SiC UMOSFET device with N-type buried layer structure and preparation method thereof
By using N-zone buried layer structures in the epitaxial layer in SiC UMOSFET devices with different concentrations of N-zone buried layer structures in the SiC UMOSFET devices to adjust the electric field at the bottom of the trench gate and reduce the body diode defects under bipolar operating conditions, the high trench gate electric field strength and double-dimensional in SiC MOSFET devices are solved. The problem of extreme degradation effect improves the reliability and stability of the device.
Patent Information
- Application Number
- CN202411298565.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-18
- Publication Date
- 2024-12-03
AI Technical Summary
The excessive electric field strength at the bottom of the trench gate in SiC MOSFET devices causes the gate oxide layer to break early, affecting device reliability, and the bipolar degradation effect at the body diode under bipolar operating conditions is severe, limiting the large-scale application of the device.
Using N-zone buried layer structure with different concentrations in the epitaxial layer, in the device blocking state, the N-zone buried layer position depletion layer is preferentially expanded, and the N+zone buried layer position depletion layer is relatively slow to adjust the electric field at the bottom of the trench gate Direction, reduce the electric field strength, and reduce defect spread at the body diode by heavily doped N+ region buried layer structure under bipolar operating conditions.
It effectively protects the gate oxide layer at the bottom of the trench gate, reduces the electric field strength, improves the reliability of the device, improves the bipolar degradation effect during bipolar operation, and improves the stability of the device.
Smart Images

Figure CN119069356A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a SiC UMOSFET device with an N-type buried layer structure and a preparation method thereof. Background Art
[0002] Silicon carbide metal oxide semiconductor field effect transistor SiC MOSFET has the characteristics of low on-resistance, high frequency, high voltage, etc. and is widely used in electric vehicles, rail transportation, smart grids and other fields, and has become one of the hot spots in current power device research.
[0003] The technical route of SiC MOSFET is divided into two different structural types: planar gate and trench gate.
[0004] The gate process of planar SiC MOSFET is relatively simple, and it is easy to achieve good gate oxide layer quality. However, compared with Si IGBT, the defect density of SiC / SiO2 interface is still 1-2 orders of magnitude higher than that of Si / SiO2. The higher defect density will cause a significant reduction in gate oxide quality, resulting in serious reliability problems in the actual application of the device.
[0005] The trench gate SiC MOSFET adopts a trench gate structure, and the conductive channel is changed from horizontal to vertical, which effectively saves device area and greatly improves power density. However, the electric field strength borne by the silicon dioxide gate in the trench gate SiC MOSFET is much higher than that in the planar gate SiC MOSFET. Figure 1 As shown in the figure: the two corners at the bottom of the trench gate will produce electric field concentration. The high electric field strength will easily cause the gate oxide layer at the corner to break prematurely, causing a sharp rise in Igss and device failure. Therefore, the reliability of the gate oxide layer has become a major obstacle to the large-scale practical application of SiC MOSFET devices. Summary of the invention
[0006] The present invention improves the bottom of the trench gate of the SiC UMOSFET device, and utilizes the N region buried layer structure with different concentrations in the epitaxial layer. - The depletion layer at the buried layer position of the region expands first, N + The depletion layer at the buried layer position in the region expands relatively slowly, thereby achieving the effect of adjusting the electric field direction at the bottom of the trench gate, so that the electric field strength at the two corners at the bottom of the trench gate decreases, protecting the gate oxide layer; at the same time, under bipolar operating conditions, N + The buried layer structure can also improve the bipolar degeneration effect at the body diode.
[0007] The technical solution of the present invention is: A method for preparing a SiC UMOSFET device with an N-type buried layer structure comprises the following steps: S100, in heavily doped N + The N-type buffer layer and the primary N-type buffer layer are grown on the substrate layer. - drift layer; S200, in one N - The drift layer is then doped with heavily doped N + region and lightly doped N - district; S300, in one N - Drift layer, N + Area and N - A second N - drift layer; S400, in the secondary N - A P-well region is formed on the drift layer by ion implantation, and a heavily doped NP region and a heavily doped PP region are formed on the P-well region by ion implantation. After the implantation, high temperature ion activation is performed; S500, forming a trench on the NP region by dry etching; and sequentially forming a gate oxide layer and a Poly layer in the trench; S600, forming a dielectric layer on the Poly layer to isolate the gate electrode and the source electrode metal; S700, forming a source ohmic contact alloy layer on the NP region and the PP region by a sputtering process; S800, forming a source metal layer on the source ohmic contact alloy layer and the dielectric layer by metal sputtering, and leading out a source electrode; S900, in N + The back side of the substrate layer reduces N + The thickness of the substrate layer is prepared to form a drain metal layer and lead out a drain electrode.
[0008] Specifically, in step S100, N + The substrate layer is doped with N ions with a doping concentration of 1e 19 cm -2 ±10%; N-type buffer layer is doped with N ions, with a doping concentration of 1e 18 cm -2 ±10%.
[0009] Specifically, in step S100, N - The drift layer is doped with N ions with a doping concentration of 8e 15 -2e 16 cm -2 .
[0010] Specifically, in step S200, N + The region is doped with N ions with a doping concentration of 2e17 -5e 18 cm -2 .
[0011] Specifically, in step S300, N - The region is doped with Al ions, and the doping concentration is 1e 14 -8e 14 cm -2 .
[0012] Specifically, in step S400, the second N - The drift layer is doped with N ions, and the N - Drift layer and secondary N - The total thickness of the drift layer (6) is 5-20 um.
[0013] Specifically, in step S400, the P-well region is doped with Al ions at a doping concentration of 1e 17 -1e 18 cm -2 .
[0014] Specifically, in step S400, the NP region is doped with N ions at a doping concentration of 1e 18 -5e 18 cm -2 .
[0015] Specifically, in step S400, the PP region is doped with Al ions at a doping concentration of 5e 18 -1e 19 cm -2 .
[0016] An N-type buried layer SiC UMOSFET device comprises a drain metal layer, an N-type buried layer, and a drain metal layer. + Substrate layer, N-type buffer layer, N - Drift layer, P-well region, NP region, source ohmic contact alloy layer and source metal layer; The N - The drift layer contains: N + There are several zones, arranged at intervals in the N - In the drift layer; N - There are several zones, arranged at intervals in the N - The middle part of the drift layer; - Area and N + The areas are arranged at equal intervals and in the same plane; The top surface of the NP region has a bottom extending to N - The gate oxide layer of the region is in a U-shaped structure and is filled with a Poly layer; The top surface of the NP region is provided with a dielectric layer covering the gate oxide layer and the Poly layer; A PP region extending downward is disposed at the outer end of the NP region. The PP region extends from the top surface of the P-well region and is spaced apart from the bottom surface of the P-well region.
[0017] Beneficial effects of the present invention: Improving Gate Oxide Reliability in Trench UMOSFETs: The electric field strength borne by the silicon dioxide gate in the trench gate SiC MOSFET is much higher than that in the planar gate SiC MOSFET. The present invention utilizes the N region buried layer structure with different concentrations in the epitaxial layer. In the device blocking state, N - The depletion layer at the buried layer position in the region expands first, N + The depletion layer at the buried layer position expands relatively slowly, thereby achieving the effect of adjusting the direction of the electric field at the bottom of the trench gate, so that the electric field strength at the two corners at the bottom of the trench gate decreases, protecting the gate oxide layer; 2. Improve bipolar degradation effect: During bipolar operation, the energy released by the recombination of electrons and holes causes stacking faults to spread to the surface of the chip at the BPD, reducing the effective active area of the chip. + The buried layer structure in the region injects a large number of hole carriers into the epitaxial layer at the body diode during the bipolar operation of the device and reacts with the heavily doped N + The majority of electron carriers in the buried layer structure recombine in advance, reducing the chance of BPD defects on the excited substrate to propagate and improving the bipolar degradation effect of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a structural schematic diagram of step S1500 of the present invention; Figure 2 It is a structural schematic diagram of step S100 of the present invention; Figure 3 It is a structural schematic diagram of step S200 of the present invention; Figure 4 It is a structural schematic diagram of step S300 of the present invention; Figure 5 is a schematic structural diagram of step S400 of the present invention; Figure 6 is a schematic structural diagram of step S500 of the present invention; Figure 7 is a schematic structural diagram of step S600 of the present invention; Figure 8 is a schematic diagram of the structure of step S700 of the present invention; Fig. 9is a structural schematic diagram of step S800 of the present invention; Fig.10 is a structural schematic diagram of step S900 of the present invention; Fig.11 is a structural schematic diagram of step S1000 of the present invention; Fig.12 is a structural schematic diagram of step S1100 of the present invention; Fig.13 is a schematic diagram of the structure of step S1200 of the present invention; Fig.14 is a schematic diagram of the structure of step S1300 of the present invention; Fig.15 is a schematic structural diagram of step S1400 of the present invention; In the figure, 1 is N + The substrate layer, 2 is the N-type buffer layer, 3 is the primary N - Drift layer, 4 is N + Area, 5 is N - Area, 6 is the second N - Drift layer, 7 is the P-well region, 8 is the NP region, 9 is the PP region, 10 is the trench, 11 is the gate oxide layer, 12 is the Poly layer, 13 is the dielectric layer, 14 is the source ohmic contact alloy layer, 15 is the source metal layer, and 16 is the drain metal layer. DETAILED DESCRIPTION
[0019] The present invention is described in detail below in conjunction with specific practical cases. Examples of the embodiments are shown in the accompanying drawings, and the schematic implementation methods of the present invention and their descriptions are only used to explain the present invention and are not intended to limit the present invention.
[0020] In the description of the present invention, it should be understood that the terms "upper", "lower", "left", "right", "vertical", "horizontal", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present invention. In the description of the present invention, unless otherwise specified, "plurality" means two or more.
[0021] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0022] A method for manufacturing an N-type buried layer SiC UMOSFET device comprises the following steps: S100, refer to Figure 2 As shown, in heavily doped N + An N-type buffer layer 2 is grown on the substrate layer 1; N in step S100 + Substrate layer 1 is doped with N ions, with a thickness of 360-400um and a doping concentration of 1e 19 cm -2 ±10%, the N-type buffer layer is also doped with N ions, with a thickness of 0.8-1.2um and a doping concentration of 1e 18 cm -2 ±10%.
[0023] S200, refer to Figure 3 As shown, a layer of N type buffer layer 2 is epitaxially grown. - Drift layer 3; The N of step S200 - The drift layer 3 is doped with N ions at a doping concentration of 8e 15 -2e 16 cm -2 .
[0024] S300, refer to Figure 4 As shown, in one N - The drift layer 3 is heavily doped with N + Zone 4; N in step S300 + Area 4 is doped with N ions, with a thickness of 0.8-1.5um and a doping concentration of 1e 17 -1e 18 cm -2 Except for the area directly below the groove, the remaining area N + The regions 4 are arranged at equal intervals and the lateral spacing is not limited, and the longitudinal spacing with the P-well region 7 is also not limited.
[0025] S400, refer to Figure 5 As shown, in one N - The drift layer (3) is lightly doped with N by ion implantation. - Zone 5; N in step S400 - Area 5 is doped with Al ions, and the epitaxial concentration in this area is reduced by combining P-type doping and N-type doping. - The thickness of region 5 is 0.8-1.5um and the doping concentration is 1e 14 -1e 15 cm-2 , and is located directly below the groove and N + The regions 5 are arranged at equal intervals and the lateral spacing is not limited, and the longitudinal spacing with the P-well region 7 is also not limited.
[0026] S500, refer to Figure 6 As shown, in one N - Drift layer 3, N region 4, N - A second N layer is epitaxially grown on region 5. - Drift layer 6; The secondary N of step S500 - The drift layer 6 is doped with N ions. - Drift layer 3 and secondary N - The total thickness of the drift layer 6 is 5-20um, and the doping concentration is the same as that of the primary N - The drift layer 3 is consistent.
[0027] S600, refer to Figure 7 As shown, in the secondary N - A P-well region 7 is formed on the drift layer 6 by ion implantation; The P-well region 7 in step S600 is doped with Al ions with a thickness of 0.6-1um and a doping concentration of 1e 17 -1e 18 cm -2 .
[0028] S700, reference Figure 8 As shown, a heavily doped NP region 8 is formed on the P-well region 7 by ion implantation; The NP region 8 in step S700 is doped with N ions with a thickness of 0.2-0.5um and a doping concentration of 1e 18 -5e 18 cm -2 .
[0029] S800, reference Fig. 9 As shown, a heavily doped PP region 9 is formed on the P-well region 7 by ion implantation, and high temperature ion activation is performed after the implantation is completed; In step S800, the PP region 9 is doped with Al ions with a thickness of 0.3-0.8 μm and a doping concentration of 5 e 18 -1e 19 cm -2 , where the PP region 9 is connected to the side of the NP region 8, the thickness of the PP region 9 is greater than or equal to the thickness of the NP region 8 and less than or equal to the thickness of the P-well region 7; in this case, a high-temperature annealing furnace is used, and annealing is performed after covering the C film. The annealing temperature is 1600-1800℃, the annealing time is 10-30min, and ion activation is used.
[0030] S900, refer to Fig.10 As shown, a trench 10 is formed on the upper surface of the NP region 8 by dry etching; In step S900, the trench 10 is etched to a depth of 1-2 um, wherein the bottom two corners of the trench 10 must be included in N - Inside Zone 5.
[0031] S1000, refer to Fig.11 As shown, a gate oxide layer 11 is formed in the trench 10 by a dry oxygen thermal oxidation process, and a channel is formed at the interface with the P-Well region 7; In step S1000 , the gate oxide layer 11 is grown at a temperature of 1250-1350° C. and a thickness of 40-60 nm. It needs to be annealed in a NO atmosphere at a temperature of 1250° C. for 1 hour to improve the compactness of the gate oxide layer 11 and reduce defects.
[0032] S1100, reference Fig.12 As shown, a Poly layer 12 is formed on the gate oxide layer 11 by depositing polysilicon, and a gate electrode is led out; S1200, refer to Fig.13 As shown, a dielectric layer 13 is formed by depositing oxide on the Poly layer 12 to isolate the gate electrode and the source electrode metal; S1300, refer to Fig.14 As shown, Ni metal is sputtered on the NP region 8 and the PP region 9 and then alloyed by RTA high temperature annealing to form a source ohmic contact alloy layer 14; In step S1300 , the source ohmic contact alloy layer 14 is annealed at a temperature of 1000° C. for 5 minutes to form an alloy and achieve an ohmic contact effect.
[0033] S1400, reference Fig.15 As shown, a source metal layer 15 is formed on the source ohmic contact alloy layer 14 and the dielectric layer 13 by sputtering Ti / AlCu metal to lead out a source electrode; S1500, refer to Figure 1 As shown, in N + The back side of the substrate layer 1 is thinned to reduce N + The substrate layer 1 is 1000 mm thick, and then Ni metal is sputtered and Ti / Ni / Ag metal is evaporated to form a drain metal layer 16 to lead out a drain electrode.
[0034] In step S1500, the drain metal layer 16 needs to be laser annealed after Ni metal sputtering, and the laser energy is 2-4mJ / cm 2 ; Ti / Ni / Ag multilayer metal is then evaporated, with a total thickness of 1.4-2um.
[0035] An N-type buried layer SiC UMOSFET device comprises a drain metal layer 16, an N-type buried layer 20 and a drain metal layer 31 arranged in sequence from bottom to top. + Substrate layer 1, N-type buffer layer 2, N - Drift layer, P-well region 7, NP region 8, source ohmic contact alloy layer 14 and source metal layer 15; The N - The drift layer contains: N + Area 4, with a plurality of, spaced apart in the N - In the drift layer; N - Area 5, with a plurality of, spaced apart in the N - The middle part of the drift layer; - Area 5 and N + The zones 4 are arranged at equal intervals and in the same plane; the N - Zone 5 and N + Area 4 and N - A gap is provided between the top surface and the bottom surface of the drift layer; The top surface of the NP region 8 has a bottom surface extending to the N - The gate oxide layer 11 of the region 5; the gate oxide layer 11 is in a U-shaped structure and is filled with a Poly layer 12; the top surface of the Poly layer 12 is flush with the top surface of the NP region 8; The top surface of the NP region 8 is provided with a dielectric layer 13 covering the gate oxide layer 11 and the Poly layer 12; the source ohmic contact alloy layer 14 is located on the side of the dielectric layer 13; The outer end of the NP zone 8 is provided with a PP zone 9 extending downward; P-well area 7 from the secondary N - The top surface of the drift layer 6 extends downward, and the NP region 8 and the PP region 9 extend downward from the top surface of the P-well region 7 respectively, and the side walls of the two regions are in contact with each other.
[0036] The gate oxide layer 11 is formed by providing a groove 10 extending downwardly in the middle of the top surface of the NP region 8, and the bottom of the groove 10 is connected to the N - Area 5 contacts, whose corners are contained in N - Inside the region 5; a gate oxide layer 11 is provided in the groove 10; a Poly layer 12 is provided on the inner surface of the gate oxide layer 11; a dielectric layer 13 is provided on the top surfaces of the NP region 8, the gate oxide layer 11 and the Poly layer 12; a source ohmic contact alloy layer 14 is provided on the top surfaces of the NP region 8 and the PP region 9, and its sidewalls are in contact with the dielectric layer 13.
[0037] The present invention improves the bottom of the trench gate of the SiC UMOSFET device, and utilizes the N region buried layer structure with different concentrations in the epitaxial layer. -The depletion layer at the buried layer position of the region expands first, N + The depletion layer at the buried layer position in the region expands relatively slowly, thereby achieving the effect of adjusting the electric field direction at the bottom of the trench gate, so that the electric field strength at the two corners at the bottom of the trench gate decreases, protecting the gate oxide layer; at the same time, under bipolar operating conditions, N + The buried layer structure can also improve the bipolar degeneration effect at the body diode.
Claims
1. A method for preparing a SiC UMOSFET device with an N-type buried layer structure, characterized in that: The steps include: S100, in heavily doped N + An N-type buffer layer (2) and a primary N-type - Drift layer (3); S200, in one N - The drift layer (3) is formed by ion implantation in sequence with heavily doped N + Region (4) and lightly doped N - Area (5); S300, in one N - Drift layer (3), N + Area (4) and N - A second N layer is grown epitaxially on region (5) - Drift layer (6); S400, in the secondary N - A P-well region (7) is formed on the drift layer (6) by ion implantation, and in the P-well region (7) A heavily doped NP region (8) and a heavily doped PP region (9) are formed by ion implantation, and high temperature ion activation is performed after the implantation is completed; S500, forming a trench (10) on the NP region (8) by dry etching; and sequentially forming a gate oxide layer (11) and a Poly layer (12) in the trench (10); S600, forming a dielectric layer (13) on the Poly layer (12) to isolate the gate electrode and the source electrode metal; S700, forming a source ohmic contact alloy layer (14) on the NP region (8) and the PP region (9) by a sputtering process; S800, forming a source metal layer (15) on the source ohmic contact alloy layer (14) and the dielectric layer (13) by metal sputtering, and leading out a source electrode; S900, in N + The back side of the substrate layer (1) reduces N + The substrate layer (1) has a thickness of 1000 nm, a drain metal layer (16) is prepared, and a drain electrode is led out.
2. The method for preparing a SiC UMOSFET device with an N-type buried layer structure according to claim 1, characterized in that: In step S100, N + The substrate layer (1) is doped with N ions at a doping concentration of 1e 19 cm -2 ±10%; N-type buffer layer (2) is doped with N ions, with a doping concentration of 1e 18 cm -2 ±10%.
3. The method for preparing a SiC UMOSFET device with an N-type buried layer structure according to claim 1, characterized in that: In step S100, N - The drift layer (3) is doped with N ions at a doping concentration of 8e 15 -2e 16 cm -2 .
4. The method for preparing a SiC UMOSFET device with an N-type buried layer structure according to claim 1, characterized in that: In step S200, N + Region (4) is doped with N ions at a concentration of 2e 17 -5e 18 cm -2 .
5. The method for preparing a SiC UMOSFET device with an N-type buried layer structure according to claim 1, characterized in that: In step S300, N - Region (5) is doped with Al ions at a concentration of 1e 14 -8e 14 cm -2 .
6. The method for preparing a SiC UMOSFET device with an N-type buried layer structure according to claim 1, characterized in that: In step S400, the second N - The drift layer (6) is doped with N ions, once N - Drift layer (3) and secondary N - The total thickness of the drift layer (6) is 5-20 um.
7. The method for preparing a SiC UMOSFET device with an N-type buried layer structure according to claim 1, characterized in that: In step S400, the P-well region (7) is doped with Al ions at a doping concentration of 1e 17 -1e 18 cm -2 .
8. The method for preparing a SiC UMOSFET device with an N-type buried layer structure according to claim 1, characterized in that: In step S400, the NP region (8) is doped with N ions at a doping concentration of 1e 18 -5e 18 cm -2 .
9. The method for manufacturing an N-type buried SiC UMOSFET device according to claim 1, characterized in that: In step S400, the PP region (9) is doped with Al ions at a doping concentration of 5e 18 -1e 19 cm -2 .
10. An N-type buried layer SiC UMOSFET device, prepared by the method for preparing an N-type buried layer SiC UMOSFET device according to any one of claims 1 to 9, characterized in that: The drain metal layer (16), N + Substrate layer (1), N-type buffer layer (2), N - Drift layer, P-well region (7), NP region (8), source ohmic contact alloy layer (14) and source metal layer (15); The N - The drift layer contains: N + Area (4) is provided with a plurality of - In the drift layer; N - Area (5) is provided with a plurality of - The middle part of the drift layer; - Area (5) and N + Zone (4) is arranged at equal intervals and in the same plane; The top surface of the NP region (8) has a - A gate oxide layer (11) of the region (5); the gate oxide layer (11) is in a U-shaped structure and is filled with a Poly layer (12); The top surface of the NP region (8) is provided with a dielectric layer (13) covering the gate oxide layer (11) and the Poly layer (12); A PP zone (9) extending downward is provided at the outer end of the NP zone (8), and the PP zone (9) extends downward from the top surface of the P-well zone (7).