Repair method for repairing glaze layer on surface of pottery clay glazed tile
By marking the areas to be repaired on damaged parts of the glazed tiles, cleaning and filling the repair slurry, rolling and coating the glaze paint, the problem of refiring glazed tiles in the existing technology is solved, and the problem of refiring glazed tiles in the existing technology is shortened. The repair cycle has been improved and the original retention effect has been improved.
Patent Information
- Application Number
- CN202411020401.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-11-15
AI Technical Summary
The prior art usually requires refiring when repairing clay glazed tiles, resulting in a greater degree of intervention in the exterior walls of historical buildings, affecting the original retention effect after repair, and a longer repair cycle.
By marking the areas to be repaired on the damaged parts of the glazed tiles, checking and cleaning the loose and peeling surface layer, preparing and filling the repair slurry, rolling and smoothing, drawing the texture with a mold, and applying glaze paint after drying , form a layer of repaired glaze to avoid refiring.
The repair cycle of historical buildings has been shortened, the degree of intervention in the exterior wall has been reduced, the original retention effect after repair has been improved, and the crack resistance performance has been improved by pre-embedding of crack-resistant mesh, continuing the original appearance of glazed tiles.
Smart Images

Figure CN118958730A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of building repair, and more specifically to a repair method for repairing a glaze layer on the surface of a clay glazed tile. Background Art
[0002] Glazed tiles are tiles whose surface has been glazed and fired at high temperature and high pressure. They are composed of two parts: the clay embryo and the glaze on the surface. Glazed tiles have rich colors and patterns, many specifications, are easy to clean, and have a wide range of choices. The glaze layer on the surface of glazed tiles can be made into various patterns and designs, which are richer in color and pattern than polished tiles. Some historical buildings have exterior walls in the form of clay glazed tiles. At present, the restoration of clay glazed tiles is almost all replaced and repaired by re-firing the original glazed tiles, resulting in a large degree of intervention in the exterior walls of historical buildings, affecting the original state preservation effect of the historical buildings after repair, and the repair cycle of historical buildings is relatively long. In view of this, we propose a repair method for repairing the glaze layer on the surface of clay glazed tiles. Summary of the invention
[0003] In order to overcome the deficiencies of the prior art, the present invention provides a repair method for repairing the glaze layer on the surface of clay glazed tiles to solve the problems raised in the above-mentioned background technology.
[0004] To achieve the above object, the present invention provides the following technical solution: a method for repairing the glaze layer on the surface of clay glazed tiles, comprising the following steps:
[0005] SP01: Mark the area to be repaired on the damaged part of the glazed tile;
[0006] SP02: Check the damaged parts of the glazed tiles and evaluate the quality of the surface layer around the damaged parts of the glazed tiles;
[0007] SP03: Clean the area to be repaired of the glazed tiles and remove the loose and peeling surface layer on the area to be repaired of the glazed tiles;
[0008] SP04: Prepare repair slurry, fill the repair slurry on the area to be repaired, and the repair slurry after filling forms the surface layer of the repair area;
[0009] SP05: Roll and smooth the surface of the repair area;
[0010] SP06: If the glazed tile surface has texture requirements, use a mold to draw the texture;
[0011] SP07: Dry the surface layer of the repair area to make it harden to form a repair germ layer, and apply glaze paint on the surface of the dried and hardened repair germ layer to obtain a repair glaze layer.
[0012] As a preferred technical solution of the present invention, the marking of the area to be repaired is specifically to use a marker pen to draw a marking line along the edge of the damaged part of the glazed tile to form the area to be repaired.
[0013] As a preferred technical solution of the present invention, the process of inspecting glazed tiles includes the following steps:
[0014] SP11: Use a rubber hammer to tap the surface layer around the damaged part of the glazed tile to observe whether it is loose or peeling;
[0015] SP12: If the surface layer around the damaged part of the glazed tile does not become loose or peeled off, determine the area to be repaired;
[0016] SP13: If the surface layer around the damaged part of the glazed tile becomes loose and peeling, use a marker to draw expansion marking lines along the edge of the loose and peeling part to redefine the area to be repaired.
[0017] As a preferred technical solution of the present invention, the process of cleaning glazed tiles comprises the following steps:
[0018] SP21: Use a copper brush to preliminarily remove the surface residue in the area to be repaired;
[0019] SP22: After the initial cleaning is completed, use dry sandpaper to polish the surface of the area to be repaired;
[0020] SP23: After sanding, use a soft brush to clean the debris on the surface of the area to be repaired.
[0021] As a preferred technical solution of the present invention, the filling of the repair slurry is specifically to wet the area to be repaired with water, divide the repair slurry into three layers and fill it on the area to be repaired, and pre-embed the anti-cracking mesh between two adjacent layers of repair slurry.
[0022] As a preferred technical solution of the present invention, the repair slurry is prepared by mixing clay, external wall elastic aggregate, brick powder, stone powder, adhesive and water.
[0023] As a preferred technical solution of the present invention, the weight proportions of the components in the repair slurry are 25-30 of clay, 15-20 of external wall elastic aggregate, 20-25 of brick powder, 15-20 of stone powder, 10-15 of adhesive and 15-20 of water.
[0024] As a preferred technical solution of the present invention, the rolling and smoothing treatment is specifically to use a pressure roller to repeatedly roll on the surface layer of the repair area so that the surface layer of the repair area is compacted, and then use a trowel to smooth the compacted surface layer of the repair area.
[0025] As a preferred technical solution of the present invention, the texture drawing specifically comprises selecting a mold of corresponding texture, and according to the texture of the glaze layer on the surface of the undamaged part of the glazed tile, scraping the mold along the surface layer of the repaired area to draw the texture, so that the texture of the glaze layer on the surface of the undamaged part of the glazed tile is adapted and docked with the texture on the surface layer of the repaired area.
[0026] As a preferred technical solution of the present invention, the process of obtaining the repaired glaze layer comprises the following steps:
[0027] SP31: Use the warm air flow generated by the heater to evenly blow to the surface of the repair area to speed up the drying and hardening of the surface layer in the area;
[0028] SP32: After the surface layer of the repaired area is completely hardened, the repair germ layer is obtained, and the repair germ layer is cleaned with water, and the repair germ layer is wiped with absorbent cotton;
[0029] SP33: After the repair germ layer is dry, select the corresponding glaze paint according to the glaze layer on the surface of the undamaged part of the glazed tile, and use a spray gun to evenly spray the glaze paint on the repair germ layer to form a repair glaze layer;
[0030] SP34: Use an air dryer to air-dry the repaired glaze layer until the repaired glaze layer has the same smoothness as the glaze layer on the undamaged part of the glazed tile.
[0031] Compared with the prior art, the present invention has the following beneficial effects:
[0032] 1. The present invention marks the area to be repaired on the damaged part of the glazed tile, inspects the damaged part of the glazed tile, evaluates the quality of the surface layer around the damaged part of the glazed tile, cleans the area to be repaired of the glazed tile, removes the loose and peeling surface layer on the area to be repaired of the glazed tile, prepares repair slurry, fills the repair slurry on the area to be repaired, and the repair slurry after filling forms the surface layer of the repair area, rolls and smoothes the surface layer of the repair area, uses a mold to draw texture, dries the surface layer of the repair area, hardens the surface layer of the repair area to form a repair germ layer, and applies glaze paint on the surface of the dried and hardened repair germ layer to obtain a repair glaze layer, thereby eliminating the need to re-fire the original glazed tile for replacement and repair, which is convenient for shortening the repair cycle of historical buildings, helping to reduce the degree of intervention in the exterior walls of historical buildings, and improving the original state preservation effect of historical buildings after repair.
[0033] 2. The present invention wets the area to be repaired with water, divides the repair slurry into three layers and fills them on the area to be repaired, and pre-buries an anti-crack mesh between two adjacent layers of repair slurry. The use of each anti-crack mesh can effectively improve the anti-crack performance.
[0034] 3. The present invention selects a mold with a corresponding texture, and according to the texture of the glaze layer on the surface of the undamaged part of the glazed tile, scrapes the mold along the surface of the repaired area to draw the texture, so that the texture of the glaze layer on the surface of the undamaged part of the glazed tile is adapted and connected with the texture on the surface of the repaired area, thereby better continuing the original appearance of the glazed tile. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] Figure 1 A schematic diagram of the process steps of a repair method for repairing the glaze layer on the surface of a clay glazed tile according to the present invention;
[0036] Figure 2 A schematic diagram of the process steps of inspecting glazed tiles in a repair method for repairing the glazed layer on the surface of clay glazed tiles according to the present invention;
[0037] Figure 3 A schematic diagram of the process steps of cleaning glazed tiles in a repair method for repairing the glazed layer on the surface of clay glazed tiles according to the present invention;
[0038] Figure 4 A schematic diagram of the process steps for obtaining a repaired glaze layer in a repair method for a glazed clay tile surface according to the present invention;
[0039] Figure 5 The present invention is a schematic diagram of the cross-sectional structure of a glazed tile in a repair method for repairing a glazed layer on the surface of a clay glazed tile.
[0040] In the figure: 1. Glazed tiles; 2. Repair slurry; 3. Repair area surface layer; 4. Repair glaze layer; 5. Anti-cracking mesh. DETAILED DESCRIPTION
[0041] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0042] like Figures 1 to 5 As shown, the present invention provides a method for repairing the glaze layer on the surface of clay glazed tiles, comprising the following steps:
[0043] SP01: Mark the area to be repaired on the damaged part of glazed tile 1;
[0044] SP02: Check the damaged part of glazed tile 1 and evaluate the quality of the surface layer around the damaged part of glazed tile 1;
[0045] SP03: Clean the area to be repaired of the glazed tile 1 and remove the loose and peeling surface layer on the area to be repaired of the glazed tile 1;
[0046] SP04: Prepare the repair slurry 2, fill the repair slurry 2 on the area to be repaired, and the repair slurry 2 after filling forms the repair area surface layer 3;
[0047] SP05: Roll and smooth the surface layer 3 of the repair area;
[0048] SP06: If the surface of glazed tile 1 has texture requirements, use a mold to draw the texture;
[0049] SP07: Dry the surface layer 3 of the repair area so that the surface layer 3 of the repair area hardens to form a repair germ layer, and apply glaze paint on the surface of the dried and hardened repair germ layer to obtain a repair glaze layer 4.
[0050] Among them, marking the area to be repaired specifically involves using a marker pen to draw a marking line along the edge of the damaged part of the glazed tile 1 to form the area to be repaired.
[0051] Among them, Figure 2 As shown, the process of inspecting the glazed tile 1 includes the following steps:
[0052] SP11: Use a rubber hammer to tap the surface layer around the damaged part of glazed tile 1 to observe whether it is loose or peeling;
[0053] SP12: If the surface layer around the damaged part of the glazed tile 1 does not become loose or peeled off, determine the area to be repaired;
[0054] SP13: If the surface layer around the damaged part of the glazed tile 1 becomes loose and peeling, use a marker to draw an enlarged marking line along the edge of the loose and peeling part to redefine the area to be repaired.
[0055] Among them, Figure 3 As shown, the process of cleaning the glazed tile 1 includes the following steps:
[0056] SP21: Use a copper brush to preliminarily remove the surface residue in the area to be repaired;
[0057] SP22: After the initial cleaning is completed, use dry sandpaper to polish the surface of the area to be repaired;
[0058] SP23: After sanding, use a soft brush to clean the debris on the surface of the area to be repaired.
[0059] Among them, Figure 2 As shown, the repair slurry 2 is filled by wetting the area to be repaired with water, and the repair slurry 2 is divided into three layers and filled on the area to be repaired, and the anti-crack mesh 5 is pre-buried between two adjacent layers of the repair slurry 2. The use of each anti-crack mesh 5 can effectively improve the anti-crack performance.
[0060] Among them, Figure 2 As shown, the repair slurry 2 is prepared by mixing clay, exterior wall elastic aggregate, brick powder, stone powder, adhesive and water, so that the repair slurry 2 is made of the same original material as the glazed tile 1, thereby ensuring the overall repair effect of the repair slurry 2.
[0061] Among them, Figure 2 As shown, the weight proportions of the components in the repair slurry 2 are 25-30 of clay, 15-20 of external wall elastic aggregate, 20-25 of brick powder, 15-20 of stone powder, 10-15 of adhesive and 15-20 of water, so that the repair slurry 2 has good bonding and adhesion properties.
[0062] Among them, Figure 2 As shown, the rolling and smoothing treatment is specifically to use a pressure roller to repeatedly roll on the surface layer 3 of the repair area so that the surface layer 3 of the repair area is compacted, and then use a trowel to smooth the compacted surface layer 3 of the repair area to improve the structural compactness of the surface layer 3 of the repair area.
[0063] Among them, Figure 2 As shown, drawing the texture specifically involves selecting a mold of the corresponding texture, and according to the texture of the glaze layer on the surface of the undamaged part of the glazed tile 1, scraping the mold along the surface layer 3 of the repair area to draw the texture, so that the texture of the glaze layer on the surface of the undamaged part of the glazed tile 1 is adapted and connected with the texture on the surface layer 3 of the repair area, thereby better continuing the original appearance effect of the glazed tile 1.
[0064] Among them, Figure 4 As shown, the process of obtaining the repaired glaze layer 4 includes the following steps:
[0065] SP31: Use the warm air flow generated by the heater to evenly blow to the surface layer 3 of the repair area to accelerate the drying and hardening speed of the surface layer in the area;
[0066] SP32: After the surface layer 3 of the repaired area is completely hardened, the repair germ layer is obtained, and the repair germ layer is cleaned with water, and the repair germ layer is wiped with absorbent cotton;
[0067] SP33: After the repair germ layer is dried, select the corresponding glaze paint according to the glaze layer on the surface of the undamaged part of the glazed tile 1, and use a spray gun to evenly spray the glaze paint on the repair germ layer to form a repair glaze layer 4;
[0068] SP34: Use an air dryer to air-dry the repaired glaze layer 4 so that the repaired glaze layer 4 has the same smoothness as the surface glaze layer of the undamaged part of the glazed tile 1.
[0069] In summary:
[0070] The method includes marking the area to be repaired on the damaged part of the glazed tile 1, inspecting the damaged part of the glazed tile 1, evaluating the quality of the surface layer around the damaged part of the glazed tile 1, cleaning the area to be repaired of the glazed tile 1, removing the loose and peeling surface layer on the area to be repaired of the glazed tile 1, preparing a repair slurry 2, filling the repair slurry 2 on the area to be repaired, and forming a surface layer 3 of the repair area with the repair slurry 2 after filling. The surface layer 3 of the repair area is rolled and smoothed. If the glazed tile surface 1 has texture requirements, a mold is used to draw the texture, and the surface layer 3 of the repair area is dried so that the surface layer 3 of the repair area is hardened to form a repair germ layer. Glaze paint is applied on the surface of the dried and hardened repair germ layer to obtain a repair glaze layer, thereby eliminating the need to re-fire the original glazed tile for replacement and repair, thereby shortening the repair cycle of historical buildings and reducing the degree of intervention in the exterior walls of historical buildings.
[0071] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0072] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for repairing the glaze layer on the surface of a clay glazed tile, characterized in that: The following steps are involved: SP01: Mark the area to be repaired on the damaged part of the glazed tile (1); SP02: Inspect the damaged part of the glazed tile (1) and evaluate the quality of the surface layer around the damaged part of the glazed tile (1); SP03: Cleaning the area to be repaired of the glazed tile (1) and removing the loose and peeling surface layer on the area to be repaired of the glazed tile (1); SP04: preparing a repair slurry (2), filling the repair slurry (2) on the area to be repaired, and the repair slurry (2) after filling forms a surface layer (3) of the repair area; SP05: Roll and smooth the surface layer (3) of the repair area; SP06: If the glazed tile (1) has a texture requirement on its surface, use a mold to draw the texture; SP07: Drying the surface layer (3) of the repaired area so that the surface layer (3) of the repaired area hardens to form a repair germ layer, and coating the surface of the dried and hardened repair germ layer with glaze paint to obtain a repair glaze layer (4).
2. A method for repairing the glaze layer on the surface of clay glazed tiles according to claim 1, characterized in that: The marking of the area to be repaired specifically involves using a marking pen to draw a marking line along the edge of the damaged part of the glazed tile (1) to form the area to be repaired.
3. A method for repairing the glaze layer on the surface of clay glazed tiles according to claim 1, characterized in that: The process of inspecting the glazed tile (1) comprises the following steps: SP11: Use a rubber hammer to tap the surface layer around the damaged part of the glazed tile (1) to see if it is loose or peeling off. SP12: If the surface layer around the damaged part of the glazed tile (1) does not become loose or peeled off, the area to be repaired is determined; SP13: If the surface layer around the damaged part of the glazed tile (1) becomes loose and flaking, use a marker to draw an enlarged marking line along the edge of the loose and flaking part to redefine the area to be repaired.
4. A method for repairing the glaze layer on the surface of clay glazed tiles according to claim 1, characterized in that: The process of cleaning the glazed tiles (1) comprises the following steps: SP21: Use a copper brush to preliminarily remove the surface residue in the area to be repaired; SP22: After the initial cleaning is completed, use dry sandpaper to polish the surface of the area to be repaired; SP23: After sanding, use a soft brush to clean the sanding debris on the surface of the area to be repaired.
5. A method for repairing the glaze layer on the surface of clay glazed tiles according to claim 1, characterized in that: The filling and laying of the repair slurry (2) specifically comprises wetting the area to be repaired with water, dividing the repair slurry (2) into three layers and laying them on the area to be repaired, and pre-burying the anti-cracking mesh (5) between two adjacent layers of the repair slurry (2).
6. A method for repairing the glaze layer on the surface of clay glazed tiles according to claim 5, characterized in that: The repair slurry (2) is prepared by mixing clay, external wall elastic aggregate, brick powder, stone powder, adhesive and water.
7. A method for repairing the glaze layer on the surface of clay glazed tiles according to claim 6, characterized in that: The weight proportions of the components in the repair slurry (2) are 25-30 of clay, 15-20 of external wall elastic aggregate, 20-25 of brick powder, 15-20 of stone powder, 10-15 of adhesive and 15-20 of water.
8. A method for repairing the glaze layer on the surface of clay glazed tiles according to claim 1, characterized in that: The rolling and smoothing treatment specifically involves using a roller to repeatedly roll the surface layer (3) of the repair area so that the surface layer (3) of the repair area is compacted, and then using a trowel to smooth the compacted surface layer (3) of the repair area.
9. A method for repairing the glaze layer on the surface of clay glazed tiles according to claim 1, characterized in that: The texture drawing specifically comprises selecting a mold corresponding to the texture, and according to the texture of the glazed layer on the surface of the undamaged part of the glazed tile (1), scraping the mold along the surface layer (3) of the repaired area to draw the texture, so that the texture of the glazed layer on the surface of the undamaged part of the glazed tile (1) is adapted to and docked with the texture on the surface layer (3) of the repaired area.
10. A method for repairing the glaze layer on the surface of clay glazed tiles according to claim 1, characterized in that: The process of obtaining the repaired glaze layer (4) comprises the following steps: SP31: Use a warm air blower to evenly blow the warm air flow generated by the warm air blower to the surface layer of the repair area (3), thereby accelerating the drying and hardening speed of the surface layer of the area; SP32: After the surface layer (3) of the repaired area is completely hardened to obtain the repair germ layer, the repair germ layer is cleaned with water and wiped with absorbent cotton; SP33: After the repair germ layer is dried, a corresponding glaze paint is selected according to the glaze layer on the surface of the undamaged part of the glazed tile (1), and the glaze paint is evenly sprayed onto the repair germ layer using a spray gun to form a repair glaze layer (4); SP34: Use an air dryer to air dry the repaired glaze layer (4) so that the repaired glaze layer (4) has the same smoothness as the glaze layer on the undamaged part of the glazed tile (1).