Semiconductor memory device and manufacturing method thereof
By using the direct contact portion of the upper metal layer and the lower silicide layer in semiconductor memory devices, combined with heat treatment technology, the contact resistance and defect problems in semiconductor memory device manufacturing are solved, and the performance and reliability of the device are improved.
Patent Information
- Application Number
- CN202410197691.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-25
- Filing Date
- 2024-02-22
- Publication Date
- 2024-11-26
AI Technical Summary
With the increasing integration of semiconductor memory devices, manufacturing processes become more complex and difficult, especially when design rules are reduced, it is difficult to effectively reduce contact resistance and reduce necking and cutting defects.
Using direct contact portions including metal upper layer and silicide lower layer, direct contact holes are formed in the cell array area of the substrate, the active region is exposed, and the lower silicide is combined with the metal upper layer by heat treatment, reducing contact resistance and reducing Voids appearing in polysilicon.
It effectively reduces contact resistance, reduces necking and cutting defects caused by narrow areas, and improves the performance and reliability of semiconductor devices.
Smart Images

Figure CN119031705A_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims the priority of Korean Patent Application No. 10-2023-0067545 filed on May 25, 2023 in the Korean Intellectual Property Office, the entire contents of which are incorporated herein by reference. Technical Field
[0003] The present disclosure relates to a semiconductor device and a method for manufacturing the same, and more particularly, to a semiconductor memory device and a method for manufacturing the same. Background Art
[0004] As the integration of semiconductor memory devices increases, circuits become more sophisticated, thereby reducing design rules. As a result, the manufacturing process of semiconductor memory devices becomes more complex and difficult. Summary of the invention
[0005] An embodiment of the present disclosure provides a semiconductor memory device, comprising: a substrate having a cell array region and a core region located near the cell array region; a buried contact portion located in the cell array region and connected to a storage element; a direct contact portion located in the cell array region and comprising an upper layer and a lower layer; a bit line contacting the upper layer of the direct contact portion; and a word line crossing the bit line, wherein the lower layer of the direct contact portion is located in a direct contact hole of the substrate, the direct contact hole exposes the active region of the substrate, the lower layer contacts the active region of the substrate through the bottom surface of the direct contact hole, the upper layer comprises a metal, and the lower layer comprises a silicide of the metal.
[0006] An embodiment of the present disclosure provides a method for manufacturing a semiconductor memory device, the manufacturing method comprising: forming a direct contact hole by stacking a cell insulating film on a cell array region of a substrate and etching the cell insulating film, the direct contact hole exposing an active area of the substrate; forming a lower layer on the exposed active area and in the direct contact hole, the lower layer comprising a semiconductor; forming an upper layer on the lower layer, the upper layer comprising a metal; converting at least a portion of the lower layer into a silicide of the metal; forming a bit line on the upper layer; and forming a direct contact portion by etching the upper and lower layers using the bit line as a mask. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Features will become apparent to those skilled in the art by describing in detail exemplary embodiments with reference to the accompanying drawings, in which:
[0008] Figure 1 is a partial plan view of a cell array region of a semiconductor device according to an embodiment of the present disclosure.
[0009] Figures 2 to 5 Along Figure 1Cross-sectional views taken along lines AA, BB, CC and DD.
[0010] Figures 6 to 10 yes Figure 2 A cross-sectional view of a semiconductor device at a stage in the manufacturing process. DETAILED DESCRIPTION
[0011] In the following detailed description, only certain exemplary embodiments of the present disclosure are shown and described by way of illustration only. As will be appreciated by those skilled in the art, the described embodiments may be modified in a variety of different ways, all without departing from the spirit or scope of the present disclosure. Therefore, the drawings and descriptions should be considered illustrative rather than restrictive in nature. Throughout the specification, similar reference numerals represent similar elements.
[0012] Figure 1 is a diagram showing a partial structure of a cell array region CA of a semiconductor device according to an embodiment of the present disclosure. Figures 2 to 5 Along Figure 1 Cross-sectional views taken along lines AA, BB, CC and DD. Figure 2 , Figure 4 and Figure 5 A portion of the core area CORE excluding the cell array area CA is shown. Although the drawings show a dynamic random access memory (DRAM), example embodiments may be implemented in any suitable semiconductor device.
[0013] refer to Figure 1 and Figure 2 , the semiconductor device according to the embodiment of the present disclosure may include a cell array region CA and a core region CORE. The core region CORE may be located near the cell array region CA, for example, adjacent to the cell array region CA.
[0014] The cell array region CA may include a plurality of active regions AC. The active regions AC may be formed in Figure 2 The substrate 10 Figure 2 As the design rules of semiconductor devices are reduced, the active area AC can be arranged in the form of diagonal or oblique lines (eg, relative to the direction of the word line WL), such as Figure 1 shown.
[0015] A plurality of word lines WL may intersect the active region AC to form a plurality of gate electrodes. The plurality of word lines WL may extend parallel to each other in, for example, a first direction (x-axis direction) and may be arranged at uniform intervals. The width of each word line WL or the gap between adjacent word lines in the word line WL may be determined according to a design rule.
[0016] Each of the active regions AC may cross two word lines WL, thereby being divided into three parts, wherein the middle part may be a bit line connection region, and the end part may be a storage element connection region. Since the active region AC extends in a diagonal direction, the angle formed by the word line WL and the active region AC may be less than 90°.
[0017] A plurality of bit lines BL may cross the word line WL, and may be, for example, orthogonal to the word line WL. A plurality of bit lines BL may each extend in, for example, the second direction (y-axis direction), and may be located on the word line WL. A plurality of bit lines BL may be arranged parallel to each other at uniform intervals. The width of the bit line BL or the gap between the bit lines BL may be determined according to a design rule.
[0018] The semiconductor device according to the embodiment of the present disclosure may include various types of contact structures on the active region AC. Figure 1 As shown, a semiconductor device according to example embodiments may include a direct contact DC, a buried contact BC, a landing pad LP, and the like.
[0019] The direct contact DC may be a contact structure electrically connecting the active area AC to the bit line BL. The buried contact BC may be a contact structure connecting the active area AC to the lower electrode of the capacitor.
[0020] In the arrangement structure of the buried contact BC, the contact area between the buried contact BC and the active area AC can be small, and a conductive landing pad LP can be used between the active area AC and the buried contact BC to increase the contact area. Alternatively, the landing pad LP can be inserted between the buried contact BC and the lower electrode of the capacitor to increase the contact area between the lower electrode of the capacitor and the buried contact BC. The contact resistance between the active area AC and the lower electrode of the capacitor can be reduced by increasing the contact area through the landing pad LP.
[0021] The direct contact DC may be connected to the bit line connection region of the active region AC, and the buried contact BC may be connected to the storage element connection region. Therefore, the landing pad LP may be adjacent to or partially (or completely) overlap the buried contact BC of the active region AC. In other words, the buried contact BC may be formed to overlap the active region AC and the isolation layer 14A between adjacent word lines WL and between adjacent bit lines BL.
[0022] The plurality of buried contacts BC may be arranged to be spaced apart from each other in the first direction (x-axis direction) and the second direction (y-axis direction).
[0023] In an embodiment of the present disclosure, the word line WL may be buried in the substrate 10. The word line WL may be arranged to cross the active region AC between direct contacts DC or between buried contacts BC.
[0024] The direct contact portion DC may be arranged symmetrically and thus be arranged in a line in the first direction (x-axis direction) and the second direction (y-axis direction). The buried contact portion BC may also be arranged symmetrically and thus be arranged in a line in the first direction (x-axis direction) and the second direction (y-axis direction). However, unlike the direct contact portion DC and the buried contact portion BC, the landing pad LP may be arranged in a Z shape in the second direction (y-axis direction) in which the bit line BL extends. Alternatively, the landing pad LP may be arranged to overlap with the same side of the bit line BL in the first direction (x-axis direction) in which the word line WL extends. For example, the landing pad LP in the first column may overlap with the left side of the bit line BL corresponding thereto, and the landing pad LP in the second column may overlap with the right side of the corresponding bit line BL.
[0025] refer to Figures 2 to 5 , a semiconductor device according to an embodiment of the present disclosure includes a substrate 10 .
[0026] The substrate 10 may include a cell array region CA and a core region CORE separated from each other by a cell region separation layer 14C. The cell array region CA and the core region CORE may include active regions 12A and 12B defined by isolation layers 14A and 14B, respectively. That is, since the active regions 12A and 12B are defined by the isolation layers 14A and 14B, the isolation layers 14A and 14B are arranged around the active regions 12A and 12B.
[0027] In the cell array region CA, the plurality of active regions 12A may each have a relatively long island shape having a short axis and a long axis, such as Figure 1 shown in top view. Figures 2 to 5 The active region 12A in corresponds to Figure 1 The active area AC in.
[0028] For example, the substrate 10 may be a silicon substrate or a silicon on insulator (SOI). In another example, the substrate 10 may include silicon germanium, silicon germanium on insulator (SGOI), indium antimonide, lead telluride, indium arsenide, indium phosphide, gallium arsenide, or gallium antimonide.
[0029] The isolation layers 14A and 14B and the cell region separation layer 14C may have a shallow trench isolation (STI) structure, which has excellent isolation characteristics. The isolation layers 14A and 14B and the cell region separation layer 14C may include silicon oxide, silicon nitride, silicon oxynitride, or a combination thereof. For example, Figures 2 to 5 As shown, the isolation layers 14A and 14B and the cell region separation layer 14C may be a single layer. In another example, the isolation layers 14A and 14B and the cell region separation layer 14C may be formed as one insulating layer or multiple insulating layers according to their widths. Figures 2 to 5 As shown, the upper surfaces of the isolation layers 14A and 14B and the upper surface of the cell region separation layer 14C may be flush with the upper surface of the substrate 10 .
[0030] The semiconductor device according to an embodiment of the present disclosure may include a word line having a buried structure in the cell array region CA. In an embodiment of the present disclosure, a cell gate structure GS including a structure corresponding to the word line may be formed in the substrate 10 and the isolation layer 14A.
[0031] The cell gate structure GS may intersect the isolation layer 14A and the active region 12A defined by the isolation layer 14A. The cell gate structure GS may include a cell gate insulating layer 22, a cell gate electrode 24, and a cell gate cap 26. Here, the cell gate electrode 24 may correspond to Figure 1 For example, the cell gate structure GS may further include a cell gate capping conductive layer.
[0032] refer to Figure 3 , a cell gate insulating layer 22 may be formed along the sidewall and bottom surface of the cell gate trench T1 according to the profile of at least a portion of the cell gate trench T1. The cell gate insulating layer 22 may include, for example, at least one of silicon oxide, silicon nitride, silicon oxynitride, or a high-k material having a dielectric constant higher than that of silicon oxide. The high-k material may include, for example, at least one of hafnium oxide, hafnium silicon oxide, hafnium aluminum oxide, lanthanum oxide, lanthanum aluminum oxide, zirconium oxide, zirconium silicon oxide, tantalum oxide, titanium oxide, barium strontium titanium oxide, barium titanium oxide, strontium titanium oxide, yttrium oxide, aluminum oxide, lead scandium tantalum oxide, lead zinc niobate, or a combination thereof.
[0033] The cell gate electrode 24 may be formed on the cell gate insulating layer 22 . The cell gate electrode 24 may fill a portion of the cell gate trench T1 . When the cell gate capping conductive layer is provided, the cell gate capping conductive layer may extend along an upper surface of the cell gate electrode 24 .
[0034] The cell gate electrode 24 may include, for example, at least one of the following: a metal, a metal alloy, a conductive metal nitride, a conductive metal carbonitride, a conductive metal carbide, a metal silicide, a doped semiconductor material, a conductive metal oxynitride, and a conductive metal oxide. The cell gate electrode 24 may include, for example, at least one of the following: TiN, TaC, TaN, TiSiN, TaSiN, TaTiN, TiAlN, TaAlN, WN, Ru, TiAl, TiAlC-N, TiAlC, TiC, TaCN, W, Al, Cu, Co, Ti, Ta, Ni, Pt, Ni-Pt, Nb, NbN, NbC, Mo, MoN, MoC, WC, Rh, Pd, Ir, Ag, Au, Zn, V, RuTiN, TiSi, TaSi, NiSi, CoSi, IrOx 、RuO x The cell gate capping conductive layer may include, for example, polysilicon or polysilicon-germanium.
[0035] The cell gate capping 26 may be disposed on the cell gate electrode 24 (or the cell gate capping conductive layer). The cell gate capping 26 may fill the remaining space of the cell gate trench T1 not occupied by the cell gate electrode 24. Figure 3 As shown, a cell gate insulating layer 22 may be formed along the sidewall of the cell gate cap 26. The cell gate cap 26 may include, for example, at least one of the following: silicon nitride (SiN), silicon oxynitride (SiON), silicon oxide (SiO 2 ), silicon carbonitride (SiCN), silicon oxycarbonitride (SiOCN), or a combination thereof.
[0036] For example, an impurity-containing region into which impurities are implanted may be disposed on at least one side of the cell gate structure GS. The impurity-containing region may be a source / drain region of a transistor.
[0037] like Figure 2 As shown, Figure 1 The cell line CL corresponding to the bit line BL in the cell array area CA may be arranged in the cell array area CA, and the cell line capping layer CLC may be arranged on the cell line CL. In this specification, the cell line CL and the cell line capping layer CLC will be collectively referred to as a "cell line structure CS". In an embodiment of the present disclosure, the cell line structure CS may be located on the substrate 10 and may intersect the isolation layer 14A and the active area AC. The cell line structure CS may also intersect the cell gate structure GS and, for example, may extend in the second direction (y-axis direction).
[0038] The unit conductor CL may be multi-layered. Figure 2 As shown, the cell conductive line CL may include, for example, a lower conductive layer 41A, an intermediate conductive layer 42A, and an upper conductive layer 43A that are sequentially stacked.
[0039] Each of the three conductive layers 41A, 42A, and 43A may include, for example, at least one of a doped semiconductor material, a conductive silicide compound, a conductive metal nitride, a metal, or a metal alloy. For example, the lower conductive layer 41A may include a doped semiconductor material (e.g., doped polysilicon, etc.), the middle conductive layer 42A may include at least one of a conductive silicide compound or a conductive metal nitride, and the upper conductive layer 43A may include at least one of a metal or a metal alloy.
[0040] The direct contact DC may electrically connect the cell wire CL and the substrate 10. The direct contact DC may be disposed at a point where the cell wire CL intersects a center point on the long island-shaped active region 12A. The direct contact DC may be formed on a bit line connection region of the active region 12A.
[0041] refer to Figure 2 , the direct contact portion DC may include a lower layer 36 and an upper layer 37. The lower layer 36 may be located in the direct contact hole DCH exposing the active region 12A of the substrate 10 and may contact the active region 12A through the bottom surface of the direct contact hole DCH, and the upper layer 37 may contact the lower surface of the cell conductive line CL.
[0042] The upper layer 37 may include a metal element, such as W, Rh, Cu, Co, Mo, or TiN. The lower layer 36 may be a silicide or a metal silicide (i.e., a combination of the metal element of the upper layer 37 and single crystal or polycrystalline silicon), and the contact resistance between the upper layer 37 and the active region 12A may be reduced. When the direct contact portion DC includes the upper layer 37 formed of a metal and the lower layer 36 formed of a silicide instead of polycrystalline silicon, the necking and cutting defects caused by the narrow area may be reduced, the contact resistance may be reduced, and the occurrence of voids in the polycrystalline silicon may be reduced in subsequent processes.
[0043] The cell line capping layer CLC may include, for example, at least one of silicon nitride, silicon oxynitride, silicon carbonitride, or silicon carbon nitride oxide. Figure 2 As shown, the cell line capping layer CLC may have a three-layer structure. For example, the cell line capping layer CLC may include a cell line capping layer 44A, a cell line insulating layer 45A, and a mask layer 47A. The cell line capping layer 44A, the cell line insulating layer 45A, and the mask layer 47A may include, for example, at least one of silicon nitride, silicon oxynitride, silicon carbonitride, or silicon carbon nitride oxide.
[0044] For example, Figures 2 to 5 As shown, the cell line capping layer CLC may be a three-layer structure. In another example, the cell line capping layer CLC may have a single-layer, two-layer, or four-layer or more-layer structure. The mask layer 47A and the cell line insulating layer 45A of the cell line capping layer CLC may increase the height of the cell line structure CS to support the landing pad LP while separating the landing pad LP and the cell conductive line CL from each other.
[0045] The cell insulating films 31, 32 and 33 may be formed on the substrate 10 and the isolation layer 14A. Specifically, the cell insulating films 31, 32 and 33 may be disposed on a region of the substrate 10 on which the direct contact portion DC and the buried contact portion BC do not exist (e.g., disposed in a region that does not vertically overlap with the direct contact portion DC and the buried contact portion BC). The cell insulating films 31, 32 and 33 may be located between the substrate 10 and the cell conductor CL and between the isolation layer 14A and the cell conductor CL in the third direction (z-axis direction) (e.g., located in a region that vertically overlaps with a portion of the cell region separation layer 14C and the isolation layer 14A). The cell insulating films 31, 32 and 33 may be a single film or a plurality of films including a first insulating film 31, a second insulating film 32 and a third insulating film 33.
[0046] For example, the first insulating film 31 may include a silicon oxide film, the second insulating film 32 may include a metal oxide film, and the third insulating film 33 may include a silicon nitride film. For example, the first insulating film 31 and the third insulating film 33 including silicon oxide films and silicon nitride films may have a two-layer structure.
[0047] The cell line spacer 50 may be disposed on the sidewalls of the cell line structure CS and the direct contact portion DC. The cell line spacer 50 may extend to the upper surface of the first insulating film 31 outside the direct contact hole DCH while filling the direct contact hole DCH around the direct contact portion DC. The cell line spacer 50 according to an embodiment of the present disclosure may include two or more types of spacers. The spacer may include, for example, at least one of silicon oxide, silicon nitride, silicon oxynitride (SiON), silicon oxycarbonitride (SiOCN), air, or a combination thereof. Reference Figure 2 , the cell line spacer 50 may include first to fourth spacers 51 , 52 , 53 , and 54 .
[0048] like Figure 2 As shown, the first spacer 51 may cover both sidewalls of the cell line structure CS, directly contact a portion of the inner wall of the hole DCH not covered with the cell line structure CS (eg, Fig.10The first spacer 51 may be provided with a first spacer 52 and a second spacer 53. The second spacer 52 may be provided with a first spacer 51 and a second spacer 53. The second spacer 52 may be provided with a first spacer 51 and a second spacer 53. The second spacer 52 may be provided with a first spacer 51 and a second spacer 53. The second spacer 52 may be provided with a first spacer 51 and a second spacer 53. The second spacer 52 and the fourth spacer 54 may be provided with a first spacer 51 and a second spacer 53. The second spacer 52 and the fourth spacer 54 may be provided with a first spacer 51 and a second spacer 53. The second spacer 52 and the fourth spacer 54 may be provided with a first spacer 51 and a second spacer 53. The second spacer 52 and the fourth spacer 54 may be provided with a first spacer 51 and a second spacer 53. The third spacer 53 may be provided with a first spacer 51 and a second spacer 53. The third spacer 53 may be provided with a first spacer 51 and a second spacer 53.
[0049] refer to Figure 3 , the partition wall 48A may be disposed on the substrate 10 and the isolation layer 14A. In an embodiment of the present disclosure, the partition wall 48A may overlap with the cell gate structure GS formed on the substrate 10 and the isolation layer 14A. The partition wall 48A may be located between the cell line structures CS extending in the second direction (y-axis direction). The partition wall 48A may include, for example, at least one of silicon oxide, silicon nitride, silicon oxynitride, or a combination thereof.
[0050] At least a portion of the buried contact BC may be buried in the substrate 10. That is, a lower surface of the buried contact BC may be lower than an upper surface of the substrate 10. Figure 2 As shown, the upper surface of the buried contact BC may be higher than the upper surface of the substrate 10 .
[0051] The buried contact BC may be located between adjacent cell conductors CL in the first direction (x-axis direction). The buried contact BC may be located between adjacent partition walls 48A in the second direction (y-axis direction). The buried contact BC may overlap the substrate 10 and the isolation layer 14A between adjacent cell conductors CL. The buried contact BC may be connected to the storage element connection region of the active region 12A.
[0052] The buried contact BC may include, for example, at least one of a doped semiconductor material, a conductive silicide, a conductive metal nitride, or a metal. The buried contact BC may include a doped semiconductor material, for example, doped polysilicon. The buried contact BC may include, for example, polysilicon doped with phosphorus, arsenic, boron, or a combination thereof.
[0053] The cell spacer 58 may cover the outer side of the cell line spacer 50 on both sidewalls of the cell line structure CS and the sidewall of the partition wall 48A contacting the landing pad LP. Figure 2In some embodiments, when the buried contact hole is formed to accommodate the buried contact BC, the upper portion of the cell line spacer 50 may be removed, resulting in a reduced height thereof, and thus the cell spacer 58 may cover the upper portion of the cell line spacer 50 .
[0054] A plurality of landing pads LP may be formed on the buried contacts BC corresponding thereto. Each of the landing pads LP may be electrically connected to one of the buried contacts BC and connected to the storage element connection region of the active region 12A. The landing pad LP may overlap a portion of the upper surface of the cell line structure CS.
[0055] refer to Figure 2 Each of the landing pads LP may include a conductive barrier layer 64A and a conductive layer 66A. The conductive barrier layer 64A may be, for example, a stacked structure of Ti, TiN, or Ti / TiN. The conductive layer 66A may include, for example, at least one of a doped semiconductor material, a conductive silicide, a conductive metal nitride, a conductive metal carbide, a metal, or a metal alloy.
[0056] The pad separation insulating layer 70 may be disposed between a plurality of landing pads LP isolated from each other, and may contact portions of the cell line structure CS and the cell line spacer 50. Upper surfaces of the landing pads LP may or may not be covered with the pad separation insulating layer 70. For example, the upper surfaces of the landing pads LP may be at the same height as the pad separation insulating layer 70 relative to the upper surface of the substrate 10.
[0057] The pad separation insulating layer 70 may include an insulating material and electrically disconnect the plurality of landing pads LP from each other. For example, the pad separation insulating layer 70 may include at least one of silicon oxide, silicon nitride, silicon oxynitride, silicon carbon oxynitride, or silicon carbon nitride.
[0058] refer to Figure 2 , the core gate structure CGS may be disposed in the core region CORE on the substrate 10. The core gate structure CGS may be located on the active region 12B defined by the isolation layer 14B.
[0059] The core gate structure CGS may include a core gate dielectric layer 35B, a core gate electrode CGE, and a core gate cap 44B sequentially stacked on the substrate 10. The core gate structure CGS may further include a core gate spacer 56 on sidewalls of the core gate electrode CGE and the core gate cap 44B.
[0060] The core gate electrode CGE may be a single layer, or may include a plurality of layers. Figure 2 , Figure 4 and Figure 5An example is shown in which the core gate electrode CGE includes a lower conductive layer 41B, an intermediate conductive layer 42B, and an upper conductive layer 43B sequentially stacked on the core gate dielectric layer 35B. For example, two core gate structures CGS may be disposed between adjacent isolation layers 14B.
[0061] The insulating liner 45B may be disposed on the substrate 10. The insulating liner 45B may be formed according to the curvature of the core gate structure CGS. The insulating liner 45B may be disposed on the core gate cap 44B and the cell region separation layer 14C. The core gate spacer 56 may be disposed to cover the side surfaces of the first and second insulating films 31 and 32, the core gate dielectric layer 35B, the three conductive layers 41B, 42B and 43B, and the core gate cap 44B.
[0062] The insulating liner 45B may be disposed on the core gate spacer 56. The insulating liner 45B may include, for example, at least one of silicon nitride, silicon oxynitride, silicon carbonitride, or silicon carbon oxynitride.
[0063] The buried insulating layer 46 may be formed between the plurality of core gate structures CGS. According to some embodiments, when the insulating liner 45B is formed, the buried insulating layer 46 may be disposed on the insulating liner 45B. The buried insulating layer 46 may also be formed on the cell region separation layer 14C.
[0064] The buried insulating layer 46 may include an insulating material having excellent gap filling characteristics. The buried insulating layer 46 may be made of, for example, a borophosphosilicate glass (BPSG) film, a high density plasma (HDP) oxide film, an O 3 -TEOS film, undoped silicate glass (USG) or Ton-Sulphur-Silazane (TOSZ) material. In an embodiment of the present disclosure, the buried insulating layer 46 may include silicon oxide formed of a TOSZ material.
[0065] For example, the upper surface of buried insulating layer 46 may be flush with the insulating liner 45B extending along the upper surface of core gate structure CGS. According to some embodiments, when insulating liner 45B is not provided, the upper surface of buried insulating layer 46 may be flush with the upper surface of core gate structure CGS.
[0066] The mask layer 47B may be disposed on the core gate structure CGS and the buried insulating layer 46. In some embodiments, when the insulating liner 45B is disposed, the mask layer 47B may cover the insulating liner 45B extending along the upper surface of the core gate structure CGS and the buried insulating layer 46. For example, relative to the upper surface of the substrate 10, the height of the upper surface of the mask layer 47B may be the same as the height of the upper surface of the cell line capping layer CLC.
[0067] In embodiments, mask layer 47B may include a material different from that of buried insulating layer 46. For example, when buried insulating layer 46 includes silicon oxide, mask layer 47B may include at least one of silicon nitride, silicon oxynitride, silicon carbonitride, and silicon carbon oxynitride.
[0068] The contact plug CP may be disposed at both sides of the core gate structure CGS. The contact plug CP may extend to the active region 12B in the substrate 10 while passing through the mask layer 47B and the buried insulating layer 46. The interconnection line may be disposed on the mask layer 47B. The contact plug CP and the interconnection line may be separated from each other by an interconnection separation groove. In an embodiment of the present disclosure, the contact plug CP may be formed simultaneously with the landing pad LP and may therefore include the same material as that of the landing pad LP.
[0069] For example, the contact plug CP may include a conductive barrier layer 64B and a conductive layer 66B. The conductive barrier layer 64B may be formed simultaneously with the conductive barrier layer 64A of the landing pad LP and thus may include the same material as that of the conductive barrier layer 64A, and the conductive layer 66B may be formed simultaneously with the conductive layer 66A of the landing pad LP and thus may include the same material as that of the conductive layer 66A.
[0070] refer to Figure 2 , the contact plug CP may be accommodated in the contact plug hole. Most of the sidewalls of the contact plug hole may be covered with the contact plug spacer 59, but the inner wall of the contact plug hole located in the substrate 10 may be covered with the metal silicide layer 62B. Therefore, the conductive barrier layer 64B of the contact plug CP may contact the metal silicide layer 62B in the substrate 10 to be electrically connected to the active region 12B in the substrate 10, and due to the contact plug spacer 59, the conductive barrier layer 64B may be insulated from the outside of the substrate 10.
[0071] The metal silicide layer 62B may be formed of a metal (eg, cobalt, titanium, or nickel) that reacts with silicon to form silicide, and the contact plug spacer 59 may include, for example, at least one of silicon nitride, silicon oxynitride, silicon carbonitride, or silicon carbon oxynitride.
[0072] For example, the contact plug spacer 59 may be applied to all the contact plugs CP of the core region CORE. In another example, the contact plug spacer 59 may be disposed only on the sidewalls of some of the contact plugs CP in the core region CORE.
[0073] The contact plug spacer 59 can increase the distance between the contact plug CP and the core gate structure CGS, and is therefore particularly useful for highly reduced semiconductor devices. In addition, a contact plug hole for forming the contact plug CP can be formed to be larger than a desired size, and its size can be controlled using the contact plug spacer 59. Therefore, the aspect ratio of the contact plug hole to be patterned can be reduced, thereby reducing the burden of the patterning process.
[0074] Next, we will refer to Figures 6 to 10 A method for manufacturing a semiconductor device according to an embodiment of the present disclosure is described in detail. Figures 6 to 10 yes Figure 2 A cross-sectional view of a semiconductor device at a stage in the manufacturing process.
[0075] Some components to be formed in the cell array region CA may be formed simultaneously with some components to be formed in the core region CORE.
[0076] refer to Figure 6 , isolation layers 14A and 14B and a cell region separation layer 14C may be formed on the substrate 10. The isolation layers 14A and 14B and the cell region separation layer 14C may be formed by a shallow trench isolation (STI) process.
[0077] A cell array region CA and a core region CORE separated from each other by a cell region separation layer 14C may be formed on a substrate 10. A plurality of active regions 12A and 12B defined by isolation layers 14A and 14B may be formed in the cell array region CA and the core region CORE.
[0078] According to some embodiments, in a configuration including a buried word line WL (see Figure 1 In the method for manufacturing a semiconductor device of the present invention, the bit line BL (see Figure 1 ) before forming a buried word line WL in the substrate 10.
[0079] According to some embodiments, a plurality of cell gate trenches T1 may be formed in the cell array region CA of the substrate 10 (see Figure 3 ) to manufacture a cell gate structure GS including a buried word line WL (see Figures 3 to 5 ). The plurality of cell gate trenches T1 may extend parallel to each other in the first direction (x-axis direction), and each of the cell gate trenches T1 may have a line shape crossing the plurality of active regions 12A. The cell gate insulating layer 22 (see Figures 3 to 5 ), the cell gate electrode 24 (see Figures 3 to 5 ) and cell gate cap 26 (see Figures 3 to 5) may be sequentially formed in the cell gate trench T1. The cell gate electrode 24 may correspond to the word line WL as described above. In some embodiments, a cell gate capping conductive layer may be additionally formed between the cell gate electrode 24 and the cell gate capping 26. The upper surface of the cell gate capping 26 may be located at approximately the same height as the upper surface of the substrate 10.
[0080] In an embodiment of the present disclosure, after forming the unit gate structure GS, impurity ions may be implanted into two regions outside the unit gate structure GS to form source / drain regions having a certain depth from the upper surface of the active region 12A. According to another embodiment of the present disclosure, an impurity ion implantation process may be performed before forming the unit gate structure GS to form the source / drain regions.
[0081] Next, the first insulating film 31, the second insulating film 32, and the third insulating film 33 may be sequentially formed in the cell array region CA and the core region CORE of the substrate 10, and then the second insulating film 32 and the third insulating film 33 may be removed from the core region CORE to expose the active region 12B of the substrate 10. Thereafter, the gate dielectric film 35 may be formed on the core region CORE of the substrate 10 while the cell array region CA is covered with a mask layer. Figure 6 The side walls of the first to third insulating films 31, 32, and 33 are shown to be in contact with the side walls of the gate dielectric film 35 at the midpoint on the cell region separation layer 14C, but the first to third insulating films 31, 32, and 33 and the gate dielectric film 35 may be formed so as not to overlap or contact each other on the cell region separation layer 14C. The first insulating film 31 may be an oxide film, the second insulating film 32 may be a metal oxide film, and the third insulating film 33 may be a nitride film.
[0082] The gate dielectric film 35 may include at least one selected from a silicon oxide film, a silicon nitride film, a silicon oxynitride film, an oxide / nitride / oxide (ONO) film, or a high-k dielectric film having a dielectric constant higher than that of the silicon oxide film. For example, the gate dielectric film 35 may have a dielectric constant of about 10 to 25. In an embodiment of the present disclosure, the gate dielectric film 35 may include at least one of hafnium oxide (HfO), hafnium silicate (HfSiO), hafnium oxynitride (HfON), hafnium silicon oxynitride (HfSiON), lanthanum oxide (LaO), lanthanum aluminum oxide (LaAlO), zirconium oxide (ZrO), zirconium silicate (ZrSiO), zirconium oxynitride (ZrON), zirconium silicon oxynitride (ZrSiON), tantalum oxide (TaO), titanium oxide (TiO), barium strontium titanium oxide (BaSrTiO), barium titanium oxide (BaTiO), strontium titanium oxide (SrTiO), yttrium oxide (YO), aluminum oxide (AlO), and lead scandium tantalum oxide (PbScTaO). For example, the gate dielectric film 35 may include HfO2 、Al 2 O 3 、HfAlO 3 、 2 O 3 、TiO 2 At least one of .
[0083] Afterwards, the first to third insulating films 31, 32, and 33 and the substrate 10 in the cell array region CA may be etched to form a pre-direct contact hole PDCH. A bottom surface of the pre-direct contact hole PDCH includes (eg, exposes) a portion of the active region 12A.
[0084] Afterwards, refer to Figure 7 , the charging spacer 34 may be formed on the sidewall of the pre-direct contact hole PDCH. According to an embodiment of the present disclosure, the charging spacer 34 may include three charging insulating films 34A, 34B, and 34C, the middle charging insulating film 34B may include silicon oxide, and the other two charging insulating films 34A and 34C may include silicon nitride. The charging spacer 34 may protect the sidewall of the pre-direct contact hole PDCH, especially the sidewall of the substrate 10, in subsequent processes.
[0085] During the formation of the charging spacer 34 , a portion of the active region 12A exposed at the bottom of the pre-direct contact hole PDCH may be recessed (eg, recessed) to a certain extent.
[0086] refer to Figure 8 , a portion of the active region 12A exposed through the pre-direct contact hole PDCH may be grown, or polysilicon having a high impurity concentration may be stacked and etched to form a lower layer 36 of the direct contact part DC.
[0087] Next, refer to Fig. 9 , a metal or the like may be stacked and etched to form an upper layer 37 of the direct contact portion DC. In this case, by appropriately performing heat treatment or the like, the metal element of the upper layer 37 is allowed to penetrate the single crystal silicon or polycrystalline silicon of the lower layer 36, and at least a portion of the lower layer 36 is converted into silicide. When the direct contact portion DC includes an upper layer 37 formed of a metal and a lower layer 36 formed of a silicide instead of polycrystalline silicon, it is possible to reduce necking and cutting defects due to narrow areas, reduce contact resistance, and reduce the occurrence of voids in polycrystalline silicon in subsequent processes.
[0088] Afterwards, refer to Fig.10 , a lower conductive layer, an intermediate conductive layer, an upper conductive layer and a capping layer may be sequentially stacked on the third insulating film 33 and the gate dielectric film 35. The three conductive layers may include metal, etc. The capping layer may include, for example, at least one of silicon nitride, silicon oxynitride, silicon carbonitride or silicon carbon nitride oxide.
[0089] The gate dielectric film 35, the lower conductive layer, the middle conductive layer, the upper conductive layer and the capping layer in the core region CORE can be patterned while the cell array region CA is covered with a mask layer. Therefore, a core gate electrode CGE stacked with a lower conductive layer 41B, an middle conductive layer 42B and an upper conductive layer 43B is formed on the core gate dielectric layer 35B. The core gate cap 44B can be disposed on the core gate electrode CGE. The core gate spacer 56 can be formed on both sidewalls of the stacked structure of the core gate dielectric layer 35B, the core gate electrode CGE and the core gate cap 44B.
[0090] The core gate spacer 56 may include, for example, oxide, nitride, or a combination thereof. The core gate spacer 56 may be formed on the first insulating film 31 and the second insulating film 32 on the cell region separation layer 14C, the etched sidewalls of the three conductive layers and the capping layer, and the two sidewalls of the stacked structure of the core gate dielectric layer 35B, the core gate electrode CGE, and the core gate cap 44B on the core region CORE.
[0091] Thereafter, an insulating layer may be formed on the entire surface of the core region CORE and the cell array region CA. The insulating layer may include, for example, at least one of silicon nitride, silicon oxynitride, silicon carbonitride, or silicon carbon nitride oxide.
[0092] The space between the upper surface of the insulating layer and the core gate structure CGS may be filled with a buried insulating layer 46. The buried insulating layer 46 may be formed of an insulating material having an excellent gap-filling property.
[0093] The buried insulating layer 46 may be made of, for example, a borophosphosilicate glass (BPSG) film, a high density plasma (HDP) oxide film, an O 3 -TEOS film, undoped silicate glass (USG) or Tosinane silazane (TOSZ) material. In addition, the buried insulating layer 46 can be formed by at least one of the thin film formation techniques for providing excellent step coverage. For example, the buried insulating layer 46 can be formed by performing a deposition method (e.g., chemical vapor deposition (CVD), CVD below atmospheric pressure (SACVD), low pressure CVD (LPCVD), plasma enhanced CVD (PECVD) or physical vapor deposition (PVD)).
[0094] In an embodiment, the buried insulating layer 46 may be formed using Toshin silazane (TOSZ). The TOSZ film may be a polysilazane film. The TOSZ film may be formed by a spin coating method, and the TOSZ film may be formed by supplying O after performing spin coating. 2 and H 2 O, and an annealing process is performed to remove ammonia and hydrogen from the TOSZ film. Therefore, the TOSZ film may be a silicon oxide film.
[0095] Thereafter, the upper surface of the buried insulating layer 46 may be planarized through a planarization process. Thus, the upper surface of the buried insulating layer 46 may be flush with the upper surface of the insulating layer.
[0096] Next, an insulating layer is formed on the insulating layer and the buried insulating layer 46, and the insulating layer is patterned by a photolithography process to form a mask layer 47B and an insulating liner 45B on the core region CORE, and a plurality of mask layers 47A and a plurality of cell line insulating layers 45A are formed in the cell array region CA. According to an embodiment of the present disclosure, the mask layer may not be etched in the core region CORE, but may be retained.
[0097] In embodiments, mask layers 47A and 47B may include a material different from that of buried insulating layer 46. For example, when buried insulating layer 46 includes silicon oxide, mask layers 47A and 47B may include at least one of silicon nitride, silicon oxynitride, silicon carbonitride, or silicon carbon oxynitride.
[0098] Thereafter, the capping layer 44, the three conductive layers 41, 42 and 43, the upper layer 37 and the lower layer 36 of the direct contact part DC, the charging spacer 34, and the second insulating film 32 and the third insulating film 33 can be etched using the mask layers 47A and 47B, the cell line insulating layer 45A and the insulating liner 45B located below the capping layer 44, the three conductive layers 41, 42 and 43, the upper layer 37 and the lower layer 36 of the direct contact part DC, the charging spacer 34, and the second insulating film 32 and the third insulating film 33 as etching masks to form a cell line structure CS, a direct contact part DC and a direct contact hole DCH in the cell array area CA.
[0099] According to an embodiment of the present disclosure, by using a Cl-based 2 / N 2 O 2 The plasma dry etching is used to increase the etching selectivity of the upper layer 37 formed of metal and the lower layer 36 formed of silicide of the direct contact portion DC relative to the silicon active region 12A. For example, the type of etching gas to be used may vary depending on the depth of etching. Cl may be used in the initial etching stage. 2 / N 2 Gas, Cl can be used in the intermediate etching stage 2 / N 2 +2O 2 gas, and Cl can be used in the final etching stage 2 / N 2 +SO 2 gas.
[0100] Although the third insulating film 33 may be partially removed during etching of the upper layer 37 and the lower layer 36 of the direct contact portion DC, the second insulating film 32 formed of a metal oxide having a high etching selectivity relative to metal is not removed, and thus the film below the second insulating film 32 is not removed.
[0101] The cell line structure CS may include a cell wire CL and a cell line capping layer CLC located on the cell wire CL, the cell wire CL may include a lower conductive layer 41A, an intermediate conductive layer 42A and an upper conductive layer 43A, and the cell line capping layer CLC may include a cell line cap 44A, a cell line insulating layer 45A and a mask layer 47A.
[0102] The cell conductor CL may be connected to the active region 12A of the substrate 10 through the direct contact DC. When the cell conductor CL includes three conductive layers 41A, 42A, and 43A, the lower conductive layer 41A may extend to the inside of the direct contact hole DCH to contact the upper layer 37 of the direct contact DC.
[0103] Since the width of the direct contact portion DC is smaller than the diameter of the direct contact hole DCH, the direct contact hole DCH may have an empty space not filled with the direct contact portion DC, that is, a gap G. Since the cell conductor CL extends longer in the y-axis direction, the direct contact portion DC may not be completely surrounded by one gap G, but a pair of separated gaps G may exist outside the two side walls of the direct contact portion DC (that is, at the opposite sides relative to the direct contact portion DC). That is, there may be one direct contact portion DC and a pair of gaps G located in the direct contact hole DCH, and the pair of gaps G may be separated from each other by the direct contact portion DC.
[0104] refer to Figure 2 , structures such as first to fourth spacers 51 , 52 , 53 , and 54 , landing pads LP, and pad separation insulating layer 70 may be formed, thereby completing the manufacture of the semiconductor device according to an embodiment of the present disclosure.
[0105] By way of summary and review, embodiments relate to semiconductor devices with reduced defects and improved performance. That is, according to embodiments, defects in semiconductor devices can be reduced by forming a direct contact portion to include an upper layer formed of metal and a lower layer formed of silicide rather than polysilicon, thereby reducing necking and cutting defects due to narrow areas, reducing contact resistance, and reducing voids occurring in polysilicon.
[0106] Example embodiments have been disclosed herein, and although specific terms are employed, they are used and should be interpreted only in a general descriptive sense and not for purposes of limitation. In some cases, as will be appreciated by those of ordinary skill in the art submitting this application, features, characteristics, and / or elements described in conjunction with a particular embodiment may be used alone or in combination with features, characteristics, and / or elements described in other embodiments, unless expressly stated otherwise. Therefore, it will be understood by those skilled in the art that various changes in form and detail may be made without departing from the spirit and scope of the invention as set forth in the appended claims.
Claims
1. A semiconductor memory device, include: A substrate including a cell array region and a core region located near the cell array region, wherein the cell array region includes a direct contact hole exposing an active region; a buried contact connected to a storage element in the cell array region; a direct contact portion, in the cell array region, the direct contact portion comprising an upper layer and a lower layer, the upper layer comprising a metal, and the lower layer directly contacts the active region in the direct contact hole and comprises a silicide of the metal; a bit line in contact with an upper layer of the direct contact portion; as well as A word line crosses the bit line.
2. The semiconductor memory device according to claim 1, in, The upper layer includes at least one of W, Rh, Cu, Co, Mo and TiN.
3. The semiconductor memory device according to claim 2, in, The upper layer includes TiN. 4 . The semiconductor memory device according to claim 1 , further comprising a cell insulating film on the substrate, the cell insulating film not overlapping the buried contact portion and the direct contact portion.
5. The semiconductor memory device according to claim 4, in, The unit insulating film has a three-layer structure.
6. The semiconductor memory device according to claim 5, in: The unit insulating film includes a first insulating film, a second insulating film, and a third insulating film stacked in sequence, the first insulating film includes a semiconductor oxide film, The second insulating film includes a metal oxide film, and The third insulating film includes a semiconductor nitride film.
7. A method for manufacturing a semiconductor memory device, the method include: stacking a cell insulating film on a cell array region of a substrate; forming a direct contact hole by etching the cell insulating film so that the direct contact hole exposes an active region of the substrate; forming a lower layer in the direct contact hole so that the lower layer includes a semiconductor in contact with the active area through the direct contact hole; forming an upper layer on the lower layer, the upper layer comprising a metal; converting at least a portion of the underlying layer into a silicide of the metal; forming a bit line on the upper layer; as well as A direct contact is formed by etching the upper layer and the lower layer using the bit line as a mask.
8. The manufacturing method according to claim 7, in, The upper layer and the lower layer are etched by a dry etching method.
9. The manufacturing method according to claim 8, in, Based on Cl 2 / N 2 O 2 The upper layer and the lower layer are etched by plasma.
10. The manufacturing method according to claim 9, in, Etching the upper layer and the lower layer includes changing an etching gas according to an etching depth.
11. The manufacturing method according to claim 10, in, Etching the upper layer and the lower layer comprises: using Cl 2 / N 2 Gas, Cl is used in the intermediate etching stage 2 / N 2 +2O 2 gases, and Cl in the final etching stage 2 / N 2 +SO 2 gas.
12. The manufacturing method according to claim 7, in, The upper layer is formed of at least one of W, Rh, Cu, Co, Mo, and TiN.
13. The manufacturing method according to claim 12, in, The upper layer is formed of TiN.
14. The manufacturing method according to claim 7, in, The cell insulating film is formed to have a three-layer structure.
15. The manufacturing method according to claim 14, in: The unit insulating film is formed to include a first insulating film, a second insulating film, and a third insulating film stacked in sequence, The first insulating film is formed of a semiconductor oxide film, The second insulating film is formed of a metal oxide film, and The third insulating film is formed of a semiconductor nitride film.
16. The manufacturing method according to claim 15, further comprising: include: After forming the bit line, the second insulating film and the third insulating film are etched.
17. The manufacturing method according to claim 7, in, Forming the lower layer includes growing the active region.
18. The manufacturing method according to claim 7, in, Forming the lower layer includes stacking a semiconductor on the active region and etching the semiconductor.
19. The manufacturing method according to claim 18, in, Forming the lower layer includes stacking polysilicon on the active region and etching the polysilicon.
20. The manufacturing method according to claim 19, in, Forming the lower layer includes stacking high impurity concentration polysilicon on the active region, and etching the high impurity concentration polysilicon.
Citation Information
Patent Citations
Magnetic carbon nanoparticles in which activated carbon and iron oxide nanoparticles are covalently linked, and method for preparing the same
KR1020230067545A