Wafer grounding method using wafer edge back coating exclusion area

By forming an exclusion area on the back of the semiconductor wafer, the electrical connection problem caused by the back mask is solved, stable and flexible electrical contact is achieved, and the efficiency and quality of wafer processing are improved.

CN118946949APending Publication Date: 2024-11-12ASML NETHERLANDS BV
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202380029575.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-10
Filing Date
2023-03-16
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Prior Art When semiconductor wafer processing is performed using charged particle beam devices, the back surface of the wafer substrate is often covered with a non-conductive back film, making it difficult to achieve reliable electrical connections, especially in the case of thick films, traditional electric shocks. The penetration method and penetration method are difficult to overcome the back mask, and the pin impact method may damage the chip.

Method used

By forming exclusion areas on the back of the wafer, the presence of the back mask is avoided, and the wafer is grounded, using a charged particle beam inspection method to inspect the wafer at different angles, and by system and method to form exclusion areas in the processing chamber for electrical connection.

Benefits of technology

It realizes stable electrical contact of the wafer in the presence of the back mask, reduces the risk of particle contamination and interlacing errors, improves the duration and stability of the electrical connection, and provides greater design flexibility and inspection flexibility. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118946949A_ABST
    Figure CN118946949A_ABST
Patent Text Reader

Abstract

There is provided a method for coupling a wafer (604; 605) in a charged particle beam apparatus. 904) to ground. The systems and methods include a backside film (608; 908) of a sufficient size is provided for a removal region (613; 911) of the charged particle beam device to allow the wafer to contact electrical contacts (612; 912) in the housing. The systems and methods include contacting a pin body with a surface of a wafer, the surface of the wafer having a coating, and the pin body including a first tip and a second tip, each tip extending from the pin body; wherein the contacting occurs at a first excluded region of the coating by any of the first tip, the second tip, or any combination thereof. A method for forming a coating on a surface of a wafer is also provided, including masking a first exclusion region on the surface of the wafer with a first exclusion mask.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority to U.S. application 63 / 323,728 filed on March 25, 2022, U.S. application 63 / 341,334 filed on May 12, 2022, and U.S. application 63 / 489,643 filed on March 10, 2023, and the entire contents of which are incorporated herein by reference. Technical Field

[0003] The description herein relates to the field of semiconductor manufacturing, and more particularly to wafer grounding and biasing that may be useful for semiconductor wafer processing using charged particle beam devices. Background Art

[0004] Charged particle beam devices can produce a two-dimensional image of a wafer substrate by detecting secondary electrons, backscattered electrons, mirror electrons or other types of electrons generated when the charged particle beam generated by the charged particle beam device hits the surface of the wafer substrate. In the semiconductor industry, various charged particle beam devices are used for semiconductor wafers for various purposes, such as wafer processing (e.g., electron beam direct writing lithography system), process monitoring (e.g., critical dimension scanning electron microscope (CD-SEM)), wafer inspection (e.g., electron beam inspection system), defect analysis (e.g., defect inspection SEM, or DR-SEM and focused ion beam system or FIB), etc. When such a device performs its function, the potential of the wafer substrate can be maintained at a predetermined value or bias for better imaging. This can be achieved by electrically connecting the target wafer substrate, more specifically, connecting a resistor to a programmable DC voltage source (e.g., a wafer bias power supply). When the wafer substrate interacts with the charged particle beam, an electrical connection can be achieved, and in the process, excess charge is brought to the wafer substrate. This process can be referred to as wafer biasing.

[0005] For wafer bias, electrical contact from the wafer bias power supply to the wafer substrate is typically made on the back side of the wafer substrate using one or more electrical contacts pressed against the back side surface of the wafer substrate. The front side surface of the wafer is typically not suitable for placement of electrical contacts because features are formed on the front side surface. Sometimes there is an electrically insulating film (e.g., a back side film) on the back side surface of the wafer. The back side film may make it difficult to establish a reliable electrical connection between the electrical contacts and the conductive surface of the wafer. Summary of the invention

[0006] Embodiments of the present disclosure include systems and methods for wafer grounding using an exclusion zone on a wafer backside film. In some embodiments, the exclusion zone is an area on the backside surface where no backside film material is present. Embodiments of the present disclosure provide clean contact between an electrical contact (e.g., a ground pin) and a conductive surface of a wafer.

[0007] Embodiments of the present disclosure include wafers having an exclusion zone of a backside film for grounding the wafer, the exclusion zone may be located, for example, at the periphery, at the center region, or at an intermediate region between the center and the periphery of the wafer backside.

[0008] Embodiments of the present disclosure include a wafer grounding system having ground pins for contacting an exclusion zone of a backside film. The ground pins and exclusion zone may be located, for example, at the periphery, the center region, or an intermediate region between the center and the periphery of the wafer backside.

[0009] Embodiments of the present disclosure include a charged particle beam inspection method for inspecting a wafer having an exclusion zone on a backside film. The method may include inspecting the wafer in two different inspection steps, wherein the wafer is supported at two different angles in the wafer plane. One or more exclusion zones are configured so that the wafer can be grounded at the exclusion zone during the two inspection steps.

[0010] Embodiments of the present disclosure include systems and methods for fabricating wafers with backside film exclusion areas. Various exemplary systems and methods are disclosed for shielding or otherwise preventing film formation on selected areas during the process of forming a thick backside film in a processing chamber.

[0011] Embodiments of the present disclosure include systems and methods for electrically connecting to a wafer. The systems and methods may include contacting a pin body to a surface of a wafer, the surface of the wafer having a coating, and the pin body including a first tip and a second tip, each tip extending from the pin body; wherein contact occurs at a first exclusion area of ​​the coating by any of the first tip, the second tip, or any combination thereof.

[0012] Other objects and advantages of the disclosed embodiments will be set forth in part in the following description, will be apparent in part from the description, or may be understood through the practice of the embodiments. Some objects and advantages of the disclosed embodiments may be achieved and obtained through the elements and combinations set forth in the claims. However, the embodiments of the present disclosure do not necessarily need to achieve such exemplary objects or advantages, and some embodiments may not achieve any of the described objects or advantages.

[0013] It is to be understood that both the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the disclosed embodiments, as claimed. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 is a schematic diagram illustrating an example electron beam inspection (EBI) system consistent with embodiments of the present disclosure.

[0015] Figure 2is a schematic diagram showing an exemplary electron beam tool consistent with embodiments of the present disclosure, which may be Figure 1 A portion of an exemplary electron beam inspection system.

[0016] Figure 3 is an illustration of an example system for wafer grounding consistent with embodiments of the present disclosure.

[0017] FIG. 4A to FIG. 4D The operating stages of an example system for wafer grounding in a comparative embodiment are shown.

[0018] Figure 5 is an illustration of potential problems caused by holes in the film on the back side of the wafer.

[0019] Figure 6A-6C is a diagram of an example subsystem for wafer grounding consistent with embodiments of the present disclosure.

[0020] Fig.6D Example relationships between exclusion zone radial position, size, and rotational positioning accuracy consistent with embodiments of the present disclosure are shown.

[0021] Figure 7A-7B is a diagram of an example subsystem for wafer grounding consistent with embodiments of the present disclosure.

[0022] Figure 8A-B is a diagram of an example subsystem for wafer grounding consistent with embodiments of the present disclosure.

[0023] Figure 9A-9B is a diagram of an example subsystem for wafer grounding consistent with embodiments of the present disclosure.

[0024] Fig.10 is an illustration of an example wafer having a backside film exclusion area consistent with embodiments of the present disclosure.

[0025] Fig.11A is a diagram of an example backside film-forming chamber in a comparative embodiment of the present disclosure.

[0026] Fig. 11B In the comparative embodiment of the present disclosure, Fig.11A Illustration of an example wafer backside film formed in a chamber.

[0027] Fig. 12A is an illustration of an example backside film-forming chamber consistent with an embodiment of the present disclosure.

[0028] Fig. 12B It is consistent with the embodiment of the present disclosure and can be Fig. 12A Illustration of an example wafer backside film formed in a chamber.

[0029] Fig. 12CFIG. 1 is a diagram of an exemplary backside film forming chamber consistent with an embodiment of the present disclosure

[0030] Fig.13A is a diagram of an exemplary backside film forming chamber in a comparative embodiment of the present invention.

[0031] Fig. 13B In the comparative embodiment of the present disclosure, Fig.13A Illustration of an example wafer backside film formed in a chamber.

[0032] Fig.14A is an illustration of an example backside film-forming chamber consistent with an embodiment of the present disclosure.

[0033] Fig. 14B It is possible to be consistent with the embodiments of the present disclosure Fig.14A Illustration of an example wafer backside film formed in a chamber.

[0034] Fig.15 is a flow chart illustrating an example method for forming a wafer backside film consistent with embodiments of the present disclosure.

[0035] Fig.16 is a flow chart illustrating an example method for grounding a wafer having a backside film consistent with embodiments of the present disclosure.

[0036] Fig.17 An exemplary keep-out area for a wafer having a single tip ground pin location is shown.

[0037] Fig.18 An exemplary keep-out area of ​​a wafer having dual tip ground pin locations consistent with embodiments of the present disclosure is shown.

[0038] Fig.19 An exemplary keep-out area of ​​a wafer having dual tip ground pin locations consistent with embodiments of the present disclosure is shown.

[0039] Fig. 20 An exemplary wafer is shown with a backside film in contact with dual tip ground pins consistent with embodiments of the present disclosure.

[0040] Fig.21 A cross-sectional view of an exemplary dual-tipped ground pin consistent with embodiments of the present disclosure is shown.

[0041] Fig. 22 An exemplary wafer holder having ground pins consistent with embodiments of the present disclosure is shown. DETAILED DESCRIPTION

[0042] Reference will now be made in detail to example embodiments, examples of which are shown in the accompanying drawings. The following description refers to the accompanying drawings, wherein, unless otherwise specified, the same reference numerals in different figures represent the same or similar elements. The implementations set forth in the following example embodiment descriptions do not represent all implementations consistent with the present disclosure. Instead, they are merely examples of devices and methods consistent with aspects related to the subject matter described in the appended claims. Without limiting the scope of the present disclosure, some embodiments may be described in the context of providing a detection system and a detection method in a system utilizing an electron beam ("e-beam"). However, the present disclosure is not so limited. Other types of charged particle beams (e.g., including protons, ions, muons, or any other particles carrying a charge) may be similarly applied. In addition, systems and methods for detection may be used in other imaging systems, such as optical imaging, photon detection, x-ray detection, ion detection, and the like.

[0043] Electronic devices are made up of circuits formed on a sheet of semiconductor material called a substrate. The semiconductor material may include, for example, silicon, gallium arsenide, indium phosphide, or silicon germanium. Many circuits can be formed together on the same silicon wafer and are called an integrated circuit, or IC. The size of these circuits has been greatly reduced so that more can fit on a substrate. For example, the IC chip in a smartphone can be as small as a thumbnail but may contain more than 2 billion transistors, each less than one thousandth the size of a human hair.

[0044] Manufacturing these ICs, which have extremely small structures or components, is a complex, time-consuming, and expensive process that typically involves hundreds of individual steps. An error in even one step can cause a defect in the finished IC, rendering it unusable. Therefore, one goal of the manufacturing process is to avoid such defects in order to maximize the number of functional ICs manufactured in the process; that is, to increase the yield of the overall process.

[0045] An integral part of improving yield is monitoring the chip manufacturing process to ensure that a sufficient number of functional integrated circuits are produced. One way to monitor the process is to inspect the chip circuit structures at various stages of their formation. Inspection can be performed using a scanning charged particle microscope ("SCPM"). For example, the SCPM can be a scanning electron microscope (SEM). The SEM can be used to image these extremely small structures, in effect taking a "photograph" of the wafer structure. The image can be used to determine if the structure is formed correctly in the correct location. If the structure is defective, the process can be adjusted to reduce the likelihood that the defect will occur again.

[0046] The working principle of SEM is similar to that of a camera. A camera takes pictures by receiving and recording the intensity of light reflected or emitted from a person or object. SEM takes pictures by receiving and recording the energy or number of electrons reflected or emitted from a wafer structure. Before taking such a "picture", an electron beam can be projected onto the structure, and when the electrons are reflected or emitted ("leave") from the structure (e.g., from the wafer surface, from the structure below the wafer surface, or both), the detector of the SEM can receive and record the energy or number of these electrons to generate an inspection image. In order to take such a "picture", the electron beam can scan the wafer (e.g., in a line-by-line or zigzag manner), and the detector can receive the leaving electrons from the area (called a "beam spot") under the projection of the electron beam. The detector can simultaneously receive and record the leaving electrons from each beam spot, and combine the information recorded for all beam spots to generate an inspection image. Some SEMs use a single electron beam (called "single-beam SEM") to take a single "picture" to generate an inspection image, while some SEMs use multiple electron beams (called "multi-beam SEM") to take multiple "sub-pictures" of the wafer in parallel and stitch them together to generate an inspection image. By using multiple electron beams, the SEM can provide more electron beams to the structure to obtain these multiple "sub-pictures", resulting in more electrons leaving the structure. Therefore, the detector can receive more leaving electrons at the same time and generate inspection images of the wafer structure with higher efficiency and faster speed.

[0047] Typically, structures are made on a substrate (e.g. a silicon wafer) that is placed on a platform called a stage for imaging. When the electron beams hit the structures, they may charge the substrate so that it is no longer electrically neutral. The charged substrate may acquire a voltage and affect the leaving electrons, thus affecting the image quality. Therefore, to improve imaging, it may be advantageous to ground the substrate.

[0048] For grounding, the substrate can be electrically connected to a power source. The electrical connection between the power source and the substrate can be achieved by pressing one or more conductive ground pins or probes against the back surface of the substrate (i.e., the surface without IC structures). The back surface of the substrate can be covered by a thin layer ("back film") of material.

[0049] However, the back film is not conductive. Various methods can be used to overcome this non-conductive back film and achieve electrical connection. For example: (1) electrical breakdown method; (2) penetration method; (3) pin impact method.

[0050] In the electrical breakdown method, the ground pins are pressed into and partially penetrate, but not completely penetrate, the back film. A power source generates a high voltage (e.g., tens of kilovolts) electrical signal ("breakdown signal") between the ground pins to break through the back film, thereby establishing an electrical connection between the ground pins and the wafer. The breakdown signal causes electrical breakdown between the ground pins and the wafer, thereby breaking through the back film.

[0051] In the penetration method, the ground pin can be pressed into the substrate to penetrate the backside film and directly contact the substrate. However, the penetration method may cause damage to the backside film, which may lead to damage to the substrate during the manufacturing process. It also causes excessive particle generation, which may cause contamination of the SEM vacuum chamber. In addition, as described below, neither the penetration method nor the breakdown method can overcome all types of backside films.

[0052] Some wafers require thicker backside films than others. For example, some complex IC structures may contain a large number of layers. Such multi-layer structures may cause the surface tension of the wafer to be higher than otherwise. The high tension may cause the wafer to warp or bend, resulting in errors (e.g., blurriness) in the inspection image. To avoid wafer warping or bending due to such complex structures, the wafer may be coated with a thickened backside film to enhance its mechanical strength. However, when the backside film is thick enough to prevent the wafer from warping or bending, it may be too thick to achieve acceptable wafer grounding by electrical breakdown methods or conventional penetration methods.

[0053] To overcome the thick film wafer problem, the "pin impact" method was proposed. Unlike the penetration method, which simply presses the pin into the backside film, the wafer grounding system can activate the grounding pin to generate a high impact force and "punch through" the thickened backside film. After penetrating the thickened backside film by impact, an electrical connection between the grounding pin and the conductive surface of the wafer can be established to achieve wafer grounding. However, some backside films are so thick that the force required by the pin impact method may damage the wafer. The deformation caused by the impact may cause overlay errors and generate contaminant particles in the wafer environment. In addition, even if the punch-through is successful, it may be difficult to maintain the conductivity of the ground connection.

[0054] Embodiments of the present disclosure include systems and methods for wafer grounding using an exclusion zone of a backside film. The exclusion zone may be an area on the backside surface where the backside film is not present, or is thinned or otherwise modified (e.g., using a material with a different conductivity). Embodiments of the present disclosure provide clean contact between the ground pin and the conductive surface of the wafer while reducing the risk of particle contamination and deformation-based overlay errors. In addition, the duration and stability of the electrical connection may be improved.

[0055] Embodiments of the present disclosure allow for greater design flexibility in the wafer grounding system. For example, the exclusion zone may be located at the periphery of the wafer, and at least some of the wafer grounding pins may be advantageously moved away from the central region of the wafer. In some embodiments, the wafer may include multiple exclusion zones around the periphery to enable SEM inspection at multiple angular orientations of the wafer. In some embodiments, the wafer may include a single annular exclusion zone around the periphery of the wafer. This enables SEM inspection to have a set of continuously variable angular orientations to choose from.

[0056] Other embodiments of the present disclosure include wafers with backside film exclusion areas, and systems and methods for manufacturing wafers with backside film exclusion areas. Various exemplary systems and methods are disclosed for masking, modifying or preventing film formation at selected areas during formation of a thick backside film.

[0057] In some embodiments, the backside film is formed on the entire surface of the wafer, and portions of the film in the exclusion area are removed during subsequent processing steps. In some embodiments, the exclusion area includes a conductive film having the same or similar thickness as the non-conductive backside film to achieve good electrical contact with a high degree of planarity on the backside surface of the wafer.

[0058] The ground pin may have a single tip to contact the exclusion zone of the wafer. Since the exclusion zone of the wafer may be small, the positional accuracy of the single tip ground pin contacting the exclusion zone may be low. In some embodiments, in order to improve the positional accuracy of the ground pin contacting the exclusion zone of the wafer, each ground pin may include a pin body having two tips extending from the pin body (a "double tip" ground pin). The distance between the first tip and the second tip of the ground pin may be substantially equal to the width of the exclusion zone of the wafer to improve the positional accuracy of the ground pin contacting the exclusion zone of the wafer. The double tip ground pin can be flexibly adjusted so that the chance of the ground pin contacting the exclusion zone of the wafer is increased (i.e., the double tip ground pin can improve the positional accuracy).

[0059] In some embodiments, the ground pin may include a spring structure in the wafer holder, wherein the spring structure may be configured to reduce wafer warpage or wafer bowing by reducing forces on the wafer.

[0060] For the sake of clarity, the relative sizes of the components in the figures may be exaggerated. In the following description of the figures, the same or similar reference numerals denote the same or similar components or entities, and only the differences with respect to the various embodiments are described.

[0061] As used herein, unless otherwise expressly stated, the term "or" encompasses all possible combinations unless not feasible. For example, if a certain component is stated to include either A or B, then, unless otherwise expressly stated or not feasible, the component may include A, or B, or A and B. As a second example, if a certain component is stated to include either A, B, or C, then, unless otherwise expressly stated or not feasible, the component may include A, or B, or C, or A and B, or A and C, or B and C, or A and B and C. Expressions such as "at least one" do not necessarily modify the entire contents of the following list, nor do they necessarily modify each member of the list, so "at least one of A, B, and C" should be understood to include only one of A, only one of B, only one of C, or any combination of A, B, and C. The phrase "one of A and B" or "any one of A and B" should be interpreted in the broadest sense to include one of A or one of B.

[0062] Figure 1 An exemplary electron beam inspection (EBI) system 100 consistent with embodiments of the present disclosure is shown. The EBI system 100 may be used to image or otherwise process a wafer. The wafer may be grounded. Figure 1 As shown, the EBI system 100 includes a main chamber 101, a load / lock chamber 102, a beam tool 104, and an equipment front end module (EFEM) 106. The beam tool 104 is located in the main chamber 101. The EFEM 106 includes a first load port 106a and a second load port 106b. The EFEM 106 may include additional load ports. The first load port 106a and the second load port 106b receive a wafer front opening transport box (FOUP) containing a wafer (e.g., a semiconductor wafer or a wafer made of other materials) or a sample to be inspected (wafers and samples can be used interchangeably). "Batch" refers to a plurality of wafers that can be loaded and processed as a batch.

[0063] One or more robots (not shown) in the EFEM 106 can transport the wafer to the load / lock chamber 102. The load / lock chamber 102 is connected to a load / lock vacuum pump system (not shown), which removes gas molecules in the load / lock chamber 102 to reach a first pressure below atmospheric pressure. After reaching the first pressure, one or more robots (not shown) can transport the wafer from the load / lock chamber 102 to the main chamber 101. The main chamber 101 is connected to a main chamber vacuum pump system (not shown), which removes gas molecules in the main chamber 101 to reach a second pressure below the first pressure. After reaching the second pressure, the wafer will be inspected by the beam tool 104. The beam tool 104 can be a single beam system or a multi-beam system.

[0064] The controller 109 is electrically connected to the beam tool 104. The controller 109 may be a computer configured to perform various controls of the EBI system 100. Figure 1 The controller 109 is shown in FIG. 1 as being external to the structure including the main chamber 101 , the load / lock chamber 102 , and the EFEM 106 , but it will be appreciated that the controller 109 may be part of the structure.

[0065] In some embodiments, the controller 109 may include one or more processors (not shown). The processor may be a general or special electronic device capable of manipulating or processing information. For example, the processor may include any number of any combination of the following: a central processing unit (or "CPU"), a graphics processing unit (or "GPU"), an optical processor, a programmable logic controller, a microcontroller, a microprocessor, a digital signal processor, an intellectual property (IP) core, a programmable logic array (PLA), a programmable array logic (PAL), a general array logic (GAL), a complex programmable logic device (CPLD), a field programmable gate array (FPGA), a system on a chip (SoC), an application-specific integrated circuit (ASIC), and any type of circuit capable of data processing. The processor may also be a virtual processor, which includes one or more processors distributed on multiple machines or devices coupled via a network.

[0066] In some embodiments, the controller 109 may also include one or more memories (not shown). The memory may be a general or specific electronic device capable of storing processor-accessible code and data (e.g., via a bus). For example, the memory may include any number of any combination of the following: random access memory (RAM), read-only memory (ROM), optical disk, magnetic disk, hard disk, solid-state drive, flash drive, secure digital (SD) card, memory stick, compact flash (CF) card, or any type of storage device. The code may include an operating system (OS) and one or more application programs (or "apps") for specific tasks. The memory may also be a virtual memory, which includes one or more memories distributed on multiple machines or devices coupled via a network.

[0067] Figure 2 An example imaging system 200 is shown in accordance with an embodiment of the disclosure. Figure 2 The electron beam tool 104 may be configured for use with reference to Figure 1 The EBI system 100 discussed herein. The electron beam tool 104 may be a single beam device or a multi-beam device. Figure 2As shown, the electron beam tool 104 includes a motorized sample stage 201, and a wafer holder 202 supported by the motorized sample stage 201 for holding a wafer 203 to be inspected. The electron beam tool 104 also includes an objective lens assembly 204, an electron detector 206, an objective lens aperture 208, a focusing lens 210, a beam limiting aperture 212, a gun aperture 214, an anode 216, and a cathode 218. In some embodiments, the objective lens assembly 204 may include a modified swinging objective retarding immersion lens (SORIL) including a pole piece 204a, a control electrode 204b, a deflector 204c, and an excitation coil 204d. The electron beam tool 104 may also include an energy dispersive X-ray spectrometer (EDS) detector (not shown) to characterize the material on the wafer 203.

[0068] A primary electron beam 220 is emitted from the cathode 218 by applying an accelerating voltage between the anode 216 and the cathode 218. The primary electron beam 220 passes through the gun aperture 214 and the beam limiting aperture 212, both of which can determine the size of the electron beam entering the focusing lens 210, which is located below the beam limiting aperture 212. The focusing lens 210 focuses the primary electron beam 220 before the beam enters the objective lens aperture 208 to set the size of the electron beam before entering the objective lens assembly 204. The deflector 204c deflects the primary electron beam 220 to facilitate beam scanning on the wafer. For example, during the scanning process, the deflector 204c can be controlled to deflect the primary electron beam 220 to different locations on the top surface of the wafer 203 at different time points in sequence to provide data for image reconstruction of different parts of the wafer 203. In addition, the deflector 204c can be controlled to deflect the primary electron beam 220 to different sides of the wafer 203 at a specific position at different time points to provide data for stereoscopic image reconstruction of the wafer structure at the position. In addition, in some embodiments, the anode 216 and the cathode 218 can generate multiple primary electron beams 220, and the electron beam tool 104 can include multiple deflectors 204c to simultaneously project multiple primary electron beams 220 to different parts / sides of the wafer to provide data for image reconstruction of different parts of the wafer 203.

[0069] The excitation coil 204d and the pole piece 204a generate a magnetic field that starts at one end of the pole piece 204a and ends at the other end of the pole piece 204a. A portion of the wafer 203 scanned by the primary electron beam 220 may be immersed in the magnetic field and may be charged, thereby generating an electric field. The electric field reduces the energy of the primary electron beam 220 that strikes near the surface of the wafer 203 before colliding with the wafer 203. The control electrode 204b is electrically isolated from the pole piece 204a, and controls the electric field on the wafer 203 to prevent micro-arcing of the wafer 203 and ensure proper beam focusing.

[0070] After receiving the primary electron beam 220, a secondary electron beam 222 may be emitted from a portion of the wafer 203. The secondary electron beam 222 may form a beam spot on a sensor surface of the electron detector 206. The electron detector 206 may generate a signal (e.g., voltage, current, etc.) representing the intensity of the beam spot and provide the signal to the image processing system 250. The intensity of the secondary electron beam 222 and the beam spot generated thereby may vary according to the external or internal structure of the wafer 203. In addition, as described above, the primary electron beam 220 may be projected onto different locations on the top surface of the wafer or different sides of the wafer at a specific location to generate the secondary electron beam 222 (and the beam spot generated thereby) of different intensities. Therefore, by mapping the intensity of the beam spot with the location of the wafer 203, the processing system may reconstruct an image reflecting the internal or surface structure of the wafer 203.

[0071] The imaging system 200 can be used to inspect a wafer 203 on a motorized sample stage 201 and includes an electron beam tool 104, as described above. The imaging system 200 can also include an image processing system 250, which includes an image acquisition device 260, a memory 270, and a controller 109. The image acquisition device 260 can include one or more processors. For example, the image acquisition device 260 can include a computer, a server, a mainframe, a terminal, a personal computer, any type of mobile computing device, etc., or a combination thereof. The image acquisition device 260 can be connected to the detector 206 of the electron beam tool 104 through a medium such as an electrical conductor, a fiber optic cable, a portable storage medium, IR, Bluetooth, the Internet, a wireless network, radio, or a combination thereof. The image acquisition device 260 can receive a signal from the detector 206 and can construct an image. Therefore, the image acquisition device 260 can acquire an image of the wafer 203. The image acquisition device 260 can also perform various post-processing functions, such as generating a contour, superimposing an indicator on the acquired image, etc. The image acquisition device 260 can perform brightness and contrast adjustments on the acquired image, etc. The memory 270 may be a storage medium such as a hard disk, cloud storage, random access memory (RAM), other types of computer-readable memory, etc. The memory 270 may be coupled to the image acquirer 260 and may be used to save the scanned raw image data as raw images and post-processed images. The image acquirer 260 and the memory 270 may be connected to the controller 109. In some embodiments, the image acquirer 260, the memory 270, and the controller 109 may be integrated together as a control unit.

[0072] In some embodiments, the image acquirer 260 may acquire one or more images of the sample based on the imaging signal received from the detector 206. The imaging signal may correspond to a scanning operation for performing charged particle imaging. The acquired image may be a single image including multiple imaging regions. The single image may be stored in the memory 270. The single image may be an original image that may be divided into multiple regions. Each region may include an imaging region that includes a feature of the wafer 203.

[0073] Wafer grounding can be achieved by conducting charge from wafer 203 to wafer holder 202 to make wafer 203 electrically neutral. In a comparative grounding system, wafer grounding can be performed using a penetration method or an electrical breakdown method. In these methods, a wafer can be placed on a wafer stage with its back supported by the wafer stage. A coating (e.g., a back film applied to the back of the wafer) can be present on the surface of the back of the wafer substrate. The back film can be non-conductive. Two or more ground pins made of a conductive material (e.g., metal) can be pressed on the back film without completely piercing it.

[0074] In the electrical breakdown method, current can enter the wafer from the first ground pin through the back film through the first dielectric breakdown, and flow out of the wafer from the back film to the second ground pin through the second dielectric breakdown. The dielectric breakdown can result in a stable electrical path (e.g., a direct current (DC) path) through the back film, which can be referred to as a "bias path". The bias path can have an effective resistance. For example, the resistance of the back film can contribute to the effective resistance, which represents the resistance of the bias path from the first ground pin through the wafer to the second ground pin.

[0075] Figure 3 It is a schematic diagram of a wafer grounding system 300 in a comparative embodiment. The system 300 includes a subsystem 302 for fixing a wafer, an electrical signal generator 314 , a sensor 316 , a controller 322 , and a control parameter optimizer 324 .

[0076] Subsystem 302 includes electrostatic holder 306 and wafer 304. In some embodiments, wafer 304 and Figure 2 The chip 203 is similar or identical to the electrostatic holder 306. Figure 2The subsystem 302 may be similar or identical to the wafer holder 202 in FIG. 304. The wafer 304 includes a back film 308. The back film 308 may be non-conductive. The electrostatic holder 306 may include at least one electrode 310. When powered, the electrode 310 may attract and fix the wafer 304 to the electrostatic holder 306 through an electrostatic field. The subsystem 302 also includes at least one ground pin (or "probe") 312. The ground pin 312 may be electrically connected between the electrical signal generator 314 and the wafer 304. In some embodiments, the ground pin 312 may be pressed against the back film 308 without completely penetrating the back film 308. The ground pin 312 may be electrically connected to the electrical signal generator 314 and the sensor 316.

[0077] The electrical signal generator 314 can generate a breakdown signal for grounding the wafer 304. In some embodiments, the electrical signal generator 314 is a driver. The breakdown signal can have a high voltage for causing dielectric breakdown between the ground pin 312 and the wafer 304 through the back film 308. The sensor 316 can be used to detect or measure an electrical characteristic 320 associated with electrical breakdown. For example, the electrical characteristic 320 can include at least one of the following: impedance, resistance, capacitive reactance, admittance, emissivity, conductance, capacitive susceptance, or any parameter indicating wafer characteristics. In some embodiments, the electrical characteristic 320 can be associated with an electrical path including the ground pin and the wafer. For example, the subsystem 302 can be a single-pin system including a single ground pin 312. In the single-pin system, the sensor 316 can be electrically connected to the wafer 304, and the electrical characteristic 320 indicating electrical breakdown between the ground pin 312 and the wafer 304 can be measured through the back film 308. Figure 3 Further details of the system can be found in International Publication No. WO2021 / 037827, the entire contents of which are incorporated herein by reference.

[0078] In some embodiments, it is necessary to fabricate highly complex structures on a wafer. Such complex structures may include a large number of layers. For example, the complex structure may include a three-dimensional circuit that includes one or more non-AND ("NAND") gates, such as a NAND flash memory circuit. The multi-layered complex structure may cause higher tension on the surface of the wafer than other structures, which may cause the wafer to bend or warp. A warped wafer may cause problems during inspection, as portions of the wafer may deviate from the primary electron beam (e.g., Figure 2 These problems may result in a decrease in the quality of the inspection image (e.g., out of focus, blur, distortion, etc.).

[0079] In order to avoid the wafer warping or bending caused by this complex structure, in some embodiments, the wafer can be coated with a thickened back film to enhance its mechanical strength. The back film can be thickened 2 times, 5 times or 10 times or more. For example, in some comparative cases, the thickness of the back film can be 0.1-0.3 μm. In order to avoid the wafer warping or bending, the thickness of the back film can be increased (for example, increased to 1.4-2.2 μm or more). However, the thickened back film may be too thick, so that both the electrical breakdown method and the penetration method cannot effectively achieve wafer grounding. For example, the thickened back film may be too thick, so that there is no dielectric breakdown in the electrical breakdown method to break it down. In another example, the thickened back film may be too thick, so that it cannot be penetrated by pressing the ground pin through the penetration method.

[0080] In order to ground a wafer having a thickened backside film, a "pin-bumping method" has been proposed. Figure 4A-4D 4 shows the operation stages of a comparative system 400 for pin-impacting wafer grounding. The system 400 may be any system for wafer grounding (e.g., Figure 3 A subsystem of the system 300). Figure 4A-4D Only one ground pin is shown, but it should be noted that any single-pin system (e.g. Figure 3 The subsystem 302 in the embodiment of the present invention or the multi-pin system can be configured to implement the pin shock method compatibly. For example, in a multi-pin system, the pin shock method can be implemented compatibly on one or more ground pins of the multi-pin system.

[0081] exist Figure 4A-4D In the embodiment, system 400 includes wafer 404, backside film 408, ground pins 412, and an actuator (not shown). Backside film 408 may be connected to Figure 3 In some embodiments, the back film 408 may be the same or similar to the back film 308 in the embodiment. In some embodiments, the back film 408 may be thickened. For example, the thickness of the back film 408 may exceed 0.3 μm (e.g., 1.4-2.2 μm). In some embodiments, the actuator may include one of the following: an electric actuator (e.g., an electromechanical actuator such as an electric motor, or an electrohydraulic actuator including a hydraulic accumulator), a magnetic actuator (e.g., an electric motor), a spring (e.g., a coil spring or a coil polymer), a pneumatic actuator, or a hydraulic actuator.

[0082] Figure 4A An initial stage of using the system 400 is shown, wherein the ground pin 412 may be controlled (e.g., by Figure 3322 in the controller 322) to contact the back film 408. For example, the actuator in the initial stage can be disabled. In other words, the ground pin 412 can be in a default position in the initial stage, where the default position causes the ground pin 412 to contact the back film 408. This configuration in the initial stage can ensure the ground compatibility of the system 400 for wafers without a thickened back film. For example, when a wafer without a thickened back film is placed in the system 400, by Figure 4A In the illustrated setup initialization phase, the system 400 may perform other methods for wafer grounding (eg, an electric shock method or a penetration method) without invoking the pin shock method.

[0083] Figure 4B The first stage of the system 400 implementing the pin impact method is shown, wherein the ground pin 412 is moved away (as indicated by the arrow) from the back film 408. In some embodiments, the actuator can move the ground pin 412 away from the back film 408. In some embodiments, the ground pin 412 can be moved away from the back film 408 so that the distance between the ground pin 412 (e.g., measured from the tip of the ground pin 412) and the back film 408 can exceed 100 microns. For example, the distance can exceed 1 mm. In some embodiments, by moving the ground pin 412 away from the back film 408, the ground pin 412 can have enough room for acceleration, as described below.

[0084] Figure 4C The second stage of the pin impact method implementation of the system 400 is shown, in which an actuator (not shown) can actuate (e.g., accelerate) the ground pin 412 toward the back film 408 (as shown by the arrow). In some embodiments, the acceleration can end before the ground pin 412 impacts the back film 408. In some embodiments, the actuator can actuate the ground pin 412 so that the kinetic energy of the ground pin 412 before impacting the back film 408 can exceed, for example, 0.0002 joules (e.g., in the case of a maximum travel distance of 3 mm for the ground pin 412). It should be noted that the kinetic energy of the ground pin before impacting the back film 408 can depend on the distance it travels under the actuation of the actuator and is not limited to the above examples.

[0085] Figure 4D The final stage of the pin-shocking method implemented by the system 400 is shown, in which the ground pin 412 is Figure 4CThe back film 408 is penetrated by impact using the kinetic energy obtained in the second stage described in . In some embodiments, the ground pin 412 can completely penetrate the back film 408 and directly contact the wafer 404 without drilling into it. In this case, an electrical connection between the ground pin 412 and the wafer 404 can be established using a penetration method for wafer grounding to ground the wafer 404. In some embodiments, the ground pin 412 may not completely penetrate the back film 408, so that the distance between the tip of the ground pin 412 and the surface of the wafer 404 (e.g., a conductive surface) can be less than or equal to 0.3 microns. In this case, an electrical connection between the ground pin 412 and the wafer 404 can be established for grounding the wafer 404 using an electric shock method for wafer grounding. For more details on the pin impact method, please refer to International Publication No. WO2021 / 037827.

[0086] Pin impacting may not overcome all the shortcomings of existing technologies. For example, the destructive action of piercing a thick backside film may introduce particulate contaminants into the wafer environment. The impact force may damage the ground pin and shorten its service life. Even if the impact is successful, it is difficult to maintain conductivity between the wafer and the ground pin. The impact force may also cause the wafer to deform, which affects the overlay performance. Since the impact energy required to pierce the film is higher, the risk of deformation increases with the thickness of the film. In addition, as described below, if the location of the impact hole is not selected properly, additional overlay errors may be introduced in subsequent processes.

[0087] Figure 5 Figure 1 shows an overlay problem in subsequent processing that can be caused by improper placement of the pin impact holes. Figure 5 In the embodiment, during a subsequent processing stage, the wafer that has undergone the inspection process is located on a different wafer holder. For example, the wafer holder can be a wafer table WT and the processing stage can be a lithographic exposure of another device layer in a microlithographic exposure device. The wafer 504 is supported at the back film 508 by a plurality of burls B, which are a series of protrusions that form a planar support surface SS. During the previous inspection step, holes H were created in the back film 508 for grounding the wafer 504. If the wafer 504 is mounted on the wafer table WT so that the hole H is located above one of the burls B, the wafer may not be properly supported. This can cause sagging, which can lead to overlay errors in the exposure process.

[0088] Embodiments of the present disclosure reflect an improved method for grounding wafers, including wafers with thick backside films. Rather than punching a large hole in the backside film during setup for the inspection process, an exclusion zone is created in the backside film during film formation. The grounding pin can easily make stable electrical contact with the conductive surface of the wafer because there is no film impeding contact at the grounding location. Alternatively, there may be a modified film in the exclusion zone where it is easier for the grounding pin to make electrical contact with the wafer than with other portions of the backside film. The advantages of the present disclosure will be described in conjunction with the embodiments discussed herein.

[0089] Fig. 6A Subsystem 600 and wafer 604 are shown consistent with some embodiments of the present disclosure. Subsystem 600 may be a subsystem of any system for wafer grounding (e.g., Figure 3 In the system 300). Fig. 6A , an exclusion zone 613 is formed in the back film 608 and aligned with the ground pin 612. The exclusion zone 613 can be formed as a plurality of spaced-apart regions, a single continuous region, or any geometric configuration. Alternatively or additionally, any one of the ground pin 612, the wafer 604, the holder 606, or a sub-component, a stage, or other supporting component of the holder 606 can be moved by an actuator so as to align the ground pin 612 with the exclusion zone 613. The back film 608 can include a non-conductive material or a material having a lower conductivity than the material of the wafer 604. For example, the back film can include silicon dioxide, and the wafer can include silicon. The film can be, for example, silicon nitride, other oxides, nitrides, carbides, or other suitable film materials for providing structural support, for example, to prevent the wafer from bending or warping. The exclusion zone 613 can be a portion of the film material missing or modified in the back film 608 layer. The missing portion exposes the conductive surface of the wafer 604 to the ground pin 612. However, in some embodiments, the back film material may not be completely missing from some or all of the exclusion zones 613. In some embodiments, the backside film 608 is only thinner than the surrounding portions to allow grounding by any wafer grounding method, such as through-the-wire, breakdown, or pin-boosting.

[0090] although Fig. 6A Two ground pins are shown, but it should be noted that a single-pin system can be configured (e.g. Figure 3 subsystem 302 in) or a multi-pin system to compatibly implement the exclusion zone method. Figure 6BIn the multi-pin system shown, an exclusion zone can be formed for each position of its multiple ground pins, or an exclusion zone can be formed for a subset of the positions of its multiple ground pins. The exclusion zone can be more or less than the ground pins. It should be understood that other variations are consistent with some embodiments of the present invention. For example, there can be a single or multiple ground pins 612. There can be a single or multiple exclusion zones 613. The number of pins 612 can be less than, greater than, or equal to the number of exclusion zones 613. One or more ground pins in the ground pins 612 can be configured to perform an exclusion grounding method, a penetration method, a breakdown method, a pin impact method, or any other suitable wafer grounding method or a combination of wafer grounding methods. The ground pins 612 and the retainer 606 can be compatible with various wafers, including thin and thick back film wafers, wafers with exclusion zones, and wafers without exclusion zones.

[0091] Figure 6C is a diagram of an example system 600 for wafer grounding position adjustment consistent with an embodiment of the present disclosure. Figure 6C The configuration in the beam tool 104 of the main chamber 101 is disclosed, but the present disclosure is not limited to this arrangement, and not all of the illustrated arrangements will appear in all possible embodiments. In some embodiments, the system 600 can be located in the main chamber 101, such as the load lock chamber 102 or the beam tool 104. However, in general, the system 600 can be applied to any system or module that supports the wafer 604 during a process step. The system 600 may include a subsystem 602 configured to support the wafer 604, a controller 615, a sensor 616, and a target adjustment 614. The subsystem 602 may be similar to Figure 3 Subsystem 302 or Figure 6A-6B 602 in the wafer stage and may include a wafer 604, a holder 606, a backside film 608, an electrode 610, a ground pin 612, a top portion 607 of the wafer stage, a bottom portion 609 of the wafer stage, and an actuator including a lifter 608.

[0092] Sensor 616 can measure the position or orientation of wafer 604. Alternatively or additionally, sensor 616 can measure the position or orientation of exclusion zone 613. The position or orientation can be relative to ground pin 612, holder 606, stage top 607, stage bottom 609, or another reference position or orientation. Sensor 616 can be located above, below, or near wafer 604. Sensor 616 can be embedded or mounted in holder 606, stage top 607, stage bottom 609, or any other structural component that enables the sensor to determine the desired parameters. Sensor 616 can be configured to access the back surface of wafer 604 through a hole or other opening in the middle component. For example, sensor 616 can be located on stage top 607 and configured to view wafer 604 through an opening in holder 606. Sensor 616 can be configured to detect reference features, such as alignment notches or flats, wafer edges, fiducial marks, etc. For example, sensor 616 may include a laser or other radiation source located above or below the wafer, and a camera configured to detect radiation, such as a CCD, CMOS, or other detection device. Sensor 616 may include, for example, an alignment or pre-alignment measurement unit configured to detect alignment features. Sensor 616 may be configured as a z-height sensor or other profilometer for identifying exclusion zone 613 by wafer backside topography, which is caused by changes in backside film thickness. Typically, sensor 616 may be optical, capacitive, ultrasonic, or any other configuration to achieve the desired detection. For example, sensor 616 may use imaging, time of flight, interferometry, ellipsometry, capacitance, ultrasonic, or any other detection system to determine an exclusion zone or reference position.

[0093] In some embodiments, target adjustment 614 may include parameter values ​​used by controller 615 to control an actuator of subsystem 602 to align the ground pin 612 position with a target position. For example, the target position may include the position of exclusion zone 613. In some embodiments, data for target adjustment 614 may be stored in a database (e.g., Figure 1 The actuator may include an electric actuator, a magnetic actuator, an electromagnetic actuator, a hydraulic actuator, a mechanical actuator, or any suitable type of actuator. In some embodiments, the wafer stage (including the top 607 and the bottom 609) may be Figure 2 The motorized sample stage 201 in FIG.

[0094] Controller 615 may be electrically connected to sensors 616 and actuators, including lifter 608 and an actuator (not shown) mechanically connected to top 607. Controller 615 may control the actuators to move various parts of subsystem 602, such as lifter 608, top 607, ground pins 612, or other mechanical components (e.g., a robotic arm) for moving wafer 604. For example, a dashed arrow between controller 615 and top 607 may indicate that controller 615 may control an actuator (not shown) to move top 607 horizontally, vertically, or both. A dashed arrow between controller 615 and lifter 608 may indicate that controller 615 may control lifter 608 to move wafer 604 vertically. In some embodiments, controller 615 may also be connected to a database to retrieve parameters for controlling actuators or to store data received from sensor 616. For example, controller 615 may access a database storing target adjustments 614. In some embodiments, controller 615 may be implemented as Figure 1-Figure 2 In some embodiments, the controller 615 may be implemented as a controller independent of the controller 109, such as a software module or a hardware module.

[0095] In some embodiments, the bottom 609 can be fixed and the top 607 can be movable. For example, the top 607 can be movable (e.g., in a vertical direction, a horizontal direction, or both) or can rotate in a horizontal direction, or both. In some embodiments, the holder 606 can be fixed to the top 607 or can move with it. In some embodiments, the top 607 can support the wafer 604 via the holder 606 and fix the ground pin 612. For example, one end of the ground pin can be fixed to the top 607 or can move with the top 607. When the wafer 604 rests on the top 607 (e.g., on the top of the holder 606), the ground pin 612 can contact the bottom surface of the wafer 604 (e.g., the back film 608).

[0096] In some embodiments, the actuator can move the top. For example, the actuator may include a rotating mechanism (not shown) to rotate the top 607 in a horizontal direction, such as rotating a certain azimuth angle. In some embodiments, the actuator may include a lifter 608. The first end of the lifter may be fixed to the bottom 609, and the second end of the lifter may be moved vertically. For example, the first end of the lifter may be fixed horizontally to the bottom 609 (for example, by penetrating a hole in the bottom 609) and may be moved vertically. The second end of the lifter may be raised or lowered by a moving mechanism (for example, an electromagnetic actuator or a hydraulic actuator). The second end of the lifter may pass through the top 607, the holder 606, and the electrode 610, such as by penetrating a hole or groove therein. The second end of the lifter may be moved outside the top surface of the holder 606 and contact the bottom surface of the wafer 604. In the subsystem 602, by lifting the lifter to a certain height (for example, a few millimeters), the wafer 604 can be lifted to leave the top surface of the holder 606 and separate from the ground pin 612.

[0097] In some embodiments, the lifter 608 can be fixed vertically and horizontally, while the top 607 can be moved vertically. When the top 607 is lowered, the ground pins 612 and the holder 606 can also be lowered. However, the lifter 608 can support the wafer 604, while the wafer 604 can be fixed vertically. By lowering the top 607, the holder 606 can be lowered to leave the bottom surface of the wafer 604, and the ground pins 612 can be separated from the bottom surface.

[0098] In some embodiments for wafer grounding position adjustment, the wafer can be loaded into a predetermined position or orientation based on the determined position of the exclusion zone. For example, a reference feature, such as an alignment notch or plane, can be determined using visual inspection, pre-alignment detection, or other sensing operations. The exclusion zone position can then be determined by the known relationship between the reference feature and the exclusion zone. Alternatively or additionally, the exclusion zone position can be directly determined using a sensor. In some embodiments, the position of the exclusion zone or reference feature can be determined using a sensor 616 as described above. Based on the determined position of the exclusion zone, the wafer can then be loaded into an appropriate position or orientation so that the ground pin 612 is aligned with the desired exclusion zone 613.

[0099] In some embodiments, the controller 615 can adjust the relative displacement between the ground pin 612 and the exclusion zone 613 based on the position error determined between them. For example, the controller 615 can control the sensor 616 to measure a parameter indicating the relative position or orientation of the ground pin 612 and the exclusion zone 613. The controller 615 can also retrieve the target adjustment 614 (e.g., the value of the target position or rotation angle). The controller 615 can compare the target position or angle with the current position or angle, for example by determining the difference between them. The controller 615 can then control the various actuators discussed above to adjust the ground position. In some embodiments, the controller 615 can store computer-readable instructions in an accessible memory, such as a software module, and execute such instructions to perform the above operations. Additional actuation details can be found in the international publication number WO2021 / 037827 cited above, which is incorporated herein by reference in its entirety.

[0100] The size of the exclusion area 613 can be designed to allow easy and stable electrical contact between the ground pin 612 and the wafer 604. The size of the exclusion area 613 can be expressed as a proportion of the total area of ​​the wafer 604, or can be relative to the ground pin 612 or other elements. For example, the size of each exclusion area 613 can be at least as large as the cross-sectional contact area of ​​each ground pin 612. The size of the exclusion area 613 can be large enough to account for alignment errors between the ground pin and the centroid of the exclusion area. In some embodiments, the area of ​​each exclusion area 613 can be at least 1, 1.5, 2, 3, 5, 10, or 20 times the cross-sectional contact area of ​​the corresponding ground pin 612. The exclusion area can be, for example, 0.04 to 0.06 mm 2 In some embodiments, each exclusion zone 613 may have a diameter of at least 0.01, 0.1, 0.5, 1, 1.5, 2, 3, or 5 mm. 2 or larger area.

[0101] In some embodiments, the size of the exclusion zone can be designed according to the predetermined positioning accuracy of the ground pin relative to the exclusion zone. For example, if the positioning accuracy of the center of the ground pin relative to the center of the exclusion zone is + / -90μm, the exclusion zone size can be equal to the width of the ground pin plus 180μm. Alternatively, a larger tolerance can be added to account for unforeseen errors or other problems. For example, the size of the exclusion zone with the same conditions as above can be designed to have a positioning tolerance of + / -250μm. In this case, the exclusion zone size can be equal to the width of the ground pin plus 500μm.

[0102] Due to limitations in rotational positioning accuracy, the exclusion zone size may also depend on the radial position on the wafer. Fig.6DAs shown, the bottom surface of the wafer 604 has two circular exclusion zones: an inner exclusion zone 613i located near the center of the wafer 604 and an outer exclusion zone 613o located near the periphery. For a given exclusion zone size, the angular range θ1 of the inner exclusion zone 613i will be greater than the angular range θ2 of the outer exclusion zone 613o. Therefore, when the exclusion zone is located close to the edge of the wafer, it may be subject to tighter positioning tolerances (such as Fig.6D center) or the increased size in the circumferential direction (as shown in Fig.6D However, since the exclusion zone can be created during the film formation process, there is a lot of design flexibility that allows the use of peripheral exclusion zones.

[0103] In some embodiments, the size of the exclusion zone in the first direction may be different from the size in the second direction. For example, the first direction may be a radial direction on the wafer surface, and the second direction may be a circumferential direction on the wafer surface. The size in the first direction may be at least 0.1, 0.5, 1, 1.5, 2, 3, or 5 mm or more. The size in the second direction may be greater than the size in the first direction. In some embodiments, the size in the second direction may be 2 times, 5 times, 10 times, or 50 times or more of the size in the first direction. The size in the second direction may surround the entire wafer. Alternatively, the size in the second direction may be the same as or smaller than the size in the first direction.

[0104] In some embodiments, the ground pins can have geometries such as pointed, elongated, or domed. In some embodiments, the additional freedom provided by customizing the keep-out regions can allow for pins of different sizes or geometries than currently used. For example, the keep-out regions can be made large enough to accommodate larger ground pins to increase contact area, stability, or durability. Additionally, the ground pins can have different geometries, such as blunt tips or flat cylinders, to increase the contact surface area between the pin and the wafer while achieving a mechanically stable connection.

[0105] Figure 7A-7B Subsystem 700 and wafer 704 are shown consistent with some embodiments of the present disclosure. Subsystem 700 may be a subsystem of any system for wafer grounding (e.g., Figure 3 System 300). Fig. 7AThe back side of a wafer 704 in a subsystem 700 is schematically shown. A holder 706 supports the wafer 704 and contacts a back side film 708 of the wafer 704. The holder 706 may be an electrostatic holder including at least one electrode 710. A ground pin 712 is located in a peripheral region. The peripheral region may be located at the periphery of the wafer 704. An exclusion zone 713 is annular and surrounds the periphery of the wafer 704. In this arrangement, the exclusion zone 713 may avoid overlay problems, for example, if the exclusion zone 713 is located outside a burl region of the wafer stage or holder 706. For example, as described above with respect to Figure 5 As described, there may be a plurality of burls B protruding from the wafer table WT to form a planar support surface, and if no exclusion zone is provided, it may be possible to create holes H in the backside film for grounding the wafer in the burl region. Alternatively, even if the annular exclusion zone is located above the protrusions, any resulting wafer sag may be more symmetrical and therefore may be easier to compensate for. In some embodiments, positioning the ground pins 712 at the periphery of the wafer 704 may also provide greater flexibility or simplicity in the design of the holder 706 and the electrode 710.

[0106] Figure 7B Subsystem 700 is shown along Fig. 7A The ground pin 712 is able to make direct electrical contact with the conductive surface of the wafer 704 regardless of which portion of the annular exclusion zone 713 is located above it. In this way, the annular exclusion zone 713 allows for greater flexibility. The wafer 704 can be rotated as needed, such as for alignment purposes, and then the wafer 704 can be grounded by deploying the ground pin 712. For example, in some embodiments, it may be desirable to scan the electron beam in a particular direction relative to a device feature of a wafer that is undergoing inspection or lithography. It may be desirable to orient the electron beam at a selected angle. Fig. 7A In some embodiments, it may be desirable to scan the wafer multiple times using multiple different angular orientations. Figure 7A-7B In the embodiment of the present invention, the ground pins 712 can contact the conductive surface in the exclusion area 713 regardless of the angular orientation of the mounting wafer 704.

[0107] Figure 7A-7BThe arrangement of shows a single ground pin 712 and a continuous exclusion zone 713, but it should be understood that other variations are consistent with some embodiments of the present disclosure. For example, there may be multiple ground pins 712 or multiple discrete exclusion zones 713. The number of ground pins 712 may be less than, greater than, or equal to the number of exclusion zones 713. The ground pin 712 may be configured to perform any of the following: an exclusion grounding method, a penetration method, a breakdown method, a pin impact method, or any other suitable wafer grounding method or combination of wafer grounding methods of the present disclosure. The ground pin 712 and the retainer 706 may be compatible with a variety of wafers, including thin and thick back film wafers, wafers with exclusion zones, and wafers without exclusion zones.

[0108] Figure 8A-B Subsystem 800 and wafer 804 are shown consistent with some embodiments of the present disclosure. Subsystem 800 can be any system for wafer grounding (e.g., Figure 3 A subsystem of the system 300). Fig. 8A The back side of a wafer 804 in a subsystem 800 is schematically shown. A holder 806 supports the wafer 804 and contacts a back side film 808 of the wafer 804. The subsystem 800 includes a plurality (e.g., three) of ground pins 812 spaced apart at equal angular offsets (e.g., offset by 120°) and arranged to contact the periphery of the wafer 804. The wafer 804 includes a plurality (e.g., six) of exclusion zones 813 located at the periphery of the wafer 804, spaced apart at equal angular offsets (e.g., offset by 60°), the angular offsets corresponding to the offsets of the ground pins 812 or multiples thereof (e.g., 2). Alternatively or additionally, the ground pins 812 may be moved by an actuator so as to be positioned below the exclusion zones 813. The wafer 804 may be mounted such that the ground pins 812 are positioned below the first set of exclusion zones 813a or the second set of exclusion zones 813b. The size of the exclusion zone in the circumferential direction may be large enough to accommodate angular adjustments of the wafer 804 .

[0109] Figure 8B shows a subsystem 800 along Fig. 8A The ground pin 812 is able to make direct electrical contact with the conductive surface of the wafer 804 at any exclusion zone 813 located above it. In this way, multiple exclusion zones 813 allow for greater flexibility, as described above with respect to Figure 7A-7B described.

[0110] For example, the method may include: supporting a wafer on a holder at a first angular orientation; grounding the wafer by contacting a ground pin to a first exclusion zone; performing a first charged particle beam process (such as a first SEM inspection) on the wafer at the first angular orientation; supporting the wafer on a holder at a second angular orientation different from the first angular orientation; grounding the wafer by contacting a ground pin to a second exclusion zone; and performing a second charged particle beam process (such as a second SEM inspection) on the wafer at the second angular orientation. The first and second exclusion zones may be first and second portions of a continuous exclusion zone (such as Fig. 7A 713 shown), or first and second discrete exclusion zones (such as Fig. 8A 813a and 813b shown).

[0111] Figure 9A-9B 904 and a wafer 904. Figure 9A-9B , the exclusion area includes a second material 911 having a higher conductivity than the first material 909 of the back film 908. The second material may include a conductive material such as aluminum, tungsten, gold, copper or any other metal or conductive material. The second material 911 may partially or completely fill the gap in the back film 908. The second material 911 may be substantially coplanar with the back film 908. The second material 911 may be used to increase further support for wafer bending or warping. Compared to other embodiments, the second material 911 may increase the back flatness of the wafer 904 while still providing a stable electrical connection between the ground pin 912 and the wafer 904.

[0112] The first material 909 and the second material 911 of the back film may have different properties in addition to conductivity. For example, the hardness of the second material 911 may be less than the hardness of the first material 909 of the back film 908. The back film 908 may be configured to allow the ground pin 912 to penetrate the second material 911 more easily than the first material 909.

[0113] The exclusion zone configuration is not limited to the configurations in FIGS. 7-9 . Fig.10 A number of possible exclusion zones on wafers (a)-(f) are shown by way of example and not limitation. In general, the number, size, shape, area or any similar parameter of the exclusion zones may vary as desired. The exclusion zones may have at least one of annular, arcuate, rectangular and circular shapes. The exclusion zones may be located in the center, peripheral or middle regions, or in a combination of these regions. The exclusion zones may include voids where the back film material is completely absent, regions where the back film is relatively thinner than the rest of the back film layer, or regions containing a second material having a higher conductivity (or some other property) than the first back film material. Although Fig.10The arrangement is symmetrical, but the exclusion zones need not be arranged in a rotationally or mirror-symmetrical manner. In some embodiments, a single exclusion zone may be located on the wafer, for example, at the periphery.

[0114] Fig.11A A processing chamber 1100 for forming a backside film on a wafer 1104 in a comparative embodiment is shown. The processing chamber may include a suspension unit 1150 for suspending the wafer 1104 above a processing unit 1160 to expose the backside of the wafer 1104 to a processing material 1170 in a processing region. The processing material 1170 may include, for example, a process gas, a target material, a chemical precursor, a plasma, or a combination of these processing materials, depending on the nature of the film forming process. The suspension unit 1150 includes one or more support members 1152 for supporting the backside of the wafer 1104 at one or more points. The comparative embodiment is not designed to form an exclusion zone for grounding the wafer 1104 during a subsequent SEM inspection process or other semiconductor manufacturing process. The support member 1152 has a narrow contact point at the backside of the wafer 1104 to suspend the wafer 1104 while allowing the backside film 1308 to be formed on substantially the entire backside surface.

[0115] The processing chamber 1100 may be configured to perform any film forming process known in semiconductor manufacturing. By way of example and not limitation, the film forming process may include chemical vapor deposition (CVD), plasma enhanced chemical vapor deposition (PECVD), low pressure chemical vapor deposition (LPCVD), high density plasma chemical vapor deposition (HDPCVD), physical vapor deposition (PVD), plasma enhanced physical vapor deposition (PEPVD), atomic layer deposition (ALD), plasma enhanced atomic layer deposition (ALD), sputtering, passivation, or any process for depositing, coating, or growing a backside film on the wafer 1104. In some embodiments, the processing chamber 1100 is a PECVD chamber. The processing unit 1160 may include a showerhead electrode electrically connected to a high frequency power supply (not shown) and configured to introduce a process gas 1170 including a backside film material precursor. The wafer 1104 is connected to a ground electrode (not shown), and the electrode and the high frequency power supply ionize the precursor in the process gas 1170 to form a plasma, and some reactants in the plasma are deposited as a backside film 1108.

[0116] Fig. 11B Shown in Fig.11A A back view of a wafer 1104 being processed in a processing chamber. Fig. 11BAs shown, the wafer backside film 1108 formed in the processing chamber 1100 includes a plurality of film reduction points 1114. The film reduction points are locations where the formation of the backside film 1108 is hindered to some extent by the support member 1152. The film reduction points 1114 can be considered as partially excluded areas that are smaller than the ideal size or do not fully expose the conductive surface. For example, the size of the film reduction points in the radial direction can be, for example, between 0.1-1.5 mm.

[0117] Comparative embodiments may be designed to prevent film reduction points 1114 as much as possible, and film reduction points 1114 may not fully expose the conductive surface of wafer 1104, or may not expose enough conductive surface area to achieve optimal grounding through the excluded area method. However, in some embodiments, the grounding method may include connecting film reduction points 1114 to ground pins (such as Figures 7A-9B The grounding method may include grounding the chip 1104 using a penetration method, a breakdown method, a pin-striking method, or any other suitable chip grounding method or combination of chip grounding methods.

[0118] Compared to the comparative embodiment, the exclusion grounding method can be designed to form an exclusion zone for the grounding process. The exclusion grounding method can include determining the location of the exclusion zone. Determining the location of the exclusion zone can be based on information obtained during the determination process or previously known information.

[0119] The information acquired during the determination process may include, for example, optical or visual inspection information. For example, a special inspection may be performed to locate the exclusion area on the back side of the wafer. The inspection may be a visual inspection performed by an operator. The inspection may be an optical inspection. The optical inspection may distinguish the exclusion area from its surroundings by detecting differences in the optical properties (e.g., reflection, refraction, absorption, filtering, or other properties) of the back side of the wafer relative to ambient light or projected light. The inspection may be an optical inspection for distinguishing the exclusion area from its surroundings by detecting differences in the optical properties (e.g., reflection, refraction, or filtering properties) of ambient light or projected light passing through the wafer. Alternatively, data from another inspection may be used to determine the location of the exclusion area. The inspection may determine the location, shape, size, or type (e.g., voids, thin film areas, alternative materials, etc.) of the exclusion area. The information acquired during the determination process may include an electrical inspection. For example, electrical detection may utilize a sensor 316 to detect or measure electrical properties 320, as described above with respect to Figure 3 Measurements of electrical properties at different points on the wafer surface can be used to determine the location, shape, size or type of the exclusion zone.

[0120] The previously known information may include the location, shape, size, or type of the exclusion zone provided by the manufacturer or supplier of the wafer. For example, the center location of the exclusion zone may be provided in polar coordinates relative to a reference mark (such as a pre-alignment notch). The location may be given by its overlapping features, such as a band around the pre-alignment notch with a certain thickness (e.g., 0.01, 0.1, 0.5, 1, 1.5, 2, 3, or 5 mm), or an annular ring extending radially inward from the edge a certain distance (e.g., 0.01, 0.1, 0.5, 1, 1.5, 2, 3, or 5 mm). The previously known information may include information acquired as described above, wherein the acquired information is acquired from a different wafer.

[0121] Fig. 12A A processing chamber 1200 consistent with some embodiments of the present disclosure is shown. The processing chamber 1200 can be similar to the processing chamber 1100, except as described herein. The suspension unit 1250 includes one or more support members 1253 configured to cover one or more exclusion zones 1213 (see Fig. 12B ). Support member 1253 can be configured to support wafer 1204 during the film formation process. At the same time, support member 1253 can be configured as an exclusion mask, which is sized and shaped to prevent the formation of a thin film at exclusion area 1213. Support member 1253 can have a size, shape, and configuration corresponding to any exclusion area disclosed or contemplated herein, including exclusion areas 613, 713, 813, 913, and 1013. For example, support member 1253 can take the form of an arc or ring around the back side of wafer 1204, or any other shape as needed to create a desired exclusion area.

[0122] Fig. 12B A wafer 1204 is shown with exclusion zones formed thereon consistent with some embodiments of the present disclosure. The wafer 1204 has a backside film 1208 formed in a processing chamber 1200. Since the support member 1253 contacts the backside of the wafer 1204 at the exclusion zones 1213 during formation of the backside film 1208, film formation is reduced or eliminated in the exclusion zones 1213. Thus, a thick backside film may be formed while providing exclusion zones 1213 having any desired number, size, shape, location, and orientation. For example, the exclusion zones 1213 may be formed with respect to Fig.10 public form or any other desired form.

[0123] Fig. 12C A process chamber 1201 consistent with some embodiments of the present invention is shown. The process chamber 1201 may be similar to Fig. 12A Processing chamber 1200 or Fig.11AThe processing chamber 1100 is shown in FIG. 1200 , except as described below. The suspension unit 1250 includes a proximity exclusion mask 1254 near the back side of the wafer 1204. In some embodiments, the exclusion mask 1254 does not contact the wafer 1204. In some embodiments, the exclusion mask 1254 contacts the wafer 1204 but does not substantially support the weight of the wafer 1204. Support is provided by another mechanism, such as one or more support members (not shown). The support members may be connected to the wafer 1204. Fig.11A The support member 1152 or Fig. 12A The support member 1253 in FIG. 1204 may be the same or similar. Alternatively, the wafer 1204 may be held on its upper surface by a clamping or chuck device. Fig. 12C In the non-contact embodiment shown, the gap 1255 can be small enough so that the exclusion mask 1254 reduces or eliminates film formation in the exclusion area. The necessary or optimal gap distance may vary depending on the specific film formation method selected. By way of example and not limitation, in some embodiments, the distance of the gap 1255 can be between 1-10 μm, between 5-50 μm, between 10-100 μm, between 50 μm-1 mm, or between 500 μm-10 mm. Although the exclusion mask 1254 is depicted as a rigid object, it can also take any form that reduces or prevents the formation of a film at the exclusion area 1213. For example, the exclusion mask 1254 can be a removable film or a treatment applied to the wafer 1204 prior to the backside film formation process in the processing chamber 1200 or 1201. Alternatively or additionally, the exclusion area 1213 can be formed by a post-deposition process (such as an etching process). Fig. 12C The exclusion zone formed by the chamber may have the same Fig.10 and Fig. 12B The same or similar designs as discussed, or they may take any other desired form.

[0124] In addition to the various exclusion zones that may be achieved by the present disclosure, the backside film may also be advantageously made thicker. In comparative embodiments, the film thickness may be limited by the need to ground the wafer by penetration, breakdown, or pin impact. Since the challenge of grounding the wafer through a thick insulating layer can be overcome, the backside film thickness can be increased. In some embodiments of the present disclosure, the wafer may have a backside film having a thickness of, for example, 1-2.2 μm, 2-5 μm, 5-10 μm, or 10-50 μm. The increased thickness can provide additional structural rigidity to prevent the wafer from bending or warping while maintaining stable electrical contact with the conductive surface of the wafer during the wafer grounding process. The increased thickness can also be used to compensate for any loss of rigidity caused by the lack of material in the exclusion zone. Therefore, a thicker backside film can provide additional design flexibility for the exclusion zone, for example, a larger size and position selection.

[0125] Fig.13AA processing chamber 1300 for forming a backside film on a wafer 1304 in a comparative embodiment is shown. The processing chamber 1300 may include a workbench 1350 for holding the wafer 1304 below the processing unit 1360 to expose the backside of the wafer 1304 facing upward to the processing material 1370. The workbench 1450 may be, for example, a susceptor, a burl plate, or other device for supporting the wafer from below. The workbench 1350 includes a support surface for holding the backside of the wafer 1304 facing upward. The comparative embodiment is not designed to form an exclusion zone for grounding the wafer 1304 during a subsequent SEM inspection process or other semiconductor manufacturing process. The workbench 1350 does not substantially block a portion of the backside of the wafer 1304 facing upward. Therefore, substantially the entire backside may be coated with a backside film 1308. The film may be, for example, silicon dioxide, silicon nitride, other oxides, nitrides, carbides, or other suitable film materials for providing structural support, for example, to prevent the wafer from bending or warping.

[0126] The processing chamber 1300 may be configured to perform any film forming process known in the semiconductor manufacturing industry. By way of example and not limitation, the film forming process may include chemical vapor deposition (CVD), plasma enhanced chemical vapor deposition (PECVD), low pressure chemical vapor deposition (LPCVD), high density plasma chemical vapor deposition (HDPCVD), physical vapor deposition (PVD), plasma enhanced physical vapor deposition (PEPVD), atomic layer deposition (ALD), plasma enhanced atomic layer deposition (ALD), sputtering, passivation, or any process for depositing, coating, or growing a backside film on the wafer 1304. In some embodiments, the processing chamber 1300 is a PECVD chamber. The processing unit 1360 may include a showerhead electrode electrically connected to a high frequency power supply (not shown) and configured to introduce a process gas 1370 including a backside film material precursor. The wafer 1304 is connected to a ground electrode (not shown). The electrode and the high frequency power supply ionize the precursor in the process gas 1370 to form a plasma, and some reactants of the plasma are deposited as a backside film 1308.

[0127] Fig. 13B Shown in Fig.13A A back view of a wafer 1304 being processed in a processing chamber. Fig. 13B As shown, the wafer backside film 1308 formed in the process chamber 1300 covers substantially the entire backside of the wafer 1304. There are no film reduction points or exclusion areas.

[0128] Fig.14AA processing chamber 1400 consistent with some embodiments of the present disclosure is shown. The processing chamber 1400 can be similar to the processing chamber 1300, except as described herein. The workstation 1450 includes one or more exclusion masks 1454 configured to cover one or more exclusion areas 1413 (see Fig. 14B ). The exclusion mask 1454 can have a size, shape, and configuration corresponding to any exclusion area disclosed or contemplated herein, including exclusion areas 613, 713, 813, 913, and 1013. For example, the exclusion mask 1454 can have an arc or ring shape provided around the back side of the wafer 1404, or any other shape as needed to create the desired exclusion area. The exclusion mask 1454 can be mounted on the workbench 1450, or can be placed directly on the wafer 1404. The latter is particularly advantageous when forming the exclusion area 1413 at the central area of ​​the wafer 1404. The exclusion mask 1454 can be in contact with the upward-facing back side of the wafer 1404, or it can be a proximity-type exclusion mask separated from the surface by a gap 1455. In the case of Fig.14A In the non-contact embodiment shown, the gap 1455 can be small enough so that the exclusion mask 1454 reduces or eliminates film formation in the exclusion area 1413. The necessary or optimal gap distance can vary depending on the specific film formation method selected. For example, but not limited to this, in some embodiments, the distance of the gap 1455 can be 1-10μm, 5-50μm, 10-100μm, 50μm-1mm or 500μm-10mm. Although the exclusion mask 1454 is depicted as a rigid object, it can also take any form that reduces or prevents the formation of a film at the exclusion area 1413. For example, the exclusion mask 1454 can be a removable film, or other treatment applied to the wafer 1404 before the backside film formation process in the processing chamber 1400. Alternatively or additionally, the exclusion area 1413 can be formed by a post-deposition process (such as an etching process).

[0129] Fig. 14B A wafer 1404 is shown with exclusion regions formed thereon consistent with some embodiments of the present disclosure. The wafer 1404 has a backside film 1408 formed in a process chamber 1400. Since the exclusion mask 1454 is in contact or proximity with the backside of the wafer 1404 during the formation of the backside film 1408, film formation is reduced or eliminated in the exclusion regions 1413. Thus, a thick backside film can be formed while providing exclusion regions 1413 having any desired number, size, shape, location, and orientation.

[0130] Fig.15A method 1500 of forming a backside film with an exclusion zone according to an embodiment of the present disclosure is shown. In step 1502, a wafer is loaded into a processing chamber. The processing chamber can be any suitable processing chamber, such as Fig. 12A , Fig. 12C or Fig.14A In step 1504, an exclusion mask is used to mask areas of the wafer according to the desired exclusion areas as described above. The exclusion mask may be Fig. 12A , Fig. 12C or Fig.14A 1253, 1254 or 1454 in. The exclusion mask can be a removable film as described above or other treatment applied to the wafer. In some embodiments, the step of shielding the wafer occurs simultaneously, before or after the wafer is loaded into the processing chamber. Step 1504 may include selecting the formation position of the exclusion area. It can be predetermined where to form the exclusion area. In some embodiments, the position of the formed exclusion area can be determined. The selection of the formation position of the exclusion area can be based on wafer alignment, scanning mode or characteristics related to the IC features formed on the other side of the wafer. In step 1506, a back film is formed on the wafer according to a film formation process. In step 1508, the wafer is unloaded. In step 1510, the exclusion mask is removed from the wafer to expose the exclusion area in the back film. In some embodiments, the step of unloading the wafer occurs simultaneously, before or after the step of removing the exclusion mask.

[0131] Fig.16 A method 1600 for grounding a wafer held on a wafer holder consistent with an embodiment of the present disclosure is shown. The wafer may have a coating on its surface. The wafer holder may be, for example, Figure 2 The electron beam tool shown, Figure 3 The wafer grounding system shown or Figures 6A-9B A portion of the wafer ground subsystem is shown.

[0132] In step 1602, the location of the exclusion zone of the coating is determined. The location of the exclusion zone can be determined based on information obtained during the determination process or previously known information. The information obtained during the determination process can include, for example, optical or visual inspection information as described above. The information obtained during the determination process can include hardness testing, thickness measurement, or any measurement process that determines a characteristic related to the wafer or the exclusion zone. In some embodiments, the information obtained during the determination process can be based on electrical inspection. For example, the electrical inspection can utilize sensor 316 to detect or measure electrical characteristic 320, as described above with respect to Figure 3The previously known information may include the location, shape, size or type of the exclusion zone provided by the manufacturer or supplier of the wafer. The previously known information may include a wafer map. The previously known information may include information acquired as described above, wherein the acquired information is acquired from different wafers.

[0133] In some embodiments, step 1602 may include, for example, detecting a reference feature and determining a location of the exclusion zone based on a predetermined relationship between the reference feature and the exclusion zone. For example, a pre-alignment detection system may be used to determine the location or orientation of an alignment notch or flat, a wafer edge, a fiducial, or a reference feature in step 1602. Alternatively or additionally, the reference feature may be determined by manual inspection by an operator.

[0134] In some embodiments, step 1602 may include, for example, directly detecting the location of the exclusion zone. For example, the location of the exclusion zone may be determined by optical inspection, a z-height sensor, or other profilometer to identify the exclusion zone 613 by wafer backside topography. The detection may be optical, capacitive, ultrasonic, or any other configuration to achieve the desired detection as described above.

[0135] At step 1604, the position or orientation of the wafer or the first electrical contact is adjusted so that the exclusion zone is aligned with the first electrical contact. The first electrical contact can be a ground pin. The adjustment can be performed before, during, or after the wafer is loaded onto the holder. The position or orientation adjustment can be based on a determined position of the exclusion zone relative to the electrical contact. For example, the wafer can be rotated or translated so that the exclusion zone is positioned above the first electrical contact. Alternatively, the first electrical contact can be actuated so that it is located below the exclusion zone. The adjustment can include a combination of movement of the wafer and the first electrical contact.

[0136] In some embodiments, to improve the positional accuracy of the ground pin in contact with the keep-out region of the wafer, the ground pin may include a pin body having two tips extending from the pin body (a "double-tipped" ground pin). Double-tipped ground pins (e.g., Fig. 20 The double-tipped ground pin 2012, Fig.21 The position of the dual-tip ground pin 2112) can be flexibly adjusted, thereby increasing the chance of the ground pin contacting the exclusion area of ​​the chip.

[0137] In step 1606, the first electrical contact is contacted with the wafer surface. The first electrical contact can be actuated in the height direction so that the first electrical contact establishes sufficient electrical contact with the wafer to achieve biasing or grounding operation. The contact can include any of the following: the exclusion grounding method, the penetration method, the breakdown method, the pin impact method, or any other suitable wafer grounding method or combination of wafer grounding methods of the present disclosure.

[0138] At step 1608, a charged particle beam process is performed while the wafer is biased or grounded. The charged particle beam may include wafer processing (e.g., electron beam direct write lithography system), process monitoring (e.g., critical dimension scanning electron microscope (CD-SEM)), wafer inspection (e.g., electron beam inspection system), defect analysis (e.g., defect inspection SEM, or DR-SEM and focused ion beam system, or FIB), or any other wafer processing operation that is beneficial to controlling the electrical properties of the wafer.

[0139] Fig.17 An exemplary exclusion area 1713 of a wafer is shown with the location of a single pointed ground pin. Exclusion area 1713 may be an area of ​​the wafer without a backside film, thereby providing an area for the ground pin to easily make stable electrical contact with the conductive surface of the wafer. Exclusion area 1713 may have a width 1713w.

[0140] A typical ground pin has a single tip that contacts the wafer or the back film of the wafer. Since the exclusion area of ​​the wafer may be very small, the position accuracy of the single tip ground pin that contacts the exclusion area may be very low. For example, the position 1712a of the single tip ground pin can only be adjusted by half of the width 1713w of the exclusion area 1713. That is, if the single tip ground pin is located at position 1712a, the single tip ground pin (or wafer) can adjust the width 1713bw so that the ground pin is located at position 1712b, or adjust the width 1713cw so that the ground pin is located at position 1712c. Width 1713bw and width 1713cw can each be half of width 1713w. However, the position of the single tip ground pin can only be adjusted to one of position 1712b or position 1712c, but not to both positions at the same time. That is, the position error tolerance of the single tip ground pin may be only half of width 1713w.

[0141] Therefore, if the single tip ground pin is positioned over a coated area (e.g., an area of ​​the wafer having a backside film), the single tip ground pin may not be adjusted such that the single tip ground pin contacts the exclusion area 1713. Therefore, the single tip ground pin may not be able to ground the wafer.

[0142] It is worth noting that although Fig.17 Positions 1712a, 1712b, and 1712c and widths 1713w, 1713bw, and 1713c are shown, but in reality these elements may not actually be included on the wafer.

[0143] Fig.18 A wafer consistent with some embodiments of the present disclosure is shown (e.g., Figure 2 Chip 203, Figure 3 Wafer 304, Figure 4A-4D Crystal Figure 8A-B Chip 804, Figure 9A-9B Chip 904, Fig.10 Wafers (a)-(f) Fig. 12A and Fig. 12C Chip 1204, Fig.14A Chip 1404, Fig. 20 2004) having a dual-tip ground pin location of an exemplary exclusion area 1813 (e.g., Figure 6A-6C Exclusion area 613, Fig.6D The inner exclusion area 613i, Fig.6D The external exclusion zone 613o, Fig. 7A Exclusion area 713, Fig. 8A Exclusion areas 813a-813b, Fig.10 Exclusion area 1013, Fig. 12B Exclusion area 1213, Fig. 14B Exclusion area 1413, Fig. 20 The exclusion area 1813 may have a width 1813w.

[0144] In some embodiments, to improve the positional accuracy of the ground pins in contact with the exclusion zone of the wafer, each ground pin may include a pin body having two tips extending from the pin body (a "double-tipped" ground pin). The distance between the first tip and the second tip of the ground pin may be substantially equal to the width 1813w of the exclusion zone 1813 (e.g., 0.01, 0.1, 0.5, 1, 1.5, 2, 3, or 5 mm or more) to improve the positional accuracy of the ground pins in contact with the exclusion zone 1813 of the wafer. The position 1812a of the double-tipped ground pin may be flexibly adjusted so that the chance of the ground pins in contact with the exclusion zone of the wafer increases (i.e., the double-tipped ground pins may improve the positional accuracy).

[0145] For example, the dual-tipped ground pin may have a first tip at position 1802a and a second tip at position 1802b. The position 1812a of the dual-tipped ground pin may adjust the width 1813a of the exclusion zone 1813 (e.g., linearly adjusted in the x or y direction) (e.g., by adjusting the dual-tipped ground pin, the wafer, or any combination thereof). In some embodiments, the position 1812a of the dual-tipped ground pin or the wafer may be adjusted by rotating the dual-tipped ground pin (e.g., in an angular direction parallel to or perpendicular to the wafer surface). Thus, if the dual-tipped ground pin is at position 1812a, the dual-tipped ground pin may be adjusted by adjusting the width 1813w to position 1812b or adjusting the width 1813w to position 1812c. That is, the position error tolerance of the dual-tipped ground pin may be twice the width 1813.

[0146] Thus, if a dual-tip ground pin is located above a coated area (e.g., an area of ​​a wafer having a backside film), the dual-tip ground pin or the wafer can be adjusted so that at least one tip of the dual-tip ground pin contacts the exclusion area 1813 and grounds the wafer.

[0147] In some embodiments, the width of the exclusion zone can be along the circumference / perimeter of the wafer (i.e., the width can extend in the same direction as the circumference / perimeter of the wafer). In some embodiments, the width of the exclusion zone can extend toward the center of the wafer, or along any direction of the wafer. That is, the direction and orientation of the width of the exclusion zone are not limited.

[0148] It is worth noting that although Fig.18 Positions 1812a, 1812b, 1812c, 1802a, and 1802b and width 1813w are depicted in FIG, but in reality these elements may not actually be included on the wafer.

[0149] Fig.19 A wafer consistent with some embodiments of the present disclosure is shown (e.g., Figure 2 Chip 203, Figure 3 Wafer 304, Figure 4A-4D Chip 404, Figure 6A-6D Chip 604, Figure 7A-7B Chip 704, Figure 8A-B Chip 804, Figure 9A-9B Chip 904, Fig.10 Wafers (a)-(f) Fig. 12A and Fig. 12C Chip 1204, Fig.14A Exemplary exclusion areas 1913 and 1915 of wafer 1404 having locations of dual tip ground pins (e.g., Figure 6A-6C Exclusion area 613, Fig.6D The inner exclusion area 613i, Fig.6D The external exclusion zone 613o, Fig. 7A Exclusion area 713, Fig. 8A Exclusion areas 813a-813b, Fig.10 Exclusion area 1013, Fig. 12B Exclusion area 1213, Fig. 14B Exclusion area 1413).

[0150] In some embodiments, as described above, the distance between the first tip and the second tip of the dual-tip ground pin can be substantially equal to the width of the exclusion zone (e.g., the exclusion zones 1913 and 1915) to improve the position accuracy of the ground pin contacting the exclusion zones 1913 and 1915 of the wafer. The position 1912 of the dual-tip ground pin can be flexibly adjusted so that the chance of the ground pin contacting the exclusion zone of the wafer increases (i.e., the dual-tip ground pin can improve the position accuracy).

[0151] For example, the position 1912 of the dual-tipped ground pin can be adjusted (e.g., linearly adjusted in the x or y direction) by the width of the exclusion zone 1913 (e.g., by adjusting the dual-tipped ground pin, the wafer, or any combination thereof). In some embodiments, the position 1912 of the dual-tipped ground pin or the wafer can be adjusted by rotating the dual-tipped ground pin (e.g., in an angular direction parallel to or perpendicular to the wafer surface). Therefore, if the dual-tipped ground pin is located at position 1912, the dual-tipped ground pin can be adjusted by the width of the exclusion zone 1913 to cover the tolerance zone 1912t, or adjusted by the width of the exclusion zone 1913 to cover the exclusion zone 1913. That is, the position error tolerance of the dual-tipped ground pin can be a width 1913w2, which is twice the width of the exclusion zone 1913.

[0152] Similarly, the position 1914 of the second dual-tipped ground pin can adjust the width of the exclusion zone 1915 (e.g., linearly adjusted in the x or y direction) (e.g., by adjusting the dual-tipped ground pin, the wafer, or any combination thereof). In some embodiments, the position 1914 of the dual-tipped ground pin or the wafer can be adjusted by rotating the dual-tipped ground pin (e.g., in an angular direction parallel or perpendicular to the wafer surface). Therefore, if the dual-tipped ground pin is located at position 1914, the dual-tipped ground pin can adjust the width of the exclusion zone 1915 to cover the tolerance zone 1914t, or adjust the width of the exclusion zone 1915 to cover the exclusion zone 1915. That is, the position error tolerance of the dual-tipped ground pin can be a width 1915w2, which is twice the width of the exclusion zone 1915.

[0153] In some embodiments, the width of the exclusion zone can be along the circumference / perimeter of the wafer (i.e., the width can extend in the same direction as the circumference / perimeter of the wafer). In some embodiments, the width of the exclusion zone can extend toward the center of the wafer, or along any direction of the wafer. That is, the direction and orientation of the width of the exclusion zone are not limited.

[0154] It is worth noting that although Fig.19Positions 1912 and 1914, tolerance areas 1912t and 1914t, and widths 1913w2 and 1915w2 are depicted in FIG, but in reality these elements may not actually be included on the wafer.

[0155] Fig. 20 A backside film 2008 ( FIG. 2008 ) having contacts with dual-tipped ground pins 2012 is shown consistent with some embodiments of the present disclosure. Figure 3 Back film 308, Figure 4A-4D Back film 408, Figures 6A-6C Back film 608, Figure 7B Back film 708, Figure 8B Back film 808, Figures 9A-9B Back film 908, Fig. 12B Back film 1208, Fig. 14B An exemplary wafer 2004 (eg, Figure 2 Chip 203, Figure 3 Wafer 304, Figure 4A-4D Chip 404, Figure 6A-6D Chip 604, FIG. 7A to FIG. 7B Chip 704, FIG. 8A to FIG. 8B Chip 804, FIG. 9A to FIG. 9B Chip 904, Fig.10 Wafers (a)-(f), Figures 12 to Fig. 12C Chip 1204, Fig.14A The dual-tip ground pin 2012 may include a first tip 2012a and a second tip 2012b, each tip extending from a body of the dual-tip ground pin 2012.

[0156] In some embodiments, the wafer 2004 may include an exclusion zone 2013 (e.g., Figure 6A-6C Exclusion area 613, Fig.6D The inner exclusion area 613i, Fig.6D The external exclusion zone 613o, Fig. 7A Exclusion area 713, Fig. 8A Exclusion areas 813a-813b, Fig.10 Exclusion area 1013, Fig. 12B Exclusion area 1213, Fig. 14B Exclusion area 1413).

[0157] In some embodiments, as described above, the distance between the first tip 2012a and the second tip 2012b can be substantially equal to the width of the exclusion zone 2013 (eg, Fig.181813w) to improve the position accuracy of the double-tip ground pin 2012 contacting the exclusion area 2013 of the wafer 2004. The position of the double-tip ground pin 2012 can be flexibly adjusted (for example, Fig.18 Location 1812a, Fig.19 Location 1912, Fig.19 The position 1914 of the dual-tipped ground pin 2012 increases the chance of contacting the exclusion area 2013 of the wafer 2004 (ie, the dual-tipped ground pin can improve the position accuracy).

[0158] For example, Fig. 20 As shown in view (a) of FIG. 2 , the second tip 2012b of the double-tip ground pin 2012 may contact the back film 2008. However, as Fig. 20 As shown in view (b) of FIG. 2004 , the dual-tip ground pin 2012 can be flexibly tilted so that the first tip 2012a of the dual-tip ground pin 2012 can contact the exclusion area 2013, thereby grounding the chip 2004.

[0159] Fig. 20 A single dual-tipped ground pin 2012 is shown in FIG. 2004 , but it should be understood that a plurality of dual-tipped ground pins may be included, each dual-tipped ground pin corresponding to an exclusion area 2013 of the wafer 2004 .

[0160] In some embodiments, the width of the exclusion zone can be along the circumference / perimeter of the wafer (i.e., the width can extend in the same direction as the circumference / perimeter of the wafer). In some embodiments, the width of the exclusion zone can extend toward the center of the wafer, or along any direction of the wafer. That is, the direction and orientation of the width of the exclusion zone are not limited.

[0161] Fig.21 An exemplary dual-tipped ground pin 2112 (eg, Fig. 20 The dual-tip ground pin 2112 may have a first tip 2112a (eg, Fig. 20 The first tip 2012a and the second tip 2112b (eg, Fig. 20 A second tip 2012b), each tip extending from the body of the dual-tipped ground pin 2112.

[0162] Fig. 22 An exemplary wafer holder 2206 (eg, Figure 2 Wafer holder 202, Figure 3 The electrostatic retainer 306, Figure 7A-7B Retainer 706, Figure 8A-B Retainer 806, Figure 9A-9B retainer 906). Fig. 22 As shown in views (a) and (b) of FIG. 2006 , the wafer holder 2206 may include a ground pin 2212, wherein the ground pin 2212 may include a spring structure. The spring structure of the ground pin 2212 may be configured to reduce the back film 2008 ( Figure 3 Back film 308, Figure 4A-4D Back film 408, Figure 6A-6C The back film 608, Figure 7B Back film 708, Figure 8B Back film 808, Figure 9A-9B Back film 908, Fig. 12B Back film 1208, Fig. 14B Back film 1408, Fig. 20 of the wafer 2004) of the wafer 2204 (e.g., Figure 2 Chip 203, Figure 3 Wafer 304, FIG. 4A to FIG. 4D Chip 404, Figures 6A to 6D Chip 604, FIG. 7A to FIG. 7B Chip 704, FIG. 8A to FIG. 8B Chip 804, FIG. 9A to FIG. 9B Chip 904, Fig.10 Wafers (a)-(f) Fig. 12A and Fig. 12C Chip 1204, Fig.14A The force on the wafer 1404) is used to reduce wafer warpage or wafer bending. Fig. 22 As shown in view (b) of FIG. 22, the ground pin 2212 may be located in an exclusion area (eg, Figure 6A-6C Exclusion area 613, Fig.6D The inner exclusion area 613i, Fig.6D The external exclusion zone 613o, Fig. 7A Exclusion area 713, Fig. 8A Exclusion areas 813a-813b, Fig.10 Exclusion area 1013, Fig. 12B Exclusion area 1213, Fig. 14B Exclusion area 1413, Fig. 20 The chip 2204 is contacted at the exclusion area 2013) to ground the chip 2204.

[0163] Fig. 22 A single ground pin 2212 is shown in FIG. 2 , but it should be understood that the wafer holder 2206 may include multiple ground pins, each ground pin corresponding to an exclusion area of ​​the wafer 2204.

[0164] A non-transitory computer readable medium may be provided that stores information for use by a processor (e.g., Figure 1 The processor of the controller 109 performs image processing, data processing, database management, graphic display, operation of a charged particle beam device or another imaging device, controls chip grounding, controls chip grounding position adjustment, implements pin impact method, Figure 15-16 Common forms of non-transitory media include, for example, floppy disks, flexible disks, hard disks, solid-state drives, magnetic tapes or any other magnetic data storage media, CD-ROMs, any other optical data storage media, any physical media with a pattern of holes, RAM, PROM and EPROM, FLASH-EPROM or any other flash memory, NVRAM, caches, registers, any other memory chips or cartridges, and networked versions thereof.

[0165] The block diagram in the figure shows the possible implementation architecture, function and operation of the system, method and computer hardware or software product according to various example embodiments of the present disclosure. In this regard, each box in the flow chart or block diagram can represent a part of a module, segment or code, which includes one or more executable instructions for implementing a specified logical function. It should be understood that in some alternative implementations, the functions indicated in the box may not occur in the order shown in the figure. For example, two boxes displayed in succession can be executed or implemented substantially at the same time, or sometimes two boxes can be executed in reverse order, depending on the functions involved. Some boxes can also be omitted. It should also be understood that each box in the block diagram and the combination of boxes can be implemented by a special hardware system that performs a specified function or action, or by a combination of special hardware and computer instructions.

[0166] The embodiments may also be described using the following terms:

[0167] 1. A method for electrically connecting to a wafer, comprising:

[0168] A first electrical contact is brought into contact with a surface of the wafer having a coating on the surface; wherein the contact occurs at a first exclusion zone of the coating.

[0169] 2. The method according to clause 1, further comprising:

[0170] determining a location of the first exclusion zone; and

[0171] The position of the wafer or the first electrical contact is adjusted so that the first exclusion zone is aligned with the first electrical contact.

[0172] 3. The method of clause 2, wherein adjusting the position of the wafer comprises:

[0173] A wafer holder holding the wafer is translated.

[0174] 4. The method of clause 2, wherein adjusting the position of the wafer comprises:

[0175] The wafer holder holding the wafer is rotated.

[0176] 5. The method of clause 2, wherein adjusting the position of the wafer comprises: unloading the wafer from a first holding position in a wafer holder; and

[0177] The wafer is reloaded to a second holding position on the wafer holder that is different from the first holding position.

[0178] 6. The method of clause 2, wherein adjusting the position of the wafer comprises: unloading the wafer from a first holding orientation in a wafer holder; and

[0179] The wafer is reloaded onto the wafer holder in a second holding orientation different from the first holding orientation.

[0180] 7. The method of clause 2, wherein adjusting the position of the first electrical contact comprises:

[0181] The first electrical contact is actuated.

[0182] 8. The method of clause 1, wherein the coating is a backside film configured to reduce wafer warpage or wafer bowing.

[0183] 9. The method of clause 1, wherein the exclusion zone has a dimension in a radial direction of the surface of at least 1.5 mm.

[0184] 10. The method of clause 1, wherein a size of the exclusion zone is at least twice a size of a cross-sectional contact area between the first electrical contact and the wafer.

[0185] 11. The method of clause 1, wherein the wafer has a first electrical conductivity, the coating has a second electrical conductivity, and the first electrical conductivity is higher than the second electrical conductivity.

[0186] 12. The method of clause 1, wherein the first exclusion zone comprises a void in the coating that exposes an area on the surface of the wafer.

[0187] 13. The method of clause 1, wherein the coating has a first thickness in the first exclusion zone and a second thickness in a zone adjacent to the first exclusion zone, and the second thickness is greater than the first thickness.

[0188] 14. The method of clause 1, wherein the coating has a thickness of at least 1 μm.

[0189] 15. The method of clause 1, wherein the first exclusion zone comprises a first material having a first electrical conductivity, the coating comprises a second material having a second electrical conductivity, and the first electrical conductivity is higher than the second electrical conductivity.

[0190] 16. The method of clause 15, wherein the first material and the second material are substantially coplanar.

[0191] 17. The method according to clause 1, further comprising:

[0192] placing a second electrical contact in contact with the surface of the wafer,

[0193] The first electrical contact and the second electrical contact are in contact with the wafer at the same time.

[0194] 18. The method of clause 17, wherein the second electrical contact contacts the wafer at a second exclusion zone different from the first exclusion zone.

[0195] 19. The method of clause 17, wherein the first exclusion zone comprises a first portion and a second portion, the method further comprising:

[0196] The first electrical contact is brought into contact with the surface at the first portion, and the second electrical contact is brought into contact with the surface at the second portion.

[0197] 20. The method according to 19, wherein the first exclusion zone has an annular shape.

[0198] 21. The method of clause 1, wherein the first exclusion zone has at least one of an annular, arcuate, rectangular, or circular shape.

[0199] 22. The method of clause 1, wherein the surface of the wafer includes a second exclusion zone that is different from the first exclusion zone.

[0200] 23. The method of clause 1, wherein the first exclusion zone is located at a periphery of the surface.

[0201] 24. The method according to clause 1, further comprising:

[0202] separating the first electrical contact from the first exclusion zone; and

[0203] A second electrical contact is placed in contact with the first exclusion zone, wherein the second electrical contact is different from the first electrical contact.

[0204] 25. The method according to clause 1, further comprising:

[0205] subjecting the wafer to a charged particle beam process;

[0206] Wherein the first electrical contact contacts the surface of the wafer during the charged particle beam process.

[0207] 26. The method of clause 25, wherein the charged particle beam process is a scanning electron microscopy inspection of the wafer.

[0208] 27. The method according to clause 1, further comprising:

[0209] The wafer is electrically connected to a bias power source through the first electrical contact.

[0210] 28. The method of clause 1, further comprising supplying a DC voltage to the wafer through the first electrical contact.

[0211] 29. The method of clause 1, further comprising conducting charge away from the wafer through the first electrical contact.

[0212] 30. The method of clause 29, wherein conducting the charge away from the wafer causes the wafer to become electrically neutral.

[0213] 31. A non-transitory computer readable medium storing a set of instructions executable by at least one processor of a device to cause the device to perform a method comprising: contacting a first electrical contact with a surface of a wafer, the wafer having a coating on the surface;

[0214] Wherein said contacting occurs at a first exclusion zone of said coating.

[0215] 32. The non-transitory computer-readable medium of clause 31, wherein the set of instructions executable by the at least one processor of the device causes the device to perform a method, the method further comprising:

[0216] determining a location of the first exclusion zone; and

[0217] The position of the wafer or the first electrical contact is adjusted so that the first exclusion zone is aligned with the first electrical contact.

[0218] 33. The non-transitory computer readable medium of clause 32, wherein adjusting the position of the wafer comprises:

[0219] A wafer holder holding the wafer is translated.

[0220] 34. The non-transitory computer readable medium of clause 32, wherein adjusting the position of the wafer comprises:

[0221] The wafer holder holding the wafer is rotated.

[0222] 35. The non-transitory computer-readable medium of clause 32, wherein adjusting the position of the wafer comprises:

[0223] unloading the wafer from a first holding position in a wafer holder; and

[0224] The wafer is reloaded into a second holding position on the wafer holder that is different from the first holding position.

[0225] 36. The non-transitory computer readable medium of clause 32, wherein adjusting the position of the wafer comprises:

[0226] unloading the wafer from a first holding orientation in a wafer holder; and

[0227] The wafer is reloaded onto the wafer holder in a second holding orientation different from the first holding orientation.

[0228] 37. The non-transitory computer-readable medium of clause 32, wherein adjusting the position of the first electrical contact comprises:

[0229] The first electrical contact is actuated.

[0230] 38. The non-transitory computer readable medium of clause 31, wherein the coating is a backside film configured to reduce wafer warpage or wafer bowing.

[0231] 39. The non-transitory computer-readable medium of clause 31, wherein the exclusion zone has a dimension of at least 1.5 millimeters in a radial direction of the surface.

[0232] 40. The non-transitory computer readable medium of clause 31, wherein a size of the exclusion zone is at least twice a size of a cross-sectional contact area between the first electrical contact and the wafer.

[0233] 41. The non-transitory computer readable medium of clause 31, wherein the wafer has a first electrical conductivity, the coating has a second electrical conductivity, and the first electrical conductivity is higher than the second electrical conductivity.

[0234] 42. The non-transitory computer-readable medium of clause 31, wherein the first exclusion area comprises a void in the coating that exposes an area on the surface of the wafer.

[0235] 43. The non-transitory computer-readable medium of clause 31, wherein the coating has a first thickness within the first exclusion zone and a second thickness within a zone adjacent to the first exclusion zone, and the second thickness is greater than the first thickness.

[0236] 44. The non-transitory computer readable medium of clause 31, wherein the coating has a thickness of at least 1 μm.

[0237] 45. The non-transitory computer-readable medium of clause 31, wherein the first exclusion zone comprises a first material having a first conductivity, the coating comprises a second material having a second conductivity, and the first conductivity is higher than the second conductivity.

[0238] 46. ​​The non-transitory computer-readable medium of clause 45, wherein the first material is substantially coplanar with the second material.

[0239] 47. The non-transitory computer-readable medium of clause 31, wherein the set of instructions executable by at least one processor of the device causes the device to further perform:

[0240] placing a second electrical contact in contact with the surface of the wafer,

[0241] The first electrical contact and the second electrical contact are in contact with the wafer at the same time.

[0242] 48. The non-transitory computer readable medium of clause 47, wherein the second electrical contact contacts the wafer at a second exclusion zone different from the first exclusion zone.

[0243] 49. The non-transitory computer-readable medium of clause 47, wherein the first exclusion zone comprises a first portion and a second portion, the method further comprising:

[0244] The first electrical contact is brought into contact with the surface at the first portion, and the second electrical contact is brought into contact with the surface at the second portion.

[0245] 50. The non-transitory computer-readable medium of clause 49, wherein the first exclusion zone has an annular shape.

[0246] 51. The non-transitory computer-readable medium of clause 31, wherein the first exclusion zone has at least one of an annular, arcuate, rectangular, or circular shape.

[0247] 52. The non-transitory computer readable medium of clause 31, wherein the surface of the wafer comprises a second exclusion zone different from the first exclusion zone.

[0248] 53. The non-transitory computer-readable medium of clause 31, wherein the first exclusion zone is located at a periphery of the surface.

[0249] 54. The non-transitory computer-readable medium of clause 31, wherein the set of instructions executable by at least one processor of the device causes the device to further perform:

[0250] separating the first electrical contact from the first exclusion zone; and

[0251] A second electrical contact is placed in contact with the first exclusion zone, wherein the second electrical contact is different from the first electrical contact.

[0252] 55. The non-transitory computer-readable medium of clause 31, wherein the set of instructions executable by the at least one processor of the device causes the device to further perform:

[0253] performing a charged particle beam process on the wafer;

[0254] Wherein the first electrical contact contacts the surface of the wafer during the charged particle beam process.

[0255] 56. The non-transitory computer readable medium of clause 55, wherein the charged particle beam process is a scanning electron microscopy inspection of the wafer.

[0256] 57. The non-transitory computer-readable medium of clause 31, wherein the set of instructions executable by at least one processor of the device causes the device to further perform:

[0257] The wafer is electrically connected to a bias power source through the first electrical contact.

[0258] 58. The non-transitory computer-readable medium of clause 31, wherein the set of instructions executable by at least one processor of the device causes the device to further perform:

[0259] A DC voltage is supplied to the wafer through the first electrical contact.

[0260] 59. The non-transitory computer-readable medium of clause 31, wherein the set of instructions executable by at least one processor of the device causes the device to further perform:

[0261] Charge is conducted away from the wafer through the first electrical contact.

[0262] 60. The non-transitory computer-readable medium of clause 59, wherein conducting the charge away from the wafer causes the wafer to become electrically neutral.

[0263] 61. A charged particle beam device comprising:

[0264] a wafer holder configured to hold a wafer having a coating on a surface of the wafer; a first electrical contact;

[0265] a charged particle beam source configured to expose the wafer to a charged particle beam; and a controller configured to cause the first electrical contact to contact the surface of the wafer at a first exclusion zone of the coating.

[0266] 62. A charged particle beam apparatus according to clause 61, wherein the controller is further configured to:

[0267] determining a location of the first exclusion zone; and

[0268] The position of the wafer or the first electrical contact is adjusted so that the first exclusion zone is aligned with the first electrical contact.

[0269] 63. The charged particle beam apparatus of clause 62, wherein adjusting the position of the wafer comprises:

[0270] The wafer holder is translated.

[0271] 64. The charged particle beam apparatus of clause 62, wherein adjusting the position of the wafer comprises:

[0272] The wafer holder is rotated.

[0273] 65. The charged particle beam apparatus of clause 62, wherein adjusting the position of the wafer comprises:

[0274] unloading the wafer from a first holding position in the wafer holder; and

[0275] The wafer is reloaded to a second holding position on the wafer holder that is different from the first holding position.

[0276] 66. The charged particle beam apparatus of clause 62, wherein adjusting the position of the wafer comprises:

[0277] unloading the wafer from a first holding orientation in the wafer holder; and

[0278] The wafer is reloaded onto the wafer holder in a second holding orientation different from the first holding orientation.

[0279] 67. The charged particle beam apparatus of clause 62, wherein adjusting the position of the first electrical contact comprises:

[0280] The first electrical contact is actuated.

[0281] 68. The charged particle beam apparatus of clause 61, wherein the coating is a backside film configured to reduce wafer warpage or wafer bowing.

[0282] 69. A charged particle beam apparatus according to clause 61, wherein the dimension of the exclusion zone in a radial direction of the surface is at least 1.5 mm.

[0283] 70. The charged-particle beam apparatus of clause 61, wherein a size of the exclusion zone is at least twice a size of a cross-sectional contact area between the first electrical contact and the wafer.

[0284] 71. A charged particle beam apparatus according to clause 61, wherein the wafer has a first electrical conductivity, the coating has a second electrical conductivity, and the first electrical conductivity is higher than the second electrical conductivity.

[0285] 72. A charged particle beam apparatus according to clause 61, wherein the first exclusion zone comprises a void in the coating exposing an area on the surface of the wafer.

[0286] 73. A charged particle beam device according to clause 61, wherein the coating has a first thickness in the first exclusion region and a second thickness in a region adjacent to the first exclusion region, and the second thickness is greater than the first thickness.

[0287] 74. The charged particle beam device of clause 61, wherein the coating has a thickness of at least 1 μm.

[0288] 75. A charged particle beam device according to clause 61, wherein the first exclusion region comprises a first material having a first conductivity, the coating comprises a second material having a second conductivity, and the first conductivity is higher than the second conductivity.

[0289] 76. A charged particle beam device according to clause 75, wherein the first material is substantially coplanar with the second material.

[0290] 77. The charged particle beam apparatus of clause 61, wherein the controller is further configured to cause a second electrical contact to contact the surface of the wafer; and

[0291] The first electrical contact and the second electrical contact are configured to contact the wafer simultaneously.

[0292] 78. The charged particle beam apparatus of clause 77, wherein the second electrical contact is configured to contact the wafer at a second exclusion zone different from the first exclusion zone.

[0293] 79. A charged particle beam apparatus according to clause 77, wherein:

[0294] The first exclusion zone includes a first portion and a second portion;

[0295] The controller is also configured to:

[0296] The first electrical contact is brought into contact with the surface at the first portion, and the second electrical contact is brought into contact with the surface at the second portion.

[0297] 80. A charged particle beam device according to clause 79, wherein the first exclusion zone has an annular shape.

[0298] 81. A charged particle beam device according to clause 61, wherein the first exclusion zone has at least one of an annular, arc-shaped, rectangular or circular shape.

[0299] 82. The charged particle beam apparatus of clause 61, wherein the surface of the wafer comprises a second exclusion zone that is different from the first exclusion zone.

[0300] 83. A charged particle beam device according to clause 61, wherein the first exclusion zone is located at the periphery of the surface.

[0301] 84. A charged particle beam apparatus according to clause 61, wherein the controller is further configured to:

[0302] separating the first electrical contact from the first exclusion zone; and

[0303] A second electrical contact is placed in contact with the first exclusion zone, wherein the second electrical contact is different from the first electrical contact.

[0304] 85. A charged particle beam apparatus according to clause 61, wherein the controller is further configured to:

[0305] performing a charged particle beam process on the wafer;

[0306] Wherein the first electrical contact contacts the surface of the wafer during the charged particle beam process.

[0307] 86. The charged particle beam apparatus of clause 85, wherein the charged particle beam process is a scanning electron microscopy inspection of the wafer.

[0308] 87. The charged particle beam apparatus of clause 61, further comprising:

[0309] Wafer bias power supply;

[0310] The controller is further configured to electrically connect the wafer to a bias power source through the first electrical contact.

[0311] 88. The charged particle beam apparatus of clause 61, wherein the controller is further configured to supply a DC voltage to the wafer through the first electrical contact.

[0312] 89. The charged particle beam apparatus of clause 61, wherein the first electrical contact is configured to conduct charge away from the wafer.

[0313] 90. The charged particle beam apparatus of clause 89, wherein conducting the charge away from the wafer causes the wafer to become electrically neutral.

[0314] 91. A wafer holding mechanism of a wafer processing system, comprising:

[0315] a wafer holder configured to hold a wafer in a process chamber configured to form a coating on the wafer; and

[0316] A first exclusion mask is configured to cover a first exclusion area of ​​the wafer, wherein the first exclusion mask is configured to reduce or prevent film formation at the first exclusion area during a film formation process in the process chamber.

[0317] 92. A wafer holding mechanism according to clause 91, wherein the first exclusion mask is a support member of the wafer holder, and the support member is configured to support the wafer at the first exclusion area.

[0318] 93. The wafer holding mechanism of clause 92, further comprising a second exclusion mask configured to cover a second exclusion area of ​​the wafer.

[0319] 94. A wafer holding mechanism according to clause 93, wherein the second exclusion mask does not substantially support the wafer.

[0320] 95. The wafer holding mechanism of clause 94, wherein the second exclusion mask is configured to contact the wafer at the second exclusion area without substantially supporting the wafer.

[0321] 96. A wafer holding mechanism according to clause 94, wherein the second exclusion mask is configured to reduce or prevent the formation of a thin film at the second exclusion area without contacting the wafer.

[0322] 97. A wafer holding mechanism according to clause 94, wherein the second exclusion mask comprises a removable film.

[0323] 98. The wafer holding mechanism of clause 91, wherein the first exclusion mask is configured to contact the wafer at the first exclusion area without substantially supporting the wafer.

[0324] 99. The wafer holding mechanism of clause 91, wherein the first exclusion mask is configured to reduce or prevent the formation of a thin film at the first exclusion area without contacting the wafer.

[0325] 100. The wafer holding mechanism of clause 99, wherein the wafer holder comprises a support member configured to support the wafer at an area other than the first exclusion zone.

[0326] 101. A wafer holding mechanism according to clause 91, wherein the first exclusion mask has a shape corresponding to the shape of the first exclusion area.

[0327] 102. A wafer holding mechanism according to clause 91, wherein the wafer holder comprises a table configured to support the wafer from below.

[0328] 103. The wafer holding mechanism of clause 102, wherein the first exclusion mask is configured to cover the first exclusion zone from above the wafer.

[0329] 104. A wafer holding mechanism according to clause 91, wherein the first exclusion mask comprises a removable film.

[0330] 105. The wafer holding mechanism of clause 91, wherein the processing chamber is one of: a chemical vapor deposition chamber, a physical vapor deposition chamber, an atomic layer deposition chamber, and a passivation chamber. 106. A semiconductor wafer comprising:

[0331] coatings on wafer surfaces; and

[0332] A first exclusion zone in the coating is configured to facilitate connection between electrical contacts of a charged particle beam inspection device and the wafer.

[0333] 107. The semiconductor wafer of clause 106, wherein the coating is a backside film configured to reduce wafer warpage or wafer bow.

[0334] 108. A semiconductor wafer according to clause 106, wherein a dimension of the first exclusion zone in a radial direction of the surface is at least 1.5 millimeters.

[0335] 109. The semiconductor wafer of clause 106, wherein a size of the first exclusion zone is at least twice a size of a cross-sectional contact area between the electrical contact and the wafer.

[0336] 110. The semiconductor wafer of clause 106, wherein the wafer has a first electrical conductivity, the coating has a second electrical conductivity, and the first electrical conductivity is higher than the second electrical conductivity.

[0337] 111. The semiconductor wafer of clause 106, wherein the first exclusion zone comprises a void in the coating exposing an area on the surface of the wafer.

[0338] 112. The semiconductor wafer of clause 106, wherein the coating has a first thickness in the first exclusion region and a second thickness in a region adjacent to the first exclusion region, and the second thickness is greater than the first thickness.

[0339] 113. The method of clause 106, wherein the coating has a thickness of at least 1 μm. 114. The semiconductor wafer of clause 106, wherein the first exclusion zone comprises a first material having a first electrical conductivity, the coating comprises a second material having a second electrical conductivity, and the first electrical conductivity is higher than the second electrical conductivity.

[0340] 115. The semiconductor wafer of clause 114, wherein the first material is substantially coplanar with the second material.

[0341] 116. The semiconductor wafer of clause 106, wherein the first exclusion zone has at least one of an annular, arcuate, rectangular, or circular shape.

[0342] 117. The semiconductor wafer of clause 106, wherein the surface of the wafer comprises a second exclusion zone different from the first exclusion zone.

[0343] 118. The semiconductor wafer of clause 106, wherein the first exclusion zone is located at a periphery of the surface.

[0344] 119. A method for forming a coating on a wafer surface, comprising:

[0345] loading a wafer into a processing chamber;

[0346] masking a first exclusion area on the surface of the wafer using a first exclusion mask; and performing a film forming process in the processing chamber;

[0347] Wherein the first exclusion mask reduces or eliminates filming in the first exclusion area.

[0348] 120. The method according to clause 119, further comprising:

[0349] The wafer is held by a wafer holder of the process chamber.

[0350] 121. The method of clause 120, wherein the first exclusion mask is a support member of the wafer holder, the support member being configured to support the wafer at the exclusion area.

[0351] 122. The method according to clause 121, further comprising:

[0352] A second exclusion area on the wafer surface is masked using a second exclusion mask.

[0353] 123. The method of clause 122, wherein the second exclusion mask does not substantially support the wafer.

[0354] 124. The method of clause 122, wherein the second exclusion mask contacts the wafer at the second exclusion area without substantially supporting the wafer.

[0355] 125. The method of clause 122, wherein the second exclusion mask reduces or prevents filming at the second exclusion area without contacting the wafer.

[0356] 126. The method of clause 122, wherein the second exclusion mask comprises a removable film.

[0357] 127. The method of clause 120, wherein the wafer holder comprises a support member configured to support the wafer at areas other than the first exclusion zone.

[0358] 128. The method of clause 120, wherein the wafer holder comprises a table configured to support the wafer from below.

[0359] 129. The method of clause 119, wherein the first exclusion mask is configured to contact the wafer at the first exclusion area without substantially supporting the wafer.

[0360] 130. The method of clause 119, further comprising supporting the wafer by a support member, wherein the support member is configured to support the wafer at areas other than the first exclusion area.

[0361] 131. The method of clause 119, wherein the first exclusion mask is configured to reduce or prevent filming at the first exclusion area without contacting the wafer.

[0362] 132. The method of clause 131, further comprising supporting the wafer by a support member, wherein the support member is configured to support the wafer at areas other than the first exclusion area.

[0363] 133. The method of clause 119, wherein the first exclusion mask has a shape corresponding to a shape of the first exclusion area.

[0364] 134. The method of clause 119, wherein the first exclusion mask is configured to cover the first exclusion area from above the wafer.

[0365] 135. The method of clause 119, wherein the first exclusion mask comprises a removable film.

[0366] 136. The method according to clause 119, wherein the film forming process comprises one of the following: chemical vapor deposition, physical vapor deposition, atomic layer deposition and passivation.

[0367] 137. A non-transitory computer readable medium storing a set of instructions executable by at least one processor of a device to cause the device to perform a method comprising:

[0368] loading a wafer into a processing chamber;

[0369] masking a first exclusion area on the surface of the wafer using a first exclusion mask; and performing a film forming process in the processing chamber;

[0370] The first exclusion mask reduces or eliminates filming in the first exclusion area.

[0371] 138. The non-transitory computer-readable medium of clause 138, wherein the set of instructions executable by at least one processor of the device causes the device to further perform:

[0372] The wafer is held by a wafer holder of the process chamber.

[0373] 139. The non-transitory computer readable medium of clause 138, wherein the first exclusion mask is a support member of the wafer holder, the support member being configured to support the wafer at the first exclusion area.

[0374] 140. The non-transitory computer-readable medium of clause 139, wherein the set of instructions executable by at least one processor of the device causes the device to further perform:

[0375] A second exclusion mask is used to mask a second exclusion area on the wafer surface.

[0376] 141. The non-transitory computer readable medium of clause 140, wherein the second exclusion mask does not substantially support the wafer.

[0377] 142. The non-transitory computer-readable medium of clause 140, wherein the second exclusion mask contacts the wafer at the second exclusion area without substantially supporting the wafer.

[0378] 143. The non-transitory computer-readable medium of clause 140, wherein the second exclusion mask reduces or prevents filming at the second exclusion area without contacting the wafer.

[0379] 144. The non-transitory computer-readable medium of clause 140, wherein the second exclusion mask comprises a removable film.

[0380] 145. The non-transitory computer readable medium of clause 138, wherein the wafer holder comprises a support member configured to support the wafer at an area other than the first exclusion zone.

[0381] 146. The non-transitory computer readable medium of clause 138, wherein the wafer holder comprises a table configured to support the wafer from below.

[0382] 147. The non-transitory computer-readable medium of clause 137, wherein the first exclusion mask is configured to contact the wafer at the first exclusion area without substantially supporting the wafer.

[0383] 148. The non-transitory computer-readable medium of clause 147, wherein the set of instructions executable by at least one processor of the device causes the device to further perform: supporting the wafer by a support member,

[0384] wherein the support member is configured to support the wafer at an area other than the first exclusion area.

[0385] 149. The non-transitory computer-readable medium of clause 137, wherein the first exclusion mask is configured to reduce or prevent filming at the first exclusion area without contacting the wafer.

[0386] 150. The non-transitory computer-readable medium of clause 149, wherein the set of instructions executable by the at least one processor of the device causes the device to further perform: supporting the wafer by a support member,

[0387] wherein the support member is configured to support the wafer at an area other than the first exclusion area.

[0388] 151. A non-transitory computer-readable medium according to clause 137, wherein the first exclusion mask has a shape corresponding to a shape of the first exclusion area.

[0389] 152. The non-transitory computer-readable medium of clause 137, wherein the first exclusion mask is configured to cover the first exclusion area from above the wafer.

[0390] 153. The non-transitory computer-readable medium of clause 137, wherein the first exclusion mask comprises a removable film.

[0391] 154. The non-transitory computer readable medium of clause 137, wherein the film formation process comprises one of: chemical vapor deposition, physical vapor deposition, atomic layer deposition, and passivation.

[0392] 155. The method according to clause 1, further comprising:

[0393] The first electrical contact is caused to contact the surface of the wafer by actuating the first electrical contact in a height direction.

[0394] 156. The method according to clause 1, further comprising:

[0395] The wafer grounding process is performed by one of a pressing method, a punching method, or a pin striking method.

[0396] 157. The method of clause 2, wherein determining the location of the first exclusion zone comprises:

[0397] detecting positions of reference features of the wafer; and

[0398] The position of the first exclusion zone is determined based on the detected position of the reference feature.

[0399] 158. The method of clause 157, wherein the reference feature is one of: an alignment notch, a flat portion of a wafer edge, or a fiducial mark.

[0400] 159. The method of clause 2, wherein determining the location of the first exclusion zone comprises:

[0401] A sensor is used to detect the position of the exclusion zone.

[0402] 160. The method of clause 159, wherein detecting the location comprises any of the following:

[0403] detecting optical properties of the surface of the wafer;

[0404] detecting a capacitive characteristic of the surface of the wafer;

[0405] detecting acoustic properties of the surface of the wafer; or

[0406] The topography of the surface of the wafer is detected.

[0407] 161. The method of clause 2, wherein adjusting the position of the wafer or the first electrical contact comprises actuating one of: a wafer holder, a wafer stage, or a wafer elevator. 162. The method of clause 1, wherein when the first electrical contact contacts the exclusion zone, the exclusion zone has a first dimension in a first direction, the first dimension being no greater than 750 μm greater than a dimension of the first electrical contact in the first direction.

[0408] 163. A method according to clause 162, wherein the exclusion zone has a second dimension in a second direction that is larger than the first dimension, and the second direction is substantially perpendicular to the first direction.

[0409] 164. The non-transitory computer-readable medium of clause 31, wherein the set of instructions executable by at least one processor of the device causes the device to further perform:

[0410] The first electrical contact is caused to contact the surface of the wafer by actuating the first electrical contact in a height direction.

[0411] 165. A non-transitory computer-readable medium as described in clause 31, wherein a set of instructions executable by at least one processor of the device causes the device to also perform a chip grounding process by one of a pressing method, a breakdown method, or a pin-impacting method.

[0412] 166. The non-transitory computer-readable medium of clause 32, wherein determining a location of the first exclusion zone comprises:

[0413] detecting positions of reference features of the wafer; and

[0414] The position of the first exclusion zone is determined based on the detected position of the reference feature.

[0415] 167. The non-transitory computer readable medium of clause 166, wherein the reference feature is one of: an alignment notch, a flat portion of a wafer edge, or a fiducial mark.

[0416] 168. The non-transitory computer-readable medium of clause 32, wherein determining a location of the first exclusion zone comprises:

[0417] A sensor is used to detect the position of the exclusion zone.

[0418] 169. The non-transitory computer-readable medium of clause 168, wherein detecting the location comprises any of:

[0419] detecting optical properties of the surface of the wafer;

[0420] detecting a capacitive characteristic of the surface of the wafer;

[0421] detecting acoustic properties of the surface of the wafer; or

[0422] The topography of the surface of the wafer is detected.

[0423] 170. The non-transitory computer readable medium of clause 32, wherein adjusting the position of the wafer or the first electrical contact comprises actuating one of: a wafer holder, a wafer stage, or a wafer elevator.

[0424] 171. A non-transitory computer readable medium as described in clause 31, wherein when the first electrical contact contacts the exclusion zone, the exclusion zone has a first dimension in a first direction, and the first dimension is no more than 750 μm larger than the dimension of the first electrical contact in the first direction.

[0425] 172. A non-transitory computer-readable medium as described in clause 171, wherein the exclusion zone has a second dimension in a second direction that is larger than the first dimension, and the second direction is substantially perpendicular to the first direction.

[0426] 173. A charged particle beam apparatus according to clause 61, wherein the controller is further configured to cause the first electrical contact to contact the surface of the wafer by actuating the first electrical contact in a height direction.

[0427] 174. A charged particle beam apparatus according to clause 61, wherein the controller is further configured to perform a wafer grounding process by one of a pressing method, a breakdown method, or a pin impact method.

[0428] 175. The charged particle beam apparatus of clause 62, wherein determining the position of the first exclusion zone comprises:

[0429] detecting positions of reference features of the wafer; and

[0430] The position of the first exclusion zone is determined based on the detected position of the reference feature.

[0431] 176. A charged particle beam apparatus according to clause 175, wherein the reference feature is one of: an alignment notch, a flat portion of a wafer edge, or a fiducial mark.

[0432] 177. The charged particle beam apparatus of clause 62, wherein determining the position of the first exclusion zone comprises:

[0433] A sensor is used to detect the position of the exclusion zone.

[0434] 178. A charged particle beam apparatus according to clause 177, wherein detecting the position comprises any of the following:

[0435] detecting optical properties of the surface of the wafer;

[0436] detecting a capacitive characteristic of the surface of the wafer;

[0437] detecting acoustic properties of the surface of the wafer; or

[0438] The topography of the surface of the wafer is detected.

[0439] 179. A charged particle beam apparatus according to clause 62, wherein adjusting the position of the chip or the first electrical contact comprises actuating one of: a chip holder, a chip stage, or a chip elevator.

[0440] 180. A charged particle beam apparatus according to clause 61, wherein when the first electrical contact contacts the exclusion zone, the exclusion zone has a first dimension in a first direction, the first dimension being no more than 750 μm larger than a dimension of the first electrical contact in the first direction.

[0441] 181. A charged particle beam device according to clause 180, wherein the exclusion zone has a second dimension in a second direction that is larger than the first dimension, and the second direction is substantially perpendicular to the first direction.

[0442] 182. A method as described in any of clauses 1 to 30 or 155 to 163, wherein the first electrical contact includes a pin body, a first tip and a second tip, and the first tip and the second tip each extend from the pin body.

[0443] 183. A method according to clause 182, wherein the distance between the first tip and the second tip is substantially equal to the width of the first exclusion zone of the coating.

[0444] 184. The method of clause 183, further comprising adjusting the lead body to contact a surface of the wafer within the width of the first exclusion zone of the coating.

[0445] 185. The method of clause 184, wherein adjusting the pin body comprises any of: adjusting the pin body in a linear direction, adjusting the pin body in an angular direction, or any combination thereof.

[0446] 186. A method according to any one of clauses 1 to 30 or 155 to 163, wherein the first electrical contact comprises a spring within a chip holder.

[0447] 187. A method according to clause 186, wherein the spring is configured to reduce wafer warping or wafer bending.

[0448] 188. A method according to any one of clauses 1 to 30, 155 to 163 or 182 to 187, wherein the first electrical contact comprises a plurality of first electrical contacts and the first exclusion zone comprises a plurality of first exclusion zones, each first electrical contact corresponding to a first exclusion zone.

[0449] 189. A non-transitory computer readable medium as described in any of clauses 31 to 60 or 164 to 172, wherein the first electrical contact includes a pin body, a first tip and a second tip, and the first tip and the second tip each extend from the pin body.

[0450] 190. A non-transitory computer readable medium as described in clause 189, wherein the distance between the first tip and the second tip is substantially equal to the width of the first exclusion zone of the coating.

[0451] 191. A non-transitory computer readable medium as described in claim 190, wherein the set of instructions executable by at least one processor of the device causes the device to also perform adjusting the pin body within the width of the first exclusion zone of the coating to contact the surface of the wafer.

[0452] 192. The non-transitory computer-readable medium of clause 191, wherein adjusting the pin body comprises any of: adjusting the pin body in a linear direction, adjusting the pin body in an angular direction, or any combination thereof.

[0453] 193. A non-transitory computer readable medium as described in any of clauses 31 to 60 or 164 to 172, wherein the first electrical contact comprises a spring within a chip holder.

[0454] 194. The non-transitory computer readable medium of clause 193, wherein the spring is configured to reduce wafer warpage or wafer bowing.

[0455] 195. A non-transitory computer readable medium as described in any of clauses 31 to 60, 164 to 172, or 189 to 194, wherein the first electrical contact comprises a plurality of first electrical contacts and the first exclusion zone comprises a plurality of first exclusion zones, each first electrical contact corresponding to a first exclusion zone.

[0456] 196. A charged particle beam device according to any one of clauses 61 to 90 or 173 to 181, wherein the first electrical contact comprises a pin body, a first tip and a second tip, the first tip and the second tip each extending from the pin body.

[0457] 197. A charged particle beam device according to clause 196, wherein the distance between the first tip and the second tip is substantially equal to the width of the first exclusion zone of the coating.

[0458] 198. A charged particle beam apparatus according to clause 197, wherein the controller is further configured to adjust the pin body to contact the surface of the wafer within the width of the first exclusion zone of the coating.

[0459] 199. A charged particle beam device according to clause 198, wherein adjusting the pin body comprises any of the following: adjusting the pin body in a linear direction, adjusting the pin body in an angular direction, or any combination thereof.

[0460] 200. A charged particle beam device according to any of clauses 61 to 90 or 173 to 181, wherein the first electrical contact comprises a spring within a wafer holder.

[0461] 201. A charged particle beam apparatus according to clause 200, wherein the spring is configured to reduce wafer warpage or wafer bowing.

[0462] 202. A charged particle beam device according to clauses 61 to 90, 173 to 181, or 196 to 201, wherein the first electrical contact comprises a plurality of first electrical contacts and the first exclusion zone comprises a plurality of first exclusion zones, each first electrical contact corresponding to a first exclusion zone.

[0463] 203. According to the chip holding mechanism according to any one of clauses 91 to 105, the chip holder also includes a spring configured to contact the first exclusion zone of the chip.

[0464] 204. A wafer holding mechanism according to clause 203, wherein the spring is configured to reduce wafer warping or wafer bending.

[0465] 205. A semiconductor wafer as described in any of clauses 106 to 118, wherein the electrical contact includes a lead body, a first tip and a second tip, the first tip and the second tip each extending from the lead body.

[0466] 206. A semiconductor wafer as described in clause 205, wherein a distance between the first tip and the second tip is substantially equal to a width of the first exclusion zone of the coating.

[0467] 207. The semiconductor wafer of clause 206, wherein the controller is further configured to adjust the lead body to contact the surface of the wafer within the width of the first exclusion zone of the coating.

[0468] 208. The semiconductor wafer of clause 207, wherein adjusting the pin body comprises any one of: adjusting the pin body in a linear direction, adjusting the pin body in an angular direction, or any combination thereof.

[0469] 209. A semiconductor chip according to any of clauses 106 to 118, wherein the electrical contact comprises a spring within a chip holder.

[0470] 210. The semiconductor wafer of clause 209, wherein the spring is configured to reduce wafer warpage or wafer bowing.

[0471] 211. A semiconductor wafer as described in any of clauses 106 to 118 or 205 to 210, wherein the electrical contact comprises a plurality of electrical contacts and the first exclusion zone comprises a plurality of first exclusion zones, each electrical contact corresponding to a first exclusion zone.

[0472] 212. A method for electrically connecting to a wafer, comprising:

[0473] The lead body is brought into contact with the surface of the wafer,

[0474] The wafer has a coating on the surface, and

[0475] The pin body includes a first tip and a second tip extending from the pin body, respectively; wherein the contact occurs at a first exclusion area of ​​the coating by any one of the first tip, the second tip, or any combination thereof.

[0476] 213. A non-transitory computer readable medium storing a set of instructions executable by at least one processor of a device to cause the device to perform a method comprising:

[0477] The lead body is brought into contact with the surface of the wafer,

[0478] The wafer has a coating on the surface, and

[0479] The pin body includes a first tip and a second tip extending from the pin body, respectively; wherein the contact occurs at a first exclusion area of ​​the coating by the first tip, the second tip, or any combination thereof.

[0480] 214. A charged particle beam device, comprising:

[0481] a wafer holder configured to hold a wafer having a coating on a surface of the wafer;

[0482] a pin body, the pin body comprising a first tip and a second tip each extending from the pin body;

[0483] a charged particle beam source configured to expose the wafer to a charged particle beam; and a controller configured to contact any of the first tip, the second tip, or any combination thereof to the surface of the wafer at a first exclusion zone of the coating.

[0484] 215. A semiconductor wafer comprising:

[0485] coatings on wafer surfaces; and

[0486] A first exclusion zone in the coating is configured to facilitate connection between the wafer and any one of a first tip extending from the lead body, a second tip extending from the lead body, or any combination thereof of a charged particle beam inspection device.

[0487] It should be understood that the embodiments of the present disclosure are not limited to the exact constructions described above and shown in the drawings, and various modifications and changes may be made without departing from the scope thereof.

Claims

1. A charged particle beam device, comprising: a wafer holder configured to hold a wafer having a coating on a surface of the wafer; a first electrical contact; a charged particle beam source configured to expose the wafer to a charged particle beam; as well as A controller is configured to cause the first electrical contact to contact the surface of the wafer at a first exclusion area of ​​the coating.

2. The charged particle beam apparatus according to claim 1, wherein the controller is further configured to: determining a location of the first exclusion zone; and The position of the wafer or the first electrical contact is adjusted so that the first exclusion zone is aligned with the first electrical contact.

3. The charged particle beam apparatus according to claim 2, wherein determining the position of the first exclusion zone comprises: detecting a position of a reference feature of the wafer; as well as The position of the first exclusion zone is determined based on the detected position of the reference feature. The charged particle beam apparatus according to claim 1 , wherein the exclusion zone has a dimension of at least 1.5 mm in a radial direction of the surface. 5 . The charged particle beam device according to claim 1 , wherein the wafer has a first electrical conductivity, the coating has a second electrical conductivity, and the first electrical conductivity is higher than the second electrical conductivity. 6 . The charged particle beam apparatus of claim 1 , wherein the first exclusion zone comprises a void in the coating, the void exposing an area on the surface of the wafer. 7 . The charged particle beam device according to claim 1 , wherein the coating has a first thickness in the first exclusion region and a second thickness in a region adjacent to the first exclusion region, and the second thickness is greater than the first thickness.

8. The charged particle beam device of claim 1, wherein the coating has a thickness of at least 1 μm. 9 . The charged particle beam device of claim 1 , wherein the first exclusion zone comprises a first material having a first conductivity, the coating comprises a second material having a second conductivity, and the first conductivity is higher than the second conductivity.

10. The charged particle beam device according to claim 1, wherein The controller is further configured to cause a second electrical contact to contact the surface of the wafer; and The first electrical contact and the second electrical contact are configured to contact the wafer simultaneously. 11 . The charged particle beam apparatus according to claim 1 , wherein the first exclusion zone has at least one of the following shapes: annular, arcuate, rectangular or circular.

12. The charged particle beam apparatus according to claim 1, wherein the controller is further configured to: performing a charged particle beam process on the wafer; Wherein the first electrical contact contacts the surface of the wafer during the charged particle beam process.

13. The charged particle beam apparatus according to claim 1, further comprising: Wafer bias power supply; The controller is further configured to electrically connect the wafer to a bias power source via the first electrical contact.

14. A non-transitory computer-readable medium storing a set of instructions executable by at least one processor of a device to cause the device to perform a method comprising: contacting a first electrical contact with a surface of the wafer, the wafer having a coating on the surface; Wherein said contacting occurs at a first exclusion zone of said coating.

15. A method for forming a coating on a wafer surface, comprising: loading a wafer into a processing chamber; masking a first exclusion area on the surface of the wafer with a first exclusion mask; as well as performing a film forming process in the processing chamber; Wherein the first exclusion mask reduces or eliminates film formation in the first exclusion area.

Citation Information

Patent Citations

  • Method, apparatus, and system for wafer grounding

    WO2021037827A1