Inkjet recording method
By continuously performing the ink and reaction liquid adhesion process in inkjet printing and dyeing technology, using the inkjet method of self-dispersed pigment and coagulant, the problem of equipment complexity and color rendering in the prior art is solved, and high color rendering is achieved Image effects of sexuality and fastness.
Patent Information
- Application Number
- CN202410700427.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-06-02
- Filing Date
- 2024-05-31
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-05-31
AI Technical Summary
In the existing inkjet printing and dyeing technology, the adhesion process of the pretreatment liquid and the coating liquid requires large-scale equipment and cumbersome processes, and continuous processing in the same device may lead to a decrease in color rendering.
The first ink adhesion process, the reaction liquid adhesion process and the second ink adhesion process are continuously carried out by inkjet method, and the ink composition containing a self-dispersed pigment, the reaction liquid composition and the reaction liquid composition containing a coagulant are ejected, and the The adhesion is completed in a very short time, with a time difference of less than 45 milliseconds.
The color rendering and fastness of the image are improved, the equipment complexity and process cumbersomeness are reduced, the coagulation reaction of the ink composition is enhanced, and the pigment remains well on the surface of the fabric.
Smart Images

Figure HDA0004870890660000011 
Figure HDA0004870890660000021 
Figure HDA0004870890660000031
Abstract
Description
Technical Field
[0001] The present invention relates to an inkjet recording method. Background Art
[0002] Inkjet printing is not only used for recording images on paper, but also for printing on fabrics, and various inkjet printing methods are being studied. Inkjet inks used for printing contain colorants, and dyes and pigments are used as colorants to obtain images of desired colors. In addition, in inkjet printing, many studies are being conducted on inks and recording methods.
[0003] For example, in inkjet printing, in order to improve the color development and fastness of the image, the application of pretreatment to the fabric and the coating of the image are studied. For example, Patent Document 1 discloses that an attempt is made to treat with a pretreatment liquid in pigment printing, and the ink is directly attached without the process of drying the pretreatment liquid.
[0004] Prior art literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Application Publication No. 2016-089288 Summary of the invention
[0007] However, the application of the pretreatment liquid and the coating liquid is often performed by separate devices, requiring large-scale equipment and complicated processes. On the other hand, when the treatment liquid and the coating liquid are attached continuously in the same device, the color development may be reduced.
[0008] One embodiment of the inkjet recording method according to the present invention comprises:
[0009] A first ink adhesion step of ejecting an ink composition containing a self-dispersible pigment by an inkjet method and adhering the ink composition to a fabric;
[0010] a reaction liquid attachment step of ejecting a reaction liquid composition by an inkjet method and attaching it to a cloth, wherein the reaction liquid composition contains a coagulant for aggregating components in the ink composition; and
[0011] In the second ink adhesion step, an ink composition containing a self-dispersible pigment is ejected by an inkjet method and adhered to the fabric.
[0012] The first ink attaching step, the reaction liquid attaching step and the second ink attaching step are performed successively in sequence.
[0013] The time difference from the time when the ink composition is attached by the first ink attaching step to the time when the reaction liquid composition is attached to the region to which the ink composition is attached by the reaction liquid attaching step is within 45 milliseconds.
[0014] The time difference from the reaction liquid composition being attached in the reaction liquid attaching step to the ink composition being attached to the region to which the reaction liquid composition is attached in the second ink attaching step is within 45 milliseconds. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic diagram of an inkjet recording apparatus applicable to the inkjet recording method according to the present embodiment.
[0016] Figure 2 It is a schematic diagram of one example of an inkjet head of an inkjet recording device.
[0017] Figure 3 Table 1 shows the compositions of reaction liquid compositions used in Examples and Comparative Examples.
[0018] Figure 4 Table 2 shows the compositions of ink compositions used in Examples and Comparative Examples.
[0019] Figure 5 Table 3 shows the compositions of the clear ink compositions used in Examples and Comparative Examples.
[0020] Figure 6 Table 4 shows the conditions and evaluation results of Examples.
[0021] Figure 7 Table 5 shows conditions and evaluation results of Examples and Comparative Examples.
[0022] Description of Reference Numerals
[0023] 1: control unit; 10: medium supply unit; 11: supply shaft unit; 12: bearing unit; 20: medium conveying unit; 21: conveying roller; 22: conveying roller; 23: endless belt; 23a: surface; 23b: inner circumference; 24: belt rotating roller; 25: belt driving roller; 26: conveying roller; 27: heating unit; 28: conveying roller; 29: adhesive; 30: medium recovery unit; 31: winding shaft unit; 32: bearing unit; 40: printing unit; 41: nozzle row; 42a to 42b g: inkjet head; 43: bracket; 45: bracket moving part; 45a: guide rail; 45b: guide rail; 46: pressure plate; 50: cleaning unit; 51: cleaning part; 52: pressing part; 53: moving part; 54: cleaning tank; 55: scraper; 56: cylinder; 57: ball bushing; 58: cleaning roller; 60: medium sealing part; 61: pressing part; 69: abutting part; 90: machine body; 91: belt supporting part; 95: cloth; 99: floor surface; 100: recording device. DETAILED DESCRIPTION
[0024] The following describes the embodiments of the present invention. The embodiments described below are examples for illustrating the present invention. The present invention is not limited to the following embodiments in any way, and also includes various modifications implemented within the scope of the present invention. It should be noted that the structures described below are not necessarily all necessary structures of the present invention.
[0025] 1. Inkjet recording method
[0026] The inkjet recording method according to the present embodiment comprises: a first ink attaching step of ejecting an ink composition containing a self-dispersible pigment by an inkjet method and attaching it to a cloth; a reaction liquid attaching step of ejecting a reaction liquid composition by an inkjet method and attaching it to a cloth, wherein the reaction liquid composition contains a coagulant for aggregating components in the ink composition; and a second ink attaching step of ejecting an ink composition containing a self-dispersible pigment by an inkjet method and attaching it to a cloth; the first ink attaching step, the reaction liquid attaching step and the second ink attaching step are performed successively in this order,
[0027] The time difference from the time when the ink composition is attached by the first ink attachment step to the time when the ink reaction liquid composition is attached to the region to which the composition is attached by the reaction liquid attachment step is within 45 milliseconds, and the time difference from the time when the reaction liquid composition is attached by the reaction liquid attachment step to the time when the ink composition is attached to the region to which the reaction liquid composition is attached by the second ink attachment step is within 45 milliseconds.
[0028] 1.1. First ink adhesion step
[0029] In the first ink adhesion step, an ink composition containing a self-dispersible pigment is ejected by an inkjet method and adhered to the fabric.
[0030] 1.1.1. Ink composition
[0031] The ink composition contains a self-dispersible pigment.
[0032] 1.1.1.(1) Self-dispersible pigments
[0033] The self-dispersible pigment contained in the ink composition is not a pigment dispersed by a dispersant, etc., but is a self-dispersible pigment that can be dispersed without a dispersant, etc. by oxidizing or sulfonating the surface of the pigment particles using, for example, ozone, hypochlorous acid, fuming sulfuric acid, etc. As the self-dispersible pigment contained in the ink composition, for example, color pigments such as black, cyan, yellow, magenta, red, green, orange, and special pigments such as white can be used, and these pigments are self-dispersible pigments.
[0034] The self-dispersible pigment may be a mixture. The pigment is excellent in storage stability such as light resistance, weather resistance, and gas resistance, and from this viewpoint, an organic pigment is preferred.
[0035] Specifically, the pigment uses azo pigments such as insoluble azo pigments, condensed azo pigments, azo lakes, chelated azo pigments, phthalocyanine pigments, perylene and pyrene pigments, anthraquinone pigments, quinacridone pigments, dioxane pigments, thioindigo pigments, isoindolinone pigments, quinophthalone pigments and other polycyclic pigments, dye chelating agents, dye lakes, nitro pigments, nitroso pigments, aniline black, daylight fluorescent pigments, carbon black, etc. The above-mentioned pigments can be used alone or in combination of two or more. In addition, as long as it is a self-dispersible pigment, white pigments, brilliant pigments, etc. can also be used.
[0036] Specific examples of the pigment that can be modified to be a self-dispersible type are not particularly limited, and examples thereof include the following.
[0037] Examples of the black pigment include No. 2300, No. 900, MCF88, No. 33, No. 40, No. 45, No. 52, MA7, MA8, MA100, and No. 2200B (all manufactured by Mitsubishi Chemical Corporation), Raven 5750, Raven 5250, Raven 5000, Raven 3500, Raven 1255, and Raven 700 (all manufactured by Carbon Columbia), Regal 400R, Regal 330R, Regal 660R, Mogul L, Monarch 700, Monarch 800, Monarch 880, Monarch 900, Monarch 1000, Monarch 1100, Monarch 1300, and Monarch 1400 (all manufactured by Cabot Corporation). KK)), Color Black FW1, Color Black FW2, Color Black FW2V, Color Black FW18, Color Black FW200, ColorB1ack S150, Color Black S160, Color Black S170, Printex 35, Printex U, Printex V, Printex 140U, Special Black 6, Special Black 5, Special Black 4A, Special Black 4 (all manufactured by Degussa).
[0038] Examples of the yellow pigment include CI Pigment Yellow 1, 2, 3, 4, 5, 6, 7, 10, 11, 12, 13, 14, 16, 17, 24, 34, 35, 37, 53, 55, 65, 73, 74, 75, 81, 83, 93, 94, 95, 97, 98, 99, 108, 109, 110, 113, 114, 117, 120, 124, 128, 129, 133, 138, 139, 147, 151, 153, 154, 167, 172, and 180.
[0039] Examples of the magenta pigment include CI Pigment Red 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 14, 15, 16, 17, 18, 19, 21, 22, 23, 30, 31, 32, 37, 38, 40, 41, 42, 48 (Ca), 48 (Mn), 57 (Ca), 57:1, 88, 112, 114, 122, 123, 144, 146, 149, 150, 166, 168, 170, 171, 175, 176, 177, 178, 179, 184, 185, 187, 202, 209, 219, 224, 245, and CI Pigment Violet 19, 23, 32, 33, 36, 38, 43, and 50.
[0040] Examples of the cyan pigment include CI Pigment Blue 1, 2, 3, 15, 15:1, 15:2, 15:3, 15:34, 15:4, 16, 18, 22, 25, 60, 65, 66, and CI Vat Blue 4 and 60.
[0041] Pigments other than magenta, cyan and yellow are not particularly limited, and examples thereof include CI Pigment Green 7, 10, CI Pigment Brown 3, 5, 25, 26, and CI Pigment Orange 1, 2, 5, 7, 13, 14, 15, 16, 24, 34, 36, 38, 40, 43, and 63.
[0042] As the white pigment, for example, metal compounds such as metal oxides, barium sulfate, and calcium carbonate can be cited. As the metal oxide, for example, titanium dioxide, zinc oxide, silicon dioxide, aluminum oxide, and magnesium oxide can be cited. In addition, particles having a hollow structure can be used as the white pigment, and as the particles having a hollow structure, known particles can be used.
[0043] The self-dispersible pigment is preferably capable of being stably dispersed in a dispersion medium, and more preferably a black pigment capable of self-dispersing carbon black. In addition, in pigment printing and dyeing, the color rendering of black is prone to deterioration, and therefore, by making the self-dispersible pigment a black pigment, the effect of improving the color rendering can be further improved.
[0044] The content of the self-dispersible pigment is preferably 0.3% by mass to 20% by mass, more preferably 0.5% by mass to 15% by mass, relative to the total mass of the ink composition. Also, it is preferably 1% by mass to 10% by mass, more preferably 2% by mass to 7% by mass.
[0045] The volume average particle size of the self-dispersible pigment particles is preferably 10 nm to 300 nm, more preferably 30 nm to 250 nm, further preferably 50 nm to 250 nm, particularly preferably 70 nm to 200 nm, and preferably 80 nm to 150 nm.
[0046] 1.1.1.(2) Other ingredients
[0047] (water)
[0048] The ink composition may contain water. Examples of the water include pure water such as ion exchange water, ultrafiltration water, reverse osmosis water, and distilled water, and water from which ionic impurities are removed as much as possible, such as ultrapure water. In addition, when water is sterilized by irradiation with ultraviolet rays or addition of hydrogen peroxide, the generation of bacteria and fungi can be reduced when the composition is stored for a long time.
[0049] The content of water is 30% by mass or more, preferably 40% by mass or more, more preferably 45% by mass or more, and further preferably 50% by mass or more, relative to the total amount of the ink composition. It should be noted that, when referring to water in the ink composition, for example, it refers to the crystal water contained in the raw material and the added water. By making the water content 30% by mass or more, the ink composition can be made to have a lower viscosity. In addition, the upper limit of the water content is preferably 90% by mass or less, more preferably 85% by mass or less, and further preferably 80% by mass or less, relative to the total amount of the ink composition. It should be noted that in this specification, when referred to as an "aqueous composition", it refers to a composition containing 30% by mass or more of water relative to the total mass (100% by mass) of the composition.
[0050] (Anionic resin)
[0051] The ink composition may contain resin particles. The resin particles are preferably anionic resin particles. In addition, the resin particles are preferably self-dispersible. The resin particles can improve the adhesion of the image formed by the composition attached to the cloth. As anionic resin particles, for example, anionic resin particles can be mentioned among resin particles composed of polyurethane resins, acrylic resins (including styrene acrylic resins), fluorene resins, polyolefin resins, rosin-modified resins, terpene resins, polyester resins, polyamide resins, epoxy resins, vinyl chloride resins, vinyl chloride-vinyl acetate copolymers, ethylene vinyl acetate resins, silicone-acrylic resins, etc. Among them, polyurethane resins, silicone-acrylic resins, acrylic resins, polyolefin resins, and polyester resins are preferred. These resin particles are mostly treated in the form of emulsions, and can also be in the form of powders. In addition, the resin particles can be used alone or in combination of two or more.
[0052] Polyurethane resin is a general term for resins having urethane bonds. Examples of polyurethane resins include polyether polyurethane resins having ether bonds in the main chain in addition to urethane bonds, polyester polyurethane resins having ester bonds in the main chain, and polycarbonate polyurethane resins having carbonate bonds in the main chain. In addition, as the polyurethane resin, commercially available products can be used, for example, SUPERFLEX 460, 460s, 840, E-4000 (trade names, manufactured by Dai-ichi Kogyo Seiyaku Co., Ltd.), RESAMINE D-1060, D-2020, D-4080, D-4200, D-6300, D-6455 (trade names, manufactured by Dainichi Seika Industries, Ltd.), TAKELAC WS-6021, W-512-A-6 (trade names, manufactured by Mitsui Chemicals Polyurethanes, Ltd.), SANCURE 2710 (trade name, manufactured by LUBRIZOL), PERMARIN UA-150 (trade name, manufactured by Sanyo Chemical Industries, Ltd.), ETERNACOLLUW series, for example, UW-1527 (manufactured by Ube Industries, Ltd.) and the like can be used.
[0053] Acrylic resin is a general term for polymers obtained by polymerizing at least acrylic monomers such as (meth)acrylic acid and (meth)acrylate as a single component, and examples thereof include resins obtained from acrylic monomers and copolymers of acrylic monomers and other monomers. Examples thereof include acrylic-vinyl resins which are copolymers of acrylic monomers and vinyl monomers. In addition, examples of vinyl monomers include styrene and the like.
[0054] As acrylic monomers, acrylamide, acrylonitrile, etc. can also be used. The resin emulsion using acrylic resin as raw material can use commercial products, such as FK-854 (trade name, made by Chuo Rika Industry Co., Ltd.), Mowinyl 952B, 718A, 6760 (trade name, made by Nippon Synthetic Chemical Industry Co., Ltd.), Nipol LX852, LX874 (trade name, made by Japan ZEON Co., Ltd.), etc. can be selected.
[0055] It should be noted that, in the present specification, the acrylic resin may be a styrene-acrylic resin. In addition, in the present specification, the term (meth)acrylic acid means at least one of acrylic acid and methacrylic acid.
[0056] Styrene-acrylic resins are copolymers obtained from styrene monomers and (meth)acrylic monomers, and examples thereof include styrene-acrylic acid copolymers, styrene-methacrylic acid copolymers, styrene-methacrylic acid-acrylate copolymers, styrene-α-methylstyrene-acrylic acid copolymers, and styrene-α-methylstyrene-acrylic acid-acrylate copolymers. As the styrene-acrylic resin, commercially available products can be used. For example, JONCRYL 62J, 7100, 390, 711, 511, 7001, 632, 741, 450, 840, 74J, HRC-1645J, 734, 852, 7600, 775, 537J, 1535, PDX-7630A, 352J, 352D, PDX-7145, 538J, 7640, 7641, 631, 790, 780, 7610 (trade names, manufactured by BASF), Mowinyl 966A, 975N (trade names, manufactured by Nippon Synthetic Chemical Industry Co., Ltd.), VINYBLAN 2586 (manufactured by Nissin Chemical Industry Co., Ltd.), etc. can be used.
[0057] As the silicone-acrylic copolymer resin, a commercially available product can be used. For example, FE-230N, FE-502, E-370, RU-911, R-170, R170S, LC-190, and R-170BX of the CHALINE series of Nissin Chemical Industry Co., Ltd., SYMAC US-380SYMAC US-450, and SYMAC US-480 of Toagosei Co., Ltd., IE-7170, SE1980CLEAR, BY22-826EX, and Propylene Oxy LON-MF-40 of Dow Corning Toray Co., Ltd., LEXAN EXL of SABIC INNOVATIVE PLASTICS JAPAN, TAFLON NEO of Idemitsu Kosan Co., Ltd., Banstar-S-806 of Saiden Chemical Co., Ltd., Mowinyl of Nippon Gosei Co., Ltd., COATAX of Toray Co., Ltd., and DAITOSOL of Daito Kasei Kogyo Co., Ltd. 5000SJ, "YODOSOL GH41" from NSC Co., Ltd., Shin-Etsu Chemical Co., Ltd.'s acrylate / ethylhexyl acrylate / dimethylsiloxane methacrylate) copolymer (trade name: KP578), DIC Co., Ltd.'s VONCOAT, CERANATE, JSR's acrylic silicone emulsion "SIFCLEAR S101", "SIFCLEAR S102", etc.
[0058] The polyolefin resin has olefins such as ethylene, propylene, and butene in the structural skeleton, and known materials can be appropriately selected. As the olefin resin, commercially available products can be used, such as Arrow Base CB-1200, CD-1200 (trade name, manufactured by Unitika Co., Ltd.), etc.
[0059] In addition, the resin particles may be provided in the form of an emulsion. Examples of commercially available products of such resin emulsions include MICROGEL E-1002, E-5002 (trade name manufactured by Nippon Paint Co., Ltd., styrene-acrylic resin emulsion), VONCOAT4001 (trade name manufactured by DIC Co., Ltd., acrylic resin emulsion), VONCOAT5454 (trade name manufactured by DIC Co., Ltd., styrene-acrylic resin emulsion), POLYSOL AM-710, AM-920, AM-2300, AP-4735, AT-860, PSASE-4210E (acrylic resin emulsion), POLYSOL AP-7020 (styrene-acrylic resin emulsion), POLYSOL SH-502 (vinyl acetate resin emulsion), POLYSOL AD-13, AD-2, AD-10, AD-96, AD-17, AD-70 (ethylene-vinyl acetate resin emulsion), POLYSOL PSASE-6010 (ethylene-vinyl acetate resin emulsion) (trade name of Showa Denko Co., Ltd.), POLYSOL SAE1014 (trade name, styrene-acrylic resin emulsion, manufactured by Nippon ZEON Co., Ltd.), SAIVINOL SK-200 (trade name, acrylic resin emulsion, manufactured by Saiden Chemical Co., Ltd.), AE-120A (trade name, acrylic resin emulsion manufactured by JSR Co., Ltd.), AE373D (trade name, carboxyl-modified styrene-acrylic resin emulsion manufactured by E-TEK Co., Ltd.), SEIKADYNE 1900W (trade name, ethylene-vinyl acetate resin emulsion manufactured by Dainichi Seika Industries Co., Ltd.), VINYBLAN 2682 (acrylic resin emulsion), VINYBLAN 2886 (vinyl acetate-acrylic resin emulsion), VINYBLAN 5202 (acetic acid acrylic resin emulsion) (trade name of Nissin Chemical Industry Co., Ltd.), ELITEL KA-5071S, KT-8803, KT-9204, KT-8701, KT-8904, KT-0507 (Unitika's trade name, polyester resin emulsion), HYTEC SN-2002 (Toho Chemical's trade name, polyester resin emulsion), TAKELAC W-6020, W-635, W-6061, W-605, W-635, W-6021, WS-5100 (Mitsui Chemicals Polyurethane Co., Ltd.'s trade name, polyurethane resin emulsion), SUPERFLEX 870, 800, 150, 420, 460, 470, 610, 700 (Daiichi Kogyo Seiyaku Co., Ltd.'s trade name,Polyurethane resin emulsion), PERMARIN UA-150 (manufactured by Sanyo Chemical Industries, Ltd., polyurethane resin emulsion), SANCURE 2710 (manufactured by Nippon Lubrizol, polyurethane resin emulsion), NeoRez R-9660, R-9637, R-940 (manufactured by Kusumoto Chemicals, Ltd., polyurethane resin emulsion), ADEKA BONTIGHTER HUX-380, 290K (manufactured by ADEKA Corporation, polyurethane resin emulsion), Mowinyl 966A, Mowinyl 7320 (manufactured by Nippon Synthetic Chemical Co., Ltd.), JONCRYL 7100, 390, 711, 511, 7001, 632, 741, 450, 840, 74J, HRC-1645J, 734, 852, 7600, 775, 537J, 1535, PDX-7630A, 352J, 352D, PDX-7145, 538J, 7640, 7641, 631, 790, 780, 7610 (all manufactured by BASF), NK Binder R-5HN (manufactured by Shin-Nakamura Chemical Co., Ltd.), HYDRAN WLS-210 (non-crosslinking polyurethane: manufactured by DIC Corporation), JONCRYL 7610 (manufactured by BASF), etc.
[0060] The acid value of the resin contained in the resin particles is not particularly limited, but is preferably 1 to 300 KOHmg / g, more preferably 10 to 200 KOHmg / g, and further preferably 20 to 100 KOHmg / g. When the acid value of the resin is within the above range, the resin particles tend to be anionic.
[0061] When the ink composition contains anionic resin particles, the content of the resin particles is preferably 20% by mass or more relative to the total amount of non-volatile components. The content of the resin particles in the ink composition is more preferably 30% by mass or more relative to the total amount of non-volatile components, and further preferably 40% by mass or more.
[0062] When the resin particles are anionic resin particles, the rubbing fastness of the image can be improved while maintaining good color development. This is because when it is desired to mix a fixing resin in the ink composition, the pigment needs to be reduced, which tends to cause poor color development. However, when the fixing resin is anionic resin particles, there is no need to reduce the pigment.
[0063] (Moisturizer)
[0064] The ink composition may contain a moisturizer. The moisturizer is not particularly limited, and examples thereof include glycerol, 2-pyrrolidone, urea, triethanolamine, propylene glycol, 1-(2-hydroxyethyl)-2-pyrrolidone, trimethylolpropane, triethylene glycol, 1,5-pentanediol, triethylene glycol monomethyl ether, and AMINOCOAT. One of these moisturizers may be used alone, or two or more may be used.
[0065] (Other solvents)
[0066] The ink composition may contain other solvents. As such a solvent, a water-soluble organic solvent is preferred. One of the functions of the organic solvent is to improve the wettability of the treatment liquid composition to the fabric and to improve the moisture retention of the treatment liquid composition. In addition, the organic solvent may also be used as a penetrant.
[0067] Examples of organic solvents include esters, alkylene glycol ethers, cyclic esters, nitrogen-containing solvents, polyols, etc. Examples of nitrogen-containing solvents include cyclic amides, non-cyclic amides, etc. Examples of non-cyclic amides include alkoxyalkylamides, etc.
[0068] Examples of the esters include glycol monoacetates such as ethylene glycol monomethyl ether acetate, ethylene glycol monoethyl ether acetate, and ethylene glycol monobutyl ether acetate; and glycol diesters such as ethylene glycol diacetate, diethylene glycol diacetate, and propylene glycol diacetate.
[0069] The alkylene glycol ethers may be monoethers or diethers of alkylene glycol, and alkyl ethers are preferred. Specific examples include alkylene glycol monoalkyl ethers such as ethylene glycol monomethyl ether, ethylene glycol monoethyl ether, ethylene glycol monoisopropyl ether, ethylene glycol monobutyl ether, diethylene glycol monomethyl ether, and triethylene glycol monobutyl ether, and alkylene glycol dialkyl ethers such as ethylene glycol dimethyl ether, ethylene glycol diethyl ether, ethylene glycol dibutyl ether, diethylene glycol dimethyl ether, and diethylene glycol diethyl ether.
[0070] Examples of the cyclic esters include cyclic esters (lactones) such as β-propiolactone, γ-butyrolactone, δ-valerolactone, ε-caprolactone, and β-butyrolactone, and compounds in which the hydrogen atoms of the methylene groups adjacent to the carbonyl groups are substituted with alkyl groups having 1 to 4 carbon atoms.
[0071] Examples of alkoxyalkylamides include 3-methoxy-N,N-dimethylpropionamide, 3-methoxy-N,N-diethylpropionamide, 3-methoxy-N,N-methylethylpropionamide, 3-ethoxy-N,N-dimethylpropionamide, 3-ethoxy-N,N-diethylpropionamide, 3-ethoxy-N,N-methylethylpropionamide, 3-n-butoxy-N,N-dimethylpropionamide, 3-n-butoxy-N,N-diethylpropionamide, and 3-n-butoxy-N,N-methylethylpropionamide.
[0072] Examples of the cyclic amides include lactams, and examples thereof include pyrrolidones such as 2-pyrrolidone, 1-methyl-2-pyrrolidone, 1-ethyl-2-pyrrolidone, 1-propyl-2-pyrrolidone, and 1-butyl-2-pyrrolidone.
[0073] As the alkoxyalkylamides, compounds represented by the following general formula (1) are also preferably used.
[0074] R 1 -O-CH2CH2-(C=O)-NR 2 R 3 ··· (1)
[0075] In the above formula (1), R 1 represents an alkyl group having 1 to 4 carbon atoms, R 2 and R 3 Each independently represents a methyl group or an ethyl group. The "alkyl group having 1 or more and 4 or less carbon atoms" can be a linear or branched alkyl group, for example, a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, a sec-butyl group, an isobutyl group, or a tert-butyl group. The compound represented by the above formula (1) can be used alone or in combination of two or more.
[0076] Examples of the polyol include 1,2-alkanediols (e.g., ethylene glycol, propylene glycol (also known as propane-1,2-diol), 1,2-butanediol, 1,2-pentanediol, 1,2-hexanediol, 1,2-heptanediol, 1,2-octanediol and other alkanediols), polyols other than 1,2-alkanediol (polyols) (e.g., diethylene glycol, dipropylene glycol, 1,3-propanediol, 1,3-butanediol (also known as 1,3-butenediol), 1 , 4-butanediol, 1,5-pentanediol, 1,6-hexanediol, 2-ethyl-2-methyl-1,3-propanediol, 2-methyl-2-propyl-1,3-propanediol, 2-methyl-1,3-propanediol, 2, 2-dimethyl-1,3-propanediol, 3-methyl-1,3-butanediol, 2-ethyl-1,3-hexanediol, 3-methyl-1,5-pentanediol, 2-methylpentane-2,4-diol, trimethylolpropane, glycerol, etc.) and the like.
[0077] Examples of polyols include alkanediols and polyols. Alkanediols are diols of alkanes having 5 or more carbon atoms. The number of carbon atoms of the alkane is preferably 5 to 15, more preferably 6 to 10, and even more preferably 6 to 8. 1,2-alkanediol is preferred.
[0078] The polyols are polyols of alkanes having 4 or less carbon atoms or intermolecular condensates of hydroxyl groups of polyols of alkanes having 4 or less carbon atoms. The carbon number of the alkane is preferably 2 to 3. The number of hydroxyl groups in the molecule of the polyols is 2 or more, preferably 5 or less, and more preferably 3 or less. When the polyols are the above-mentioned intermolecular condensates, the number of intermolecular condensations is 2 or more, preferably 4 or less, and more preferably 3 or less. The polyols may be used alone or in combination of two or more.
[0079] Alkanediols and polyols can be used mainly as penetrating solvents and / or moisturizing solvents. However, alkanediols tend to have strong properties as penetrating solvents, and polyols tend to have strong properties as moisturizing solvents.
[0080] The ink composition may contain a surfactant. The surfactant has the function of adjusting the surface tension of the composition, for example, adjusting the wettability with fabrics, etc. Among the surfactants, for example, acetylene glycol-based surfactants, silicone-based surfactants, and fluorine-based surfactants can be preferably used.
[0081] The acetylene glycol surfactant is not particularly limited, and examples thereof include SURFYNOL 104, 104E, 104H, 104A, 104BC, 104DPM, 104PA, 104PG-50, 104S, 420, 440, 465, 485, SE, SE-F, 504, 61, DF37, CT111, CT121, CT131, CT136, TG, GA, DF110D (all trade names, manufactured by Air Products & Chemicals Co., Ltd.), OLFINE B, Y, P, A, STG, SPC, E1004, E1010, PD-001, PD-002W, PD-003, PD-004, EXP.4001, EXP.4036, EXP.4051, AF-103, AF-104, AK-02, SK-14, AE-3 (all of the above are trade names, manufactured by Nissin Chemical Industry Co., Ltd.), SURFYNOL E00, E00P, E40, E100 (all of the above are trade names, manufactured by Kawaken Fine Chemicals Co., Ltd.).
[0082] The silicone-based surfactant is not particularly limited, but preferably a polysiloxane-based compound is used. The polysiloxane-based compound is not particularly limited, but for example, a polyether-modified silicone is used. Examples of commercially available products of the polyether-modified organosiloxane include BYK-306, BYK-307, BYK-333, BYK-341, BYK-345, BYK-346, and BYK-348 (these are trade names, manufactured by BYK Chemical Japan Co., Ltd.), KF-351A, KF-352A, KF-353, KF-354L, KF-355A, KF-615A, KF-945, KF-640, KF-642, KF-643, KF-6020, X-22-4515, KF-6011, KF-6012, KF-6015, and KF-6017 (these are trade names, manufactured by Shin-Etsu Chemical Co., Ltd.), SILFACE SAG002, 005, 503A, 008 (these are trade names, manufactured by Nissin Chemical Industry Co., Ltd.) and the like.
[0083] As the fluorine-based surfactant, a fluorine-modified polymer is preferably used. Specific examples thereof include BYK-3440 (manufactured by BYK Chemical Japan Ltd.), SURFLON S-241, S-242, S-243 (these are trade names, manufactured by AGC Seimi Chemical Co., Ltd.), and FTERGENT 215M (manufactured by NEOS Co., Ltd.).
[0084] When the ink composition contains a surfactant, it may contain multiple types. When the ink composition contains a surfactant, the content of the surfactant may be 0.1% by mass or more and 2% by mass or less, preferably 0.3% by mass or more and 1.5% by mass or less, and more preferably 0.4% by mass or more and 1.0% by mass or less relative to the total mass of the ink composition.
[0085] (additive)
[0086] The ink composition may contain additives, such as pH adjusters, sugars, chelating agents, preservatives, antifungal agents, and rust inhibitors.
[0087] The pH adjuster is not particularly limited, and may be an appropriate combination of an acid, a base, a weak acid, and a weak base. Examples of the acid and base used in such a combination include sulfuric acid, hydrochloric acid, nitric acid, and the like as inorganic acids, lithium hydroxide, sodium hydroxide, potassium hydroxide, potassium dihydrogen phosphate, disodium hydrogen phosphate, potassium carbonate, sodium carbonate, sodium bicarbonate, ammonia, and the like as inorganic bases, triethanolamine, diethanolamine, monoethanolamine, tripropanolamine, triisopropanolamine, diisopropanolamine, trishydroxymethylaminomethane (THAM), and the like as organic acids, adipic acid, citric acid, succinic acid, lactic acid, N,N-bis(2-hydroxyethyl)-2-aminoethanesulfonic acid (BES), 4-(2-hydroxyethyl)-2-aminoethanesulfonic acid (BES), and the like. Good's buffers such as ethanolamine hydrochloride, N-tris(hydroxymethyl)methyl-2-aminoethanesulfonic acid (TES), acetylaminoglycine, tris(hydroxymethyl)methylglycine (tricine), glycineamide, and N,N-dihydroxyethylglycine (BICINE), phosphate buffer, citrate buffer, and tris buffer. Among them, when a tertiary amine such as triethanolamine and triisopropanolamine and a carboxyl group-containing organic acid such as adipic acid, citric acid, succinic acid, and lactic acid are contained as part or all of the pH adjuster, the pH buffering effect can be more stably obtained, which is preferred.
[0088] Specific examples of sugars include glucose, mannose, fructose, ribose, xylose, arabinose, galactose, aldonic acid, glucitol (sorbitol), maltose, cellobiose, lactose, sucrose, trehalose, and maltotriose.
[0089] Examples of the chelating agent include ethylenediaminetetraacetic acid and salts thereof (eg, disodium dihydrogen ethylenediaminetetraacetate, nitrilotriacetate, hexametaphosphate, pyrophosphate, or metaphosphate of ethylenediamine).
[0090] Examples of the preservative and antifungal agent include sodium benzoate, sodium pentachlorophenol, sodium 2-pyridinethiol-1-oxide, sodium sorbate, sodium dehydroacetate, PROXEL CRL, PROXEL BDN, PROXEL GXL, PROXEL XL-2, PROXEL IB, and PROXEL TN (all trade names, manufactured by Lonza Japan Co., Ltd.), and 4-chloro-3-methylphenol (Preventol CMK manufactured by Bayer Co., Ltd., etc.).
[0091] Examples of the rust inhibitor include benzotriazole, acidic sulfites, sodium thiosulfate, ammonium thioglycolate, diisopropylammonium nitrite, pentaerythritol tetranitrate, dicyclohexylamine nitrite, etc. Among them, benzotriazole is particularly preferred.
[0092] Examples of other additives include viscosity modifiers, antifungal agents, antioxidants, and oxygen absorbers.
[0093] 1.1.1.(3) Manufacturing and physical properties
[0094] In attaching the ink composition to fabric by an inkjet method, the viscosity of the ink composition at 20° C. is preferably 1.5 mPa·s to 15 mPa·s, more preferably 1.5 mPa·s to 7 mPa·s, and even more preferably 1.5 mPa·s to 5.5 mPa·s.
[0095] From the viewpoint of making the wetting and spreading property on the fabric suitable, the surface tension of the ink composition at 25° C. is preferably 40 mN / m or less, preferably 38 mN / m or less, more preferably 35 mN / m or less, and further preferably 30 mN / m or less. In addition, the surface tension is preferably 20 mN / m or more, and more preferably 25 mN / m or more.
[0096] The ink composition is obtained by mixing the aforementioned components in an arbitrary order and filtering or the like to remove impurities as needed. As a method for mixing the components, it is preferable to use a method of sequentially adding the materials to a container equipped with a stirring device such as a mechanical stirrer or a magnetic stirrer and stirring and mixing. As a filtering method, centrifugal filtration, filter filtration, etc. can be performed as needed.
[0097] The surface tension can be measured by confirming the surface tension when a platinum plate is wetted with the composition in an environment of 25° C. using an automatic surface tension meter CBVP-Z (manufactured by Kyowa Interface Science Co., Ltd.).
[0098] 1.1.2. Attachment scheme
[0099] The first ink adhesion step is performed by inkjet method. The adhesion amount of the ink composition in the ink adhesion step is preferably 15 g / m 2 Above and 80g / m 2 Below, more preferably 20g / m 2 Above and 40g / m 2 Below, more preferably 25g / m 2 Above and 30g / m 2 the following.
[0100] 1.2. Reaction solution adhesion process
[0101] In the reaction liquid attachment step, the reaction liquid composition is ejected by an inkjet method and attached to the fabric. The reaction liquid composition contains a coagulant for aggregating the components in the ink composition.
[0102] 1.2.1. Reaction solution composition
[0103] The reaction liquid composition contains a coagulant for aggregating the components in the ink composition.
[0104] 1.2.1.(1) Coagulants
[0105] The reaction liquid composition contains a coagulant for aggregating the components of the ink composition. The coagulant has the function of aggregating the pigment and the resin particles by reacting with the components such as the pigment contained in the ink composition and the resin particles that may be contained in the ink composition and the transparent ink composition. By such aggregating, for example, the color development of the pigment can be improved, the fixability of the resin particles can be improved, and / or the viscosity of the ink can be increased.
[0106] The coagulant is not particularly limited, and examples thereof include metal salts, inorganic acids, organic acids, cationic compounds, etc. As the cationic compound, cationic resins (cationic polymers), cationic surfactants, etc. can be used. Among them, as the metal salt, a polyvalent metal salt is preferred, and as the cationic compound, a cationic resin is preferred. Therefore, as the coagulant, in terms of particularly excellent image quality, scratch resistance, gloss, etc., it is preferably selected from cationic resins, organic acids, and polyvalent metal salts.
[0107] As the metal salt, a polyvalent metal salt is preferred, but metal salts other than polyvalent metal salts may also be used. Among these coagulants, at least one selected from metal salts and organic acids is preferably used from the perspective of excellent reactivity with the components contained in the ink. In addition, among cationic compounds, cationic resins are preferably used from the perspective of easy dissolution in the treatment liquid. In addition, multiple coagulants may be used in combination.
[0108] The polyvalent metal salt refers to a compound composed of a divalent or higher metal ion and an anion. Examples of divalent or higher metal ions include ions of calcium, magnesium, copper, nickel, zinc, barium, aluminum, titanium, strontium, chromium, cobalt, and iron. Among the metal ions constituting the polyvalent metal salt, at least one of calcium ion and magnesium ion is preferred from the perspective of excellent cohesion of the components of the ink.
[0109] As anions constituting the polyvalent metal salt, it is an inorganic ion or an organic ion. That is, the polyvalent metal salt in the present invention is composed of an inorganic ion or an organic ion and a polyvalent metal. As such inorganic ions, there can be mentioned: chloride ion, bromide ion, iodide ion, nitrate ion, sulfate ion, hydroxide ion, etc. As organic ions, there can be mentioned organic acid ions, for example, carboxylic acid ions.
[0110] It should be noted that the polyvalent metal compound is preferably an ionic polyvalent metal salt, and particularly, when the polyvalent metal salt is a magnesium salt or a calcium salt, the stability of the treatment solution becomes better. In addition, as the counter ion of the polyvalent metal, it can be any one of an inorganic acid ion or an organic acid ion.
[0111] As specific examples of the above-mentioned polyvalent metal salts, calcium carbonates such as heavy calcium carbonate and light calcium carbonate, calcium nitrate, calcium chloride, calcium sulfate, magnesium sulfate, calcium hydroxide, magnesium chloride, magnesium carbonate, barium sulfate, barium chloride, zinc carbonate, zinc sulfide, aluminum silicate, calcium silicate, magnesium silicate, copper nitrate, calcium formate, calcium acetate, magnesium acetate, aluminum acetate, etc. can be cited. These polyvalent metal salts can be used alone or in combination of two or more. Among them, in order to ensure sufficient solubility in water and reduce the residual traces of the treatment solution (the traces become less obvious), preferably at least any one of calcium formate, magnesium sulfate, calcium nitrate and calcium chloride, more preferably calcium formate and calcium nitrate. It should be noted that these metal salts can have hydration water in the form of raw materials.
[0112] Examples of the metal salt other than the polyvalent metal salt include monovalent metal salts such as sodium salts and potassium salts, and examples thereof include sodium sulfate and potassium sulfate.
[0113] As the organic acid, preferably, for example, poly(meth)acrylic acid, acetic acid, glycol acid, malonic acid, malic acid, maleic acid, ascorbic acid, succinic acid, glutaric acid, fumaric acid, citric acid, tartaric acid, lactic acid, sulfonic acid, orthophosphoric acid, pyrrolidonecarboxylic acid, pyrancarboxylic acid, pyrrolecarboxylic acid, furancarboxylic acid, pyridinecarboxylic acid, coumaric acid, thiophenecarboxylic acid, nicotinic acid or derivatives of these compounds or salts thereof can be mentioned. One organic acid can be used alone or two or more organic acids can be used in combination. Metal salts as salts of organic acids are also included in the above-mentioned metal salts.
[0114] Examples of the inorganic acid include sulfuric acid, hydrochloric acid, nitric acid, phosphoric acid, etc. The inorganic acid may be used alone or in combination of two or more.
[0115] Examples of the cationic resin (cationic polymer) include cationic acrylic resins, cationic polyurethane resins, cationic olefin resins, cationic amine resins, cationic surfactants, etc. The cationic polymer is preferably water-soluble.
[0116] As the cationic acrylic resin, commercially available products can be used, for example, SUPERFLEX (registered trademark) 620 and 650 from Dai-ichi Kogyo Seiyaku Co., Ltd., PARASURF UP-22 from OHARA PARAGIUM CHEMICAL Co., Ltd., PERMARIN (registered trademark) UC-20 from Sanyo Chemical Industries, Ltd., Arrow Base (registered trademark) CB-1200 and CD-1200 from Unitika Co., Ltd., VINYBLAN (registered trademark) 2687 from Nissin Chemical Industry Co., Ltd., and Mowinyl 7820 from Japan Coating Resin Co., Ltd.
[0117] As the cationic polyurethane resin, commercially available products can be used, for example, HYDRAN CP-7010, CP-7020, CP-7030, CP-7040, CP-7050, CP-7060, CP-7610 (trade names, manufactured by DIC Corporation), SUPERFLEX 600, 610, 620, 630, 640, 650 (trade names, manufactured by Dai-ichi Kogyo Seiyaku Co., Ltd.), polyurethane emulsions WBR-2120C and WBR-2122C (trade names, manufactured by Taisei Fine Chemicals Co., Ltd.), etc. can be used.
[0118] Cationic olefin resin has olefins such as ethylene and propylene on the structural skeleton, and known materials can be appropriately selected. In addition, cationic olefin resin can be an emulsion state formed by being dispersed in a solvent including water and an organic solvent. As cationic olefin resin, commercially available products can be used, for example: Arrow Base CB-1200, CD-1200 (trade name, Unitika Co., Ltd. system) etc. can be cited.
[0119] As cationic amine resins (cationic polymers), any known material can be appropriately selected as long as it is a resin having an amino group in its structure. Examples thereof include polyamine resins, polyamide resins, and polyallylamine resins. Polyamine resins are resins having an amino group in the main skeleton of the resin. Polyamide resins are resins having an amide group in the main skeleton of the resin. Polyallylamine resins are resins having a structure derived from an allyl group in the main skeleton of the resin.
[0120] In addition, examples of cationic polyamine resins include: UNISENSE KHE103L manufactured by Senka Co., Ltd. (hexamethylenediamine / epichlorohydrin resin, a 1% aqueous solution has a pH of about 5.0, a viscosity of 20 to 50 (mPa·s), and an aqueous solution with a solid content concentration of 50% by mass), UNISENSE KHE104L (dimethylamine / epichlorohydrin resin, a 1% aqueous solution has a pH of about 7.0, a viscosity of 1 to 10 (mPa·s), and an aqueous solution with a solid content concentration of 20% by mass), etc. Specific examples of commercially available cationic polyamine resins include FL-14 (manufactured by SNF), ARAFIX 100, 251S, 255, 255LOX (manufactured by Arakawa Chemical Co., Ltd.), DK-6810, 6853, 6885; WS-4010, 4011, 4020, 4024, 4027, 4030 (manufactured by Starlight PMC Co., Ltd.), PAPIOGEN P-105 (manufactured by Senka Co., Ltd.), Sumirez Resin 650 (30), 675A, 6615, SLX-1 (manufactured by TAOKA CHEMICAL INDUSTRY CO., LTD.), Catiomaster (registered trademark) PD-1, 7, 30, A, PDT-2, PE-10, PE-30, DT-EH, EPA-SK01, TMHMDA-E (manufactured by Yokkaichi Synthetic Co., Ltd.), JETFIX 36N, 38A, 5052 (manufactured by Satoda Chemical Co., Ltd.).
[0121] As the polyamine resin, polyallylamine resin can also be mentioned. As the polyallylamine resin, for example, polyallylamine hydrochloride, polyallylamine amide sulfate, allylamine hydrochloride-diallylamine hydrochloride copolymer, allylamine acetate-diallylamine acetate copolymer, allylamine acetate-diallylamine acetate copolymer, allylamine hydrochloride-dimethylallylamine hydrochloride copolymer, allylamine-dimethylallylamine copolymer, polydiallylamine hydrochloride, polymethyldiallylamine hydrochloride, polymethyldiallylamine amide sulfate, polymethyldiallylamine acetate, polydiallyldimethylammonium chloride, diallylamine acetate-sulfur dioxide copolymer, diallylmethylethylethylammonium sulfate-sulfur dioxide copolymer, methyldiallylamine hydrochloride-sulfur dioxide copolymer, diallyldimethylammonium chloride-sulfur dioxide copolymer, diallyldimethylammonium chloride-acrylamide copolymer, etc. can be mentioned.
[0122] Examples of the cationic surfactant include primary, secondary and tertiary amine salt compounds, alkylamine salts, dialkylamine salts, aliphatic amine salts, benzalkonium salts, quaternary ammonium salts, quaternary alkylammonium salts, alkylpyridinium salts, sulfonium salts, phosphonium salts, onium salts and imidazolinium salts.
[0123] These coagulants can use multiple. In addition, in these coagulants, if at least one of polyvalent metal salt, organic acid, cationic resin is selected, the coagulation of at least the above-mentioned self-dispersible pigment is better, therefore, it is possible to form an image with higher (particularly good color development) quality.
[0124] The total content of the coagulant in the reaction liquid composition is not limited, and is, for example, 0.1 mass % to 15 mass % relative to the total mass of the reaction liquid composition, preferably 1 mass % to 10 mass % and more preferably 2 mass % to 10 mass % .
[0125] 1.2.1.(2) Other ingredients
[0126] The reaction liquid composition may include water, humectants, polyols, other solvents, surfactants, and additives, wherein the water, humectants, other solvents, surfactants, and additives are the same as those of the ink composition, and thus will not be described in detail.
[0127] The reaction liquid composition preferably contains a polyol among the above-mentioned other solvents. In addition, when the reaction liquid composition contains a polyol, the content of the polyol in the reaction liquid composition is preferably 70% by mass or more, more preferably 80% by mass or more, and further preferably 85% by mass or more relative to the total amount of the organic solvent in the reaction liquid composition. In this way, the permeability of the polyol is small, so the reaction liquid composition is more likely to stay near the surface of the fabric, which can make the color development of the image better.
[0128] It should be noted that the content of the colorant in the reaction liquid composition is preferably 0.1% by mass or less relative to the total amount of the reaction liquid composition. That is, the reaction liquid composition is preferably not intended for coloring.
[0129] 1.2.1.(3) Manufacturing and physical properties
[0130] In attaching the reaction liquid composition to the fabric by inkjet method, the viscosity of the reaction liquid composition at 20°C is preferably greater than 1.5 mPa·s and less than 15 mPa·s, more preferably greater than 1.5 mPa·s and less than 7 mPa·s, and more preferably greater than 1.5 mPa·s and less than 5.5 mPa·s.
[0131] From the viewpoint of making the wettability and diffusibility on the fabric appropriate, the surface tension of the reaction liquid composition at 25°C is preferably 40 mN / m or less, preferably 38 mN / m or less, more preferably 35 mN / m or less, and further preferably 30 mN / m or less. In addition, the surface tension is preferably 25 mN / m or more, more preferably 28 mN / m or more. When the surface tension of the reaction liquid composition is high, it is less likely to scatter when sprayed from the nozzle, and it is less likely to generate mist when sprayed, which can make the spraying stability better.
[0132] The reaction liquid composition is obtained by mixing the aforementioned components in an arbitrary order and filtering as needed to remove impurities. As a mixing method for each component, it is preferred to use a method in which materials are sequentially added to a container equipped with a stirring device such as a mechanical stirrer or a magnetic stirrer and stirred and mixed. As a filtering method, centrifugal filtration, filter filtration, etc. can be performed as needed.
[0133] 1.2.2. Attachment scheme
[0134] The reaction solution adhesion step is performed by inkjet method. The adhesion amount of the ink composition in the reaction solution adhesion step is preferably 15 g / m 2 Above and 80g / m 2 Below, more preferably 30g / m 2 Above 60g / m 2 Below, more preferably 30g / m 2 Above and 50g / m 2 the following.
[0135] 1.3. Second ink adhesion process
[0136] In the second ink adhesion step, an ink composition containing a self-dispersible pigment is ejected by an inkjet method and adhered to the fabric.
[0137] 1.3.1. Ink composition
[0138] The ink composition attached to the fabric in the second ink attachment step has the same components and physical properties as the ink composition attached in the first ink attachment step, and therefore, they are not described in detail. The ink composition attached to the fabric in the second ink attachment step may be the same as or different from the ink composition attached in the first ink attachment step.
[0139] 1.3.2. Attachment scheme
[0140] The second ink adhesion step is performed by inkjet method. The adhesion amount of the ink composition in the second ink adhesion step is preferably 15 g / m 2 Above and 80g / m 2 Below, more preferably 20g / m 2 Above and 40g / m 2 Below, more preferably 25g / m 2 Above and 30g / m 2 the following.
[0141] 1.4. Other processes
[0142] 1.4.1. Resin dispersion pigment ink adhesion process
[0143] The inkjet recording method of the present embodiment may include a resin-dispersed pigment ink adhering step. In the resin-dispersed pigment ink adhering step, a resin-dispersed pigment ink composition containing a resin-dispersed pigment is ejected by an inkjet method and is adhered to a fabric.
[0144] 1.4.1.(1) Resin-dispersed pigment ink composition
[0145] The resin-dispersed pigment ink composition contains a resin-dispersed pigment.
[0146] 1.4.1.(1-1) Resin-dispersed pigments
[0147] Resin-dispersed pigments are pigments that are dispersed using a dispersant instead of being self-dispersed as described in the above "1.1.1. Ink composition". Examples of the dispersant include resin dispersants, which are selected from substances that can provide good dispersion stability of the pigment in the resin-dispersed pigment ink composition.
[0148] Examples of the resin dispersant (dispersant resin) include (meth)acrylic acid resins and salts thereof such as poly(meth)acrylic acid, (meth)acrylic acid-acrylonitrile copolymers, (meth)acrylic acid-(meth)acrylic ester copolymers, vinyl acetate-(meth)acrylic ester copolymers, vinyl acetate-(meth)acrylic acid copolymers, and vinylnaphthalene-(meth)acrylic acid copolymers; styrene-(meth)acrylic acid copolymers, styrene-(meth)acrylic acid-(meth)acrylic ester copolymers, styrene-α-methylstyrene-(meth)acrylic acid copolymers, Styrene resins and their salts such as styrene-α-methylstyrene-(meth)acrylic acid-(meth)acrylate copolymers, styrene-maleic acid copolymers, and styrene-maleic anhydride copolymers; polyurethane resins and their salts with or without cross-linked structures, which are polymer compounds (resins) containing urethane bonds formed by the reaction of isocyanate groups and hydroxyl groups, and can be linear and / or branched; polyvinyl alcohols; vinylnaphthalene-maleic acid copolymers and their salts; vinyl acetate-maleic acid ester copolymers and their salts; and water-soluble resins such as vinyl acetate-crotonic acid copolymers and their salts. Among them, copolymers of monomers having hydrophobic functional groups and monomers having hydrophilic functional groups, and polymers composed of monomers having both hydrophobic functional groups and hydrophilic functional groups are preferred. As a form of copolymer, it can be used in any form of random copolymers, block copolymers, alternating copolymers, and graft copolymers.
[0149] Commercially available products of styrene-based resin dispersants include, for example, X-200, X-1, X-205, X-220, and X-228 (manufactured by Seikyo PMC Co., Ltd.), NOPCOSPERSE (registered trademark) 6100 and 6110 (manufactured by SAN NOPCO Co., Ltd.), JONCRYL 67, 586, 611, 678, 680, 682, and 819 (manufactured by BASF), DISPERBYK-190 (manufactured by BYK Chemical Japan Ltd.), N-EA137, N-EA157, N-EA167, N-EA177, N-EA197D, N-EA207D, and E-EN10 (manufactured by Dai-ichi Kogyo Seiyaku).
[0150] Examples of commercially available acrylic resin dispersants include BYK-187, BYK-190, BYK-191, BYK-194N, and BYK-199 (manufactured by BYK Corporation), ARON A-210, A6114, AS-1100, AS-1800, A-30SL, A-7250, and CL-2 (manufactured by Toagosei Co., Ltd.).
[0151] Examples of commercially available polyurethane resin dispersants include BYK-182, BYK-183, BYK-184, and BYK-185 (manufactured by BYK Corporation), TEGO Disperse 710 (manufactured by Evonic Tego Chemi Co., Ltd.), and Borchi (registered trademark) Gen 1350 (manufactured by OMG Borschers Co., Ltd.).
[0152] Dispersants can be used alone or in combination of two or more. The total content of the dispersants is preferably 0.1 mass parts or more and 30 mass parts or less relative to 50 mass parts of the pigment, more preferably 0.5 mass parts or more and 25 mass parts or less, further more preferably 1 mass parts or more and 20 mass parts or less, and further preferably 1.5 mass parts or more and 15 mass parts or less. By making the content of the dispersant 0.1 mass parts or more relative to 50 mass parts of the pigment, the dispersion stability of the pigment can be further improved. In addition, if the content of the dispersant is less than 30 mass parts relative to 50 mass parts of the pigment, the viscosity of the obtained dispersion can be controlled to be smaller.
[0153] Among the dispersants exemplified above, at least one selected from anionic dispersant resins is more preferred. In addition, in this case, the weight average molecular weight of the dispersant is more preferably 500 or more. Furthermore, it is preferably 5000 or more and 100000 or less, and more preferably 10000 or more and 50000 or less.
[0154] By using such a resin dispersant as a dispersant, the dispersion and aggregation of the pigment can be further improved, and better dispersion stability and a better quality image can be obtained.
[0155] The anionic dispersant resin is a resin having anionic functional groups, thereby exhibiting anionic properties. Examples of the anionic functional groups include carboxyl groups, sulfonyl groups, and phosphoric acid groups. Among these groups, carboxyl groups are more preferred.
[0156] The dispersant resin preferably has an acid value, and the acid value is preferably 5 mgKOH / g or more, more preferably 10 to 200 mgKOH / g, further preferably 15 to 150 mgKOH / g, and preferably 20 to 100 mgKOH / g, further preferably 25 to 70 mgKOH / g.
[0157] The acid value can be measured by neutralization potentiometric titration in accordance with JIS K 0070. As a titration apparatus, for example, "AT610" manufactured by Kyoto Electronics Industries, Ltd. can be used.
[0158] The resin dispersion pigment ink composition is preferably a cyan ink. When the ink composition is a black ink containing a self-dispersible black pigment, the resin dispersion pigment ink composition is a cyan ink to form a mixed black image, thereby improving the color development of black.
[0159] 1.4.1.(1-2) Other ingredients
[0160] The resin-dispersed pigment ink composition may contain other components. Other components are the same as those described in "1.1.1. (2) Other components" and are not described in detail.
[0161] 1.4.1.(1-3) Manufacturing and physical properties
[0162] In terms of attaching the resin-dispersed pigment ink composition to fabric by inkjet method, the viscosity of the resin-dispersed pigment ink composition at 20°C is preferably greater than 1.5 mPa·s and less than 15 mPa·s, more preferably greater than 1.5 mPa·s and less than 7 mPa·s, and more preferably greater than 1.5 mPa·s and less than 5.5 mPa·s.
[0163] From the viewpoint of making the wettability and diffusibility on the fabric appropriate, the surface tension of the resin-dispersed pigment ink composition at 25°C is preferably 40 mN / m or less, preferably 38 mN / m or less, more preferably 35 mN / m or less, and further preferably 30 mN / m or less. In addition, the surface tension is preferably 25 mN / m or more, more preferably 28 mN / m or more. When the surface tension of the resin-dispersed pigment ink composition is high, it is less likely to scatter when ejected from the nozzle, and it is less likely to generate mist when ejected, which can make the ejection stability better.
[0164] The resin-dispersed pigment ink composition is obtained by mixing the aforementioned components in an arbitrary order and filtering or the like as needed to remove impurities. As a method for mixing the components, it is preferred to use a method of sequentially adding the materials to a container equipped with a stirring device such as a mechanical stirrer or a magnetic stirrer and stirring and mixing. As a filtering method, centrifugal filtration, filter filtration, etc. can be performed as needed.
[0165] 1.4.1.(2) Attachment scheme
[0166] The resin dispersion pigment ink adhesion step is performed by an inkjet method. The adhesion amount of the ink composition in the resin dispersion pigment ink adhesion step is preferably 15 g / m 2 Above and 80g / m 2 Below, more preferably 20g / m 2 Above and 40g / m 2 Below, more preferably 25g / m 2 Above and 30g / m 2 the following.
[0167] 1.4.2. Transparent ink adhesion process
[0168] The inkjet recording method of the present embodiment may include a clear ink attaching step. In the clear ink attaching step, a clear ink composition containing resin particles is ejected by an inkjet method and attached to a cloth.
[0169] 1.4.2.(1) Transparent ink composition
[0170] The clear ink composition contains resin particles (resin dispersion).
[0171] 1.4.2.(1-1) Resin particles
[0172] The resin particles are the same as the anionic resin particles that can be contained in the ink composition, so they are not described in detail. When the inkjet recording method includes a transparent ink attachment step, when the reaction liquid composition and the transparent ink composition come into contact, the resin particles contained in the transparent ink composition are easily aggregated and are not easily deposited inside the fabric, so that the color development of the obtained image becomes better.
[0173] 1.4.2.(1-2) Other ingredients
[0174] The clear ink composition may contain other components. The other components are the same as those described in "1.1.1. (2) Other components" and are not described in detail.
[0175] In addition, in the clear ink composition, the content of the colorant is preferably 0.1% by mass or less relative to the total amount of the clear ink composition. That is, the clear ink composition is preferably not specifically used for coloring.
[0176] 1.4.2.(1-3) Manufacturing and physical properties
[0177] In attaching the transparent ink composition to the fabric by inkjet method, the viscosity of the transparent ink composition at 20°C is preferably 1.5 mPa·s to 15 mPa·s, more preferably 1.5 mPa·s to 7 mPa·s, and more preferably 1.5 mPa·s to 5.5 mPa·s.
[0178] From the viewpoint of making the wetting and spreading property on the fabric appropriate, the surface tension of the transparent ink composition at 25°C is preferably 40 mN / m or less, preferably 38 mN / m or less, more preferably 35 mN / m or less, and further preferably 30 mN / m or less. In addition, the surface tension is preferably 25 mN / m or more, more preferably 28 mN / m or more. When the surface tension of the transparent ink composition is high, it is less likely to scatter when ejected from the nozzle, and it is less likely to generate mist when ejected, which can make the ejection stability better.
[0179] The transparent ink composition is obtained by mixing the aforementioned components in an arbitrary order and filtering or the like to remove impurities as required. As a method for mixing the components, it is preferable to use a method of sequentially adding the materials to a container equipped with a stirring device such as a mechanical stirrer or a magnetic stirrer and stirring and mixing. As a filtering method, centrifugal filtration, filter filtration, etc. can be performed as required.
[0180] 1.4.2.(2) Attachment scheme
[0181] The clear ink attaching step is performed by inkjet method. The amount of the clear ink composition attached in the clear ink attaching step is preferably 15 g / m 2 Above and 80g / m 2 Below, more preferably 20g / m 2 Above and 40g / m 2 Below, more preferably 25g / m 2 Above and 30g / m 2 the following.
[0182] 1.4.3. Other processes
[0183] (Drying process)
[0184] The recording method involved in this embodiment may include a drying process between or before and after each of the above-mentioned processes. As the drying process, it can be performed by a device that uses a drying mechanism to dry the cloth. As the device that uses a drying mechanism to dry the cloth, there can be cited: a device that blows air at room temperature and warm air to the cloth (blowing type), a device that irradiates the cloth with radiation that generates heat (infrared rays, etc.) (radiation type), a component that contacts the cloth to transfer heat to the cloth (conduction type), and a combination of two or more of these devices. In the case of having a drying process, it is preferably performed by a drying mechanism that heats the cloth. In particular, the case where a drying mechanism that heats the cloth is used as the drying mechanism is called a heating process.
[0185] The surface temperature of the fabric when attaching each composition is preferably 45°C or less, more preferably 20°C or more and 45°C or less. In addition, it is preferably 27.0°C or more and 40°C or less, more preferably 28°C or more and 30°C or less. This temperature is the surface temperature of the portion on the recording surface of the fabric that receives the liquid during the attachment process, and is the highest temperature during the attachment process in the recording area. When the surface temperature is within the above range, it is more preferred in terms of image quality, scratch resistance, and reduced clogging.
[0186] The method for heating the fabric is not particularly limited, and examples thereof include hot pressing, normal pressure steam method, high pressure steam method, thermosetting method, etc. The heat source for heating is not particularly limited, and for example, an infrared lamp can be used. The heating temperature is preferably a temperature at which the resin particles in the ink fuse and the medium such as water evaporates. For example, it is preferably above 100°C and below 200°C, more preferably below 170°C, and further preferably below 160°C. Among them, the heating temperature in the heating process refers to the surface temperature of the image formed on the fabric. The time for applying heating is not particularly limited, and for example, it is above 30 seconds and below 20 minutes.
[0187] In addition, it is also preferable not to have a drying step, because this allows an image with good color development to be obtained in a shorter time.
[0188] 1.5. Sequence and interval of each process
[0189] In the inkjet recording method according to the present embodiment, the first ink attaching step, the reaction liquid attaching step, and the second ink attaching step are performed continuously in sequence. The continuous performance means that after the ink composition is attached to a predetermined area of the fabric, the reaction liquid composition is directly attached without attaching a composition other than the reaction liquid composition, and then the ink composition is directly attached without attaching a composition other than the ink composition.
[0190] In addition, in the inkjet recording method involved in this embodiment, the time difference from the time when the ink composition is attached by the first ink attachment step to the time when the reaction liquid composition is attached to the area to which the ink composition is attached by the reaction liquid attachment step is within 45 milliseconds, and the time difference from the time when the reaction liquid composition is attached by the reaction liquid attachment step to the time when the ink composition is attached to the area to which the reaction liquid composition is attached by the second ink attachment step is within 45 milliseconds.
[0191] More strictly speaking, the time from the time point when the attachment of the ink composition through the first ink attachment step is completed to the time point when the reaction liquid composition starts to attach to the area through the reaction liquid attachment step is within 45 milliseconds, and the time from the time point when the attachment of the reaction liquid composition through the reaction liquid attachment step is completed to the time point when the ink composition starts to attach to the area through the second ink attachment step is within 45 milliseconds.
[0192] Thus, the ink composition is continuously attached in a very short time before and after the reaction liquid is attached to the fabric. Thus, even on the fabric as an absorbent recording medium, the ink composition and the reaction liquid are easily mixed, and the coagulation reaction of the ink composition is easily carried out. Thus, the pigment in the ink is easy to stay near the surface of the fabric, which can make the color development good. In addition, since the self-dispersible pigment has a higher reactivity with the coagulant, it is easier to stay near the surface, which can make the color development good.
[0193] Furthermore, when the inkjet recording method includes the resin dispersion pigment ink attaching step, the resin dispersion pigment ink attaching step can be performed at least one of before the first ink attaching step and after the second ink attaching step.
[0194] In addition, when the resin-dispersed pigment ink attachment process is performed before the first ink attachment process, the time difference between the resin-dispersed pigment ink composition being attached to the area to which the ink composition is attached by the first ink attachment process through the resin-dispersed pigment ink attachment process is preferably 3.5 milliseconds or more, more preferably 7 milliseconds or more, and even more preferably 7.3 milliseconds or more.
[0195] On the other hand, when the resin-dispersed pigment ink attachment process is performed after the second ink attachment process, the time difference from the attachment of the ink composition by the second ink attachment process to the attachment of the resin-dispersed pigment ink composition to the area to which the ink composition is attached by the resin-dispersed pigment ink attachment process is preferably 3.5 milliseconds or more, more preferably 7 milliseconds or more, and even more preferably 7.3 milliseconds or more.
[0196] In this way, the time interval between the adhesion of the resin-dispersed pigment ink and the adhesion of the ink composition is relatively large, so that the resin-dispersed pigment ink droplets after dripping are easy to wet and spread, the filling property of the image is improved, and the color development property becomes better.
[0197] Furthermore, when the inkjet recording method includes a resin-dispersed pigment ink attachment process, and the resin-dispersed pigment ink attachment process is performed before the first ink attachment process, the time difference from the attachment of the resin-dispersed pigment ink composition through the resin-dispersed pigment ink attachment process to the attachment of the ink composition to the area to which the resin-dispersed pigment ink composition is attached through the first ink attachment process is preferably 55 milliseconds or less, more preferably 45 milliseconds or less, and even more preferably 43 milliseconds or less.
[0198] On the other hand, when the inkjet recording method includes a resin-dispersed pigment ink adhesion step, and the resin-dispersed pigment ink adhesion step is performed after the second ink adhesion step, the time difference from the adhesion of the ink composition by the second ink adhesion step to the adhesion of the resin-dispersed pigment ink composition to the area to which the ink composition is adhered by the resin-dispersed pigment ink adhesion step is preferably 55 milliseconds or less, more preferably 45 milliseconds or less, and even more preferably 43 milliseconds or less.
[0199] In this way, the time interval between the adhesion of the resin-dispersed pigment ink and the adhesion of the ink composition will not be too long. Therefore, the distance between the nozzle that ejects the resin-dispersed pigment ink composition and the nozzle that ejects the reaction liquid composition can be longer, thereby suppressing coagulation near the nozzle and making the ejection stability better.
[0200] Furthermore, in the case where the inkjet recording method includes a transparent ink adhesion process, preferably, the resin-dispersed pigment ink adhesion process is performed after the second ink adhesion process, and the resin-dispersed pigment ink composition is adhered by the resin-dispersed pigment ink adhesion process, and the transparent ink composition is adhered to the area to which the resin-dispersed pigment ink composition is adhered by the transparent ink adhesion process.
[0201] In this way, the image formed by the ink composition and the resin-dispersed pigment ink composition is coated with the transparent ink composition, thereby improving the fastness of the image. In addition, the reduction in friction fastness caused by the colorant staying near the surface of the cloth to improve the color development can be reduced.
[0202] 2. An example of a recording device
[0203] refer to Figure 1 , an example of an inkjet printing device (recording device) including an inkjet head that can be applied to the recording method involved in this embodiment is described.
[0204] It should be noted that in Figure 1 In order to make each layer and each component have a size that can be recognized, the size of each layer and each component is different from the actual size. Figure 1 In the figure, for convenience of explanation, the X-axis, Y-axis, and Z-axis are shown as three axes orthogonal to each other, and the tip side of the arrow indicating the axis direction in the figure is referred to as the "+ side", and the base side is referred to as the "- side". The direction parallel to the X-axis is referred to as the "X-axis direction", the direction parallel to the Y-axis is referred to as the "Y-axis direction", and the direction parallel to the Z-axis is referred to as the "Z-axis direction".
[0205] 2.1. Overall schematic composition
[0206] Figure 1 1 is a schematic diagram showing a schematic overall configuration of the recording device 100. Figure 1 , the overall structure of the recording device 100 is described.
[0207] like Figure 1 As shown, the recording device 100 includes a medium conveying unit 20, a medium sealing unit 60, a belt supporting unit 91, a printing unit 40, a heating unit 27, a cleaning unit 50, etc. In the recording device 100, at least one of the medium sealing unit 60 and the belt supporting unit 91 corresponds to a heating unit for heating the endless belt 23. In addition, the recording device 100 also includes a control unit 1 for controlling the above-mentioned parts. The parts of the recording device 100 are installed in the body 90.
[0208] It should be noted that, when a heating unit for heating the endless belt is provided, it only needs to be located at the upstream side of the conveying direction relative to the printing unit 40, and can be provided at a position different from the medium sealing unit 60 and the belt supporting unit 91. For example, the heating unit can be located at the upstream side of the conveying direction relative to the medium sealing unit 60. By adopting such a configuration, the heating unit can also dry the endless belt 23 that is wetted during cleaning. In addition, the heating unit can be a heating unit for non-contact heating of the endless belt.
[0209] The medium conveying unit 20 conveys the cloth 95 in the conveying direction and includes a medium supply unit 10 , conveying rollers 21 , 22 , an endless belt 23 , a belt rotating roller 24 , a belt driving roller 25 as a driving roller, conveying rollers 26 , 28 , and a medium collecting unit 30 .
[0210] 2.2. Medium conveying unit
[0211] First, the conveying path of the cloth 95 from the medium supply unit 10 to the medium recovery unit 30 will be described. Figure 1In the figure, the direction along the direction of gravity is referred to as the Z-axis direction, the direction in which the cloth 95 is conveyed in the printing unit 40 is referred to as the +X-axis direction, and the width direction of the cloth 95 intersecting both the Z-axis direction and the X-axis direction is referred to as the Y-axis direction. In addition, the positional relationship along the conveying direction of the cloth 95 or the moving direction of the endless belt 23 is also referred to as the "upstream side" and the "downstream side".
[0212] The medium supply unit 10 supplies the cloth 95 for forming an image to the printing unit 40 side. The medium supply unit 10 includes a supply shaft 11 and a bearing 12. The supply shaft 11 is formed in a cylindrical or columnar shape and is rotatably arranged in the circumferential direction. The supply shaft 11 is rolled with a strip of cloth 95. The supply shaft 11 is detachably mounted on the bearing 12. Thus, the cloth 95 pre-wound on the supply shaft 11 can be mounted on the bearing 12 together with the supply shaft 11.
[0213] The bearing portion 12 supports both ends of the supply shaft portion 11 in the axial direction so that the two ends can rotate. The medium supply portion 10 has a rotation drive portion (not shown) that drives the supply shaft portion 11 to rotate. The rotation drive portion rotates the supply shaft portion 11 in the direction in which the cloth 95 is fed. The operation of the rotation drive portion is controlled by the control portion 1. The conveying rollers 21 and 22 relay the cloth 95 between the medium supply portion 10 and the endless belt 23.
[0214] The endless belt 23 is held between at least two rollers that rotate the endless belt 23. The endless belt 23 supports the cloth 95 and transports it along the conveying direction (+X axis direction) by rotating. In detail, the endless belt 23 is a seamless belt formed by seamlessly connecting the two ends of a belt-shaped belt, and is hung between two rollers of a belt rotating roller 24 and a belt driving roller 25.
[0215] The endless belt 23 is held under a predetermined tension so that the portion between the belt rotating roller 24 and the belt driving roller 25 is horizontal. An adhesive 29 for bonding the fabric 95 is applied to the surface (supporting surface) 23a of the endless belt 23. That is, the endless belt 23 has an adhesive layer composed of the adhesive 29. The fabric 95 is bonded to the endless belt 23 via the adhesive 29. The endless belt 23 is supplied by the conveying roller 22 and supports (holds) the fabric 95 bonded to the adhesive 29 in the medium bonding section 60 described later.
[0216] The adhesive 29 preferably has an adhesive property that increases by heating. By using an adhesive 29 whose adhesive property increases by heating, the fabric 95 and the adhesive layer can be well adhered to each other. As such an adhesive 29, for example, a hot melt adhesive having a thermoplastic elastomer SIS (styrene-isoprene-styrene) as a main component can be cited.
[0217] The belt rotating roller 24 and the belt driving roller 25 support the inner circumferential surface 23b of the endless belt 23. An abutment portion 69, a belt supporting portion 91, and a pressing plate 46 for supporting the endless belt 23 are provided between the belt rotating roller 24 and the belt driving roller 25. The abutment portion 69 is provided in a region opposite to a pressing portion 61 described later across the endless belt 23, the pressing plate 46 is provided in a region opposite to the printing portion 40 across the endless belt 23, and the belt supporting portion 91 is provided between the abutment portion 69 and the pressing plate 46. By supporting the endless belt 23 by the abutment portion 69, the belt supporting portion 91, and the pressing plate 46, vibration of the endless belt 23 as the endless belt 23 moves can be suppressed.
[0218] The belt drive roller 25 is a driving unit that transports the cloth 95 in the transport direction by rotating the endless belt 23, and has a motor (not shown) that drives the belt drive roller 25 to rotate. The belt drive roller 25 is provided at a position closer to the downstream side than the printing unit 40 in the transport direction of the cloth 95, and the belt rotation roller 24 is provided at a position closer to the upstream side than the printing unit 40. When the belt drive roller 25 is driven to rotate, the endless belt 23 rotates with the rotation of the belt drive roller 25, and the rotation of the endless belt 23 drives the belt rotation roller 24 to rotate. The rotation of the endless belt 23 transports the cloth 95 supported on the endless belt 23 in the transport direction (+X axis direction), and forms an image on the cloth 95 through the printing unit 40 described later.
[0219] exist Figure 1 In the example shown, the cloth 95 is supported on the side (+Z axis side) of the surface 23a of the endless belt 23 opposite to the printing section 40, and the cloth 95 is conveyed together with the endless belt 23 from the belt rotating roller 24 side to the belt driving roller 25 side. In addition, on the side (-Z axis side) of the surface 23a of the endless belt 23 opposite to the cleaning unit 50, only the endless belt 23 moves from the belt driving roller 25 side to the belt rotating roller 24 side.
[0220] The transport roller 26 peels off the cloth 95 on which the image is formed and the adhesive 29 of the endless belt 23 . The transport rollers 26 and 28 relay the cloth 95 between the endless belt 23 and the medium recovery unit 30 .
[0221] The medium recovery unit 30 recovers the cloth 95 conveyed by the medium conveying unit 20. The medium recovery unit 30 includes a winding shaft unit 31 and a bearing unit 32. The winding shaft unit 31 is formed in a cylindrical or columnar shape and is rotatably arranged in the circumferential direction. The cloth 95 in a strip shape is wound around the winding shaft unit 31 in a roll shape. The winding shaft unit 31 is detachably mounted on the bearing unit 32. Thus, the cloth 95 wound around the winding shaft unit 31 can be removed together with the winding shaft unit 31.
[0222] The bearing portion 32 supports both ends of the winding shaft portion 31 in the axial direction so that both ends can rotate. The medium recovery portion 30 has a rotation drive portion (not shown) that drives the winding shaft portion 31 to rotate. The rotation drive portion rotates the winding shaft portion 31 in the direction in which the fabric 95 is wound. The operation of the rotation drive portion is controlled by the control unit 1.
[0223] Next, the heating section, the printing section 40 , the heating unit 27 , and the cleaning unit 50 provided along the medium conveying section 20 will be described.
[0224] 2.3. Heating unit
[0225] It is preferable that at least one of the contact portion 69 and the belt support portion 91 is provided with a heater for heating the endless belt 23. The heater constitutes the heating portion. When the heater is provided on the contact portion 69, it is possible to apply pressing force and heat to the endless belt 23 by the pressing portion 61, and therefore, it is preferable in that the closeness of the fabric 95 to the endless belt 23 can be improved. Therefore, when a heater is provided on one of the contact portion 69 and the belt support portion 91, it is more preferable to provide it on the contact portion 69.
[0226] The heating unit heats the adhesive layer to soften it and exert its adhesiveness, thereby improving the adhesion between the cloth 95 and the adhesive layer. Thus, the cloth 95 is prevented from moving on the endless belt 23, and good conveying accuracy can be obtained.
[0227] A heater is provided on at least one of the contact portion 69 and the belt support portion 91. When the endless belt 23 is heated, the temperature of the surface 23a of the endless belt 23 is preferably below 80 degrees, more preferably below 70 degrees Celsius, and further preferably below 60 degrees Celsius. When the temperature of the surface 23a of the endless belt 23 is within the above range, the reactivity of the resin particles contained in the ink composition may be suppressed, thereby making it easier to clean the belt. It should be noted that the lower limit of the temperature of the surface 23a of the endless belt 23 is preferably above 30 degrees Celsius, more preferably above 35 degrees Celsius, and further preferably above 40 degrees Celsius, as long as the adhesiveness of the adhesive layer is exerted. It should be noted that the temperature of the surface 23a of the endless belt 23 can be measured, for example, by a radiation thermometer, a contact thermometer, etc., and more preferably by a radiation thermometer.
[0228] When a heater is provided on at least one of the contact portion 69 and the belt support portion 91, a temperature detection portion (not shown) for detecting the surface temperature of the endless belt 23 may be provided. As the temperature detection portion, for example, a thermocouple or the like may be used. Thus, the control portion 1 controls the heater based on the temperature detected by the temperature detection portion, so that the endless belt 23 is at a predetermined temperature. It should be noted that a non-contact thermometer using infrared rays may also be used as the temperature detection portion.
[0229] 2.4. Printing Department
[0230] The printing unit 40 is arranged above (on the +Z axis side) relative to the arrangement position of the endless belt 23, and prints on the cloth 95 placed on the surface 23a of the endless belt 23. The printing unit 40 includes an inkjet head 42, a carriage 43 on which the inkjet head 42 is mounted, and a carriage moving unit 45 that moves the carriage 43 in the width direction (Y axis direction) of the cloth 95 intersecting the conveying direction.
[0231] The inkjet head 42 is a device that ejects a liquid composition supplied from a liquid box (not shown) from a plurality of nozzles and attaches it to a cloth 95 under the control of the control unit 1. The inkjet head 42 has a plurality of nozzles, and the plurality of nozzles eject the liquid composition to the cloth 95 to which the liquid composition is to be attached, and attaches it to the cloth 95. The above plurality of nozzles are arranged in a row to form a nozzle row, and the nozzle row is separately configured corresponding to the liquid composition. The liquid composition is supplied to the inkjet head 42 from each liquid box, and is ejected from the nozzle as droplets through a brake (not shown) in the inkjet head 42. The droplets of the ejected liquid composition fall on the cloth 95, forming images, texts, patterns, colors, etc. in the printing and dyeing area of the cloth 95.
[0232] The liquid composition mentioned here can be the above-mentioned reaction liquid composition, ink composition, resin-dispersed pigment ink composition, and clear ink composition. In addition, the type and amount of these liquid compositions can be appropriately set.
[0233] In the inkjet head, a piezoelectric element is used as a brake, and the brake is a driving device, but it is not limited to this method. For example, an electromechanical conversion element that displaces a vibration plate as a brake by electrostatic adsorption and an electrothermal conversion element that ejects a liquid composition as droplets by utilizing bubbles generated by heating can also be used.
[0234] Figure 2 FIG. 1 is a schematic diagram showing an example of an arrangement of inkjet heads. Figure 2 In the example of FIG. 4 , seven inkjet heads 42 a to 42 g are mounted on the carriage 43 , and each of the seven inkjet heads 42 a to 42 g has two nozzle rows 41 .
[0235] exist Figure 2 In the example, for example, it can be configured that no composition is ejected from the inkjet head 42a, a resin-dispersed pigment ink composition is ejected from the inkjet head 42b, an ink composition is ejected from the inkjet head 42c, a reaction liquid composition is ejected from the inkjet head 42d, an ink composition is ejected from the inkjet head 42e, a resin-dispersed pigment ink composition is ejected from the inkjet head 42f, and a transparent ink composition is ejected from the inkjet head 42g.
[0236] The arrangement and number of inkjet heads on the carriage 43 can be changed appropriately. The time interval for the attachment of each composition in the inkjet recording method of this embodiment can be adjusted by, for example, changing the interval d between the inkjet heads. In addition, the time interval for the attachment of each composition can also be adjusted by, for example, mounting a plurality of inkjet heads on the carriage 43 and depending on whether or not a composition is ejected from each head.
[0237] Each inkjet head can attach each composition to the same area of the fabric at appropriate timing in one main scan.
[0238] The carriage moving unit 45 is provided above the endless belt 23 (on the +Z axis side). The carriage moving unit 45 has a pair of guide rails 45a and 45b extending in the Y axis direction. The inkjet head 42 is supported by the guide rails 45a and 45b so as to be reciprocable along the Y axis direction together with the carriage 43.
[0239] The carriage moving part 45 has a moving mechanism and a power source which are not shown in the figure. As the moving mechanism, for example, a mechanism composed of a ball screw and a ball nut or a linear guide mechanism can be used. In addition, the carriage moving part 45 has a motor (not shown) as a power source for moving the carriage 43 along the guide rails 45a and 45b. As the motor, various motors such as a stepping motor, a servo motor, and a linear motor can be used. When the motor is driven by the control of the control unit 1, the inkjet head 42 moves along the Y-axis direction together with the carriage 43.
[0240] 2.5. Heating unit
[0241] The heating unit 27 can be provided between the conveying roller 26 and the conveying roller 28. The heating unit 27 heats the ink composition and the treatment liquid ejected onto the cloth 95. Thus, there is a tendency that the resin particles contained in the ink composition can be fully reacted. By fully reacting the resin particles, it is possible to form an image with good friction fastness. It should be noted that the heating unit 27 can also be used to dry the cloth 95. The heating unit 27 includes, for example, an IR heater, and by driving the IR heater, the ink composition and the treatment liquid ejected onto the cloth 95 can be reacted in a short time. Thus, the strip-shaped cloth 95 on which an image or the like is formed can be wound around the winding shaft portion 31.
[0242] 2.6. Cleaning unit
[0243] The cleaning unit 50 is disposed between the belt rotating roller 24 and the belt driving roller 25 along the X-axis direction. The cleaning unit 50 includes a cleaning portion 51, a pressing portion 52, and a moving portion 53. The moving portion 53 moves the cleaning unit 50 as a whole along the floor surface 99 and fixes it at a predetermined position.
[0244] The pressing part 52 is a lifting device composed of, for example, a cylinder 56 and a ball bushing 57, and the cleaning part 51 provided on the upper part thereof abuts against the surface 23a of the endless belt 23. The cleaning part 51 is hung between the belt rotating roller 24 and the belt driving roller 25 under a predetermined tension, and cleans the surface (supporting surface) 23a of the endless belt 23 moving from the belt driving roller 25 toward the belt rotating roller 24 from below (in the -Z-axis direction).
[0245] The cleaning section 51 includes a cleaning tank 54, a cleaning roller 58, and a scraper 55. The cleaning tank 54 is a tank for storing a cleaning liquid for cleaning ink or foreign matter attached to the surface 23a of the endless belt 23, and the cleaning roller 58 and the scraper 55 are provided inside the cleaning tank 54. As the cleaning liquid, for example, water and a water-soluble solvent (such as an alcohol aqueous solution) can be used, and a surfactant and a defoaming agent can be added as needed.
[0246] When the cleaning roller 58 rotates, the cleaning liquid is supplied to the surface 23a of the endless belt 23, and the cleaning roller 58 and the endless belt 23 slide. Thus, the ink composition and fibers of the cloth 95 attached to the endless belt 23 are removed by the cleaning roller 58.
[0247] The scraper 55 can be formed of a flexible material such as silicone rubber. The scraper 55 is provided downstream of the cleaning roller 58 in the conveying direction of the endless belt 23. The cleaning liquid remaining on the surface 23a of the endless belt 23 is removed by sliding between the endless belt 23 and the scraper 55.
[0248] According to such a recording device 100 , the recording method of this embodiment can be easily executed.
[0249] 3. Examples and Comparative Examples
[0250] The present invention is specifically described below by way of examples, but the present invention is not limited to these examples. In the following, unless otherwise specified, "parts" and "%" are weight standards. It should be noted that, unless otherwise specified, the evaluation was performed under an environment of a temperature of 25° C. and a relative humidity of 40.0%.
[0251] 3.1. Preparation of each composition
[0252] The reaction liquid composition, ink composition, and clear ink composition were prepared as follows.
[0253] 3.1.1. Preparation of reaction solution composition
[0254] Each component was placed in a container to form the composition shown in Table 1, mixed and stirred for 2 hours with a magnetic stirrer, and then filtered with a membrane filter having a pore size of 5 μm to obtain a reaction solution composition used in Examples and Comparative Examples. It should be noted that the numerical values in the table represent the solid content.
[0255] 3.1.2. Preparation of ink composition
[0256] Each component was placed in a container to obtain the composition shown in Table 2, mixed and stirred for 2 hours using a magnetic stirrer, and then filtered using a membrane filter having a pore size of 5 μm to obtain ink compositions for Examples and Comparative Examples. The numerical values in the table represent the solid content.
[0257] The anionic self-dispersible pigment, the anionic resin-dispersible pigment, and the anionic dispersant-dispersible pigment used a pigment dispersion prepared as follows.
[0258] <Anionic Self-Dispersible Pigments>
[0259] 500 g of bulk carbon black powder (primary particle size = 18 nm, BET specific surface area = 180 m 2 / g, DBP absorption = 186mL / 100g) was added with 3750g of ion exchange water, stirred with a dissolver, and heated to 45°C. Then, it was crushed by a sand mill using zirconium oxide beads with a diameter of 0.8mm, and at the same time, 30000g of an aqueous solution of sodium hypochlorite (effective chlorine concentration = 12%) was added dropwise at 45°C for 3.5 hours. Then, the sand mill was continued to crush for 30 minutes to obtain a reaction solution containing self-dispersible carbon black. The reaction solution was filtered with a 400-mesh screen to separate the zirconium oxide beads, unreacted carbon black and the reaction solution. A 5% aqueous solution of potassium hydroxide was added to the separated reaction solution to adjust the pH to 7.5. Desalination and purification were carried out by ultrafiltration membrane in a manner that the conductivity of the liquid became 1.5mS / cm. Desalination and purification were carried out again using an electrodialysis machine in a manner that the conductivity of the liquid became 1.0mS / cm. The liquid was concentrated so that the concentration of the self-dispersible carbon black was 17% by mass. The concentrated liquid was centrifuged to remove coarse particles and filtered with a 0.6 μm filter. Ion exchange water was added to the obtained filtrate, and the self-dispersible carbon black was diluted and dispersed so that the concentration was 15% by mass to obtain a self-dispersible pigment dispersion.
[0260] <Anionic Resin Dispersed Pigments>
[0261] To 15 parts by mass of carbon black, 10 parts by mass of ammonium salt of styrene-acrylic acid copolymer (weight average molecular weight 10,000) (as a polymer component) and 55 parts by mass of ion exchange water were added as a dispersant, and after being fully mixed, the mixture was dispersed together with glass beads (diameter 1.7 mm, 1.5 times the amount of the mixture) in a sand mill (manufactured by Yaskawa Seisakusho Co., Ltd.) for 2 hours. After dispersion, the glass beads were removed to obtain a resin-dispersed pigment dispersion.
[0262] <Anionic dispersant-dispersed pigment>
[0263] Pure water was added to 20% by mass of a pigment (CI Pigment Blue 15:3) and 7% by mass of a sodium hydroxide neutralized product of a styrene-acrylic acid copolymer (acid value 175 mgKOH / g, molecular weight 10,000) to make the total 100% by mass, and the mixture was stirred and mixed to obtain a mixture. The mixture was charged into a wet sand mill filled with zirconia beads having a diameter of 0.3 mm and dispersed for 6 hours. Then, the zirconia beads were removed by a separator and filtered with a cellulose acetate filter having a pore size of 3.0 μm, thereby obtaining a pigment dispersion A shown in the table. It should be noted that JONCRYL 678 (trade name, manufactured by BASF) was used as the styrene-acrylic acid copolymer. The volume average particle size D50 of the pigment in the obtained dispersion was 100 nm.
[0264] 3.1.3. Preparation of transparent ink composition
[0265] Each component was placed in a container to form the composition shown in Table 3, mixed and stirred for 2 hours with a magnetic stirrer, and then filtered with a membrane filter having a pore size of 5 μm to obtain treatment liquids used in Examples and Comparative Examples. It should be noted that the numerical values in the table represent the solid content.
[0266] Supplementary explanations are given for the abbreviations and product names shown in Tables 1 to 3.
[0267] ·OLFINE E1010: Acetylene glycol surfactant manufactured by Nissin Chemical Industry Co., Ltd.
[0268] PD002W: Acetylene glycol surfactant manufactured by Nissin Chemical Industry Co., Ltd.
[0269] · SILFACE SAG503A: Silicone surfactant manufactured by Nissin Chemical Industry Co., Ltd.
[0270] ·PROXEL XL2: manufactured by Lonza Japan. Preservative and antifungal agent
[0271] ·UW-1527F: ETERNACOLL UW series polyurethane resin manufactured by Ube Industries, Ltd.
[0272] PB15:3: Cyan pigment CI pigment blue 15:3
[0273] Evaluation methods
[0274] 3.2.1. Production of records
[0275] Printing was performed using a modified Evo Tre 16 (manufactured by Seiko Epson Corporation). A 100% cotton white wide cloth was used as the recording medium. The inkjet head used had a nozzle spacing of 600 dpi in the width direction of the recording medium and 600 nozzles.
[0276] As recording conditions, the recording resolution was set to 1200×600 dpi and the ink mass per line was set to 27 g / m 2 A solid pattern image was formed on an A3-sized cloth by four passes to obtain a printed product. The duty of the solid pattern of each composition was 100%. The printed product was heated in an oven at 160° C. for 3 minutes to dry it.
[0277] Here, the “solid pattern image” refers to an image in which dots are recorded in all pixels that are the minimum recording unit area defined by the recording resolution.
[0278] 3.2.2. Evaluation of color rendering
[0279] The OD value of black was measured for the printed product of each example using a fluorescence spectrometer ("FD-7", manufactured by Konica Minolta Inc.), and the color development was evaluated according to the following criteria. The results are shown in Tables 4 and 5.
[0280] AAA: OD value is above 1.50;
[0281] AA: OD value is above 1.47 and below 1.50;
[0282] A: OD value is above 1.44 and below 1.47;
[0283] B: OD value is above 1.41 and below 1.44;
[0284] C: OD value is lower than 1.41.
[0285] 3.2.3. Evaluation of blockage
[0286] Evaluation method: After continuous printing for 2 hours on a 100% pure cotton white wide cloth using the above device, the number of nozzles with dropped color (Bk) was counted using the nozzle check mode. Evaluation was performed according to the following criteria, and the results are shown in Tables 4 and 5.
[0287] AAA: less than 5;
[0288] AA: 5 or more and less than 10;
[0289] A: more than 10 and less than 15;
[0290] B: more than 15 and less than 20;
[0291] C: 20 or more and less than 30.
[0292] 3.3. Evaluation results
[0293] As can be seen from the tables, in each embodiment, there is: a first ink adhesion step, in which an ink composition containing a self-dispersible pigment is ejected by an inkjet method and attached to a fabric; a reaction liquid adhesion step, in which a reaction liquid composition is ejected by an inkjet method and attached to a fabric, the reaction liquid composition contains a coagulant that causes the components in the ink composition to coagulate; and a second ink adhesion step, in which an ink composition containing a self-dispersible pigment is ejected by an inkjet method and attached to a fabric, the first ink adhesion step, the reaction liquid adhesion step, and the second ink adhesion step are performed continuously in sequence, and the time difference from the adhesion of the ink composition by the first ink adhesion step to the adhesion of the reaction liquid composition to the area to which the ink composition is attached by the reaction liquid adhesion step is within 45 milliseconds, and the time difference from the adhesion of the reaction liquid composition by the reaction liquid adhesion step to the adhesion of the ink composition to the area to which the ink composition is attached by the second ink adhesion step is within 45 milliseconds, and as a result, the color development is good.
[0294] The present invention includes a configuration substantially the same as the configuration described in the embodiment, such as a configuration having the same function, method and result, or a configuration having the same purpose and effect. In addition, the present invention also includes a configuration formed by replacing a non-essential part of the configuration described in the embodiment. In addition, the present invention also includes a configuration that can play the same role and effect as the configuration described in the embodiment or a configuration that achieves the same purpose. In addition, the present invention also includes a configuration formed by adding a known technology to the configuration described in the embodiment.
[0295] The following contents are derived from the above-mentioned embodiment and modified examples.
[0296] The inkjet recording method has:
[0297] A first ink adhesion step of ejecting an ink composition containing a self-dispersible pigment by an inkjet method and adhering the ink composition to a fabric;
[0298] a reaction liquid attachment step of ejecting a reaction liquid composition by an inkjet method and attaching it to a cloth, wherein the reaction liquid composition contains a coagulant for aggregating components in the ink composition; and
[0299] In the second ink adhesion step, an ink composition containing a self-dispersible pigment is ejected by an inkjet method and adhered to the fabric.
[0300] The first ink attaching step, the reaction liquid attaching step and the second ink attaching step are performed successively in sequence.
[0301] The time difference from the time when the ink composition is attached by the first ink attaching step to the time when the reaction liquid composition is attached to the region to which the ink composition is attached by the reaction liquid attaching step is within 45 milliseconds.
[0302] The time difference from the reaction liquid composition being attached in the reaction liquid attaching step to the ink composition being attached to the region to which the reaction liquid composition is attached in the second ink attaching step is within 45 milliseconds.
[0303] According to the recording method, the ink composition is continuously attached in a very short time before and after the reaction liquid is attached to the cloth. As a result, the ink composition and the reaction liquid are easily mixed even on the cloth as an absorbent recording medium, and the coagulation reaction of the ink composition is easily carried out. As a result, the pigment in the ink is easy to stay near the surface of the cloth, which can make the color development good. In addition, since the self-dispersible pigment has a higher reactivity with the coagulant, it is easier to stay near the surface, which can make the color development good.
[0304] In the above-mentioned inkjet recording method,
[0305] Optionally, the self-dispersible pigment is a black pigment.
[0306] According to this recording method, since the self-dispersible pigment is a black pigment, the effect of improving the color development property is higher. This is because the color development property of black is easily deteriorated in pigment printing.
[0307] In the above-mentioned inkjet recording method,
[0308] Optionally, the coagulant is selected from polyvalent metal salts, cationic resins, and organic acids.
[0309] According to this recording method, the aggregation property of the self-dispersible pigment can be further improved.
[0310] In the above-mentioned inkjet recording method,
[0311] Optionally, the ink composition further contains resin particles,
[0312] The resin particles are self-dispersing resins.
[0313] According to this recording method, since the resin particles are self-dispersible resins, the rubbing fastness of the image can be improved while maintaining good color development. This is because when it is desired to mix a fixing resin in the ink composition, the pigment needs to be reduced, which tends to deteriorate the color development, but by making the fixing resin a self-dispersible resin, there is no need to reduce the pigment.
[0314] In the above-mentioned inkjet recording method,
[0315] Optionally, further comprising:
[0316] The resin dispersion pigment ink adhesion step is to eject a resin dispersion pigment ink composition containing a resin dispersion pigment by an inkjet method and adhere it to the fabric.
[0317] The resin-dispersed pigment ink attaching step is performed at least one of before the first ink attaching step and after the second ink attaching step.
[0318] The time difference from the resin-dispersed pigment ink composition being attached by the resin-dispersed pigment ink attaching step to the ink composition being attached to the area to which the resin-dispersed pigment ink composition is attached by the first ink attaching step is 7 milliseconds or more.
[0319] The time difference from the time when the ink composition is attached in the second ink attaching step to the time when the resin-dispersed pigment ink composition is attached to the region to which the ink composition is attached in the resin-dispersed pigment ink attaching step is 7 milliseconds or more.
[0320] According to this recording method, the time interval between the adhesion of the resin-dispersed pigment ink and the adhesion of the ink composition is relatively large, so that the resin-dispersed pigment ink droplets after dripping are easily wet and spread, the filling property of the image is improved, and the color development property becomes better.
[0321] In the above-mentioned inkjet recording method,
[0322] Optionally, the time difference from the resin-dispersed pigment ink composition being attached by the resin-dispersed pigment ink attaching step to the ink composition being attached to the area to which the resin-dispersed pigment ink composition is attached by the first ink attaching step is 45 milliseconds or less,
[0323] After the ink composition is attached in the second ink attaching step, a time difference between when the resin-dispersed pigment ink composition is attached to the region to which the ink composition is attached in the resin-dispersed pigment ink attaching step is 45 milliseconds or less.
[0324] According to this recording method, when the time interval between the adhesion of the resin-dispersed pigment ink and the adhesion of the ink composition is not too long, the distance between the nozzle ejecting the resin-dispersed pigment ink composition and the nozzle ejecting the reaction liquid composition can be made longer, thereby making it possible to achieve better ejection stability.
[0325] In the above-mentioned inkjet recording method,
[0326] Optionally, the resin-dispersed pigment ink composition may be a cyan ink.
[0327] According to this recording method, by using cyan ink to produce mixed color black, the color development property of black can be improved.
[0328] In the above-mentioned inkjet recording method,
[0329] Optionally, the resin dispersed pigment ink attachment process is performed after the second ink attachment process.
[0330] Further having:
[0331] The transparent ink attaching step is to eject the transparent ink composition containing the resin particles by the ink jet method and attach it to the cloth.
[0332] After the resin-dispersed pigment ink composition is attached in the resin-dispersed pigment ink attaching step, the clear ink composition is attached to the region to which the resin-dispersed pigment ink composition is attached in the clear ink attaching step.
[0333] According to this recording method, the image is coated with a transparent ink composition, so the fastness of the image is improved. In addition, the reduction in rubbing fastness caused by the colorant being retained near the surface of the cloth in order to improve the color development can be reduced.
[0334] In the above-mentioned inkjet recording method,
[0335] Optionally, the clear ink composition contains anionic resin particles.
[0336] According to this recording method, the transparent ink composition is easily aggregated and is less likely to be deposited on the cloth, so the color development property of the image is further improved.
[0337] In the above-mentioned inkjet recording method,
[0338] Optionally, the reaction liquid composition contains a polyol,
[0339] The content of the polyol in the reaction liquid composition is 80% by mass or more relative to the total amount of the organic solvent in the reaction liquid composition.
[0340] According to this recording method, since the permeability of the polyol is low, the reaction liquid is more likely to stay near the surface of the fabric, and the color development of the image can be improved.
[0341] In the above-mentioned inkjet recording method,
[0342] Optionally, the surface tension of the reaction liquid composition is greater than 28 mN / m.
[0343] According to this recording method, the reaction liquid composition has high surface tension and is less likely to scatter, and is less likely to generate mist during discharge, thereby making it possible to achieve better discharge stability.
Claims
1. An inkjet recording method, characterized in that: have: A first ink adhesion step of ejecting an ink composition containing a self-dispersible pigment by an inkjet method and adhering the ink composition to a fabric; a reaction liquid attachment step of ejecting a reaction liquid composition by an inkjet method and attaching it to a cloth, wherein the reaction liquid composition contains a coagulant for aggregating components in the ink composition; and In the second ink adhesion step, an ink composition containing a self-dispersible pigment is ejected by an inkjet method and adhered to the fabric. The first ink attaching step, the reaction liquid attaching step and the second ink attaching step are performed successively in sequence. The time difference from the attachment of the ink composition in the first ink attachment step to the attachment of the reaction liquid composition to the region to which the ink composition is attached in the reaction liquid attachment step is within 45 milliseconds, The time difference from the reaction liquid composition being attached in the reaction liquid attaching step to the ink composition being attached to the region to which the reaction liquid composition is attached in the second ink attaching step is within 45 milliseconds.
2. The inkjet recording method according to claim 1, wherein The self-dispersible pigment is a black pigment.
3. The inkjet recording method according to claim 1 or 2, wherein: The coagulant is selected from polyvalent metal salts, cationic resins, and organic acids.
4. The inkjet recording method according to claim 1 or 2, wherein: The ink composition further comprises resin particles, The resin particles are self-dispersing resins.
5. The inkjet recording method according to claim 1, wherein Also features: The resin dispersion pigment ink attaching step is to eject a resin dispersion pigment ink composition containing a resin dispersion pigment by an inkjet method and attach it to the fabric. The resin-dispersed pigment ink attaching step is performed at least one of before the first ink attaching step and after the second ink attaching step. The time difference from the resin-dispersed pigment ink composition being attached in the resin-dispersed pigment ink attaching step to the ink composition being attached to the area to which the resin-dispersed pigment ink composition is attached in the first ink attaching step is 7 milliseconds or more. The time difference from the attachment of the ink composition in the second ink attachment step to the attachment of the resin-dispersed pigment ink composition to the region to which the ink composition is attached in the resin-dispersed pigment ink attachment step is 7 milliseconds or more.
6. The inkjet recording method according to claim 5, wherein: The time difference from the resin-dispersed pigment ink composition being attached in the resin-dispersed pigment ink attaching step to the ink composition being attached to the area to which the resin-dispersed pigment ink composition is attached in the first ink attaching step is 45 milliseconds or less. The time difference from the attachment of the ink composition in the second ink attachment step to the attachment of the resin-dispersed pigment ink composition to the region to which the ink composition is attached in the resin-dispersed pigment ink attachment step is 45 milliseconds or less.
7. The inkjet recording method according to claim 5, wherein: The resin-dispersed pigment ink composition is a cyan ink.
8. The inkjet recording method according to any one of claims 5 to 7, wherein The resin dispersion pigment ink attaching step is performed after the second ink attaching step, and the inkjet recording method further comprises: The transparent ink attaching step is to eject the transparent ink composition containing the resin particles by the ink jet method and attach it to the cloth. After the resin-dispersed pigment ink composition is attached in the resin-dispersed pigment ink attaching step, the clear ink composition is attached to the region to which the resin-dispersed pigment ink composition is attached in the clear ink attaching step.
9. The inkjet recording method according to claim 8, wherein The clear ink composition contains anionic resin particles.
10. The inkjet recording method according to claim 1 or 2, wherein: The reaction liquid composition contains a polyol, The content of the polyol in the reaction liquid composition is 80% by mass or more relative to the total amount of the organic solvent in the reaction liquid composition.
11. The inkjet recording method according to claim 1 or 2, wherein: The surface tension of the reaction liquid composition is greater than or equal to 28 mN / m.
Citation Information
Patent Citations
Cartridge For Nucleic Acid Amplification Reaction And Cartridge Kit For Nucleic Acid Amplification Reaction
CN104673622A
Ink-jet textile printing ink, ink-jet printing process and instrument making use of the same, and processed article obtained
EP0620116A2
Ink-jet recording method
JP1997207424A
Aqueous inkjet ink composition, inkjet recording method and inkjet recording device
JP2018154805A
Ink set and recording method
US20190292391A1