MOSFET (Metal-Oxide-Semiconductor Field Effect Transistor) for enhancing follow current capability of body diode and preparation
By fabricating a first heavily doped body region in the MOSFET and controlling the source trench depth, a Schottky contact diode is integrated to form a superjunction structure. This solves the problem of insufficient freewheeling capability of the body diode, reduces freewheeling loss and reverse leakage current, and enhances the commercial potential of the MOSFET.
Patent Information
- Application Number
- CN202411023038.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-07-29
AI Technical Summary
Existing technologies in MOSFETs with integrated Schottky diodes suffer from insufficient body diode freewheeling capability and additional process steps, which affect forward current carrying capacity and increase reverse leakage current.
By fabricating a first heavily doped body region within the epitaxial wafer and controlling the depth of the source trench, a Schottky contact diode is integrated at the bottom of the source trench to form a superjunction structure. The low turn-on voltage and high current characteristics of the Schottky diode are utilized to reduce the freewheeling loss of the body diode. Furthermore, two process steps, namely the source trench and the Schottky contact metal, are added to the fabrication process.
This technology reduces body diode freewheeling loss and reverse leakage current while maintaining forward current carrying capacity, thereby enhancing the commercial value of MOSFETs without adding extra process steps.
Smart Images

Figure CN118969737A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a MOSFET with enhanced body diode freewheeling capability and a preparation method thereof. Background Art
[0002] In the field of power electronic device technology, MOSFET, as a commonly used power semiconductor, has replaced triode and become one of the most commonly used switching devices in the power semiconductor field.
[0003] During the decades of iteration of MOSFET, the freewheeling capability of the body diode has received more and more attention. Currently, an important technology to improve the freewheeling capability of the body diode is to integrate a Schottky diode, which utilizes the low turn-on voltage and high current characteristics of the Schottky diode to reduce the freewheeling loss of the body diode.
[0004] At present, there are related patents for MOSFETs with integrated Schottky diodes. The patent with publication number CN117334748A discloses a source trench integrated SBD and HK dielectric SiCUMOS and a preparation method. This method passes the source trench through the body region and extends it to the withstand voltage region. The current expansion layer under the MOSFET body region and the Schottky contact metal in the trench form the SBD. In order to reduce the reverse leakage of the integrated SBD, a high-K dielectric is prepared under the Schottky contact metal. However, the solution is relatively different from that of ordinary trench MOS. First, an additional process step is required to prepare a current expansion layer to reduce the on-resistance of the SBD. Second, preparing a high-K dielectric under the Schottky contact metal can reduce the reverse leakage of the integrated SBD, but it also weakens the forward current capacity of the integrated SBD and the forward current capacity of the MOSFET, and additional process steps are also required. Other patent documents such as publication numbers CN117334746A, CN117334747A, CN117334745A, and CN110473914B have similar shortcomings. Summary of the invention
[0005] Aiming at the research and development direction of improving the freewheeling capability of the body diode, the present invention provides a MOSFET with enhanced freewheeling capability of the body diode and a preparation method thereof, thereby reducing the process steps and the process difficulty. Without affecting the forward current conduction capability of the integrated SBD and the forward current conduction capability of the MOSFET device, the reverse leakage of the integrated SBD is reduced.
[0006] The technical solution of the present invention is: A method for preparing a MOSFET with enhanced body diode freewheeling capability comprises the following steps: Step S100, preparing mutually spaced first heavily doped body regions in the epitaxial wafer; Step S200, preparing a second heavily doped source region in the epitaxial wafer; Step S300, preparing a gate trench in the epitaxial wafer; Step S400, sequentially preparing a gate dielectric and polysilicon in the trench; Step S500, depositing an isolation layer on the epitaxial wafer, opening a window to prepare a source trench, wherein the bottom of the source trench extends to the inside of the first heavily doped body region, and the trench width is greater than the spacing width of the first heavily doped body region; Step S600, preparing a Schottky contact metal at the bottom of the source trench to form a Schottky contact with the second lightly doped voltage-resistant region, wherein the upper surface of the Schottky contact metal is lower than the lower surface of the second heavily doped source region; Step S700, preparing an ohmic contact metal in the source trench to form an ohmic contact with the first heavily doped body region and the second heavily doped source region, and the ohmic contact metal and the Schottky contact metal in the source trench together constitute a source metal; Step S800, opening a window at the gate trench, preparing gate metal, and preparing drain metal on the back of the epitaxial wafer, and the entire device is prepared.
[0007] Specifically, step S100 includes: Step S110: adopting a photolithography process and using a mask to protect the outer area of the first heavily doped body region; and forming mutually spaced first heavily doped body regions through a diffusion process or an ion implantation process.
[0008] Specifically, step S200 includes: Step S210: adopting a photolithography process and using a mask to protect the outer area of the second heavily doped source region; and forming the second heavily doped source region by a diffusion process or an ion implantation process.
[0009] Specifically, step S300 includes: Step S310, using a photolithography process and a mask to protect the outer area of the gate trench; and forming the gate trench by an etching process; Specifically, step S400 includes: Step S410, using a mask to protect the outer area of the gate trench through a photolithography process, and using a thermal oxidation technology to prepare a gate dielectric in the gate trench; Step S420 , preparing polysilicon in the gate trench by chemical vapor deposition.
[0010] Specifically, step S500 includes: Step S510, preparing an isolation layer by chemical vapor deposition, protecting the outer region of the source trench by a photolithography process using a mask, and opening a window at the source trench by an etching process, wherein the bottom of the source trench extends to the inside of the first heavily doped body region, and the trench width is greater than the spacing width of the first heavily doped body region; Specifically, step S600 includes: Step S610, preparing a Schottky contact metal at the bottom of the source trench by a stripping process or an etching process, the Schottky contact metal forms a Schottky contact with the second lightly doped voltage-withstand region, and the upper surface of the Schottky contact metal is lower than the lower surface of the second heavily doped source region; Specifically, step S700 includes: Step S710, preparing an ohmic contact metal in the source trench by a stripping process or an etching process, the ohmic contact metal forms an ohmic contact with the first heavily doped body region and the second heavily doped source region, and the ohmic contact metal and the Schottky contact metal in the source trench together constitute a source metal; Specifically, step S800 includes: Step S810, using a mask to protect the outer area of the gate trench window through a photolithography process, opening a window at the gate trench through an etching process, and preparing a gate metal, and preparing a drain metal at the bottom of the epitaxial wafer through a thinning process and a back-gold process, and the entire device is prepared; A MOSFET with enhanced freewheeling capability of a body diode, comprising a drain metal, an epitaxial wafer and an isolation layer arranged in sequence from bottom to top; The epitaxial wafer is provided with: A plurality of first heavily doped body regions are provided, extending downward from the top of the epitaxial wafer and spaced apart from each other; the bottom surface of the first heavily doped body region is higher than the bottom surface of the second lightly doped voltage-resistant region; a second heavily doped source region extending downward from the top surface of the epitaxial wafer and connected to the top surface of the first heavily doped body region; A plurality of gate dielectrics are provided, and the cross-section is U-shaped, and each of them extends downward from the top surface of the second heavily doped source region, passes through the first heavily doped body region, and extends into the second lightly doped voltage-resistant region; Polysilicon, extending downward from the top surface of the gate dielectric to fill the gate dielectric; A Schottky contact metal is disposed between adjacent first heavily doped body regions, and an end portion thereof extends into the first heavily doped body region; the Schottky contact metal is connected to the second lightly doped voltage-withstand region to form a Schottky contact; an upper surface of the Schottky contact metal is lower than a lower surface of the second heavily doped source region; An ohmic contact metal extending upward from the top surface of the Schottky contact metal and sequentially passing through the first heavily doped body region, the second heavily doped source region and the isolation layer; A gate metal extends downward from the top surface of the isolation layer into the polysilicon to form an ohmic contact with the polysilicon; The first doping region and the second doping region have opposite doping types, namely, a P region and an N region, or an N region and a P region, respectively.
[0011] Beneficial effects of the present invention: The present invention integrates a Schottky contact diode at the bottom of the source trench by preparing an interval of first heavily doped body regions and controlling the source trench depth, and utilizes the low turn-on voltage and high current characteristics of the Schottky diode to achieve the purpose of reducing the body diode freewheeling loss. At the same time, the second lightly doped voltage-resistant region of the Schottky diode of the present invention is flanked by the interval of first heavily doped body regions, forming a super junction structure of the first heavily doped body region, the second lightly doped voltage-resistant region, and the first heavily doped body region. The super junction structure has an excellent shielding effect, effectively reduces the electric field strength of the second lightly doped voltage-resistant region, and thereby reduces the reverse leakage of the integrated Schottky diode.
[0012] The structure of the second lightly doped voltage-withstand region below the first heavily doped body region of the device of the present invention is consistent with that of an ordinary trench MOSFET, and no special additional process steps are required to reduce the reverse leakage of the integrated Schottky diode. The preparation process of the present invention is fully compatible with the preparation process of a traditional trench MOSFET, and only two additional process steps of preparing a source trench and a Schottky contact metal are required. Compared with existing comparative documents, the special additional process steps are reduced to reduce the reverse leakage of the integrated Schottky diode, and the forward current conduction capacity of the integrated SBD and the forward current conduction capacity of the MOSFET are not affected, which is conducive to the advancement of the commercialization process and has higher commercial value. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 It is a process flow chart of the present invention; Figure 2 is a schematic diagram of the cross-sectional structure of the device in step S100; Figure 3 is a schematic diagram of the cross-sectional structure of the device in step S200; Figure 4 is a schematic diagram of the cross-sectional structure of the device in step S300; Figure 5 It is a schematic diagram of the structure of preparing a gate dielectric in a trench; Figure 6 It is a schematic diagram of the structure of preparing polysilicon in the trench; Figure 7 is a schematic diagram of the cross-sectional structure of the preparation of the isolation layer; Figure 8 is a schematic diagram of a cross-sectional structure for preparing a source trench; Fig. 9 is a schematic diagram of a structure for preparing a Schottky contact metal at the bottom of a source trench; Fig.10 It is a schematic diagram of the structure for preparing ohmic contact metal inside the source trench; Fig.11 is a schematic diagram of the cross-sectional structure of the gate metal window; Fig.12is a schematic diagram of the cross-sectional structure of the gate metal; Fig.13 is a schematic diagram of the structure for preparing drain metal; In the figure, 1 is the epitaxial wafer, 2 is the first heavily doped body region, 3 is the second heavily doped source region, 4 is the gate trench, 5 is the gate dielectric, 6 is polysilicon, 7 is the isolation layer, 8 is the source trench, 9 is the Schottky contact metal, 10 is the ohmic contact metal, 11 is the gate metal window, 12 is the gate metal, 13 is the drain metal, 14 is the second heavily doped substrate region, and 15 is the second lightly doped voltage-resistant region. DETAILED DESCRIPTION
[0014] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0015] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0016] Reference below Figure 1-13 describe the invention; Step S100, preparing a plurality of mutually spaced first heavily doped body regions 2 in the epitaxial wafer 1, referring to Figure 2 As shown; Step S110, using a photolithography process and a mask to protect the outer area of the first heavily doped body region 2; forming mutually spaced first heavily doped body regions 2 by a diffusion process or an ion implantation process; The first doping region and the second doping region are of opposite doping types, namely, a P region and an N region, or an N region and a P region, respectively. Preferably, the first doping region (including the first heavily doped body region 2) is a P region, and the second doping region (including the second heavily doped source region 3, the second heavily doped substrate region 14, and the second lightly doped withstand voltage region 15) is an N region.
[0017] Accordingly, the epitaxial wafer 1 of this embodiment is a Si-based N-type epitaxial wafer; The epitaxial wafer 1 is composed of a second heavily doped substrate region 14 and a second lightly doped voltage-resistant region 15 from bottom to top. The thickness of the epitaxial wafer 1 is 100-2000um, the thickness of the second heavily doped substrate region 14 is 90-1500um, the thickness of the second lightly doped voltage-resistant region 15 is 10-500um, the thickness of the first heavily doped body region 2 is 1-5um, the spacing distance is set to 1-10um, and the doping concentration range of the N-type doping is 1e 14 .cm -3 -1e 20 .cm -3 , the doping concentration range of P-type doping is 1e 15 .cm -3 -1e 20 .cm -3 , the relevant parameter settings are related to the electrical design of the device; In this embodiment, the thickness of the epitaxial wafer 1 is 350 um, the thickness of the second heavily doped substrate region 14 is 330 um, and the doping concentration is 1e 19 .cm -3 The second lightly doped voltage-resistant region 15 has a thickness of 20 μm and a doping concentration of 1e 16 .cm -3 The thickness of the first heavily doped region 2 is 2um, the spacing is 1um, and the doping concentration is 3e 18 .cm -3 , a first heavily doped body region 2 is prepared using an ion implantation process.
[0018] Step S200, preparing a second heavily doped source region 3 in the epitaxial wafer 1, referring to Figure 3 As shown; Step S210, using a photolithography process and a mask to protect the outer area of the second heavily doped source region 3; forming the second heavily doped source region 3 by a diffusion process or an ion implantation process; Correspondingly, the second heavily doped source region 3 extends downward from the top surface of the first heavily doped body region 2, and its bottom surface is higher than the bottom surface of the first heavily doped body region 2. The thickness is set to 0.5-3um, and the doping concentration range is 1e 18 .cm -3 -1e 20 .cm -3 , the relevant parameter settings are related to the electrical design of the device; In this embodiment, the thickness of the second heavily doped source region 3 is 1 um, and the doping concentration is 1e 19. cm -3 , a second heavily doped source region 3 is prepared using an ion implantation process.
[0019] Step S300, preparing a gate trench 4 in the epitaxial wafer 1, which passes through the second heavily doped source region 3 and the first heavily doped body region 2 in sequence downward, referring to Figure 4 As shown; Step S310, using a photolithography process and a mask to protect the outer area of the gate trench 4; and forming the gate trench 4 by an etching process; Accordingly, the gate trench 4 extends downward from the top surface of the epitaxial wafer 1, and its bottom surface is lower than the bottom surface of the first heavily doped body region 2 and higher than the bottom surface of the second lightly doped voltage-resistant region 15, and the width range is set to 1-10um, and the relevant parameter settings are related to the device electrical design; In this embodiment, the gate trench 4 has a depth of 4 um and a width of 2 um, and the trench 4 is prepared by using an ICP dry etching process.
[0020] Step S400, sequentially preparing a gate dielectric 5 and polysilicon 6 in the gate trench 4, referring to Figure 5 , Figure 6 As shown; Step S410, using a mask to protect the outer area of the gate trench 4 through a photolithography process, and using a thermal oxidation technique to prepare a gate dielectric 5 in the gate trench 4; Step S420, preparing polysilicon 6 in the gate trench 4 by chemical vapor deposition; Correspondingly, the gate dielectric 5 is located in the trench 4, and is in contact with the second heavily doped source region 3, the first heavily doped body region 2, and the second lightly doped voltage-resistant region 15, respectively. The polysilicon 6 is located in the trench 4, fills the trench 4, and is in contact with the gate dielectric 5. The upper surface of the polysilicon 6 is level with the upper surface of the gate trench 4. The gate dielectric 5 is made of SiO2, and the thickness is set to 40-500nm. In this embodiment, 80 nm SiO2 is prepared as the gate dielectric 5 by using thermal oxidation technology, and polysilicon 6 is prepared by using chemical vapor deposition.
[0021] Step S500, depositing an isolation layer 7 on the epitaxial wafer 1, and opening a window to prepare a source trench 8, the bottom of the source trench 8 extends to the inside of the adjacent first heavily doped body region 2, and the trench width is greater than the spacing width of the first heavily doped body region 2, referring to Figure 7 , Figure 8 As shown; Step S510, preparing an isolation layer 7 by chemical vapor deposition, using a mask to protect the outer area of the source trench 8 by photolithography, and opening a window at the source trench 8 by etching, wherein the bottom of the source trench 8 extends to the inside of the first heavily doped body region 2, and the trench width is greater than the spacing width of the first heavily doped body region 2; Accordingly, the isolation layer 7 plays a protective role, and the material is SiO2 or Si3N4, and the thickness is set to 10-5000nm. The source trench 8 is prepared by ICP dry etching, and the source trench 8 extends downward from the top surface of the isolation layer 7 to the inside of the first heavily doped body region 2, and its bottom surface is higher than the bottom surface of the first heavily doped body region 2. The groove width is greater than the spacing width of the first heavily doped body region 2, and the width range is set to 1-10um. The relevant parameter settings are related to the device electrical design; In this embodiment, Si3N4 is used as the isolation layer 7, the thickness of which is set to 200 nm, and ICP dry etching is used to open a window to prepare a source trench 8. The source trench 8 has a depth of 2 um and a width of 1.5 um. The source trench 8 is prepared using an ICP dry etching process.
[0022] Step S600, a Schottky contact metal 9 is prepared at the bottom of the source trench 8 to form a Schottky contact with the second lightly doped voltage-resistant region 15. The upper surface of the Schottky contact metal 9 is lower than the lower surface of the second heavily doped source region 3. Fig. 9 As shown; Step S610, preparing a Schottky contact metal 9 at the bottom of the source trench 8 by a stripping process or an etching process, the Schottky contact metal 9 forms a Schottky contact with the second lightly doped voltage-resistant region 15, and the upper surface of the Schottky contact metal 9 is lower than the lower surface of the second heavily doped source region 3; Correspondingly, the Schottky contact metal 9 is arranged at the bottom of the source trench 8 to form a Schottky contact with the second lightly doped voltage-resistant region 15, and its upper surface is lower than the lower surface of the second heavily doped source region 3; In this embodiment, a lift-off process is used to prepare two layers of Ni / Al metal with a thickness of 200 nm at the bottom of the source trench 8 as Schottky contact metal 9 , and Ni and the second lightly doped voltage-resistant region 15 form a Schottky contact.
[0023] Step S700, preparing an ohmic contact metal 10 in the source trench 8 to form an ohmic contact with the first heavily doped body region 2 and the second heavily doped source region 3. The ohmic contact metal 10 in the source trench and the Schottky contact metal 9 together form a source metal. Fig.10 As shown; Step S710, preparing an ohmic contact metal 10 in the source trench 8 by a stripping process or an etching process, the ohmic contact metal 10 forms an ohmic contact with the first heavily doped body region 2 and the second heavily doped source region 3, and the ohmic contact metal 10 in the source trench and the Schottky contact metal 9 together constitute a source metal; Accordingly, the ohmic contact metal 10 is disposed inside the source trench 8, with its lower surface being level with the Schottky contact metal 9 and its upper surface being level with the upper surface of the isolation layer 7, forming an ohmic contact with the first heavily doped body region 2 and the second heavily doped source region 3; In this embodiment, a lift-off process is used to prepare a 1.8 um thick Ti / Al two-layer metal in the source trench 8 as the ohmic contact metal 10 , and Ti forms an ohmic contact with the first heavily doped body region 2 and the second heavily doped source region 3 .
[0024] Step S800, a window is opened at the gate trench 4, a gate metal 12 is prepared, and a drain metal 13 is prepared on the back of the epitaxial wafer 1. The entire device is prepared. Fig.11 , Fig.12 , Fig.13 shown.
[0025] Step S810, using a mask to protect the outer area of the gate trench 4 at the window opening by photolithography, opening a window at the gate trench 4 by etching, and preparing the gate metal 12, and preparing the drain metal 13 at the bottom of the epitaxial wafer 1 by thinning and back-gold processes, and the entire device is prepared; Correspondingly, the window depth at the gate trench 4 is greater than the thickness of the isolation layer 7, the gate metal 12 extends downward from the top surface of the isolation layer 7 into the polysilicon 6, and forms an ohmic contact with the polysilicon 6, and the drain metal 13 forms an ohmic contact with the second heavily doped substrate region 14 on the bottom surface of the epitaxial wafer 1; In this embodiment, a window is opened at the gate groove 4 through an etching process with a window depth of 1um. A stripping process is used to prepare a 1um thick Ti / Al two-layer metal as the gate metal 12 to form an ohmic contact with the polysilicon 6. A thinning process is used to thin the 350um thick epitaxial wafer 1 to 180um, and the Ti / Al two-layer metal is used to prepare the drain metal 13.
[0026] A MOSFET with enhanced freewheeling capability of a body diode, comprising a drain metal 13, an epitaxial wafer 1 and an isolation layer 7 arranged in sequence from bottom to top; The epitaxial wafer 1 is provided with: A plurality of first heavily doped body regions 2 are provided, extending downward from the top of the epitaxial wafer 1 and spaced apart from each other; the top surface of the first heavily doped body region 2 is lower than the top surface of the epitaxial wafer 1, and the bottom surface is higher than the bottom surface of the second lightly doped voltage-resistant region 15; A second heavily doped source region 3 extends downward from the top surface of the epitaxial wafer 1 and is connected to the top surface of the first heavily doped body region 2; The gate dielectric 5 is provided with a plurality of gate dielectrics 5, and the cross section is a U-shaped structure, which respectively extends downward from the top surface of the second heavily doped source region 3, passes through the first heavily doped body region 2, and extends into the second lightly doped voltage-resistant region 15; that is, the gate dielectric 5 is respectively connected to the second heavily doped source region 3, the first heavily doped body region 2, and the second lightly doped voltage-resistant region 15; Polysilicon 6, extending downward from the top surface of the gate dielectric 5, filling the gate dielectric 5; The Schottky contact metal 9 is arranged between adjacent first heavily doped body regions 2, and its end extends into the first heavily doped body region 2, that is, the lateral width of the Schottky contact metal 9 is greater than the spacing width of adjacent first heavily doped body regions 2; the Schottky contact metal 9 is connected to the second lightly doped voltage-resistant region 15 to form a Schottky contact; the upper surface of the Schottky contact metal 9 is lower than the lower surface of the second heavily doped source region 3; The ohmic contact metal 10 extends upward from the top surface of the Schottky contact metal 9 and passes through the first heavily doped body region 2, the second heavily doped source region 3 and the isolation layer 7 in sequence, and its upper surface is flush with the upper surface of the isolation layer 7; the ohmic contact metal 10 forms an ohmic contact with the first heavily doped body region 2 and the second heavily doped source region 3, and together with the Schottky contact metal 9, constitutes a source metal; The gate metal 12 extends downward from the top surface of the isolation layer 7 into the polysilicon 6 to form an ohmic contact with the polysilicon 6 .
[0027] The drain metal 13 forms an ohmic contact with the second heavily doped substrate region 14 on the bottom surface of the epitaxial wafer 1 .
[0028] The present invention has the following advantages: By preparing an interval of the first heavily doped body region 2 and controlling the depth of the source trench 8, a Schottky contact diode is integrated at the bottom of the source trench 8, and the low turn-on voltage and high current characteristics of the Schottky diode are utilized to achieve the purpose of reducing the body diode freewheeling loss. At the same time, the second lightly doped voltage-resistant region 15 of the Schottky diode of the present invention is flanked by the interval of the first heavily doped body region 2, forming a super junction structure of the first heavily doped body region 2, the second lightly doped voltage-resistant region 15, and the first heavily doped body region 2. The super junction structure has an excellent shielding effect, which effectively reduces the electric field strength of the second lightly doped voltage-resistant region 15, thereby reducing the reverse leakage of the integrated Schottky diode.
[0029] The structure of the second lightly doped voltage-withstand region 15 below the first heavily doped body region 2 of the device of the present invention is consistent with that of an ordinary trench MOSFET, and no special additional process steps are required to reduce the reverse leakage of the integrated Schottky diode. The preparation process of the present invention is fully compatible with the preparation process of the traditional trench MOSFET, and only two additional process steps of preparing the source trench 8 and the Schottky contact metal 9 are required. Compared with the existing comparative documents, the reverse leakage of the integrated Schottky diode is reduced by reducing the special additional process steps, and the forward current conduction capacity of the integrated SBD and the forward current conduction capacity of the MOSFET are not affected, which is conducive to the advancement of the commercialization process and has higher commercial value.
[0030] Regarding the contents disclosed in this case, there are a few points that need to be explained: (1) The drawings of the embodiments disclosed in this case only involve the structures involved in the embodiments disclosed in this case. Other structures can refer to the general design; (2) In the absence of conflict, the embodiments and features of the embodiments disclosed in this case may be combined with each other to obtain new embodiments; The above are only specific implementation methods disclosed in this case, but the protection scope of the present disclosure is not limited thereto. The protection scope disclosed in this case should be based on the protection scope of the claims.
Claims
1. A method for preparing a MOSFET with enhanced body diode freewheeling capability, characterized in that: The following steps are involved: Step S100, preparing mutually spaced first heavily doped body regions (2) in the epitaxial wafer (1); Step S200, preparing a second heavily doped source region (3) in the epitaxial wafer (1); Step S300, preparing a gate trench (4) in the epitaxial wafer (1); Step S400, preparing a gate dielectric (5) and polysilicon (6) in sequence in the trench (4); Step S500, depositing an isolation layer (7) on the epitaxial wafer (1), opening a window to prepare a source trench (8), wherein the bottom of the source trench (8) extends to the inside of the first heavily doped body region (2), and the trench width is greater than the spacing width of the first heavily doped body region (2); Step S600, preparing a Schottky contact metal (9) at the bottom of the source trench (8) to form a Schottky contact with the second lightly doped voltage-resistant region (15), wherein the upper surface of the Schottky contact metal (9) is lower than the lower surface of the second heavily doped source region (3); Step S700, preparing an ohmic contact metal (10) in the source trench (8) to form an ohmic contact with the first heavily doped body region (2) and the second heavily doped source region (3), wherein the ohmic contact metal (10) in the source trench and the Schottky contact metal (9) together constitute a source metal; Step S800, opening a window at the gate trench (4), preparing a gate metal (12), and preparing a drain metal (13) on the back side of the epitaxial wafer (1), and the entire device is prepared.
2. The method for preparing a MOSFET with enhanced body diode freewheeling capability according to claim 1, characterized in that: Step S100 includes: Step S110, adopting a photolithography process and using a mask to protect the outer area of the first heavily doped body region (2); and forming a plurality of first heavily doped body regions (2) spaced apart from each other through a diffusion process or an ion implantation process.
3. The method for preparing a MOSFET with enhanced body diode freewheeling capability according to claim 1, characterized in that: Step S200 includes: Step S210, adopting a photolithography process and using a mask to protect the outer area of the second heavily doped source region (3); and forming the second heavily doped source region (3) through a diffusion process or an ion implantation process.
4. The method for preparing a MOSFET with enhanced body diode freewheeling capability according to claim 1, characterized in that: Step S300 includes: Step S310: using a photolithography process and using a mask to protect the outer region of the gate trench (4); and forming the gate trench (4) through an etching process.
5. The method for preparing a MOSFET with enhanced body diode freewheeling capability according to claim 1, characterized in that: Step S400 includes: Step S410, using a mask to protect the outer region of the gate trench (4) through a photolithography process, and using a thermal oxidation technique to prepare a gate dielectric (5) in the gate trench (4); Step S420, preparing polysilicon (6) in the gate trench (4) by chemical vapor deposition.
6. The method for preparing a MOSFET with enhanced body diode freewheeling capability according to claim 1, characterized in that: Step S500 includes: Step S510, preparing an isolation layer (7) by chemical vapor deposition, protecting the outer region of the source trench (8) by a photolithography process using a mask, and opening a window at the source trench (8) by an etching process, wherein the bottom of the source trench (8) extends to the inside of the first heavily doped body region (2), and the trench width is greater than the spacing width of the first heavily doped body region (2).
7. The method for preparing a MOSFET with enhanced body diode freewheeling capability according to claim 1, characterized in that: Step S600 includes: Step S610, preparing a Schottky contact metal (9) at the bottom of the source trench (8) by a stripping process or an etching process, the Schottky contact metal (9) forming a Schottky contact with the second lightly doped voltage-resistant region (15), and the upper surface of the Schottky contact metal (9) being lower than the lower surface of the second heavily doped source region (3).
8. The method for preparing a MOSFET with enhanced body diode freewheeling capability according to claim 1, characterized in that: Step S700 includes: Step S710, preparing an ohmic contact metal (10) in the source trench (8) by a stripping process or an etching process, the ohmic contact metal (10) forms an ohmic contact with the first heavily doped body region (2) and the second heavily doped source region (3), and the ohmic contact metal (10) and the Schottky contact metal (9) in the source trench together constitute a source metal.
9. The method for preparing a MOSFET with enhanced body diode freewheeling capability according to claim 1, characterized in that: Step S800 includes: Step S810, using a photolithography process, using a mask to protect the outer area of the gate trench (4) where the window is opened, using an etching process to open a window at the gate trench (4), and preparing a gate metal (12), and using a thinning process and a back-gold process to prepare a drain metal (13) at the bottom of the epitaxial wafer (1), and the entire device is prepared.
10. A MOSFET with enhanced body diode freewheeling capability, prepared by the method for preparing a MOSFET with enhanced body diode freewheeling capability according to any one of claims 1 to 9, characterized in that: It comprises a drain metal (13), an epitaxial wafer (1) and an isolation layer (7) which are arranged in sequence from bottom to top; The epitaxial wafer (1) is provided with: A plurality of first heavily doped body regions (2) are provided, extending downward from the top of the epitaxial wafer (1) and spaced apart from each other; the bottom surface of the first heavily doped body region (2) is higher than the bottom surface of the second lightly doped voltage-resistant region (15); a second heavily doped source region (3), extending downward from the top surface of the epitaxial wafer (1) and connected to the top surface of the first heavily doped body region (2); A plurality of gate dielectrics (5) are provided, and the cross-section is in a U-shaped structure, and each of them extends downward from the top surface of the second heavily doped source region (3), passes through the first heavily doped body region (2), and extends into the second lightly doped voltage-resistant region (15); Polycrystalline silicon (6), extending downward from the top surface of the gate dielectric (5) to fill the gate dielectric (5); A Schottky contact metal (9) is arranged between adjacent first heavily doped body regions (2), with its end extending into the first heavily doped body region (2); the Schottky contact metal (9) is connected to the second lightly doped voltage-resistant region (15) to form a Schottky contact; the upper surface of the Schottky contact metal (9) is lower than the lower surface of the second heavily doped source region (3); An ohmic contact metal (10) extending upward from the top surface of the Schottky contact metal (9) and passing through the first heavily doped body region (2), the second heavily doped source region (3) and the isolation layer (7) in sequence; A gate metal (12) extending downward from the top surface of the isolation layer (7) into the polysilicon (6) to form an ohmic contact with the polysilicon (6); The first doping region and the second doping region have opposite doping types, namely, a P region and an N region, or an N region and a P region, respectively.
Citation Information
Patent Citations
SiC grooved metal oxide semiconductor field effect transistor (MOSFET) with integration of Schottky diode and fabrication method of SiC grooved MOSFET
CN105633168A
Groove type SiC MOSFET and preparation method thereof
CN118213275A
Shielded gate trench (SGT) MOSFET cells implemented with a schottky source contact
US20060209887A1
Power MOSFET Device with Self-Aligned Integrated Schottky and its Manufacturing Method
US20110316076A1
Trench mosfet with integrated schottky rectifier in same cell
US20120037983A1