Shale gas flow conductivity measuring device and method

By designing a device for shale gas flow diversion capacity measurement, using a pressure stabilization pump to simulate the pressure of the geological layer, combined with a flow meter and a pressure detector, the problem of measurement results deviation in the prior art is solved, and the different pressure conditions are achieved The precise flow diversion capacity measurement under the following is suitable for actual shale gas mining.

CN119044002APending Publication Date: 2024-11-29JIANGSU INST OF GEOLOGY & MINERAL RESOURCES DESIGN
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411396167.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-08
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The prior art cannot accurately measure the fracture flow diversion capacity of the shale layer under different geological pressure conditions, and the poor sealing properties lead to deviations in the test results, making it unable to be suitable for actual shale gas mining.

Method used

A shale gas flow-through capacity measurement device including core sealed container assembly, proppant mixing assembly and mixed liquid collection assembly was designed. The pressure of the geological layer is simulated through a pressure stabilization pump, combined with a flow meter and a pressure detector to measure different concentrations. The proppant's flow-guiding ability ensures sealing and precision.

Benefits of technology

The precise measurement of the shale layer flow diversion capacity under different pressure values ​​is achieved, which reduces the deviation of the test results, improves the practicality of the measurement and is accurate in the actual environment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119044002A_ABST
    Figure CN119044002A_ABST
Patent Text Reader

Abstract

The invention discloses a shale gas flow conductivity measuring device and method.The shale gas flow conductivity measuring device comprises a rock core sealing container assembly, a proppant mixing assembly and a mixed liquid collecting assembly, the proppant mixing assembly mixes a proppant in a pressurized mode through a booster pump, and the proppant sequentially flows through a first flow meter, a pressure detector, a switch valve, the rock core sealing container assembly and the mixed liquid collecting assembly; a pressure stabilizing pump is arranged on one side of the rock core sealing container assembly, a second flow meter is arranged between the rock core sealing container assembly and the mixed liquid collecting assembly, the rock core sealing container assembly comprises a sealing box body and a sealing cover plate, and a first sealing groove is formed in the top end face of the sealing box body so that it can be determined that under the condition of the same pressure value, the flow meter can meter the mixed liquid; the flow guide conditions of the proppants with different concentration values are adjusted according to different pressure values applied to actual geological stratums, the proppants with the optimal concentration values are correspondingly measured, and the flow value of shale gas can be obtained through testing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of shale gas conductivity testing, and in particular to a shale gas conductivity measuring device and method. Background Art

[0002] Hydraulic fracturing is the most effective measure for shale gas development at this stage. After hydraulic fracturing, the effective conductivity of the fractures supported by proppants is also the key to evaluating the success of the transformation measures. The conductivity of shale fractures is tested using liquid as the displacement medium.

[0003] Publication (Announcement) No.: CN217132892U, discloses an integrated device for measuring shale gas conductivity, including a measuring mechanism, an air intake mechanism and a liquid intake mechanism; the measuring mechanism includes a flow diversion chamber, an inlet pipe, a flow meter, a first pressure sensor, a second pressure sensor and a displacement sensor; the air intake mechanism includes a gas cylinder and a gas valve; the liquid intake mechanism includes a liquid storage tank and a liquid intake valve. The beneficial effect of the technical solution proposed by the utility model is: when it is necessary to measure the gas-measured flow conductivity of the fracturing proppant, the liquid intake valve is closed and the air valve is opened, so that the gas in the gas cylinder enters the flow diversion chamber through the inlet pipe and is discharged from the outlet; when it is necessary to measure the liquid-measured flow conductivity of the fracturing proppant, the air valve is closed and the liquid intake valve is opened, so that the liquid in the liquid storage tank enters the flow diversion chamber through the inlet pipe and is discharged from the outlet, so that the gas-measured flow conductivity and the liquid-measured flow conductivity of the fracturing proppant can be measured simultaneously by this device.

[0004] The technical problems existing in the prior art are: First, it is impossible to measure the precise fracture conductivity by simulating mixed proppants at different concentrations under different geological pressure conditions, which results in great limitations in shale layer conductivity testing and makes it impossible to use it in actual shale gas extraction.

[0005] Second, shale layer testing is currently still based on glass plates or flat plate structures, which limits the simulation testing of geological layers in actual environments, and the assembly and sealing of shale layers cannot be effectively guaranteed, resulting in poor sealing, which can easily cause large deviations in simulated geological pressure and conductivity.

[0006] Therefore, it is necessary to provide a shale gas conductivity measurement device and method. Summary of the invention

[0007] In view of the problems existing in the above-mentioned prior art, the present invention provides a shale gas conductivity measurement device and method, the purpose of which is to achieve micro-fracture conductivity to ensure the seepage capacity of the micro-fracture system with smaller proppants, thereby improving the gas supply capacity of the matrix to the macro-hydraulic fractures. Based on the dynamic migration and laying process of the proppant in the micro-fracture, by constructing an experimental platform and evaluation method for measuring shale gas conductivity, dynamic sand laying and conductivity test evaluation of micro-fracture rock samples are carried out to reveal the relationship between the conductivity of the propped micro-fracture under the steady pressure value under different sand laying concentration conditions.

[0008] In order to achieve the above-mentioned purpose, the present invention is implemented through the following technical scheme: a shale gas conductivity measurement device, including a core sealing container assembly, a proppant mixing assembly, and a mixed liquid collection assembly. The proppant mixing assembly is pressurized by a booster pump to mix the proppant and flow through a flow meter 1, a pressure detector, a switch valve, a core sealing container assembly and a mixed liquid collection assembly in sequence. A pressure-stabilizing pump is provided on one side of the core sealing container assembly, and a flow meter 2 is provided between the core sealing container assembly and the mixed liquid collection assembly. The core sealing container assembly includes a sealing box body and a sealing cover plate. The top end surface of the sealing box body is provided with a sealing groove 1, and the bottom end surface of the sealing box body is provided with an outlet. The middle part of the sealing groove 1 is provided with a core accommodating chamber, and the core accommodating chamber is provided with a core accommodating chamber. The cavity extends to the inside of the sealing box along its axial direction, a boosting hole is arranged outside the sealing box, the boosting hole is connected with the core accommodating chamber, a pressure-stabilizing pump is installed in the boosting hole, a cylindrical core is placed inside the core accommodating chamber, and a sealing sleeve is arranged between the cylindrical core and the core accommodating chamber, a sealing plug-in plate is arranged on the side of the sealing cover plate facing the sealing box, a sealing groove 2 is arranged in the middle of the sealing plug-in plate, the sealing groove 2 is sleeved and installed with the part of the cylindrical core extending out of the core accommodating chamber, an inlet is arranged in the middle of the sealing cover plate, and the inlet is connected with the sealing groove 2, a threaded hole 1 is arranged on the circumferential surface of the sealing box outside the sealing groove 1, a threaded hole 2 is arranged on the sealing cover plate at a position corresponding to the threaded hole 1, and the threaded hole 1 and the threaded hole 2 are installed by bolts.

[0009] Preferably, heating holes are circumferentially distributed on a surface of the sealing groove at the periphery of the core accommodating cavity, the heating holes extend to the interior of the sealing box, and heating rods are arranged inside the heating holes.

[0010] Preferably, the proppant mixing assembly includes a mixing section and a pressure section, a piston is provided between the mixing section and the pressure section, a pre-loaded proppant container is provided in communication with the mixing section, a stirring fan is provided at the bottom of the mixing section, and a booster pump is provided in communication with the pressure section.

[0011] Preferably, a filter layer is provided in the middle of the mixed liquid collection component to perform solid-liquid separation on the collected proppant.

[0012] A method for measuring shale gas conductivity, according to any one of claims 1 to 4, wherein the measuring method is: Step 1: Select a cylindrical core with a slit width of 0.26 mm opened along the long axis direction, and place the cylindrical core seal in a sealed box, and seal and install it with the sealed box through a sealing cover plate to ensure the sealing setting of the cylindrical core. A pressure-stabilizing pump is set on one side of the sealed box, and the pressure-stabilizing pump simulates the pressure value of the geological layer in the core containing cavity of the sealed box. The inlet of the sealed box is sequentially provided with a switch valve, a pressure detector, a flow meter 1, and a proppant mixing component. The proppant mixing component is connected to a booster pump and a pre-installed proppant container, and the outlet of the sealed box is sequentially connected to a mixed liquid collection component and a flow meter 2; Step 2: After the sealing installation is completed in step 1, close the valve between the pre-installed proppant container and the proppant mixing assembly, close the valve of the second flow meter, pressurize the piston with a booster pump to compress the gas in the mixing part into the overall test production line, observe the pressure change of the pressure detector, and the pressure detector keeps the value unchanged, confirming that the overall test production line is well sealed; Step 3: After the sealing test in step 2 is completed, the concentration of the prefabricated mixed proppant is configured to be 0kg / m2 to 1kg / m2 of sand concentration, and each concentration value corresponds to the pressure value of the pressure regulating pump of 1MPa, 5MPa, 10MPa, 15MPa, 20MPa, and 25MPa, respectively. The flow conductivity of the columnar core opening is tested through flow meter 2.

[0013] Step 4: The test in step 3 shows that when the sand concentration is 0kg / m2 and the pressure of the pressure-stabilizing pump is 1MPa, the conductivity of the propped crack is 6.472µm2*cm. When the pressure of the pressure-stabilizing pump gradually increases to 10MPa, the conductivity of the propped crack measured by flow meter 2 drops to 1.023µm2*cm.

[0014] Step 5: When the concentration of sand was 0kg / m2 and 0.0371kg / m2, respectively, and the pressure value of the pressure-stabilizing pump was 1MPa, the conductivity of the cylindrical core openings was 6.472µm2*cm and 3.535µm2*cm, respectively. When the pressure value of the pressure-stabilizing pump gradually increased to 25MPa, the conductivity of the cylindrical core openings decreased to 0.343µm2*cm and 0.638µm2*cm, respectively, with a decrease of 94.70% and 81.95%, respectively.

[0015] Step 6: When the concentration of sand is 0.078kg / m2, the flow conductivity reaches the maximum when the pressure values ​​of the pressure-stabilizing pump are 20MPa and 25MPa, which are 1.497µm2*cm and 1.246µm2*cm respectively.

[0016] Step 7: Test the flow conductivity by using different pressure-stabilizing pump pressure values ​​corresponding to different sand concentrations in steps 3-6, and then obtain the proppant conductance based on the flow measured by flow meter 2. The difference between the flow measured by flow meter 1 can be used to obtain the amount of sand retained in the columnar core openings, and then obtain the amount of sand retained in the columnar core openings at different pressure-stabilizing pump pressure values.

[0017] Step 8: Based on step 7, the concentration of the sand in step 3 is measured, and the amount of sand retained in the columnar core opening is obtained under different pressure values ​​of the pressure regulating pump.

[0018] In summary, the present invention provides a shale gas conductivity measurement device and method, which obtains the flow rate of the proppant discharged through the flow meter 2 test, obtains the difference between the measurement of the flow meter 1 and the measurement of the flow meter 2, obtains the mixed proppant concentration values ​​corresponding to different pressure values ​​of the pressure regulating pump, and obtains the amount of sand retained inside the fracture of the columnar core, so as to measure the support strength surface size of proppant with different concentrations under different pressure values; And by testing the conductivity of different mixed proppant concentrations under different pressure conditions of the stabilizing pump: testing the conductivity of the mixed proppant flowing through the core sealing container assembly to simulate the conductivity of different mixed proppant concentrations. The patented structure has wide practicality and is closer to the conductivity of the actual rock formation under different pressure values.

[0019] The sealing box and the sealing cover are sealed and installed, and the cylindrical core is sealed and installed in the sealing box, so that the test of the conductivity of the cylindrical core fracture is more accurate, and the sealing reason is avoided, which causes a large deviation in the conductivity. Through the use of the sealing box of this patent, the accurate test of the diversion of the proppant is realized. By setting a boosting hole on the top of the sealing box, the boosting hole is connected to a pressure-stabilizing pump, and the pressure value of the simulated geological pressure inside the sealing box is simulated by the pressure-stabilizing pump, such as 1MPa, 5MPa, 10MPa and other pressure values. Under the conditions of simulating different pressure values, the diversion capacity of proppants with different concentrations is tested, such as 0kg / m2, 0.0371kg / m2, 0.0568kg / m2, and 0.0873kg / m2 of proppant concentrations; to determine the diversion of proppants with different concentrations under the same pressure value, so as to apply to different pressure values ​​of the actual geological layer, to correspond to the proppant with the preferred concentration value measured, and to test and obtain the flow value of shale gas. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is a schematic diagram of the shale gas conductivity measurement structure of the present invention; Figure 2 It is a schematic structural diagram of a core sealing container assembly of the present invention; Figure 3 It is a schematic diagram of the structure of the sealed box of the present invention; Figure 4 It is a schematic diagram of the structural analysis of the sealing cover plate of the present invention; Figure 5 It is a data table of the test evaluation results of the flow conductivity of cylindrical core fractures of the present invention; Figure 6 Schematic diagram of the relationship between the conductivity and the pressure value of the pressure-stabilizing pump under different proppant concentration conditions of the present invention; Figure 7 It is a schematic diagram of the relationship curve between the fracture conductivity and the concentration of the sand under the high pressure-stabilizing pump pressure value condition of the present invention; Figure 8 Schematic diagram of the relationship between the concentration of retained sand in the fracture and the pressure value of the pressure regulating pump under different proppant concentration conditions of the present invention; In the figure: core sealing container assembly 1, proppant mixing assembly 2, mixed liquid collecting assembly 3, booster pump 4, flow meter 1 5, pressure detector 6, switch valve 7, pressure stabilizing pump 11, flow meter 2 12, sealing box 13, sealing cover plate 14, sealing groove 1 15, outlet 16, core accommodating chamber 17, booster hole 21, cylindrical core 22, sealing sleeve 23, sealing groove 2 24, inlet 25, threaded hole 1 26, threaded hole 27, heating hole 31, mixing section 32, pressure section 33, pre-loaded proppant container 34, stirring blade 35, filter layer 36. DETAILED DESCRIPTION

[0021] The present invention will be further described below in conjunction with the accompanying drawings.

[0022] like Figures 1 to 8 As shown: The present invention is a shale gas conductivity measuring device, comprising a core sealed container assembly 1, a proppant mixing assembly 2, and a mixed liquid collecting assembly 3. The proppant mixing assembly 2 is pressurized by a booster pump 4 to mix proppant and flow through a flow meter 15, a pressure detector 6, a switch valve 7, a core sealed container assembly 1, and a mixed liquid collecting assembly 3 in sequence. A pressure-stabilizing pump 11 is provided on one side of the core sealed container assembly 1. A flow meter 2 12 is provided between the core sealed container assembly 1 and the mixed liquid collecting assembly 3. The core sealed container assembly 1 comprises a sealed box body 13 and a sealed cover plate 14. The top end surface of the sealed box body 13 is provided with a sealing groove 15. The bottom end surface of the sealed box body 13 is provided with an outlet 16. The middle part of the sealing groove 15 is provided with a core accommodating chamber 17. The core accommodating chamber 17 extends to the inside of the sealed box body 13 along its axial direction. The sealed box body 13 is provided with a sealing groove 15. The sealing groove 15 is provided with an outlet 16. The middle part of the sealing groove 15 is provided with a core accommodating chamber 17. The core accommodating chamber 17 extends to the inside of the sealed box body 13 along its axial direction. A boosting hole 21 is arranged on the outside of 13, and the boosting hole 21 is connected with the core accommodating chamber 17, and a pressure-stabilizing pump 11 is installed in the boosting hole 21, a cylindrical core 22 is placed inside the core accommodating chamber 17, and a sealing sleeve 23 is arranged between the cylindrical core 22 and the core accommodating chamber 17, a sealing plug-in plate 141 is arranged on the side of the sealing cover plate 14 facing the sealing box body 13, a sealing groove 24 is arranged in the middle of the sealing plug-in plate 141, and the sealing groove 24 and the part of the cylindrical core 22 extending out of the core accommodating chamber 17 are sleeved and installed, an inlet 25 is arranged in the middle of the sealing cover plate 14, and the inlet 25 is connected with the sealing groove 24, a threaded hole 126 is arranged on the circumferential surface of the sealing box body 13 outside the sealing groove 15, and a threaded hole 27 is arranged on the sealing cover plate 14 at a position corresponding to the threaded hole 126, and the threaded hole 126 and the threaded hole 27 are installed by bolts.

[0023] In order to solve the problems in the prior art that the conductivity of the shale layer fracturing environment cannot be simulated according to different mixed proppant concentrations under different pressure conditions to adapt to the actual shale gas extraction; and the sealing test of the rock block is poor, resulting in poor accuracy of the rock formation fracturing conductivity test; for this reason, the technical structure adopted by the patent is: the proppant mixing component 2 is pre-loaded with mixed proppant, and different concentrations of mixed proppant are pre-loaded in the proppant mixing component 2 according to the measurement order, such as 0kg / m2, 0.0371kg / m2, 0.0568kg / m2, 0.0873kg / m2; The piston is pressurized by the booster pump 4, so that the mixed proppant in the mixing part 32 flows through the flow meter 5 to measure the initial flow value, and the pressure flow rate of the proppant is detected by the pressure detector 6 to ensure that the pressure value of the pressure-stabilizing pump 11 in the simulated core sealing container assembly 1 can make the proppant pass through the core sealing container assembly 1 smoothly, so as to finally measure the flow conductivity under the pressure value of the pressure-stabilizing pump 11; after the pressure-stabilizing pump 11 determines the simulated pressure value in the core sealing container assembly 1, such as 1MPa, 5MPa, 10MPa and other pressure values; The switch valve 7 is opened and closed to make the proppant flow from the inlet 25 to the middle crack of the cylindrical core 22. Some sand particles in the proppant enter the crack of the cylindrical core 22, and part of the sand particles are brought into the mixed liquid collection component 3 by the diversion effect. The flow rate of the diverted proppant is tested by the flow meter 12. The difference between the measurement of the flow meter 15 and the measurement of the flow meter 2 12 is obtained under different pressure values ​​of the constant pressure pump 11 and corresponding to different mixed proppant concentrations. The amount of sand retained in the crack of the cylindrical core 22 is obtained, so as to measure the support strength surface size of proppants with different concentrations under different pressure values; And by testing the conductivity of different mixed proppant concentrations under different pressure values ​​of the pressure-stabilizing pump 11: testing the conductivity of the mixed proppant flowing through the core sealing container assembly 1, to simulate the conductivity of different mixed proppant concentrations. The patent structure has wide practicality and is closer to the conductivity of the actual rock formation under different pressure values.

[0024] A core accommodating chamber 17 is opened inside the sealed box 13, a cylindrical core 22 is sealed and sleeved by a sealing sleeve 23, and the cylindrical core 22 is loaded into the core accommodating chamber 17, and the sealing cover plate 14 is sealed and covered with the sealed box 13 to seal the cylindrical core 22 inside the core accommodating chamber 17, so that the mixed proppant flows from the inlet 25, the fracture of the cylindrical core 22, and the outlet 16 to the flow meter 12 to measure the flow rate, so as to test and obtain the conductivity; The sealing box 13 seals the cylindrical core 22 in the following manner: a sealing groove 15 is provided at the inlet end of the sealing box 13, a sealing plug-in plate 141 is provided corresponding to the sealing groove 15 on the sealing cover plate 14, the sealing plug-in plate 141 is preferably made of a soft material, such as a rubber material, a threaded hole 26 is provided circumferentially at the inlet end of the sealing box 13, a threaded hole 27 is provided circumferentially corresponding to the threaded hole 26 on the sealing cover plate 14, a sealing groove 24 for sealing the cylindrical core 22 is provided in the middle of the sealing plug-in plate 141, when the sealing box 13 and the sealing cover plate 14 are sealed and installed, the sealing groove 24 is sealed and installed on the cylindrical core 22, the sealing plug-in plate 141 is sealed and plugged into the sealing groove 15, and the threaded hole 26 and the threaded hole 27 are installed by bolts to realize the sealing installation of the sealing box 13 and the sealing cover plate 14, and the sealing of the cylindrical core 22 is achieved. The seal 22 is installed in the sealing box 13, which makes the test of the conductivity of the columnar core 22 fracture more accurate, avoids the large deviation of the conductivity caused by the sealing reason, and realizes the accurate test of the conductivity of the proppant by using the sealing box 13 of the present patent. By setting the boosting hole 21 on the top of the sealing box 13, the boosting hole 21 is connected to the pressure-stabilizing pump 11, and the pressure value of the simulated geological pressure inside the sealing box 13 is simulated by the pressure-stabilizing pump 11, such as 1MPa, 5MPa, 10MPa and other pressure values. Under the conditions of simulating different pressure values, the conductivity of proppants with different concentrations is tested to determine the conductivity of proppants with different concentrations under the same pressure value, so as to apply different pressure values ​​of the actual geological layer, to correspond to the proppant with the preferred concentration value measured, and to obtain the flow value of shale gas through testing.

[0025] In at least one embodiment, in order to test the temperature conditions in the rock formation geological environment, the structure adopted is: heating holes 31 are circumferentially distributed on the surface of the sealing groove 15 outside the core accommodating chamber 17, and the heating holes 31 extend to the inside of the sealing box 13. A heating rod is arranged inside the heating hole 31. By controlling the temperature of the core accommodating chamber 17, a more accurate simulation of the flow conductivity of the geological environment can be achieved.

[0026] In at least one embodiment, the proppant mixing assembly 2 includes a mixing section 32 and a pressure section 33, a piston is provided between the mixing section 32 and the pressure section 33, a pre-loaded proppant container 34 is provided in communication with the mixing section 32, a stirring blade 35 is provided at the bottom of the mixing section 32, and a booster pump 4 is provided in communication with the pressure section 33.

[0027] The mixed proppant in the mixing section 32 is mixed by the stirring blades 35 to improve the concentration of the proppant for accurate use and meet the actual measurement conditions for testing the proppant diversion. The piston of the booster pump 4 is pressurized to inject the mixed proppant in the mixing section 32 into the cracks of the columnar core 22, and the outflowing flow is measured by the flow meter 12 to obtain the diversion capacity of proppants with different concentrations under different pressure conditions.

[0028] In at least one embodiment, a filter layer 36 is provided in the middle of the mixed liquid collection component 3 to separate the collected proppant into solid and liquid. The water and sand particles in the proppant pass through the filter layer 36 to obtain a measured value of the diversion, so as to obtain a diversion capacity value for the collection and recovery of the proppant.

[0029] A method for measuring shale gas conductivity, according to any one of claims 1 to 4, wherein the measuring method is: Step 1: Select a cylindrical core 22 with a slit width of 0.26 mm opened along the long axis direction, and seal the cylindrical core 22 in a sealed box 13, and seal and install it with the sealed box 13 through a sealing cover plate 14 to ensure the sealing of the cylindrical core 22. A pressure-stabilizing pump 11 is arranged on one side of the sealed box 13, and the pressure-stabilizing pump 11 simulates the pressure value of the geological layer for the core containing cavity 17 of the sealed box 13. The inlet 25 of the sealed box 13 is sequentially provided with a switch valve 7, a pressure detector 6, a flow meter 1 5, and a proppant mixing component 2. The proppant mixing component 2 is connected to a booster pump 4 and a pre-installed proppant container 34, and the outlet 16 of the sealed box 13 is sequentially connected to a mixed liquid collection component 3 and a flow meter 2 12; Step 2: After the sealing installation is completed in step 1, close the valve between the pre-installed proppant container 34 and the proppant mixing assembly 2, close the valve of the flow meter 2 12, pressurize the piston with the booster pump 4 to compress the gas in the mixing part 32 into the overall test production line, observe the pressure change of the pressure detector 6, and the pressure detector 6 keeps the value unchanged, confirming that the overall test production line is well sealed; Step 3: If Figure 5 As shown in the data: after the sealing test in step 2 is completed, the concentration of the prefabricated mixed proppant is configured to be 0kg / m2 to 1kg / m2 of sand concentration, and each concentration value corresponds to the pressure value of the pressure regulating pump 11 of 1MPa, 5MPa, 10MPa, 15MPa, 20MPa, and 25MPa, respectively. The flow conductivity of the slit of the columnar core 22 is tested by the flow meter 12, and the diversion data at different pressure values ​​are obtained and recorded by the terminal computer.

[0030] Step 4: Figure 5Data shows: Through the terminal computer data recording test in step 3, it is concluded that when the sand concentration is 0kg / m2 and the pressure value of the pressure-stabilizing pump 11 is 1MPa, the conductivity of the support crack is 6.472µm2*cm. When the pressure value of the pressure-stabilizing pump 11 gradually increases to 10MPa, the conductivity of the support crack measured by the flow meter 12 drops to 1.023µm2*cm.

[0031] Step 5: Figure 5 , Figure 6 The data shows that when the concentration of the sand is 0kg / m2 and 0.0371kg / m2, respectively, and the pressure value of the pressure-stabilizing pump 11 is 1MPa, the conductivity of the slits of the cylindrical core 22 is 6.472µm2*cm and 3.535µm2*cm, respectively. When the pressure value of the pressure-stabilizing pump 11 gradually increases to 25MPa, the conductivity of the slits of the cylindrical core 22 decreases to 0.343µm2*cm and 0.638µm2*cm, respectively, with a decrease of 94.70% and 81.95%, respectively.

[0032] Step 6: Figure 7 The data shows: Through the comparison of terminal computer data, it is concluded that when the sand concentration is 0.078kg / m2, the flow conductivity reaches the maximum when the pressure values ​​of the pressure-stabilizing pump 11 are 20MPa and 25MPa respectively, which are 1.497µm2*cm and 1.246µm2*cm respectively.

[0033] Step 7: Figure 8 As shown in the data: the flow conductivity is tested by using different pressure values ​​of the pressure-stabilizing pump 11 corresponding to different sand concentrations in steps 3-6, and then the proppant conduction volume is obtained based on the flow measurement of the flow meter 12. The difference between the flow measurement of the flow meter 15 and the sand volume retained in the slit of the columnar core 22 can be obtained, and then the sand volume retained in the slit of the columnar core 22 under different pressure values ​​of the pressure-stabilizing pump 11 can be obtained by testing different concentrations of proppant.

[0034] Step 8: On the basis of step 7, the concentration of the sand in step 3 is measured, and the amount of sand retained in the slits of the columnar core 22 with different proppant concentrations is obtained under different pressure values ​​of the pressure-stabilizing pump 11.

[0035] The embodiments of the present invention are only used to illustrate the present invention and do not constitute a limitation on the scope of the claims. Other substantially equivalent substitutes that can be thought of by those skilled in the art are all within the protection scope of the present invention.

Claims

1. A shale gas conductivity measuring device, characterized in that: The invention comprises a core sealing container assembly (1), a proppant mixing assembly (2), and a mixed liquid collecting assembly (3). The proppant mixing assembly (2) is pressurized by a booster pump (4) to mix proppant and flow through a flow meter (5), a pressure detector (6), a switch valve (7), a core sealing container assembly (1), and a mixed liquid collecting assembly (3) in sequence. A pressure-stabilizing pump (11) is arranged on one side of the core sealing container assembly (1). A flow meter (12) is arranged between the core sealing container assembly (1) and the mixed liquid collecting assembly (3). The core sealing container assembly (1) comprises a sealing box (13) and a sealing cover plate (14). The top end surface of the sealing box (13) is provided with a sealing groove (15). The bottom end surface of the sealing box (13) is provided with an outlet (16). The middle part of the sealing groove (15) is provided with a core accommodating chamber (17). The core accommodating chamber (17) extends along its axial direction to the inside of the sealing box (13). A pressurizing hole (12) is arranged on the outside of the sealing box (13). 21), the boost hole (21) is connected to the core accommodating chamber (17), a pressure-stabilizing pump (11) is installed in the boost hole (21), a cylindrical core (22) is placed inside the core accommodating chamber (17), and a sealing sleeve (23) is arranged between the cylindrical core (22) and the core accommodating chamber (17), a sealing plug-in plate (141) is arranged on the side of the sealing cover plate (14) facing the sealing box body (13), and a sealing groove 2 (24) is provided in the middle of the sealing plug-in plate (141), and the sealing groove 2 The sealing cover plate (14) is provided with an inlet (25) in the middle part thereof, and the inlet (25) is connected with the sealing groove (24). The sealing box body (13) is provided with a threaded hole (26) on the circumferential surface of the sealing groove (15). The sealing cover plate (14) is provided with a threaded hole (27) at a position corresponding to the threaded hole (26). The threaded hole (26) and the threaded hole (27) are installed by bolts.

2. A shale gas conductivity measuring device according to claim 1, characterized in that: Heating holes (31) are circumferentially distributed on the surface of the sealing groove 1 (15) outside the core accommodating chamber (17), the heating holes (31) extend to the inside of the sealing box (13), and a heating rod is arranged inside the heating hole (31).

3. The shale gas conductivity measuring device according to claim 1, characterized in that: The proppant mixing assembly (2) comprises a mixing section (32) and a pressure section (33), a piston is arranged between the mixing section (32) and the pressure section (33), a pre-installed proppant container (34) is arranged in communication with the mixing section (32), a stirring blade (35) is arranged at the bottom of the mixing section (32), and a booster pump (4) is arranged in communication with the pressure section (33).

4. A shale gas conductivity measurement device and method according to claim 1, characterized in that: A filter layer (36) is provided in the middle of the mixed liquid collection component (3) to perform solid-liquid separation on the collected proppant.

5. A method for measuring shale gas conductivity, characterized in that: According to any one of claims 1-4, the measuring method is: Step 1: Select a cylindrical core (22) with a slit width of 0.26 mm opened along the long axis direction, and seal the cylindrical core (22) in a sealed box (13). The cylindrical core (22) is sealed and installed with the sealed box (13) through a sealing cover plate (14) to ensure the sealing of the cylindrical core (22). A pressure-stabilizing pump (11) is arranged on one side of the sealed box (13). The pressure-stabilizing pump (11) simulates the pressure value of the geological layer in the core containing chamber (17) of the sealed box (13). The inlet (25) of the sealed box (13) is sequentially provided with a switch valve (7), a pressure detector (6), a flow meter (5), and a proppant mixing component (2). The proppant mixing component (2) is connected to a booster pump (4) and a pre-installed proppant container (34). The outlet (16) of the sealed box (13) is sequentially connected to a mixed liquid collection component (3) and a flow meter (12). Step 2: After the sealing installation is completed in step 1, close the valve between the pre-installed proppant container (34) and the proppant mixing assembly (2), close the valve of the second flow meter (12), pressurize the piston with the booster pump (4) to compress the gas in the mixing part (32) into the overall test production line, observe the pressure change of the pressure detector (6), and the pressure detector (6) keeps the value unchanged, to determine that the overall test production line is well sealed; Step 3: After the sealing test in step 2 is completed, the concentration of the prefabricated mixed proppant is configured to be 0kg / m2 to 1kg / m2 of the sand-laying concentration, and each concentration value corresponds to the pressure value of the pressure-regulating pump (11) of 1MPa, 5MPa, 10MPa, 15MPa, 20MPa, and 25MPa, respectively, and the flow conductivity of the opening of the columnar core (22) is tested through the second flow meter (12); Step 4: Through the test in step 3, it is found that when the concentration of the sand is 0kg / m2 and the pressure value of the pressure-stabilizing pump (11) is 1MPa, the conductivity of the propped crack is 6.472µm2*cm. When the pressure value of the pressure-stabilizing pump (11) gradually increases to 10MPa, the conductivity of the propped crack measured by the flow meter 2 (12) decreases to 1.023µm2*cm. Step 5: When the concentration of the sand is 0kg / m2 and 0.0371kg / m2, respectively, and the pressure value of the pressure-stabilizing pump (11) is 1MPa, the conductivity of the slits of the columnar core (22) is 6.472µm2*cm and 3.535µm2*cm, respectively. When the pressure value of the pressure-stabilizing pump (11) gradually increases to 25MPa, the conductivity of the slits of the columnar core (22) decreases to 0.343µm2*cm and 0.638µm2*cm, respectively, with a decrease of 94.70% and 81.95%, respectively. Step 6: When the concentration of the sand is 0.078 kg / m2, the flow conductivity reaches the maximum when the pressure of the pressure regulating pump (11) is 20 MPa and 25 MPa, respectively, which are 1.497 µm2*cm and 1.246 µm2*cm, respectively; Step 7: The flow conductivity is tested by using different pressure values ​​of the pressure regulating pump (11) corresponding to different sand concentrations in steps 3-6, and then the proppant flow conductivity is obtained based on the flow measured by the flow meter 2 (12). The difference between the flow measured by the flow meter 1 (5) can be used to obtain the amount of sand retained in the slit of the columnar core (22), and then the amount of sand retained in the slit of the columnar core (22) under different pressure values ​​of the pressure regulating pump (11) can be obtained; Step 8: Based on step 7, the concentration of the sand in step 3 is measured, and the amount of sand retained in the slits of the columnar core (22) is obtained under different pressure values ​​of the pressure regulating pump (11).