Lithium ion battery life prediction method based on electrochemical-thermal coupling model
Through the lithium-ion battery life prediction method based on the electrochemical-thermal coupling model, the problem of lack of universality and accuracy in the prior art is solved, and the accurate prediction of the cycle and storage life of lithium-ion battery is achieved, and electricity is considered The chemical aging mechanism improves the accuracy of prediction and the universality of the model.
Patent Information
- Application Number
- CN202411088107.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-15
AI Technical Summary
The existing lithium-ion battery life prediction methods lack universality, cannot accurately predict cycle life and storage life, and fail to effectively reflect the electrochemical aging mechanism, making it difficult to ensure the accuracy of the model.
Using the lithium-ion battery life prediction method based on the electrochemical-thermal coupling model, the electrochemical-thermal coupling model is established and corrected by collecting experimental battery information, adding aging mechanism and setting aging conditions, using experimental data to correct the model, and finally predicting the battery life. This method combines geometric information, electrochemical parameters and thermal properties, and considers a variety of aging mechanisms, including SEI membranes, lithium evolution, active material peeling and porosity reduction.
Accurate prediction of the cycle life, storage life and calendar life of lithium-ion batteries is achieved, and the inflection point of accelerated life attenuation can be simulated, and the correlation with aging parameters and factors is provided, which improves the accuracy and universality of battery life prediction.
Smart Images

Figure CN118962505A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of lithium-ion batteries, and in particular relates to a lithium-ion battery life prediction method based on an electrochemical-thermal coupling model. Background Art
[0002] Lithium-ion batteries have the advantages of high operating voltage, high energy density, no memory effect and low self-discharge rate. They have been widely used in portable electronic products. In recent years, they have been widely used in electric vehicles and energy storage fields.
[0003] The life of lithium-ion batteries mainly includes cycle life, storage life, etc. Customers in different fields have different needs. The power field pays more attention to cycle life, while the energy storage field pays more attention to storage life. The test cycle of cycle life is about more than two years, and the test cycle of storage life is even longer, which is several years.
[0004] Chinese patent application number CN202410074690.9 discloses a method for predicting the cycle life of lithium-ion batteries based on an attenuation mechanism model. It only involves cycle life and does not involve other aging conditions, so this method is not universal. In addition, the simulation results do not reflect the inflection point of the life curve, that is, they do not reflect the advantages of mechanism aging.
[0005] Chinese patent application number CN202211545066.X discloses a lithium-ion battery life simulation method, device, equipment, storage medium and vehicle. It only involves cycle life and storage life, and does not involve other aging conditions, so this method is not universal. Although it mentions storage conditions, it only mentions that there is no explanation about the setting of storage conditions, so it can be considered as only cycle life. In addition, regarding the calibration of the electrochemical aging mechanism model, only more than 400 weeks of cycle data were used to calibrate the key parameters, so the accuracy of the model is difficult to guarantee.
[0006] Therefore, a more accurate and universal lithium-ion battery life prediction method is urgently needed. Summary of the invention
[0007] In order to solve the defects of the prior art, the present invention discloses a method based on an electrochemical-thermal coupling model. Lithium-ion battery life prediction method.
[0008] The present application provides a method for predicting the life of a lithium-ion battery based on an electrochemical-thermal coupling model, comprising the following steps: S1: Collect information of experimental battery; S2: Establish an electrochemical-thermal coupling model of the experimental battery; S3: Modified electrochemical-thermal coupling model; S4: Add aging mechanism, set aging conditions, and establish an aging model for the experimental battery; S5: Using the aging experimental data of the experimental battery, correct the above aging model; S6: Based on the above-mentioned corrected aging model, predict the life of the experimental battery.
[0009] Preferably, in step S1, the information of the experimental battery includes geometric information, design information, electrochemical physical property parameters, thermal physical property parameters, and experimental data.
[0010] Preferably, the geometric information includes the geometric information of the battery cell level, specifically: the thickness of the copper foil, the thickness of the negative electrode single-sided coating, the thickness of the separator, the thickness of the positive electrode single-sided coating, the thickness of the aluminum foil, the length and width of the positive electrode sheet, and the total number of positive electrode sheets. This information is used for the electrochemical model; The geometric information also includes the geometric information of the battery cell level, specifically: the width, thickness, and height of the battery. This information is used for the geometry of the thermal model, which is simplified using a square block; Design information includes: the surface density and compaction density of the positive and negative electrodes; Electrochemical physical parameters include: maximum lithium insertion concentration of positive and negative electrodes, active particle radius, solid phase diffusion coefficient, active specific surface area, rate constant, tortuosity coefficient, SOC range, equilibrium potential, entropy thermal coefficient, conductivity, liquid phase diffusion coefficient of electrolyte, ion migration number, conductivity, activity coefficient, and porosity of diaphragm; Thermophysical parameters include: battery density, specific heat capacity, and thermal conductivity; The experimental data includes: current, voltage and temperature data of rate charge and discharge.
[0011] Preferably, the electrochemical-thermal coupling model in step S2 is established in Comsol Multiphysics (multi-physics simulation software) 6.0 using a lithium-ion battery module and a solid heat transfer module to establish an electrochemical-thermal coupling model of the experimental battery; The coupling between the electrochemical model and the thermal model is achieved by setting two variables Qh and T, and These two variables are called in the model input parameters to realize the real-time transmission of parameters between the electrochemical model and the thermal model. The Qh refers to the heat generated by the electrochemical model, and the T refers to the temperature of the thermal model.
[0012] Preferably, step S3 uses the rate experimental data of the experimental battery to correct the electrochemical-thermal coupling model, and the correction method includes: S3.1: Setting of working conditions and probes: Using the electrochemical-thermal coupling model established in step S2, set the rate working conditions consistent with the experimental battery in the electrochemical model; set a domain point probe in the thermal model, recorded as probe 1, and the detection position of probe 1 must be consistent with the temperature detection position of the experimental battery; S3.2: Calculation of working conditions and processing of results: perform calculations, process simulation result data after calculations are completed, draw voltage-capacity curves at various rates, and draw the temperature curve of probe 1; S3.3: Compare the experimental curve, adjust the model parameters, and continue to calculate: compare the voltage-capacity curves of each rate of the simulation results with the voltage-capacity curves of the corresponding rates of the experimental battery, and adjust the key physical parameters of the electrochemical model according to the degree of agreement between the simulation curve and the experimental curve; compare the temperature curve of probe 1 of the simulation result with the temperature curve of the experiment, and adjust the key physical parameters of the thermal model; then recalculate; Repeat this process until the voltage-capacity curves at each rate of the simulation results are well matched with the voltage-capacity curves at the corresponding rates of the experimental battery, and the temperature curve of probe 1 of the simulation results is well matched with the temperature curve of the experiment; At this point, the correction of the electrochemical-thermal coupling model is completed.
[0013] Preferably, in step S4, the aging mechanism includes SEI film, lithium precipitation, active material peeling, electrolyte consumption, gas production, porosity reduction, etc., and the aging condition is one of cycle, storage, calendar, etc., and the specific aging condition needs to be consistent with the aging condition of the experimental battery; Adding an aging mechanism specifically includes three steps: S4.1: Setting of Dissolved-Deposited Species: In the setting of the porous electrode node of the electrochemical model, set the name, density, and molar mass of the side reaction substance in the Dissolved-Deposited Species column; if you add several aging mechanisms, you need to set several substances; it is generally believed that the side reaction causes the decrease in porosity, so check the option to subtract the volume change from the electrode liquid volume fraction; in addition, when setting the membrane group, if the side reaction occurs at the negative electrode, it needs to be set in the negative electrode node; if the side reaction occurs at the positive electrode, it needs to be set in the positive electrode node; S4.2: Define the local current density of various side reactions. This can be achieved through variable definition or ODE equation. Each side reaction needs to define its local current density; S4.3: Add porous electrode reaction: Under the above porous electrode node, add multiple porous electrode reactions, which are used to define different side reactions. One porous electrode reaction corresponds to one side reaction, that is, one aging mechanism. In the setting of each porous electrode reaction, the equilibrium potential, local current density, and stoichiometric coefficient of the corresponding side reaction need to be set.
[0014] Preferably, in step S4, the aging condition is set, and specifically needs to be set according to the aging condition of the experimental battery, that is, the aging condition is set consistent with the experimental battery, and different aging conditions need to be set using different nodes.
[0015] Preferably, in step S5, the aging test data of the experimental battery is one of cycle, storage, calendar, etc., and the key aging parameters of the aging model are corrected using the aging test data of the experimental battery.
[0016] Preferably, in step S6, predicting the life of the experimental battery is predicting the life of the experimental battery under an aging condition corresponding to the experimental battery.
[0017] Compared with the prior art, the beneficial effects of the present invention are: this prediction method is modeled from the perspective of electrochemical mechanism, and can take into account various aging mechanisms, which is close to the actual state of the battery. It can accurately predict various battery lifespans, such as cycle life including constant current cycle and constant power cycle, storage life, calendar life, etc., especially considering the aging mechanisms of lithium precipitation and porosity reduction, and can simulate and predict the inflection point of accelerated life decay, that is, the diving point, which cannot be obtained by other non-electrochemical mechanism models.
[0018] By associating the aging parameters with the aging factors, the aging life under different aging factors can be simulated and predicted. For example, in the cycle condition, the aging parameters are associated with the temperature and the rate, and the cycle life under different temperatures and rates can be simulated and predicted. For example, in the storage condition, the aging parameters are associated with the temperature and the storage SOC, and the storage life under different temperatures and different storage SOC can be simulated and predicted.
[0019] In addition, based on this model, parametric scanning can be performed to analyze the main electrochemical physical parameters and aging parameters that affect battery life, which can provide advice for battery design. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 is a flow chart of the method of the present invention; Figure 2 is a comparison diagram of the 0.33C charging simulation capacity-voltage curve and the experimental curve in Example 1; Figure 3 is a comparison diagram of the 0.33C discharge simulation capacity-voltage curve and the experimental curve in Example 1; Figure 4 is a comparison diagram of the 0.5C charging simulation capacity-voltage curve and the experimental curve in Example 1; Figure 5 is a comparison diagram of the 0.5C discharge simulation capacity-voltage curve and the experimental curve in Example 1; Figure 6is a comparison diagram of the 1C charging simulation capacity-voltage curve and the experimental curve in Example 1; Figure 7 is a comparison diagram of the 1C discharge simulation capacity-voltage curve and the experimental curve in Example 1; Figure 8 is a comparison diagram of the 2C charging simulation capacity-voltage curve and the experimental curve in Example 1; Fig. 9 is a comparison diagram of the 2C discharge simulation capacity-voltage curve and the experimental curve in Example 1; Fig.10 is a comparison diagram of the 3C charging simulation capacity-voltage curve and the experimental curve in Example 1; Fig.11 is a comparison diagram of the 3C discharge simulation capacity-voltage curve and the experimental curve in Example 1; Fig.12 is a comparison diagram of the 0.33C charge-stand-0.33C discharge simulation temperature curve and the experimental curve in Example 1; Fig.13 is a comparison diagram of the 0.5C charge-standby-0.5C discharge simulation temperature curve and the experimental curve in Example 1; Fig.14 is a comparison diagram of the 1C charge-standby-1C discharge simulation temperature curve and the experimental curve in Example 1; Fig.15 is a comparison diagram of the 2C charge-standby-2C discharge simulation temperature curve and the experimental curve in Example 1; Fig.16 is a comparison diagram of the 3C charge-stand-3C discharge simulation temperature curve and the experimental curve in Example 1; Fig.17 is a comparison diagram of the capacity retention rate curve of the 25°C 1C / 1C cycle simulation and the experimental curve in Example 1; Fig.18 is a comparison diagram of the capacity retention rate curve of the 25°C 0.5C / 0.5C cycle simulation and the experimental curve in Example 1; Fig.19 It is a prediction diagram of the simulation calculation of the cycle life at different rates at 25°C in Example 1; Fig. 20 is a comparison diagram of the 25°C 1C charging simulation capacity-voltage curve and the experimental curve in Example 2; Fig.21 is a comparison diagram of the 25°C 0.5C discharge simulation capacity-voltage curve and the experimental curve in Example 2; Fig. 22 is a comparison diagram of the 25°C 1C discharge simulation capacity-voltage curve and the experimental curve in Example 2; Fig.23is a comparison diagram of the 25°C 2C discharge simulation capacity-voltage curve and the experimental curve in Example 2; Fig.24 is a comparison diagram of the 25°C 3C discharge simulation capacity-voltage curve and the experimental curve in Example 2; Fig.25 is a comparison diagram of the 25°C 4C discharge simulation capacity-voltage curve and the experimental curve in Example 2; Fig.26 It is a comparison chart of the capacity retention rate curve of the storage life simulation and the experimental curve at 25℃ 30%SOC storage; Fig. 27 is a comparison diagram of the capacity retention rate curve of the storage life simulation and the experimental curve of 25°C 100% SOC storage in Example 2;
[0021] Fig.28 This is a prediction diagram of the simulation calculation of the storage life of different SOC storage at 25°C in Example 2. DETAILED DESCRIPTION
[0022] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0023] S1: Collect information about the experimental battery Experimental battery information, including geometry information, design information, electrochemical physical parameters, thermal physical parameters, and experimental data; The geometric information includes the geometric information of the cell level, specifically: the thickness of the copper foil, the single-sided coating of the negative electrode The thickness of the battery, the thickness of the separator, the thickness of the single-sided coating of the positive electrode, the thickness of the aluminum foil, the length and width of the positive electrode sheet, and the total number of layers of the positive electrode sheet are used for the electrochemical model. It also includes the geometric information of the battery cell level, specifically: the width, thickness, and height of the battery. This information is used for the geometry of the thermal model, and the thermal model geometry is simplified using a block.
[0024] The design information includes: the surface density and compaction density of the positive and negative electrodes.
[0025] The electrochemical physical properties include: maximum lithium insertion concentration of the positive and negative electrodes, active particle radius, solid phase diffusion coefficient, active specific surface area, rate constant, tortuosity coefficient, SOC range, equilibrium potential, entropy thermal coefficient, conductivity, liquid phase diffusion coefficient of the electrolyte, ion migration number, conductivity, activity coefficient, and porosity of the diaphragm.
[0026] Thermophysical parameters include: battery density, specific heat capacity, and thermal conductivity.
[0027] The experimental data includes: current, voltage and temperature data of rate charge and discharge.
[0028] S2: Establishing the electrochemical-thermal coupling model of the experimental battery In Comsol Multiphysics (multi-physics simulation software) 6.0, the electrochemical-thermal coupling model of the experimental battery is established using the lithium-ion battery module and the solid heat transfer module.
[0029] S3: Modified electrochemical-thermal coupling model The electrochemical-thermal coupling model is modified using the rate test data of the experimental battery.
[0030] In the electrochemical model, a rate condition consistent with that of the experimental battery is set; in the thermal model, a domain point probe is set, denoted as probe one, and the detection position of probe one must be consistent with the temperature detection position of the experimental battery.
[0031] Perform calculations, and after the calculations are completed, process the simulation result data, draw the voltage-capacity curves at each rate, and draw the temperature curve of probe one; compare the voltage-capacity curves at each rate of the simulation results with the voltage-capacity curves at the rates corresponding to the experimental battery, and adjust some key physical parameters of the electrochemical model according to the degree of agreement between the simulation curve and the experimental curve; compare the temperature curve of probe one of the simulation results with the temperature curve of the experiment, and adjust some key physical parameters of the thermal model; then recalculate.
[0032] Repeat this process until the voltage-capacity curves at each rate of the simulation results are well matched with the voltage-capacity curves at the corresponding rates of the experimental battery, and the temperature curve of probe 1 in the simulation results is well matched with the temperature curve of the experiment.
[0033] At this point, the correction of the electrochemical-thermal coupling model is completed.
[0034] S4: Add aging mechanism, set aging conditions, and establish aging model for experimental battery The aging mechanism includes SEI film, lithium precipitation, active material peeling, electrolyte consumption, gas production, porosity reduction, etc. The aging condition is one of cycle, storage, calendar, etc. The specific setting of the aging condition needs to be consistent with the aging condition of the experimental battery.
[0035] Addition of aging mechanisms: Setting of dissolved-deposited substances: In the setting of the porous electrode node of the electrochemical model, set the name, density, and molar mass of the side reaction substance in the dissolved-deposited substance column; to add several aging mechanisms, you need to set several substances; it is generally believed that side reactions cause a decrease in porosity, so check the box to subtract the volume change from the electrode liquid volume fraction; in addition, set the membrane group.
[0036] If the side reaction occurs at the negative electrode, it needs to be set in the negative electrode node; if the side reaction occurs at the positive electrode, it needs to be set in the positive electrode node.
[0037] Defining the local current density of various side reactions can be achieved through variable definition or ODE equations.
[0038] Add porous electrode reactions: Under the above porous electrode node, add multiple porous electrode reactions to define different side reactions. One porous electrode reaction corresponds to one side reaction, that is, one aging mechanism. In the settings of each porous electrode reaction, the equilibrium potential, local current density, and stoichiometric coefficient of the corresponding side reaction need to be set.
[0039] Set the aging conditions consistent with the experimental battery. Different aging conditions need to be set using different nodes. For example, for constant current cycle conditions, you can directly use the charge and discharge cycle in the electrode node of the electrochemical model, mainly setting the charge and discharge current, cut-off current, cut-off voltage, shelf time, etc.; for constant power cycle, you need to first establish a probe to define the battery voltage, and then use the relationship of current = power / voltage to define the battery current variable, and then you can use the charge and discharge cycle in the electrode node of the electrochemical model to define the constant power cycle; other aging conditions, such as storage, calendar, etc., need to be implemented through customization using event nodes.
[0040] S5: Use the aging test data of the experimental battery to correct the above aging model The aging test data of the experimental battery is one of the cycle, storage, calendar and so on. Some key aging parameters of the above aging model are corrected by using the aging test data of the experimental battery. The key aging parameters here are mainly the pre-exponential factors and powers in the local current density expressions of various side reactions. The aging curve of lithium-ion batteries generally has segmented characteristics, and the attenuation rates in different stages are different. Therefore, the values of the aging parameters need to be appropriately segmented according to this characteristic of the experimental curve.
[0041] S6: Based on the above corrected aging model, predict the life of the experimental battery Based on the above corrected aging model, the life of the experimental battery corresponding to the aging condition is predicted. For example, the cycle conditions of the experimental battery and the established cycle condition aging model can predict the cycle life of the experimental battery; further, if the simulation model establishes the relationship between the aging parameters and the temperature and rate, the cycle life of the experimental battery at different temperatures and rates can be predicted through simulation calculations. For example, the storage conditions of the experimental battery and the established storage condition aging model can predict the storage life of the experimental battery; further, if the simulation model establishes the relationship between the aging parameters and the temperature and storage SOC, the storage life of the experimental battery at different temperatures and storage SOC can be predicted through simulation calculations. The life of other aging conditions can also be predicted. If there are both cycle condition aging models and storage condition aging models, the calendar life of the experimental battery can be predicted.
[0042] The scheme of the present invention will be explained below in conjunction with Example 1.
[0043] S1: Collect information about the experimental battery: For a certain model of battery of the company, collect its battery information, including geometric information, design information, electrochemical physical parameters, thermal physical parameters, and experimental data.
[0044] The experimental conditions of this battery: Rate conditions: 25℃, rates 0.33C / 0.33C, 0.5C / 0.5C, 1C / 1C, 2C / 2C, 3C / 3C; upper limit voltage 3.65V, lower limit voltage 2V; leave for 1h; during this process, the temperature of the center point of the large surface of the battery outer surface was monitored.
[0045] Aging conditions: 25℃, 1C / 1C cycle and 0.5C / 0.5C cycle, upper limit voltage 3.65V, lower limit voltage 2V; leave for 30 minutes.
[0046] S2: Establishing electrochemical-thermal coupling model: The electrochemical-thermal coupling model of this battery is established in Comsol Multiphysics 6.0. The rate condition is set in accordance with the experimental rate condition mentioned above. Specifically, it can be achieved through the charge and discharge cycle of the electrode node, and the stop condition is set to the lower limit voltage of the battery. A domain point probe is set in the thermal model, denoted as probe 1, and the detection position of probe 1 is consistent with the temperature detection position of the experimental battery.
[0047] S3: Modified electrochemical-thermal coupling model: Submit the calculation, process the settlement results, draw the voltage-capacity curves of 0.33C, 0.5C, 1C, 2C, and 3C charging and discharging respectively, and then compare them with the voltage-capacity curves of 0.33C, 0.5C, 1C, 2C, and 3C charging and discharging of the experimental battery respectively; then adjust some key physical parameters of the electrochemical model according to the degree of fit between each simulation curve and each experimental curve; compare the temperature curve of the simulation result probe one with the experimental temperature curve, and adjust some key physical parameters of the thermal model; then recalculate; repeat this process until the voltage-capacity curves of 0.33C, 0.5C, 1C, 2C, and 3C charging and discharging of the simulation results are well matched with the voltage-capacity curves of 0.33C, 0.5C, 1C, 2C, and 3C charging and discharging of the experimental battery, and the temperature curve of the simulation result probe one is well matched with the experimental temperature curve, so far, the correction of the electrochemical-thermal coupling model is completed.
[0048] The voltage-capacity curves of the simulation results at 0.33C, 0.5C, 1C, 2C, and 3C charging and discharging are compared with the voltage-capacity curves of the test battery at 0.33C, 0.5C, 1C, 2C, and 3C charging and discharging. Figure 2-11 As shown in the figure, the temperature curve of probe 1 in the simulation result is compared with the temperature curve in the experiment. Figure 12-16 shown.
[0049] S4: Add aging mechanism, set aging conditions, and establish aging model of experimental battery: Adding aging mechanisms, for lithium-ion batteries in the lithium iron phosphate system, three aging mechanisms are mainly considered here: SEI film, lithium precipitation, and reduction of porosity.
[0050] In the settings of the negative porous electrode node of the electrochemical model, set the name, density, and molar mass of the side reaction substances (SEI and lithium) in the Dissolved-Deposited Species column. For the decrease in porosity, check the box "Subtract the volume change from the electrode liquid volume fraction" and the calculation formula is as shown in formula ③. In addition, set the membrane group.
[0051] The local current density of SEI film and lithium precipitation reaction are defined respectively, and the calculation formulas are as formula ① and ② respectively, which can be realized by variable definition or ODE equation.
[0052] Under the Porous Electrode node of the negative electrode, add two porous electrode reactions to define the SEI film and lithium precipitation reaction respectively.
[0053] The equilibrium potential, local current density and stoichiometric coefficient of the SEI film and lithium precipitation reaction are set respectively. The setting of the stoichiometric coefficient is based on reaction equations ④ and ⑤ respectively.
[0054] Set the aging condition. The aging condition of this experimental battery is a constant current cycle condition. You can directly use the charge and discharge cycle in the electrode node, 1C / 1C cycle: during the charging process, the charging current is set to 1C current value; check constant current and constant voltage charging, and set the cut-off current to 1C / 20; check shelve, and set the shelve time to 1800s; during the discharge process, the discharge current is set to a negative 1C current value, check shelve, and set the shelve time to 1800s. Set the stop condition to the number of cycles. The settings for the 0.5C / 0.5C cycle are similar. At this point, the aging model of the experimental battery has been established.
[0055] The local current density j of the SEI film reaction SEI : ① Among them C EC s Calculated according to the following formula:
[0056] Where a is the active specific surface area of the electrode, F is the Faraday constant, k 0,SEI is the rate constant of SEI film reaction, C EC s is the concentration of the solvent EC on the graphite surface, R film is the module resistance, U SEI is the equilibrium potential of the SEI film reaction, φ s is the solid phase potential, φ e is the liquid phase potential, j tot is the total volume current density.
[0057] The local current density j of the lithium deposition reaction lpl : ② where i 0,lpl is the exchange current density of the lithium evolution reaction.
[0058] Calculation of porosity ε: ③ The film thickness δ film Calculated according to the following formula:
[0059] Where M is the molar mass and ρ is the density.
[0060] Among them C SEI , C Li Calculated according to the following formula:
[0061] Chemical formula of SEI film reaction: ④ The chemical formula of lithium precipitation reaction: ⑤ S5: Using the aging test data of the experimental battery, the above aging model is corrected: The experimental data of battery aging are 1C / 1C and 0.5C / 0.5C cycles.
[0062] The simulation results of the above 1C / 1C cycle are processed, and the capacity retention rate-cycle number curve is plotted and compared with the experimental curve of 1C / 1C cycle. The pre-exponential factor and power in the local current density expression of SEI film and lithium precipitation reaction are adjusted and recalculated.
[0063] This process is repeated until the capacity retention rate-cycle number curve of the 1C / 1C simulation result is in good agreement with the experimental curve of the 1C / 1C cycle; at this point, the correction of the aging model is completed.
[0064] The cycle curve of lithium-ion batteries in the lithium iron phosphate system is generally divided into three stages: rapid decay in the early stage, slow decay in the middle stage, and rapid decay in the late stage. Therefore, the value of the aging parameter needs to be appropriately segmented according to this feature of the experimental curve. This example uses the 200th week and the 950th week as the dividing points for segmentation. The correction of the aging parameters of the 0.5C / 0.5C simulation cycle is similar.
[0065] Based on the revised model, the calculated capacity retention curve of 1C / 1C cycle is compared with the experimental curve, as shown in Fig.17 As shown; the comparison of the calculated 0.5C / 0.5C cycle capacity retention curve and the experimental curve, as shown Fig.18 shown.
[0066] S6: Based on the above corrected aging model, predict the life of the experimental battery: Based on the above modified aging model, the cycle life of the experimental battery under 25℃ condition of 1C / 1C cycle and 0.5C / 0.5C cycle can be directly predicted. The prediction results are shown in Fig.19 The solid line in .
[0067] In addition, using the aging parameters of 1C / 1C cycle and 0.5C / 0.5C cycle, the relationship between each aging parameter and the rate is established, such as linear or idempotent. Then, the relationship between each aging parameter and the rate is defined. Then, the cycle life at other different rates can be predicted through simulation calculation, such as 2C / 2C, 1.5C / 1.5C, 1.25C / 1.25C, 0.8C / 0.8C, 0.3C / 0.3C, etc. The prediction results are shown in Fig.19 The dotted line in .
[0068] By distinguishing charging and discharging based on aging parameters, the cycle life with different charging and discharging rates, such as 1C / 0.5C and 0.5C / 1C cycles, can be predicted.
[0069] The scheme of the present invention will be explained below in conjunction with Example 2.
[0070] S1: Collect information about the experimental battery: For a certain model of battery of the company, collect its battery information, including geometric information, design information, electrochemical physical parameters, thermal physical parameters, and experimental data.
[0071] The experimental working conditions of this battery are: rate conditions: 25℃, rate discharge, 1C charge, 0.5C, 1C, 2C, 3C, 4C discharge, upper limit voltage 3.65V, lower limit voltage 2.5V.
[0072] Aging conditions: 25℃, 30%SOC and 100%SOC storage. The first 6 storage cycles are 30 days, 15 days, 15 days, 15 days, 15 days and 90 days respectively. The storage periods after the 6th cycle are 60 days.
[0073] S2: Establishing electrochemical-thermal coupling model: The electrochemical-thermal coupling model of this battery is established in Comsol Multiphysics 6.0.
[0074] The setting of the rate condition is consistent with the above experimental rate condition. Specifically, 1C charging is calculated separately, and the stop condition is set to the upper limit of the voltage; then, a parametric scan is used to calculate 0.5C, 1C, 2C, 3C, and 4C discharges, and the stop condition is set to the lower limit of the voltage.
[0075] S3: Modified electrochemical-thermal coupling model: Submit the calculation, process the settlement results, draw the voltage-capacity curves of 1C charging, 0.5C, 1C, 2C, 3C, and 4C discharging respectively, and compare them with the voltage-capacity curves of 1C charging, 0.5C, 1C, 2C, 3C, and 4C discharging of the experimental battery respectively, and then adjust some key physical parameters of the electrochemical model according to the degree of fit between each simulation curve and each experimental curve, and then recalculate; repeat this process until the voltage-capacity curves of 1C charging, 0.5C, 1C, 2C, 3C, and 4C discharging of the simulation results are in good agreement with the voltage-capacity curves of 1C charging, 0.5C, 1C, 2C, 3C, and 4C discharging of the experimental battery. At this point, the correction of the electrochemical-thermal coupling model is completed.
[0076] The voltage-capacity curves of the simulation results 1C charging, 0.5C, 1C, 2C, 3C, 4C discharging are compared with the voltage-capacity curves of the test battery 1C charging, 0.5C, 1C, 2C, 3C, 4C discharging. Figure 20-25 shown.
[0077] S4: Add aging mechanism, set aging conditions, and establish aging model of experimental battery: Adding aging mechanism, for storage aging conditions, two aging mechanisms are mainly considered here: SEI membrane and reduction of porosity.
[0078] In the settings of the negative porous electrode node of the electrochemical model, set the name, density, and molar mass of the side reaction substance (SEI) in the Dissolved-Deposited Species column. For the decrease in porosity, check the box Subtract the volume change from the electrode liquid volume fraction; in addition, set the membrane group.
[0079] The local current density of the SEI film reaction is defined, and the calculation formula is as Formula ① in Example 1, which can be achieved through variable definition or ODE equation.
[0080] Under the porous electrode node of the negative electrode, add a porous electrode reaction to define the SEI membrane reaction. Set the equilibrium potential, local current density, and stoichiometric coefficient of the SEI membrane reaction. The setting of the stoichiometric coefficient is based on the reaction formula ④ in Example 1.
[0081] Set the aging condition. The aging condition of this experimental battery is the storage condition. In the storage condition, before each storage cycle, it is necessary to discharge the battery, set the capacity, and adjust the SOC according to the set capacity value. These can only be achieved through the event function of the software and need to be defined by yourself. At this point, the aging model of the experimental battery has been established.
[0082] S5: Using the aging test data of the experimental battery, the above aging model is corrected: The experimental battery aging test data is stored at 25℃ 30%SOC and 100%SOC.
[0083] The simulation results of the above 30% SOC storage were processed, and the capacity retention rate-time curve was plotted and compared with the experimental curve of 30% SOC storage. The pre-exponential factor and power in the local current density expression of the SEI membrane reaction were adjusted and recalculated.
[0084] This process is repeated until the capacity retention rate-time curve of the simulation result of 30% SOC storage is well consistent with the experimental curve of 30% SOC storage; at this point, the correction of the aging model is completed.
[0085] The aging curve of lithium-ion batteries generally has segmented characteristics, and the attenuation rates in different stages are different. Therefore, the values of aging parameters need to be appropriately segmented according to this characteristic of the experimental curve.
[0086] This example uses the 1st and 6th storage cycles as dividing points for segmentation, and the correction of the aging parameters of 100% SOC storage is similar.
[0087] Based on the modified aging model, the calculated capacity retention curve of 30% SOC storage is compared with the experimental curve, as shown in Fig.26 As shown; the comparison between the calculated 100% SOC storage capacity retention curve and the experimental curve, as shown Fig. 27 shown.
[0088] S6: Based on the above corrected aging model, predict the life of the experimental battery: Based on the above modified aging model, the storage life of the experimental battery at 25°C, 30% SOC and 100% SOC can be directly predicted. The prediction results are shown in Fig.28 The solid line in .
[0089] In addition, using the aging parameters stored at 30% SOC and 100% SOC, the relationship between each aging parameter and the stored SOC, such as linearity, is established. Then, the relationship between each aging parameter and the stored SOC is defined. Then, the storage life under other different SOC storage conditions, such as 40% SOC, 50% SOC, 60% SOC, 70% SOC, etc., can be predicted through simulation calculation. The prediction results are shown in Fig.28 The dotted line in .
Claims
1. A lithium-ion battery life prediction method based on an electrochemical-thermal coupling model, characterized in that: The following steps are involved: S1: Collect information of experimental battery; S2: Establish an electrochemical-thermal coupling model of the experimental battery; S3: Modified electrochemical-thermal coupling model; S4: Add aging mechanism, set aging conditions, and establish an aging model for the experimental battery; S5: Using the aging experimental data of the experimental battery, correct the above aging model; S6: Based on the above-mentioned corrected aging model, predict the life of the experimental battery.
2. The method for predicting the life of a lithium-ion battery based on an electrochemical-thermal coupling model according to claim 1, characterized in that: In step S1, the information of the experimental battery includes geometric information, design information, electrochemical physical parameters, thermal physical parameters, and experimental data.
3. The method for predicting the life of a lithium-ion battery based on an electrochemical-thermal coupling model according to claim 2, characterized in that: The geometric information includes the geometric information of the cell level, specifically: the thickness of the copper foil, the thickness of the negative electrode single-sided coating, the thickness of the separator, the thickness of the positive electrode single-sided coating, the thickness of the aluminum foil, the length and width of the positive electrode sheet, and the total number of positive electrode sheets. This information is used for the electrochemical model; The geometric information also includes the geometric information of the battery cell level, specifically: the width, thickness, and height of the battery. This information is used for the geometry of the thermal model, which is simplified using a square block; Design information includes: the surface density and compaction density of the positive and negative electrodes; Electrochemical physical parameters include: maximum lithium insertion concentration of positive and negative electrodes, active particle radius, solid phase diffusion coefficient, active specific surface area, rate constant, tortuosity coefficient, SOC range, equilibrium potential, entropy thermal coefficient, conductivity, liquid phase diffusion coefficient of electrolyte, ion migration number, conductivity, activity coefficient, and porosity of diaphragm; Thermophysical parameters include: battery density, specific heat capacity, and thermal conductivity; The experimental data includes: current, voltage and temperature data of rate charge and discharge.
4. The method for predicting the life of a lithium-ion battery based on an electrochemical-thermal coupling model according to claim 1, characterized in that: The electrochemical-thermal coupling model in step S2 is established in Comsol Multiphysics (multi-physics simulation software) 6.0 using a lithium-ion battery module and a solid heat transfer module to establish an electrochemical-thermal coupling model of the experimental battery; The coupling between the electrochemical model and the thermal model is achieved by setting two variables Qh and T, and These two variables are called in the model input parameters to realize the real-time transmission of parameters between the electrochemical model and the thermal model. The Qh refers to the heat generated by the electrochemical model, and the T refers to the temperature of the thermal model.
5. The method for predicting the life of a lithium-ion battery based on an electrochemical-thermal coupling model according to claim 1, characterized in that: Step S3 uses the rate test data of the experimental battery to correct the electrochemical-thermal coupling model, and the correction method includes: S3.1: Setting of working conditions and probes: Using the electrochemical-thermal coupling model established in step S2, set the rate working conditions consistent with the experimental battery in the electrochemical model; set a domain point probe in the thermal model, recorded as probe 1, and the detection position of probe 1 must be consistent with the temperature detection position of the experimental battery; S3.2: Calculation of working conditions and processing of results: perform calculations, process simulation result data after calculations are completed, draw voltage-capacity curves at various rates, and draw the temperature curve of probe 1; S3.3: Compare the experimental curve, adjust the model parameters, and continue to calculate: compare the voltage-capacity curves of each rate of the simulation results with the voltage-capacity curves of the corresponding rates of the experimental battery, and adjust the key physical parameters of the electrochemical model according to the degree of agreement between the simulation curve and the experimental curve; compare the temperature curve of probe 1 of the simulation result with the temperature curve of the experiment, and adjust the key physical parameters of the thermal model; then recalculate; Repeat this process until the voltage-capacity curves at each rate of the simulation results are well matched with the voltage-capacity curves at the corresponding rates of the experimental battery, and the temperature curve of probe 1 of the simulation results is well matched with the temperature curve of the experiment; At this point, the correction of the electrochemical-thermal coupling model is completed.
6. The method for predicting the life of a lithium-ion battery based on an electrochemical-thermal coupling model according to claim 1, characterized in that: In step S4, the aging mechanism includes SEI film, lithium precipitation, active material peeling, electrolyte consumption, gas production, porosity reduction, etc. The aging condition is one of cycle, storage, calendar, etc., and the specific aging condition needs to be consistent with the aging condition of the experimental battery; Adding an aging mechanism specifically includes three steps: S4.1: Setting of Dissolved-Deposited Species: In the setting of the porous electrode node of the electrochemical model, set the name, density, and molar mass of the side reaction substance in the Dissolved-Deposited Species column; if you add several aging mechanisms, you need to set several substances; It is generally believed that the side reaction causes the decrease in porosity. Check the box to subtract the volume change from the electrode liquid volume fraction. In addition, when setting the membrane group, if the side reaction occurs at the negative electrode, it needs to be set in the negative electrode node; if the side reaction occurs at the positive electrode, it needs to be set in the positive electrode node; S4.2: Define the local current density of various side reactions. This can be achieved through variable definition or ODE equation. Each side reaction needs to define its local current density; S4.3: Add porous electrode reaction: Under the above porous electrode node, add multiple porous electrode reactions, which are used to define different side reactions. One porous electrode reaction corresponds to one side reaction, that is, one aging mechanism. In the setting of each porous electrode reaction, the equilibrium potential, local current density, and stoichiometric coefficient of the corresponding side reaction need to be set.
7. The method for predicting the life of a lithium-ion battery based on an electrochemical-thermal coupling model according to claim 1, characterized in that: In step S4, the aging condition is set. Specifically, the aging condition needs to be set according to the aging condition of the experimental battery, that is, the aging condition is set to be consistent with the experimental battery. Different aging conditions need to be set using different nodes.
8. The method for predicting the life of a lithium-ion battery based on an electrochemical-thermal coupling model according to claim 1, characterized in that: In step S5, the aging test data of the experimental battery is one of cycle, storage, calendar, etc. The key aging parameters of the aging model are corrected using the aging test data of the experimental battery.
9. The method for predicting the life of a lithium-ion battery based on an electrochemical-thermal coupling model according to claim 1, characterized in that: In step S6, predicting the life of the experimental battery is predicting the life of the experimental battery under an aging condition.
Citation Information
Cited By
Electrochemical-thermal-aging coupled battery model parameter identification method and device, medium and equipment
CN119738724A
Method for predicting service life of composite electrode battery
CN119939856A
Service life prediction method based on lithium battery service condition monitoring
CN119959808A
Lithium battery residual capacity prediction method and system, electronic equipment and storage medium