Repairing method for reading circuit of ultra-large area array infrared focal plane detector
Through OBIRCH testing and FIB-SEM etching technology, the fault points caused by metal residues in infrared focal plane detectors are accurately positioned and repaired, solving the problem of high difficulty in repairing the readout circuit, improving the yield rate and reducing costs.
Patent Information
- Application Number
- CN202410945746.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-15
- Publication Date
- 2024-11-12
AI Technical Summary
The difficulty of repairing readout circuit faults caused by the increase in chip size in infrared focal plane detectors is very difficult, and the existing technology cannot accurately locate and repair circuit bridge phenomenon caused by metal residues, which affects the yield rate and cost.
The XY coordinates of the fault point were determined by using the OBIRCH tester, and the FIB-SEM dual-beam scanning electron microscope was etched layer by layer to form a stepped structure until the circuit layer completely disappeared in the fault point area, combined with the beam current and gas-assisted etching system repair.
Accurate positioning and repair of fault points is achieved, the difficulty of repair is reduced, the uniformity and yield of the circuit are improved, the repair steps and material waste are reduced, and the overall repair cost is reduced.
Smart Images

Figure CN118943035A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of infrared focal plane detectors, and in particular to a method for repairing a readout circuit of an ultra-large array infrared focal plane detector. Background Art
[0002] Infrared focal plane array technology has developed from a small scale (such as 128×128 pixels) at the beginning of this century to a large scale (such as 1k×1k pixels) array produced at a low rate at the end of this century. The maturity of large-array infrared focal plane array technology has provided astronomers with new capabilities for wide field of view, high-resolution imaging and spectral analysis. With the improvement of the focal plane preparation process, the scale of single linear and array focal plane devices has continued to expand, and the development of infrared focal plane detectors has begun to pursue larger arrays.
[0003] As the number of detector arrays continues to increase, it is necessary to consider the problems caused by increasing the chip size of the detector. The increase in chip size leads to an increase in the size of the readout circuit and the size of the detector material and restricts the scale of infrared detectors, making them difficult to manufacture and difficult to solve problems such as low cost, high performance and high uniformity.
[0004] The increase in chip size leads to a larger readout circuit size. The processing technology of large-size chips at the front-end manufacturing (FAB) plant is unstable and has poor consistency. Metal residues lead to circuit bridging, which makes the electrical signal output abnormal and the chip yield is low, seriously affecting the subsequent readout circuit testing and optimization. Therefore, it is necessary to repair the faulty circuit to save financial, material and time costs.
[0005] Since the metal residue in the circuit processing process is random and its shape and position are uncontrollable, online detection means cannot locate and remove it in time, resulting in it being covered in subsequent processes.
[0006] As a solution to the problem of metal residue, the circuit design can be changed: first test the existing circuit to obtain its performance, and then concentrate on the contents that need to be improved during the second tape-out process to save processing costs; however, the existing circuits have more or less circuit bridging and cannot be used normally, so the circuit needs to be fault-located and repaired.
[0007] In the related technology, the method for locating the fault point is to use the optical beam induced resistance change (OBIRCH) technology for positioning, but it is impossible to accurately locate the shape, size, and depth of the metal residue; and the conventional circuit repair method is mainly to cut off redundant lines and overlap multiple circuits. Since the metal residue may not be a simple line connection, it is impossible to give an accurate circuit repair plan, which makes the circuit repair very difficult. Summary of the invention
[0008] The invention provides a method for repairing a readout circuit of an ultra-large array infrared focal plane detector, which solves the problem that the readout circuit is difficult to repair a fault caused by metal residue in the infrared focal plane detector.
[0009] In order to achieve the above objectives, this application adopts the following technical solutions:
[0010] A method for repairing a readout circuit of an ultra-large array infrared focal plane detector is provided, comprising:
[0011] Conduct continuity test on the chip to screen out faulty chips;
[0012] A rectangular coordinate system is established based on the surface of the faulty chip, and a fault point of a readout circuit and its XY coordinate area are determined on the surface of the chip by an OBIRCH tester;
[0013] The fault point is marked by the laser of the OBIRCH tester and marked by a marker pen;
[0014] The XY coordinate area of the fault point is etched layer by layer from the surface of the circuit layer to the inside thereof by using a FIB-SEM dual-beam scanning electron microscope, and the etching area is reduced layer by layer to form a stepped etching structure until the circuit layer in the fault point area completely disappears.
[0015] In a first possible implementation manner, the method further includes:
[0016] Testing whether the resistance value of the faulty chip meets the use requirements;
[0017] If the resistance value does not meet the use requirements, a certain range of areas is set with the fault point as the center, and bombardment cleaning is performed using the FIB-SEM dual-beam scanning electron microscope with a set beam current and time, and then the resistance value is retested to see if it meets the use requirements.
[0018] Based on the first possible implementation manner, in a second possible implementation manner, an area of the region within a certain range is larger than an area of an XY coordinate region of the fault point.
[0019] Based on any of the foregoing possible implementations, in a third possible implementation, the mark is a recessed area of a specific size.
[0020] Based on any of the above possible implementations, in a fourth possible implementation, the XY coordinate region of the fault point is etched layer by layer from the surface of the circuit layer to the inside thereof by a FIB-SEM dual-beam scanning electron microscope, and the etching region is reduced layer by layer to form a stepped etching structure until the circuit layer in the fault point region completely disappears, including:
[0021] Step a, taking the fault point as the center, setting the physical area of the i-th set value, and etching a passivation layer by using the set beam current and the IEE gas-assisted etching system; keeping the beam current unchanged, and then etching a metal layer by using the EE gas-assisted etching system;
[0022] Step b, taking the fault point as the center, setting the physical area of the i+1th set value, keeping the beam current unchanged, etching a passivation layer with the IEE gas-assisted etching system, and then etching a metal layer with the EE gas-assisted etching system while keeping the beam current unchanged;
[0023] Repeat step a to step b until the remaining circuit layer in the physical area of the Nth set value completely disappears.
[0024] Based on the fourth possible implementation manner, in a fifth possible implementation manner, the shape of the entity area is rectangular or circular.
[0025] Based on the fourth possible implementation manner, in a sixth possible implementation manner, the i-th set value is greater than the (i+1)-th set value.
[0026] Based on the fourth possible implementation, in a seventh possible implementation, bombardment cleaning is performed by using the FIB-SEM dual-beam scanning electron microscope with a set beam current and time, specifically including:
[0027] The EE gas-assisted etching system was used to bombard the sample for 3 minutes using a set beam current.
[0028] Beneficial effects:
[0029] By using the OBIRCH tester, the present application can accurately determine the size and XY coordinates of the fault point; by reducing the etching area layer by layer, the fault point can be accurately isolated or repaired, the defective area is turned into a short circuit, and the resistance of the entire circuit is restored to normal, while avoiding excessive damage to the surrounding normal circuits, and can still be used for subsequent infrared detector processing technology. Compared with traditional repair methods, the present application reduces the difficulty of repairing the readout circuit, has a better repair effect, and a more efficient fault point repair process, which can reduce unnecessary repair steps and material waste, thereby reducing the overall repair cost; the present application is not only suitable for short-circuit repair of circuit chips, but also can provide reference and reference for the detection, positioning and repair of other micro-nano structures, and promote technological progress and development in related fields. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 A schematic flow chart of a method for repairing a readout circuit of an ultra-large array infrared focal plane detector provided in an embodiment of the present application;
[0031] Figure 2 A schematic diagram of the steps of marking a fault point and marking it with a marker pen provided in an embodiment of the present application;
[0032] Figure 3 An actual effect diagram of a step of marking a fault point and marking it with a marker pen provided in an embodiment of the present application;
[0033] Figure 4 A schematic diagram of a layer-by-layer etching step and a stepped etching structure provided in an embodiment of the present application;
[0034] Figure 5 An actual effect diagram of a rectangular stepped etching structure provided in an embodiment of the present application;
[0035] Figure 6 An actual effect diagram of a circular stepped etching structure provided in an embodiment of the present application;
[0036] Figure 7 A flowchart of another method for repairing a readout circuit of an ultra-large array infrared focal plane detector provided in an embodiment of the present application. DETAILED DESCRIPTION
[0037] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined purpose, the technical solutions in the embodiments of the present application are clearly described. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field belong to the scope of protection of the present application.
[0038] The terms "first", "second", etc. in the specification and claims of the present application are used to distinguish similar objects, and are not used to describe a specific order or sequence. It should be understood that the terms used in this way are interchangeable where appropriate, so that the embodiments of the present application can be implemented in an order other than those illustrated or described herein, and the objects distinguished by "first", "second", etc. are generally of one type, and the number of objects is not limited. For example, the first object can be one or more. In addition, "and / or" in the specification and claims represents at least one of the connected objects, and the character " / " generally indicates that the objects associated with each other are in an "or" relationship.
[0039] The description of the method flow in the specification of the present application and the steps of the flowchart in the drawings of the present specification do not have to be strictly executed according to the step numbers, and the method steps can be executed in a different order. Moreover, some steps can be omitted, multiple steps can be combined into one step, and / or one step can be decomposed into multiple steps.
[0040] The following is a detailed description of the method for repairing the readout circuit of the ultra-large array infrared focal plane detector provided in the embodiment of the present application in combination with the accompanying drawings and preferred embodiments.
[0041] First, the application scenario of the method for repairing the readout circuit of a very large array infrared focal plane detector according to an embodiment of the present application is described in detail.
[0042] The readout circuit of the ultra-large array is a multi-layer circuit structure. At the same time, the size of a single chip is as high as tens of millimeters, and the processing area is large, resulting in poor uniformity and consistency of circuit processing, and even multiple defects, among which excess metal residue is the most typical. Excess metal residue causes short circuits between adjacent metal lines on the same layer or short circuits between two adjacent layers of metal at the same position, and bridging occurs, causing circuit failure and inability to power on. Due to the uncertainty of metal residue, the cause of the failure may not be a simple line connection, but also include tiny particles or films that are more difficult to identify and process.
[0043] There are two problems that need to be solved during the circuit repair process: First, the fault point is inside the circuit, and it is impossible to use optical or electro-optical methods to observe and determine the location of the fault point. In the related technology, the conventional positioning method is the laser thermal effect excited resistance change technology (OBIRCH), which uses a laser beam with a wavelength of 1340nm to heat the integrated circuit point by point. If the resistance value of a device or a certain area on the integrated circuit changes due to the increase in temperature, under constant voltage conditions, the current drawn by the corresponding lead will change due to the increase in temperature. OBIRCH locates the leakage current point in the integrated circuit and the abnormal area of the semiconductor material (ie, defect) by detecting the change in current, so it is impossible to accurately determine the shape, size and depth of the metal residue. Second, the conventional repair method is difficult to repair the bridging phenomenon caused by metal residues, which is time-consuming and labor-intensive, and even difficult to achieve effective repair.
[0044] Therefore, an embodiment of the present application proposes a readout circuit repair method for an ultra-large array infrared focal plane detector. A surface detection method is combined with a marking method to establish a connection between the internal fault point and the surface mark, thereby achieving precise positioning of the fault point. Then, based on an etching method, an etching operation is performed on the located defective area to form a stepped structure, thereby turning the defective area into a short circuit. At this time, the resistance of the entire circuit returns to normal and can still be used for subsequent infrared detector processing technology.
[0045] See also Figure 1 The present application embodiment provides a method for repairing a readout circuit of an ultra-large array infrared focal plane detector, such as Figure 1 As shown, the readout circuit repair method of the embodiment of the present application includes:
[0046] Step S1, performing a conduction test on the chips to screen out faulty chips.
[0047] Solder the pin leads of the circuit chips processed by the FAB factory, test the conductivity, and screen out the short-circuited chips.
[0048] Step S2, establishing a rectangular coordinate system based on the surface of the faulty chip, and determining the fault point of the readout circuit and its XY coordinate area on the chip surface by using an OBIRCH tester.
[0049] Use the OBIRCH tester to test the short-circuited chip and determine the size of the fault point and the XY coordinates.
[0050] Step S3, marking the fault point by using the laser of the OBIRCH tester and marking it with a marker pen; the marking is a concave area of a specific size.
[0051] See also Figure 2-3 , Figure 2 is a schematic diagram of this step. Figure 3 This is the actual effect diagram of this step. The fault point is marked with the laser of the OBIRCH tester and marked with a marker pen. The mark is a laser-etched recessed area, and its size can be set according to the actual situation.
[0052] For example, the mark can be 15 μm×10 μm×2 μm in size and is marked with a professional marker. The etched mark is difficult to find, so a simple and intuitive mark is combined with a marking method to facilitate finding under a FIB-SEM dual-beam scanning electron microscope in the subsequent step.
[0053] Step S4, etching the XY coordinate area of the fault point from the circuit layer surface to the inside layer by layer through a FIB-SEM dual-beam scanning electron microscope, and gradually reducing the etching area to form a stepped etching structure until the circuit layer in the fault point area completely disappears.
[0054] See also Figure 4In the specific implementation, a specific beam current (such as (2.5-9.3) nA) and a gas-assisted etching system (such as IEE and EE) are used for precise control, and the materials around the fault point (such as the passivation layer and the metal layer) are etched layer by layer, and the etching area is gradually reduced in a step-like manner until the fault point is completely isolated or repaired, including: step a, taking the fault point as the center, setting a physical area of the i-th set value, and etching a passivation layer with a set beam current and an IEE gas-assisted etching system; the beam current remains unchanged, and then a metal layer is etched with an EE gas-assisted etching system;
[0055] Step b, taking the fault point as the center, setting the physical area of the i+1th set value, keeping the beam current unchanged, etching a passivation layer with the IEE gas-assisted etching system, and then etching a metal layer with the EE gas-assisted etching system while keeping the beam current unchanged;
[0056] Repeat step a to step b until the remaining circuit layer in the physical area of the Nth set value completely disappears.
[0057] Among them, the i-th setting value is greater than the i+1-th setting value.
[0058] Exemplarily: the fault point size is 10 μm×4 μm;
[0059] With the fault point as the center, a φ40μm solid circular area or a rectangular solid area is set, and a passivation layer is etched using a (2.5~9.3)nA beam current and an IEE gas-assisted etching system. The beam current remains unchanged and then a metal layer is etched using the EE gas-assisted etching system; with the fault point as the center, a φ35μm solid circular area is set, and the beam current remains unchanged and an IEE gas-assisted etching system is used to etch a passivation layer. The beam current remains unchanged and then a metal layer is etched using the EE gas-assisted etching system; with the fault point as the center, a φ30μm solid circular area is set, and the beam current remains unchanged and an IEE gas-assisted etching system is used to etch a passivation layer. The beam current remains unchanged and then a metal layer is etched using the EE gas-assisted etching system; with the fault point as the center, a φ25μm solid circular area is set, and the beam current remains unchanged. The IEE gas-assisted etching system is used to etch until the remaining circuit layer in the area completely disappears, and then the chip is removed.
[0060] See also Figure 5-6 In some possible practical methods, the shape of the XY coordinate area of the fault point that is etched layer by layer can be any geometric figure. The embodiment of the present application uses rectangular or circular areas to etch layer by layer, and the corresponding stepped etching structure is shown in the figure.
[0061] See also Figure 7 In some possible implementations, the method further includes:
[0062] Step S5, testing whether the resistance value of the faulty chip meets the use requirements.
[0063] Step S6, if the resistance value does not meet the use requirements, a certain range of areas is set with the fault point as the center, and bombardment cleaning is performed by the FIB-SEM dual-beam scanning electron microscope with a set beam current and time, and then the resistance value is retested to see if it meets the use requirements. The area of the re-set certain range of areas is slightly larger than the area of the XY coordinate area of the fault point.
[0064] With the fault point as the center, set a rectangular area of a certain size (such as 45μm×35μm), use appropriate beam current and time to bombard and clean, and then retest the resistance value. If it still does not meet the use requirements, you can choose to repeat step S6, or steps S2-S6 again.
[0065] Exemplarily, the chip resistance value is tested to see if it meets the use requirements. If it is lower than the use requirements, the EE gas-assisted etching system needs to be used to clean the exposed metal wires on the sidewalls. Taking the operation of step S4 as an example, a solid rectangular area of 45μm×35μm is set with the fault point as the center, and the chip resistance value is retested after bombarding with a beam current of (2.5-9.3)nA for 3 minutes with the help of the EE gas-assisted etching system. Among them, the parameters such as beam current, pattern size and shape can be adjusted according to the specific process.
[0066] The principles of this application are:
[0067] The OBIRCH test cannot determine the exact shape and depth of the excess metal, but because the circuit wiring is a mesh structure, hollowing out the circuit layer in a certain area will not affect the electrical signals in other areas. Therefore, the defective area can be directly etched in a large area, so that the interior of the area is hollowed out to form a stepped pit, and the exposed metal on the side wall is etched flat to solve the problem of short circuits between adjacent metals on the side wall. The short circuit problem that originally caused the resistance value to be low and unable to be powered on is turned into a short circuit in the etched area. Although the pixels in the etched area become blind pixels in the later testing process, due to the mesh design of the circuit, the pixels in other areas are still in normal voltage state and can still be imaged normally.
[0068] For ultra-large array readout circuits, defects are located under infrared and visible laser points are located through defect positioning and laser marking. The FIB-SEM dual-beam scanning electron microscope etches the defect area to make it a short circuit, and the resistance of the entire circuit returns to normal. It can still be used for subsequent infrared detector processing technology, namely the flip-chip interconnection between the circuit and the infrared detector.
[0069] In summary, the present application can accurately determine the size and XY coordinates of the fault point by using the OBIRCH tester; by reducing the etching area layer by layer, the fault point can be accurately isolated or repaired, the defective area is turned into a short circuit, and the resistance of the entire circuit is restored to normal, while avoiding excessive damage to the surrounding normal circuits, and can still be used for subsequent infrared detector processing technology. Compared with traditional repair methods, the present application reduces the difficulty of repairing the readout circuit, has a better repair effect, and the fault point repair process is more accurate and efficient, which can reduce unnecessary repair steps and material waste, thereby reducing the overall repair cost; the present application is not only suitable for short-circuit repair of circuit chips, but also can provide reference and reference for the detection, positioning and repair of other micro-nano structures, and promote technological progress and development in related fields.
[0070] It should be noted that, in this article, the terms "comprise", "include" or any other variant thereof are intended to cover non-exclusive inclusion, so that the process, method, article or device including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise one..." do not exclude the presence of other identical elements in the process, method, article or device including the element. In addition, it should be pointed out that the scope of the methods and devices in the embodiments of the present application is not limited to performing functions in the order shown or discussed, and may also include performing functions in a substantially simultaneous manner or in reverse order according to the functions involved, for example, the described method may be performed in an order different from that described, and various steps may also be added, omitted, or combined. In addition, the features described with reference to certain examples may be combined in other examples.
[0071] The embodiments of the present application are described above in conjunction with the accompanying drawings, but the present application is not limited to the above-mentioned specific implementation methods. The above-mentioned specific implementation methods are merely illustrative and not restrictive. Under the guidance of the present application, ordinary technicians in this field can also make many forms without departing from the purpose of the present application and the scope of protection of the claims, all of which are within the protection of the present application.
Claims
1. A method for repairing a readout circuit of an ultra-large array infrared focal plane detector, characterized in that: include: Conduct continuity test on the chip to screen out faulty chips; A rectangular coordinate system is established based on the surface of the faulty chip, and a fault point of a readout circuit and its XY coordinate area are determined on the surface of the chip by an OBIRCH tester; The fault point is marked by the laser of the OBIRCH tester and marked by a marker pen; The XY coordinate area of the fault point is etched layer by layer from the surface of the circuit layer to the inside thereof by using a FIB-SEM dual-beam scanning electron microscope, and the etching area is reduced layer by layer to form a stepped etching structure until the circuit layer in the fault point area completely disappears.
2. The method according to claim 1, characterized in that The method further comprises: Testing whether the resistance value of the faulty chip meets the use requirements; If the resistance value does not meet the use requirements, a certain range of areas is set with the fault point as the center, and bombardment cleaning is performed using the FIB-SEM dual-beam scanning electron microscope with a set beam current and time, and then the resistance value is retested to see if it meets the use requirements.
3. The method according to claim 2, characterized in that The area of the certain range is larger than the area of the XY coordinate area of the fault point.
4. The method according to claim 1, characterized in that: The markings are recessed areas of specific sizes.
5. The method according to any one of claims 1 to 4, characterized in that: The XY coordinate area of the fault point is etched layer by layer from the surface of the circuit layer to the inside thereof by using a FIB-SEM dual-beam scanning electron microscope, and the etching area is reduced layer by layer to form a stepped etching structure until the circuit layer in the fault point area completely disappears, including: Step a, taking the fault point as the center, setting the physical area of the i-th set value, and etching a passivation layer by using the set beam current and the IEE gas-assisted etching system; keeping the beam current unchanged, and then etching a metal layer by using the EE gas-assisted etching system; Step b, taking the fault point as the center, setting the physical area of the i+1th set value, keeping the beam current unchanged, etching a passivation layer with the IEE gas-assisted etching system, and then etching a metal layer with the EE gas-assisted etching system while keeping the beam current unchanged; Repeat step a to step b until the remaining circuit layer in the physical area of the Nth set value completely disappears.
6. The method according to claim 5, characterized in that The shape of the solid area is rectangular or circular.
7. The method according to claim 5, characterized in that The i-th set value is greater than the (i+1)-th set value.
8. The method according to claim 5, characterized in that The FIB-SEM dual-beam scanning electron microscope is used to perform bombardment cleaning using a set beam current and time, specifically including: The EE gas-assisted etching system was used to bombard the sample for 3 minutes using a set beam current.