Multi-element mineral fertilizer produced from potassium-rich slate and preparation process of multi-element mineral fertilizer
By crushing, removing heavy metals, mixing and firing the potassium-rich slate, making multi-element mineral fertilizers, the problem of traditional utilization methods not being able to fully realize their potential is solved, and the recycling of resources and soil management is realized. Various elements are used to promote crop growth and meet environmental protection requirements.
Patent Information
- Application Number
- CN202411232581.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-04
- Publication Date
- 2024-11-22
AI Technical Summary
Traditional use methods have failed to fully utilize the potential of potassium-rich slate, resulting in waste of resources and environmental pollution, and soil treatment and improvement are difficult to improve crop yield and quality.
By selecting potassium-rich slate in tailings, crushing and grinding, removing excessive lead and arsenic, mixing with other materials and compounds, firing and physical activation, it is made into a mineral fertilizer containing multi-elements, and providing plants with the plant. Mineral nutrients required.
It realizes efficient utilization of potassium-rich slate, provides a variety of elements required by plants, promotes comprehensive mineral nutrient replenishment and cation exchange of soil, solves the problems of soil management and crop growth, and is environmentally friendly and has no low-value tail waste, which is in line with Green development requirements.
Smart Images

Figure CN118993816A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of mineral agricultural fertilizers, and more specifically, to a multi-element mineral fertilizer produced from potassium-rich slate and a preparation process thereof. Background Art
[0003] At present, fertilizers widely used in agricultural production mostly rely on the mining of new mines, which not only causes waste of resources, but also brings the risk of environmental pollution. At the same time, soil management and improvement are crucial to improving crop yields and quality. Potassium-rich slate is a rich mineral resource with high K2O grade, total reserves of 1.67 billion tons, and an average K2O content of 13.0% in the ore, but traditional utilization methods have failed to fully tap its potential.
[0004] In order to solve the above problems, the present application provides a method for producing multi-element mineral fertilizer from potassium-rich slate and a preparation process thereof. Summary of the invention
[0005] The present application provides a potassium-rich slate for producing multi-element mineral fertilizer and a preparation process thereof, which adopts the following technical scheme:
[0006] A multi-element mineral fertilizer produced from potassium-rich slate and a preparation process thereof, comprising the following components: 31.49 parts of SiO2, 5.87 parts of MgO, 9.51 parts of CaO, and 20.57 parts of K2O;
[0007] The limited components include: S content of 0.02%, Cl content of 0.000059%, Na content of 0.03%, As content of 1.1ppm, Cd content of 2.6ppm, Pb content of 28.8ppm, Cr content of 12.4ppm;
[0008] It also includes: H2O content of 0.08%, Fe content of 346 mg / kg, B content of 40.5 mg / kg, Zn content of 53 mg / kg, and Cu content of 8.7 mg / kg.
[0009] Further, the following steps are included:
[0010] S1: Select potassium-rich slate from tailings as raw material, crush and grind it to obtain mineral powder with a particle size of less than 180 mesh;
[0011] S2: removing excessive lead and arsenic in potassium-rich slate by magnetic separation and flotation in the process of iron separation to obtain slate raw materials with a potassium oxide content of more than 12%;
[0012] S3: uniformly mixing the treated slate raw material with material ①, material ② and a compound thereof to form a mixed raw material;
[0013] S4: forming the homogenized materials into a shape suitable for subsequent firing;
[0014] S5: performing a sintering process on the formed materials to make the prepared mixed raw materials into mature materials;
[0015] S6: Finally, physical activation treatment is carried out, the clinker is cooled and crushed to obtain multi-element mineral fertilizer.
[0016] Furthermore, in step S5, the firing temperature ranges from 850 to 1200° C., and the firing time ranges from 20 to 170 minutes.
[0017] Furthermore, material ① is a material containing trace amounts of iron, manganese, copper, zinc and molybdenum.
[0018] Furthermore, material ② is a mixture of at least one material selected from iron-containing materials, aluminum-containing materials, calcium-containing materials and magnesium-containing materials.
[0019] Furthermore, the compound is selected from at least one compound of sodium hydroxide, potassium carbonate, potassium hydroxide, potassium silicate and sodium silicate.
[0020] In summary, this application includes the following beneficial technical effects:
[0021] The various mineral nutrient materials of the present invention activate the mineral nutrients in potassium-rich slate into mineral nutrients that are easily absorbed by plants, do not pollute the environment, can provide trace elements such as iron, manganese, boron, zinc, copper, etc., medium elements such as silicon, calcium, magnesium, and macroelements such as potassium required by plants, can be directly used for rapid fertilization of newly opened cultivated land, cultivation of fertile arable layers, soil acidification, saline-alkali land, soil degradation control, desertification control and other soil management, and provide comprehensive mineral nutrients and cation exchange for the soil. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 This is the XRD diffraction pattern of the large particle sample of this application;
[0023] Figure 2 This is the XRD diffraction pattern of the medium particle sample of this application;
[0024] Figure 3 XRD diffraction pattern of the fine powder sample of this application;
[0025] Figure 4 The following is a flow chart of the pest removal process of this application;
[0026] Figure 5 It is the weak magnetic separation index under different grinding particle sizes of this application;
[0027] Figure 6It is the weak magnetic separation index under different magnetic field strengths of this application. DETAILED DESCRIPTION
[0028] The technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application; obviously, the described embodiments are only part of the embodiments of the present application, rather than all the embodiments, and all other embodiments obtained by ordinary technicians in this field based on the embodiments in the present application without making creative work are within the scope of protection of the present application.
[0029] In the description of the present application, it should be noted that the terms "upper", "lower", "inner", "outer", "top / bottom" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present application. In addition, the terms "first" and "second" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0030] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "provided with", "set / connected", "connected", etc. should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0031] Example:
[0032] The present application discloses a method for producing multi-element mineral fertilizer from potassium-rich slate and its preparation process. Figure 1-Figure 4 , comprising the following raw materials in weight percentage: SiO2 content of 1-53.03 weight%, Al2O3 content of 1-14.09 weight%, Fe2O3 content of 1-11.45 weight%, MgO content of 1-3.15 weight%, CaO content of 1-3.14 weight%, Na2O content of 0.1-0.52 weight%, K2O content of 1-11.29 weight%, TiO2 content of 0.1-0.37 weight%, LOI content of 1-2.66 weight%, lead and arsenic;
[0033] Embodiment 1;
[0034] The Example 2 includes a SiO2 content of 56.55 weight %, an Al2O3 content of 14.81 weight %, a Fe2O3 content of 8.31 weight %, a MgO content of 2.30 weight %, a CaO content of 2.64 weight %, a Na2O content of 0.61 weight %, a K2O content of 12.39 weight %, a TiO2 content of 0.28 weight %, a LOI content of 1.81 weight %, lead and arsenic.
[0035] Embodiment 2;
[0036] The Example 3 includes a SiO2 content of 48.27 weight %, an Al2O3 content of 11.57 weight %, a Fe2O3 content of 17.63 weight %, a MgO content of 4.87 weight %, a CaO content of 2.27 weight %, a Na2O content of 1.16 weight %, a K2O content of 10.09 weight %, a TiO2 content of 0.81 weight %, a LOI content of 3.03 weight %, lead and arsenic.
[0037] The process includes the following steps:
[0038] S1: Select potassium-rich slate from tailings as raw material, crush and grind it to obtain mineral powder with a particle size of less than 180 mesh;
[0039] S2: Remove excessive lead and arsenic in potassium-rich slate by magnetic separation and flotation in the process of iron selection to obtain slate raw materials with a potassium oxide content of more than 12%. The raw materials are detoxified and passed through the ore sample analysis department. The heavy metal lead and arsenic content in potassium-rich slate in some areas exceeds the national agricultural standard limit. The raw materials are coarsely crushed to -50mm by a jaw crusher, and then finely crushed to -10mm by a jaw crusher, and then ground to more than 90% of -180 mesh by a ball mill. The ground ore powder is passed through a field strength of 170 kA / m weak magnetic separator, 90.7% of the roughly selected potassium-rich slate concentrate was obtained, and 9.3% of the iron-containing minerals were selected; then the roughly selected potassium-rich slate concentrate was passed through a strong magnetic separator with a field strength of 1.0T to obtain 87.2% of the carefully selected potassium-rich slate concentrate. Under the conditions of grinding particle size -0.074mm accounting for 91% and magnetic field strength of 172kA / m, the iron grade of the potassium-rich ore obtained by weak magnetic separation was 5.90%, the recovery rate was 56.29%, the K2O content was 13.69%, and the iron removal rate was 43.71%. The weak magnetic selection potassium-rich tailings were further enriched with potassium by strong magnetic separation (magnetic field strength of 1.0T) to remove iron, and the iron removal rate was 38.02%. Finally, through the "weak magnetic separation-strong magnetic separation" process, potassium-rich tailings with an iron content of 4.30% and a comprehensive recovery rate of 34.89% were obtained, and the potassium content was 14.60%;
[0040] S3: uniformly mixing the processed slate raw material with material ①, material ② and a compound thereof to form a mixed raw material;
[0041] S4: forming the homogenized materials into a shape suitable for subsequent firing;
[0042] S5: performing a sintering process on the formed materials to make the prepared mixed raw materials into mature materials;
[0043] S6: Finally, physical activation treatment is carried out, and the clinker is cooled and crushed to obtain multi-element mineral fertilizer. According to the above steps, tailings resources are efficiently utilized, and potassium-rich slate, which may have been regarded as solid waste, is efficiently converted into multi-element mineral fertilizer for agricultural use, realizing the recycling of resources, environmental protection and no low-value tailings. No low-value by-products are produced during the entire preparation process, which is environmentally friendly and meets the requirements of green development. It alleviates the problem of potassium deficiency. Multi-element mineral fertilizers are rich in potassium and other elements required by various plants, which helps to alleviate the problem of potassium deficiency in my country's agriculture and balance the supplementation of soil nutrients. The trace elements, medium elements and macroelements in the fertilizer are reasonably proportioned, which can fully supplement the mineral nutrients in the soil and promote the balanced growth of crops.
[0044] The temperature range during firing in step S5 is 850-1200°C, and the firing time is 20-170 minutes. The mixed raw materials after homogenization are placed in a high temperature environment for firing. The temperature range of this step is controlled at 850-1200°C, and the firing time is 20-170 minutes. This high-temperature treatment process not only activates the mineral nutrients in the raw materials, but also promotes the formation of multi-element mineral fertilizers. During the firing process, the temperature must be strictly controlled to ensure that it fluctuates within the specified range. Too low a temperature may not fully activate the mineral nutrients, while too high a temperature may cause the raw materials to melt or produce harmful substances. The choice of firing time is also critical. Too short a time may not allow the reaction to proceed completely, while too long a time may increase energy consumption and reduce production efficiency. The prepared mixed raw materials are placed in a specific high temperature environment for heat treatment, and the temperature range is set at 850-1200°C, and the firing time is 20-170 minutes. This step aims to promote chemical reactions between components through high temperature, achieve effective activation and combination of mineral nutrients, form a stable mineral fertilizer structure, and activate the mineral nutrients in the material through firing at different temperature ranges, turning them into a form that is easily absorbed by plants.
[0045] Material ① is a material containing trace amounts of iron, manganese, copper, zinc and molybdenum, which provides plants with essential trace elements.
[0046] Material ② is selected from at least one of iron-containing materials, aluminum-containing materials, calcium-containing materials and magnesium-containing materials, and is mixed with slate raw materials to form the intermediate elements and part of the basic nutrients of the fertilizer.
[0047] The compound is selected from at least one of sodium hydroxide, potassium carbonate, potassium hydroxide, potassium silicate and sodium silicate, and is used to adjust the reaction conditions and promote the activation and combination of mineral nutrients.
[0048] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A potassium-rich slate for producing multi-element mineral fertilizers, It is characterized by: The composition includes the following parts: SiO2 content is 31.49 parts, MgO content is 5.87 parts, CaO content is 9.51 parts, and K2O content is 20.57 parts; The limited components include: S content of 0.02%, Cl content of 0.000059%, Na content of 0.03%, As content of 1.1ppm, Cd content of 2.6ppm, Pb content of 28.8ppm, Cr content of 12.4ppm; It also includes: H2O content of 0.08%, Fe content of 346 mg / kg, B content of 40.5 mg / kg, Zn content of 53 mg / kg, and Cu content of 8.7 mg / kg.
2. A process for preparing multi-element minerals from potassium-rich slate. It is characterized by: The following steps are involved: S1: Select potassium-rich slate from tailings as raw material, crush and grind it to obtain mineral powder with a particle size of less than 180 mesh; S2: removing excessive lead and arsenic in potassium-rich slate by magnetic separation and flotation in the process of iron separation to obtain slate raw materials with a potassium oxide content of more than 12%; S3: uniformly mixing the processed slate raw material with material ①, material ② and a compound thereof to form a mixed raw material; S4: forming the homogenized materials into a shape suitable for subsequent firing; S5: performing a sintering process on the formed materials to make the prepared mixed raw materials into mature materials; S6: Finally, physical activation treatment is carried out, the clinker is cooled and crushed to obtain multi-element mineral fertilizer.
3. A process for preparing multi-element minerals from potassium-rich slate according to claim 2, Features: The firing temperature in step S5 is in the range of 850 to 1200° C., and the firing time is in the range of 20 to 170 minutes.
4. A process for preparing multi-element minerals from potassium-rich slate according to claim 2, Features: Material ① is a material containing trace amounts of iron, manganese, copper, zinc and molybdenum.
5. A process for preparing multi-element minerals from potassium-rich slate according to claim 2, Features: Material ② is a mixture of at least one material selected from iron-containing materials, aluminum-containing materials, calcium-containing materials and magnesium-containing materials.
6. A process for preparing multi-element minerals from potassium-rich slate according to claim 2, Features: The compound is at least one compound selected from the group consisting of sodium hydroxide, potassium carbonate, potassium hydroxide, potassium silicate and sodium silicate.