Method and system for tracking and evaluating surface skid resistance of asphalt mixture pavement
Through wear experiments and image processing technology, the anti-slip performance of asphalt mixture is evaluated, and the problem of inaccurate anti-slip performance evaluation in the prior art is solved, and effective tracking and estimation of road wear and anti-slip performance is achieved.
Patent Information
- Application Number
- CN202410918367.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-10
- Publication Date
- 2024-11-15
AI Technical Summary
The existing technology is difficult to effectively evaluate and design the anti-slip performance of asphalt mixtures. A single anti-slip threshold cannot meet the road safety requirements under different conditions. The laboratory simulation research is inconsistent with the actual road conditions research conclusions, resulting in the anti-slip performance of the road surface. There are differences in mix design and evaluation.
Texture data was collected through wear experiments, converted into grayscale images and binarized. Combined with structural similarity and apparent texture bonding, multi-scale wear indexes were calculated to evaluate the anti-slip properties of asphalt mixture.
A method for real-time tracking of road wear and anti-slip decay is provided for laboratory simulation and practical applications, helping preventive maintenance and life estimates, and improving surface layer performance tracking and service life assessment.
Smart Images

Figure CN118967556A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of road engineering, and in particular to a method and system for tracking and evaluating the anti-skid performance of an asphalt mixture pavement surface. Background Art
[0002] The friction between road tires and the road surface is an important safety parameter for road safety and has been used to assist maintenance and repair decisions. Steel bridge deck pavements usually use fine-grained mixtures to prevent water seepage, and their long-term skid resistance has been questioned. Researchers have targeted this type of pavement for mixture improvement design. The design scheme usually only verifies the skid resistance of a specific material before and after loading through the critical value of a certain skid resistance index. In addition, preventive maintenance (covering, sealing layer), etc. are also usually evaluated in this way. However, studies on different combinations of conditions (such as alignment and environment) have shown that a single skid resistance threshold is not reasonable for evaluating road safety. The skid resistance design threshold in existing specifications can be used to evaluate road driving safety, but cannot be used for mixture design. There are many studies on skid resistance durability, mainly including performance degradation analysis based on road condition surveys and laboratory simulation studies. Performance degradation studies are often data-oriented, while laboratory studies usually simulate actual wear processes. Due to the complexity of actual projects, the conclusions drawn from road condition studies are often inconsistent. In summary, at the engineering application level, the objectives of mixture design and evaluation of pavement anti-skid performance vary greatly. Most existing studies set specific threshold ranges for safety judgment, which makes it difficult to apply them to anti-skid performance life estimation and material design.
[0003] Therefore, the present invention aims to provide a method that can reflect the anti-skid performance of the surface and obtain the road surface wear level and anti-skid performance decay situation in real time through wear experiments. Summary of the invention
[0004] The purpose of the present invention is to provide a method and system for tracking and evaluating the anti-skid performance of an asphalt mixture pavement surface, which can obtain the pavement wear level and anti-skid performance decay in real time through wear experiments, and reflect the anti-skid performance of the road surface.
[0005] To achieve the above object, the present invention provides the following solutions:
[0006] A method for tracking and evaluating the anti-skid performance of an asphalt mixture pavement surface, comprising:
[0007] Collect texture data of asphalt mixture specimens;
[0008] Converting the texture data into a grayscale image, and converting the grayscale image into a binary image;
[0009] Filling the binary image to obtain the apparent texture bonding condition of the asphalt mixture specimen;
[0010] The structural similarity is calculated based on the grayscale image, and the wear condition of the asphalt mixture specimen is obtained in combination with the apparent texture bonding condition, and the anti-skid performance of the asphalt mixture specimen is further obtained.
[0011] Optionally, collecting texture data of the asphalt mixture specimen includes:
[0012] The load, number of abrasions, abrasion and scanning direction are preset, and an abrasion test is performed on the asphalt mixture specimen to collect the texture data, wherein the texture data includes micro texture data and macro texture data.
[0013] Optionally, before converting the texture data into a grayscale image, the method further includes preprocessing the texture data, and the preprocessing includes:
[0014] The texture data is converted into spectrum data by using fast Fourier transform, and the spectrum data is filtered, wherein the micro texture data is low-pass filtered and the macro texture data is band-pass filtered;
[0015] The filtered spectrum data is subjected to inverse fast Fourier transform to obtain macroscopic and microscopic separated texture data.
[0016] Optionally, performing filling processing on the binary image to obtain the apparent texture bonding condition of the asphalt mixture specimen includes:
[0017] Using a four-connected seed filling algorithm to search for connected regions in the binary image, and obtaining the number of pixels and the number of connected regions in the largest connected region in the binary image;
[0018] Based on the number of pixels in the maximum connected area and the number of connected areas, the apparent texture bonding condition of the asphalt mixture specimen is quantified.
[0019] Optionally, the method for quantifying the apparent texture bonding of the asphalt mixture specimen is:
[0020]
[0021] Among them, CON is the connectivity indicator, MNC is the number of pixels in the largest connected area, NCA is the number of connected areas, M is the number of horizontal pixels in the test area, and N is the number of vertical pixels in the test area.
[0022] Optionally, the calculation method for the wear condition of the asphalt mixture specimen is:
[0023] Multi-scale SSIM-T = (SSIMi + SSIMa + SSIMg + CON) / 4
[0024] Among them, SSIMi is the micro texture similarity index, SSIMa is the macro texture similarity index, SSIMg is the grayscale similarity index, and CON is the connectivity index.
[0025] To further achieve the above-mentioned purpose, the present invention also provides a system for tracking and evaluating the anti-skid performance of an asphalt mixture pavement surface, comprising: a detection module, a processing module, and an evaluation module;
[0026] The detection module is used to collect texture data of the asphalt mixture specimen based on the detection device;
[0027] The processing module is used to process the texture data to obtain a grayscale image and a binary image;
[0028] The evaluation module is used to obtain the apparent texture bonding condition of the asphalt mixture specimen based on the binary image, calculate the structural similarity based on the grayscale image, and perform multi-scale wear condition and anti-skid performance evaluation on the asphalt mixture specimen in combination with the apparent texture bonding condition and structural similarity.
[0029] Optionally, the detection device includes: a loading device, a loading device running track, a scanning device, a scanning device running track, and a slot, the asphalt mixture specimen is placed in the slot, the loading device runs on the asphalt mixture specimen via the loading device running track, the scanning device runs on the asphalt mixture specimen via the scanning device running track, and the scanning device running track is arranged on the loading device.
[0030] The beneficial effects of the present invention are:
[0031] The present invention provides effective tools and methods for simulating the surface wear of asphalt mixture pavement in the laboratory, tracking the wear process, testing the decay of anti-skid performance and influencing factors, and can be used for performance tracking and service life estimation of surface preventive maintenance technologies. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0033] Figure 1 This is a flow chart of a method for tracking and evaluating the anti-skid performance of an asphalt mixture pavement surface according to an embodiment of the present invention;
[0034] Figure 2It is a schematic diagram of the structure of a detection device according to an embodiment of the present invention;
[0035] Figure 3 The effect diagrams of the filtering of the macro and micro texture separation of the embodiment of the present invention are completed, wherein (a) is a macro texture filtering effect diagram, and (b) is a micro texture filtering effect diagram;
[0036] Figure 4 The distribution of aggregates on the surface of asphalt mixture at different wear stages of the embodiment of the present invention, wherein (a) is the initial wear stage, (b) is the middle wear stage, and (c) is the late wear stage;
[0037] Figure 5 A grayscale image converted from texture data of an embodiment of the present invention;
[0038] Figure 6 A binary image converted from a grayscale image according to an embodiment of the present invention;
[0039] Figure 7 A schematic diagram of the maximum connected area of surface texture according to an embodiment of the present invention;
[0040] Figure 8 It is a schematic diagram of the change of multi-scale SSIM-T index during the loading and abrasion process of asphalt mixture specimens of different specifications according to an embodiment of the present invention;
[0041] Fig. 9 It is a schematic diagram of the correlation between the friction coefficient index and the multi-scale SSIM-T index of asphalt mixtures of different specifications according to an embodiment of the present invention. DETAILED DESCRIPTION
[0042] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0043] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.
[0044] This embodiment provides a method for tracking and evaluating the anti-skid performance of an asphalt mixture pavement surface. Figure 1 As shown, including:
[0045] Collect texture data of asphalt mixture specimens, including:
[0046] The load, abrasion times, abrasion and scanning direction are preset, and abrasion experiments are carried out on asphalt mixture specimens to collect texture data, wherein the texture data includes micro texture data and macro texture data.
[0047] Furthermore, if Figure 2 As shown, the detection device includes: a loading device, a loading device running track, a scanning device, a scanning device running track, and a slot. The asphalt mixture specimen is placed in the slot. The loading device runs on the asphalt mixture specimen through the loading device running track, and the scanning device runs on the asphalt mixture specimen through the scanning device running track. The scanning device running track is set on the loading device.
[0048] Among them, the card slot is a steel loading card slot, in which a combination of test pieces of different sizes or test pieces for overall paving can be placed. The upper equipment can also be used for testing of actual paved roads, and the tire type can be replaced.
[0049] Loading and wear theory is used to carry out loading and wear experiments based on set load levels, and 3D laser photography sensors are used to obtain 3D point cloud and grayscale image data.
[0050] Convert texture data into grayscale images, and convert grayscale images into binary images;
[0051] Furthermore, before converting the texture data into a grayscale image, the texture data is preprocessed, including:
[0052] The texture data is converted into spectrum data by using fast Fourier transform, and the spectrum data is filtered, wherein the micro texture data is low-pass filtered and the macro texture data is band-pass filtered;
[0053] The filtered spectrum data is subjected to inverse fast Fourier transform to obtain macroscopic and microscopic separated texture data.
[0054] Specifically, the macro / micro textures are separated according to the wavelength range (mm) of the macro / micro textures. The wavelength is converted back to the frequency range (m -1 ), the frequency range of the macro texture is [2,200]m -1 , the frequency range of the micro texture is [200, +∞]m -1 .
[0055]
[0056] For the process of separating macro / micro texture of road surface, first, the spatial data of road surface texture (road surface texture depth matrix) is transformed into spectral data by using Fast Fourier Transform (FFT). FFT is a fast algorithm for discrete Fourier transform, which is obtained by improving the algorithm of discrete Fourier transform according to the characteristics of odd, even, imaginary, and real of discrete Fourier transform. Regarding the road surface texture section as a discrete signal with n data points, the complete texture section curve can be represented by a polynomial as shown in the following formula:
[0057]
[0058] In the formula: a0, a1, a2,..., a n are the coefficients of each term of the polynomial, and x 0 , x 1 , x 2 ,..., x n are n texture sampling points.
[0059] FFT divides the polynomial A(x) into two parts according to the parity of the subscripts as shown in the following formula:
[0060]
[0061] These two parts are respectively denoted as A0(x) and A1(x):
[0062]
[0063]
[0064] At this time, A(x) can be represented by A0(x) and A1(x):
[0065] A(x) = A0(x 2 ) + x * A1(x 2 )
[0066] At this time, A0(x 2 ) and A1(x 2 ) can only take positive values. To solve this problem, FFT introduces the concept of complex numbers. Assuming k < n, x is replaced by the nth root of unity for expression, that is Then A(x) can be expressed as:
[0067]
[0068] For the symmetric signal side It can be expressed as:
[0069]
[0070] According to the principle of multiplying complex numbers, multiplying the modulus length and adding the angle, we can get A(x) and Further changes lead to:
[0071]
[0072]
[0073] At this point, we only need to calculate That is, the value of A(x) can be obtained, and the amount of calculation is reduced by one time compared with Fourier transformation. Therefore, the FFT method can be used to convert the road surface texture data into spectrum data.
[0074] Considering that FFT for 2m -1 It is difficult to achieve such a low cutoff frequency in the following frequency ranges, and the frequency is below 2m -1 The range of is very small and can be ignored. The frequency range of macro texture is adjusted to [0,200]m -1 In addition, the data sampling rate should be greater than twice the highest frequency of the original signal, so as to avoid the occurrence of spectrum aliasing and restore the original signal without distortion. Set the texture section sampling rate to 0.15mm, corresponding to a frequency of 667m -1 . According to the minimum sampling frequency is at least twice the maximum frequency, the corresponding frequency is 1334m -1 , that is, the FFT sampling frequency should be greater than 1334m -1 Through testing, it was found that the upper cut-off frequency is 3846m -1 The micro texture can be better extracted. Therefore, the frequency range of the micro texture is corrected to [200,3846]m -1 The macro texture was filtered using a MATLAB low-pass filter, and the micro texture was filtered using a MATLAB band-pass filter.
[0075] After filtering is completed, the inverse fast Fourier variation (IFFT) is used to transform it back into meaningful texture geometry data. IFFT is equivalent to taking the reciprocal of each unit root. Perform another FFT to convert the frequency domain data back to spatial texture data. The effect of filtering the macro and micro texture separation is as follows: Figure 3 As shown, (a) is a macro texture filtering effect diagram, and (b) is a micro texture filtering effect diagram.
[0076] It can be seen that the separation effect of the road surface macro and micro textures is good, and both achieve a good frequency cutoff at the threshold of their respective frequency ranges. Therefore, it can be seen that the road surface macro and micro texture features restored by inverse fast Fourier transform are real, without distortion due to filtering, and the macro and micro textures are successfully separated.
[0077] Fill the binary image to obtain the apparent texture bonding of the asphalt mixture specimen;
[0078] Furthermore, the binary image is filled to obtain the apparent texture bonding of the asphalt mixture specimen, including:
[0079] The four-connected seed filling algorithm is used to search the connected regions of the binary image to obtain the number of pixels and the number of connected regions in the largest connected region in the binary image.
[0080] The apparent texture bonding of asphalt mixture specimens was quantified based on the number of pixels in the largest connected area and the number of connected areas.
[0081] Specifically, through the observation of asphalt mixture specimens from molding to the wear stage, it was found that when the asphalt mixture was just formed, due to the presence of a large amount of asphalt film on the surface, there was adhesion between the surface aggregates exposed by the asphalt, such as Figure 4 As abrasion occurs, the asphalt film on the surface of the mixture is worn away, and the aggregates are distributed more evenly, as shown in Figure 2. Figure 4 As abrasion continues, the protrusions of the aggregate will be worn away, and the adhesion between the aggregates will begin to reappear, as shown in (b). Figure 4 (c) The three images were taken in similar light source environments and no image brightness adjustment was performed.
[0082] Based on the above analysis, the distribution and adhesion of aggregates on the surface of asphalt mixture are quantitatively described to characterize the different wear stages of asphalt mixture and understand the changes in the distribution of surface aggregates during the wear process.
[0083] The surface image of asphalt mixture is composed of a large amount of black, gray, and white. The black is the color of asphalt and the darker concave parts of the texture; the gray is most of the aggregate; the white is the top reflection of the aggregate and the artificial markings. Therefore, by eliminating human interference, the aggregate distributed on the surface can be distinguished from the color of the image.
[0084] For the texture data collected by laser scanning, the surface texture can be converted into grayscale image data according to the depth. The image data is a data range of distribution [0,1], 1 represents white, 0 represents black, and the interval of 0-1 represents different degrees of gray, such as Figure 5 shown.
[0085] By binarizing the grayscale image, setting a threshold surface, and recording the data above and below the threshold surface as 1 and 0 respectively, a binary image of the road surface texture is obtained, as shown in Figure 6 It can be seen that the distribution of aggregates protruding from the surface can be better obtained for binary images.
[0086] In order to further obtain the size and shape of each aggregate raised area, this embodiment adopts the idea of pixel point region growth and uses the four-connected seed filling algorithm to search for connected regions in the binary image. The four-connected seed filling algorithm is a region filling algorithm based on image processing, which is used to fill the area defined by the specified seed point in the digital image. The algorithm performs pixel-level traversal and judgment on the image, and compares the area of the specified seed point with the adjacent pixels in the four directions around it, thereby achieving the filling operation. The following are the basic steps of the four-connected seed filling algorithm:
[0087] (1) Input: the image to be filled and the coordinates of the seed point. The seed coordinates are created starting from the upper left corner of the image.
[0088] (2) Create a marker image of the same size as the input image to record the filling status of the pixels. Initially, the marker value of all pixels is 0.
[0089] (3) Set the mark value of the seed point to 1, indicating that the point has been filled.
[0090] (4) Initialize an empty seed queue and add the seed point to the queue.
[0091] (5) When the seed queue is not empty, perform the following steps: take a seed point from the queue; check the four adjacent pixels (upper, lower, left, and right) of the seed point; if the adjacent pixel is not filled and has the same color as the seed point, set its mark value to 1 and add it to the seed queue; mark the pixel of the current seed point.
[0092] (6) Repeat step (5) until the seed queue is empty.
[0093] (7) Output the padded image.
[0094] The key to the four-connected seed filling algorithm is to use a queue to manage the seed points to be filled. By continuously expanding the filling area, the algorithm can effectively fill the connected area and ensure that the filled pixels have the same color as the seed points. Through the four-connected seed filling algorithm, the pixel positions of each connected area can be accurately obtained. For example, the maximum connected area found by the four-connected seed filling algorithm is as follows Figure 7 The white part in the middle indicates.
[0095] According to the maximum number of connections (MNC) and the number of connected areas (NCA), the adhesion of the surface texture can be quantified. Since the number of pixels in the maximum connected area and the number of connected areas are not in the same order of magnitude, they are normalized to the range of 0 to 1.
[0096] The connectivity indicator CON (Connectivity) is established as an evaluation indicator of connectivity, as follows:
[0097]
[0098] The structural similarity is calculated based on the grayscale image, and the wear condition of the asphalt mixture specimen is obtained in combination with the apparent texture bonding condition, and the anti-skid performance of the asphalt mixture specimen is further obtained.
[0099] Specifically, the wear index is evaluated based on the multi-scale information input of the grayscale image.
[0100] The structure similarity index measure (SSIM) compares the structural information of two images in the circular area determined by the filter window (window size, WS) from the upper left corner to the lower right corner of the image, thereby calculating their similarity score. The algorithm compares the difference between two depth images based on brightness l, structure S and contrast C, and generates a comprehensive score to determine the difference between the two images. Calculation process:
[0101] SSIM(x,y)=l(x,y) α c(x,y) β s(x,y) γ
[0102] The range of L in the texture image is 400, corresponding to [-200, +200] mm -1 In grayscale images, L is the dynamic range of the pixel grayscale value, which is 255. C1=(K1L) 2 , C2=(K2L) 2 , μ x and μ y is the grayscale mean of images x and y, σ x and σ yis the grayscale variance of images x and y, K1 and K2 are constants much smaller than 1, and α, β, and γ are parameters calculated by optimization.
[0103] The brightness of the line scan image is less affected by the environment and is suitable for analyzing the changes in the sample after wear. The SSIM indicators calculated by texture data of different scales are SSIMi (microtexture similarity index) and SSIMa (macrotexture similarity index), and the SSIM indicator calculated by the grayscale image is SSIMg (grayscale similarity index).
[0104] They reflect the wear changes in different scales and directions, specifically:
[0105] Multi-scale SSIM-T = (SSIMi + SSIMa + SSIMg + CON) / 4
[0106] To further optimize the technical solution, this embodiment also provides a system for tracking and evaluating the anti-skid performance of an asphalt mixture pavement surface, including: a detection module, a processing module, and an evaluation module;
[0107] The detection module is used to collect texture data of the asphalt mixture specimen based on the detection device;
[0108] The processing module is used to process the texture data to obtain a grayscale image and a binary image;
[0109] The evaluation module is used to obtain the apparent texture bonding condition of the asphalt mixture specimen based on the binary image, calculate the structural similarity based on the grayscale image, and perform multi-scale wear condition and anti-skid performance evaluation on the asphalt mixture specimen in combination with the apparent texture bonding condition and structural similarity.
[0110] The method proposed in this embodiment is verified by using asphalt mixture specimens of three specifications: AC-13, SMA-13, and RAP. The changes of the multi-scale SSIM-T index during the loading and abrasion process are shown in the figure. Figure 8 As shown, it is proved that this method can observe the complete decay law of the wear cycle, including the early asphalt film loss texture fluctuation, stable decay and different stages of rapid decay, and can effectively determine the nodes of wear cycle and functional failure.
[0111] The correlation between friction coefficient indicators and multi-scale SSIM-T indicators is as follows: Fig. 9 As shown, it can be seen that the indicators used in this method have a good correlation with the friction coefficient indicators, which further verifies the effectiveness of this method.
[0112] The embodiments described above are only descriptions of the preferred embodiments of the present invention and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should all fall within the protection scope determined by the claims of the present invention.
Claims
1. A method for tracking and evaluating the anti-skid performance of asphalt mixture pavement surface. It is characterized in that include: Collect texture data of asphalt mixture specimens; Converting the texture data into a grayscale image, and converting the grayscale image into a binary image; Filling the binary image to obtain the apparent texture bonding condition of the asphalt mixture specimen; The structural similarity is calculated based on the grayscale image, and the wear condition of the asphalt mixture specimen is obtained in combination with the apparent texture bonding condition, and the anti-skid performance of the asphalt mixture specimen is further obtained.
2. The method for tracking and evaluating the anti-skid performance of asphalt mixture pavement surface according to claim 1, It is characterized in that Collecting the texture data of the asphalt mixture specimen includes: The load, number of abrasions, abrasion and scanning direction are preset, and an abrasion test is performed on the asphalt mixture specimen to collect the texture data, wherein the texture data includes micro texture data and macro texture data.
3. The method for tracking and evaluating the anti-skid performance of asphalt mixture pavement surface according to claim 2, It is characterized in that Before converting the texture data into a grayscale image, the texture data is preprocessed, and the preprocessing includes: The texture data is converted into spectrum data by using fast Fourier transform, and the spectrum data is filtered, wherein the micro texture data is low-pass filtered and the macro texture data is band-pass filtered; The filtered spectrum data is subjected to inverse fast Fourier transform to obtain macroscopic and microscopic separated texture data.
4. The method for tracking and evaluating the anti-skid performance of asphalt mixture pavement surface according to claim 1, It is characterized in that Filling the binary image to obtain the apparent texture bonding condition of the asphalt mixture specimen includes: Using a four-connected seed filling algorithm to search for connected regions in the binary image, and obtaining the number of pixels and the number of connected regions in the largest connected region in the binary image; Based on the number of pixels in the maximum connected area and the number of connected areas, the apparent texture bonding condition of the asphalt mixture specimen is quantified.
5. The method for tracking and evaluating the anti-skid performance of an asphalt mixture pavement surface according to claim 4, It is characterized in that The method for quantifying the apparent texture bonding of the asphalt mixture specimens is: Among them, CON is the connectivity indicator, MNC is the number of pixels in the largest connected area, NCA is the number of connected areas, M is the number of horizontal pixels in the test area, and N is the number of vertical pixels in the test area.
6. The method for tracking and evaluating the anti-skid performance of asphalt mixture pavement surface according to claim 1, It is characterized in that The calculation method of the wear condition of the asphalt mixture specimen is: Multi-scale SSIM-T = (SSIMi + SSIMa + SSIMg + CON) / 4 Among them, SSIMi is the micro texture similarity index, SSIMa is the macro texture similarity index, SSIMg is the grayscale similarity index, and CON is the connectivity index.
7. A system for tracking and evaluating the anti-skid performance of an asphalt mixture pavement surface, used to implement the method for tracking and evaluating the anti-skid performance of an asphalt mixture pavement surface according to any one of claims 1 to 6, It is characterized in that include: Detection module, processing module, and evaluation module; The detection module is used to collect texture data of the asphalt mixture specimen based on the detection device; The processing module is used to process the texture data to obtain a grayscale image and a binary image; The evaluation module is used to obtain the apparent texture bonding condition of the asphalt mixture specimen based on the binary image, calculate the structural similarity based on the grayscale image, and perform multi-scale wear condition and anti-skid performance evaluation on the asphalt mixture specimen in combination with the apparent texture bonding condition and structural similarity.
8. The asphalt mixture pavement surface anti-skid performance tracking and evaluation system according to claim 7, It is characterized in that The detection device includes: a loading device, a loading device running track, a scanning device, a scanning device running track, and a slot. The asphalt mixture specimen is placed in the slot. The loading device runs on the asphalt mixture specimen via the loading device running track. The scanning device runs on the asphalt mixture specimen via the scanning device running track. The scanning device running track is arranged on the loading device.