Thin-wall sheet metal part composite forming machining process and forming die
By preparing annular cylindrical parts in the thin-wall sheet metal forming process and forming reinforcement ribs and flange holes on their side walls, combined with the deformation force of the forming mold, the deformation and plane difference of thin-wall sheet metal parts are solved. Problem, improving processing efficiency and finished product quality.
Patent Information
- Application Number
- CN202411300360.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-18
- Publication Date
- 2024-11-15
AI Technical Summary
The existing thin-wall sheet metal forming process has problems such as poor planarity at both ends, pulling deformation of reinforcement ribs and flange profiles, and low processing efficiency, which affects the cooling effect of engine combustion chamber components and the ablation of flame cylinder test drive.
A thin-wall sheet metal composite forming processing technology is adopted, including preparing annular cylindrical parts, forming multiple reinforcement ribs at the side wall design position, processing to form flanges and flange holes, and applying deformation force through the mold , ensure the mutual position accuracy of the reinforcement ribs and the circularity of the cylinder.
The position accuracy and forming quality of the reinforcement ribs are improved, the axial and circumferential deformation caused by reinforcement ribs is solved, processing efficiency is improved, rework and trial operation are reduced, and the delivery quality and progress of components are improved.
Smart Images

Figure CN118950840A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of aerospace engine parts manufacturing, and in particular to a composite forming process and a forming die for thin-walled sheet metal parts. Background Art
[0002] like Figure 1 As shown, the matching parts of the combustion chamber casing are thin-walled sheet metal parts with multiple composite surfaces. This thin-walled sheet metal part 1 includes a straight cylindrical surface of the cylinder, right-angle flanges 12 at both ends of the cylinder, multiple reinforcing ribs 11, and multiple flanging holes 13, which constitute a composite forming process of cylinder bulging, flange rolling forming, reinforcing rib deep drawing forming, and hole flanging forming. The existing forming process flow is rounding, turning both ends, flange forming at both ends, processing flanging bottom holes, hole flanging forming, reinforcing rib forming, and rounding; the parts processed by this processing process have poor flatness at both ends, the reinforcing ribs and the flange surfaces at both ends are pulled and deformed, multiple clamp repairs are required for correction, the surface quality is poor, and the processing efficiency is low. The hole flanging size and the quality of the formed surface of this sheet metal part on this component directly affect the cooling effect of the engine combustion chamber components, and are one of the important factors affecting whether the flame tube is ablated during the test run. It is particularly important to control the forming size and surface integrity of this sheet metal part. The solution to this problem improves the delivery quality and progress of the components while reducing the test run repair of the engine. Summary of the invention
[0003] In view of this, the present application provides a composite forming processing technology and a forming mold for thin-walled sheet metal parts, which solves the problems of poor flatness, excessive size of reinforcing ribs and flanging holes, and improves product quality and processing efficiency.
[0004] On the one hand, the present application provides a thin-walled sheet metal composite forming process using the following technical solutions:
[0005] A thin-walled sheet metal composite forming process comprises the following steps:
[0006] Step 1, preparing an annular cylindrical part that meets the size of the thin-walled sheet metal part, and correcting the roundness of the annular cylindrical part;
[0007] Step 2, forming a plurality of protruding reinforcing ribs at the designed positions of the side wall of the annular cylinder part by extrusion, wherein the length direction of the reinforcing ribs is arranged along the axial direction of the annular cylinder, and the plurality of the reinforcing ribs are distributed at intervals;
[0008] Step 3, forming flanges at both ends of the annular cylinder part processed in step 2;
[0009] Step 4, forming a flanging hole at a designed position of the side wall of the annular cylinder part processed in step 3;
[0010] Step 5, correcting the roundness of the annular cylinder part processed in step 4.
[0011] Optionally, in step 2, multiple reinforcing ribs on the annular cylinder part are formed at one time.
[0012] Optionally, step 4 specifically includes:
[0013] A flange bottom hole is processed at the designed position of the side wall of the annular cylinder part processed in step 3, and the flange bottom hole is flanged to form a final flange hole.
[0014] On the other hand, the present application provides a molding die adopting the following technical solution:
[0015] A forming die, used for processing and forming a plurality of reinforcing ribs on the annular cylinder part in the above step 2;
[0016] The forming mold clamps and fits the side wall of the annular cylinder, and the forming mold simultaneously applies a deformation force to the designed positions of all the reinforcing ribs on the side wall of the annular cylinder to form a plurality of reinforcing ribs at the same time.
[0017] Optionally, the molding die comprises:
[0018] A base, for mounting on the platform of a hydraulic press;
[0019] A truncated cone, mounted on the base;
[0020] An annular top plate is placed on the base, and the annular top plate is sleeved on the outer periphery of the truncated cone;
[0021] An inner mold sleeve is used to be sleeved on the outer periphery of the circumferential side wall of the truncated cone, and the bottom of the inner mold sleeve is in contact with the top surface of the annular top plate. The inner wall surface of the inner mold sleeve is a conical profile, and the conical profile matches the outer periphery of the truncated cone. The outer wall surface of the inner mold sleeve is used to match the inner wall of the annular cylinder part, and a protrusion structure matching the inner wall surface of each reinforcing rib is provided on the outer wall surface of the inner mold sleeve. The inner mold sleeve includes a plurality of first petal structures distributed along the circumferential direction. When the outer diameter of the inner mold sleeve is in contact with the inner wall of the annular cylinder part, there are gaps between the plurality of first petal structures.
[0022] An outer mold sleeve is sleeved on the outer periphery of the outer mold sleeve, and the bottom of the outer mold sleeve abuts against the top surface of the annular top plate, the inner wall surface of the outer mold sleeve is used to match the outer wall surface of the annular cylinder part, and the inner wall surface of the outer mold sleeve is provided with a groove structure matching the outer wall surface of each reinforcing rib;
[0023] A pressing plate, used to be connected to the telescopic rod of the hydraulic press, and the pressing plate is used to apply downward pressure to the inner mold sleeve and the outer mold sleeve;
[0024] Among them, a cavity for accommodating annular cylindrical parts and forming reinforcing ribs is formed between the inner mold sleeve and the outer mold sleeve. When the annular top plate is lifted up, the inner mold sleeve moves toward the small diameter end of the cone, and several of the first petal structures approach each other to make the annular cylindrical parts sleeved on the outer periphery of the raised structure. When the pressure plate presses the inner mold sleeve and the outer mold sleeve until the annular top plate abuts the base, the inner mold sleeve approaches the large diameter end of the cone, and several of the first petal structures move away from each other. The raised structure applies an outward force to the designed position of the reinforcing ribs of the annular cylindrical parts and cooperates with the groove structure on the outer mold sleeve to form reinforcing ribs.
[0025] Optionally, a receiving groove is provided on the end surface where the plurality of first petal structures are connected, and an elastic structure connecting two adjacent first petal structures is provided in the receiving groove, and the elastic structure is used to exert a force on the plurality of first petal structures to move closer to each other.
[0026] Optionally, the outer mold sleeve includes a plurality of second petal structures distributed along the circumferential direction, and when the inner wall of the outer mold sleeve is in contact with the outer wall of the annular cylinder part, the plurality of second petal structures form a continuous annular structure, and the second petal structures are movably arranged relative to the base. The molding mold also includes a limiting assembly, and the limiting assembly is used to apply a force to the second petal structures to move closer together when the reinforcement ribs are formed so that the plurality of second petal structures form a continuous annular structure.
[0027] Optionally, the limiting assembly includes a limiting plate fixedly connected to the pressure plate, and the limiting plate is correspondingly provided on the outer side of each second petal structure, and when the limiting plate abuts against the outer wall of the second petal structure, the second petal structure forms a continuous annular structure;
[0028] Wherein, when the pressing plate is pressed downward, the second petal structure forms a continuous annular structure before the lower pressing plate contacts the inner mold sleeve, and an inclined transition surface is provided on the top outer edge of the second petal structure of the lower pressing plate and / or the bottom inner edge of the limiting plate, and the inclined transition surface gradually decreases from bottom to top.
[0029] Optionally, a connecting plate corresponding to each of the second petal structures is provided on the annular top plate, and the connecting plate is located at the outer periphery of the second petal structure. A pull rod is fixedly connected to the side wall of the second petal structure facing the connecting plate, and a through hole is provided on the connecting plate for the pull rod to slide. A spring is sleeved on the outer periphery of the pull rod on the side of the connecting plate facing away from the second petal structure, and one end of the spring away from the second petal structure is fixedly connected to the pull rod. When the second petal structure fits the outer wall of the annular cylinder part, there is a gap between the second petal structure and the connecting plate, and the spring is in a compressed state.
[0030] In summary, this application includes the following beneficial technical effects:
[0031] The multiple reinforcing ribs of the present application are formed at one time, which ensures the relative position accuracy of the reinforcing ribs; the device for forming multiple reinforcing ribs at one time and correcting the cylinder meets the roundness requirement of the cylinder after the multiple reinforcing ribs are formed; the process of the present application is to first form the reinforcing ribs and then form the flanges and flanging holes at both ends, which solves the deformation of the formed structure in the axial and circumferential directions caused by the flow of the reinforcing rib forming material, thereby improving the processing efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0033] Figure 1 This is a schematic structural diagram of a thin-walled sheet metal part according to an embodiment of the present application;
[0034] Figure 2 This is a schematic diagram of the overall structure of the molding die for this application;
[0035] Figure 3 This is a schematic diagram of the structure of the inner mold sleeve and the outer mold sleeve of this application;
[0036] Figure 4 This is a schematic diagram of the structure of the inner mold sleeve moving closer and the outer mold sleeve expanding in this application;
[0037] Figure 5 This is a schematic diagram of the structure of the forming mold when forming the reinforcement ribs in this application.
[0038] Explanation of the reference numerals in the accompanying drawings: 1. annular cylinder part; 11. reinforcing rib; 12. flange; 13. flanging hole; 2. base; 3. frustum; 4. annular top plate; 5. inner mold sleeve; 51. first petal structure; 52. receiving groove; 53. protrusion structure; 6. outer mold sleeve; 61. second petal structure; 62. limit plate; 63. inclined transition surface; 64. connecting plate; 65. pull rod; 66. spring; 67. groove structure; 7. pressure plate. DETAILED DESCRIPTION
[0039] The embodiments of the present application are described in detail below with reference to the accompanying drawings.
[0040] The following describes the implementation methods of the present application through specific examples, and those skilled in the art can easily understand other advantages and effects of the present application from the contents disclosed in this specification. Obviously, the described embodiments are only a part of the embodiments of the present application, rather than all the embodiments. The present application can also be implemented or applied through other different specific implementation methods, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present application. It should be noted that, in the absence of conflict, the following embodiments and the features in the embodiments can be combined with each other. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without making creative work belong to the scope of protection of the present application.
[0041] It should be noted that various aspects of the embodiments within the scope of the appended claims are described below. It should be apparent that the aspects described herein can be embodied in a wide variety of forms, and any specific structure and / or function described herein is merely illustrative. Based on the present application, it should be understood by those skilled in the art that an aspect described herein can be implemented independently of any other aspect, and two or more of these aspects can be combined in various ways. For example, any number of aspects described herein can be used to implement the device and / or practice the method. In addition, other structures and / or functionalities other than one or more of the aspects described herein can be used to implement this device and / or practice this method.
[0042] It should also be noted that the illustrations provided in the following embodiments are only schematic illustrations of the basic concept of the present application. The illustrations only show the components related to the present application rather than being drawn according to the number, shape and size of the components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed at will, and the component layout may also be more complicated.
[0043] Additionally, in the following description, specific details are provided to facilitate a thorough understanding of the examples. However, it will be understood by those skilled in the art that the aspects described may be practiced without these specific details.
[0044] The embodiment of the present application provides a composite forming process for thin-walled sheet metal parts.
[0045] The composite forming process of thin-walled sheet metal parts includes the following steps:
[0046] Step 1: prepare an annular cylindrical part that meets the size of the thin-walled sheet metal part and correct the roundness of the annular cylindrical part.
[0047] Step 2, forming a plurality of protruding reinforcing ribs at the designed positions of the side wall of the annular cylinder part by extrusion, wherein the length direction of the reinforcing ribs is arranged along the axial direction of the annular cylinder, and the plurality of the reinforcing ribs are distributed at intervals.
[0048] Step 3, forming flanges at both ends of the annular cylinder part processed in step 2.
[0049] Step 4, forming a flanging hole at the designed position of the side wall of the annular cylinder part processed in step 3.
[0050] Step 5, correcting the roundness of the annular cylinder part processed in step 4.
[0051] In the step 2, the plurality of reinforcing ribs on the annular cylinder part are formed at one time.
[0052] The step 4 specifically includes:
[0053] A flange bottom hole is processed at the designed position of the side wall of the annular cylinder part processed in step 3, and the flange bottom hole is flanged to form a final flange hole.
[0054] In the prior art, the reinforcing ribs are formed individually, resulting in serious ovality of the entire annular cylinder. Before the improvement, the process is to form the reinforcing ribs after the flanges and the flanging holes are formed. The forming of the reinforcing ribs causes the flanges and the flanging holes formed at both ends to deform axially and circumferentially due to material flow. The closer the reinforcing ribs are to the formed parts, the more serious the deformation.
[0055] The multiple reinforcing ribs of the present application are formed at one time, which ensures the relative position accuracy of the reinforcing ribs; the device for forming multiple reinforcing ribs at one time and correcting the cylinder meets the roundness requirement of the cylinder after the multiple reinforcing ribs are formed; the process of the present application is to first form the reinforcing ribs and then form the flanges and flanging holes at both ends, which solves the deformation of the formed structure in the axial and circumferential directions caused by the flow of the reinforcing rib forming material, thereby improving the processing efficiency.
[0056] In one embodiment, a composite forming process for thin-walled sheet metal parts from sheet material to final inspection
[0057] The process is as follows: plate blanking, bending, welding, heat treatment, rounding, turning both ends, forming ribs, forming flanges at both ends, processing bottom holes for flanging, forming holes, rounding, turning outer circles, coloring inspection, clamp processing and final inspection. Among them, plate blanking, bending, welding, heat treatment, rounding, turning both ends are step 1, forming ribs is step 2, forming flanges at both ends is step 3, processing bottom holes for flanging and forming holes is step 4.
[0058] The parts using the above forming scheme and device are 100% crack-free through fluorescent inspection, and the forming dimensions and flatness at both ends meet the design requirements, reducing rework and improving quality and processing efficiency, solving the difficult problems of forming deformation and excessive flatness at both ends of such composite formed thin-walled sheet metal parts.
[0059] The embodiment of the present application also discloses a forming mold.
[0060] A forming die is used for processing and forming a plurality of reinforcing ribs on the annular cylinder part in step 2.
[0061] The forming die clamps and fits the side wall of the annular cylinder, and the forming die simultaneously applies deformation force to the design positions of all the reinforcing ribs on the side wall of the annular cylinder to form multiple reinforcing ribs at the same time. During the reinforcing rib forming process, the forming die clamps and fits the side wall of the annular cylinder except the design positions of the reinforcing ribs, so that the device for forming multiple reinforcing ribs at one time and correcting the cylinder meets the roundness requirements of the cylinder after the multiple reinforcing ribs are formed.
[0062] Specifically, Figure 2-Figure 5 As shown, the molding die includes:
[0063] The base 2 is used to be installed on the platform of the hydraulic press; the truncated cone 3 is installed on the base 2, and the truncated cone 3 is small at the top and large at the bottom; the annular top plate 4 is placed on the base 2, and the annular top plate 4 is ring-shaped on the outer circumference of the truncated cone 3. An opening is provided on the base 2, and the lifting rod on the hydraulic press passes through it to apply an upward force to the annular top plate 4.
[0064] The inner mold sleeve 5 is used to be sleeved on the outer periphery of the circumferential side wall of the frustum 3, and the bottom of the inner mold sleeve 5 is in contact with the top surface of the annular top plate 4. The inner wall surface of the inner mold sleeve 5 is a conical surface, and the conical surface matches the outer periphery of the frustum 3. The outer wall surface of the inner mold sleeve 5 is used to match the inner wall of the annular cylinder part 1, and a protrusion structure 53 matching the inner wall surface of each reinforcing rib 11 is provided on the outer wall surface of the inner mold sleeve 5. The inner mold sleeve 5 includes a plurality of first petal structures 51 distributed along the circumferential direction. When the outer diameter of the inner mold sleeve 5 fits the inner wall of the annular cylinder part 1, there are gaps between the plurality of first petal structures 51.
[0065] The outer mold sleeve 6 is sleeved on the outer periphery of the outer mold sleeve 6, and the bottom of the outer mold sleeve 6 abuts against the top surface of the annular top plate 4, the inner wall surface of the outer mold sleeve 6 is used to match the outer wall surface of the annular cylinder part 1, and the inner wall surface of the outer mold sleeve 6 is provided with a groove structure 67 that matches the outer wall surface of each reinforcing rib 11.
[0066] The pressing plate 7 is used to be connected to the telescopic rod of the hydraulic press, and the pressing plate 7 is used to apply downward pressure to the inner mold sleeve 5 and the outer mold sleeve 6.
[0067] Among them, a cavity for accommodating the annular cylindrical part 1 and the forming of the reinforcing rib 11 is formed between the inner mold sleeve 5 and the outer mold sleeve 6. When the annular top plate 4 is lifted up, the inner mold sleeve 5 moves toward the small diameter end of the frustum 3, and several of the first petal structures 51 approach each other to make the annular cylindrical part 1 be sleeved on the outer periphery of the raised structure 53. When the pressure plate 7 presses the inner mold sleeve 5 and the outer mold sleeve 6 until the annular top plate 4 abuts the base 2, the inner mold sleeve 5 approaches the large diameter end of the frustum 3, and several of the first petal structures 51 move away from each other. The raised structure 53 applies an outward force to the designed position of the reinforcing rib 11 of the annular cylindrical part 1 and cooperates with the groove structure 67 on the outer mold sleeve 6 to form the reinforcing rib 11.
[0068] The forming process of the reinforcing rib 11 is as follows: Figure 4 As shown, the pressing plate 7 is lifted away from the inner die sleeve 5 and the outer die sleeve 6, and the hydraulic press lifts up the annular top plate 4, which drives the inner die sleeve 5 and the outer die sleeve 6 to move toward the small diameter end of the truncated cone 3, controlling the first petal structure 51 of the inner die sleeve 5 to move closer to each other, and the space between the inner die sleeve 5 and the outer die sleeve 6 is expanded, and the convex structure 53 of the inner die sleeve 5 encloses a range smaller than the inner diameter of the annular cylinder part 1, so that the annular cylinder part 1 can be sleeved on the outer periphery of the inner die sleeve 5, and the annular cylinder is placed between the inner die sleeve 5 and the outer die sleeve 6; Figure 5 As shown, the control pressure plate 7 and the annular top plate 4 are lowered, and the pressure plate 7 applies downward pressure to the inner mold sleeve 5 and the outer mold sleeve 6, and the inner mold sleeve 5 and the outer mold sleeve 6 move downward. At the large diameter end of the inner mold sleeve 5 close to the frustum 3, a plurality of first petal structures 51 gradually expand outward until the non-raised structure 53 portion of the first petal structure 51 fits with the inner wall of the annular cylinder part 1 and the inner wall of the outer mold sleeve 6 fits with the outer wall of the annular cylinder part 1. At the same time, the raised structure 53 exerts an outward force on the inner wall of the annular cylinder structure, and cooperates with the groove structure 67 on the outer mold sleeve 6 to form a reinforcing rib 11.
[0069] An accommodation groove 52 is provided on the end surface where a plurality of the first petal structures 51 are connected. An elastic structure is provided in the accommodation groove 52 to connect two adjacent first petal structures 51. The elastic structure is used to apply a force to bring the plurality of first petal structures 51 closer to each other. Under the action of the elastic structure, when the inner mold sleeve 5 moves toward the small diameter end of the truncated cone 3, all the first petal structures 51 automatically move closer to each other. The elastic structure can be a spring.
[0070] The outer mold sleeve 6 includes a plurality of second petal structures 61 distributed along the circumferential direction. When the inner wall of the outer mold sleeve 6 is in contact with the outer wall of the annular cylinder part 1, the plurality of second petal structures 61 form a continuous annular structure. The second petal structures 61 are movably arranged relative to the base 2. The molding mold also includes a limiting component. The limiting component is used to apply a force to the second petal structures 61 to move closer to each other when the reinforcing ribs 11 are formed so that the plurality of second petal structures 61 form a continuous annular structure. When the inner mold sleeve 5 and the outer mold sleeve 6 are close to the small diameter end of the frustum 3, the second petal structures 61 are moved away from each other, and the distance between the first petal structure 51 and the second petal structure 61 is enlarged, making it more convenient to place the annular cylinder part 1, and then the limiting component applies a force to the second petal structures 61 to move closer to each other when the reinforcing rib 11 is formed so that a plurality of the second petal structures 61 form a continuous annular structure, ensuring that the inner wall of the outer mold sleeve 6 matches the design surface of the outer wall of the annular cylinder structure when the reinforcing rib 11 is formed, so that the inner mold sleeve 5 and the outer mold sleeve 6 can clamp and fit the inner and outer walls of the annular cylinder when the reinforcing rib 11 is formed, thereby ensuring the roundness of the annular cylinder part 1.
[0071] The limiting assembly includes a limiting plate 62 fixedly connected to the pressure plate 7, and the outer side of each second petal structure 61 is correspondingly provided with the limiting plate 62. When the limiting plate 62 and the outer wall of the second petal structure 61 are in contact, the second petal structure 61 forms a continuous annular structure; wherein, when the pressure plate 7 is pressed down, the second petal structure 61 forms a continuous annular structure before the lower pressure plate 7 contacts the inner mold sleeve 5, and an inclined transition profile 63 is provided on the top outer edge of the second petal structure 61 and / or the bottom inner edge of the limiting plate 62 of the lower pressure plate 7, and the inclined transition profile 63 gradually decreases from bottom to top. In the embodiment of the present application, the inclined transition profile 63 is designed at the top outer edge of the outer mold sleeve 6, and in other embodiments, the inclined transition profile 63 is designed at the bottom outer edge of the limiting plate 62, or the top outer edge of the outer mold sleeve 6 and the bottom outer edge of the limiting plate 62 are both provided with an inclined transition profile 63.
[0072] When the pressure plate 7 is pressed down, the second petal structures 61 are brought closer to each other under the action of the inclined transition surface 63, and the second petal structures 61 form a continuous annular structure. The pressure plate 7 continues to be pressed down, and the limit plate 62 abuts against the outer wall of the second petal structure 61 forming a continuous annular structure, so that the petaled outer mold sleeve 6 is in a state of matching with the annular cylinder part 1. The pressure plate 7 continues to be pressed down, and the pressure plate 7 contacts the inner mold sleeve 5, the annular cylinder part 1 and the outer mold sleeve 6, so that the three move toward the large diameter end of the cone 3.
[0073] The annular top plate 4 is provided with a connecting plate 64 corresponding to each of the second petal structures 61, and the connecting plate 64 is located at the outer periphery of the second petal structure 61. A pull rod 65 is fixedly connected to the side wall of the second petal structure 61 facing the connecting plate 64, and a through hole is provided on the connecting plate 64 for the pull rod 65 to slide. The pull rod 65 is sleeved with a spring 66 on the outer periphery of the side of the connecting plate 64 facing away from the second petal structure 61, and the end of the spring 66 away from the second petal structure 61 is fixedly connected to the pull rod 65. When the second petal structure 61 is in contact with the outer wall of the annular cylindrical part 1, there is a gap between the second petal structure 61 and the connecting plate 64, and the spring 66 is in a compressed state. Before placing the annular cylindrical part 1 into the forming mold, the pressing plate 7 rises until the limiting plate 62 is separated from the outer mold sleeve 6. Under the elastic force of the spring 66, the second petal structure 61 automatically expands outward, and the first petal structure 51 automatically moves inward, thereby expanding the distance between the second petal structure 61 and the first petal structure 51, and facilitating the placement of the annular cylindrical part 1. The positions of the connecting plate 64 and the limiting plate 62 are staggered in the circumferential direction to avoid mutual interference.
[0074] The above is only a specific implementation of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed in the present application should be included in the protection scope of the present application. Therefore, the protection scope of the present application shall be based on the protection scope of the claims.
Claims
1. A composite forming process for thin-walled sheet metal parts, characterized in that: The steps include: Step 1, preparing an annular cylindrical part that meets the size of the thin-walled sheet metal part, and correcting the roundness of the annular cylindrical part; Step 2, forming a plurality of protruding reinforcing ribs at the designed positions of the side wall of the annular cylinder part by extrusion, wherein the length direction of the reinforcing ribs is arranged along the axial direction of the annular cylinder, and the plurality of the reinforcing ribs are distributed at intervals; Step 3, forming flanges at both ends of the annular cylinder part processed in step 2; Step 4, forming a flanging hole at a designed position of the side wall of the annular cylinder part processed in step 3; Step 5, correcting the roundness of the annular cylinder part processed in step 4.
2. The thin-walled sheet metal composite forming process according to claim 1, characterized in that: In the step 2, the plurality of reinforcing ribs on the annular cylinder part are formed at one time.
3. The thin-walled sheet metal composite forming process according to claim 1, characterized in that: The step 4 specifically includes: A flange bottom hole is processed at the designed position of the side wall of the annular cylinder part processed in step 3, and the flange bottom hole is flanged to form a final flange hole.
4. A molding die, characterized in that: Used in step 2 of any one of claims 1 to 3 to form a plurality of reinforcing ribs (11) on the annular cylindrical part (1); The forming die clamps and fits the side wall of the annular cylinder, and the forming die simultaneously applies a deformation force to the designed positions of all the reinforcing ribs (11) on the side wall of the annular cylinder to simultaneously form a plurality of reinforcing ribs (11).
5. The molding die according to claim 4, characterized in that: The molding die comprises: A base (2) for mounting on a platform of a hydraulic press; A truncated cone (3) mounted on the base (2); An annular top plate (4) is placed on the base (2), and the annular top plate (4) is sleeved on the outer periphery of the truncated cone (3); An inner mold sleeve (5) is used to be sleeved on the outer periphery of the circumferential side wall of the truncated cone (3), and the bottom of the inner mold sleeve (5) is in contact with the top surface of the annular top plate (4). The inner wall surface of the inner mold sleeve (5) is a conical profile surface, and the conical profile surface matches the outer periphery of the truncated cone (3). The outer wall surface of the inner mold sleeve (5) is used to match the inner wall of the annular cylinder part (1), and a protrusion structure (53) matching the inner wall surface of each reinforcing rib (11) is provided on the outer wall surface of the inner mold sleeve (5). The inner mold sleeve (5) includes a plurality of first petal structures (51) distributed along the circumferential direction. When the outer diameter of the inner mold sleeve (5) is in contact with the inner wall of the annular cylinder part (1), there are gaps between the plurality of first petal structures (51); An outer mold sleeve (6) is sleeved on the outer periphery of the outer mold sleeve (6), and the bottom of the outer mold sleeve (6) is in contact with the top surface of the annular top plate (4), the inner wall surface of the outer mold sleeve (6) is used to match the outer wall surface of the annular cylinder part (1), and the inner wall surface of the outer mold sleeve (6) is provided with a groove structure (67) matching the outer wall surface of each reinforcing rib (11); A pressing plate (7) is used to be connected to the telescopic rod of the hydraulic press, and the pressing plate (7) is used to apply downward pressure to the inner mold sleeve (5) and the outer mold sleeve (6); A cavity for accommodating the annular cylindrical part (1) and the forming of the reinforcing ribs (11) is formed between the inner mold sleeve (5) and the outer mold sleeve (6); when the annular top plate (4) is lifted up, the inner mold sleeve (5) moves toward the small diameter end of the truncated cone (3), and a plurality of the first petal structures (51) move closer to each other so that the annular cylindrical part (1) is sleeved on the outer periphery of the raised structure (53); when the pressure plate (7) presses the inner mold sleeve (5) and the outer mold sleeve (6) downward until the annular top plate (4) abuts the base (2), the inner mold sleeve (5) moves closer to the large diameter end of the truncated cone (3), and a plurality of the first petal structures (51) move away from each other; the raised structure (53) applies an outward force to the designed position of the reinforcing ribs (11) of the annular cylindrical part (1) and cooperates with the groove structure (67) on the outer mold sleeve (6) to form the reinforcing ribs (11).
6. The molding die according to claim 5, characterized in that: An accommodating groove (52) is provided on the butted end surfaces of the plurality of first petal structures (51), and an elastic structure for connecting two adjacent first petal structures (51) is provided in the accommodating groove (52), and the elastic structure is used to exert a force on the plurality of first petal structures (51) to bring them closer to each other.
7. The molding die according to claim 5, characterized in that: The outer mold sleeve (6) includes a plurality of second petal structures (61) distributed along the circumferential direction. When the inner wall of the outer mold sleeve (6) is in contact with the outer wall of the annular cylindrical part (1), the plurality of second petal structures (61) form a continuous annular structure. The second petal structures (61) are movably arranged relative to the base (2). The molding die also includes a limiting component. The limiting component is used to apply a force to the second petal structures (61) to move closer to each other when the reinforcing rib (11) is molded so that the plurality of second petal structures (61) form a continuous annular structure.
8. The molding die according to claim 7, characterized in that: The limiting assembly comprises a limiting plate (62) fixedly connected to the pressure plate (7), and the outer side of each second petal structure (61) is correspondingly provided with the limiting plate (62), and when the limiting plate (62) and the outer wall of the second petal structure (61) are in contact, the second petal structure (61) forms a continuous annular structure; Wherein, when the pressing plate (7) is pressed downward, the second petal structure (61) forms a continuous annular structure before the lower pressing plate (7) contacts the inner mold sleeve (5), and an inclined transition surface (63) is provided on the top outer edge of the second petal structure (61) of the lower pressing plate (7) and / or the bottom inner edge of the limiting plate (62), and the inclined transition surface (63) gradually decreases from bottom to top.
9. The molding die according to claim 8, characterized in that: The annular top plate (4) is provided with a connecting plate (64) corresponding to each of the second petal structures (61), and the connecting plate (64) is located on the outer periphery of the second petal structure (61). A pull rod (65) is fixedly connected to the side wall of the second petal structure (61) facing the connecting plate (64), and a through hole is provided on the connecting plate (64) for the pull rod (65) to slide. The pull rod (65) is sleeved with a spring (66) on the outer periphery of the side of the connecting plate (64) facing away from the second petal structure (61), and one end of the spring (66) away from the second petal structure (61) is fixedly connected to the pull rod (65). When the second petal structure (61) and the outer wall of the annular cylinder part (1) are in contact, there is a gap between the second petal structure (61) and the connecting plate (64), and the spring (66) is in a compressed state.
Citation Information
Patent Citations
Split expanding type mold and method for manufacturing annular piece with ribs inside
CN105499388A
Square tank with top necking down and manufacturing technology corresponding to square tank
CN106270259A
Integral forming die for gas turbine flame tube inner ring and forming method
CN112916734A
Stamping die for local forming of thin-wall metal plate
CN117340094A
Spiral expansion rib mold for manufacturing barrel
CN202921774U