Flat bending die for copper flat wire
By designing the copper flat curved mold, the rotation of the mold and the adjustment of the positioning plate, the shape consistency and production efficiency problems in the flat curved forming of the copper flat curved element are solved, and high-quality mass production and multi-variety adaptation are achieved. sex.
Patent Information
- Application Number
- CN202411460220.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-18
- Publication Date
- 2024-11-29
AI Technical Summary
The existing flat bending forming technology of copper flat wire winding components has poor shape consistency, low production efficiency, poor product quality, and cannot achieve mass production, and workers have a high labor intensity.
A copper flat line flat curve including mold seat, positioning plate, positioning bar, lower mold, upper mold, die core, body, press rod, thread sleeve, press plate, stud, handle, cylindrical pin, rod handle is designed The mold is to adjust the positioning plate and rotate the upper and lower molds to achieve flat bending forming of the winding elements.
It achieves high product consistency, high production efficiency and high operating safety. It is suitable for rapid mass production of multiple varieties, extends the service life of the mold, and improves the accuracy and durability of the mold through turning, milling, clamping processing and other methods.
Smart Images

Figure CN119035402A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of flat bending forming, in particular to a copper flat wire flat bending die. Background Art
[0002] There is no special mold for the flat bending of copper flat wire winding components. It relies on simple tooling to manually bend and form, which leads to poor shape consistency of winding components, low production efficiency, poor product quality, and inability to achieve mass production. In order to meet the needs of mass production, ensure product shape consistency, and improve product quality, a flat bending mold must be designed for production.
[0003] Disadvantages of existing flat bending technology for copper flat wire winding components:
[0004] 1. The shape consistency of winding components is poor, resulting in low production efficiency and poor product quality;
[0005] 2. The product qualification rate is low, mass production cannot be achieved, the manufacturing cycle is long, and the manufacturing cost is high;
[0006] 3. The labor intensity of workers during manufacturing is high. Summary of the invention
[0007] The purpose of the present invention is to provide a copper flat wire flat bending die, which includes a die base, a positioning plate, a positioning bar, a lower die, an upper die, a die core, a body, a pressure rod, a threaded sleeve, a pressure plate, a stud, a handle, a cylindrical pin, and a rod-shaped handle.
[0008] The mold base is provided with a plurality of through holes I for fixing the mold base.
[0009] The mold base is provided with a plurality of first screw holes for fixing the body.
[0010] The mold base is provided with a plurality of second screw holes for installing the positioning strips.
[0011] The second screw holes are distributed in parallel on one side of the mold base, and the first screw holes are evenly surrounded at the center of the mold base.
[0012] The positioning plate is an L-shaped plate structure, and a third screw hole with an axis parallel to the vertical plate is provided on the horizontal plate.
[0013] The bottom of the transverse plate of the positioning plate is provided with extension blocks on both sides of the third screw hole.
[0014] A fourth screw hole corresponding to the second screw hole of the mold base is provided on one side of the positioning strip.
[0015] A through slot for placing an extension block of the positioning plate is provided at the center of the positioning strip.
[0016] The lower die and the upper die are both stepped rotating body structures, and the diameter of the side where the two are connected is larger than the diameter of the side away from each other.
[0017] A triangular protrusion is provided at the center of the end surface of one side of the lower mold close to the upper mold, and a fan-shaped protrusion I is provided on one side of the triangular protrusion, and the triangular protrusion and the fan-shaped protrusion I are spaced a certain distance apart.
[0018] A fan-shaped protrusion II is provided on one end surface of the upper die close to the lower die.
[0019] When the lower die and the upper die are connected, the fan-shaped protrusion I and the fan-shaped protrusion II form a semicircular protrusion.
[0020] The mold core is a cylindrical structure, and an extension block is provided on one side of the top.
[0021] The top surface of the mold core is provided with a groove I, and one side of the groove I is provided with a connecting hole adapted to the rod-shaped handle.
[0022] The connecting hole is located in the extension block of the mold core.
[0023] The bottom surface of the mold core is provided with a groove II, and one side of the groove II is provided with a fifth screw hole.
[0024] The groove II is used to place the stepped end of the upper die away from the lower die.
[0025] The main body is a cylindrical structure, and a fan-shaped groove is provided on one side of the top.
[0026] A through hole II is provided at the bottom of the fan-shaped slot along the axis, and a sixth screw hole is provided on one side of the through hole II.
[0027] The through hole II is used to place the stepped end of the lower die away from the upper die.
[0028] An arched extension block is arranged in the middle of the fan-shaped slot, and a through hole III is arranged on the arched extension block along the axis.
[0029] The top surface of the body is provided with a groove III, and the bottom of the groove III is provided with a seventh screw hole.
[0030] The bottom surface of the body is provided with an eighth screw hole matched with the first screw hole of the mold base.
[0031] The pressure rod is a stepped rotating body structure as a whole, and a ninth screw hole is arranged on the top surface.
[0032] A conical groove is arranged at the center of the bottom surface of the pressure rod.
[0033] The threaded sleeve is an annular sleeve.
[0034] The pressing plate is a cylindrical structure, and an arched extension block is provided on one side of the top.
[0035] A through hole IV is provided along the axis of the arched extension block of the pressure plate.
[0036] A stepped through hole is provided at the center of the bottom surface of the pressing plate.
[0037] A baffle is arranged in the middle of the stud, and a thread is arranged on the cylindrical surface at the lower end of the baffle.
[0038] The upper end of the stud is provided with a pin hole I perpendicular to the axis.
[0039] The handle is a stepped rotating body structure, and a groove IV is provided in the center of the top.
[0040] A through hole V is provided at the bottom of the groove IV, and a pin hole II is provided on one side of the through hole V.
[0041] The mold base is fixed on the horizontal workbench by bolts, and the positioning strip and the body are installed on the mold base by screws.
[0042] Insert the extension block of the positioning plate into the through slot of the positioning strip and secure it with bolts.
[0043] Place the lower die into the through hole II of the body and fix it with screws.
[0044] Insert the mold core into the through hole III of the body, insert the upper mold into the groove II of the mold core and fix them with screws.
[0045] Put the pressing rod into the groove I of the mold core, put the threaded sleeve on the pressing rod, and fix the ninth screw hole of the pressing rod and the through hole IV of the pressing plate with screws.
[0046] Insert one end of the stud with threads into the seventh screw hole of the body, and insert the other end of the stud into the stepped through hole of the pressing plate.
[0047] Insert the part of the stud protruding from the pressure plate into the through hole V of the handle and fix it with a cylindrical pin.
[0048] Install the rod handle into the connecting hole of the mold core.
[0049] When using the copper flat wire flat bending die to flat-bend the winding component, first loosen the handle, adjust the position of the positioning plate on the positioning bar, and insert the winding component into the lower die and the upper die. The winding component is located between the triangular protrusion and the fan-shaped protrusion I of the lower die, and the end is against the positioning plate. Tighten the handle, push the rod-shaped handle, and then drive the upper die to rotate, and the fan-shaped protrusion II of the upper die and the fan-shaped protrusion I of the lower die flat-bend the winding component.
[0050] Furthermore, the processing methods of the body and the handle include turning, milling and clamping.
[0051] Furthermore, the processing methods of the lower die and the upper die include turning, heat treatment, milling and clamping.
[0052] Furthermore, a tenth screw hole is provided at the bottom of the conical groove of the pressure rod.
[0053] Furthermore, the processing method of the mold core includes turning, heat treatment, milling and clamping.
[0054] Furthermore, the processing method of the pressing plate includes turning, heat treatment, milling and clamping.
[0055] Furthermore, the processing methods of the mold base, the positioning plate and the positioning strip include milling, flat grinding and clamping.
[0056] Furthermore, the processing method of the pressure rod includes heat treatment and turning.
[0057] Furthermore, the processing methods of the threaded sleeve and the stud include heat treatment, turning and clamping.
[0058] Furthermore, the processing method of the rod-shaped handle includes heat treatment, turning, milling and clamping.
[0059] The technical effect of the present invention is unquestionable. The flat bending die of the copper flat wire winding element designed by the present invention can meet the needs of rapid batch production of multiple varieties of products and ensure product quality.
[0060] The present invention has the following advantages:
[0061] 1. Ensure good product consistency, high product qualification rate and high product production efficiency;
[0062] 2. The flat bending die is simple and firm to clamp, and the operation is safe;
[0063] 3. The flat bending die should be used for a long time;
[0064] 4. A set of flat bending dies only needs minor changes to be able to flat-bend various types of copper flat wire winding components to meet the needs of different products;
[0065] 5. Novel and simple structure;
[0066] 6. Realize the flat bending of copper flat wire winding components;
[0067] 7. Adjust the length of the winding element end by adjusting the positioning plate;
[0068] 8. The handle is safe and convenient to operate, achieving safety margin. BRIEF DESCRIPTION OF THE DRAWINGS
[0069] Figure 1 This is the front view of the copper flat wire flat bending die assembly structure;
[0070] Figure 2 This is the left view of the copper flat wire flat bending die assembly structure;
[0071] Figure 3 It is a top view of the assembly structure of the copper flat wire flat bending die;
[0072] Figure 4 This is a schematic diagram of the flat bending die operation;
[0073] Figure 5 This is a schematic diagram of the mold base structure; Figure 5 (a) is a cross-sectional view of the mold base structure; Figure 5 (b) is a top view of the mold base structure;
[0074] Figure 6 is a schematic diagram of the positioning plate structure; Figure 6 (a) is a front view of the positioning plate structure; Figure 6 (b) is the left view of the positioning plate structure; Figure 6 (c) is a top view of the positioning plate structure;
[0075] Figure 7 Schematic diagram of the positioning bar structure; Figure 7 (a) is a front view of the positioning bar structure; Figure 7 (b) is a cross-sectional view of the positioning strip structure;
[0076] Figure 8 Schematic diagram of the lower die structure; Figure 8 (a) is the front view of the lower mold structure; Figure 8 (b) is a top view of the lower mold structure;
[0077] Fig. 9 Schematic diagram of the upper die structure; Fig. 9 (a) is a bottom view of the upper die structure; Fig. 9 (b) is a front view of the upper die structure;
[0078] Fig.10 Schematic diagram of the mold core structure; Fig.10 (a) is a cross-sectional view of the core structure; Fig.10 (b) is a top view of the core structure;
[0079] Fig.11 It is a schematic diagram of the main body structure; Fig.11 (a) is a cross-sectional view of the CC plane of the main structure; Fig.11 (b) is a cross-sectional view of the main structure on the BB plane; Fig.11 (c) is a top view of the main structure;
[0080] Fig.12 It is a schematic diagram of the compression rod structure;
[0081] Fig.13 It is a schematic diagram of the threaded sleeve structure; Fig.13 (a) is a cross-sectional view of the threaded sleeve structure; Fig.13 (b) is a top view of the threaded sleeve structure;
[0082] Fig.14 It is a schematic diagram of the pressure plate structure; Fig.14 (a) is a cross-sectional view of the pressure plate structure; Fig.14 (b) is a top view of the pressure plate structure;
[0083] Fig.15 is a schematic diagram of the stud structure;
[0084] Fig.16 is a schematic diagram of the handle structure; Fig.16 (a) is a top view of the handle structure; Fig.16 (b) is a cross-sectional view of the handle structure; Fig.16 (c) is a front view of the handle structure;
[0085] Fig.17 It is a schematic diagram of the rod-shaped handle structure; Fig.17 (a) is a front view of the rod-shaped handle structure; Fig.17 (b) is a left view of the rod-shaped handle structure; Fig.17 (c) is a cross-sectional view of the rod-shaped handle structure on the AA plane;
[0086] Fig.18 This is a schematic diagram of a copper flat wire winding component before flat bending;
[0087] Fig.19 This is a schematic diagram of a copper flat wire winding component after flat bending;
[0088] In the figure, mold base 101, through hole I1011, first screw hole 1012, second screw hole 1013, positioning plate 102, third screw hole 1021, positioning bar 103, fourth screw hole 1031, through groove 1032, lower mold 104, upper mold 105, mold core 106, groove I1061, connecting hole 1062, groove II1063, fifth screw hole 1064, body 107, fan-shaped slot 1071, through hole II1072, sixth screw hole 1073, through hole III1 074, groove III 1075, seventh screw hole 1076, eighth screw hole 1077, pressure rod 108, ninth screw hole 1081, conical groove 1082, tenth screw hole 1083, threaded sleeve 109, pressure plate 110, through hole IV 1101, stepped through hole 1102, stud 111, baffle 1111, pin hole I 1112, handle 112, groove IV 1121, through hole V 1122, pin hole II 1123, cylindrical pin 113, rod-shaped handle 115. DETAILED DESCRIPTION
[0089] The present invention is further described below in conjunction with the embodiments, but it should not be understood that the above subject matter of the present invention is limited to the following embodiments. Without departing from the above technical ideas of the present invention, various substitutions and changes are made according to the common technical knowledge and customary means in the art, which should all be included in the protection scope of the present invention.
[0090] Embodiment 1:
[0091] See also Figures 1 to 19 The copper flat wire flat bending die includes a die base 101, a positioning plate 102, a positioning bar 103, a lower die 104, an upper die 105, a die core 106, a body 107, a pressure rod 108, a threaded sleeve 109, a pressure plate 110, a stud 111, a handle 112, a cylindrical pin 113, and a rod-shaped handle 115.
[0092] The mold base 101 is provided with a plurality of through holes I1011 for fixing the mold base 101 .
[0093] The mold base 101 is provided with a plurality of first screw holes 1012 for fixing the body 107 .
[0094] The mold base 101 is provided with a plurality of second screw holes 1013 for installing the positioning strips 103 .
[0095] The second screw holes 1013 are arranged in parallel on one side of the mold base 101 , and the first screw holes 1012 are evenly arranged around the center of the mold base 101 .
[0096] The positioning plate 102 is an L-shaped plate structure, and a third screw hole 1021 with an axis parallel to the vertical plate is provided on the horizontal plate.
[0097] The bottom of the horizontal plate of the positioning plate 102 is provided with extension blocks on both sides of the third screw hole 1021 .
[0098] A fourth screw hole 1031 corresponding to the second screw hole 1013 of the mold base 101 is defined on one side of the positioning bar 103 .
[0099] A through slot 1032 for accommodating the extension block of the positioning plate 102 is provided at the center of the positioning bar 103 .
[0100] The lower mold 104 and the upper mold 105 are both stepped rotating body structures, and the diameter of the side where they are connected is larger than the diameter of the side away from each other.
[0101] A triangular protrusion is provided at the center of the end surface of one side of the lower mold 104 close to the upper mold 105, and a fan-shaped protrusion I is provided on one side of the triangular protrusion, and the triangular protrusion and the fan-shaped protrusion I are spaced a certain distance apart.
[0102] A fan-shaped protrusion II is provided on one end surface of the upper mold 105 close to the lower mold 104 .
[0103] When the lower die 104 and the upper die 105 are connected, the fan-shaped protrusion I and the fan-shaped protrusion II form a semicircular protrusion.
[0104] The mold core 106 is a cylindrical structure, and an extension block is provided on one side of the top.
[0105] The top surface of the mold core 106 is provided with a groove I1061 , and one side of the groove I1061 is provided with a connecting hole 1062 adapted to the rod-shaped handle 115 .
[0106] The connection hole 1062 is located in the extension block of the mold core 106 .
[0107] A groove II1063 is formed on the bottom surface of the mold core 106 , and a fifth screw hole 1064 is formed on one side of the groove II1063 .
[0108] The groove II1063 is used to place the stepped end of the upper mold 105 facing away from the lower mold 104.
[0109] The main body 107 is a cylindrical structure, and a fan-shaped slot 1071 is provided on one side of the top.
[0110] A through hole II1072 is provided at the bottom of the fan-shaped slot 1071 along the axis, and a sixth screw hole 1073 is provided on one side of the through hole II1072 .
[0111] The through hole II1072 is used to place the stepped end of the lower mold 104 facing away from the upper mold 105.
[0112] An arched extension block is provided in the middle of the fan-shaped slot 1071, and a through hole III1074 is provided on the arched extension block along the axis.
[0113] A groove III1075 is defined on the top surface of the main body 107 , and a seventh screw hole 1076 is defined at the bottom of the groove III1075 .
[0114] The bottom surface of the body 107 is provided with an eighth screw hole 1077 adapted to the first screw hole 1012 of the mold base 101 .
[0115] The pressure rod 108 is a stepped rotating body structure as a whole, and a ninth screw hole 1081 is provided on the top surface.
[0116] A conical groove 1082 is provided at the center of the bottom surface of the pressing rod 108 .
[0117] The threaded sleeve 109 is an annular sleeve.
[0118] The pressing plate 110 is a cylindrical structure, and an arched extension block is provided on one side of the top.
[0119] A through hole IV1101 is provided along the axis of the arched extension block of the pressing plate 110 .
[0120] A stepped through hole 1102 is provided at the center of the bottom surface of the pressing plate 110 .
[0121] A baffle plate 1111 is disposed in the middle of the stud 111 , and a thread is disposed on the cylindrical surface at the lower end of the baffle plate.
[0122] The upper end of the stud 111 is provided with a pin hole I1112 perpendicular to the axis.
[0123] The handle 112 is a stepped rotating body structure, and a groove IV1121 is provided at the center of the top.
[0124] A through hole V1122 is provided at the bottom of the groove IV1121, and a pin hole II1123 is provided on one side of the through hole V1122.
[0125] The mold base 101 is fixed on a horizontal workbench by bolts, and the positioning strip 103 and the body 107 are installed on the mold base 101 by screws.
[0126] The extension block of the positioning plate 102 is inserted into the through slot 1032 of the positioning bar 103 and fixed by bolts.
[0127] The lower mold 104 is placed into the through hole II1072 of the main body 107 and fixed by screws.
[0128] The core mold 106 is inserted into the through hole III1074 of the body 107, and the upper mold 105 is inserted into the groove II1063 of the core mold 106 and fixed by screws.
[0129] Put the pressing rod 108 into the groove I1061 of the mold core 106, put the threaded sleeve 109 on the pressing rod 108, and fix the ninth screw hole 1081 of the pressing rod 108 and the through hole IV1101 of the pressing plate 110 by screws.
[0130] One end of the stud 111 with a thread is inserted into the seventh screw hole 1076 of the body 107 , and the other end of the stud 111 is inserted into the stepped through hole 1102 of the pressing plate 110 .
[0131] The portion of the stud 111 protruding from the pressure plate 110 is inserted into the through hole V1122 of the handle 112 and fixed by the cylindrical pin 113 .
[0132] The rod-shaped handle 115 is installed in the connecting hole 1062 of the mold core 106.
[0133] When the copper flat wire flat bending die is used to flat-bend the winding component, first loosen the handle 112, adjust the position of the positioning plate 102 on the positioning bar 103, and insert the winding component into the lower die 104 and the upper die 105. The winding component is located between the triangular protrusion and the fan-shaped protrusion I of the lower die 104, and the end is against the positioning plate 102. Tighten the handle 112, push the rod-shaped handle 115, and then drive the upper die 105 to rotate, and the fan-shaped protrusion II of the upper die 105 and the fan-shaped protrusion I of the lower die 104 flat-bend the winding component.
[0134] Embodiment 2:
[0135] Copper flat wire flat bending die, main technical contents are shown in Example 1. Furthermore, the processing methods of the main body 107 and the handle 112 include turning, milling and clamping.
[0136] Embodiment 3:
[0137] The copper flat wire flat bending die, the main technical content is shown in any one of embodiments 1 to 2. Furthermore, the processing methods of the lower die 104 and the upper die 105 include turning, heat treatment, milling, and clamping.
[0138] Embodiment 4:
[0139] Copper flat wire flat bending die, the main technical content is shown in any one of embodiments 1 to 3. Furthermore, a tenth screw hole 1083 is provided at the bottom of the conical groove 1082 of the pressure rod 108.
[0140] Embodiment 5:
[0141] The copper flat wire flat bending die, the main technical content is shown in any one of embodiments 1 to 4. Furthermore, the processing method of the mold core 106 includes turning, heat treatment, milling, and clamping.
[0142] Embodiment 6:
[0143] Copper flat wire flat bending die, main technical contents are shown in any one of embodiments 1 to 5. Furthermore, the processing method of the pressing plate 110 includes turning, heat treatment, milling and clamping.
[0144] Embodiment 7:
[0145] The copper flat wire flat bending die, the main technical content is shown in any one of embodiments 1 to 6. Furthermore, the processing methods of the die base 101, the positioning plate 102 and the positioning bar 103 include milling, flat grinding and clamping.
[0146] Embodiment 8:
[0147] Copper flat wire flat bending die, the main technical content is shown in any one of Examples 1 to 7. Furthermore, the processing method of the pressure rod 108 includes heat treatment and turning.
[0148] Embodiment 9:
[0149] Copper flat wire flat bending die, the main technical content is shown in any one of embodiments 1 to 8. Furthermore, the processing method of the threaded sleeve 109 and the stud 111 includes heat treatment, turning, and clamping.
[0150] Embodiment 10:
[0151] Copper flat wire flat bending die, the main technical content is shown in any one of Examples 1 to 9. Furthermore, the processing method of the rod-shaped handle 115 includes heat treatment, turning, milling, and clamping.
[0152] Embodiment 11:
[0153] See also Figures 1 to 19 The copper flat wire flat bending die includes a die base 101, a positioning plate 102, a positioning bar 103, a lower die 104, an upper die 105, a die core 106, a body 107, a pressure rod 108, a threaded sleeve 109, a pressure plate 110, a stud 111, a handle 112, a cylindrical pin 113, and a rod-shaped handle 115.
[0154] The mold base 101 is provided with a plurality of through holes I1011 for fixing the mold base 101 .
[0155] The mold base 101 is provided with a plurality of first screw holes 1012 for fixing the body 107 .
[0156] The mold base 101 is provided with a plurality of second screw holes 1013 for installing the positioning strips 103 .
[0157] The second screw holes 1013 are arranged in parallel on one side of the mold base 101 , and the first screw holes 1012 are evenly arranged around the center of the mold base 101 .
[0158] The positioning plate 102 is an L-shaped plate structure, and a third screw hole 1021 with an axis parallel to the vertical plate is provided on the horizontal plate.
[0159] The bottom of the horizontal plate of the positioning plate 102 is provided with extension blocks on both sides of the third screw hole 1021 .
[0160] A fourth screw hole 1031 corresponding to the second screw hole 1013 of the mold base 101 is defined on one side of the positioning bar 103 .
[0161] A through slot 1032 for accommodating the extension block of the positioning plate 102 is provided at the center of the positioning bar 103 .
[0162] The lower mold 104 and the upper mold 105 are both stepped rotating body structures, and the diameter of the side where they are connected is larger than the diameter of the side away from each other.
[0163] A triangular protrusion is provided at the center of the end surface of one side of the lower mold 104 close to the upper mold 105, and a fan-shaped protrusion I is provided on one side of the triangular protrusion, and the triangular protrusion and the fan-shaped protrusion I are spaced a certain distance apart.
[0164] A fan-shaped protrusion II is provided on one end surface of the upper mold 105 close to the lower mold 104 .
[0165] When the lower die 104 and the upper die 105 are connected, the fan-shaped protrusion I and the fan-shaped protrusion II form a semicircular protrusion.
[0166] The mold core 106 is a cylindrical structure, and an extension block is provided on one side of the top.
[0167] The top surface of the mold core 106 is provided with a groove I1061 , and one side of the groove I1061 is provided with a connecting hole 1062 adapted to the rod-shaped handle 115 .
[0168] The connection hole 1062 is located in the extension block of the mold core 106 .
[0169] A groove II1063 is formed on the bottom surface of the mold core 106 , and a fifth screw hole 1064 is formed on one side of the groove II1063 .
[0170] The groove II1063 is used to place the stepped end of the upper mold 105 facing away from the lower mold 104.
[0171] The main body 107 is a cylindrical structure, and a fan-shaped slot 1071 is provided on one side of the top.
[0172] A through hole II1072 is provided at the bottom of the fan-shaped slot 1071 along the axis, and a sixth screw hole 1073 is provided on one side of the through hole II1072 .
[0173] The through hole II1072 is used to place the stepped end of the lower mold 104 facing away from the upper mold 105.
[0174] An arched extension block is provided in the middle of the fan-shaped slot 1071, and a through hole III1074 is provided on the arched extension block along the axis.
[0175] A groove III1075 is defined on the top surface of the main body 107 , and a seventh screw hole 1076 is defined at the bottom of the groove III1075 .
[0176] The bottom surface of the body 107 is provided with an eighth screw hole 1077 adapted to the first screw hole 1012 of the mold base 101 .
[0177] The pressure rod 108 is a stepped rotating body structure as a whole, and a ninth screw hole 1081 is provided on the top surface.
[0178] A conical groove 1082 is provided at the center of the bottom surface of the pressing rod 108 .
[0179] The threaded sleeve 109 is an annular sleeve.
[0180] The pressing plate 110 is a cylindrical structure, and an arched extension block is provided on one side of the top.
[0181] A through hole IV1101 is provided along the axis of the arched extension block of the pressing plate 110 .
[0182] A stepped through hole 1102 is provided at the center of the bottom surface of the pressing plate 110 .
[0183] A baffle plate 1111 is disposed in the middle of the stud 111 , and a thread is disposed on the cylindrical surface at the lower end of the baffle plate.
[0184] The upper end of the stud 111 is provided with a pin hole I1112 perpendicular to the axis.
[0185] The handle 112 is a stepped rotating body structure, and a groove IV1121 is provided at the center of the top.
[0186] A through hole V1122 is provided at the bottom of the groove IV1121, and a pin hole II1123 is provided on one side of the through hole V1122.
[0187] The mold base 101 is fixed on a horizontal workbench by bolts, and the positioning strip 103 and the body 107 are installed on the mold base 101 by screws.
[0188] The extension block of the positioning plate 102 is inserted into the through slot 1032 of the positioning bar 103 and fixed by bolts.
[0189] The lower mold 104 is placed into the through hole II1072 of the main body 107 and fixed by screws.
[0190] The core mold 106 is inserted into the through hole III1074 of the body 107, and the upper mold 105 is inserted into the groove II1063 of the core mold 106 and fixed by screws.
[0191] Put the pressing rod 108 into the groove I1061 of the mold core 106, put the threaded sleeve 109 on the pressing rod 108, and fix the ninth screw hole 1081 of the pressing rod 108 and the through hole IV1101 of the pressing plate 110 by screws.
[0192] One end of the stud 111 with a thread is inserted into the seventh screw hole 1076 of the body 107 , and the other end of the stud 111 is inserted into the stepped through hole 1102 of the pressing plate 110 .
[0193] The portion of the stud 111 protruding from the pressure plate 110 is inserted into the through hole V1122 of the handle 112 and fixed by the cylindrical pin 113 .
[0194] The rod-shaped handle 115 is installed in the connecting hole 1062 of the mold core 106.
[0195] When the copper flat wire flat bending die is used to flat-bend the winding component, first loosen the handle 112, adjust the position of the positioning plate 102 on the positioning bar 103, and insert the winding component into the lower die 104 and the upper die 105. The winding component is located between the triangular protrusion and the fan-shaped protrusion I of the lower die 104, and the end is against the positioning plate 102. Tighten the handle 112, push the rod-shaped handle 115, and then drive the upper die 105 to rotate, and the fan-shaped protrusion II of the upper die 105 and the fan-shaped protrusion I of the lower die 104 flat-bend the winding component.
[0196] like Figures 1 to 3 As shown in the figure, after the flat bending die is assembled, the die base 101 is fixed on the horizontal workbench with two bolts and nuts. First, the handle 112 is loosened, and one end of the copper flat wire winding element is inserted into the lower die 104 and the upper die 105, with the end against the positioning plate 102, and then the handle 112 is tightened, and finally the rod-shaped handle 115 is held to move the flat bending die toward the lower die 104 and the upper die 105. Figure 4 Push in the direction shown, the copper flat wire winding element is flat-bent into place, and the copper flat wire winding element is taken out after releasing the handle 112. By adjusting the positioning plate 102, various end length requirements of the copper flat wire winding element can be met.
[0197] Embodiment 12:
[0198] Copper flat wire flat bending die, main technical contents are shown in Example 11. Furthermore, the processing methods of the main body 107 and the handle 112 include turning, milling and clamping.
[0199] Embodiment 13:
[0200] Copper flat wire flat bending die, main technical contents are shown in any one of Examples 11 to 12. Furthermore, the processing methods of the lower die 104 and the upper die 105 include turning, heat treatment, milling, and clamping.
[0201] The lower die 104 and the upper die 105 are processed by turning, heat treatment, turning, milling and clamping.
[0202] Embodiment 14:
[0203] The copper flat wire flat bending die, the main technical content is shown in any one of Examples 11 to 13. Furthermore, a tenth screw hole 1083 is provided at the bottom of the conical groove 1082 of the pressure rod 108, which is a process hole for processing.
[0204] Embodiment 15:
[0205] Copper flat wire flat bending die, main technical contents are shown in any one of embodiments 11 to 14. Furthermore, the processing method of the die core 106 includes turning, heat treatment, milling and clamping.
[0206] The mold core 106 is processed by turning, heat treatment, turning, milling and clamping.
[0207] Embodiment 16:
[0208] Copper flat wire flat bending die, main technical contents are shown in any one of embodiments 11 to 15. Furthermore, the processing method of the pressing plate 110 includes turning, heat treatment, milling and clamping.
[0209] The pressing plate 110 is processed by turning, heat treatment, turning, milling and clamping.
[0210] Embodiment 17:
[0211] The copper flat wire flat bending die, the main technical content is shown in any one of Examples 11 to 16. Furthermore, the processing methods of the die base 101, the positioning plate 102 and the positioning bar 103 include milling, flat grinding and clamping.
[0212] Embodiment 18:
[0213] Copper flat wire flat bending die, the main technical content is shown in any one of Examples 11 to 17. Furthermore, the processing method of the pressure rod 108 includes heat treatment and turning.
[0214] Embodiment 19:
[0215] Copper flat wire flat bending die, the main technical content is shown in any one of Examples 11 to 18. Furthermore, the processing method of the threaded sleeve 109 and the stud 111 includes heat treatment, turning, and clamping.
[0216] Embodiment 20:
[0217] Copper flat wire flat bending die, the main technical content is shown in any one of Examples 11 to 19. Furthermore, the processing method of the rod-shaped handle 115 includes heat treatment, turning, milling, and clamping.
[0218] Embodiment 21:
[0219] See also Figures 1 to 19 The copper flat wire flat bending die includes a die base 101, a positioning plate 102, a positioning bar 103, a lower die 104, an upper die 105, a die core 106, a body 107, a pressure rod 108, a threaded sleeve 109, a pressure plate 110, a stud 111, a handle 112, a cylindrical pin 113, a rod handle 115, a plurality of screws and a plurality of bolts.
[0220] like Figures 1 to 3 As shown in the figure, after the flat bending die is assembled, the die base 101 is fixed on the horizontal workbench with two bolts and nuts. First, the handle 112 is loosened, and one end of the copper flat wire winding element is inserted into the lower die 104 and the upper die 105, with the end against the positioning plate 102, and then the handle 112 is tightened, and finally the rod-shaped handle 115 is held to move the flat bending die toward the lower die 104 and the upper die 105. Figure 4Push in the direction shown, the copper flat wire winding element is flat-bent into place, and the copper flat wire winding element is taken out after releasing the handle 112. By adjusting the positioning plate 102, various end length requirements of the copper flat wire winding element can be met.
[0221] The copper flat wire flat bending die is assembled from twenty parts, and the material selection requires sufficient strength and rigidity. First: use lathe, milling, and clamping to process the body 107 and handle 112; lathe, heat treatment, lathe, milling, and clamping to process the lower die 104, upper die 105, die core 106, and pressure plate 110; milling, flat grinding, and clamping to process the die base 101, positioning plate 102, and positioning strip 103; heat treatment, lathe, and clamping to process the threaded sleeve 109 and stud 111; then, heat treatment, lathe, milling, and clamping to process the rod-shaped handle 115; heat treatment and lathe to process the pressure rod 108; then, select standard screws, bolts, and cylindrical pins 113; finally, press Figures 1 to 3 assembly.
Claims
1. Copper flat wire flat bending die, It is characterized in that It comprises a die base (101), a positioning plate (102), a positioning strip (103), a lower die (104), an upper die (105), a die core (106), a body (107), a pressure rod (108), a threaded sleeve (109), a pressure plate (110), a stud (111), a handle (112), a cylindrical pin (113), and a rod-shaped handle (115); The mold base (101) is provided with a plurality of through holes I (1011) for fixing the mold base (101). The mold base (101) is provided with a plurality of first screw holes (1012) for fixing the body (107); The mold base (101) is provided with a plurality of second screw holes (1013) for installing the positioning strips (103); The second screw holes (1013) are arranged in parallel on one side of the mold base (101), and the first screw holes (1012) are evenly arranged around the center of the mold base (101); The positioning plate (102) is an L-shaped plate structure, and a third screw hole (1021) with an axis parallel to the vertical plate is provided on the horizontal plate; The bottom of the horizontal plate of the positioning plate (102) is provided with extension blocks on both sides of the third screw hole (1021); A fourth screw hole (1031) corresponding to the second screw hole (1013) of the mold base (101) is provided on one side of the positioning strip (103); The center of the positioning strip (103) is provided with a through slot (1032) for accommodating an extension block of the positioning plate (102); The lower mold (104) and the upper mold (105) are both stepped rotating body structures, and the diameter of the side where the two are connected is larger than the diameter of the side away from each other; A triangular protrusion is provided at the center of the end surface of one side of the lower mold (104) close to the upper mold (105), a fan-shaped protrusion I is provided on one side of the triangular protrusion, and the triangular protrusion and the fan-shaped protrusion I are spaced a certain distance apart; A fan-shaped protrusion II is provided on one end surface of the upper mold (105) close to the lower mold (104). When the lower die (104) and the upper die (105) are connected, the fan-shaped protrusion I and the fan-shaped protrusion II form a semicircular protrusion; The mold core (106) is a cylindrical structure, and an extension block is provided on one side of the top; The top surface of the mold core (106) is provided with a groove I (1061), and one side of the groove I (1061) is provided with a connection hole (1062) adapted to the rod-shaped handle (115); The connection hole (1062) is located in the extension block of the mold core (106); The bottom surface of the mold core (106) is provided with a groove II (1063), and one side of the groove II (1063) is provided with a fifth screw hole (1064); The groove II (1063) is used to place the stepped end of the upper mold (105) facing away from the lower mold (104); The body (107) is a cylindrical structure, and a fan-shaped slot (1071) is provided on one side of the top; A through hole II (1072) is provided at the bottom of the fan-shaped slot (1071) along the axis, and a sixth screw hole (1073) is provided on one side of the through hole II (1072); The through hole II (1072) is used to place the stepped end of the lower mold (104) away from the upper mold (105); An arched extension block is provided in the middle of the fan-shaped slot (1071), and a through hole III (1074) is provided on the arched extension block along the axis; The top surface of the body (107) is provided with a groove III (1075), and the bottom of the groove III (1075) is provided with a seventh screw hole (1076); The bottom surface of the body (107) is provided with an eighth screw hole (1077) adapted to the first screw hole (1012) of the mold base (101); The pressure rod (108) is a stepped rotating body structure as a whole, and a ninth screw hole (1081) is provided on the top surface; A conical groove (1082) is provided at the center of the bottom surface of the pressure rod (108); The threaded sleeve (109) is an annular sleeve; The pressing plate (110) is a cylindrical structure, and an arched extension block is provided on one side of the top; A through hole IV (1101) is provided on the arched extension block of the pressing plate (110) along the axis; A stepped through hole (1102) is provided at the center of the bottom surface of the pressing plate (110); A baffle (1111) is provided in the middle of the stud (111), and a thread is provided on the cylindrical surface at the lower end of the baffle; The upper end of the stud (111) is provided with a pin hole I (1112) perpendicular to the axis; The handle (112) is a stepped rotating body structure, and a groove IV (1121) is provided at the center of the top; A through hole V (1122) is provided at the bottom of the groove IV (1121), and a pin hole II (1123) is provided on one side of the through hole V (1122); The mold base (101) is fixed on a horizontal workbench by bolts, and the positioning strip (103) and the body (107) are installed on the mold base (101) by screws; Insert the extension block of the positioning plate (102) into the through slot (1032) of the positioning strip (103) and fix it with bolts; Place the lower mold (104) into the through hole II (1072) of the body (107) and fix it with screws; Insert the mold core (106) into the through hole III (1074) of the body (107), insert the upper mold (105) into the groove II (1063) of the mold core (106) and fix them with screws; Place the pressure rod (108) into the groove I (1061) of the mold core (106), put the threaded sleeve (109) on the pressure rod (108), and fix the ninth screw hole (1081) of the pressure rod (108) and the through hole IV (1101) of the pressure plate (110) by screws; Insert one end of the stud (111) with a thread into the seventh screw hole (1076) of the body (107), and insert the other end of the stud (111) into the stepped through hole (1102) of the pressing plate (110); Insert the portion of the stud (111) protruding from the pressure plate (110) into the through hole V (1122) of the handle (112) and fix it with a cylindrical pin (113); Install the rod-shaped handle (115) in the connecting hole (1062) of the mold core (106); When the copper flat wire flat bending die is used to flat-bend a winding component, the handle (112) is first loosened, the position of the positioning plate (102) on the positioning bar (103) is adjusted, and the winding component is inserted into the lower die (104) and the upper die (105); the winding component is located between the triangular protrusion and the fan-shaped protrusion I of the lower die (104), and the end is against the positioning plate (102); the handle (112) is tightened, and the rod-shaped handle (115) is pushed, thereby driving the upper die (105) to rotate, and the fan-shaped protrusion II of the upper die (105) and the fan-shaped protrusion I of the lower die (104) flat-bend the winding component.
2. The copper flat wire flat bending die according to claim 1, It is characterized in that The processing methods of the body (107) and the handle (112) include turning, milling and clamping.
3. The copper flat wire flat bending die according to claim 1, It is characterized in that The processing methods of the lower die (104) and the upper die (105) include turning, heat treatment, milling and clamping.
4. The copper flat wire flat bending die according to claim 1, It is characterized in that A tenth screw hole (1083) is provided at the bottom of the conical groove (1082) of the pressure rod (108).
5. The copper flat wire flat bending die according to claim 1, It is characterized in that The processing method of the mold core (106) includes turning, heat treatment, milling and clamping.
6. The copper flat wire flat bending die according to claim 1, It is characterized in that The processing method of the pressing plate (110) includes turning, heat treatment, milling and clamping.
7. The copper flat wire flat bending die according to claim 1, It is characterized in that The processing methods of the mold base (101), the positioning plate (102) and the positioning strip (103) include milling, flat grinding and clamping.
8. The copper flat wire flat bending die according to claim 1, It is characterized in that The processing method of the pressure rod (108) includes heat treatment and turning.
9. The copper flat wire flat bending die according to claim 1, It is characterized in that The processing methods of the threaded sleeve (109) and the stud (111) include heat treatment, turning and clamping.
10. The copper flat wire flat bending die according to claim 1, It is characterized in that The processing method of the rod-shaped handle (115) includes heat treatment, turning, milling and clamping.
Citation Information
Patent Citations
Labor-saving bending device for steel bar bending
CN111203496A
Flat copper wire bender for motor
CN207823804U
Flat wire flat bend manufacturing tool
CN211539298U