to form the TSVs.

[0045] At step 1005, a single crystal proof mass layer on the membrane wafer is selectively etched. For example, a patterned transducer resist or mask layer is formed on the single crystal proof mass layer to protect selected portions of the single crystal proof mass layer, and then a deep reactive ion etching (DRIE) process may be used to selectively etch and remove exposed portions of the single crystal proof mass layer. The selective etching of the single crystal proof mass layer defines a single crystal MEMS proof mass element secured to the membrane wafer.

[0046] A release etch process is applied to the membrane wafer to release the single crystal MEMS proof mass elements at step 1006. In selected embodiments, the release etch process may include a vapor release etch (VPE) applied to remove sacrificial dielectric or insulator layers from beneath the MEMS proof mass elements, thereby releasing these elements.

[0047] The membrane wafer and handle wafer are bonded to a cap wafer at step 1007. In selected embodiments, the cap wafer is bonded to the combined membrane / handle wafer using AlGe eutectic bonding.

[0048] Additional MEMS wafer processing steps are applied at step 1008. For example, the cap wafer may be thinned and contacts to TSVs and redistribution wiring layers (RDLs) fabricated before a final passivation step.

[0049] At step 1009 , the manufacturing process ends.

[0050] Various illustrative embodiments of the present disclosure have been described in detail with reference to the accompanying drawings. Although various details are set forth in the foregoing description, it should be understood that the present disclosure can be practiced without these specific details, and many implementation-specific decisions can be made to the present disclosure described herein to achieve the specific goals of the device designer, such as compliance with process technology or design-related constraints, which vary from implementation to implementation. Although this development work may be complex and time-consuming, it is nothing more than a routine task routine for those of ordinary skill in the art who benefit from the present disclosure. For example, selected aspects are described with reference to simplified cross-sectional views of example MEMS device wafer structures, without including each device feature or geometry, to avoid limiting or obscuring the present disclosure. In addition, the method of the present disclosure can be applied using materials different from those explicitly set forth herein. In addition, the process steps can be performed in other alternative orders different from the order presented. For example, the order of the wafer bonding step can be reversed. In addition, it should be noted that throughout this specific embodiment, certain material layers will be deposited and removed to form the depicted MEMS device wafer structure. Without describing in detail specific procedures for depositing or removing such layers, any desired technique may be used to deposit, remove, or otherwise form such layers at an appropriate thickness. Such details are well known and are not considered necessary to teach one skilled in the art how to make or use the present disclosure. In addition, while the disclosed MEMS devices may be implemented with accelerometers and / or gyroscope sensors, the manufacturing processes described herein are not limited to such MEMS sensors or any other type of sensor, but are also applicable to any of a number of MEMS devices that include a certain type of structure that is movably suspended by one or more springs and formed by bonding an active wafer to a reference wafer. Non-limiting examples of such devices include various types of accelerometers and switches, optical MEMS system components, and other MEMS system devices that use drive and sense electrodes.

[0051] It should also be noted that throughout this specific embodiment, certain elements in the drawings are illustrated for simplicity and clarity and are not necessarily drawn to scale, so that the illustrated dimensions of some elements in the drawings may be enlarged relative to other elements to help improve the understanding of embodiments of the present invention. Therefore, the specific embodiments disclosed above are only illustrative and should not be regarded as limitations of the present invention, because the present invention can be modified and practiced in different but equivalent ways, which are obvious to those skilled in the art who benefit from the teachings herein. Therefore, the foregoing description is not intended to limit the present invention to the specific form set forth, but on the contrary, it is intended to cover such alternatives, modifications and equivalents as may be included in the spirit and scope of the present invention as defined by the appended claims, so that those skilled in the art should understand that they can make various changes, substitutions and variations in its broadest form without departing from the spirit and scope of the present invention.

[0052] Benefits, other advantages, and solutions to problems have been described above with respect to specific embodiments. However, these benefits, advantages, solutions to problems, and any elements that may make any benefit, advantage, or solution occur or become more obvious should not be construed as important, necessary, or essential features of the elements of any or all claims. As used herein, the term "comprises" or any other variation thereof is intended to cover a non-exclusive inclusion, such that a process, method, article, or apparatus that includes a list of elements includes not only those elements, but may also include other elements not expressly listed or inherent to such process, method, article, or apparatus.

Claims

1. A MEMS sensor device, characterized in that: include: a first inertial converter element formed in a multi-layer semiconductor structure; as well as a capping device bonded to the multi-layer semiconductor structure to protect the first inertial transducer element from ambient environmental conditions, wherein the first inertial transducer element comprises a first single crystal semiconductor proof mass element and a second conductive electrode element separated from each other by an air sensing gap, and Wherein at least a first sensing gap surface of the first single crystal semiconductor proof mass element is a first roughened surface that has been selectively etched to reduce stiction between the first single crystal semiconductor proof mass element and the second conductive electrode element.

2. The MEMS sensor device according to claim 1, characterized in that: At least a second sensing gap surface of the second conductive electrode element is a second roughened surface that has been selectively etched to reduce stiction between the first single crystalline semiconductor proof mass element and the second conductive electrode element.

3. The MEMS sensor device according to claim 1, characterized in that: The first inertial transducer element includes a z-axis accelerometer sensor.

4. The MEMS sensor device according to claim 1, characterized in that: The first single crystal semiconductor proof mass element includes a cantilevered single crystal silicon crossbar anchored to the multi-layer semiconductor structure.

5. The MEMS sensor device according to claim 4, characterized in that: The second conductive electrode element includes a conductive polysilicon layer formed in the multi-layer semiconductor structure, the conductive polysilicon layer to be positioned aligned with but separated from the cantilevered single crystal silicon crossbar.

6. The MEMS sensor device according to claim 1, characterized in that: The cap assembly is bonded to the multi-layer semiconductor structure using a high temperature eutectic seal ring bonding structure to form a vacuum in a first sensor cavity housing the first inertial transducer element.

7. The MEMS sensor device according to claim 1, characterized in that: At least the first sensing gap surface of the first single crystalline semiconductor proof mass element includes an unevenly deposited polymer layer that has been selectively etched to form the first roughened surface.

8. The MEMS sensor device according to claim 2, characterized in that: At least the second sensing gap surface of the second conductive electrode element includes an unevenly deposited polymer layer that has been selectively etched to form the second roughened surface.

9. A method for manufacturing a converter, characterized in that: include: Providing a MEMS wafer structure comprising a first semiconductor electrode and a first semiconductor layer formed above the first semiconductor electrode; selectively etching the first semiconductor layer to form a first MEMS inertial transducer element and a surrounding frame support element; applying a structure release etching process to release the first MEMS inertial transducer element and expose a first sensing gap surface of the first MEMS inertial transducer element and a second sensing gap surface of the first semiconductor electrode; applying a surface wear etching process to roughen one or both of the first sensing gap surface of the first MEMS inertial transducer element or the second sensing gap surface of the first semiconductor electrode, thereby reducing stiction between the first MEMS inertial transducer element and the first semiconductor electrode; as well as A first cap wafer structure is attached to the MEMS wafer structure using a first bonding process.

10. A high aspect ratio converter, characterized in that: include: a first cap structure including a substrate, a plurality of first metal interconnect bonding spacer structures, and a high vacuum cavity formed in the substrate to define a first inertial converter space; a first semiconductor substrate structure attached to the plurality of first metal interconnect bonding spacer structures, the first semiconductor substrate structure comprising: a first surface, a second patterned metal layer formed on the first surface and the second patterned metal layer bonded to the plurality of first metal interconnect bonding spacer structures, a first high aspect ratio proof mass element spatially aligned with the first inertial transducer, and a second surface on which a plurality of spacer structures are formed to define out-of-plane semiconductor sensing electrode spaces; as well as a second semiconductor substrate structure attached to the plurality of spacer structures and comprising an out-of-plane semiconductor sense electrode aligned with the first high aspect ratio proof mass element, wherein at least a first sensing gap surface of the first high aspect ratio proof mass element is a first roughened surface that has been selectively etched to reduce stiction between the first high aspect ratio proof mass element and the out-of-plane semiconductor sense electrode.