High density resistive random access memory (RRAM)
The RRAM cell structure with a silicided semiconductor fin and configurable dielectric layer addresses the need for high-density applications by enabling efficient conductive and non-conductive states for data storage.
Patent Information
- Application Number
- CN202411175486.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2015-04-16
- Filing Date
- 2015-12-30
- Publication Date
- 2024-12-03
AI Technical Summary
There is a need for a resistive random access memory (RRAM) cell structure suitable for high-density applications.
A nonvolatile integrated circuit memory cell is designed with a resistive random access memory structure comprising a silicided semiconductor fin, a dielectric material layer with configurable resistance properties, and metal electrodes, integrated with a transistor and interconnects to support high-density fabrication.
The proposed structure enables high-density RRAM fabrication and efficient operation by forming conductive and non-conductive states for data storage, supporting high-density memory applications.
Smart Images

Figure CN119072134A_ABST
Abstract
Description
[0001] Divisional Application Instructions
[0002] This application is a divisional application of the Chinese patent application with the application date of December 30, 2015, application number 201910990201.3, and name “High-density resistive random access memory (RRAM)”. Technical Field
[0003] The present invention relates to integrated circuits and in particular to semiconductor non-volatile memories of the resistive random access memory (RRAM) type. Background Art
[0004] Regarding non-volatile integrated circuit memory devices, resistive random access memory (RRAM) is an emerging technology. RRAM devices are memory structures that use resistance values (rather than charge) to store data bits. Each RRAM cell includes a resistive material layer, the resistance value of which can be changed to represent the storage of a logical "0" data bit or a logical "1" data bit. The resistive material (usually in the form of a dielectric layer) can be made to conduct electricity through a filament or conductive path formed by applying a first programming voltage across the dielectric layer. In the conductive state, the cell is programmed to store one of a logical "0" data value or a logical "1" data value. The filament or conductive path can be reset by applying a second programming voltage across the dielectric layer, causing the dielectric layer to be non-conductive. In the non-conductive state, the cell is programmed to store the other of a logical "0" data value or a logical "1" data value.
[0005] There is a need in the art to provide a RRAM cell structure suitable for high-density applications. Summary of the invention
[0006] In an embodiment, a nonvolatile integrated circuit memory cell includes: a supporting substrate; a resistive random access memory structure, which includes: a first electrode, the first electrode including a silicided semiconductor fin on the supporting substrate and a first metal liner layer covering the silicided semiconductor fin; a dielectric material layer, the dielectric material layer having configurable resistance properties and covering at least a portion of the first metal liner layer; and a second electrode, the second electrode including a second metal liner layer covering the dielectric material layer and a metal filler in contact with the second metal liner layer; a transistor, the transistor having a first source-drain terminal connected to one of the first electrode and the second electrode; a source line, the source line connected to a second source-drain terminal of the transistor; a word line, the word line connected to a gate terminal of the transistor; and a bit line, the bit line connected to the other of the first electrode and the second electrode.
[0007] In an embodiment, a resistive random access memory (RRAM) structure includes: a supporting substrate; a first electrode, the first electrode including a silicided semiconductor fin on the supporting substrate and a first metal liner layer covering the silicided semiconductor fin; a dielectric material layer, the dielectric material layer having configurable resistance properties and covering at least a portion of the first metal liner layer; and a second electrode, the second electrode including: a second metal liner layer covering the dielectric material layer and a metal filler in contact with the second metal liner layer.
[0008] In an embodiment, a method includes: patterning a semiconductor material to form a semiconductor fin on a supporting substrate; silicideing the semiconductor fin to produce a silicided semiconductor fin; depositing a first metal liner layer, the first metal liner layer covering the silicided semiconductor fin; depositing a dielectric material layer, the dielectric material layer having configurable resistance properties and covering the first metal liner layer; depositing a second metal liner layer, the second metal liner layer covering the dielectric material layer; depositing a metal filler on each side of the silicided semiconductor fin in contact with the second metal liner layer; electrically contacting the first metal liner layer and the silicided semiconductor fin to provide a first electrode of a resistive random access memory (RRAM) structure; and electrically contacting the metal filler and the second metal liner layer to provide a second electrode of the RRAM structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] For a better understanding of the embodiments, reference will now be made, by way of example only, to the accompanying drawings, in which:
[0010] Figures 1 to 11 Process steps for forming a resistive random access memory (RRAM) structure for use in a nonvolatile memory cell are shown;
[0011] Fig.12 is a schematic diagram of a non-volatile memory cell incorporating a RRAM structure; and
[0012] Figures 13 to 23 Process steps for forming a RRAM structure for use in a nonvolatile memory cell are shown. DETAILED DESCRIPTION
[0013] Now refer to Figures 1 to 11 , Figures 1 to 11 Process steps for forming a resistive random access memory (RRAM) structure for use in a nonvolatile memory cell are shown. It will be understood that the drawings do not necessarily show features that are drawn to scale.
[0014] Figure 1A silicon-on-insulator (SOI) semiconductor substrate 10 is shown, which includes a stacked semiconductor substrate 12, an insulating layer 14, and a semiconductor layer 16. The semiconductor layer 16 may be doped, or alternatively may be undoped (in which case the SOI substrate 10 is of the "fully depleted" type) depending on the application. For example, the semiconductor layer 16 may have a thickness of 35nm-50nm. The insulating layer 14 is generally referred to in the art as a buried oxide (BOX) layer.
[0015] Then, a layer including silicon dioxide (SiO 2 ) layer 32 and a silicon nitride (SiN) layer 34. For example, the silicon dioxide layer 32 may be deposited using a chemical vapor deposition (CVD) process with a thickness of, for example, about 3 nm-10 nm. For example, the silicon nitride layer 34 may be deposited using a chemical vapor deposition (CVD) process with a thickness of, for example, about 20 nm-40 nm. Figure 2 The results are shown in .
[0016] A plurality of fins 100 are then defined from the semiconductor layer 16 using a photolithography process known in the art. The hard mask 30 is patterned to leave mask material 36 at the desired locations of the fins 100. An etching operation is then performed through the mask to open a plurality of holes 102 on each side of each fin 100. In a preferred embodiment, the etching that defines the fins 100 extends to a depth that reaches the insulating layer 14. The fins 100 may have a width (w) of 6nm-12nm and a pitch (p) of 25nm-45nm (with a spacing between adjacent fins of 15nm-35nm). The results of the etching process are shown in FIG. Figure 3 middle.
[0017] Outside of the region 18 where the fins 100 are located, an insulator such as for shallow trench isolation (STI) is raised as shown at reference numeral 20. This can be achieved, for example, by depositing a flowable oxide on the substrate, followed by patterning and removing the oxide in the region 18 of the fins 100. The mask material 36 is also removed. Figure 4 The results are shown in .
[0018] Then, as in Figure 5 As shown in FIG. 1 , a nickel platinum (NiPt) layer 110 is deposited to cover the fins 100. For example, the layer 110 may have a thickness of 3 nm to 10 nm. Then, an anneal is performed (e.g., at 400° C. with an optional laser anneal at 800° C.). The anneal converts at least a portion of the silicon material of the fins 100 into a metal silicide (e.g., NiSi x) in order to convert the silicon fin material to form a plurality of silicided fins 112. The unreacted portions of layer 110 are removed after the annealing. In an embodiment, the dimensions of the fins 100, the thickness of layer 110, the materials used, and the nature of the annealing performed are selected so that the silicided fins 112 are fully silicided structures (in which case all of the semiconductor material of the fins 100 is converted to silicide). Figure 6 The results are shown in . The silicided fin 112 provides one electrode of the RRAM structure.
[0019] A liner layer 120 of a metal material (such as, for example, titanium nitride TiN) is deposited using a chemical vapor deposition (CVD) process to cover the silicided fins 112 and the insulating layer 14. For example, the layer 120 may have a thickness of 5 nm-10 nm. A dielectric material (such as, for example, hafnium oxide HfO) is deposited using an atomic layer deposition (ALD) process. 2 ) layer 122 to cover metal layer 120. A patterning operation is performed to provide removal of layer 120 and layer 122 outside of region 18. Figure 7 The results are shown in Figure 7 Focus now on region 18. Layer 120 assists in forming a low resistance state across dielectric layer 122 for RRAM operation.
[0020] A liner layer 124 of a metal material (such as, for example, titanium nitride TiN) is deposited using a chemical vapor deposition (CVD) process to cover layer 122. For example, layer 124 may have a thickness of 5 nm-10 nm. Region 18 is then filled with a metal material (such as, for example, tungsten) to provide a metal fill 126. A chemical mechanical polishing (CMP) operation is performed to planarize the top surface of fill 126 at a level coplanar with layer 124. Figure 8 The result is shown in . Layer 124 assists in forming a low resistance state across dielectric layer 122 for RRAM operation. Metal fill 126 provides another electrode of the RRAM structure.
[0021] Then, a wet etching process is used to recess the top surface of the metal fill 126 to a level below the top surface of the silicided fins 112. For example, the depth d of this recessing process can be 10nm-20nm. The portion of the layer 124 located above the top surface of the recessed metal fill 126' is also removed (e.g., using a wet stripping process). The portion of the layer 122 located above the top surface of the recessed metal fill 126' is also removed (e.g., using a wet stripping process). Fig. 9 The results are shown in .
[0022] Then, a conformal insulating material deposition is performed, wherein a subsequent directional etch is performed to define a plurality of sidewall spacers 130 on the side surfaces of the layer 120 on each side of the silicided fins 112. Fig.10 The results are shown in .
[0023] Then, various conventional back-end-of-line (BEOL) processes are performed to deposit and planarize the pre-metallization dielectric (PMD) layer 140 and to form metal contacts 150 and 152. Fig.11 The result is shown in . One or more metallization layers may then be provided over the PMD layer 140 to assist in making circuit interconnects to the contacts 150 and 152 .
[0024] Accordingly, the resistive random access memory structure 200 is formed to include a first metal plate or electrode (layer 120 on the silicided fin 112), a dielectric layer 122, and a second metal plate (layer 124 and recessed fill 126'). It will be noted that the structure 200 includes two fins 112, but this is by way of example only, and it should be understood that each structure 200 can be formed by patterning and silicideing any suitable number of fins 112. The structure 200 can be included in a non-volatile memory cell 202, such as in Fig.12 1 and 2. The cell 202 includes a transistor 204 having a first source-drain region connected to a first metal plate of the structure 200 via a contact 152 and a second source-drain region connected to a source line SL. The transistor 204 may be supported by or integrated within the substrate 10, wherein the transistor is manufactured using a variety of well-known transistor manufacturing techniques before or simultaneously with the manufacture of the structure 200. A word line (WL) for the cell 202 is connected to a gate terminal of the transistor 204. A bit line (BL) for the cell 202 is connected to a second metal plate of the structure 200 via a contact 150. Source lines, word lines, and bit lines may be provided using (and / or coupled to) these metallization layers.
[0025] Because of the use of fins, the resulting structure supports high-density RRAM fabrication.
[0026] The operation of the RRAM structure within the memory cell is as follows: When the word line is set to logic high, transistor 204 is turned on. The source line is preset to logic high. If the bit line voltage is set to >0.85V, a conductive wire is formed in the hafnium oxide dielectric layer. The current rises and the cell enters a low resistance state. The source line is then discharged and the voltage decreases. When the bit line voltage is set below -1.25V (which is the reset voltage) and the word line is set to logic high, the conductive wire dissolves and the cell returns to a high resistance state.
[0027] Now refer to Figures 13 to 23 , Figures 13 to 23 Process steps for forming a RRAM structure for use in a non-volatile memory cell are shown.It will be understood that the drawings do not necessarily show features that are drawn to scale.
[0028] Fig.13 A bulk semiconductor substrate 10' is shown including a semiconductor layer 16'. The semiconductor layer 16' may be doped, or alternatively may be undoped, depending on the application. For example, the semiconductor layer 16' may have a thickness of 30nm-80nm.
[0029] Then, a layer including silicon dioxide (SiO 2 ) layer 32 and a silicon nitride (SiN) layer 34. For example, the silicon dioxide layer 32 may be deposited using a chemical vapor deposition (CVD) process with a thickness of, for example, about 3 nm-10 nm. For example, the silicon nitride layer 34 may be deposited using a chemical vapor deposition (CVD) process with a thickness of, for example, about 20 nm-40 nm. Fig.14 The results are shown in .
[0030] A photolithography process known in the art is then used to define a plurality of fins 100' from an upper portion of the semiconductor layer 16'. The hard mask 30 is patterned to leave mask material 36 at the desired locations of the fins 100'. An etching operation is then performed through the mask to open a plurality of holes 102' on each side of each fin 100'. In a preferred embodiment, the etch that defines the fins 100' extends to a depth of 35nm-50nm from the top surface of the semiconductor layer 16'. The fins 100 may have a width (w) of 6nm-12nm and a pitch (p) of 25nm-45nm (with a spacing between adjacent fins of 15nm-35nm). The results of the etching process are shown in FIG. Fig.15 middle.
[0031] The deposition of the flowable oxide material is performed and then planarized using a chemical mechanical polishing (CMP) process. In the region 18 where the fins 100' are located, the flowable oxide material deposition is recessed using a dry etching process so as to leave an insulating layer 22 around the bottom portion 114 of the fins 100'. Outside of the region 18, the insulation is raised as shown at reference numeral 20. The masking material 36 is also removed. Fig.16 The results are shown in .
[0032] Then, as in Fig.17As shown in FIG. 1 , a nickel platinum (NiPt) layer 110 is deposited to cover the fins 100 ′. For example, the layer 110 may have a thickness of 3 nm-10 nm. Then, an anneal is performed (e.g., at 400° C., with an optional laser anneal at 800° C.). The anneal converts at least a portion of the silicon material within the upper portion 113 of the fins 100 ′ into a metal silicide (e.g., NiSi x ) in order to convert the silicon fin material to form a plurality of silicided fins 112'. The unreacted portions of layer 110 are removed. In an embodiment, the dimensions of the fins 100', the thickness of layer 110', the materials used, and the nature of the annealing performed are selected so that these silicided fins 112' are fully silicided structures (in this case, all of the semiconductor material of the fins 100' within the upper portion 113 is converted to silicide). Fig.18 The result is shown in . It will be noted that the bottom 114 of the fin 100', made of non-silicided semiconductor material, remains to support each fin 112'. The silicided fin 112' provides one electrode of the RRAM structure.
[0033] A liner layer 120 of a metal material (such as, for example, titanium nitride TiN) is deposited using a chemical vapor deposition (CVD) process to cover the silicided fins 112' and the insulating layer 22. For example, the layer 120 may have a thickness of 5 nm-10 nm. A dielectric material (such as, for example, hafnium oxide HfO) is deposited using an atomic layer deposition (ALD) process. 2 ) layer 122 to cover metal layer 120. A patterning operation is performed to permit removal of layer 120 and layer 122 outside of region 18. Fig.19 The results are shown in , focusing now on region 18. Layer 120 assists in forming a low resistance state across dielectric layer 122 for RRAM operation.
[0034] A liner layer 124 of a metal material (such as, for example, titanium nitride TiN) is deposited using a chemical vapor deposition (CVD) process to cover layer 122. For example, layer 124 may have a thickness of 5 nm-10 nm. Region 18 is then filled with a metal material (such as, for example, tungsten) to provide a metal fill 126. A chemical mechanical polishing (CMP) operation is performed to planarize the top surface of fill 126 at a level coplanar with layer 124. Fig. 20 The result is shown in . Layer 124 assists in forming a low resistance state across dielectric layer 122 for RRAM operation. Metal fill 126 provides another electrode of the RRAM structure.
[0035] Then, a wet etching process is used to recess the top surface of the metal fill 126 to a level below the top surface of the silicided fins 112'. For example, the depth d of this recessing process can be 10nm-20nm. The portion of the layer 124 located above the top surface of the recessed metal fill 126' is also removed (e.g., using a wet stripping process). The portion of the layer 122 located above the top surface of the recessed metal fill 126' is also removed (e.g., using a wet stripping process). Fig.21 The results are shown in .
[0036] Then, a conformal insulating material deposition is performed, wherein a subsequent directional etch is performed to define a plurality of sidewall spacers 130 on the side surfaces of the layer 120 on each side of the silicided fins 112'. Fig. 22 The results are shown in .
[0037] Then, various conventional back-end-of-line (BEOL) processes are performed to deposit and planarize the pre-metallization dielectric (PMD) layer 140 and to form metal contacts 150 and 152. Fig.23 The result is shown in . One or more metallization layers may then be provided over the PMD layer 140 to assist in making circuit interconnects to the contacts 150 and 152 .
[0038] Accordingly, the resistive random access memory structure 200 is formed to include a first metal plate (layer 120 on the silicided fin 112'), a dielectric layer 122, and a second metal plate (layer 124 and recessed fill 126'). It will be noted that the structure 200 includes two fins 112', but this is merely by way of example, and it should be understood that each structure 200 can be formed by patterning and silicideing any suitable number of fins 112'. The structure 200 can be included in a non-volatile memory cell 202, such as in Fig.12 Schematically shown in (described previously).
[0039] The foregoing description has been provided by way of illustrative and non-limiting examples of a complete and informative description of exemplary embodiments of the present invention. However, various modifications and adaptations will become apparent to those skilled in the relevant art in view of the foregoing description when this specification is read in conjunction with the accompanying drawings and the appended claims. However, all such and similar modifications to the present teachings will still fall within the scope of the present invention as determined by the appended claims.
Claims
1. A method comprising: electrically coupling a first conductive terminal of a transistor to a first electrode of a resistive random access memory (RRAM) device, electrically coupling a second conductive terminal of the transistor to a source line, and electrically coupling a control terminal of the transistor to a word line; electrically coupling a bit line to a second electrode of the RRAM device; asserting the word line and the source line so that the transistor is turned on; setting the bit line to a read voltage threshold so that current flowing through the transistor and into the first electrode and through the first silicided semiconductor fin of the RRAM device forms a conductive path in a hafnium oxide layer stacked on the first silicided semiconductor fin of the RRAM device; discharging the source line; as well as The bit line is reset to break up the conductive path.
2. The method according to claim 1, wherein: The conductive path includes conductive filaments.