Surface relief waveguide with high refractive index resist
Through high refractive index nanoimprintable resist and continuous recycling technology, the problem of residual layer thickness changes caused by resist application in traditional technology is solved, and high-quality surface relief waveguide manufacturing is achieved, which improves image uniformity and Brightness reduces manufacturing costs.
Patent Information
- Application Number
- CN202380027915.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-01-20
- Filing Date
- 2023-01-20
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2043-01-20
AI Technical Summary
In traditional nanoimprint replication techniques, the application of resist causes changes in residual layer thickness, introduces optical artifacts, and the larger residual layer thickness under smaller features reduces image uniformity, especially in augmented reality and mixed reality systems. There are problems in eyepiece applications.
Using high-refractive nanoimprintable resist, the volume distribution of the resist is accurate and uniform through continuous recirculation and sub-2 picoliters on demand, and the high-refractive resist and substrate are used. Refractive index matching reduces the residual layer thickness variation, and further optimizes the residual layer thickness through imprint template and etching technology.
High-quality surface relief waveguide manufacturing is achieved, reducing optical artifacts, improving image uniformity and brightness, reducing manufacturing costs, and meeting the needs of high-yield and low-cost optical equipment manufacturing.
Smart Images

Figure CN118946451A_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims the benefit of U.S. Patent Application No. 63 / 301,318, filed on January 20, 2022, entitled “Surface Relief Waveguides with High Refractive Index Resist,” the entire contents of which are incorporated herein by reference. Technical Field
[0003] Embodiments described herein generally relate to systems and methods for fabricating surface relief waveguides for eyepieces using a fluid having a high refractive index, and optical devices created thereby. Background Art
[0004] Traditionally, resists for nanoimprint replication of waveguides or other optical elements are applied by spin coating a solvent-diluted material on a substrate, resulting in a flat, uniform layer across the substrate. One advantage of this approach for optical applications is the local uniformity of the material, which can reduce scattering or phase changes of incident light due to local roughness or height variations. However, using spin coating for replication in manufacturing can also result in variations in residual layer thickness. In particular, step variations in residual layer thickness from one feature set to another can introduce undesirable optical artifacts, while larger residual layer thicknesses at smaller features can result in reduced image uniformity, such as when the optical element is used in an eyepiece in an augmented reality and / or mixed reality system. Summary of the invention
[0005] The present disclosure describes methods and systems for reliably manufacturing high-quality surface relief waveguides for eyepieces. The optical features in the surface relief waveguides have high nanofeature fidelity and high uniformity of residual layer thickness in areas where there may be different requirements for resist volume. The innovative aspects described in the present disclosure include: i) the use of high refractive index nanoimprintable resists with room temperature viscosity and surface tension to allow controlled volumetric dispensing of the resist; ii) continuous recirculation of high refractive index nanoimprintable fluids in a dispensing device to maintain reliable dispensing of the resist through narrow fluid channels and nozzles; and iii) sub-2 picoliter (pL) on-demand drop-wise dispensing of high refractive index nanoimprintable resists to provide a thin uniform layer whose thickness can be closely matched to an imprint template, where different areas of the imprint template are associated with different total resist volumes on the substrate surface. In some embodiments, the substrate may include: inorganic amorphous materials (e.g., dense tantalum flint glass TADF55, quartz, etc.), crystalline materials (e.g., LiNbO3, LiTaO3, SiC, etc.), high refractive index polymers (e.g., containing sulfur, aromatics, etc.), and / or other polymer materials (e.g., polycarbonate (PC), polyethylene terephthalate (PET), etc.).
[0006] Embodiments include a system for manufacturing an optical device, the system comprising: a reservoir configured to store resist; a fluid dispenser including a dispensing mechanism configured to dispense droplets of resist onto a substrate; a meniscus pump configured to move resist from the reservoir to the fluid dispenser through a first channel; a fluid pump configured to move undispensed resist from the fluid dispenser to the reservoir through a second channel; a fluid control device communicatively coupled to the fluid pump and the meniscus pump, the fluid control device configured to control operation of the fluid pump and the meniscus pump to maintain a continuous flow of resist between the reservoir and the fluid dispenser; and an imprint mechanism that operates to create the optical device by applying an imprint template to the resist that has been dispensed onto the substrate, wherein applying the imprint template creates a pattern of one or more structures in the resist, and wherein the pattern corresponds to the imprint template.
[0007] In some embodiments, the system further includes a control module communicatively coupled to the fluid control device, the fluid dispenser, and the stamping mechanism. The control module can be programmed to send signals that control the operation of the fluid control device, the fluid dispenser, and the stamping mechanism.
[0008] In some embodiments, the volume of the droplet of resist is less than 6 picoliters, less than 4 picoliters, or less than 2 picoliters.
[0009] In some embodiments, the refractive index of the resist is greater than 1.5 or 1.6 for light having a wavelength of 532 nanometers. In some embodiments, the refractive index of the substrate is in the range of 1.5 to 2.7.
[0010] In some embodiments, the imprint template includes at least two regions having structures of different heights.
[0011] Embodiments also include a method for manufacturing an optical device, the method comprising: operating a fluid dispenser including a dispensing mechanism to dispense droplets of resist onto a substrate; operating a meniscus pump to move the resist from a reservoir to the fluid dispenser through a first channel; operating a fluid pump to move undispensed resist from the fluid dispenser to the reservoir through a second channel, wherein the fluid pump and the meniscus pump operate to maintain a continuous flow of resist between the reservoir and the fluid dispenser; and operating an imprint mechanism to create an optical device by applying an imprint template to the resist dispensed onto the substrate, wherein applying the imprint template creates a pattern of one or more structures in the resist, and the pattern corresponds to the imprint template.
[0012] In some embodiments, the method further comprises etching at least a portion of the optical device to reduce a residual layer thickness (RLT) of the resist on the substrate, wherein etching comprises one or more of applying heat or atmospheric etching.
[0013] In some embodiments, etching further reduces the size of at least one structure of the pattern created by applying the imprint template.
[0014] Embodiments also include a waveguide comprising: a substrate; and a plurality of structures imprinted into a volume of resist dispensed onto the substrate, wherein the resist comprises a polymer, wherein a refractive index of the resist is in a range of 1.5 to 2.1, and wherein an RLT of the resist in at least a portion of the substrate is in a range of 0 nm to 50 nm.
[0015] In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 0 nm to 10 nm, 40 nm to 50 nm, 30 nm to 40 nm, 20 nm to 30 nm, or 10 nm to 20 nm. In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 0 nm to 40 nm, 0 nm to 30 nm, 0 nm to 20 nm, or 0 nm to 10. In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 10 nm to 40 nm or 10 nm to 30 nm. In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 20 nm to 40 nm.
[0016] In some embodiments, a plurality of structures provide one or more optically active regions that include one or more of: an input coupler, a combined pupil expander, an exit pupil expander, an orthogonal pupil expander, a recirculator, or an anti-reflection feature.
[0017] In some embodiments, the plurality of structures are imprinted with nano-geometries comprising one or more of: binary geometry, tilted geometry, blazed geometry, sawtooth geometry, multi-step geometry, meta-feature geometry, one-dimensional geometry, two-dimensional geometry, or three-dimensional geometry.
[0018] In some embodiments, the substrate has a refractive index in the range of 1.5 to 2.7.
[0019] In some embodiments, multiple structures are imprinted onto a single side of a substrate. In some embodiments, multiple structures are imprinted onto both sides of a substrate.
[0020] In some embodiments, sub-2 pL dispensing can be achieved by gravity without the use of a pump (e.g., without a meniscus pump, a fluid pump, or both). One embodiment includes dispensing droplets of resist onto a substrate, contacting the resist with an imprint template to produce a pattern of one or more structures in the resist, wherein the pattern corresponds to the imprint template, polymerizing the resist to produce an imprinted nanostructure, and separating the imprint template from the imprinted nanostructure. The resist has a refractive index in the range of 1.5 to 2.1, a residual layer thickness (RLT) of the resist in at least a portion of the substrate is in the range of 0 nm to 50 nm, and the substrate includes an inorganic material.
[0021] Implementations of this embodiment may have one or more of the following features.
[0022] In some embodiments, the volume of each droplet of the resist is less than 6 picoliters, less than 5 picoliters, less than 4 picoliters, 3 picoliters, or less than 2 picoliters. In some embodiments, the volume of each droplet of the resist is less than 1 picoliter.
[0023] In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 0 to 10 nm, 10 to 20 nm, 20 to 30 nm, 30 to 40 nm, or 40 to 50 nm. In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 0 to 40 nm, 0 to 30 nm, 0 to 20 nm, or 0 to 10 nm. In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 10 to 40 nm or 10 to 30 nm. In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 20 to 40 nm.
[0024] In some embodiments, the substrate includes glass, LiTaO 3 , LiNbO 3 , SiC, or a combination thereof.
[0025] In some embodiments, the resist contains no inorganic nanoparticles. In this case, the refractive index of the resist is typically in the range of 1.5 to 1.8.
[0026] In some embodiments, the resist includes inorganic nanoparticles (e.g., TiO2, ZrO2, or both). The average diameter of the inorganic nanoparticles is generally in the range of 5nm to 15nm. The inorganic nanoparticles may account for about 10vol% to about 60vol% of the resist. The refractive index of the resist is generally in the range of 1.5 to 2.1.
[0027] In some embodiments, the viscosity of the resist is in the range of 5 to 25 centipoise (cP) at 25°C.
[0028] In some embodiments, the surface tension of the resist is in the range of 20 to 60 millinewtons (mN) per meter (m) at 25°C.
[0029] In some embodiments, dispensing droplets of resist includes pumping the resist from a reservoir to a fluid dispenser through a first channel. Some embodiments include maintaining a continuous flow of resist between the reservoir and the fluid dispenser. In some embodiments, maintaining a continuous flow of resist between the reservoir and the fluid dispenser includes pumping undispensed resist from the fluid dispenser to the reservoir through a second channel.
[0030] In some embodiments, droplets are dispensed without pumping the resist (eg, without using a meniscus pump, a fluid pump, or both to pump the resist).
[0031] Other features and advantages of the present application will be apparent from the following detailed description and drawings, and from the claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 An example system for fluid dispensing and imprinting according to an embodiment of the present disclosure is shown.
[0033] Figure 2 A flow chart of an example manufacturing process is depicted in accordance with an embodiment of the present disclosure.
[0034] Figure 3 Example results of different imprinting processes are depicted.
[0035] FIG. 4A to FIG. 4C Depicted are example imprinted nanostructures according to embodiments of the present disclosure.
[0036] Figures 5A to 5N Images of various example nanostructure geometries are shown in accordance with embodiments of the present disclosure.
[0037] Fig. 6A and Figure 6B Depicted are example eyepiece designs in accordance with embodiments of the present disclosure.
[0038] 7A to 7E Images showing simulated test results for waveguides fabricated using various techniques. DETAILED DESCRIPTION
[0039] Embodiments described herein provide a drop-on-demand, controlled volume dispensing technique for dispensing fluid onto a substrate and precisely controlling the volume of the dispensed droplets and the position of the dispensed droplets on the substrate. The dispensed fluid can then be imprinted to create a patterned optical device suitable for augmented reality (AR) and / or mixed reality (MR) systems and / or other suitable optical applications. The innovative techniques described herein are capable of dispensing droplets of dispensed fluid (which may also be described as a resist, photoresist, or resin) smaller than the droplet size used in previously available drop-on-demand jetting techniques. Specifically, the embodiment uses a droplet size less than two picoliters (pL), which provides a thin and uniform distribution of a resist layer, and its target volume can be matched with an imprint template having different regions, which are associated with different total resist volumes suitable for filling the template. Compared with previously available techniques using larger droplet sizes, the use of smaller droplet sizes can also significantly reduce the variation of the interconnection residual layer thickness (RLT) on the entire substrate surface. In addition, the technology described herein uses a dispensed resist with a high refractive index that can more closely match the refractive index of the substrate, thereby reducing optical artifacts in the manufactured optical device. The viscosity of the resist with a high refractive index may also be higher than the resist used in the previously available technology. Therefore, in order to ensure that the higher viscosity resist is reliably dispensed with a smaller droplet size, the embodiment uses a resist dispensing system that provides substantially continuous recirculation of the resist fluid. This recirculation enables the system to operate the fluid at room temperature viscosity and surface tension while maintaining reliable dispensing through narrow fluid channels and nozzles, thereby facilitating high-throughput manufacturing of high-quality optical devices.
[0040] High refractive index materials are commonly used as substrate materials for surface relief-based diffractive waveguides in AR and / or MR systems. The use of high refractive index substrates helps support a wide field of view of a virtual image that can be coupled into and ejected from the waveguide to the user's eyes. However, the surface relief diffractive features are typically composed of a material with a lower refractive index (e.g., a refractive index less than 1.6) than the substrate. When used as an optical combiner in an AR / MR system, this refractive index mismatch can lead to undesirable optical artifacts and limit image brightness and overall uniformity, including the user-to-world ratio of image brightness. In one example, for a single-sided design with surface features on one side of the substrate, the user-to-world ratio can increase from 1:1 to 1.25:1 as the resist refractive index increases from 1.53 to 1.65. As provided by the embodiments described herein, the use of a higher refractive index resist allows the use of a grating with a higher diffraction efficiency than using a similar grating with the same nano-geometry, thereby allowing higher values of image brightness and uniformity within the desired eye box position or range.
[0041] Larger RLTs and / or variations in RLT uniformity (such as those produced using conventional techniques) can also result in optical artifacts. Accordingly, embodiments described herein also provide higher quality optical devices by using smaller resist droplet sizes during resist dispensing, resulting in less variation in overall RLT uniformity and less variation between regions with different feature heights (if desired). Embodiments described herein provide a system and method for manufacturing high quality optical devices that allow the use of high refractive index resist materials to minimize the difference between the refractive index of the resist and the substrate, thereby reducing adverse effects caused by refractive index differences. Embodiments also provide for the manufacture of devices having thin and / or uniform RLT to meet cost and yield considerations for high volume manufacturing of optical devices.
[0042] As used herein, optical transparency generally refers to a physical property that allows light to pass through a material without being scattered or absorbed. As used herein, high refractive index generally refers to a refractive index (n) (e.g., the refractive index of an imprinted polymer resist) greater than 1.5, or greater than 1.6 or 1.7. In one example, high refractive index refers to n greater than 1.6 or 1.7 and less than 1.9. In one example, high refractive index refers to n in the range of 1.5 to 1.8.
[0043] As used herein, total thickness variation (TTV) refers to the difference between the maximum and minimum values of the thickness of the substrate in a series of point measurements over the entire size of the substrate. For a substrate with a patterned surface, TTV refers to an approximate value evaluated by ignoring the contribution of pattern features to the thickness. For example, the thickness (or height) of a typical feature on a patterned substrate may be in the range of about 10 nanometers (nm) to 150nm. The thickness is at least partially determined by the groove depth of the template, which can vary by 10% (e.g., 1nm to 15nm). The TTV of an unpatterned substrate is typically over 100nm, sometimes in the micron range. Therefore, the additional thickness variation introduced by the pattern features of the patterned substrate can be ignored and can be ignored as an approximation. Therefore, the thickness of a patterned substrate evaluated at a position including a protrusion can be approximated by subtracting a given feature thickness from the evaluated thickness to obtain an adjusted thickness, while the thickness of the patterned substrate evaluated at a position without a protrusion remains unchanged. That is, the adjusted (e.g., reduced) thickness of the feature area and the original (native) thickness of the unpatterned area can be used to calculate the TTV of a substrate with a patterned surface. The low TTV values described herein are derived, at least in part, from flat optical grade glass substrates that are polished to meet the desired flatness, and the methods described herein to minimize or reduce non-uniform material shrinkage during the curing process. Low TTV can also be imparted to inorganic material substrates by extrusion. Low TTV can also be imparted to polymeric substrate materials and achieved from the mold surface when molding (e.g., injection molding, ultraviolet (UV) or thermal molding, extrusion, etc.) such substrates, which are composed of high refractive index polymers (e.g., containing sulfur, aromatic, etc.) and other polymeric materials (e.g., polycarbonate (PC), polyethylene terephthalate (PET), etc.).
[0044] Figure 1 is a system diagram illustrating an example system 100 for dispensing a fluid (eg, a high refractive index nanoimprint resist) onto a substrate and imprinting the dispensed fluid to create a pattern on the substrate. .
[0045] like Figure 1As shown, the system 100 may include a substrate 102 supported by a platform 104. The substrate 102 may be composed of any suitable material, such as glass or polymer. The platform 104 may be configured to support the substrate 102 and stabilize the substrate 102 during fluid dispensing, imprinting, curing, etching and / or other manufacturing operations. The fluid dispenser 106 is configured to dispense droplets (or drops) of a fluid 120 (e.g., a resist) onto the substrate 102. The fluid dispenser 106 may also be described as one or more print heads. The fluid 120 is held in a reservoir 108, which is connected to the fluid dispenser 106 by one or more channels (e.g., tubes, conduits, etc.) of suitable type, material, and size. The fluid pump 110 operates to circulate the fluid 120 between the reservoir 108 and the fluid dispenser 106. The meniscus pump 112 operates to extract drops of the fluid 120 from the reservoir 108, and the fluid 120 flows from the reservoir 108 to the fluid dispenser 106.
[0046] Fluid controller 114 is communicatively coupled to pumps 110 and 112 and sends signals to pumps 110 and 112 to control their operation and maintain continuous circulation of fluid 120 within the system. As described herein, continuous circulation of fluid 120 enables reliable dispensing of high refractive index, high viscosity fluids with smaller drop sizes than conventional techniques. System 100 may include one or more pressure sensors 116 for measuring the pressure of fluid 120 as it circulates within the system. Although Figure 1 An example using two pressure sensors 116(1) and 116(2) is depicted, but the system may include any suitable number and type of pressure sensors 116 at any suitable location in the system. The fluid controller 114 is communicatively coupled to the pressure sensors 116 and may receive pressure data describing the pressure of the fluid 120 at one or more locations in the system from the pressure sensors 116. The fluid controller 114 may use the pressure data to control the circulation flow of the fluid 120 in the system and ensure a substantially continuous circulation (e.g., recirculation) flow.
[0047] In system 100, fluid recirculation through the print head can be maintained by combining a diaphragm fluid pump with a meniscus vacuum pump, wherein the diaphragm fluid pump supplies fluid to the inlet of the print head at a positive pressure, and the meniscus vacuum pump applies a negative pressure to the outlet of the print head. Alternatively, a second diaphragm fluid pump can be used to apply a negative pressure to the outlet. By applying appropriate inlet and outlet pressures, the meniscus pressure at the print head nozzle and the pressure difference through the print head can be independently controlled. The meniscus pressure set point is selected to prevent fluid from dripping from the nozzle of the print head and air from entering the print head through the nozzle. The pressure can be set in a range between -10 and -40 mbar. The pressure difference is proportional to the resist flow rate through the print head and is set to deliver a flow rate between about 50 and 150 milliliters (mL) / minute.
[0048] To ensure system reliability, the various hardware elements of the system may be designed with consideration for the composition of the specific resist circulating within the system. The composition of the system components that interact with the resist may be critical, as some weaker polymer components may begin to chemically dissolve and mix with the resist fluid over time. Therefore, more chemically resistant components (e.g., made of polytetrafluoroethylene (PTFE), nylon, etc.) may be used to ensure reliable operation of the printhead system, including components involved in fluid recirculation.
[0049] The control module 118 is communicatively coupled to the fluid controller 114 and the fluid dispenser 106 to control their operation. In some embodiments, the control module 118 is a computing device including at least one processor and a memory. The memory may store a computer program including instructions that, when executed by at least one processor, cause the processor to perform operations to control the fluid controller 114, the fluid dispenser 106, and / or other components of the system. The control module 118 may be any suitable type of computing device, such as a personal computer, and may communicate with other computing devices to receive instructions, provide data, etc.
[0050] In some embodiments, the system 100 includes a mechanism (not shown) that moves the platform 104 and the substrate 102 along the platform travel direction 122 between multiple stages of the process of manufacturing an optical device. The mechanism can also be controlled by the control module 118. The platform 104 (and the substrate 102) can be moved from a first position where a fluid 120 is dispensed onto the substrate 102 during the first stage of the manufacturing process to a second position. At the second position, the substrate 102 is imprinted during the second stage using an imprint template 124, which forms the fluid 120 into a desired pattern to create an optical device. The imprint template 124 can be operated by an imprint mechanism 126 that can be controlled by the control module 118. During one of the stages or in a separate stage, light (e.g., UV light), heat, and / or a combination of light and heat can also be used to cure the fluid 120. Alternatively, the system can be configured so that the dispensing, imprinting, and / or curing of the fluid 120 are performed at the same position of the platform 104.
[0051] although Figure 1An example of a system 100 including a single fluid dispenser 106 is shown, but other embodiments are possible. The system can be a single fluid circulation system that includes multiple fluid dispensers to distribute resist to different substrates and / or different parts of the substrate in parallel to achieve more efficient and higher capacity manufacturing. In addition, the system can include multiple fluid circulation systems to circulate different resist fluids (e.g., having different refractive indices) and distribute different resists to different areas of the substrate through different print heads. For example, a first resist having a first refractive index can be distributed to a combined pupil expander (CPE) area of the substrate, while a second resist having a second refractive index can be distributed (e.g., in parallel with the first resist) to different areas, such as an in-coupling grating (ICG) or a recirculator. Therefore, manufacturing can include a single distribution and imprinting step that distributes and imprints multiple resists in different areas. Alternatively, multiple systems can circulate and distribute the same fluid to achieve higher throughput during the manufacturing process.
[0052] Conventional systems employ spin coating techniques to apply resist to substrates. In such systems, application of resist for nanoimprint replication of waveguides or other optical elements is accomplished by spin coating a solvent-diluted material onto a substrate, resulting in a uniform, flat layer across the substrate. The advantages of this conventional approach are that it is an industrially mature process and that it provides excellent local uniformity of dispensed material. This uniformity minimizes scattering or phase changes of incident light due to local roughness or height variations. However, there are also disadvantages to using conventional spin coating techniques for manufacturing replication. If the goal is to create non-uniform target features (e.g., with varying heights and / or duty cycles), the amount of resist required to fill the template features during the nanoimprint process will vary. Because the underlying applied film starts out essentially uniformly distributed, spin coating can result in the final film (e.g., after template imprinting) having varying RLTs, such as Figure 3 As shown in Figure 2. Large step changes in RLT can introduce undesirable optical artifacts when moving from one feature set to another. Large RLTs at smaller features can lead to reduced image uniformity, especially on the temple side. Another manufacturing disadvantage of spin coating is that more than 95% of the resist solution is wasted, significantly increasing manufacturing costs.
[0053] Unlike spin coating, an improved version of drop-on-demand jetting and flash imprint lithography (J-FIL) process is used in the embodiment to apply the resist for nanoimprinting. The J-FIL process locally adjusts the amount of fluid to fit the filling feature, thereby reducing the large step change of RLT from one feature area to another feature area compared to the step change caused by spin coating. The traditional J-FIL process uses large droplets (e.g., >3pL) of dispensed material with a refractive index greater than 1.6 and produced by a standard industrial print head. However, the traditional J-FIL process also has disadvantages. Using this process, the droplets of resist will not spread to form a uniform local film, so some local non-uniformity of the thickness of the imprinted fluid is introduced at the droplet merger. In addition, due to the digital nature of the traditional J-FIL dispensing process, not all target thicknesses or boundaries can be perfectly matched.
[0054] Embodiments described herein provide a system and method that is an improvement over conventional J-FIL techniques and solves problems with conventional J-FIL techniques. Embodiments employ smaller (e.g., <2pL) droplets of high-index resist with higher resolution to improve local flatness and further reduce RLT step height variations within nanofeature-like (also referred to as features, structures, or nanostructures) regions and in transitions between two or more feature regions in an imprinted pattern. In other words, embodiments employ smaller droplets of high-index resist to improve local surface flatness (RLTu) and reduce the magnitude of RLT step variations at boundaries and / or region transition regions.
[0055] To achieve sub-2pL nanoimprinting with high refractive index resists, the techniques described herein employ a combination of: 1) a high refractive index (e.g., n>1.6) fluid whose rheological properties are compatible with a controlled volume dispensing process; 2) fluid recirculation to maintain reliable jetting in a print head of a fluid dispenser 106 (e.g., a print head) that dispenses the resist; and 3) a multi-nozzle fluid dispenser 106 capable of producing sub-2pL droplets of resist and delivering them to a substrate with sufficient precision to provide nanoimprint optical devices with minimal defects.
[0056] To be able to be dispensed via a jet dispensing process, a material must typically have a viscosity in the range of 5 to 25 centipoise (cP) and a surface tension in the range of 20 to 60 (e.g., 20 to 40) millinewtons (mN) per meter (m). Many high refractive index components (whether organic or inorganic) have properties outside of this range. In traditional jetting applications, heating is used to reduce the viscosity of more viscous materials to a jettable viscosity range. However, heating carries the risk of oxidation and gelation and is generally not applicable to reactive materials designed to be UV cured. Therefore, embodiments employ high refractive index resists having a higher refractive index than competing commercial materials while having rheological properties that allow jet dispensing at room temperature.
[0057] Embodiments support the use of various suitable types of high refractive index resists. In some embodiments, the resist (e.g., fluid 120) is a polymer-based resin to which nanoparticles (NPs) of a higher refractive index material are added. Alternatively, the resist can be a polymer-based resin without NPs incorporated therein. Adding NPs can increase the total refractive index of the material, which is conducive to more closely matching the refractive index of the substrate described herein. However, adding NPs may also cause Rayleigh scattering of light in the resist. Therefore, the selection of using a resist including NPs or omitting NPs may be based on balancing considerations, such as a higher refractive index with more scattering. For example, a resist having a refractive index of 1.6 or 1.7 and not containing NPs can provide optimal performance, thereby providing a higher refractive index (e.g., a refractive index closer to that of the substrate) while avoiding scattering caused by the presence of NPs.
[0058] Organic (meth)acrylate monomers and oligomers typically have a refractive index of about 1.5 at 532nm. Sulfur atoms and aromatics, both of which have high polarizability, can be added to these acrylate components to increase the refractive index of the formulation. This effect may be limited by the fluid viscosity limitations of the jetting process of less than 20 to 25 cP, and the upper limit of the refractive index of sulfur-containing molecules. This approach can produce jettable and imprintable resists with refractive indices as high as 1.72 at 532nm.
[0059] The addition of inorganic nanoparticles (NPs) such as ZrO2 and TiO2 can further significantly increase the refractive index. The refractive index of pure ZrO2 and TiO2 crystals at 532nm can reach 2.2 and 2.4-2.6, respectively. For the preparation of optical nanocomposites of acrylate monomers and inorganic nanoparticles, the particle size is less than 10nm to avoid excessive Rayleigh scattering. Due to their high specific surface area, high polarity, and incompatibility with the cross-linked polymer matrix, ZrO2 NPs tend to agglomerate in the polymer matrix. Surface modification of NPs can be used to overcome this problem. In this technique, the hydrophilic surface of ZrO2 is modified to be compatible with organic matter, thereby enabling the NPs to mix uniformly with the polymer. This modification can be accomplished using capping agents containing silane and carboxylic acid. One end of the capping agent is bonded to the ZrO2 surface; the other end of the capping agent either contains a functional group that can participate in acrylate crosslinking or contains a non-functional organic part. Examples of surface modified sub-10 nm ZrO2 particles include Pixelligent Technologies TM and Cerion Advanced Materials TM Particles provided. These functional nanoparticles are typically sold as a homogenous mixture uniformly suspended in a solvent and can be combined with other base materials to create resist formulations with jettable viscosities and increased refractive index.
[0060] The higher surface tension of some high refractive index components may pose a challenge to the implementation of nanoimprint lithography (NIL) processes based on jetting. High surface tension tends to support the formation of bubbles in the fluid. The formation of bubbles and subsequent air blockage of nozzles and fluid channels are common reliability issues in jetting processes. As channel and nozzle sizes are reduced to support the formation of smaller droplets (such as the droplets used in the technology described herein), this problem becomes more serious. Therefore, embodiments described herein provide systems and methods including continuous circulation of resist fluids. The continuous flow of fluid through the channels in the system 100 removes bubbles from narrow channels and maintains a stable supply of fluid.
[0061] This approach is also applicable to adding resist solutions containing higher vapor pressure solvents (e.g., high refractive index inorganic nanoparticles dispersed in a solvent) to the resist formulation. Without recirculation, solvent evaporation at the faceplate of the fluid dispenser 106 may result in increased viscosity and nozzle failure. This in turn can negatively impact the quality of the imprint, RLTu, and nanofeature fidelity, and can severely impact the image quality of the fabricated eyepiece waveguide, including image clarity, contrast, uniformity, and efficiency.
[0062] The formation and accurate placement of small droplets is particularly important for dispensing high viscosity and high surface tension fluids. High viscosity and high surface tension negatively impact the NIL process by slowing feature filling and droplet pre-spreading, respectively. Lower refractive index materials are generally easier to spread and fill and are less likely to produce RLT variations. In addition, higher refractive index imprinted layers (e.g., n>1.6) are more optically sensitive to RLT variations than imprints of lower refractive index resists (e.g., n=1.53). For resist formulations containing nanoparticles, long delays before droplet merging can lead to material phase separation and undesirable changes in the refractive index of the applied resist. When using high refractive index materials, smaller droplets with smaller droplet gap spacing have greater advantages because smaller droplets can be placed more accurately and densely on the substrate, thereby alleviating the problems of slow droplet pre-spreading and slow feature filling that can occur when using high refractive index fluids with high viscosity and high surface tension. Therefore, by modifying the conventional J-FIL process using high refractive index materials, smaller droplet sizes, and reliable operation enabled by fluid recirculation, the implementation allows for the fabrication of high performance optical components. Figure 3 Advantages provided by the embodiments described herein are further described.
[0063] Figure 2 2 is a flow chart showing an example process 200 for manufacturing an optical device according to embodiments described herein. At 202, droplets of resist are dispensed onto a substrate using a fluid dispenser. As described herein, a fluid dispenser (also referred to as a print head) may be configured to use Figure 1 The process may further include a step of curing the resist using ultraviolet light and / or heat, as described herein.
[0064] In some embodiments, one or more additional steps may be performed at 210 to further reduce the RLT, thereby creating an optical device (e.g., a waveguide) with an ultra-thin RLT. For example, an appropriate etching process may be performed to further reduce the RLT. For example, after dispensing the resist and applying the template (and, in some embodiments, curing), the etching may reduce the RLT from an initial level (50 nm or less) to a RLT in the range of about 0 to 10 nm. This RLT reduction may be accomplished on the surface of the substrate or within a specific area (e.g., at least a portion of the pupil expander (EPE) area of the waveguide). In some examples, the etching may employ a template or other type of mask to control which areas are etched to reduce the RLT.
[0065] In some embodiments, the RLT in one or more regions of the substrate can be reduced by applying heat. For example, heat in the range of 120 to 200° Celsius (C) can be applied to the substrate and / or the imprinted pattern to reduce the RLT. Such heat application can also reduce the size of the imprinted nanofeatures. The applied heat can reduce the RLT and / or nanofeatures by causing thermal contraction of the cross-linked polymer chains. For example, if the desired nanogeometry includes features with a height of 20nm (e.g., relative to the RLT), the dispensing and imprinting can be configured to create taller features and then reduce them to the desired height by applying heat. Similarly, if the desired final RLT is less than 10nm, the initial RLT of 20nm can be reduced to the desired RLT by applying heat. Similarly, we can start with a 30nm imprint and end up with a sub-10nm imprint, and in some cases, approach 0nm after post-heat treatment.
[0066] In some embodiments, atmospheric plasma etching (e.g., using a plasma of an Argon and O2 mixture) can reduce the RLT to 0 nm as desired, thereby providing essentially free-standing nanostructures on the substrate. This solution can be used in cases where the template may have a predefined biased imprint geometry, which allows for isotropic etching loss of feature width when removing the RLT. At relatively low temperatures, such as temperatures below 60°C, the use of atmospheric plasma can also smoothly reduce nano-geometry features. Ar in plasma afterglow +The presence of ions and O radicals can physically and / or chemically remove organic materials isotropically. In some embodiments, UV O3 treatment at atmospheric pressure and temperatures below 50°C can also reduce nano-geometry and RLT imprinted on such substrates. In this example, oxygen radicals generated from O3 in the presence of UV light tend to react and isotropically remove organic materials. In some embodiments, reactive ion etching at pressures below atmospheric pressure can also be used to achieve more anisotropic etching in the presence of a mixture of one or more of Ar, O2, N2, He, and CF4.
[0067] In some cases, one or more operations in process 200 are replaced or combined with another operation, the order of one or more operations is interchanged, two or more operations occur simultaneously or sequentially, or any combination thereof. In some cases, process 200 may include one or more additional operations described herein.
[0068] Figure 3 A diagram 300 is provided showing example results of three different imprinting processes. As described above, after dispensing the resist onto the substrate 102, an imprint template 124 is applied to the resist (e.g., fluid 120) to imprint a pattern onto the substrate 102. In this particular example, the template 124 includes three regions 302(1), 302(2), and 302(3) that include features of different heights, 90 nm, 60 nm, and 30 nm, respectively. It should be noted that Figure 3 The specific dimensions and other values shown in are examples, and embodiments are not limited to these examples. The goal of the imprinting process is to use template 124 to imprint a pattern that most accurately reflects template 124 onto substrate 102. In this example, the goal is to create a pattern on substrate 102 that includes three corresponding regions 304(1), 304(2), and 304(3) having corresponding height differences and minimal RLT variation. Figure 3 The specific template 124 shown in FIG. 1 is an example, and embodiments are not limited thereto.
[0069] Embodiments may employ any suitable template that imprints any suitable pattern onto substrate 102. Furthermore, although the present example depicts substrate 102 as 350 μm glass with a refractive index of 2.0, embodiments may employ substrates of any suitable size and material. For example, substrate 102 may be composed of a polymer material rather than glass.
[0070] Figure 3Three example results 306, 308, and 310 produced by three different imprinting techniques are shown. In the first example 306, spin coating is used. In this example, a uniform 100nm spin-coated resist is paired with an example template with three different feature height regions, which can be found in a diffractive optical element. Due to the shortcomings of the spin coating technique as described above, this process results in a 15nm step variation in the RLT height between the feature regions 304. The second example 308 shows the results using a traditional J-FIL technique. Using this process, the amount of fluid can be locally varied to match the feature requirements, thereby reducing but not eliminating the RLT step variation between regions. As described above, the large droplet sizes used in traditional J-FIL still result in local thickness inconsistencies, which can cause RLT variations between regions.
[0071] The third example 310 shows the results of using the improved J-FIL technique according to the embodiments described herein. Because the embodiments are able to use smaller droplets with smaller pitch, the local fluid density and boundaries can be more effectively controlled, thereby greatly reducing or eliminating the variation of RLT between regions, and a smaller overall RLT can also be achieved, as shown. The smaller pitch corresponds to a reduction in the gap size between droplets. The advantage of using a smaller droplet size is that the packing density of the droplets can be increased while still maintaining the required total volume of the dispensed resist. Smaller and more densely packed droplets can provide better RLT uniformity in nano-feature areas as well as in blank areas without features.
[0072] The techniques described herein enable high refractive index resists to be dispensed and imprinted on a substrate, thereby providing very low RLTs compared to previously available solutions. For example, embodiments described herein can provide RLTs of less than 30 nm or even less than 15 nm. This can be achieved because the dispensing mechanism is able to dispense drops of resist to locations on the substrate where the resist is needed, depending on the template used for imprinting. In other words, the mechanism enables more precise control of the spatial and volumetric placement of the resist on the substrate, thereby enabling more resist to be placed where the template is creating larger structures that may require a larger volume of resist, for example, in order to more optimally fill the template during imprinting. The techniques described herein are also able to imprint more complex or more sophisticated structures than can be created using previously available methods, because the dispensing mechanism is able to place drops precisely at locations corresponding to the structures to be created by the template, compared to traditional (e.g., spin coating) techniques that apply a substantially uniform layer of fluid over an area of the substrate. This dispensing mechanism provides flexibility for imprinting more complex features to achieve desired optical effects in waveguides, and provides more control over the specific RLT that may be imparted to different areas of the substrate.
[0073] In some examples, a diffractive surface relief imprint is made on a substrate composed of a high refractive index resist polymer with an ultrathin RLT in the range of 0nm to 50nm. In some embodiments where imprinting is performed to fabricate waveguides for optical devices such as AR / MR devices, a RLT of 10 to 20nm may be used for various parts of the waveguide, such as input coupling regions, combined pupil expanders, exit pupils, orthogonal pupil expanders, recirculators, anti-reflection features, etc. In each gradient region of the waveguide eyepiece, a high refractive index ultrathin RLT imprint on the waveguide substrate can provide the desired nano-feature gradient in duty cycle and / or feature height.
[0074] High refractive index ultrathin imprinting can be performed on substrates to create nano-geometries in various configurations. For example, nano-geometries can include features such as binary (e.g., rectangular), tilted, flared, sawtooth, multi-step, and / or more complex features. These features can include one-dimensional lines and spaces, two-dimensional features (e.g., symmetrical columns or holes), alternating gratings or two-dimensional features with the same or different pitches, and / or three-dimensional features (e.g., asymmetric columns or holes).
[0075] Figures 4A to 4C Depicted are example imprinted nanostructures according to embodiments of the present disclosure, such as a triangular or sawtooth structure 410, a trapezoidal structure 420, and a diamond structure 430. Other suitable types of nanostructures may also be created. Figures 5A to 5N Captured images of various geometric shapes created using the techniques described herein are shown. Figures 5A to 5F , scale bar is 100 nm. Figures 5A to 5E Rectangular gratings of various sizes and spacings are shown. Fig. 5F A sawtooth grating is shown. Figure 5G A multi-order grating is shown. Figure 5H A sawtooth grating is shown. Fig.5I A tilted grating is shown. Figure 5J A multi-level embedding feature is shown. Figure 5K A two-dimensional structure is shown. Figure 5L A three-dimensional structure with two sets of grating stacks is shown. Figure 5M A three-dimensional structure with lines and holes is shown. Figure 5N A three-dimensional blazed grating array is shown.
[0076] In some examples, a refractive index resist has a refractive index of about 1.5 to 2.1 and is imprinted on a substrate having a refractive index of about 1.5 to 2.7 to create a surface relief diffractive waveguide. A high refractive index resist dispensed drop-on-demand is used to imprint with a controlled RLT (e.g., in the range of 5nm to 1000nm) in different regions and / or to provide RLT modulation on the waveguide surface to change the way light propagates through the eyepiece. In one example, different regions can be created using different RLTs, such as a first RLT region at a first grating height in the CPE optical path (e.g., RLT<30nm), a second RLT region at a second grating height (e.g., RLT>40nm), and a third RLT region on the remainder of the CPE grating height region (e.g., RLT<30nm), such that the second region is located between the first and third regions. Imprinting can be performed on one or both sides of the substrate and can be performed on any suitable substrate form, such as a wafer, film, sheet, etc.
[0077] As described herein, the imprinting techniques described herein may be used to fabricate waveguides for eyepieces of AR / MR devices or other suitable optical devices. Fig. 6A and 6B Depicted are example eyepiece designs having example dimensions in accordance with embodiments of the present disclosure. Fig. 6A is a schematic diagram 600 of the world side (eg, facing outward) of an example eyepiece design. Figure 6B is a schematic diagram of the eye side (e.g., facing inward) of an example eyepiece design 650. The scale values on the horizontal and vertical axes are in millimeters (mm).
[0078] refer to Fig. 6A, the bottom 602 of the example eyepiece design is a CPE area that combines the functions of an optical pupil expander (OPE) and an EPE. The top 604 of the design is a recycler area, including a grating that sends light that would otherwise escape from the eyepiece or be absorbed at the edge of the eyepiece back to the eyepiece. In this example, the diameter of the eyepiece is 36.3mm. On the left side 606 of the eyepiece, the grating depth is 90nm. On the right side 608 of the eyepiece, the grating depth is 15nm. The middle area 610 includes multiple areas, and the grating depth of these areas decreases from 90nm on the left to 15nm on the right. Each area can include thousands of grating lines, and the width of each grating line can be about 200nm. Each area can have a substantially uniform grating depth across the area. In some examples, the grating depth corresponds to the height of the feature and is measured from the top of the feature to its bottom, with a substantially uniform RLT in each area and / or domain. Alternatively, the RLT can be different in different areas or domains. The width of these areas is 1mm and is tilted at an angle of -30 degrees relative to the vertical direction. The gratings in these regions are square ridge cross-sections tilted -60 degrees relative to vertical. Region 612 includes multiple pie-shaped slice regions. These regions are anti-reflection structures. One of these regions may include an ICG 614 approximately 33 mm from the center of the CPE, as shown in the example shown.
[0079] for Figure 6B The side view of the eye shown can be used with Fig. 6A The same dimensions as described in . The grating groove direction is +60 degrees and the depth gradient direction is inclined +30 degrees relative to the vertical direction.
[0080] In some embodiments, different grating patterns may be used in different regions. For example, the ICG region may include triangular features in its grating pattern, while the CPE region may include binary (e.g., rectangular) shaped features in its grating pattern. Different patterns may be used as needed to provide different optical effects.
[0081] In this example configuration of the eyepiece, the projector that inputs graphics into the eyepiece may be located on the right side of the figure, corresponding to the location of the ICG. Therefore, light input by the projector may propagate to the left through the waveguide and be output to the user's eye at various points in the CPE area. The grating depth may increase with distance from the projector to provide greater outcoupled power as the distance from the projector increases. Given that propagating light may be attenuated as it travels through the waveguide, a greater grating depth at greater distances from the projector may result in more uniform outcoupling of light across the eyepiece surface, overall.
[0082] Figures 7A to 7EAn image showing the results of simulation tests of waveguides made using various techniques. The simulations performed show how well the different types of waveguides propagate an input image that is uniform across the entire field of view of the display. The simulations modeled the same grating pattern for all five results, and the variable that was varied was the RLT. Fig. 7A Image 710 in shows the results of a simulation test of a waveguide manufactured according to the innovative techniques described herein to provide a constant and small RLT throughout the area of the waveguide. As shown, the result of a constant and small (e.g., about 20 nm) RLT is that the resulting image is best transmitted to the eye of a user of the optical system, for example, given a uniform input image in the field of view, the result here is a substantial reproduction of the uniform input test image. The simulation can produce an energy in the eye zone (EBE) score, which describes what percentage of the energy of the input image is ultimately transmitted to the eye zone (the area occupied by the eye). The EBE score of 710 is 7.91%. The simulation can also produce a low frequency 80 / 20 (LF8020) score, which is 80% brightness minus 20% brightness, divided by 50% brightness. Ideally, this score should be zero. The LF8020 score of 710 is 1.32.
[0083] Figures 7B to 7E Simulation results are shown for previously available methods (e.g., spin coating dispensing methods) that can only apply a constant volume of resist on the substrate surface, and therefore require dispensing a larger volume of resist to ensure that the template is completely filled. As a result, these traditional methods produce products with thicker and / or less uniform RLT than the innovative techniques described herein. Figure 7B Image 720 in shows the result of applying a constant volume of resist with a minimum RLT of 20 nm. The EBE score for this simulation is 7.39% and the LF8020 score is 1.70. Figure 7C Image 730 in shows the result of applying a constant volume of resist with a minimum RLT of 30 nm. The EBE score for this simulation is 7.2% and the LF8020 score is 1.77. Fig.7D Image 740 in shows the result of applying a constant volume of resist with a minimum RLT of 40 nm. The EBE score for this simulation is 6.87% and the LF8020 score is 1.956. Fig. 7E Image 750 in shows the result of applying the resist with an RLT of 200nm. As shown in the output image, the resulting output using the innovative techniques described herein is much more uniform compared to other more traditional methods. It is worth noting that the simulations here were performed using more traditional methods, assuming RLTs of 20, 30, and 40nm. This is much lower than typical values for industry standard techniques currently in use, which tend to produce RLTs of 100 to 200nm.
[0084] In some embodiments, sub-2 pL dispensing can be achieved by gravity without the use of a pump. One embodiment includes dispensing droplets of a resist onto a substrate, contacting the resist with an imprint template to produce a pattern of one or more structures in the resist, wherein the pattern corresponds to the imprint template, polymerizing the resist to produce an imprinted nanostructure, and separating the imprint template from the imprinted nanostructure. The refractive index of the resist is in the range of 1.5 to 2.1, the residual layer thickness (RLT) of the resist in at least a portion of the substrate is in the range of 0 nm to 50 nm, and the substrate is composed of an inorganic material.
[0085] Implementations of this embodiment may have one or more of the following features.
[0086] In some embodiments, the volume of each droplet of the resist is less than 6 picoliters, less than 5 picoliters, less than 4 picoliters, 3 picoliters, or less than 2 picoliters. In some embodiments, the volume of each droplet of the resist is less than 1 picoliter.
[0087] In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 0 to 10 nm, 10 to 20 nm, 20 to 30 nm, 30 to 40 nm, or 40 to 50 nm. In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 0 to 40 nm, 0 to 30 nm, 0 to 20 nm, or 0 to 10 nm. In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 10 to 40 nm or 10 to 30 nm. In some embodiments, the RLT of the resist in at least a portion of the substrate is in the range of 20 to 40 nm.
[0088] In some embodiments, the substrate includes glass, LiTaO 3 , LiNbO 3 , SiC, or a combination thereof.
[0089] In some embodiments, the resist contains no inorganic nanoparticles. In this case, the refractive index of the resist is typically in the range of 1.5 to 1.8.
[0090] In some embodiments, the resist includes inorganic nanoparticles (e.g., TiO2, ZrO2, or both). The average diameter of the inorganic nanoparticles is generally in the range of 5nm to 15nm. The inorganic nanoparticles may account for about 10vol% to about 60vol% of the resist. The refractive index of the resist is generally in the range of 1.5 to 2.1.
[0091] In some embodiments, the viscosity of the resist is in the range of 5 to 25 centipoise (cP) at 25°C.
[0092] In some embodiments, the surface tension of the resist is in the range of 20 to 60 millinewtons (mN) per meter (m) at 25°C.
[0093] In some embodiments, dispensing droplets of resist includes pumping the resist from a reservoir to a fluid dispenser through a first channel. Some embodiments include maintaining a continuous flow of resist between the reservoir and the fluid dispenser. In some embodiments, maintaining a continuous flow of resist between the reservoir and the fluid dispenser includes pumping undispensed resist from the fluid dispenser to the reservoir through a second channel.
[0094] Embodiments of the present disclosure
[0095] Embodiment 1 is a system for manufacturing an optical device, the system comprising:
[0096] a storage device configured to store a resist;
[0097] a fluid dispenser including a dispensing mechanism configured to dispense droplets of the resist onto a substrate;
[0098] a meniscus pump configured to move the resist from the reservoir to the fluid dispenser through a first passage;
[0099] a fluid pump configured to move undispensed resist from the fluid dispenser to the reservoir through a second passage;
[0100] a fluid control device communicatively coupled to the fluid pump and the meniscus pump, the fluid control device being configured to control operation of the fluid pump and the meniscus pump to maintain a continuous flow of the resist between the reservoir and the fluid dispenser; and
[0101] An imprint mechanism creates the optical device by applying an imprint template to the resist dispensed onto the substrate, wherein applying the imprint template creates a pattern of one or more structures in the resist, wherein the pattern corresponds to the imprint template.
[0102] Embodiment 2 is the system described in embodiment 1, further comprising:
[0103] A control module is communicatively coupled to the fluid control device, the fluid dispenser, and the stamping mechanism, the control module being programmed to send signals that control the operation of the fluid control device, the fluid dispenser, and the stamping mechanism.
[0104] Embodiment 3 is the system of embodiment 1 or 2, wherein the fluid dispenser is configured to dispense droplets of the resist having a volume less than 6 picoliters.
[0105] Embodiment 4 is the system of embodiment 3, wherein the fluid dispenser is configured to dispense droplets of the resist having a volume less than 4 picoliters.
[0106] Embodiment 5 is the system of embodiment 4, wherein the fluid dispenser is configured to dispense droplets of the resist having a volume less than 2 picoliters.
[0107] Embodiment 6 is the system of any of embodiments 1-5, wherein the resist has a refractive index greater than 1.6 for light having a wavelength of 532 nanometers.
[0108] Embodiment 7 is the system of any one of embodiments 1 to 6, wherein the refractive index of the substrate is in the range of 1.5 to 2.7.
[0109] Embodiment 8 is the system of any one of embodiments 1 to 7, wherein the imprint template comprises at least two regions having structures of different heights.
[0110] Embodiment 9 is a method for manufacturing an optical device, the method comprising:
[0111] operating a fluid dispenser including a dispensing mechanism to dispense droplets of resist onto the substrate;
[0112] operating a meniscus pump to move the resist from a reservoir to the fluid dispenser through a first passage;
[0113] operating a fluid pump to move undispensed resist from the fluid dispenser to the reservoir through a second passage, wherein the fluid pump and the meniscus pump operate to maintain a continuous flow of the resist between the reservoir and the fluid dispenser; and
[0114] An imprint mechanism is operated to create the optical device by applying an imprint template to the resist dispensed onto the substrate, wherein applying the imprint template creates a pattern of one or more structures in the resist, wherein the pattern corresponds to the imprint template.
[0115] Embodiment 10 is the method described in embodiment 9, further comprising:
[0116] At least a portion of the optical device is etched to reduce a residual layer thickness (RLT) of the resist on the substrate, wherein the etching comprises one or more of applying heat or atmospheric etching.
[0117] Embodiment 11 is the method of embodiment 10, wherein the etching further reduces the size of at least one structure of the pattern created by applying the imprint template.
[0118] Embodiment 12 is a waveguide comprising:
[0119] substrate; and
[0120] A plurality of structures are imprinted into a volume of resist dispensed onto the substrate, wherein the resist is comprised of a polymer, wherein the refractive index of the resist is in the range of 1.5 to 2.1, and wherein a residual layer thickness (RLT) of the resist in at least a portion of the substrate is in the range of 0 nm to 50 nm.
[0121] Embodiment 13 is the waveguide of embodiment 12, wherein the RLT of the resist in at least a portion of the substrate is in the range of 10 to 20 nm.
[0122] Embodiment 14 is the waveguide of embodiment 12, wherein the RLT of the resist in at least a portion of the substrate is in the range of 20 to 30 nm.
[0123] Embodiment 15 is the waveguide of embodiment 12, wherein the RLT of the resist in at least a portion of the substrate is in the range of 30 to 40 nm.
[0124] Embodiment 16 is the waveguide of embodiment 12, wherein the RLT of the resist in at least a portion of the substrate is in the range of 40 to 50 nm.
[0125] Embodiment 17 is a waveguide as described in any one of embodiments 12 to 16, wherein the plurality of structures provide one or more optically active regions comprising one or more of: an input coupler, a combined pupil expander, an exit pupil expander, an orthogonal pupil expander, a recirculator, or an anti-reflection feature.
[0126] Embodiment 18 is a waveguide as described in any one of embodiments 12 to 17, wherein the plurality of structures are imprinted with nano-geometries, and the nano-geometries include one or more of the following: binary geometry, tilted geometry, blazed geometry, sawtooth geometry, multi-step geometry, meta-feature geometry, one-dimensional geometry, two-dimensional geometry, or three-dimensional geometry.
[0127] Embodiment 19 is the waveguide of any one of embodiments 12 to 18, wherein the refractive index of the substrate is in the range of 1.5 to 2.7.
[0128] Embodiment 20 is the waveguide of any one of embodiments 12 to 19, wherein the plurality of structures are imprinted onto a single side of the substrate.
[0129] Embodiment 21 is the waveguide of any one of embodiments 12 to 19, wherein the plurality of structures are imprinted onto both sides of the substrate.
[0130] Embodiment 22 is an imprint lithography method, comprising:
[0131] dispensing droplets of resist on the substrate; and
[0132] contacting the resist with an imprint template to produce a pattern of one or more structures in the resist, wherein the pattern corresponds to the imprint template;
[0133] polymerizing the resist to produce an imprinted nanostructure; and
[0134] separating the imprint template from the imprinted nanostructure,
[0135] in:
[0136] The refractive index of the resist is in the range of 1.5 to 2.1,
[0137] The resist has a residual layer thickness (RLT) in at least a portion of the substrate in the range of 0 nm to 50 nm, and
[0138] The substrate is composed of inorganic materials.
[0139] Embodiment 23 is the imprint lithography method of embodiment 22, wherein the volume of each droplet of the resist is less than 6 picoliters, less than 5 picoliters, less than 4 picoliters, 3 picoliters, or less than 2 picoliters.
[0140] Embodiment 24 is the imprint lithography method of embodiment 23, wherein the volume of each droplet of the resist is less than 1 picoliter.
[0141] Embodiment 25 is the imprint lithography method described in any one of Embodiments 22 to 24, wherein the RLT of the resist in at least a portion of the substrate is in the range of 0 to 10 nm, 10 to 20 nm, 20 to 30 nm, 30 to 40 nm, or 40 to 50 nm.
[0142] Embodiment 26 is the imprint lithography method of any one of embodiments 22 to 24, wherein the RLT of the resist in at least a portion of the substrate is in the range of 0 to 40 nm, 0 to 30 nm, 0 to 20 nm, or 0 to 10 nm.
[0143] Embodiment 27 is the imprint lithography method of any one of embodiments 22 to 24, wherein the RLT of the resist in at least a portion of the substrate is in the range of 10 to 40 nm or 10 to 30 nm.
[0144] Embodiment 28 is the imprint lithography method of any one of embodiments 22 to 24, wherein the RLT of the resist in at least a portion of the substrate is in the range of 20 to 40 nm.
[0145] Embodiment 29 is the imprint lithography method of any one of embodiments 22 to 28, wherein the substrate comprises glass, LiTaO3, LiNbO3, SiC, or a combination thereof.
[0146] Embodiment 30 is the imprint lithography method of any one of embodiments 22 to 29, wherein the resist does not contain inorganic nanoparticles.
[0147] Embodiment 31 is the imprint lithography method described in Embodiment 30, wherein the refractive index of the resist is in the range of 1.5 to 1.8.
[0148] Embodiment 32 is the imprint lithography method of any one of embodiments 22 to 29, wherein the resist comprises inorganic nanoparticles.
[0149] Embodiment 33 is the imprint lithography method described in embodiment 32, wherein the inorganic nanoparticles include TiO2, ZrO2, or both.
[0150] Embodiment 34 is the imprint lithography method described in Embodiment 32 or 33, wherein the average diameter of the inorganic nanoparticles is in the range of 5 nm to 15 nm.
[0151] Embodiment 35 is the imprint lithography method of any one of embodiments 32 to 34, wherein the inorganic nanoparticles account for 10 vol% to 60 vol% of the resist.
[0152] Embodiment 36 is the imprint lithography method of any one of embodiments 32 to 35, wherein the refractive index of the resist is in the range of 1.5 to 2.1.
[0153] Embodiment 37 is the imprint lithography method of any one of embodiments 22 to 36, wherein the viscosity of the resist is in the range of 5 to 25 centipoise (cP) at 25°C.
[0154] Embodiment 38 is the imprint lithography method of any one of embodiments 22 to 37, wherein the surface tension of the resist is in the range of 20 to 60 millinewtons (mN) per meter (m) at 25°C.
[0155] Embodiment 39 is the imprint lithography method of any one of embodiments 22 to 38, wherein dispensing droplets of the resist comprises pumping the resist from a reservoir to a fluid dispenser through a first channel.
[0156] Embodiment 40 is the imprint lithography method of any one of embodiments 22 to 39, further comprising: maintaining a continuous flow of the resist between the reservoir and the fluid dispenser.
[0157] Embodiment 41 is the imprint lithography method of embodiment 40, wherein maintaining a continuous flow of the resist between the reservoir and the fluid dispenser comprises pumping undispensed resist from the fluid dispenser to the reservoir through a second channel.
[0158] Embodiment 42 is the imprint lithography method of any one of embodiments 22 to 38, wherein the droplets are dispensed without pumping the resist.
[0159] Embodiment 43 is the imprint lithography method of embodiment 42, wherein the droplets are dispensed without using a meniscus pump, a fluid pump, or both to pump the resist.
[0160] Although the present disclosure contains many specific embodiment details, these details should not be interpreted as limitations on the scope of the subject matter or the scope of what may be claimed, but rather as descriptions of features of specific embodiments. Certain features described in the present disclosure in the context of separate embodiments may also be implemented in combination in a single embodiment. Conversely, various features described in the context of a single embodiment may also be implemented individually or in any suitable sub-combination in multiple embodiments. In addition, although previously described features may be described as working in certain combinations and even initially claimed, in some cases, one or more features from the claimed combination may be deleted from the combination, and the claimed combination may be directed to a sub-combination or a variation of the sub-combination.
[0161] Specific embodiments of the subject matter have been described. It will be apparent to those skilled in the art that other embodiments, variations, and permutations of the described embodiments are within the scope of the following claims. Although operations are described in a particular order in the drawings or claims, it should not be understood that these operations must be performed in the particular order shown or in the sequential order, or that all of the operations shown must be performed (some operations may be deemed optional) to achieve the desired results.
[0162] Therefore, the embodiments described above do not define or limit the present disclosure. Other changes, substitutions and alterations are also possible without departing from the spirit and scope of the present disclosure.
Claims
1. A system for manufacturing an optical device, the system include: a storage device configured to store a resist; a fluid dispenser including a dispensing mechanism configured to dispense droplets of the resist onto a substrate; a meniscus pump configured to move the resist from the reservoir to the fluid dispenser through a first passage; a fluid pump configured to move undispensed resist from the fluid dispenser to the reservoir through a second passage; a fluid control device communicatively coupled to the fluid pump and the meniscus pump, the fluid control device configured to control operation of the fluid pump and the meniscus pump to maintain a continuous flow of the resist between the reservoir and the fluid dispenser; as well as An imprint mechanism creates the optical device by applying an imprint template to the resist dispensed onto the substrate, wherein applying the imprint template creates a pattern of one or more structures in the resist, wherein the pattern corresponds to the imprint template.
2. The system according to claim 1, further comprising: include: A control module is communicatively coupled to the fluid control device, the fluid dispenser, and the stamping mechanism, the control module being programmed to send signals that control the operation of the fluid control device, the fluid dispenser, and the stamping mechanism.
3. The system according to claim 1, in, The fluid dispenser is configured to dispense droplets of the resist having a volume less than 2 picoliters.
4. The system according to claim 1, in, The fluid dispenser is configured to dispense droplets of the resist having a volume less than 4 picoliters.
5. The system according to claim 1, in, The fluid dispenser is configured to dispense droplets of the resist having a volume less than 6 picoliters.
6. The system according to claim 1, in, The resist has a refractive index greater than 1.6 for light having a wavelength of 532 nanometers.
7. The system according to claim 1, in, The refractive index of the substrate is in the range of 1.5 to 2.
7.
8. The system according to claim 1, in, The imprint template comprises at least two regions having structures of different heights.
9. A method for manufacturing an optical device, the method include: operating a fluid dispenser including a dispensing mechanism to dispense droplets of resist onto the substrate; operating a meniscus pump to move the resist from a reservoir to the fluid dispenser through a first passage; operating a fluid pump to move undispensed resist from the fluid dispenser to the reservoir through a second passage, wherein the fluid pump and the meniscus pump operate to maintain a continuous flow of the resist between the reservoir and the fluid dispenser; and An imprint mechanism is operated to create the optical device by applying an imprint template to the resist dispensed onto the substrate, wherein applying the imprint template creates a pattern of one or more structures in the resist, wherein the pattern corresponds to the imprint template.
10. The method according to claim 9, further comprising: include: At least a portion of the optical device is etched to reduce a residual layer thickness (RLT) of the resist on the substrate, wherein the etching comprises one or more of applying heat or atmospheric etching.
11. The method according to claim 10, in, The etching further reduces the size of at least one structure of the pattern created by applying the imprint template.
12. A waveguide, include: substrate; as well as A plurality of structures are imprinted into a volume of resist dispensed onto the substrate, wherein the resist is comprised of a polymer, wherein the refractive index of the resist is in the range of 1.5 to 2.1, and wherein a residual layer thickness (RLT) of the resist in at least a portion of the substrate is in the range of 0 nm to 50 nm.
13. The waveguide according to claim 12, in, The RLT of the resist in at least a portion of the substrate is in a range of 0 nm to 10 nm, 10 nm to 20 nm, 20 nm to 30 nm, 30 nm to 40 nm, or 40 nm to 50 nm.
14. The waveguide according to claim 12, in, The RLT of the resist in at least a portion of the substrate is in a range of 0 nm to 40 nm, 0 nm to 30 nm, 0 nm to 20 nm, or 0 nm to 10 nm.
15. The waveguide according to claim 12, in, The RLT of the resist in at least a portion of the substrate is in a range of 10 nm to 40 nm or 10 nm to 30 nm.
16. The waveguide according to claim 12, in, The RLT of the resist in at least a portion of the substrate is in the range of 20 to 40 nm.
17. The waveguide according to claim 12, in, The plurality of structures provide one or more optically active regions that include one or more of: an input coupler, a combined pupil expander, an exit pupil expander, an orthogonal pupil expander, a recirculator, or an anti-reflection feature.
18. The waveguide according to claim 12, in, The plurality of structures are imprinted with nano-geometries including one or more of: binary geometry, tilted geometry, blazed geometry, sawtooth geometry, multi-step geometry, meta-feature geometry, one-dimensional geometry, two-dimensional geometry, or three-dimensional geometry.
19. The waveguide according to claim 12, in, The refractive index of the substrate is in the range of 1.5 to 2.
7.
20. The waveguide according to claim 12, in, The plurality of structures are imprinted onto a single side of the substrate.
21. The waveguide according to claim 12, in, The plurality of structures are imprinted onto both sides of the substrate.
22. An imprint lithography method, include: dispensing droplets of resist on a substrate; as well as contacting the resist with an imprint template to produce a pattern of one or more structures in the resist, wherein the pattern corresponds to the imprint template; polymerizing the resist to produce an imprinted nanostructure; and separating the imprint template from the imprinted nanostructure, in: The refractive index of the resist is in the range of 1.5 to 2.1, The resist has a residual layer thickness (RLT) in at least a portion of the substrate in the range of 0 nm to 50 nm, and The substrate is composed of inorganic materials.
23. The imprint lithography method according to claim 22, in, The volume of each droplet of the resist is less than 6 picoliters, less than 5 picoliters, less than 4 picoliters, 3 picoliters, or less than 2 picoliters.
24. The imprint lithography method according to claim 23, in, The volume of each droplet of the resist is less than 1 picoliter.
25. The imprint lithography method according to claim 22, in, The RLT of the resist in at least a portion of the substrate is in a range of 0 to 10 nm, 10 to 20 nm, 20 to 30 nm, 30 to 40 nm, or 40 to 50 nm.
26. The imprint lithography method according to claim 22, in, The RLT of the resist in at least a portion of the substrate is in a range of 0 to 40 nm, 0 to 30 nm, 0 to 20 nm, or 0 to 10 nm.
27. The imprint lithography method according to claim 22, in, The RLT of the resist in at least a portion of the substrate is in the range of 10 to 40 nm or 10 to 30 nm.
28. The imprint lithography method according to claim 22, in, The RLT of the resist in at least a portion of the substrate is in the range of 20 to 40 nm.
29. The imprint lithography method according to claim 22, in, The substrate includes glass, LiTaO 3 、LiNbO 3 , SiC, or a combination thereof.
30. The imprint lithography method according to claim 22, in, The resist does not contain inorganic nanoparticles.
31. The imprint lithography method according to claim 30, in, The refractive index of the resist is in the range of 1.5 to 1.
8.
32. The imprint lithography method according to claim 22, in, The resist includes inorganic nanoparticles.
33. The imprint lithography method according to claim 32, in, The inorganic nanoparticles include TiO 2 、ZrO 2 , or both.
34. The imprint lithography method according to claim 32, in, The average diameter of the inorganic nanoparticles is in the range of 5 nm to 15 nm.
35. The imprint lithography method according to claim 32, in, The inorganic nanoparticles account for 10 vol % to 60 vol % of the resist.
36. The imprint lithography method according to claim 32, in, The refractive index of the resist is in the range of 1.5 to 2.
1.
37. The imprint lithography method according to claim 22, in, The viscosity of the resist is in the range of 5 to 25 centipoise (cP) at 25°C.
38. The imprint lithography method according to claim 22, in, The surface tension of the resist is in the range of 20 to 60 millinewtons (mN) per meter (m) at 25°C.
39. The imprint lithography method according to claim 22, in, Dispensing droplets of the resist includes pumping the resist from the reservoir to a fluid dispenser through a first channel.
40. The imprint lithography method according to claim 39, further comprising: include: A continuous flow of the resist is maintained between the reservoir and the fluid dispenser.
41. The imprint lithography method according to claim 40, in, Maintaining a continuous flow of the resist between the reservoir and the fluid dispenser includes pumping undispensed resist from the fluid dispenser to the reservoir through a second channel.
42. The imprint lithography method according to claim 22, in, The droplets are dispensed without pumping the resist.
43. The imprint lithography method according to claim 43, in, The droplets are dispensed without using a meniscus pump, a fluid pump, or both to pump the resist.
Citation Information
Patent Citations
System and method for controlling placement of fluid resist droplets
CN111093836A
Waveguides with high index materials and methods of fabrication thereof
CN113811803A
Method for forming a pattern of semiconductor device
KR1020090072673A
Exposure apparatus, exposure method, and method for producing device
US20070139628A1
Large Area Patterning of Nano-Sized Shapes
US20100120251A1