Three-electrode lithium ion battery correction method

By setting three layers of diaphragm and reference electrode between the positive and negative electrode sheets of the battery cell, recording the potential difference and correcting the negative electrode potential, the problem of the diaphragm pressure difference affecting the potential is solved, and the accurate evaluation of the lithium-ion state of the battery cell is achieved and the charging ability is achieved. True reflection.

CN119069853APending Publication Date: 2024-12-03HEFEI GUOXUAN HIGH TECH POWER ENERGY
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202411145714.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

When the existing three-electrode lithium-ion battery is equipped with reference electrodes in the separator, the reference electrode potential cannot truly reflect the actual potential of the negative electrode due to the separator pressure difference, which affects the accuracy of the charging step and cannot accurately judge whether the battery cell is lithium-ionized. .

Method used

By setting three layers of diaphragms between the positive and negative electrode sheets of the battery cell and two reference electrodes between the diaphragms, the potential difference of the reference electrode is recorded to correct the actual potential of the negative electrode sheet and ensure the accuracy of the charging process.

Benefits of technology

This method can more accurately judge whether the battery cell is lithium-extracted, which truly reflects the charging ability of the battery cell at different temperatures and magnifications, solves the impact of the diaphragm pressure difference on the lithium-extracted potential, and improves the accuracy of the charging step.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119069853A_ABST
    Figure CN119069853A_ABST
Patent Text Reader

Abstract

The invention relates to a three-electrode lithium ion battery correction method which comprises the following steps: S1, preparing a three-electrode lithium ion battery, arranging three layers of diaphragms between a positive plate and a negative plate which are adjacent to each other in the three-electrode lithium ion battery, and arranging a reference electrode between any two adjacent diaphragms, the reference electrode close to the negative plate is defined as a reference electrode A, and the other reference electrode is defined as a reference electrode B; s2, charging the three-electrode lithium ion battery, and recording the potential VA of the first reference electrode and the potential VB of the second reference electrode; and S3, calculating to obtain a diaphragm pressure difference V diaphragm according to a formula V diaphragm = VA-VB, and correcting the actual potential of the negative plate in the charging process to V = VA + V diaphragm. According to the invention, by measuring the pressure difference of the diaphragm and correcting the actual potential of the negative plate in the charging process, whether the lithium precipitation condition of the battery cell occurs or not can be judged more accurately, and the charging capability of the battery cell at different temperatures and different multiplying powers can be truly reflected.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of lithium ion batteries, and in particular to a correction method for a three-electrode lithium ion battery. Background Art

[0002] Lithium-ion batteries have high energy density per unit volume / mass, no memory effect, low internal resistance, low self-discharge, and long cycle life, and are widely used in many industries. The design system of each battery cell is different according to different use areas and customer requirements; therefore, according to customer requirements or product positioning, a reasonable charging process should be formulated for each battery cell to ensure that the battery cell reaches full charge in the fastest time, without lithium deposition during the cycle, and reduce the rate of cell capacity attenuation and the risk of the diaphragm being pierced by lithium branch crystals.

[0003] The most effective method to analyze a single electrode during the battery charging and discharging process is to introduce a three-electrode system, which can effectively monitor the changes in the positive and negative electrode potentials relative to the reference electrode, and then analyze the electrochemical reactions occurring at each electrode.

[0004] The patent with publication number CN115360447A discloses a three-electrode lithium-ion battery, in which the reference electrode of the three-electrode lithium-ion battery is arranged between the positive electrode sheet and the negative electrode sheet at the outermost edge of the battery cell, and the reference electrode is inserted into the battery cell and covered with a first diaphragm and a second diaphragm. However, the three-electrode lithium-ion battery sets the reference electrode in the diaphragm, and because there is a diaphragm between the reference electrode and the negative electrode sheet, the potential of the reference electrode cannot truly reflect the actual potential of the negative electrode, and the position of the reference electrode in the electrode sheet is not clearly described. However, the different positions of the reference electrode in the electrode sheet will lead to potential differences during the charging process, and the corresponding reference electrode potential will also be different, and the lithium plating potential of the negative electrode cannot be accurately grasped, resulting in the charging process being not precise enough. Summary of the invention

[0005] Based on this, the purpose of the present invention is to provide a three-electrode lithium-ion battery correction method, which takes into account the position of the reference electrode and the diaphragm pressure difference, and corrects the actual potential of the negative electrode during the charging process. It can more accurately judge whether the battery cell is lithium-deposited, and truly reflect the charging capacity of the battery cell at different temperatures and different rates. It can solve the influence of the diaphragm pressure difference on the lithium deposition potential in the existing three-electrode evaluation method.

[0006] To achieve the above object, the present invention adopts the following technical solutions:

[0007] The present invention provides a three-electrode lithium-ion battery correction method, which comprises the following steps:

[0008] S1. Prepare a three-electrode lithium-ion battery, wherein three layers of separators are arranged between adjacent positive and negative electrode sheets, and a reference electrode is arranged between any two adjacent separators, the reference electrode close to the negative electrode sheet is defined as reference electrode A, and the other reference electrode is defined as reference electrode B;

[0009] S2. Charge the three-electrode lithium-ion battery and record the potential V of the reference electrode A. A , the potential of the reference electrode B is V B ;

[0010] S3. According to formula V 隔膜 =V A -V B Calculate the diaphragm pressure difference V 隔膜 , the actual potential of the negative electrode during charging is corrected to V = V A +V 隔膜 .

[0011] The present invention arranges a three-layer diaphragm between a positive and negative electrode sheet of the battery cell and arranges a reference electrode between any two adjacent diaphragms in the three-layer diaphragm. Meanwhile, considering the different positions of the reference electrodes, the three-electrode lithium-ion battery is charged and tested, and the potentials of the reference electrodes A and B are measured to obtain the diaphragm pressure difference V 隔膜 , the actual potential of the negative electrode during charging is corrected to V = V A +V 隔膜 It can more accurately judge whether the battery cell has lithium deposition, truly reflect the charging capacity of the battery cell at different temperatures and different rates, and solve the influence of the diaphragm pressure difference on the lithium deposition potential in the existing three-electrode evaluation method.

[0012] As a further improvement of the above solution of the present invention, the lengths of the reference electrodes A and B between the diaphragms are kept consistent and the positive projections of the reference electrodes A and B on the negative electrode sheet overlap. The reference electrodes A and B are kept consistent to ensure the accuracy of the diaphragm pressure difference.

[0013] As a further improvement of the above scheme of the present invention, an area is divided with the center of the negative electrode sheet as the center, and the width of the area is 60%-90% of the width of the negative electrode sheet; the ends of the reference electrode A and the reference electrode B located between the diaphragms are defined as the first end A and the first end B respectively, and the positive projections of the first end A and the first end B on the negative electrode sheet are both located in the area.

[0014] As a further improvement of the above solution of the present invention, the height of the region is 60%-90% of the height of the negative electrode sheet.

[0015] The current distribution and temperature distribution of the electrode are different, and the lithium deposition status at different positions of the negative electrode may also be different. This should also be considered when arranging the reference electrode. The reference electrode can be located in the middle or around the edge of the diaphragm, or at the diaphragm position corresponding to the negative electrode at the bottom of the tab. The specific position can be arranged according to needs to ensure that it can accurately judge whether the battery cell has lithium deposition and truly reflect the charging capacity of the battery cell at different temperatures and different rates.

[0016] As a further improvement of the above solution of the present invention, reference electrode A and reference electrode B are both copper wires with a diameter of 10-100 μm.

[0017] As a further improvement of the above solution of the present invention, the diameters of the reference electrodes A and B are 10-30 μm.

[0018] As a further improvement of the above scheme of the present invention, the section of reference electrode A and reference electrode B located between the diaphragms needs to be pretreated, and the pretreatment process is: soaking with concentrated sulfuric acid or grinding with sandpaper, then cleaning with anhydrous ethanol, and drying. The oxide layer on the surface of reference electrode A and reference electrode B is removed to ensure the accuracy of detection.

[0019] Compared with the prior art, the present invention has the following beneficial effects:

[0020] The present invention arranges a three-layer diaphragm between a positive and negative electrode sheet of the battery cell and arranges a reference electrode between any two adjacent diaphragms in the three-layer diaphragm. Meanwhile, considering the different positions of the reference electrodes, the three-electrode lithium-ion battery is charged and tested, and the potentials of the reference electrodes A and B are measured to obtain the diaphragm pressure difference V 隔膜 , the actual potential of the negative electrode during charging is corrected to V = V A +V 隔膜 It can more accurately judge whether the battery cell has lithium deposition, truly reflect the charging capacity of the battery cell at different temperatures and different rates, and solve the influence of the diaphragm pressure difference on the lithium deposition potential in the existing three-electrode evaluation method. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is a schematic diagram of the structure of a three-electrode lithium-ion battery in Example 1 of the present invention;

[0022] Figure 2 Schematic diagram of the structure of a three-electrode lithium-ion battery M in Example 1 of the present invention;

[0023] Figure 3 Schematic diagram of the structure of a three-electrode lithium-ion battery N in Example 1 of the present invention;

[0024] Figure 4 Schematic diagram of the structure of a three-electrode lithium-ion battery P in a comparative example of the present invention;

[0025] Figure 5 1 is a charging curve diagram of a three-electrode lithium-ion battery M and a three-electrode lithium-ion battery P;

[0026] Figure 6 1 is a charging curve diagram of a three-electrode lithium-ion battery M and a three-electrode lithium-ion battery N;

[0027] Figure 7 This is the negative electrode interface diagram of the three-electrode lithium-ion battery M and the three-electrode lithium-ion battery N when fully charged at 1.5C.

[0028] Figure numerals: 1, positive electrode sheet; 2, negative electrode sheet; 3, separator. DETAILED DESCRIPTION

[0029] For ease of understanding of the present invention, the present invention will be described more fully below in conjunction with specific embodiments. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thoroughly understood.

[0030] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used in the specification of the present invention herein are only for the purpose of describing specific embodiments and are not intended to limit the present invention.

[0031] Example 1

[0032] In view of the current three-electrode lithium-ion battery, when setting a reference electrode, it is necessary to set two layers of diaphragms between adjacent positive and negative electrode sheets, and then set a reference electrode between the two layers of diaphragms. Because there is a diaphragm between the reference electrode and the negative electrode sheet, the potential of the reference electrode cannot truly reflect the actual potential of the negative electrode, resulting in the charging process being set inaccurate. This embodiment proposes a three-electrode lithium-ion battery correction method, including the following steps:

[0033] S1. First prepare a three-electrode lithium-ion battery: Combine Figure 1 First, a positive electrode sheet 1 and a negative electrode sheet 2 are arranged in a continuous interval, and a diaphragm 3 is arranged between any adjacent positive electrode sheet 1 and negative electrode sheet 2, and three layers of diaphragms 3 are arranged between the adjacent positive electrode sheets 1 and negative electrode sheets 2, and a reference electrode is arranged between any two adjacent diaphragms 3 in the three layers of diaphragms 3, and the reference electrode close to the negative electrode sheet 2 is defined as reference electrode A, and the other reference electrode is defined as reference electrode B; the lithium ion battery cell with the reference electrode is assembled, sealed, injected, formed and divided. It should be noted that the ceramic and rubber surfaces on each diaphragm 3 are in the same direction.

[0034] In this embodiment, the region is divided with the center of the negative electrode sheet 2 as the center, the width of the region is 60%-90% of the width of the negative electrode sheet, and the height of the region is 60%-90% of the height of the negative electrode sheet; the ends of the reference electrode A and the reference electrode B located between the diaphragm 3 are defined as the first end A and the first end B, respectively, and the positive projections of the first end A and the first end B on the negative electrode sheet 2 are both located in the region. In other words, the reference electrode can be located in the middle or around the edge of the diaphragm, or at the diaphragm position corresponding to the negative electrode sheet at the lower part of the pole ear, and the specific position can be arranged according to needs.

[0035] In this embodiment, the reference electrode A and the reference electrode B of the three-electrode lithium-ion battery are both copper wires with a diameter of 10-100 μm, preferably 10-30 μm. The reference electrode A and the reference electrode B located between the diaphragms need to be pretreated, and the pretreatment process is: soaking in concentrated sulfuric acid or grinding with sandpaper, and then cleaning with anhydrous ethanol.

[0036] S2. Charge the three-electrode lithium-ion battery and record the potential V of the reference electrode A of the three-electrode lithium-ion battery. A , the potential of the reference electrode B is V B .

[0037] S3. According to formula V 隔膜 =V A -V B Calculate the diaphragm pressure difference V 隔膜 , the actual potential of the negative electrode during charging is corrected to V = V A +V 隔膜 .

[0038] According to the above method, two three-electrode lithium-ion batteries are prepared, and the two three-electrode lithium-ion batteries are respectively defined as three-electrode lithium-ion battery M and three-electrode lithium-ion battery N. Figure 2 In the three-electrode lithium-ion battery M of this embodiment: the lengths of the reference electrodes A and B between the diaphragms are kept consistent and the positive projections of the reference electrodes A and B on the negative electrode sheet overlap. The ends of the reference electrodes A and B between the diaphragms are defined as the first end A and the first end B, respectively. The positive projections of the first end A and the first end B on the negative electrode sheet are both located at the center of the negative electrode sheet. Figure 3 In the three-electrode lithium-ion battery N of this embodiment: the lengths of the reference electrode A and the reference electrode B between the diaphragms are kept consistent and the orthographic projections of the reference electrode A and the reference electrode B on the negative electrode sheet coincide; the ends of the reference electrode A and the reference electrode B between the diaphragms are defined as the first end A and the first end B, respectively, and the orthographic projections of the first end A and the first end B on the negative electrode sheet are both at the edge of the short side of the negative electrode sheet and the distance between the short side edge and the negative electrode sheet is 10% of the width of the negative electrode sheet.

[0039] The three-electrode lithium-ion battery M and the three-electrode lithium-ion battery N were charged at 0.33C and 1.5C respectively, and the three-electrode lithium-ion battery M was also charged at 0.5C. The potential V of the reference electrode A of each three-electrode lithium-ion battery was recorded. A , the potential of the reference electrode B is V B .

[0040] Comparative Example

[0041] This comparative example adopts the same implementation method as Example 1, and the difference from Example 1 is that: Figure 4 As shown, a three-electrode lithium-ion battery P is prepared in this comparative example, wherein two layers of separators 3 are arranged between adjacent positive electrode sheets 1 and negative electrode sheets 2 of the three-electrode lithium-ion battery P, and a reference electrode C is arranged between the two layers of separators 3, and the end of the reference electrode C located between the separators is defined as the first end C, and the positive projection of the first end C on the negative electrode sheet is located at the center of the negative electrode sheet; the three-electrode lithium-ion battery P is charged at 2.5C, and the potential V of the reference electrode C is recorded. C .

[0042] Figure 5 The charging curves of the three-electrode lithium-ion battery M and the three-electrode lithium-ion battery P are shown in FIG. In the three-electrode lithium-ion battery M, a layer of diaphragm 3 is placed between the reference electrode A and the negative electrode sheet, and two layers of diaphragm 3 are placed between the reference electrode B and the negative electrode sheet. Figure 5 It can be seen that under the same charging SOC, the potential of reference electrode B is small, indicating that there is a voltage difference in the setting of the diaphragm, which cannot truly reflect the lithium deposition potential on the negative electrode surface. By calculating the potential difference between reference electrode A and reference electrode B, the diaphragm pressure difference of each diaphragm layer can be obtained, V 隔膜 =V A -V B , the potential of the reference potential A needs to be corrected, so the actual potential during the negative electrode charging process is: V = V A +V 隔膜 It can be seen that the actual potential of the negative electrode is higher than that of the reference electrode, which can further improve the charging rate of the battery cell; at the same time, it can be seen that at different charging rates, at the same SOC, the potential value of the reference electrode C is lower, and there is more lithium on the surface of the negative electrode sheet, which cannot be embedded into the negative electrode sheet in time. At high SOC, the negative electrode potential can reach 0V or below.

[0043] Figure 6 The charging curves of the three-electrode lithium-ion battery M and the three-electrode lithium-ion battery N at a small rate of 0.33C and a large rate of 1.5C are shown in FIG. Figure 6It can be seen that at a small rate, such as 0.33C, at the same SOC, the reference electrode potentials at the middle and edge positions of the electrode are basically the same; while at a large rate of 1.5C, at the same SOC, especially after 90% SOC, the reference potential value in the middle area is smaller than that in the edge area, indicating that the charge state in the middle area is larger than that in the edge area, and it is easier to reach or reach the lithium deposition potential first. Figure 7 When the negative electrode interface is disassembled under full charge at 1.5C, it can be seen that lithium deposition in the middle area is easier than at the edge.

[0044] The above comparison shows that setting up three electrodes can non-destructively detect the lithium deposition state of the battery cell, but the pressure difference of the diaphragm needs to be considered, and the reference potential needs to be corrected to more accurately reflect the potential of the negative electrode; secondly, due to the different current distribution and temperature distribution of the electrode, the lithium deposition state at different positions of the negative electrode may also be different. When arranging the reference electrode, this should also be considered. At a small rate, the potential difference at different positions of the electrode is not large, but at a larger rate, the potential difference of the negative electrode is large. When setting up three electrodes, they need to be arranged at different positions to better reflect the charging capacity of the battery cell.

[0045] The reference electrode setting method of this embodiment is applicable to ternary, lithium iron (manganese) phosphate and lithium cobalt oxide batteries in soft packs or square shells.

[0046] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0047] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. A three-electrode lithium-ion battery correction method, characterized in that: It includes the following steps: S1. Prepare a three-electrode lithium-ion battery, wherein three layers of separators are arranged between adjacent positive and negative electrode sheets, and a reference electrode is arranged between any two adjacent separators, the reference electrode close to the negative electrode sheet is defined as reference electrode A, and the other reference electrode is defined as reference electrode B; S2. Charge the three-electrode lithium-ion battery and record the potential V of the reference electrode A. A , the potential of the reference electrode B is V B ; S3. According to formula V 隔膜 =V A -V B Calculate the diaphragm pressure difference V 隔膜 , the actual potential of the negative electrode during charging is corrected to V = V A +V 隔膜 .

2. The three-electrode lithium-ion battery repair method according to claim 1, characterized in that: The lengths of the reference electrode A and the reference electrode B between the diaphragms remain consistent and the positive projections of the reference electrode A and the reference electrode B on the negative electrode sheet overlap.

3. The three-electrode lithium-ion battery repair method according to claim 2, characterized in that: An area is divided with the center of the negative electrode sheet as the center, and the width of the area is 60%-90% of the width of the negative electrode sheet; the ends of the reference electrode A and the reference electrode B located between the diaphragms are defined as the first end A and the first end B, respectively, and the positive projections of the first end A and the first end B on the negative electrode sheet are both located in the area.

4. The three-electrode lithium-ion battery repair method according to claim 3, characterized in that: The height of the region is 60%-90% of the height of the negative electrode sheet.

5. The three-electrode lithium-ion battery repair method according to claim 1, characterized in that: Reference electrode A and reference electrode B are both copper wires with a diameter of 10-100 μm.

6. The three-electrode lithium-ion battery repair method according to claim 4, characterized in that: The diameters of reference electrode A and reference electrode B are 10-30 μm.

7. The three-electrode lithium-ion battery repair method according to claim 1, characterized in that: The section of reference electrode A and reference electrode B between the diaphragms needs to be pretreated. The pretreatment process is: soaking with concentrated sulfuric acid or grinding with sandpaper, then cleaning with anhydrous ethanol and drying.

Citation Information

Patent Citations

  • Copper-silicon composite anode material, preparation method thereof and lithium battery containing same

    CN108232149A

  • Experiment method for monitoring cathode lithium precipitation via use of reference electrode

    CN108427077A

  • Method for representing lithium ion concentration change in electrolyte during cyclic process

    CN108519410A

  • Three-electrode cell structure and preparation method thereof, and method for testing potential of negative electrode

    CN113258156A

  • Three-electrode performance testing device for sodium-ion battery and use method of three-electrode performance testing device