Plane gate MOSFET integrated with PN junction and Schottky junction and preparation method thereof

By integrating the planar gate structure of PN junction and Schottky junction in MOSFET, the MOSFET body diode free-flow capability is solved by leveraging the low opening voltage and high current characteristics of Schottky diode and combining the forward surge capability of the PN junction diode. The problem of insufficient results has achieved better performance and process advantages.

CN118969738AActive Publication Date: 2024-11-15YANGZHOU YANGJIE ELECTRONIC TECH CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411023043.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-11-15
Estimated Expiration
2044-07-29

AI Technical Summary

Technical Problem

In MOSFETs, it is difficult for the prior art to simultaneously enhance the free-flow capability of the bulk diode and the forward flow capability of the Schottky diode. In addition, the Schottky diode reduces the forward surge capability after replacing the PN junction diode, which makes the preparation process complex And it is difficult to reduce the cell size.

Method used

Using a planar gate MOSFET preparation method that integrates PN junction and Schottky junction, the spaced P body region, N+ region and P channel region are prepared on the epitaxial sheet, and Schottky contact metal is prepared at the bottom of the source trench, combined with Ohmic contact with metal forms the structure of Schottky diode and PN junction diode. The low opening voltage and high current characteristics of Schottky diode reduce the free-current loss of the body diode, and the PN junction diode enhances the forward surge capability to form a super Junction structure to reduce reverse leakage.

Benefits of technology

It realizes the reduction of the free-flow loss of the body diode, enhances the forward surge capability, reduces the reverse leakage of Schottky diodes, and does not affect the forward flow capability, and has better performance and process advantages.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118969738A_ABST
    Figure CN118969738A_ABST
Patent Text Reader

Abstract

The invention relates to a plane gate MOSFET integrated with a PN junction and a Schottky junction and a preparation method thereof. Relates to the technical field of semiconductors. Comprising the following steps: step S100, preparing a plurality of spaced P body regions in an epitaxial wafer, preparing N + regions in the P body regions, and preparing a plurality of spaced P channel regions in the N + regions; s200, preparing a gate medium on the epitaxial wafer, and preparing a plurality of pieces of polycrystalline silicon arranged at intervals on the gate medium above the P channel region; s300, depositing an isolation layer on the epitaxial wafer, and windowing to prepare a source trench which passes through the N + region and extends into the P body region; s400, preparing an N region at the bottom of the source trench, wherein the N region is connected with the N-type voltage-withstanding region of the epitaxial wafer; s500, Schottky contact metal is prepared on the top surface of the N region, Schottky contact is formed between the Schottky contact metal and the N region, and the upper surface of the Schottky contact metal is lower than the lower surface of the N + region; the planar gate MOSFET for enhancing the freewheeling capability of the body diode and the preparation method of the planar gate MOSFET have more excellent performance advantages and process advantages.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a planar gate MOSFET integrating a PN junction and a Schottky junction and a preparation method thereof. Background Art

[0002] In the field of power electronic device technology, MOSFET, as a commonly used power semiconductor, has replaced triode and become one of the most commonly used switching devices in the power semiconductor field.

[0003] After decades of iteration, MOSFET has become one of the mainstream power semiconductor devices. In some applications, the body diode of MOSFET plays an important role in freewheeling. Currently, conventional MOSFET mainly uses PN junction body diode for freewheeling. PN junction body diode has the disadvantages of large turn-on voltage and weak current carrying capacity. Therefore, how to improve the performance of MOSFET body diode has always been a hot topic of research.

[0004] Integrating Schottky diodes in MOSFETs is a solution to improve the performance of MOSFET body diodes. There are currently several patents studying this technology, which generally has its limitations, such as: An article titled "Planar MOSFET with integrated SBD and its process method" was announced on June 25, 2024, with publication number CN118248553A; this patent uses a Schottky diode to replace a PN junction body diode, but the Schottky diode completely replaces the PN junction body diode, which reduces the forward surge capability of the body diode, and the preparation process requires N-type ion implantation of the entire P-Well from the surface of the epitaxial wafer. The N-type ion implantation penetrates the entire P-Well area, which is prone to lateral diffusion and makes it difficult to reduce the cell size.

[0005] An article titled "A SiC planar MOS with source trench integrated SBD and preparation method" was announced on January 2, 2024, with publication number CN117334747A. This patent passes the source trench through the body region and extends it to the voltage-resistant region, and uses the current expansion layer under the MOSFET body region and the Schottky contact metal in the trench to form an SBD. In order to reduce the reverse leakage of the integrated SBD, a P+ shielding layer is prepared under the Schottky contact metal. However, preparing the P+ shielding layer in the voltage-resistant region also weakens the forward current conduction capability of the integrated SBD and the forward current conduction capability of the MOSFET.

[0006] Therefore, integrating Schottky diodes into MOSFETs to improve device performance while enhancing the freewheeling capability of MOSFET body diodes has become a technical challenge that needs to be urgently addressed in the industry. Summary of the invention

[0007] Aiming at the research and development direction of enhancing the freewheeling capability of MOSFET body diode, the present invention invents a planar gate MOSFET integrating PN junction and Schottky junction and a preparation method thereof.

[0008] The technical solution of the present invention is: A method for preparing a planar gate MOSFET integrating a PN junction and a Schottky junction comprises the following steps: Step S100, preparing a plurality of spaced P body regions in the epitaxial wafer, preparing an N+ region in the P body region, and preparing a plurality of spaced P channel regions in the N+ region; Step S200, preparing a gate dielectric on the epitaxial wafer, and preparing a plurality of polysilicon layers spaced apart on the gate dielectric above the P channel region; Step S300, depositing an isolation layer on the epitaxial wafer, and opening a window to prepare a source trench that passes through the N+ region and extends into the P body region; Step S400, preparing an N region at the bottom of the source trench, and connecting the N region to the N-type voltage-resistant region of the epitaxial wafer; Step S500, preparing a Schottky contact metal on the top surface of the N region to form a Schottky contact with the N region, wherein the upper surface of the Schottky contact metal is lower than the lower surface of the N+ region; Step S600, preparing an ohmic contact metal in the source trench to form an ohmic contact with the P body region and the N+ region, and the ohmic contact metal and the Schottky contact metal in the source trench together constitute the source metal; Step S700, opening a window in the polysilicon, preparing a gate metal, and preparing a drain metal on the back of the epitaxial wafer, and the entire device is prepared.

[0009] Specifically, step S100 includes: Step S110, using a photolithography process, using a mask to protect the outer area of ​​the P body region, and forming a plurality of spaced P body regions through a diffusion process or an ion implantation process; Step S120, using a photolithography process, using a mask to protect the area outside the N+ region, and forming the N+ region through a diffusion process or an ion implantation process; Step S130 , using a photolithography process and a mask to protect the outer area of ​​the P-channel region, and forming a plurality of spaced P-channel regions through a diffusion process or an ion implantation process.

[0010] Specifically, step S200 includes: Step S210, preparing a gate dielectric on the epitaxial wafer using a thermal oxidation technique; Step S220 , using a mask to protect the outer area of ​​the P-channel region through a photolithography process, and preparing polysilicon on the gate dielectric above the P-channel region through chemical vapor deposition.

[0011] Specifically, step S300 includes: Step S310, using chemical vapor deposition to prepare an isolation layer, using a mask to protect the outer area of ​​the source trench through a photolithography process, and using an etching process to prepare a source trench, the bottom of the source trench extends to the P body region, and the two side surfaces of the trench are located inside the N+ region.

[0012] Specifically, step S400 includes: Step S410, using a photolithography process and a mask to protect the outer area of ​​the source trench, and preparing an N region at the bottom of the source trench through a diffusion process or an ion implantation process, and connecting the N region to the N-type withstand voltage region of the epitaxial wafer.

[0013] Specifically, step S500 includes: Step S510, using a photolithography process, using a mask to protect the outer area of ​​the source trench, using a stripping process or an etching process, preparing a Schottky contact metal at the bottom of the source trench to form a Schottky contact with the N region, and the upper surface of the Schottky contact metal is lower than the lower surface of the N+ region.

[0014] Specifically, step S600 includes: Step S610, using a photolithography process, using a mask to protect the outer area of ​​the source trench, using a stripping process or an etching process, preparing an ohmic contact metal in the source trench to form an ohmic contact with the P body region and the N+ region. The ohmic contact metal and the Schottky contact metal in the source trench together constitute the source metal.

[0015] Specifically, step S700 includes: Step S710, using a photolithography process, using a mask to protect the outer area of ​​the polysilicon window, using an etching process, opening a window in the polysilicon, and then using a stripping process or an etching process to prepare the gate metal, using a thinning process and a back gold process to prepare the drain metal on the back of the epitaxial wafer, and the entire device is completed.

[0016] A planar gate MOSFET integrating a PN junction and a Schottky junction, comprising a drain metal, an epitaxial wafer, polysilicon and an isolation layer arranged in sequence from bottom to top; The top of the epitaxial wafer is provided with: P body region, provided with a plurality of and spaced from each other; N+ regions are provided in plurality and are spaced apart from each other and extend downward from the top surface of the epitaxial wafer; The P channel region is provided with a plurality of channels, each extending downward from the end of the top surface of the N+ region to the bottom surface of the N+ region; A gate dielectric is disposed on the top surface of the epitaxial wafer; The polysilicon is provided with a plurality of layers which are spaced apart from each other and are respectively located on the top surface of the gate dielectric; The isolation layer is located on the top surface of the polysilicon and the gate dielectric between adjacent polysilicon; An N region, arranged in the P body region, with a bottom surface connected to the N-type voltage-resistant region; A Schottky contact metal extends upward along the top surface of the N region to form a Schottky contact with the N region, and a top surface of the Schottky contact metal is lower than a top surface of the P body region; An ohmic contact metal extends upward along the top surface of the Schottky contact metal, and its top surface is flush with the upper surface of the isolation layer; The gate metal extends downward from the top surface of the isolation layer to the inside of the polysilicon and forms a good ohmic contact with the polysilicon.

[0017] Specifically, the epitaxial wafer includes an N+ substrate layer and an N-type voltage-resistant region from bottom to top.

[0018] Beneficial effects of the present invention: The present invention forms a structure of an integrated Schottky diode and a PN junction diode by preparing a source trench and preparing a Schottky contact at the bottom of the source trench, and uses the low turn-on voltage and high current characteristics of the Schottky diode to achieve the purpose of reducing the body diode freewheeling loss, and uses the PN junction diode to enhance the forward surge capability of the body diode. At the same time, the N region of the Schottky diode of the present invention is flanked by the P body region of the MOSFET, forming a superjunction structure, thereby reducing the reverse leakage of the integrated Schottky diode, and no special additional process steps are required to reduce the reverse leakage of the integrated Schottky diode. The epitaxial layer structure is consistent with the conventional MOSFET structure, and does not affect the forward current flow capability of the integrated SBD and the forward current flow capability of the MOSFET. Compared with the existing comparative documents, the planar gate MOSFET with enhanced body diode freewheeling capability prepared by the present invention and the preparation method thereof have more excellent performance advantages and process advantages. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a process flow chart of the present invention; Figure 2 It is a schematic diagram of the cross-sectional structure of the preparation of the P body region; Figure 3 It is a schematic diagram of the cross-sectional structure of the preparation N+ region; Figure 4 1 is a schematic diagram of the cross-sectional structure of the preparation of the P channel region; Figure 5 It is a schematic diagram of the cross-sectional structure of preparing polycrystalline silicon; Figure 6 Schematic diagram of the cross-sectional structure of the prepared isolation layer; Figure 7 is a schematic diagram of the cross-sectional structure of the device in step S300; Figure 8 is a schematic diagram of the cross-sectional structure of the device in step S400; Fig. 9 is a schematic diagram of the cross-sectional structure of the device in step S500; Fig.10 is a schematic diagram of the cross-sectional structure of the device in step S600; Fig.11 It is a schematic diagram of the cross-sectional structure of the device after the gate metal window is opened; Fig.12 is a schematic diagram of the cross-sectional structure of the device after the gate metal is prepared; Fig.13 is a schematic diagram of the cross-sectional structure of the device after the drain metal is prepared; In the figure, 1 is the epitaxial wafer, 2 is the P body region, 3 is the N+ source region, 4 is the P channel region, 5 is the gate dielectric, 6 is polysilicon, 7 is the isolation layer, 8 is the source trench, 9 is the N region, 10 is the Schottky contact metal, 11 is the ohmic contact metal, 12 is the gate metal window, 13 is the gate metal, 14 is the drain metal, 15 is the N+ substrate region, and 16 is the N-type voltage-resistant region. DETAILED DESCRIPTION

[0020] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0021] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0022] Reference below Figure 1-13 describe the invention; A method for preparing a planar gate MOSFET integrating a PN junction and a Schottky junction comprises the following steps: Step S100, a plurality of spaced P body regions 2 are prepared in the epitaxial wafer 1, an N+ region 3 is prepared in the P body region 2, and a plurality of spaced P channel regions 4 are prepared in the N+ region 3, such as Figure 2 , 3 , as shown in 4; Step S110, using a photolithography process, using a mask to protect the outer area of ​​the P body region 2, and forming a plurality of spaced P body regions 2 through a diffusion process or an ion implantation process; Step S120, using a photolithography process, using a mask to protect the outer area of ​​the N+ region 3, and forming the N+ region 3 through a diffusion process or an ion implantation process; Step S130, using a photolithography process, using a mask to protect the outer area of ​​the P channel region 4, and forming a plurality of spaced P channel regions 4 through a diffusion process or an ion implantation process; Correspondingly, the epitaxial wafer 1 is a Si-based N-type epitaxial wafer, which is composed of an N+ substrate layer 15 and an N-type voltage-resistant region 16 from bottom to top. The thickness of the epitaxial wafer 1 is 100-2000um, the thickness of the N+ substrate layer 15 is 90-1500um, and the thickness of the N-type voltage-resistant region 16 is 10-500um. The thickness of the P body region 2 is 1-20um, the width is 1-20um, and the spacing is 1-10um; The N+ region 3 extends downward from the top surface of the epitaxial wafer 1, and its bottom surface is higher than the bottom surface of the P body region 2, with a thickness of 0.5-10um and a width consistent with that of the P body region 2; The P channel region 4 extends downward from the top surface of the N+ region 3 to the bottom surface of the N+ region 3, is located on both sides of the N+ region 3, has the same thickness as the N+ region 3, and has a width set to 0.25-5um; The doping concentration range of N-type doping is 1e 14 .cm -3 -1e 20 .cm -3 , the doping concentration range of P-type doping is 1e 15 .cm -3 -1e 20 .cm -3 , the relevant parameter settings are related to the electrical design of the device; In this embodiment, the thickness of the epitaxial wafer 1 is 350um, the thickness of the N+ substrate layer 15 is 300um, and the doping concentration is 2e 19 .cm -3 , the thickness of N-type voltage-resistant region 16 is 50um, and the doping concentration is 1e 16 .cm -3 , the thickness of P body region 2 is 5um, the width is 5um, the spacing is 2um, and the doping concentration is 3e 18. cm -3 , N+ region 3 has a thickness of 3um, a width of 5um, and a doping concentration of 2e 19. cm -3 The thickness of the P channel region 4 is 3um, located on both sides of the N+ region 3, the width is 1um, and the doping concentration is 1e 18. cm -3 , use ion implantation process to prepare P body region 2, N+ region 3, and P channel region 4.

[0023] Step S200, preparing a gate dielectric 5 on the epitaxial wafer 1, and preparing a plurality of polysilicon layers 6 arranged at intervals on the gate dielectric 5, such as Figure 5 As shown; Step S210, preparing a gate dielectric 5 on the epitaxial wafer 1 using a thermal oxidation technique; Step S220, using a mask to protect the outer area of ​​the P-channel region 4 through a photolithography process, and preparing polysilicon 6 on the gate dielectric 5 above the P-channel region 4 through chemical vapor deposition; Accordingly, the gate dielectric 5 is made of SiO2, with a thickness of 40-500nm, and the thickness of the polysilicon 6 is set to 100nm-5um; In this embodiment, 80 nm SiO2 is prepared as the gate dielectric 5 by using thermal oxidation technology, and 500 nm polysilicon 6 is prepared by using chemical vapor deposition.

[0024] Step S300, depositing an isolation layer 7 on the epitaxial wafer, opening a window to prepare a source trench 8 that passes through the N+ region 3 and extends into the P body region 2, such as Figure 6 , 7 As shown; Step S310, preparing an isolation layer 7 by chemical vapor deposition, using a mask to protect the outer region of the source trench 8 by photolithography, and preparing the source trench 8 by etching, wherein the bottom of the source trench 8 extends to the inside of the P body region 2, and the two side surfaces of the trench are located inside the N+ region 3; Accordingly, the isolation layer 7 plays a protective role, and the material is SiO2 or Si3N4, and the thickness is set to 10-5000nm. The source trench 8 is prepared by ICP dry etching, and the bottom of the source trench 8 extends to the inside of the P body region 2, and the two sides of the trench are located inside the N+ region 3; In this embodiment, Si3N4 is used as the isolation layer 7, the thickness of which is set to 200 nm, and the source trench 8 is prepared by ICP dry etching. The source trench 8 has a depth of 4.28 um and a width of 2 um.

[0025] Step S400, prepare an N region 9 at the bottom of the source trench 8, and connect the N region 9 to the N-type withstand voltage region 16 of the epitaxial wafer. Figure 8 As shown; Step S410, using a photolithography process, using a mask to protect the outer area of ​​the source trench 8, and preparing an N region 9 at the bottom of the source trench 8 by a diffusion process or an ion implantation process, and connecting the N region 9 to the N-type withstand voltage region 16 of the epitaxial wafer; Correspondingly, the doping concentration range of N-type doping is 1e 14 .cm -3 -1e 20 .cm -3 ; In this embodiment, the doping concentration of N region 9 is 1e 16 .cm -3 , the N region 9 is prepared using an ion implantation process.

[0026] Step S500, a Schottky contact metal 10 is prepared on the top surface of the N region 9 to form a Schottky contact with the N region 9, and the upper surface of the Schottky contact metal 10 is lower than the lower surface of the N+ region 3, such as Fig. 9 As shown; Step S510, using a photolithography process, using a mask to protect the outer area of ​​the source trench 8, using a stripping process or an etching process, preparing a Schottky contact metal 10 in the source trench 8 to form a Schottky contact with the N region 9, and the upper surface of the Schottky contact metal 10 is lower than the lower surface of the N+ region 3; Correspondingly, the Schottky contact metal 10 is arranged at the bottom of the source trench 8 to form a Schottky contact with the N region 9, and its upper surface is lower than the lower surface of the N+ region 3; In this embodiment, a lift-off process is used to prepare a 200 nm thick Ni / Al two-layer metal at the bottom of the source trench 8 as the Schottky contact metal 9 , and the Ni and N region 9 form a Schottky contact.

[0027] Step S600, preparing an ohmic contact metal 11 in the source trench 8 to form an ohmic contact with the P body region 2 and the N+ region 3. The ohmic contact metal 11 in the source trench 8 and the Schottky contact metal 10 together form a source metal. Fig.10 As shown; Step S610, using a photolithography process, using a mask to protect the outer area of ​​the source trench 8, using a stripping process or an etching process, preparing an ohmic contact metal 11 in the source trench 8, forming an ohmic contact with the P body region 2 and the N+ region 3, and the ohmic contact metal 11 in the source trench and the Schottky contact metal 10 together constitute the source metal; Correspondingly, the ohmic contact metal 11 is arranged inside the source trench 8, with its lower surface in contact with the upper surface of the Schottky contact metal 10, and its upper surface flush with the upper surface of the isolation layer 7, forming an ohmic contact with the P body region 2 and the N+ region 3; In this embodiment, a lift-off process is used to prepare a 4.08 um thick Ti / Al two-layer metal in the source trench 8 as the ohmic contact metal 11 , and Ti forms an ohmic contact with the P body region 2 and the N+ region 3 .

[0028] Step S700, a window is opened at the polysilicon 6, a gate metal 13 is prepared, and a drain metal 14 is prepared on the back of the epitaxial wafer 1. The whole device is prepared. Figure 11-13 shown.

[0029] Step S710, using a photolithography process, using a mask to protect the outer area of ​​the polysilicon 6 where the window is opened, using an etching process, opening a window in the polysilicon 6, and then using a stripping process or an etching process to prepare the gate metal 13, using a thinning process and a back gold process to prepare the drain metal 14 on the back of the epitaxial wafer 1, and the entire device is completed.

[0030] Correspondingly, the window depth of the polysilicon 6 is greater than the thickness of the isolation layer 7, the gate metal 13 extends downward from the top surface of the isolation layer 7 into the polysilicon 6, and forms an ohmic contact with the polysilicon 6, and the drain metal 14 forms an ohmic contact with the N+ substrate layer 15 on the bottom surface of the epitaxial wafer 1; In this embodiment, a window is opened at the polysilicon 6 through an etching process, and the window depth is 1um. A stripping process is used to prepare a 1um thick Ti / Al two-layer metal as a gate metal 13 to form an ohmic contact with the polysilicon 6. A thinning process is used to thin the 350um thick epitaxial wafer 1 to 180um, and the Ti / Al two-layer metal is used to prepare the drain metal 14.

[0031] A planar gate MOSFET integrating a PN junction and a Schottky junction comprises a drain metal 14, an epitaxial wafer 1, a polysilicon 6 and an isolation layer 7 arranged in sequence from bottom to top; The top of the epitaxial wafer 1 is provided with: The P-body regions 2 are provided in a plurality and are spaced apart from each other, and the top surface thereof is lower than the top surface of the epitaxial wafer 1, and the bottom surface thereof is higher than the bottom surface of the N-type voltage-resistant region 16; N+ regions 3 are provided in plurality and are spaced apart from each other, respectively extending downward from the top surface of the epitaxial wafer 1, and the bottom surface of the N+ regions 3 is higher than the bottom surface of the P body region 2; The P channel region 4 is provided with a plurality of P channel regions 4, each extending downward from the end of the top surface of the N+ region 3 to the bottom surface of the N+ region 3; the side of the P channel region 4 away from the N+ region 3 is in the same plane as the side surface of the P body region 2; A gate dielectric 5 is arranged on the top surface of the epitaxial wafer 1; The polysilicon 6 is provided with a plurality of layers spaced apart from each other and respectively located on the top surface of the gate dielectric 5; The isolation layer 7 is located on the top surface of the polysilicon 6 and on the gate dielectric 5 between adjacent polysilicon 6; N region 9, arranged in the P body region 2, with a bottom surface connected to the N type voltage-resistant region 16, a side portion connected to the P body region 2, and a top surface lower than a top surface of the P body region 2; A Schottky contact metal 10 extends upward along the top surface of the N region 9 to form a Schottky contact with the N region 9, and a top surface thereof is lower than a top surface of the P body region 2; The ohmic contact metal 11 extends upward along the top surface of the Schottky contact metal 10, and its top surface is flush with the upper surface of the isolation layer 7; the ohmic contact metal 11 forms an ohmic contact with the P body region 2 and the N+ region 3 on the side, and the ohmic contact metal 11 and the Schottky contact metal 10 in the source trench 8 together constitute a source metal; The gate metal 13 extends downward from the top surface of the isolation layer 7 to the inside of the polysilicon 6 , and forms a good ohmic contact with the polysilicon 6 .

[0032] The epitaxial wafer 1 is a Si-based N-type epitaxial wafer, and is composed of an N+ substrate layer 15 and an N-type voltage-resistant region 16 from bottom to top. The drain metal 14 and the N+ substrate layer 15 of the epitaxial wafer 1 form a good ohmic contact.

[0033] The present invention forms a structure of an integrated Schottky diode and a PN junction diode by preparing a source trench 8 and preparing a Schottky contact at the bottom of the source trench 8, and utilizes the low turn-on voltage and high current characteristics of the Schottky diode to achieve the purpose of reducing the body diode freewheeling loss, and utilizes the PN junction diode to enhance the forward surge capability of the body diode. At the same time, the N region 9 of the Schottky diode of the present invention is flanked by the P body region 2 of the MOSFET, forming a superjunction structure, thereby reducing the reverse leakage of the integrated Schottky diode, and no special additional process steps are required to reduce the reverse leakage of the integrated Schottky diode. The epitaxial layer structure is consistent with the conventional MOSFET structure, and does not affect the forward current flow capability of the integrated SBD and the forward current flow capability of the MOSFET. Compared with the existing comparative documents, the planar gate MOSFET with enhanced body diode freewheeling capability prepared by the present invention and the preparation method thereof have more excellent performance advantages and process advantages.

[0034] Regarding the contents disclosed in this case, there are a few points that need to be explained: The drawings of the embodiments disclosed in this case only involve the structures involved in the embodiments disclosed in this case, and other structures can refer to the usual designs; In the absence of conflict, the embodiments and features of the embodiments disclosed in this case can be combined with each other to obtain new embodiments; The above are only specific implementation methods disclosed in this case, but the protection scope of the present disclosure is not limited thereto. The protection scope disclosed in this case should be based on the protection scope of the claims.

Claims

1. A method for preparing a planar gate MOSFET integrating a PN junction and a Schottky junction, characterized in that: The following steps are involved: Step S100, preparing a plurality of spaced P body regions (2) in the epitaxial wafer (1), preparing an N+ region (3) in the P body region (2), and preparing a plurality of spaced P channel regions (4) in the N+ region (3); Step S200, preparing a gate dielectric (5) on the epitaxial wafer (1), and preparing a plurality of polysilicon (6) spaced apart on the gate dielectric (5) above the P channel region (4); Step S300, depositing an isolation layer (7) on the epitaxial wafer, and opening a window to prepare a source trench (8) that passes through the N+ region (3) and extends into the P body region (2); Step S400, preparing an N region (9) at the bottom of the source trench (8), and connecting the N region (9) to the N-type voltage-resistant region (16) of the epitaxial wafer; Step S500, preparing a Schottky contact metal (10) on the top surface of the N region (9) to form a Schottky contact with the N region (9), wherein the upper surface of the Schottky contact metal (10) is lower than the lower surface of the N+ region (3); Step S600, preparing an ohmic contact metal (11) in the source trench (8) to form an ohmic contact with the P body region (2) and the N+ region (3), wherein the ohmic contact metal (11) in the source trench and the Schottky contact metal (10) together constitute a source metal; Step S700, opening a window at the polysilicon (6), preparing a gate metal (13), and preparing a drain metal (14) on the back of the epitaxial wafer (1), and the entire device is prepared.

2. The method for preparing a planar gate MOSFET with integrated PN junction and Schottky junction according to claim 1, characterized in that: Step S100 includes: Step S110, using a photolithography process and a mask to protect the outer area of ​​the P body region (2), and forming a plurality of spaced P body regions (2) through a diffusion process or an ion implantation process; Step S120, using a photolithography process and a mask to protect the outer area of ​​the N+ region (3), and forming the N+ region (3) through a diffusion process or an ion implantation process; Step S130, using a photolithography process and a mask to protect the outer area of ​​the P-channel region (4), and forming a plurality of spaced P-channel regions (4) through a diffusion process or an ion implantation process.

3. The method for preparing a planar gate MOSFET integrating a PN junction and a Schottky junction according to claim 1, characterized in that: Step S200 includes: Step S210, preparing a gate dielectric (5) on the epitaxial wafer (1) using a thermal oxidation technique; Step S220: Protect the outer area of ​​the P-channel region (4) by using a mask through a photolithography process, and prepare polysilicon (6) on the gate dielectric (5) above the P-channel region (4) through chemical vapor deposition.

4. The method for preparing a planar gate MOSFET integrating a PN junction and a Schottky junction according to claim 1, characterized in that: Step S300 includes: Step S310, using chemical vapor deposition to prepare an isolation layer (7), using a photolithography process to protect the outer region of the source trench (8) using a mask, and using an etching process to prepare the source trench (8), the bottom of the source trench (8) extending to the P body region (2), and the two side surfaces of the trench being located inside the N+ region (3).

5. The method for preparing a planar gate MOSFET integrating a PN junction and a Schottky junction according to claim 1, characterized in that: Step S400 includes: Step S410, using a photolithography process and a mask to protect the outer region of the source trench (8), preparing an N region (9) at the bottom of the source trench (8) through a diffusion process or an ion implantation process, and connecting the N region (9) to the N-type withstand voltage region (16) of the epitaxial wafer.

6. The method for preparing a planar gate MOSFET integrating a PN junction and a Schottky junction according to claim 1, characterized in that: Step S500 includes: Step S510, using a photolithography process, using a mask to protect the outer area of ​​the source trench (8), using a stripping process or an etching process, preparing a Schottky contact metal (10) at the bottom of the source trench (8) to form a Schottky contact with the N region (9), and the upper surface of the Schottky contact metal (10) is lower than the lower surface of the N+ region (3).

7. The method for preparing a planar gate MOSFET integrating a PN junction and a Schottky junction according to claim 1, characterized in that: Step S600 includes: Step S610, using a photolithography process, using a mask to protect the outer area of ​​the source trench (8), using a stripping process or an etching process, preparing an ohmic contact metal (11) in the source trench (8), forming an ohmic contact with the P body region (2) and the N+ region (3), and the ohmic contact metal (11) in the source trench and the Schottky contact metal (10) together constitute the source metal.

8. The method for preparing a planar gate MOSFET integrating a PN junction and a Schottky junction according to claim 1, characterized in that: Step S700 includes: Step S710, using a photolithography process, using a mask to protect the outer area of ​​the polysilicon (6) where the window is opened, using an etching process, opening a window at the polysilicon (6), then using a stripping process or an etching process to prepare a gate metal (13), using a thinning process and a back gold process to prepare a drain metal (14) on the back of the epitaxial wafer (1), and the entire device is prepared.

9. A planar gate MOSFET with integrated PN junction and Schottky junction, prepared by the method for preparing a planar gate MOSFET with integrated PN junction and Schottky junction according to any one of claims 1 to 9, characterized in that: It comprises a drain metal (14), an epitaxial wafer (1), polysilicon (6) and an isolation layer (7) which are arranged in sequence from bottom to top; The top of the epitaxial wafer (1) is provided with: P body region (2), provided with a plurality of mutually spaced apart; A plurality of N+ regions (3) are provided and spaced apart from each other, and are respectively provided downward from the top surface of the epitaxial wafer (1); The P channel region (4) is provided with a plurality of P channel regions, each extending downward from the end of the top surface of the N+ region (3) to the bottom surface of the N+ region (3); A gate dielectric (5) arranged on the top surface of the epitaxial wafer (1); The polysilicon (6) is provided with a plurality of layers which are spaced apart from each other and are respectively located on the top surface of the gate dielectric (5); The isolation layer (7) is located on the top surface of the polysilicon (6) and on the gate dielectric (5) between adjacent polysilicon (6); An N region (9) arranged in the P body region (2), the bottom surface of which is connected to the N-type voltage-resistant region (16); A Schottky contact metal (10) extends upward along the top surface of the N region (9) to form a Schottky contact with the N region (9), and its top surface is lower than the top surface of the P body region (2); An ohmic contact metal (11) extending upward along the top surface of the Schottky contact metal (10), wherein the top surface of the ohmic contact metal (11) is flush with the upper surface of the isolation layer (7); The gate metal (13) extends downward from the top surface of the isolation layer (7) to the inside of the polysilicon (6), and forms a good ohmic contact with the polysilicon (6).

10. The planar gate MOSFET integrating PN junction and Schottky junction according to claim 9, characterized in that: The epitaxial wafer (1) comprises, from bottom to top, an N+ substrate layer (15) and an N-type voltage-resistant region (16).

Citation Information

Patent Citations

  • Silicon carbide trench gate MOSFET device integrated with SBD and manufacturing method thereof

    CN116632065A

  • Planar gate type MOSFET integrated with Schottky diode and preparation method of planar gate type MOSFET

    CN117878142A

  • High voltage MOSFET diode reverse recovery by minimizing P-body charges

    US20110073906A1

  • Mixed trench junction barrier schottky diode and method fabricating same

    US20200119158A1