Road surface fatigue damage prediction system and method considering semi-rigid base modulus attenuation
By obtaining the traffic volume and shaft load spectrum of the pavement structure in real time, combining material tests and temperature measurements, using elastic layer theory to calculate the fatigue life and modulus attenuation of the semi-rigid base layer, the semi-rigid base material mold has not been considered in the prior art. The problem of quantity attenuation achieves accurate prediction of fatigue damage on asphalt pavement and improves the accuracy of pavement structure design and maintenance decisions.
Patent Information
- Application Number
- CN202411029759.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-07-30
AI Technical Summary
The prior art does not consider the attenuation of the modulus of semi-rigid base layer material when calculating fatigue damage of asphalt pavement structures, resulting in inaccurate calculation of fatigue damage, affecting the design and maintenance decisions of the pavement structure.
A road fatigue damage prediction system and method that considers the modulus attenuation of semi-rigid base layer is adopted. By obtaining the traffic volume and shaft load spectrum of the pavement structure in real time, combining material tests and temperature measurements, the fatigue of the semi-rigid base layer is calculated using elastic layer theory. Lifespan and modulus attenuation, accurately predict road fatigue damage.
It realizes accurate prediction of road fatigue damage, provides a reliable basis for road structure design and maintenance decisions, and improves the service quality of asphalt pavement.
Smart Images

Figure CN119026328A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of road engineering, and in particular to a road surface fatigue damage prediction system and method taking into account the attenuation of semi-rigid base modulus. Background Art
[0002] Asphalt pavement has been widely used in highway, tunnel, airport and bridge deck paving projects due to its driving comfort and durability. Asphalt pavement is subjected to repeated effects of traffic load and external environment during its service, which leads to various forms of pavement structure damage. Among them, pavement structure fatigue damage is one of the main causes of pavement structure damage. Accurate calculation and prediction of asphalt pavement fatigue damage has important guiding significance for the formulation of pavement structure design scheme and pavement structure maintenance and repair decision-making.
[0003] Semi-rigid base asphalt pavement structure is the most commonly used asphalt pavement structure in domestic highway engineering. Its fatigue damage calculation generally adopts Miner's linear damage accumulation law. However, this law does not take into account the phenomenon that the modulus of the semi-rigid base material decays with the increase of service life, that is, it ignores the weakening of the mechanical properties of the material itself with the increase of service time, which leads to greater fatigue damage of the pavement structure than the damage obtained by conventional calculation. In addition, the current fatigue damage calculation method still uses the equivalent axle load to deal with the accumulated traffic volume, which leads to the problem of inaccurate calculation of fatigue damage of asphalt pavement structure, which is not conducive to the accurate formulation of control design and maintenance and repair decisions of asphalt pavement structure, and affects the service quality of asphalt pavement. Summary of the invention
[0004] The present invention aims to solve the above-mentioned problem and provides a pavement fatigue damage prediction system and method taking into account the attenuation of the modulus of the semi-rigid base layer. By acquiring the traffic volume and axle load spectrum of the pavement structure in real time, the influence of the attenuation of the modulus of the semi-rigid base layer on the pavement fatigue damage is fully considered, and the accurate prediction of the pavement fatigue damage is achieved, which provides a basis for the formulation of pavement structure design plans and maintenance and repair decisions.
[0005] To achieve the above object, the present invention adopts the following technical solution:
[0006] A pavement fatigue damage prediction system considering the attenuation of semi-rigid base modulus, comprising a traffic dynamic weighing device, a pavement structure temperature field measuring device and a pavement data processing device;
[0007] The traffic dynamic weighing device is buried on the top of the asphalt layer of the pavement structure and is used to collect the vehicle type, speed and axle load data of the vehicles traveling on the pavement structure;
[0008] The pavement structure temperature field measuring device is buried at different depths of the pavement structure and is used to measure the internal temperature of each structural layer in the pavement structure;
[0009] The pavement data processing device is connected to the traffic dynamic weighing device and the pavement structure temperature field measuring device respectively, and is used to receive, store and process the measurement data of the traffic axle load measuring device and the pavement structure temperature field measuring device, calculate and output the pavement fatigue damage considering the attenuation of the semi-rigid base modulus.
[0010] A pavement fatigue damage prediction method considering the attenuation of the modulus of a semi-rigid base layer adopts the pavement fatigue damage prediction system considering the attenuation of the modulus of a semi-rigid base layer as described above, comprising the following steps:
[0011] Step 1, set the total duration of pavement fatigue damage prediction and divide it into multiple analysis periods by month;
[0012] Step 2, using a traffic dynamic weighing device to obtain the vehicle type, speed and axle load data of vehicles traveling on the road, and calculate the joint axle load spectrum of each analysis period;
[0013] Step 3, preparing a semi-rigid base material specimen according to the material parameters of the pavement structure, and using the semi-rigid base material specimen to conduct a bending tensile strength test and a repeated fatigue loading test to determine a fatigue life prediction model and a modulus attenuation model;
[0014] Step 4, preparing asphalt mixture specimens of each structural layer according to the material parameters of the pavement structure, and conducting a uniaxial dynamic compression modulus test using the asphalt mixture specimens to determine the dynamic modulus master curve of each structural layer;
[0015] Step 5, using a pavement structure temperature field measurement device to measure the average temperature of the asphalt layer in each analysis period and substitute it into the dynamic modulus master curve to obtain the dynamic modulus of the asphalt layer in each analysis period;
[0016] Step 6: Calculate the tensile stress at the bottom of the semi-rigid base layer under the standard axle load based on the elastic layered theory system, and combine the fatigue life prediction model to obtain the cumulative number of fatigue life actions of the semi-rigid base layer. Convert the axle load data obtained by the traffic dynamic weighing device to obtain the cumulative equivalent axle load action times of the semi-rigid base layer at the end of each analysis period.
[0017] Step 7, determining the modulus value of the semi-rigid base layer for each analysis period;
[0018] Step 8, for each analysis period, according to the dynamic modulus of the asphalt layer of the semi-rigid base material and the modulus value of the semi-rigid base, combined with the pavement structure parameters, based on the elastic layered theory system, calculate the tensile strain of the bottom of the asphalt layer of each axle type acting on each axle load interval;
[0019] Step 9, substitute the tensile strain of the bottom of the asphalt layer of each axle type in each axle load range during each analysis period into the asphalt fatigue damage model, calculate the asphalt layer damage caused by a single traffic load of each axle type in each axle load range, and obtain the fatigue damage of the asphalt layer of the pavement structure during the entire total analysis period.
[0020] Preferably, the pavement structure of the asphalt pavement is arranged from top to bottom as an asphalt layer, a semi-rigid base layer and a soil base, wherein a plurality of structural layers are arranged in the asphalt layer, which are an upper layer, a middle layer and a lower layer from top to bottom, and the semi-rigid base layer is arranged as a single-layer structure or a double-layer structure.
[0021] Preferably, the calculation formula for the combined axle load spectrum is:
[0022]
[0023] Where i is the axle type number, 1≤i≤4 and i is a positive integer, where i=1 is a single axle and single tire; i=2 is a single axle and dual tire, i=3 is a double axle, and i=4 is a triple axle; j is the axle weight interval number, j=1, 2, ..., N, N is the total number of axle weight intervals; m is the vehicle type number, 1≤m≤M and m is a positive integer, M is the total number of vehicle types; JALDF ij The NAPT is the combined axle load spectrum, which is used to indicate the percentage of different axle types in different axle load ranges. mi is the average number of axles of axle type i in the mth type of vehicle; ALDF mij is the axle load distribution coefficient of axle type i in the j-level axle load range of the m-th type vehicle; VTDC m is the wheel type distribution coefficient of the mth type of vehicle.
[0024] Preferably, in step 7, the modulus value of the semi-rigid base layer in the first analysis period is obtained by the repeated fatigue loading test in step 3;
[0025] The process of determining the modulus value of the semi-rigid base layer in the remaining analysis period is as follows:
[0026] If at the end of the current analysis period, the cumulative equivalent axial load action times of the semi-rigid base is less than the cumulative action times of the fatigue life of the semi-rigid base calculated in step 6, the modulus attenuation model is used to calculate the modulus value of the semi-rigid base in the next analysis period;
[0027] If at the end of the current analysis period, the cumulative number of equivalent axial load actions on the semi-rigid base is not less than the cumulative number of actions of the fatigue life of the semi-rigid base calculated in step 6, the modulus value of the semi-rigid base is set to a fixed value in the range of 500 to 2000 MPa.
[0028] Preferably, when the semi-rigid base layer is a double-layer structure, when the modulus value of the semi-rigid base layer is calculated using the modulus attenuation model, the calculation position of the modulus attenuation model is set at the bottom of the semi-rigid base layer.
[0029] Preferably, in step 9, the asphalt fatigue damage model is:
[0030]
[0031] in,
[0032]
[0033]
[0034] Where D ij N is the fatigue damage of the asphalt layer caused by axle type i passing through the pavement structure once within the j-level axle load range during the analysis period; fij is the fatigue life of the pavement structure when axle type i passes through the pavement structure once in the jth axle load range during the analysis period; β is the target reliability; k a k is the adjustment coefficient for seasonal frozen soil areas; b is the fatigue loading mode coefficient; k T1 is the temperature adjustment coefficient; E a is the dynamic modulus of asphalt mixture; VFA is the asphalt saturation of asphalt mixture; h a is the thickness of asphalt mixture layer; aij It is the tensile strain at the bottom of the asphalt layer generated when axle type i passes through the pavement structure in the j-th axle load range.
[0035] Preferably, the fatigue damage of the asphalt layer of the pavement structure during the total analysis period is:
[0036]
[0037] Where D is the fatigue damage of the asphalt layer of the pavement structure during the total analysis period; AADTT is the initial annual average daily traffic volume of two-way vehicles with six or more wheels on two axles measured by the traffic dynamic weighing device; DDF is the directional coefficient; LDF is the lane coefficient.
[0038] The beneficial technical effects brought by the present invention are:
[0039] The present invention proposes a pavement fatigue damage prediction system that takes into account the attenuation of the semi-rigid base modulus. By real-time measuring the traffic volume, axle load spectrum and temperature field data of the pavement structure, the specific values of the pavement structure material parameters after the pavement structure traffic volume increases are accurately obtained, providing important process data for the accurate prediction of pavement fatigue damage.
[0040] The present invention also proposes a pavement fatigue damage prediction method taking into account the modulus attenuation of the semi-rigid base layer, which fully considers the influence of the modulus attenuation of the semi-rigid base layer on the pavement fatigue damage, and cooperates with the modulus determination method of the semi-rigid base material taking into account the modulus attenuation. By observing the operation of the pavement structure during its service life, the elastic layered theoretical system is used to obtain the mechanical response of the bottom layer of the asphalt pavement structure during different analysis periods, thereby achieving accurate prediction of the fatigue damage of the pavement structure, which is beneficial to the formulation of the structural design plan and maintenance and repair decision of the asphalt pavement, and lays the foundation for the safe operation of the pavement structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] Figure 1 Schematic diagram of the pavement structure of the experimental section.
[0042] Figure 2 It is the load spectrum of single-axis single-tire axle.
[0043] Figure 3 It is the load spectrum of single-axis and double-axle.
[0044] Figure 4 It is the load spectrum of double-axle shaft.
[0045] Figure 5 It is the load spectrum of the triple axis.
[0046] Figure 6 is the dynamic modulus master curve of the asphalt layer, among which SMA13 is the dynamic modulus master curve of the upper layer, AC-20 is the dynamic modulus master curve of the middle layer, and AC-25 is the dynamic modulus master curve of the lower layer.
[0047] Figure 7 This is a graph showing the cumulative fatigue development trend of the pavement structure.
[0048] In the figure, 1 is the upper layer, 2 is the middle layer, 3 is the lower layer, 4 is the semi-rigid base layer, 5 is the semi-rigid subbase layer, and 6 is the soil base. DETAILED DESCRIPTION
[0049] The present invention is further described in detail below in conjunction with the accompanying drawings and embodiments.
[0050] Example 1
[0051] This embodiment takes a highway in a certain area as an example, and selects an asphalt road surface as an experimental section on the highway. Figure 1 As shown, the experimental road section comprises an asphalt layer, a semi-rigid base layer, a semi-rigid subbase layer and a soil base 6 from top to bottom, wherein a plurality of structural layers are arranged in the asphalt layer, which are an upper layer 1, a middle layer 2 and a lower layer 3 from top to bottom, which are respectively arranged as SMA-13 layer, AC-20 layer and AC-25 layer, and the semi-rigid base layer 4 and the semi-rigid subbase layer 5 are both cement-stabilized gravel layers, which are paved with cement-stabilized gravel.
[0052] A pavement fatigue damage prediction system considering the attenuation of the semi-rigid base modulus is installed on the experimental road section. The pavement fatigue damage prediction system considering the attenuation of the semi-rigid base modulus in this embodiment includes a traffic dynamic weighing device, a pavement structure temperature field measuring device and a pavement data processing device, wherein the traffic dynamic weighing device is buried on the top of the asphalt layer of the pavement structure, and is used to collect the vehicle type, speed and axle load data of the vehicle traveling on the pavement structure; the pavement structure temperature field measuring device is buried at different depths of the pavement structure, and is used to measure the internal temperature of each structural layer in the pavement structure; the pavement data processing device is respectively connected to the traffic dynamic weighing device and the pavement structure temperature field measuring device, and is used to receive, store and process the measurement data of the traffic axle load measuring device and the pavement structure temperature field measuring device, and calculate and output the pavement fatigue damage considering the attenuation of the semi-rigid base modulus.
[0053] The pavement fatigue damage prediction system considering the attenuation of the semi-rigid base modulus is used to obtain the real-time axle load spectrum and temperature field of the test section in real time, and the pavement fatigue damage prediction method considering the attenuation of the semi-rigid base modulus proposed by the present invention is used to predict the pavement fatigue damage of the test section, which specifically includes the following steps:
[0054] Step 1: Set the total duration of pavement fatigue damage prediction to 15 years, and divide the total duration of pavement fatigue damage prediction into 180 analysis periods on a monthly basis.
[0055] Step 2: Use a traffic dynamic weighing device to obtain the vehicle type, speed and axle load data of vehicles traveling on the road, and calculate the joint axle load spectrum of each analysis period.
[0056] In this embodiment, the traffic dynamic weighing device is used to obtain the axle load spectra of 11 types of axle-type vehicles, the two-way initial annual average daily traffic volume AADTT of two-axle vehicles with more than six wheels in each analysis period, the direction coefficient DDF, the lane coefficient LDF and the wheel type distribution coefficient, and the combined axle load spectra of various axle types are calculated, as shown in formula (1):
[0057]
[0058] Wherein, i is the axle type number, 1≤i≤4 and i is a positive integer, wherein i=1 is a single axle and a single tire; i=2 is a single axle and a double tire, i=3 is a double axle, and i=4 is a triple axle; j is the axle weight interval number, j=1,2,...,N, where N is the total number of axle weight intervals; m is the vehicle type number, 1≤m≤M and m is a positive integer, where M is the total number of vehicle types. In this embodiment, the total number of vehicle types M is 11; JALDF ij is the combined axle load spectrum, which is used to indicate the percentage of axle type i in the jth axle load interval, that is, the percentage of different axle types in different axle load intervals; NAPT miis the average number of axles of axle type i in the mth type of vehicle; ALDF mij is the axle load distribution coefficient of axle type i in the j-level axle load range of the m-th type vehicle; VTDC m is the wheel type distribution coefficient of the mth type of vehicle.
[0059] In this embodiment, the two-way initial annual average daily traffic volume AADTT and the wheel type distribution coefficient of dual-axle six-wheel or more vehicles in the 1st to 12th analysis periods are shown in Table 1, and the wheel type distribution coefficient in the 1st to 12th analysis periods is shown in Table 2. The direction coefficient DDF is 0.5 and the lane coefficient LDF is 0.5. Figure 2 to Figure 5 is the combined shaft load spectrum of various shaft types, among which, Figure 2 is the single-axis single-tire axle load spectrum, Figure 3 is the single-axis double-axle load spectrum, Figure 4 is the double-axle load spectrum, Figure 5 It is the load spectrum of the triple axis.
[0060] Table 1 AADTT in the 1st to 12th analysis period
[0061] Analysis period 1 2 3 4 5 6 7 8 9 10 11 12 AADTT 1996 1607 2205 2849 2994 3231 2838 2603 3372 2850 2342 1876
[0062] Table 2 Distribution coefficients of wheel types in the 1st to 12th analysis periods
[0063]
[0064] Step 3, prepare a semi-rigid base material specimen according to the material parameters of the pavement structure, and use the semi-rigid base material specimen to perform a flexural tensile strength test and a repeated fatigue loading test. In this embodiment, the flexural tensile strength of the flexural tensile strength test is set to 1.9 MPa, and the repeated fatigue loading test is performed using different stress ratios. The fatigue life data and modulus attenuation data of the semi-rigid base material specimen are collected, and the fatigue life prediction model and modulus attenuation model are determined by performing regression analysis on the fatigue life data and modulus attenuation data of the semi-rigid base material specimen:
[0065]
[0066] Where N is the number of fatigue loading actions; is stress ratio; σ is stress, unit is MPa; S is bending strength, unit is MPa; E N is the bending modulus of the semi-rigid base material when the number of fatigue loading is N, in MPa; E0 is the initial bending modulus of the semi-rigid base material, in MPa; e is a natural constant.
[0067] Step 4: prepare asphalt mixture specimens of each structural layer according to the material parameters of the pavement structure, conduct uniaxial dynamic compression modulus tests on the asphalt mixture specimens at different temperatures and frequencies, perform fitting analysis on the test results of the uniaxial dynamic compression modulus test, and determine the dynamic modulus master curve of each structural layer in the asphalt layer, such as Figure 6 shown.
[0068] Step 5: Use a pavement structure temperature field measurement device to measure the average temperature of the asphalt layer in each analysis period and substitute it into the dynamic modulus master curve to obtain the dynamic modulus of the asphalt layer in each analysis period.
[0069] In this embodiment, the dynamic modulus of each structural layer in the asphalt layer in the 1st to 12th analysis periods is shown in Table 3.
[0070] Table 3 Dynamic modulus of each structural layer in the asphalt layer in the 1st to 12th analysis period
[0071]
[0072] Step 6, according to the initial parameters of the pavement structure, as shown in Table 4. Based on the elastic layered theory system, the tensile stress at the bottom of the semi-rigid base layer under the standard axle load is calculated to be 0.174. Combined with the fatigue life prediction model in step 3, the cumulative number of fatigue life actions of the semi-rigid base layer is 5.1×10 9 .
[0073] Table 4 Initial parameters of pavement structure
[0074]
[0075] According to the Highway Asphalt Pavement Design Specifications, the axle load data obtained by the traffic dynamic weighing device were converted to obtain the cumulative equivalent axle load times of the semi-rigid base at the end of each analysis period, as shown in Table 5.
[0076] Table 5 Cumulative equivalent axle load times of semi-rigid base at the end of each analysis period
[0077]
[0078]
[0079] Step 7, determining the modulus value of the semi-rigid base layer in each analysis period, wherein the modulus value of the semi-rigid base layer in the first analysis period is obtained by the repeated fatigue loading test in step 3; the modulus value of the semi-rigid base layer in the remaining analysis periods is determined by:
[0080] If at the end of the current analysis period, the cumulative number of equivalent axial load actions on the semi-rigid base is less than the cumulative number of actions of the fatigue life of the semi-rigid base calculated in step 6, the modulus attenuation model is used to calculate the modulus value of the semi-rigid base in the next analysis period.
[0081] If at the end of the current analysis period, the cumulative number of equivalent axial load actions on the semi-rigid base is not less than the cumulative number of actions of the fatigue life of the semi-rigid base calculated in step 6, the modulus value of the semi-rigid base is set to a fixed value in the range of 500 to 2000 MPa.
[0082] In this embodiment, the modulus value of the semi-rigid base layer in each analysis period decays according to the modulus decay model, the equivalent cumulative number of axle load actions at the end of each analysis period, and the stress ratio of the pavement structure in the previous analysis period, and the modulus value of the semi-rigid base layer begins to take a fixed value in the 147th analysis period, as shown in Table 6.
[0083] Table 6 Semi-rigid base modulus values for each analysis period
[0084]
[0085] Step 8, according to the dynamic modulus of the asphalt layer of the semi-rigid base material and the modulus value of the semi-rigid base material in each analysis period, combined with the pavement structure parameters (including the pavement structure thickness and Poisson's ratio), based on the elastic layered theory system, calculate the tensile strain of the bottom of the asphalt layer of each axle type acting on each axle load interval in each analysis period. In this embodiment, the middle value of each axle load interval is taken as the axle load to calculate the tensile strain of the bottom of the asphalt layer. Some axle load intervals are shown in Table 7.
[0086] Table 7 Strain of the single-axle twin tire in the axle load range [108 kN, 112.5 kN] for the 1st to 12th analysis period
[0087]
[0088] Step 9, based on the tensile strain at the bottom of the asphalt layer of each axle type acting on each axle load range during each analysis period, use the asphalt fatigue damage model to calculate the asphalt layer damage caused by a single traffic load for each axle type in each axle load range, and obtain the asphalt layer fatigue damage of the pavement structure during the entire total analysis period.
[0089] In this embodiment, the asphalt fatigue damage model is:
[0090]
[0091] in,
[0092]
[0093]
[0094] Where D ij N is the fatigue damage of the asphalt layer caused by axle type i passing through the pavement structure once within the j-level axle load range during the analysis period; fij is the fatigue life of the pavement structure when axle type i passes through the pavement structure once in the jth axle load range during the analysis period; β is the target reliability; k a k is the adjustment coefficient for seasonal frozen soil areas; b is the fatigue loading mode coefficient; k T1 is the temperature adjustment coefficient; E a is the dynamic modulus of asphalt mixture; VFA is the asphalt saturation of asphalt mixture; h a is the thickness of the asphalt mixture layer, in mm; ε aij It is the tensile strain at the bottom of the asphalt layer generated when axle type i passes through the pavement structure in the j-th axle load range.
[0095] In this embodiment, the median of the axle weight range is taken as the calculated axle load when calculating the tensile strain at the bottom of the asphalt layer. The mechanical response calculation module in the existing technology "Daokedaowang" system platform (i.e., an online design system for asphalt pavement structure for national highway-related research institutes and design institutes) is used to calculate the load based on the elastic layered system theory. During the calculation process, the calculation section position is set with reference to the Asphalt Pavement Mechanical-Empirical Design Method (MEPDG) and "JTG D50-2017 Highway Asphalt Pavement Design Code" to set relevant pavement structure parameters.
[0096] Based on the fatigue damage of the asphalt layer caused by a single pass of each axle type through the pavement structure in different axle load ranges during each analysis period, combined with the initial annual average daily traffic volume, directional coefficient and lane coefficient of two-way vehicles with six or more wheels on two axles measured by the traffic dynamic weighing device, the fatigue damage of the asphalt layer of the pavement structure during the total analysis period is obtained, as shown in formula (5):
[0097]
[0098] Where D is the fatigue damage of the asphalt layer of the pavement structure during the total analysis period; AADTT is the initial annual average daily traffic volume of two-way vehicles with six or more wheels on two axles measured by the traffic dynamic weighing device; DDF is the directional coefficient; LDF is the lane coefficient.
[0099] In this embodiment, the fatigue damage of the asphalt layer of the pavement structure during the entire analysis period is calculated to be 0.56, and the cumulative fatigue development trend of the pavement structure is further obtained, such as Figure 7 As shown, analysis Figure 7 It can be seen that after the modulus of the semi-rigid base layer decays to a fixed value, the fatigue damage of the asphalt pavement increases rapidly.
[0100] It can be seen that the method of the present invention fully considers the influence of the attenuation of the modulus of the semi-rigid base layer on the fatigue damage of the pavement. The axle load spectrum and temperature field collected in real time by the system of the present invention can accurately predict the fatigue damage of the pavement structure, and provide a basis for the control design and maintenance decision-making of the asphalt pavement structure.
[0101] Of course, the above description is not a limitation of the present invention, and the present invention is not limited to the above examples. Changes, modifications, additions or substitutions made by technicians in this technical field within the essential scope of the present invention should also fall within the protection scope of the present invention.
Claims
1. A pavement fatigue damage prediction system considering the attenuation of semi-rigid base modulus, characterized in that: It includes a traffic dynamic weighing device, a pavement structure temperature field measuring device and a pavement data processing device; The traffic dynamic weighing device is buried on the top of the asphalt layer of the pavement structure and is used to collect the vehicle type, speed and axle load data of the vehicles traveling on the pavement structure; The pavement structure temperature field measuring device is buried at different depths of the pavement structure and is used to measure the internal temperature of each structural layer in the pavement structure; The pavement data processing device is connected to the traffic dynamic weighing device and the pavement structure temperature field measuring device respectively, and is used to receive, store and process the measurement data of the traffic axle load measuring device and the pavement structure temperature field measuring device, calculate and output the pavement fatigue damage considering the attenuation of the semi-rigid base modulus.
2. A pavement fatigue damage prediction method considering the attenuation of semi-rigid base modulus, characterized in that: The pavement fatigue damage prediction system considering the attenuation of the semi-rigid base modulus as claimed in claim 1 comprises the following steps: Step 1, set the total duration of pavement fatigue damage prediction and divide it into multiple analysis periods by month; Step 2, using a traffic dynamic weighing device to obtain the vehicle type, speed and axle load data of vehicles traveling on the road, and calculate the joint axle load spectrum of each analysis period; Step 3, preparing a semi-rigid base material specimen according to the material parameters of the pavement structure, and using the semi-rigid base material specimen to conduct a bending tensile strength test and a repeated fatigue loading test to determine a fatigue life prediction model and a modulus attenuation model; Step 4, preparing asphalt mixture specimens of each structural layer according to the material parameters of the pavement structure, and conducting a uniaxial dynamic compression modulus test using the asphalt mixture specimens to determine the dynamic modulus master curve of each structural layer; Step 5, using a pavement structure temperature field measurement device to measure the average temperature of the asphalt layer in each analysis period and substitute it into the dynamic modulus master curve to obtain the dynamic modulus of the asphalt layer in each analysis period; Step 6: Calculate the tensile stress at the bottom of the semi-rigid base layer under the standard axle load based on the elastic layered theory system, and combine the fatigue life prediction model to obtain the cumulative number of fatigue life actions of the semi-rigid base layer. Convert the axle load data obtained by the traffic dynamic weighing device to obtain the cumulative equivalent axle load action times of the semi-rigid base layer at the end of each analysis period. Step 7, determining the modulus value of the semi-rigid base layer for each analysis period; Step 8, for each analysis period, according to the dynamic modulus of the asphalt layer of the semi-rigid base material and the modulus value of the semi-rigid base, combined with the pavement structure parameters, based on the elastic layered theory system, calculate the tensile strain of the bottom of the asphalt layer of each axle type acting on each axle load interval; Step 9, substitute the tensile strain of the bottom of the asphalt layer of each axle type in each axle load range during each analysis period into the asphalt fatigue damage model, calculate the asphalt layer damage caused by a single traffic load of each axle type in each axle load range, and obtain the fatigue damage of the asphalt layer of the pavement structure during the entire total analysis period.
3. The pavement fatigue damage prediction method considering the attenuation of the semi-rigid base modulus according to claim 2 is characterized in that: The pavement structure of the asphalt pavement is arranged from top to bottom as an asphalt layer, a semi-rigid base layer and a soil base, wherein a plurality of structural layers are arranged in the asphalt layer, which are an upper layer, a middle layer and a lower layer from top to bottom, and the semi-rigid base layer is arranged as a single-layer structure or a double-layer structure.
4. The pavement fatigue damage prediction method considering the attenuation of the semi-rigid base modulus according to claim 2 is characterized in that: The calculation formula of the combined axle load spectrum is: Where i is the axle type number, 1≤i≤4 and i is a positive integer, where i=1 is a single axle and single tire; i=2 is a single axle and dual tire, i=3 is a double axle, and i=4 is a triple axle; j is the axle weight interval number, j=1,2,…,N, N is the total number of axle weight intervals; m is the vehicle type number, 1≤m≤M and m is a positive integer, M is the total number of vehicle types; JALDF ij The NAPT is the combined axle load spectrum, which is used to indicate the percentage of different axle types in different axle load ranges. mi is the average number of axles of axle type i in the mth type of vehicle; ALDF mij is the axle load distribution coefficient of axle type i in the j-level axle load range of the m-th type vehicle; VTDC m is the wheel type distribution coefficient of the mth type of vehicle.
5. The pavement fatigue damage prediction method considering the attenuation of the semi-rigid base modulus according to claim 2 is characterized in that: In step 7, the modulus value of the semi-rigid base layer in the first analysis period is obtained by the repeated fatigue loading test in step 3; The process of determining the modulus value of the semi-rigid base layer in the remaining analysis period is as follows: If at the end of the current analysis period, the cumulative equivalent axial load action times of the semi-rigid base is less than the cumulative action times of the fatigue life of the semi-rigid base calculated in step 6, the modulus attenuation model is used to calculate the modulus value of the semi-rigid base in the next analysis period; If at the end of the current analysis period, the cumulative number of equivalent axial load actions on the semi-rigid base is not less than the cumulative number of actions of the fatigue life of the semi-rigid base calculated in step 6, the modulus value of the semi-rigid base is set to a fixed value in the range of 500 to 2000 MPa.
6. The pavement fatigue damage prediction method considering the attenuation of the semi-rigid base modulus according to claim 5 is characterized in that: When the semi-rigid base layer is a double-layer structure, when the modulus value of the semi-rigid base layer is calculated using the modulus attenuation model, the calculation position of the modulus attenuation model is set at the bottom of the semi-rigid base layer.
7. The pavement fatigue damage prediction method considering the attenuation of the semi-rigid base modulus according to claim 4 is characterized in that: In step 9, the asphalt fatigue damage model is: in, Where D ij N is the fatigue damage of the asphalt layer caused by axle type i passing through the pavement structure once within the j-level axle load range during the analysis period; fij is the fatigue life of the pavement structure when axle type i passes through the pavement structure once in the jth axle load range during the analysis period; β is the target reliability; k a k is the adjustment coefficient for seasonal frozen soil areas; b is the fatigue loading mode coefficient; k T1 is the temperature adjustment coefficient; E a is the dynamic modulus of asphalt mixture; VFA is the asphalt saturation of asphalt mixture; h a is the thickness of asphalt mixture layer; aij It is the tensile strain at the bottom of the asphalt layer generated when axle type i passes through the pavement structure in the j-th axle load range.
8. The pavement fatigue damage prediction method considering the attenuation of the semi-rigid base modulus according to claim 7 is characterized in that: The fatigue damage of the asphalt layer of the pavement structure during the total analysis period is: Where D is the fatigue damage of the asphalt layer of the pavement structure during the total analysis period; AADTT is the initial annual average daily traffic volume of two-way vehicles with six or more wheels on two axles measured by the traffic dynamic weighing device; DDF is the directional coefficient; LDF is the lane coefficient.
Citation Information
Patent Citations
Fatigue control designing method of semi-rigid base asphalt pavement
CN103088737A
Asphalt pavement base damage judgment method based on deflection basin parameters
CN110362930A
Method for estimating fatigue damage of full-flexible asphalt pavement structure under action of multi-axis group load
CN117473597A
Asphalt pavement fatigue life prediction method considering semi-rigid base cracking
CN118094713A
Highway bituminous pavement structure real -time supervision device
CN206189245U
Cited By
Road fatigue damage prediction method, system, equipment, medium and program product
CN120708403A
Road fatigue damage prediction method, system, device, medium and program product
CN120708403B
Highway traffic volume axle load dynamic high-precision detection method
CN120932477A
A dynamic high-precision detection method for highway traffic volume and axle load
CN120932477B
Method for dynamically predicting life of concrete pavement in full life cycle under multi-field coupling action based on tension-compression difference